Semiconductor device structure and method of forming the same
Patent Information
- Application Number
- TW114105457
- Authority / Receiving Office
- TW · TW
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2024-12-19
- Filing Date
- 2025-02-14
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2045-02-13
AI Technical Summary
The complexity and manufacturing challenges increase as integrated circuits shrink in size, necessitating improved methods for processing and manufacturing.
A semiconductor device structure is developed with specific layers and materials, including an interlayer dielectric layer, semiconductor materials, and conductive structures, formed through various deposition and etching processes to create nanostructured transistors.
This structure facilitates the production of smaller and more complex integrated circuits, enhancing production capacity and reducing manufacturing costs while maintaining structural integrity.
Smart Images

Figure TWG2TB001920449_001 
Figure TWG2TB001920449_002 
Figure TWG2TB001920449_003
Abstract
Description
[Technical Field]
[0001] Embodiments of the present invention relate to semiconductor device structures, and particularly to layered materials with epitaxial structures. [Previous Technology]
[0002] The semiconductor integrated circuit industry has experienced exponential growth. Technological advancements in integrated circuit materials and design have enabled each generation of integrated circuits to have smaller and more complex circuits than the previous generation. In the evolution of integrated circuits, functional density (i.e., the number of interconnect devices per unit wafer area) typically increases as the geometry (i.e., the smallest component or line that the manufacturing process can produce) shrinks. Shrinking processes generally facilitate increased production capacity and reduced associated costs. Shrinking also increases the complexity of handling and manufacturing integrated circuits.
[0003] Therefore, it is necessary to improve the methods for processing and manufacturing integrated circuits. [Summary of the Invention]
[0004] One embodiment is a semiconductor device structure. The structure includes an interlayer dielectric layer; a first semiconductor material adjacent to the interlayer dielectric layer; and a second semiconductor material located on the first semiconductor material. The second semiconductor material covers a first portion of a side surface of the first semiconductor material. The structure further includes a silicon layer located on the second semiconductor material; and a first conductive structure located on the silicon layer.
[0005] Another embodiment is a semiconductor device structure. The structure includes an interlayer dielectric layer; a first semiconductor material adjacent to the interlayer dielectric layer; a semiconductor layer adjacent to the first semiconductor material; a second semiconductor material located between the semiconductor layer and the first semiconductor material; and a third semiconductor material located on the first semiconductor material. The third semiconductor material covers at least two sides of the first semiconductor material. The structure further includes a silicon compound layer located on the third semiconductor material; and a conductive structure located on the silicon compound layer.
[0006] Another embodiment is a method for forming a semiconductor device structure. The method includes forming a first semiconductor material on a substrate; forming an interlayer dielectric layer on the first semiconductor material; flipping the substrate; forming an opening in the substrate to expose the first semiconductor material; widening the opening; and forming a second semiconductor material on the first semiconductor material. The second semiconductor material covers a portion of the side surface of the first semiconductor material. The method further includes depositing a silicon layer on the second semiconductor material; and depositing a conductive structure on the silicon layer.
Implementation Method
[0008] The following detailed description is illustrated in conjunction with the accompanying drawings to facilitate understanding of various aspects of the invention. It is worth noting that the various structures are for illustrative purposes only and are not drawn to scale, as is customary in the art. In practice, the dimensions of various structures may be arbitrarily increased or decreased for clarity of explanation.
[0009] The different embodiments or examples provided below can implement different structures of the present invention. The specific components and arrangements described below are intended to simplify the content of the present invention and not to limit the present invention. For example, the description of forming a first component on a second component includes embodiments in which the two are in direct contact, or embodiments in which the two are separated by other additional components and are not in direct contact. Furthermore, multiple embodiments of the present invention may use the same reference numerals repeatedly for brevity, but elements with the same reference numerals in various embodiments and / or arrangements do not necessarily have the same correspondence.
[0010] In addition, spatial relative terms such as "below," "below," "lower," "above," "higher," or similar terms are used to describe the relationship between some elements or structures in the diagram and another element or structure. These spatial relative terms include different orientations of the device in use or operation, as well as the orientations described in the diagram. When the device is turned in a different orientation (rotated 90 degrees or other orientations), the spatial relative adjectives used will also be interpreted according to the orientation after the turn.
[0011] Although embodiments of the present invention are illustrated using nanostructured channel field-effect transistors such as fully wound gate field-effect transistors (e.g., horizontally wound gate field-effect transistors or vertically wound gate field-effect transistors), some embodiments of the present invention can be used in other processes and / or other devices such as planar field-effect transistors, fin field-effect transistors, or other suitable devices. Those skilled in the art should understand that other modifications are also within the scope of the embodiments of the present invention. In examples employing fully wound gate transistor structures, the fully wound gate transistor structure can be patterned by any suitable method. For example, the structure can be patterned using one or more photolithography processes, including dual patterning or multiple patterning processes. Generally, dual patterning or multiple patterning processes combine photolithography and self-alignment processes, resulting in a pattern spacing smaller than that obtained using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed on a substrate, and the sacrificial layer is patterned using a photolithography process. A self-alignment process is used to form spacers along the sides of the patterned sacrificial layer. The sacrificial layer is then removed, and the remaining spacers can later be used to pattern the fully wound gate structure.
[0012] Figures 1 to 22B illustrate exemplary processes for manufacturing the semiconductor device structure 100 in embodiments of the present invention. It should be understood that additional steps may be provided before, during, and after the processes shown in Figures 1 to 22B, and additional embodiments of the method may replace or omit some of the following steps. The order of steps / processes is not limited thereto and may be interchanged.
[0013] Figures 1, 2, 3, 4, and 5 are perspective views of various stages of manufacturing the semiconductor device structure 100 in some embodiments. As shown in Figure 1, the semiconductor device structure 100 includes a semiconductor layer stack 104 formed on the front side of a substrate 101. The substrate 101 may be a semiconductor substrate. The substrate 101 may include crystalline semiconductor materials, such as, but not limited to, silicon, germanium, silicon-germanium, gallium arsenide, indium antimonide, gallium phosphide, gallium antimonide, indium aluminum arsenide, indium gallium arsenide, gallium antimony phosphide, gallium antimony arsenide, or indium phosphide.
[0014] The substrate 101 may include various regions doped with impurities (such as p-type or n-type dopants). Depending on the circuit design, the dopant may be phosphorus used in n-type field-effect transistors or boron used in p-type field-effect transistors.
[0015] As shown in some embodiments of FIG1, the substrate 101 includes a layer 103 made of a material different from that of the substrate 101. In some embodiments, the substrate 101 is a silicon substrate, and the layer 103 is composed of silicon and germanium. The layer 103 can serve as a stop layer during back-side processing.
[0016] The semiconductor layer stack 104 includes interleaved semiconductor layers composed of different materials to facilitate the formation of nanostructure channels in multi-gate devices such as nanostructure channel field-effect transistors. In some embodiments, the semiconductor layer stack 104 includes a first semiconductor layer 106 and a second semiconductor layer 108. In some embodiments, the semiconductor layer stack 104 includes interleaved first semiconductor layers 106 and second semiconductor layers 108. The first semiconductor layer 106 and the second semiconductor layer 108 are composed of semiconductor materials with different etch selectivity and / or oxidation rates. For example, the first semiconductor layer 106 may be composed of silicon, and the second semiconductor layer 108 may be composed of silicon germanium. In some examples, the first semiconductor layer 106 may be composed of silicon germanium, and the second semiconductor layer 108 may be composed of silicon. In some embodiments, the composition of the first semiconductor layer 106 and the second semiconductor layer 108 may be changed to or include other materials such as germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, gallium arsenide phosphide, aluminum indium arsenide, aluminum gallium arsenide, indium gallium arsenide, gallium indium phosphide, gallium arsenide phosphide, or any combination thereof.
[0017] The formation method of the first semiconductor layer 106 and the second semiconductor layer 108 can be any suitable deposition process such as epitaxy. For example, the method of epitaxially growing the layered semiconductor layer stack 104 can be molecular beam epitaxy, metal-organic chemical vapor deposition, and / or other suitable epitaxial growth process.
[0018] In subsequent fabrication stages, the first semiconductor layer 106 or a portion thereof may form a nanostructure channel of the semiconductor device structure 100. The term "nanostructure" as used herein can refer to any material portion of nanometer size (or even micrometer size) having an elongated shape, regardless of the cross-sectional shape of this portion. Therefore, this term can refer to an elongated material portion with a circular or substantially circular cross-section, or a bundled or rod-shaped material portion (such as a cylinder or substantially rectangular cross-section). A gate may surround the nanostructure channel of the semiconductor device structure 100. The semiconductor device structure 100 may include a nanostructure transistor. A nanostructure transistor can be considered as a nanosheet transistor, a nanowire transistor, a fully wound gate transistor, a multi-bridge channel transistor, or any transistor having a gate surrounding the channel. The contents of the channel of the semiconductor device structure 100 defined by the first semiconductor layer 106 are as follows.
[0019] The thickness of each of the first semiconductor layers 106 may be between about 3 nm and about 30 nm, for example, about 3 nm to about 10 nm. The thickness of each of the second semiconductor layers 108 may be equal to, less than, or greater than the thickness of the first semiconductor layer 106. In some embodiments, the thickness of each of the second semiconductor layers 108 is between about 2 nm and about 50 nm. The three first semiconductor layers 106 and the three second semiconductor layers 108 are arranged alternately as shown in FIG1, which is for illustrative purposes only and is not intended to limit the embodiments of the present invention to the parts not actually described in the claim. It is understood that any number of first semiconductor layers 106 and second semiconductor layers 108 may be formed in the semiconductor layer stack 104, and the number of layers depends on the predetermined number of channels used by the semiconductor device structure 100. In some embodiments, the semiconductor layer stack 104 includes two first semiconductor layers 106. In some embodiments, the semiconductor layer stack 104 includes three first semiconductor layers 106. In some embodiments, the semiconductor layer stack 104 includes four first semiconductor layers 106.
[0020] As shown in FIG. 2, fin structures 112 are formed from the semiconductor layer stack 104. The upper portion of each fin structure 112 includes a first semiconductor layer 106 and a second semiconductor layer 108, and each substrate portion 116 is formed from a substrate 101. The fin structure 112 can be formed by patterning a hard mask layer (not shown) on the semiconductor layer stack 104, and the patterning method employs multiple patterning steps, including photolithography and etching processes. The etching process may include dry etching, wet etching, reactive ion etching, and / or other suitable processes. The photolithography process may include forming a photoresist layer (not shown) on the hard mask layer, exposing the photoresist layer to a pattern, performing a post-exposure baking process, and developing the photoresist layer to form a mask unit containing the photoresist layer. In some embodiments, the method of patterning the photoresist layer to form the mask unit may employ an electron beam lithography process. The etching process forms trenches 114 in the protected area, extending through the hard mask layer, through the semiconductor layer stack 104, and into the substrate 101, thereby retaining a plurality of extending fin structures 112. The trenches 114 extend along the X direction. The etching method for the trenches 114 may employ dry etching such as reactive ion etching, wet etching, and / or combinations thereof. In some embodiments, the trenches 114 are located on the layer 103, as shown in FIG2. In some embodiments, the trenches 114 are also formed within the layer 103, as shown in FIG15.
[0021] As shown in FIG. 3, after forming the fin structure 112, an insulating material 118 is formed on the substrate 101. The insulating material 118 fills the trenches 114 between adjacent fin structures 112 until the fin structure 112 is embedded in the insulating material 118. A planarization step, such as chemical mechanical polishing and / or etch-back, is then performed to expose the top of the fin structure 112. The insulating material 118 may be composed of silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride, silicon carbonitride, fluorosilicate glass, a low dielectric constant dielectric material, or any suitable dielectric material. The insulating material 118 may be formed by a suitable method such as low-pressure chemical vapor deposition, plasma-assisted chemical vapor deposition, or flowable chemical vapor deposition.
[0022] As shown in FIG. 4, the insulating material 118 is recessed to form an isolation region 120. The recess of the insulating material 118 exposes a portion of the fin structure 112, such as the semiconductor layer stack 104. The recess of the insulating material 118 exposes a trench 114 between adjacent fin structures 112. The isolation region 120 may be formed using a suitable process such as a dry etching process, a wet etching process, or a combination thereof. The upper surface of the insulating material 118 may be flush with or lower than the surface of the second semiconductor layer 108 contact substrate portion 116 (formed from the substrate 101). In some embodiments, the isolation region 120 is a shallow trench isolation region.
[0023] As shown in FIG. 5, one or more sacrificial gate structures 130 (only one in the figure) are formed on the semiconductor device structure 100. The sacrificial gate structure 130 is formed on a portion of the fin structure 112. Each of the sacrificial gate structures 130 may include a sacrificial gate dielectric layer 132, a sacrificial gate layer 134, and a masking layer 136. The sacrificial gate dielectric layer 132, the sacrificial gate layer 134, and the masking layer 136 may be formed by sequentially depositing a blanket layer of the sacrificial gate dielectric layer 132, the sacrificial gate layer 134, and the masking layer 136, and then patterning these layers into the sacrificial gate structure 130. Although only one sacrificial gate structure 130 is shown in the figure, some embodiments may arrange two or more sacrificial gate structures 130 along the X direction.
[0024] The sacrificial gate dielectric layer 132 may include one or more dielectric materials, such as silicon oxide as the primary material. The sacrificial gate layer 134 may include silicon, such as polycrystalline silicon or amorphous silicon. The masking layer 136 may include multiple layers, such as oxide layers and nitride layers. The portion of the fin structure 112 covered by the sacrificial gate layer 134 of the sacrificial gate structure 130 may serve as a channel region used by the semiconductor device structure 100.
[0025] Figures 6 to 14 are side sectional views of a semiconductor device structure 100 at various manufacturing stages in some embodiments, along section line AA of Figure 5. As shown in Figure 6, a first spacer 138 is deposited on the exposed surface of the semiconductor device structure 100. For example, the first spacer 138 is deposited on the fin structure 112, the isolation region 120, and the sacrificial gate structure 130. The composition of the first spacer 138 may be a dielectric material such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, silicon carbonitride, silicon carbon oxynitride, silicon carbon oxynitride, and / or combinations thereof. The first spacer 138 may be formed by any suitable process. In some embodiments, the first spacer 138 is a compliant layer formed by a compliant process such as atomic layer deposition.
[0026] As shown in FIG. 7, a second spacer 139 is deposited on the first spacer 138. The second spacer 139 may include any suitable dielectric material such as silicon oxide, silicon oxynitride, silicon nitride, carbonitride, or silicon oxycarbide. The thickness of the second spacer 139 may be from about 0.5 nm to about 5 nm. The second spacer 139 may be formed by any suitable process. In some embodiments, the deposition method of the second spacer 139 is chemical vapor deposition, plasma-assisted chemical vapor deposition, or electron cyclotron resonance chemical vapor deposition. In some embodiments, the second spacer 139 is absent, and the semiconductor device structure 100 includes only the first spacer 138, as shown in FIG. 15.
[0027] As shown in FIG8, the horizontal portions of the first spacer 138 and the second spacer 139 are removed. In some embodiments, the method for removing the horizontal portions of the first spacer 138 and the second spacer 139 may be an anisotropic etching process. The anisotropic etching process may be a selective etching process, which does not substantially affect the mask layer 136, the semiconductor layer stack 104, and the isolation region 120.
[0028] As shown in FIG. 9, portions of the fin structure 112 not covered by the sacrificial gate structure 130, the first spacer 138, and the second spacer 139 are recessed above, flush with, or below the upper surface of the isolation region 120. The method for recessing portions of the fin structure 112 can be an etching process. The etching process can be dry etching such as reactive ion etching, neutral beam etching, or similar etching, or wet etching such as using tetramethylammonium hydroxide, ammonium hydroxide, or any suitable etchant. The substrate portion 116 is exposed on both sides of the sacrificial gate structure 130, as shown in FIG. 9. In some embodiments, the first spacer 138 located on the side surface of the recessed portion of the fin structure 112 is also recessed, as shown in FIG. 15.
[0029] As shown in FIG10, the edge portions of each of the second semiconductor layers 108 of the semiconductor layer stack 104 are horizontally removed along the X direction. Removing the edge portions of the second semiconductor layers 108 may form voids. In some embodiments, the method for removing portions of the second semiconductor layers 108 may be a selective wet etching process. In the example where the second semiconductor layer 108 is composed of silicon germanium and the first semiconductor layer 106 is composed of silicon, the method for selectively etching the second semiconductor layer 108 may employ a wet etchant, such as, but not limited to, ammonium hydroxide, tetramethylammonium hydroxide, ethylenediamine o-catechol, or potassium hydroxide solution.
[0030] After removing the respective edge portions of the second semiconductor layers 108, a dielectric layer is deposited in the recesses to form dielectric spacers 144. The dielectric spacers 144 may be composed of a dielectric material with a low dielectric constant, such as silicon oxynitride, silicon carbonitride, silicon carbon oxynitride, silicon oxide, or silicon nitride. The dielectric spacers 144 may be formed by first using a compliant deposition process such as atomic layer deposition to form a compliant dielectric layer, and then removing portions of the compliant dielectric layer other than the dielectric spacers 144 by anisotropic etching. During the anisotropic etching process, the first semiconductor layer 106 protects the dielectric spacers 144. The dielectric spacers 144 cover the remaining second semiconductor layers 108 between the dielectric spacers 144 along the X direction.
[0031] As shown in FIG11, a layered structure, such as a layered structure containing a first semiconductor material 150, may be formed on the exposed substrate portion 116. In some embodiments, the first semiconductor material 150 comprises undoped silicon or undoped silicon-germanium. In some embodiments, the term undoped includes unintentionally doped material. For example, the layered structure may include dopants diffused from other regions such as the substrate portion 116. The first semiconductor material 150 may be first formed on semiconductor surfaces such as the exposed substrate portion 116 and the first semiconductor layer 106, and the formation method may be epitaxy. A subsequent etching process is performed to remove portions of the first semiconductor material 150 formed on the first semiconductor layer 106. The first semiconductor material 150 formed on the exposed substrate portion 116 may have a recessed upper surface derived from the etching process. In some embodiments, the thickness of the first semiconductor material 150 along the Z direction is from about 5 nm to about 50 nm.
[0032] As shown in FIG12, a layer 152 is formed on a first semiconductor material 150. The layer 152 may be formed by first forming a continuous layer on the exposed surface of the semiconductor device structure 100, and then performing one or more etching processes to remove portions of the continuous layer other than the layer 152. A masking layer (not shown), such as an anti-reflective coating, may be used to assist in the removal of portions of the continuous layer. The layer 152 may include any suitable material, such as silicon carbide, lanthanum oxide, aluminum oxide, aluminum oxynitride, zirconium oxide, hafnium oxide, silicon nitride, silicon, zinc oxide, zirconium nitride, aluminum zirconium oxide, titanium oxide, tantalum oxide, yttrium oxide, tantalum carbonitride, zirconium silicate, silicon carbonitride, silicon carbonitride, silicon carbonitride, hafnium silicate, or silicon oxide. In some embodiments, layer 152 includes a dielectric material and can serve as an isolation layer to prevent leakage current from subsequently formed source / drain regions to the substrate portion 116 below the second semiconductor layer 108. In some embodiments, layer 152 includes a material different from that of insulating material 118 and can serve as an etch stop layer during back-side processing. In some embodiments, the upper surface of layer 152 may be recessed due to the recessed upper surface of the first semiconductor material 150. In some embodiments, layer 152 is absent, and a second semiconductor material 154 is formed on the first semiconductor material 150.
[0033] Next, a second semiconductor material 154 is formed from the first semiconductor layer 106. The second semiconductor material 154 may be composed of one or more layers of silicon, silicon phosphide, silicon carbide, silicon arsenide, silicon antimonyide, or silicon carbide for use in an n-type channel field-effect transistor, or one or more layers of silicon, silicon germanium, or silicon germanium boride for use in a p-type channel field-effect transistor. For a p-type channel field-effect transistor, the second semiconductor material 154 may include a p-type dopant such as boron. For an n-type channel field-effect transistor, the second semiconductor material 154 may include an n-type dopant such as phosphorus or arsenic. In some embodiments, the dopant concentration of the second semiconductor material 154 may be from about 1 x 10¹⁹ cm⁻³ to about 2 x 10²¹ cm⁻³. The second semiconductor material 154 may be formed by epitaxial growth, employing chemical vapor deposition, atomic layer deposition, or molecular beam epitaxy. As shown in some embodiments of FIG12, a second semiconductor material 154 is selectively formed on a semiconductor material such as the first semiconductor layer 106, but not on a dielectric material such as the layer 152 and the dielectric spacer 144. In some embodiments, the second semiconductor material 154 includes a crystal plane that may correspond to the crystal plane of the material used in the first semiconductor layer 106. In some embodiments, the second semiconductor material 154 includes a separated portion extending from the first semiconductor layer 106 along the X direction, as shown in FIG12. In some embodiments, the second semiconductor material 154 is a continuous layer that is also formed on the side surface of the dielectric spacer 144. In these embodiments, the second semiconductor material 154 may also be formed on and in contact with the layer 152.
[0034] Next, as shown in FIG12, a third semiconductor material 156 is formed from the second semiconductor material 154. The third semiconductor material 156 may be formed by epitaxial growth, employing chemical vapor deposition, atomic layer deposition, or molecular beam epitaxy. The composition of the third semiconductor material 156 may be one or more layers of silicon, silicon phosphide, silicon carbide, or silicon carbide phosphide for use in n-type field-effect transistors, or one or more layers of silicon, silicon germanium, silicon germanium boride, or germanium for use in p-type field-effect transistors. For p-type field-effect transistors, the third semiconductor material 156 may contain p-type dopants such as boron. For n-type field-effect transistors, the third semiconductor material 156 may contain n-type dopants such as phosphorus or arsenic. In some embodiments, the second semiconductor material 154 and the third semiconductor material 156 may comprise the same semiconductor material but with different dopant concentrations. The dopant concentration of the third semiconductor material 156 may be substantially greater than the dopant concentration of the second semiconductor material 154. In some embodiments, the dopant concentration of the third semiconductor material 156 can be from about 5 x 10¹⁹ cm⁻³ to about 4 x 10²¹ cm⁻³. The third semiconductor material 156 can be epitaxially grown from the second semiconductor material 154. Due to the crystal planes of the second semiconductor material 154, the quality of the third semiconductor material 156 can be improved.
[0035] In some embodiments, a capping layer (not shown) may be formed on the third semiconductor material 156. The capping layer may include a semiconductor material. In some embodiments, the capping layer includes the same material as the third semiconductor material. The capping layer may be epitaxially grown from the third semiconductor material 156.
[0036] In some embodiments, the second semiconductor material 154 and the third semiconductor material 156 may be doped in situ during growth. If the dopant concentration of the second semiconductor material 154 and the third semiconductor material 156 is greater than the above range, it may negatively affect the quality of the second semiconductor material 154 and the third semiconductor material 156.
[0037] The second semiconductor material 154 and the third semiconductor material 156 can together serve as the source / drain region. In embodiments of the present invention, the source region and the drain region are interchangeable, and their structures are substantially the same. Furthermore, the source / drain region can be regarded independently or together as the source region or drain region, depending on the context. In some embodiments, one or more masking layers can be used to form p-type source / drain regions and n-type source / drain regions, respectively. In some embodiments, the second semiconductor material 154 and the third semiconductor material 156 are crystalline semiconductor materials.
[0038] Next, as shown in FIG12, a contact etch stop layer 162 is compliantly formed on the exposed surface of the semiconductor device structure 100. The contact etch stop layer 162 covers the second spacer 139, the isolation region 120, and the third semiconductor material 156 (or capping layer, if present). The contact etch stop layer 162 may include an oxygen-containing or nitrogen-containing material, such as silicon nitride, silicon carbonitride, silicon oxynitride, carbon nitride, silicon oxide, silicon oxycarbide, the like, or combinations thereof, and may be formed by chemical vapor deposition, plasma-assisted chemical vapor deposition, atomic layer deposition, or any suitable deposition technique. In some embodiments, the contact etch stop layer 162 is a single layer, as shown in FIG12. In some embodiments, the contact etch stop layer 162 includes two or more layers. An interlayer dielectric layer 164 is then formed on the contact etch stop layer 162. The material used for the interlayer dielectric layer 164 may include compounds containing silicon, oxygen, carbon, and / or hydrogen, such as silicon oxide, silicon hydroxide, or silicon carbide. Organic materials such as polymers may also be used for the interlayer dielectric layer 164. The deposition method for the interlayer dielectric layer 164 may be a plasma-assisted chemical vapor deposition process or other suitable deposition techniques. In some embodiments, after forming the interlayer dielectric layer 164, the semiconductor device structure 100 may be thermally processed to anneal the interlayer dielectric layer 164. After forming the interlayer dielectric layer 164, a planarization step such as chemical mechanical polishing may be performed on the semiconductor device structure 100 until the sacrificial gate layer 134 is exposed, as shown in FIG12.
[0039] Next, as shown in FIG13, the sacrificial gate structure 130 and the second semiconductor layer 108 are removed. Removing the sacrificial gate structure 130 and the second semiconductor layer 108 may form an opening between the first spacer 138 and the first semiconductor layer 106. The interlayer dielectric layer 164 may protect the second semiconductor material 156 during the removal process. The sacrificial gate structure 130 may be removed by plasma dry etching and / or wet etching. The sacrificial gate layer 134 may be removed first by any suitable process such as dry etching, wet etching, or a combination thereof, and then the sacrificial gate dielectric layer 132 may be removed by any suitable process such as dry etching, wet etching, or a combination thereof. In some embodiments, a wet etchant such as tetramethylammonium hydroxide solution may be used to selectively remove the sacrificial gate layer 134 without affecting the first spacer 138, the interlayer dielectric layer 164, and the contact etch stop layer 162.
[0040] The second semiconductor layer 108 can be removed using a wet etching process. In the example where the second semiconductor layer 108 is composed of silicon-germanium and the first semiconductor layer 106 is composed of silicon, the chemical agent used in the selective wet etching process can remove silicon-germanium without substantially affecting silicon and the dielectric material of the first spacer 138 and the dielectric spacer 144. In one embodiment, the removal method for the second semiconductor layer 108 can use a wet etchant, such as, but not limited to, hydrofluoric acid, nitric acid, hydrogen chloride, or phosphoric acid.
[0041] As shown in FIG. 14, after forming the nanostructure channel (i.e., the exposed portion of the first semiconductor layer 106), a gate dielectric layer 170 is formed around the exposed portion of the first semiconductor layer 106, and a gate layer 172 is formed on the gate dielectric layer 170. The gate dielectric layer 170 and the gate layer 172 can be considered together as a gate structure 174. In some embodiments, an interface layer (not shown) is formed between the gate dielectric layer 170 and the exposed surface of the first semiconductor layer 106. In some embodiments, the gate dielectric layer 170 includes one or more layers of dielectric material, such as silicon oxide, silicon nitride, a high dielectric constant dielectric material, other suitable dielectric materials, and / or combinations thereof. High dielectric constant dielectric materials include hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, hafnium tantalum oxide, hafnium titanium oxide, hafnium zirconium oxide, zirconium oxide, aluminum oxide, titanium oxide, hafnium oxide-aluminum oxide alloys, other suitable high dielectric constant dielectric materials, and / or combinations thereof. The gate dielectric layer 170 can be formed by chemical vapor deposition, atomic layer deposition, or any suitable deposition technique. The gate layer 172 may include one or more layers of conductive materials such as polycrystalline silicon, aluminum, copper, titanium, tantalum, tungsten, cobalt, molybdenum, tantalum nitride, nickel silicate, cobalt silicate, titanium nitride, tungsten nitride, titanium aluminum, titanium aluminum nitride, tantalum carbonitride, tantalum carbide, tantalum silicon nitride, metal alloys, other suitable materials, and / or combinations thereof. The gate layer 172 can be formed by chemical vapor deposition, atomic layer deposition, electroplating, or other suitable deposition techniques. Gate layer 172 can also be deposited on interlayer dielectric layer 164. Then, gate dielectric layer 170 and gate layer 172 on interlayer dielectric layer 164 can be removed, and the removal method can be chemical mechanical polishing until the upper surface of interlayer dielectric layer 164 is exposed.
[0042] It should be understood that the semiconductor device structure 100 can undergo subsequent processes such as metal gate dicing and / or continuous polysilicon on diffusion edges. The metal gate dicing process divides the gate layer 172 into multiple portions for independent control of these portions. The continuous polysilicon on diffusion edges forms isolation between devices.
[0043] Figures 15 and 16 are perspective views of various stages in manufacturing the semiconductor device structure 100 in some embodiments. Figure 15 shows a perspective view of the semiconductor device structure 100 shown in Figure 14. The second semiconductor material 154 is omitted for clarity. In some embodiments, the semiconductor device structure 100 includes a single first spacer 138, and an insulating material 118 extends through the layer 103, as shown in Figure 15.
[0044] Next, as shown in FIG16, another interlayer dielectric layer 184 is deposited on the semiconductor device structure 100, and a conductive structure 180 is formed in the interlayer dielectric layer 184. The material included in the interlayer dielectric layer 184 may be the same as the material of the interlayer dielectric layer 164. The conductive structure 180 may include any suitable conductive material such as a metal. In some embodiments, the conductive structure 180 includes tungsten, ruthenium, cobalt, copper, or molybdenum. The conductive structure 180 may be formed by any suitable process such as physical vapor deposition or electrochemical plating. In some embodiments, a pad 182 may be formed on the side surface of the conductive structure 180, as shown in FIG16. The pad 182 may include tantalum nitride or titanium nitride. An etch stop layer 186 is deposited on the conductive structure 180 and the interlayer dielectric layer 184. A silicon layer (not shown) may be formed between the conductive structure 180 and the third semiconductor material 156 to electrically connect the conductive structure 180 and the corresponding third semiconductor material 156. Interconnect structures (not shown) may be formed on the etch stop layer 186. The semiconductor device structure 100 can then be flipped for a back-side process, as shown in FIG16. The method for removing a portion of the substrate 101 on the layer 103 can be any suitable process, such as a polishing process. In some embodiments, the layer 103 serves as a stop layer during the polishing process. The layer 103 is then removed to expose the remaining portions of the insulating material 118 and the substrate 101, as shown in FIG16. The method for removing the layer 103 can be any suitable process.
[0045] In some embodiments, Figures 17A, 18A, 19A, 20A, 21A, and 22A are perspective views of various stages of manufacturing the semiconductor device structure 100 in some embodiments. Figures 17B, 18B, 19B, 20B, 21B, and 22B are corresponding side sectional views of the semiconductor device structures 100 of Figures 17A, 18A, 19A, 20A, 21A, and 22A in some embodiments. As shown in Figures 17A and 17B, masking layers 202 and 204 are formed on the substrate 101 and the insulating material 118. Masking layer 202 may include nitrides such as silicon nitride, while masking layer 204 may include oxides such as silicon oxide. Openings 206 are formed in masking layers 202 and 204 to expose the substrate 101 (Figure 16). In some embodiments, the size of the opening 206 in the masking layers 202 and 204 along the Y direction may be larger than the size of the substrate 101 along the Y direction. An etching process is then performed to remove the exposed portion of the substrate 101. The etching process may be a dry etching process, a wet etching process, or a combination thereof. The etching process removes the semiconductor material of the exposed portion of the substrate 101 without substantially affecting the dielectric material of the insulating material 118. In some embodiments, since the first semiconductor material 150 is also composed of a semiconductor material, the etching process also removes the first semiconductor material 150 beneath the exposed portion of the substrate 101, as shown in Figures 17A and 17B. In some embodiments, the layer 152 includes a dielectric material and may serve as an etch stop layer during the etching process. In some embodiments, after the etching process that removes a portion of the substrate 101 and the first semiconductor material 150 thereunder, another etching process may be performed to remove the exposed layer 152. In some embodiments, the material comprising the layer 152 is different from the material of the insulating material 118. The etching process removes the layer 152 but does not remove the insulating material 118, as shown in Figures 17A and 17B.
[0046] In some embodiments, the upper surface of the third semiconductor material 156 (or the upper surface of the second semiconductor material 154) in contact with the layer 152 may have a flat or convex profile, as shown in FIG16. In some embodiments, the etching process removes the layer 152 and a portion of the third semiconductor material 156 (or a portion of the second semiconductor material 154, if the second semiconductor material 154 is formed on and in contact with the layer 152, as shown in FIG12), and the upper surface of the third semiconductor material 156 (or the second semiconductor material 154) after the etching process has a recessed profile. In some embodiments, the etching process removes the layer 152 without affecting the third semiconductor material 156 (or the second semiconductor material 154), and the upper surface of the third semiconductor material 156 (or the second semiconductor material 154) remains flat or convex.
[0047] As shown in Figures 18A and 18B, the opening 206 is widened. In some embodiments, an etching process is performed after the placement process to widen the opening 206. The placement process may include placing elements into portions of the insulating material 118, the contact etch stop layer 162, the interlayer dielectric layer 164, and the first spacer 138. In some embodiments, the placement process may be oblique to minimize the elements placed into the third semiconductor material 156. The angle of the placement process may be from about 0 degrees to about 90 degrees. Compared to unplaced insulating material 118, contact etch stop layer 162, interlayer dielectric layer 164, and the first spacer 138, the elements placed into the aforementioned components may produce differences in etching selectivity. In some embodiments, the elements are argon, lanthanum, aluminum, or xenon.
[0048] After the elements are implanted onto portions of the insulating material 118, the contact etch stop layer 162, the interlayer dielectric layer 164, and the first spacer 138, an etching process, such as a wet etching process, is performed to remove the implanted portions. In some embodiments, the wet etching process may employ any suitable etchant, such as a first solution containing a mixture of ammonium hydroxide, hydrogen peroxide, and water, and a second solution containing a mixture of hydrogen chloride, hydrogen peroxide, and water, hydrogen peroxide, deionized water, deionized ozone, or diluted hydrofluoric acid. The etching process does not materially affect portions of the unimplanted insulating material 118, the contact etch stop layer 162, the interlayer dielectric layer 164, and the first spacer 138. In some embodiments, the oblique implantation process and the etching process may form steps on the side surfaces of the interlayer dielectric layer 164 and / or the first spacer 138, as shown in FIG18B.
[0049] In some embodiments, other processes may be performed to widen the opening 206, instead of the fabrication and etching processes. For example, an anisotropic etching process may be performed to remove the exposed portion of the insulating material 118 and portions of the underlying contact etch stop layer 162, interlayer dielectric layer 164, and first spacer 138. The anisotropic etching process may be a selective etching process that removes the dielectric material of portions of the insulating material 118, contact etch stop layer 162, interlayer dielectric layer 164, and first spacer 138, and the anisotropic etching process may not affect the semiconductor material of the third semiconductor material 156 (or the second semiconductor material 154).
[0050] In some embodiments, the widened opening 206 also exposes a portion of the side surface of the third semiconductor material 156 (or the second semiconductor material 154) because the first spacer 138 is recessed, as shown in FIG18B. In some embodiments, the opening 206 may be widened by about 1 nm to about 15 nm.
[0051] As shown in Figures 19A and 19B, a dielectric layer 208 is formed on the sidewall of the opening 206. In some embodiments, the dielectric layer 208 is formed on the side surfaces of the insulating material 118, the contact etch stop layer 162, and the interlayer dielectric layer 164, as shown in Figures 19A and 19B. The dielectric layer 208 may include any suitable dielectric material. In some embodiments, the dielectric layer 208 includes a nitride such as silicon nitride. The dielectric layer 208 electrically isolates the substrate portion 116 on the gate layer 172 from the subsequently formed conductive structure 220 (Figures 22A and 22B). In other words, the dielectric layer 208 can minimize the leakage current from the conductive structure 220 to the gate layer 172. In some embodiments, the dielectric layer 208 is formed by first depositing a blanket layer on the exposed surface of the semiconductor device structure 100, and then removing a portion of the blanket layer on the horizontal surface of the semiconductor device structure 100, and the removal method may be an anisotropic etching process. In some embodiments, a high bias power may be applied during an isotropic etching process to ensure that at least a portion of the sidewall surface of the third semiconductor material 156 (or the second semiconductor material 154) is exposed, as shown in FIG19B.
[0052] Next, as shown in Figures 20A and 20B, a fourth semiconductor material 210 is epitaxially grown from the exposed portion of the third semiconductor material 156 (or the second semiconductor material 154). In some embodiments, the fourth semiconductor material 210 and the third semiconductor material 156 comprise the same material, but the dopant concentration of the fourth semiconductor material 210 is greater than that of the third semiconductor material 156. For example, the dopant concentration of the fourth semiconductor material 210 is about 1 x 10¹⁹ cm⁻³ to about 1 x 10²² cm⁻³, such as about 6 x 10¹⁹ cm⁻³ to about 1 x 10²² cm⁻³. As described above, if the semiconductor material is doped in situ and the dopant concentration of the semiconductor material is greater than 5 x 10¹⁹ cm⁻³ to about 4 x 10²¹ cm⁻³, the quality of the semiconductor material may be negatively affected. Therefore, in some embodiments, the first dopant concentration of the fourth semiconductor material 210 after the epitaxial process is about 5 x 10¹⁰ cm⁻³ to about 4 x 10²¹ cm⁻³, and subsequent doping processes can be performed to increase the first dopant concentration to a second dopant concentration, such as 6 x 10¹⁹ cm⁻³ to about 1 x 10²² cm⁻³. In some embodiments, the epitaxial process for forming the fourth semiconductor material 210 is a low-temperature epitaxial process, with a process temperature of about 300°C to about 470°C. The low-temperature process ensures that the metal of the conductive structure 180 and the conductive structure in the interconnect structure are not negatively affected.
[0053] As shown in some embodiments of FIG20B, a fourth semiconductor material 210 is grown from the upper and side surfaces of a third semiconductor material 156 (or a second semiconductor material 154). Therefore, in some embodiments, the fourth semiconductor material 210 has an M-shaped cross-sectional shape. For example, the fourth semiconductor material 210 includes a longitudinal portion (horizontal portion) and two edge portions (vertical portions) extending from the longitudinal portion. In some embodiments, the lower surface of the longitudinal portion has a recessed profile derived from the recessed profile of the upper surface of the third semiconductor material 156. The upper surface of the fourth semiconductor material 210 may be flat, recessed, or convex, which can be controlled by the epitaxial process of growing the fourth semiconductor material 210. In some embodiments, the shape of the upper surface of the fourth semiconductor material 210 is the same as the shape of the upper surface of the third semiconductor material 156 (or the second semiconductor material 154). In some embodiments, the shape of the upper surface of the fourth semiconductor material 210 is different from the shape of the upper surface of the third semiconductor material 156 (or the second semiconductor material 154). The width W1 of the upper surface of the fourth semiconductor material 210 is approximately 10 nm to approximately 80 nm. The portion of the fourth semiconductor material 210 adjacent to the third semiconductor material 156 (or the second semiconductor material 154) has a lower surface width W2 of approximately 1 nm to approximately 10 nm. The thickness T1 of the fourth semiconductor material 210 can be approximately 1 nm to approximately 10 nm. The portion of the fourth semiconductor material 210 adjacent to the third semiconductor material 156 (or the second semiconductor material 154) results in an increased upper surface area of the fourth semiconductor material 210. As a result, the size of the silicon layer 212 (Figures 21A and 21B) formed on the upper surface of the fourth semiconductor material 210 is also increased, resulting in a decrease in electrical contact resistance. Furthermore, the high dopant concentration of the fourth semiconductor material 210 also reduces the electrical contact resistance.
[0054] As shown in Figures 21A and 21B, a silica layer 212 is formed on the upper surface of the fourth semiconductor material 210. The silica layer 212 may include any suitable material such as titanium silicate, molybdenum silicate, ruthenium silicate, tungsten silicate, titanium silicate, rhodium silicate, niobium silicate, iridium silicate, yttrium silicate, antimony silicate, scandium silicate, or zirconium silicate. The silica layer 212 can be formed by any suitable process. In some embodiments, a metal layer (not shown) is first formed on the exposed surface of the semiconductor device structure 100, and the metal layer reacts with the fourth semiconductor material 210 to form the silica layer 212. Next, nitriding can be performed to convert the retained metal layer into a metal nitride layer, and a selective etching process can be performed to remove the metal nitride layer without substantially affecting the silicon layer 212 and the dielectric layer 208. As described above, the dimensions of the silicon layer 212, such as the width W3 of the silicon layer 212 along the Y direction, can be increased by the fourth semiconductor material 210. In some embodiments, the width W3 is substantially equal to the width W1. The thickness of the silicon layer 212 along the Z direction can be from about 1 nm to about 10 nm. In some embodiments, the depth of the silicon layer 212 along the X direction can be from about 5 nm to about 40 nm.
[0055] As shown in Figures 22A and 22B, a conductive structure 220 is formed in the opening 206 to fill the opening 206. The conductive structure 220 and the conductive structure 180 may include the same material. A portion of the conductive structure 220 on the insulating material 118 may be removed by a planarization process such as a chemical mechanical polishing process. The thickness of the conductive structure 220 along the Z direction may be about 5 nm to about 40 nm, the width along the Y direction may be about 10 nm to about 80 nm, and the depth along the X direction may be about 5 nm to about 40 nm. As described above, having a fourth semiconductor material 210 can result in an increase in the silicon layer 212, which can increase the landing area used by the conductive structure 220. In this way, the contact resistance can be reduced, for example, by about 45%.
[0056] In some embodiments, the width W1 of the fourth semiconductor material 210 may be approximately equal to the critical dimension of the opening 206 (e.g., the dimension of the opening 206 along the Y direction), as shown in FIG20B. In these embodiments, the silicide layer 212 is a planar layer, as shown in FIG21B. In some embodiments, the width W1 of the fourth semiconductor material 210 is substantially smaller than the critical dimension of the opening 206, and the silicide layer 212 covers three sides of the fourth semiconductor material 210, as shown in FIG23. For example, the silicide layer 212 covers three surfaces of the fourth semiconductor material 210. In some embodiments, the conductive structure 220 covers three sides of the silicide layer 212, as shown in FIG23. For example, the conductive structure 220 covers three surfaces of the silicide layer 212. In some embodiments, the upper surface of the third semiconductor material 156 (or the second semiconductor material 154) contacting the fourth semiconductor material 210 may be planar, recessed, or convex. The upper surface of the fourth semiconductor material 210 in contact with the silicon layer 212 may be flat, recessed, or protruding.
[0057] Embodiments of the present invention provide a semiconductor device structure and a method for forming the same. In some embodiments, the semiconductor device structure 100 includes a source / drain region containing a first semiconductor material (such as a third semiconductor material 156 or a second semiconductor material 154) and a second semiconductor material (such as a fourth semiconductor material 210) located on the first semiconductor material. The second semiconductor material covers a portion of the side surface of the first semiconductor material. A siliconized layer 212 is located on the second semiconductor material. Some embodiments may have advantages. For example, increasing the size of the siliconized layer 212 in the second semiconductor material allows for a larger landing area used by the conductive structure. This can reduce the contact resistance.
[0058] One embodiment is a semiconductor device structure. The structure includes an interlayer dielectric layer; a first semiconductor material adjacent to the interlayer dielectric layer; and a second semiconductor material located on the first semiconductor material. The second semiconductor material covers a first portion of a side surface of the first semiconductor material. The structure further includes a silicon layer located on the second semiconductor material; and a first conductive structure located on the silicon layer.
[0059] In one embodiment, the semiconductor device structure further includes a second portion of the spacer covering the side surface of the first semiconductor material. In one embodiment, the semiconductor device structure further includes a dielectric layer contacting the first conductive structure, a silicon layer, and the second semiconductor material. In one embodiment, the semiconductor device structure further includes a contact etch stop layer contacting the spacer and the first semiconductor material. In one embodiment, the semiconductor device structure further includes a second conductive structure located in the interlayer dielectric layer. In one embodiment, the semiconductor device structure further includes an insulating material located on the interlayer dielectric layer, wherein the first conductive structure is located in the insulating material. In one embodiment, the first semiconductor material has a first dopant concentration, the second semiconductor material has a second dopant concentration, and the second dopant concentration is greater than the first dopant concentration. In one embodiment, the silicon layer covers at least two sides of the second semiconductor material, and the upper surface of the first semiconductor material has a recessed profile.
[0060] Another embodiment is a semiconductor device structure. The structure includes an interlayer dielectric layer; a first semiconductor material adjacent to the interlayer dielectric layer; a semiconductor layer adjacent to the first semiconductor material; a second semiconductor material located between the semiconductor layer and the first semiconductor material; and a third semiconductor material located on the first semiconductor material. The third semiconductor material covers at least two sides of the first semiconductor material. The structure further includes a silicon compound layer located on the third semiconductor material; and a conductive structure located on the silicon compound layer.
[0061] In one embodiment, a first semiconductor material has a first dopant concentration, a second semiconductor material has a second dopant concentration, and a third semiconductor material has a third dopant concentration. In one embodiment, the third dopant concentration is greater than the first dopant concentration, and the first dopant concentration is greater than the second dopant concentration. In one embodiment, the upper surface of the first semiconductor material is recessed or protruding. In one embodiment, the upper surface of the third semiconductor material is recessed or protruding. In one embodiment, a silicide layer covers at least two sides of the third semiconductor material. In one embodiment, a conductive structure covers at least two sides of the silicide layer.
[0062] Another embodiment is a method for forming a semiconductor device structure. The method includes forming a first semiconductor material on a substrate; forming an interlayer dielectric layer on the first semiconductor material; flipping the substrate; forming an opening in the substrate to expose the first semiconductor material; widening the opening; and forming a second semiconductor material on the first semiconductor material. The second semiconductor material covers a portion of the side surface of the first semiconductor material. The method further includes depositing a silicon layer on the second semiconductor material; and depositing a conductive structure on the silicon layer.
[0063] In one embodiment, the step of widening the opening includes performing a placement process and an etching process. In one embodiment, the placement process includes placing elements into a portion of an insulating material, a portion of an interlayer dielectric layer, a portion of a contact etch stop layer, and a portion of a spacer. In one embodiment, the element includes argon, lanthanum, aluminum, or xenon. In one embodiment, the etching process includes a wet etching process to remove the placed portions of the insulating material, interlayer dielectric layer, contact etch stop layer, and spacer.
[0064] The features of the above embodiments are beneficial for those skilled in the art to understand the present invention. Those skilled in the art should understand that the present invention can be used as a basis to design and modify other processes and structures to achieve the same purpose and / or the same advantages of the above embodiments. Those skilled in the art should also understand that these equivalent substitutions do not depart from the spirit and scope of the present invention, and changes, substitutions, or modifications can be made without departing from the spirit and scope of the present invention. [Simplified Explanation of the Diagram]
[0007] Figures 1, 2, 3, 4, and 5 are perspective views of various stages in the manufacture of a semiconductor device structure in some embodiments. Figures 6, 7, 8, 9, 10, 11, 12, 13, and 14 are side sectional views along section line AA of Figure 5 of various stages in the manufacture of a semiconductor device structure in some embodiments. Figures 15 and 16 are perspective views of various stages in the manufacture of a semiconductor device structure in some embodiments. Figures 17A, 18A, 19A, 20A, 21A, and 22A are perspective views of various stages in the manufacture of a semiconductor device structure in some embodiments. Figures 17B, 18B, 19B, 20B, 21B, and 22B are corresponding side sectional views of the semiconductor device structures of Figures 17A, 18A, 19A, 20A, 21A, and 22A in some embodiments. Figure 23 is a side sectional view of various stages in the manufacture of a semiconductor device structure in other embodiments.
Claims
1. A semiconductor device structure, comprising: One interlayer dielectric layer; A first semiconductor material is adjacent to the interlayer dielectric layer; A second semiconductor material is located on the first semiconductor material, wherein the second semiconductor material covers a first portion of the side surface of the first semiconductor material; a silicide layer is located on the second semiconductor material; a first conductive structure is located on the silicide layer; and a dielectric layer contacts the first conductive structure, the silicide layer, and the second semiconductor material.
2. The semiconductor device structure as described in claim 1 further includes a second portion of a spacer covering the side surface of the first semiconductor material.
3. The semiconductor device structure as described in claim 2 further includes a contact etch stop layer contacting the spacer and the first semiconductor material.
4. A semiconductor device structure, comprising: One interlayer dielectric layer; A first semiconductor material, adjacent to the interlayer dielectric layer; a semiconductor layer; A second semiconductor material is located between the semiconductor layer and the first semiconductor material; a third semiconductor material is located on the first semiconductor material, wherein the third semiconductor material covers at least two sides of the first semiconductor material; a silicide layer is located on the third semiconductor material; and a conductive structure is located on the silicide layer.
5. The semiconductor device structure as claimed in claim 4, wherein the first semiconductor material has a first dopant concentration, the second semiconductor material has a second dopant concentration, and the third semiconductor material has a third dopant concentration.
6. The semiconductor device structure as claimed in claim 5, wherein the third dopant concentration is greater than the first dopant concentration, and the first dopant concentration is greater than the second dopant concentration.
7. A method for forming a semiconductor device structure, comprising: A first semiconductor material is formed on a substrate; A dielectric layer is formed on the first semiconductor material; the substrate is flipped. An opening is formed in the substrate to expose the first semiconductor material; the opening is widened; a second semiconductor material is formed on the first semiconductor material, wherein the second semiconductor material covers a portion of the side surface of the first semiconductor material; a silicon layer is deposited on the second semiconductor material; and a conductive structure is deposited on the silicon layer.
8. A method for forming a semiconductor device structure as described in claim 7, wherein the step of widening the opening includes performing an implantation process and an etching process.
9. A method for forming a semiconductor device structure as claimed in claim 8, wherein the implantation process includes implanting an element into a portion of an insulating material, a portion of an interlayer dielectric layer, a portion of a contact etch stop layer, and a portion of a spacer.
Citation Information
Patent Citations
Semiconductor device and manufacturing method thereof
US20240113199A1
