Method for manufacturing a leakage-current-resistant 5000 series aluminum plate

TWI946333BActive Publication Date: 2026-11-11CHINA STEEL
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW115115692
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2026-04-22
Publication Date
2026-11-11
Estimated Expiration
2046-04-21

Smart Images

  • Figure TWG2TB001921144_001
    Figure TWG2TB001921144_001
  • Figure TWG2TB001921144_002
    Figure TWG2TB001921144_002
  • Figure TWG2TB001921144_003
    Figure TWG2TB001921144_003
Patent Text Reader

Abstract

A method for manufacturing a leakage-resistant 5000 series aluminum sheet includes: casting a modified 5000 series aluminum billet to obtain a cast aluminum billet, wherein the modified 5000 series aluminum billet comprises 3.0 wt% to 5.0 wt% magnesium based on the total weight of the modified 5000 series aluminum billet; homogenizing the cast aluminum billet to obtain a homogenized aluminum billet, wherein the homogenization temperature is above 500°C; and rolling and cooling the homogenized aluminum billet to obtain a 5000 series aluminum sheet.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for manufacturing a leakage-resistant 5000 series aluminum plate, comprising: The process involves casting modified 5000 series aluminum billets to obtain cast aluminum billets, wherein the modified 5000 series aluminum billets comprise 3.0 wt% to 5.0 wt% magnesium by weight; homogenizing the cast aluminum billets to obtain homogenized aluminum billets, wherein the homogenization temperature is above 500°C; and rolling and cooling the homogenized aluminum billets to obtain the 5000 series aluminum sheet, wherein the rolling and cooling of the homogenized aluminum billets includes: rough rolling the homogenized aluminum billets to obtain rough rolled aluminum sheet; applying water-oil cold spray and air cooling to the rough rolled aluminum sheet to obtain cooled aluminum sheet; and finish rolling the cooled aluminum sheet to obtain the 5000 series aluminum sheet, wherein the initial temperature of the finish rolling is 210°C to 290°C.

2. The method as described in claim 1, wherein, The modified 5000 series aluminum ingot contains 3.5 wt% to 4.5 wt% magnesium.

3. The method as described in claim 1, wherein, The modified 5000 series aluminum ingot contains 3.8 wt% to 4.5 wt% magnesium.

4. The method as described in claim 1, wherein, The modified 5000 series aluminum ingot contains 4.0 wt% to 4.2 wt% magnesium.

5. The method as described in claim 1, wherein, The homogenization temperature is between 520°C and 600°C.

6. The method as described in claim 1, wherein, The homogenization temperature is between 540°C and 560°C.

7. The method as described in claim 1, wherein, The thickness of the 5000 series aluminum sheets ranges from 10 mm to 60 mm.

8. The method as described in claim 1, wherein, The yield strength of the 5000 series aluminum plates ranges from 190 MPa to 250 MPa.

9. The method as described in claim 1, wherein, The modified 5000 series aluminum billet is 5083 aluminum alloy.

Citation Information

Patent Citations

  • High-magnesium 5xxx series H32 state aluminum alloy sheet and preparation method thereof

    CN119824284A

  • Aluminum plate and method for manufacturing the same

    TWI905963B