Optical modules for the ultraviolet wavelength range
Patent Information
- Application Number
- PCT/EP2024/054588
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-02-27
- Filing Date
- 2024-02-22
- Publication Date
- 2024-10-24
AI Technical Summary
Optical modules for the ultraviolet wavelength range face challenges in maintaining the optical properties of optical elements due to unwanted heating caused by absorbed radiation during the curing process of adhesives, leading to inhomogeneous refractive index changes and wavefront deformation.
The development of optical modules with a multi-layer adhesive protective coating that is highly reflective and low-absorbing at the working wavelength, allowing for flexible control of reflection, transmission, and absorption, thereby minimizing heating and radiation damage, and incorporating anti-reflective or diffractive structures to further protect the optical elements.
The solution effectively prevents undesirable heating and radiation damage, ensuring the optical properties of the optical elements remain within manufacturing tolerances, enhancing the longevity and performance of the modules by maintaining high reflection and low absorption at the working wavelength while allowing sufficient transmission for adhesive curing.
Smart Images

Figure EP2024054588_24102024_PF_FP_ABST
Abstract
Description
[0001] Optical modules for the ultraviolet wavelength range
[0002] The present invention relates to optical modules comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of an adhesive curable by irradiation at a curing wavelength in the ultraviolet wavelength range, and wherein the module has a protective adhesive coating. Furthermore, it relates to an optical system or a device comprising one of the aforementioned optical modules. The present application claims priority from German patent application 10 2023 201 742.3 of February 27, 2023, which is incorporated herein by reference.
[0003] DE 10 2011 080 369 A1 discloses an assembly, particularly for a DUV microlithography projection exposure system, consisting of a holder and a component bonded by means of an adhesive that transmits radiation in the ultraviolet spectral range. The adhesive is curable by UV light. A layer is present in the area of the adhesive that transmits UV light from the spectral range suitable for curing the adhesive and absorbs UV light from a useful spectral range. An absorbing layer made of tantalum pentoxide is indicated as particularly suitable. This layer achieves high transmission at a curing wavelength of 365 nm and very low transmission at a useful wavelength of 248 nm and below, while simultaneously achieving high absorption and consistently low reflection in both spectral ranges.
[0004] It is an object of the present invention to further develop the known assembly.
[0005] This object is achieved by an optical module comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of irradiation with an adhesive curable at a curing wavelength in the ultraviolet wavelength range, and wherein the module has an adhesive protective coating, wherein the adhesive protective coating is designed in several layers and is highly reflective and slightly absorbent at the operating wavelength.
[0006] It has been found that by providing reflective multi-layer adhesive protective coatings, suitable adhesive protective coatings can be virtually tailor-made for any combination of operating wavelengths and curing wavelengths. These coatings can also prevent unwanted changes in the optical properties of the optical element due to heating by absorbed radiation. Such changes can result in an inhomogeneous change in the refractive index in the lens, which in turn leads to undesired wavefront deformation that affects the imaging properties of the lens. The choice of layer materials, thicknesses and number of layers allows the reflection, transmission and absorption to be flexibly influenced for specific wavelengths or wavelength ranges. Overall, a wavelength is referred to as a wavelength range with a width of ±1%.For a broader wavelength range, the middle wavelength can be considered instead. In particular, not only can the reflection at the working wavelength be set as high as possible and the absorption, especially at the working wavelength, as low as possible, but the transmission, especially at the curing wavelength, can also be set sufficiently high for the adhesive's curing process. Advantageously, the absorption at both the working and curing wavelengths should be low enough to prevent unwanted heating of the optical element, which would result in a change in the optical properties beyond the manufacturing tolerances. Any residual absorption present in this range can be used to further reduce the radiation exposure of the adhesive at the working wavelength beyond the reflection at the adhesive protective layer.Highly reflective here means a reflection of 70% or more, while low absorbing means an absorption of 30% or less.
[0007] Advantageously, the adhesive protective coating has at least three layers in order to be able to influence and increase the reflection at the working wavelength in a targeted manner by selecting the layer materials and layer thicknesses.
[0008] In preferred embodiments, the adhesive protection coating comprises layers of a material with a higher refractive index at the operating wavelength and of a material with a lower refractive index at the operating wavelength, wherein the layers of material with the higher refractive index and the layers of material with the lower refractive index are arranged alternately. Reflection can occur at each layer boundary. By selecting the layer thicknesses accordingly depending on the incident wavelength, the total reflection at the adhesive protection coating can be increased and absorption reduced. It is particularly advantageous to select layer thicknesses in the range of one-quarter of the incident wavelength.To achieve the highest possible reflection at a given wavelength, it is preferable to work with optical thicknesses of a layer pair consisting of a layer of material with a higher refractive index and a layer of material with a lower refractive index in the range of half the wavelength. The refractive index of the respective layer materials influences the optical thickness.
[0009] Advantageously, the adhesive protective coating comprises at least two layers of the material with a higher refractive index at the operating wavelength and at least one layer of the material with a lower refractive index at the operating wavelength, in order to achieve an increase in reflection while simultaneously reducing absorption, particularly at the operating wavelength. Furthermore, the transmission at the curing wavelength can be kept sufficiently high for the adhesive to cure.
[0010] For these purposes, the adhesive protective coating preferably comprises between three and sixteen layers of the material with a higher refractive index at the operating wavelength and between three and sixteen layers of the material with a lower refractive index at the operating wavelength. This number of layers allows for efficient adjustment of the reflection while simultaneously keeping the coating effort to a minimum.
[0011] Advantageously, the adhesive protection coating has, on the adhesive side, as the outermost layer, a layer made of the material with a higher refractive index at the working wavelength.
[0012] It is also advantageous if the adhesive protection coating has, on its outermost layer, a layer made of a material with a higher refractive index at the working wavelength. Both measures, separately or in combination, can contribute to increasing reflection at the working wavelength. In the latter case, the thickness of the outermost layer facing away from the adhesive can preferably be different from that of the remaining layers made of material with a higher refractive index at the working wavelength. In a multi-layer adhesive protection coating optimized for particularly high reflection in the working wavelength range, this measure can increase transmission in the curing wavelength range.
[0013] Preferably, all layers of a material with a higher or lower refractive index at the operating wavelength have the same thickness. The resulting, so-to-speak, periodic structure of the adhesive protective coating can significantly increase reflection or significantly reduce absorption, particularly for narrower operating wavelength ranges with widths in the nanometer or subnanometer range. Therefore, such modules are particularly well suited for use with lasers as a radiation source.
[0014] In a preferred embodiment, the working wavelength is different from the curing wavelength, in which case the adhesive protective coating has a reflection of greater than 70%, preferably greater than 80%, particularly preferably greater than 90%, at the working wavelength and a transmission of greater than 90% at the curing wavelength. Thus, after unhindered curing, impairments to the optical properties due to unwanted heating of the optical element can be particularly effectively avoided. Most preferably, the optical module is designed for a working wavelength of around 193 nm or 248 nm and a curing wavelength of around 365 nm.
[0015] In a further preferred embodiment, the working wavelength is equal to the curing wavelength, in which case the adhesive protective coating has a reflection of greater than 70%, preferably greater than 80%, particularly preferably greater than 90%, at the working wavelength and a transmission of greater than 2%, preferably 6%, at the curing wavelength. In this way, impairment of the optical properties due to unwanted heating of the optical element can be particularly effectively avoided without preventing curing of the adhesive. Most preferably, the optical module is designed for a working and curing wavelength around 365 nm.
[0016] The adhesive protection coating preferably comprises one, preferably two materials from the group consisting of silicon dioxide, aluminum oxide, hafnium dioxide, tantalum pentoxide, titanium dioxide, zinc sulfide, aluminum fluoride, cryolite, chiolite, and magnesium fluoride. Particularly preferably, the adhesive protection coating comprises, as the material with a higher refractive index at the operating wavelength, one from the group consisting of hafnium dioxide, aluminum oxide, tantalum pentoxide, titanium dioxide, and zinc sulfide, and, as the material with a lower refractive index at the operating wavelength, one from the group consisting of silicon dioxide, aluminum fluoride, magnesium fluoride, chiolite, and cryolite. Particularly for the ultraviolet wavelength range between 150 nm and 400 nm, these materials allow the production of multilayer adhesive protection coatings with a large difference in refractive index at the operating wavelength, which can lead to correspondingly high reflection.Particularly advantageous is the combination of lower refractive index silicon dioxide with higher refractive index aluminum oxide for working wavelengths in particular around 193 nm and 248 nm or with higher refractive index hafnium dioxide in particular for a working wavelength around 248 nm and with higher refractive index tantalum pentoxide for a working wavelength around 365 nm.
[0017] In a further aspect, this object is achieved by an optical module comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of an adhesive and wherein the module has an adhesive protective coating absorbing at the operating wavelength and the adhesive protective coating has an anti-reflective coating.
[0018] This optical module offers the advantage that the adhesive's anti-reflective coating not only protects the adhesive from radiation damage, but also suppresses residual reflections that could lead to stray radiation. It is particularly well-suited for use with optical elements whose heating does not significantly affect the wavefront of an image when incorporated into the beam path of an optical system.
[0019] In a preferred embodiment, the anti-reflective coating comprises layers of a material with a higher refractive index at the operating wavelength and layers of a material with a lower refractive index in the operating wavelength range, with the layers of material with the higher refractive index and the layers of material with the lower refractive index being arranged alternately. The choice of layer materials, thicknesses, and number of layers allows for flexible influences on reflection, transmission, and absorption for specific wavelengths or wavelength ranges. Overall, a wavelength is referred to as a wavelength range with a width of ±1%. For a wider wavelength range, the mean wavelength can be considered alternatively.To achieve the lowest possible reflection at a given wavelength, optical thicknesses of a layer pair consisting of a layer of material with a higher refractive index and a layer of material with a lower refractive index are used in the range of a quarter of the wavelength, but also significantly above or below. The refractive index of the respective layer materials influences the optical thickness. Preferably, the anti-reflective adhesive protection coating, like the previously described multilayer adhesive protection coating, comprises one, preferably two materials from the group consisting of silicon dioxide, aluminum oxide, hafnium dioxide, tantalum pentoxide, titanium dioxide, zinc sulfide, aluminum fluoride, cryolite, chiolite, and magnesium fluoride.Particularly preferably, the adhesive protection coating comprises as material with higher refractive index at the working wavelength one of the group formed by hafnium dioxide, aluminum oxide, tantalum pentoxide, titanium dioxide and zinc sulfide and as material with lower refractive index at the working wavelength one of the group formed by silicon dioxide, aluminum fluoride, magnesium fluoride, chiolite and cryolite.
[0020] In another preferred embodiment, the anti-reflective coating is designed as a coating with a refractive index gradient. This provides an anti-reflective effect across a broader wavelength range. It is particularly advantageous for the refractive index to change from the refractive index of the material of the optical element to the refractive index of the material of the adhesive protective coating. A particularly good anti-reflective effect can be achieved by changing the refractive index as continuously as possible.
[0021] In a further aspect, the object is achieved by an optical module comprising an optical element for a working wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is glued to the holder by means of an adhesive and wherein the module has a diffractive structure in the region of the adhesive.
[0022] By providing a diffractive structure, it can be ensured that radiation of the working wavelength does not reach the adhesive and damage it in the process, nor that this radiation is reflected at the edge of the optical element and reduces the contrast of the image through the optical element, nor that this radiation is absorbed and thus contributes to heating of the optical element, which would have a disruptive influence on the wavefront and thus on the image, particularly in the case of inhomogeneous or only local heating. For this purpose, the diffractive structure is preferably structured in such a way that the useful radiation incident there is diffracted out of the beam path. Diffractive structures designed as periodic diffraction gratings are particularly preferably provided. The provision of a diffractive structure can also be combined with a highly reflective or, in particular, an anti-reflective adhesive protective coating in order to prevent interfering radiation of different wavelengths orwith different angles of incidence from the beam path.
[0023] The diffractive structure preferably has an angle of inclination relative to the normal of the surface of the optical element, particularly if the diffractive structure is designed as a periodic diffraction grating. This has the significant advantage that, in contrast to diffractive structures without an angle of inclination, not only the first and second orders of diffraction are diffracted from the beam path, but also the zeroth order, which is simultaneously the order with the highest intensity. With a diffractive structure with varying heights and angles of inclination, antireflection can also be achieved for a wider range of wavelengths or angles of incidence.
[0024] Advantageously, the optical module includes a radiation absorber. The beam absorber can absorb the diffracted radiation and thus efficiently remove it from the beam path.
[0025] Preferably, the optical element in all of the aforementioned modules is configured as a lens. This makes the optical modules particularly suitable for use in UV lithography devices and inspection systems for examining masks for lithographic exposure or wafers before or after exposure.
[0026] Furthermore, the object is achieved by an optical system with one of the optical modules as described above. Furthermore, the object is achieved by a device with one of the optical modules as described above or an optical system as just mentioned, wherein it is configured as a UV lithography device or inspection device.
[0027] The present invention will be explained in more detail with reference to a preferred embodiment.
[0028] Figure 1 is a schematic diagram of a UV lithography device;
[0029] Figure 2 shows a schematic diagram of an inspection system;
[0030] Figure 3 is a schematic diagram of an optical module;
[0031] Figure 4 is a schematic diagram of an adhesive protective coating of an optical module;
[0032] Figure 5 shows the reflection as a function of wavelength for a first and a second exemplary embodiment of an adhesive protection coating; Figure 6 shows the transmission as a function of wavelength for the first and second exemplary embodiment of an adhesive protection coating;
[0033] Figure 7 shows the reflection as a function of wavelength for a third and a fourth exemplary embodiment of an adhesive protection coating;
[0034] Figure 8 shows the transmission as a function of wavelength for the third and fourth exemplary embodiments of an adhesive protection coating;
[0035] Figure 9 shows the reflection as a function of wavelength for a fifth and a sixth exemplary embodiment of an adhesive protection coating;
[0036] Figure 10 shows the transmission as a function of wavelength for the fifth and sixth exemplary embodiments of an adhesive protection coating;
[0037] Figure 11 is a schematic diagram of a second optical module;
[0038] Figure 12 shows the proportion of oxygen concentration as a function of the distance from the lens surface for a first embodiment of an adhesive protective coating with anti-reflective coating;
[0039] Figure 13 shows the reflection as a function of wavelength for the first
[0040] Implementation of an adhesive protective coating with anti-reflective coating;
[0041] Figure 14 shows the reflection as a function of the angle of incidence for the first
[0042] Implementation of an adhesive protective coating with anti-reflective coating;
[0043] Figure 15 shows the reflection as a function of wavelength for a second
[0044] Implementation of an adhesive protective coating with anti-reflective coating;
[0045] Figure 16 shows the transmission as a function of wavelength for a second
[0046] Implementation of an adhesive protective coating with anti-reflective coating;
[0047] Figure 17 is a schematic diagram of a third optical module; and Figure 18 is a schematic diagram of an embodiment of the third optical module.
[0048] Figure 1 shows a schematic diagram of a device 1 for UV lithography, in particular for wavelengths in the range from 190 nm to 400 nm. The UV lithography device 1 has, as essential components, in particular two optical systems 12, 14: an illumination system 12 and a projection system 14. To carry out the lithography, a radiation source 10 is required, particularly preferably an excimer laser, which emits, for example, at 193 nm or 248 nm and which can be an integral component of the UV lithography device. A mercury lamp can also be used, wherein the emitted i-line around 368 nm can be used as the working wavelength and / or as the curing wavelength in an adhesive process carried out outside the respective optical system.The radiation 11 emitted by the radiation source 10 is processed by the illumination system 12 so that a mask 13, also called a reticle, can be illuminated. In the example shown here, the illumination system 12 has transmissive and reflective optical elements. Representative here are the transmissive optical element 120, which, for example, focuses the radiation 11, and the reflective optical element 121, which, for example, deflects the radiation. All optical elements can be part of an optical module as proposed here. In a known manner, a wide variety of transmissive, reflective, and other optical elements can be combined with one another in the illumination system 12 in any desired, even more complex, manner. It should be noted that the mask 13 can also be part of an optical module as proposed here.
[0049] The mask 13 has a structure on its surface which is transferred to an element 15 to be exposed, for example a wafer during the production of semiconductor components, with the aid of the projection system 14. In the present example, the mask 13 is designed as a transmissive optical element. In further embodiments, it can also be configured as a reflective optical element. In the example shown here, the projection system 14 has at least one transmissive optical element. In the example shown here, two transmissive optical elements 140, 141 are shown as representatives, which serve, for example, in particular to reduce the structures on the mask 13 to the size desired for exposing the wafer 15. Reflective optical elements can also be provided in the projection system 14, and a wide variety of optical elements can be combined with one another as desired in a known manner.It should be noted that optical systems without transmissive optical elements can also be provided, especially in optical systems optimized for wavelengths of less than 200 nm. All optical elements of the projection system 14 can also be part of an optical module proposed here.
[0050] Optical modules comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of irradiation with an adhesive curable at a curing wavelength range in the ultraviolet wavelength range, and wherein the module has an adhesive protective coating, wherein the adhesive protective coating is multilayered and highly reflective and low-absorbing at the operating wavelength, can also be used in wafer or mask inspection systems. An exemplary embodiment of a wafer inspection system 2 is shown schematically in Figure 2. The explanations also apply to mask inspection systems.
[0051] The wafer inspection system 2 has a radiation source 20, the radiation of which is directed onto a wafer 25 by an optical system 22. For this purpose, the radiation is reflected onto the wafer 25 by a concave mirror 220. In a mask inspection system, a mask to be examined could be arranged instead of the wafer 25. The radiation reflected, diffracted, and / or refracted by the wafer 25 is guided by a concave mirror 221, which is also part of the optical system 22, to a detector 23 for further analysis. The radiation source 20 can, for example, be precisely one radiation source or a combination of several individual radiation sources in order to provide an essentially continuous radiation spectrum. In modifications, one or more narrowband radiation sources can also be used.The inspection system illustrated here as an example is designed for an operating wavelength in the range between 190 nm and 300 nm, particularly preferably between 190 nm and 200 nm. In addition to and / or alternatively to the two concave mirrors 220, 221, lenses can also be provided in the wafer or mask inspection system. In inspection systems designed for operating wavelengths in the range of 200 nm to 400 nm, in particular 300 nm to 400 nm, all optical elements can be designed as lenses.
[0052] Figure 3 shows an embodiment of an optical module 300. In the present example, the optical element 301 is a concave lens that is transparent to an operating wavelength in the ultraviolet wavelength range. The lens 301 is mounted in a holder 303. For this purpose, the lens is glued to the holder 303 using a UV-curable adhesive 305, preferably outside the optically used area during operation. Epoxy-based adhesives, for example, are used as mounting adhesives that can be cured with UV radiation from the i-line of a mercury lamp. Irradiation of the lens during operation, particularly due to stray light or multiple reflections, can cause long-term radiation damage to the adhesive, resulting in it losing its adhesion or becoming deformed, so that the lens 301 is no longer held in the originally adjusted position in the holder 303, and imaging errors can occur.Therefore, an adhesive protection coating 307 is provided between lens 301 and adhesive 305. It is multi-layered and highly reflective and low-absorbing at the operating wavelength. Like dielectric multi-layer anti-reflection coatings typically provided on lenses, it can be applied using conventional thin-film coating processes such as thermal electron beam evaporation or magnetron sputtering. To increase the mechanical strength of optical module 300, ion-assisted coating processes are preferably selected. To simplify handling, adhesive protection coating 307 can be applied locally to lens 301 before it is bonded to holder 303. The adhesive can then be cured by irradiation (indicated by dashed arrow 309) at the curing wavelength for which adhesive protection coating 307 is sufficiently transparent.At the operating wavelength, a large portion of the incident radiation 309 is reflected out of the beam path, so that absorption at the bonding point is so low that local heating of the lens 301, which could lead to imaging errors such as wavefront aberration, does not occur. The absorption, which may be sufficiently low to prevent unwanted heating, can also contribute to protecting the adhesive 305 from radiation damage.
[0053] The area of the adhesive protective coating of the optical module is shown in more detail in Figure 4. The adhesive protective coating 407 is arranged between the optical element 401 and the adhesive 405. The adhesive protective coating 407 is multi-layered, preferably composed of at least three layers. By selecting the number of layers, the layer thickness, and the layer materials, the reflection, transmission, and absorption at the relevant wavelengths can be adjusted for any combination of operating wavelength and curing wavelength such that the reflection is as high as possible and the absorption as low as possible in order to avoid undesired heating of the optical element 401 and radiation damage to the adhesive 405, while the transmission at the curing wavelength is still sufficiently high to allow the adhesive 405 to cure.
[0054] It has proven particularly useful if the adhesive protection coating 407 has layers 471 made of a material with a higher refractive index at the working wavelength and layers 473 made of a material with a lower refractive index at the working wavelength, wherein the layers 471 made of material with the higher refractive index and the layers 473 made of material with the lower refractive index are each arranged alternately. In this way, an adhesive protection coating 407 can be designed particularly efficiently which meets the requirements of high reflection with low absorption and sufficient transmission for a freely selected working wavelength and curing wavelength in the ultraviolet wavelength range. Preferably, the adhesive protection coating 407 has at least two layers 471 of the material with a higher refractive index at the working wavelength and at least one layer 473 of the material with a lower refractive index at the working wavelength.More preferably, the adhesive protective coating 407 comprises between three and sixteen layers 471 of the material having a higher refractive index at the operating wavelength and between three and sixteen layers 473 of the material having a lower refractive index at the operating wavelength.
[0055] In the example shown in Figure 4, four layers 471 of the material with a higher refractive index at the working wavelength and three layers 473 of the material with a lower refractive index at the working wavelength are provided. Both on the adhesive side and on the side facing away from the adhesive, a layer 47T, 471 of higher-refractive material is provided as the outermost layer. In the example shown here, all layers 471 of the higher-refractive material and all layers 473 of the lower-refractive material each have the same thickness, while the thickness of the outermost layer 47T on the adhesive side is different from that of the other layers 471 made of the higher-refractive material. This essentially results in a periodic layer sequence that is characterized by particularly high reflection at one wavelength, in particular when a unit consisting of two adjacent layers 471, 473 of higher- and lower-refractive material lies at approximately a quarter of the said wavelength.If necessary, the outermost layer on the adhesive side can break the periodicity to slightly increase the transmission at the curing wavelength and allow for faster curing. Alternatively, the bottom layer 471 with higher-refractive-index material on the optical substrate 401 can have a thickness other than a quarter of the working wavelength in order to specifically achieve the highest possible transmission at the curing wavelength while maintaining a high reflection at the working wavelength. Silicon dioxide, aluminum oxide, hafnium oxide, tantalum pentoxide, titanium dioxide, zinc sulfide, aluminum fluoride, cryolite, chiolite, and magnesium fluoride in combination with one or more of these materials or one or more additional materials have proven suitable as materials for the adhesive protective coating 407.Combinations of hafnium oxide, aluminum oxide, tantalum pentoxide, titanium dioxide or zinc sulfide as higher refractive index material with silicon dioxide, aluminum fluoride, magnesium fluoride, chiolite and cryolite as lower refractive index material have proven particularly effective.
[0056] The following figures show the reflection and transmission curves for various designs of adhesive protection coatings. Figure 5 shows the reflection and Figure 6 the transmission as a function of wavelength for two adhesive protection coatings A and B, both optimized for an operating wavelength Xi of 193 nm and a curing wavelength X2 of 365 nm. Adhesive protection coating A has fourteen layers of 27 nm thickness made of aluminum oxide as a higher-refractive material and thirteen layers of 31 nm thickness made of silicon dioxide as a lower-refractive material, arranged alternately. The reflection and transmission for adhesive protection coating A are plotted as dashed lines.Adhesive protection coating B consists of only ten layers of 27 nm thick aluminum oxide as a higher-refractive material and nine layers of 31 nm thick silicon dioxide as a lower-refractive material, arranged alternately. The reflection and transmission for adhesive protection coating B are plotted as solid lines.The adhesive protection coating B exhibits a reflection of almost 80% and a transmission of almost 20% at the working wavelength Xi, and a reflection of practically 0% and a transmission of practically 100% at the curing wavelength X2. This means that virtually no absorption of the respective radiation occurs in either the working wavelength Xi or the curing wavelength X2. This prevents unwanted heating of the respective optical element, but the adhesive can cure as if no adhesive protection coating were present, while the cured adhesive is still protected from radiation damage. By increasing the number of layers in the adhesive protection coating A, a reflection of over 90% and a transmission of less than 10% at the working wavelength Xi is achieved, which provides the adhesive with even better protection against radiation damage and a correspondingly longer service life.The residual absorption in the adhesive protective coating, which is less than 1% here, leads to such minimal heating of the lens that the wavefront and imaging properties are not altered beyond the required specifications. Rather, it serves to further protect the adhesive from radiation damage by absorbing the residual radiation energy.
[0057] Figure 7 shows the reflection and Figure 8 the transmission as a function of wavelength for two adhesive protection coatings C and D, both optimized for an operating wavelength Xi of 248 nm and a curing wavelength X2 of 365 nm. The adhesive protection coating C has seven layers with a thickness of 30 nm made of hafnium oxide as a material with a higher refractive index and seven layers with a thickness of 40 nm made of silicon dioxide as a material with a lower refractive index, which are arranged alternately. The topmost layer on the adhesive side is a further layer of hafnium dioxide with a thickness of 15 nm. The reflection and transmission for the adhesive protection coating C is plotted as a dashed line. The adhesive protection coating D has only five layers with a thickness of 30 nm made of hafnium oxide as a material with a higher refractive index and five layers with a thickness of 40 nm made of silicon dioxide as a material with a lower refractive index, which are arranged alternately.The transmission for the adhesive protective coating D is plotted as a solid line. The adhesive protective coating D exhibits a reflection of almost 95% and a transmission of just over 5% at the working wavelength Xi, and a reflection of practically 0% and a transmission of practically 100% at the curing wavelength X2. This means that virtually no absorption of the respective radiation occurs in either the working wavelength Xi or the curing wavelength X2. This prevents unwanted heating of the respective optical element, but the curing of the adhesive can occur as if no adhesive protective coating were present, while the cured adhesive is still protected from radiation damage.By increasing the number of layers in the adhesive protection coating C, a reflection of almost 100% and a transmission of almost 0% are achieved at the working wavelength Xi, which provides the adhesive with even better protection against radiation damage and a correspondingly longer service life. At the curing wavelength X2, the reflection is approximately 2% and the transmission approximately 98%, which still allows the adhesive to cure completely unhindered. The residual absorption in the adhesive protection coating of less than 1% here only leads to such minimal heating of the lens that the wavefront and imaging properties are not altered beyond the required requirements. Rather, it serves to further protect the adhesive from radiation damage by absorbing the residual radiation energy.Figure 9 shows the reflection and Figure 10 the transmission as a function of wavelength for two adhesive protection coatings E and F, both for a working wavelength and a curing wavelength X, respectively. 1 / 2of 365 nm. The adhesive protection coating E has seven layers with a thickness of 42 nm made of tantalum pentoxide as the higher refractive index material and six layers with a thickness of 60 nm made of silicon dioxide as the lower refractive index material, which are arranged alternately. The reflection and transmission for the adhesive protection coating E is plotted as a dashed line. The adhesive protection coating F has only five layers with a thickness of 42 nm made of tantalum pentoxide as the higher refractive index material and four layers with a thickness of 60 nm made of silicon dioxide as the lower refractive index material, which are arranged alternately. The reflection and transmission for the adhesive protection coating F is plotted as a solid line. The adhesive protection coating E has a reflection of approximately 97% and a transmission of just over 3% at the working and curing wavelength Xi / 2so that in this wavelength range, virtually no absorption of the respective radiation occurs, thus preventing unwanted heating of the respective optical element. The rather low transmission can be compensated for by a longer irradiation time for curing the adhesive. By reducing the number of layers in the adhesive protection coating F, a reflection of approximately 93% and a transmission of approximately 7% at the working and curing wavelength X2 are still achieved, which means that the adhesive cures, to a first approximation, twice as fast as with the adhesive protection coating E.
[0058] To estimate the transmission required for the adhesive curing, for example with the i-line of 365 nm of a mercury lamp as the curing wavelength, the required irradiation dose D in J / cm 2 , the maximum permissible irradiation time t in s and the power density P in W / cm 2The mercury lamp used for curing on the optical element can be used at the curing wavelength. The required transmission at the curing wavelength in percent is then calculated as
[0059] T = 100%*D / (P*t).
[0060] The minimum permissible reflection at the working wavelength can be calculated from the guaranteed lifetime t L T in s, maximum radiation dose degradation in J / cm 2 , under which the adhesive function is still maintained, and the power density of scattered light and residual reflections P incident at the adhesive point str eu in W / cm 2 accordingly and is then calculated as R = 100%*(1 "Ddegradation / P scatter t|_"r) -
[0061] These estimates are particularly important when the curing wavelength is the same as the working wavelength. If necessary, the reflection can be increased to the desired value by increasing the number of layers. On the other hand, the transmission at the curing wavelength can be increased by appropriately tuning the outermost layer of higher-refractive material on the adhesive side by choosing a different layer thickness than the other layers of higher-refractive material.
[0062] Figure 11 illustrates an embodiment of a second optical module 1100. In the present example, the optical element 1101 is a convex lens that is transparent to an operating wavelength in the ultraviolet wavelength range. The lens 1101 is mounted in a holder 1103. For this purpose, the lens is glued to the holder 1103 using a UV-curable adhesive 1105, preferably outside the optically used area during operation. Epoxy-based adhesives, for example, are used as mounting adhesives that can be cured with UV radiation from the i-line of a mercury lamp. Irradiation of the lens during operation, particularly due to stray light or multiple reflections, can cause long-term radiation damage to the adhesive, resulting in it losing its adhesion or becoming deformed, so that the lens 1101 is no longer held in the originally adjusted position in the holder 1103, and imaging errors can occur.Therefore, an adhesive protection coating 1111 with an absorbing layer 1110 and an anti-reflective coating 1112 is provided between lens 1101 and adhesive 1105. The anti-reflective coating 1112 can be applied using conventional coating methods in thin-film technology, such as thermal electron beam evaporation or magnetron sputtering. To increase the mechanical strength of the optical module 1100, ion-assisted coating methods are preferably selected to apply the adhesive protection coating 1111 and, in particular, its anti-reflective coating 1112.
[0063] In one embodiment, the anti-reflective coating of the adhesive protective coating is designed as a coating with a refractive index gradient. Extensive anti-reflective coating is possible if the coating between the material of the optical element and the adhesive protective coating has a refractive index gradient that continuously changes from the refractive index of the material of the optical element to the refractive index of the material of the adhesive protective coating. In the present example, an optical module is considered in which the optical element is designed as a lens made of quartz glass, and the material of the absorbing layer of the adhesive protective coating is amorphous silicon, which strongly absorbs radiation of wavelengths below 400 nm.A SiOx gradient layer is applied between the lens and the amorphous silicon layer for anti-reflective coating. The gradient layer's oxygen content decreases continuously from the lens surface, where x=2, to x=0 at the transition to the silicon layer, as shown in Figure 12. For example, silicon can first be reactively sputtered from a target in a saturated oxygen atmosphere, initially forming a SiO2 layer. The oxygen content in the coating system is then continuously reduced, so that the oxygen content in the SiOx layer also decreases, and x decreases from 2 to 0. Finally, the silicon is evaporated in a high vacuum at a pressure of less than 10. -5mbar, i.e., without oxygen. Figure 13 shows the reflection for the resulting optical module at quasi-normal incidence as a function of wavelength. The vertical, different dashed lines indicate the wavelengths 193 nm, 248 nm, and 365 nm. The solid reflection curve shows the reflection of the optical module with an anti-reflective adhesive protective coating, i.e., with amorphous silicon to protect the adhesive and the anti-reflective coating with a refractive index gradient as shown in Figure 12. For comparison, the dashed reflection curve shows the reflection of a corresponding optical module without anti-reflective coating, i.e., with only amorphous silicon on quartz glass.Accordingly, Figure 14 shows the reflection at a wavelength of 248 nm as a function of the angle of incidence. The solid reflection curve shows the reflection with anti-reflective coating, and for comparison, the dashed reflection curve shows the reflection without anti-reflective coating on the amorphous silicon adhesive protective coating. The anti-reflective coating of the adhesive protective coating using a coating with a refractive index gradient results in very low reflection of less than 1% over a very wide wavelength range from 180 nm to 390 nm and over a very wide angle of incidence range up to 50°, making this type of optical module very flexible in its application.
[0064] In a further embodiment, the anti-reflective coating can comprise layers of a material with a higher refractive index at the operating wavelength and layers of a material with a lower refractive index in the operating wavelength range, wherein the layers of material with the higher refractive index and the layers of material with the lower refractive index are arranged alternately. The resulting dielectric multilayer anti-reflective coating can be described analogously to the highly reflective coating of the first optical module as shown in Figures 3 and 4. The fundamental difference is that different layer thicknesses are used.While for anti-reflective coating the optical thicknesses of a pair of layers made of higher and lower refractive index material are essentially in the range of about a quarter of the working wavelength of the respective optical element, for particularly high reflection they are in the range of about half the working wavelength. For the optical thickness, the geometric thickness is weighted by the refractive index of the respective layer material. The specific thicknesses of the higher and lower refractive index layers are optimized for the highest possible anti-reflective properties. Suitable materials for the higher refractive index layers include aluminum oxide for wavelengths of 193 nm and above, hafnium oxide for wavelengths of 248 nm and above, and tantalum pentoxide for wavelengths of 365 nm and above. These materials, given as examples, have hardly any absorption above the respective wavelengths specified.Silicon dioxide is particularly suitable as the material for the lower-refractive-index layers for wavelengths of 193 nm and above. Applying both the higher- and lower-refractive-index layers using an ion-assisted coating process ensures high mechanical stability and sufficiently good layer adhesion.
[0065] Figure 15 shows the reflection and Figure 16 the transmission as a function of wavelength for an optical module that has a dielectric multilayer anti-reflective coating on its adhesive protection coating. The dashed vertical line represents the operating wavelength of 193 nm and the dotted line represents the wavelength of 365 nm at which the adhesive is cured. The optical module has a quartz glass lens as its optical element and a 180 nm thick layer of tantalum pentoxide as its adhesive protection coating. A coating of 22 nm aluminum oxide, 33 nm silicon dioxide and 22 nm aluminum oxide is applied to this as an anti-reflective coating. The dashed reflection and transmission curves show the reflection and transmission with anti-reflective coating, and the solid reflection and transmission curves show the reflection and transmission without anti-reflective coating for comparison.By applying an anti-reflective coating using a multi-layer dielectric coating, anti-reflective coating is achieved specifically around the working wavelength, where all incident radiation is absorbed by the adhesive protection coating while transmitting only negligibly. At the curing wavelength, however, both with and without anti-reflective coating, the transmittance is very high, with low reflection and low absorption, allowing the adhesive to cure very well through the quartz glass lens and the tantalum pentoxide adhesive protection coating. Depending on the wavelength, any material that would also be suitable as a high-refractive index layer material for a multi-layer anti-reflective coating or a multi-layer highly reflective adhesive protection coating can be used as an absorbing material for an adhesive protection coating.Metals, especially chromium, are suitable for absorbing UV radiation with longer wavelengths, such as 365 nm, as they also exhibit good adhesion properties to common lens materials. For shorter wavelengths, such as those in the range of 248 nm or 193 nm, fluoride crystals such as calcium fluoride or quartz glass are suitable; for longer wavelengths, such as around 365 nm, lead-containing glasses or borosilicate glasses are suitable. Depending on the material chosen for the adhesive protective coating and for the optical element, an additional adhesion promoter can also be used.
[0066] Figures 17 and 18 schematically illustrate another optical module 1700, 1800, which includes an optical element 1701, 1801 for an operating wavelength in the ultraviolet wavelength range and a holder 1703, 1803, wherein the optical element 1701, 1801 is bonded to the holder 1703, 1803 by means of an adhesive 1705, 1805. The optical modules 1700, 1800 illustrated here include a diffractive structure 1713, 1813 in the region of the adhesive 1705, 1805. In the present example, the optical elements 1701, 1801 are designed as lenses.
[0067] By specifically structuring the lenses 1701, 1801 in their edge region, in which the respective holders 1703, 1803 are arranged, such that the radiation 1721, 1723, 1821 impinging there is diffracted from the beam path, it can be achieved that neither radiation 1721, 1723, 1821 reaches the adhesive 1705, 1805 and damages it, nor that radiation 1721, 1723, 1821 is reflected at the lens edge and thereby reduces the contrast, nor that radiation 1721, 1723, 1821 is absorbed and thus contributes to lens heating, which has a disruptive influence on the wavefront and thus the imaging. For example, a periodic diffraction grating 1713 without inclination of the diffractive structures relative to the lens surface can be selected as diffractive structures.The first and higher diffraction orders are thus deflected from the disturbing reflection path, whereby, depending on the diffraction efficiency, it must be ensured that the diffraction path leads to comparatively uncritical regions.
[0068] In the example shown in Figure 17, a radiation absorber 1715 is provided on the optical module 1700. It has a low thermal coupling to the lens 1701 and essentially absorbs the radiation 1722, 1724 incident on it, which was diffracted from the beam path by the diffraction grating 1713, thus definitively removing it from the optical module 1700.
[0069] It is very advantageous to design the diffractive structure as an inclined structure 1813, in particular gratings such as blazed gratings or echelette gratings, in which the zeroth diffraction order is already extracted from the beam path (see also Figure 18). The angle of inclination of the diffractive structure 1813 is designed in the present example such that the diffracted radiation 1822 is directed onto a radiation absorber that absorbs as completely as possible and is not shown in Figure 18 for the sake of clarity. The depth of the structures 1813 in the present example is 1 of the working wavelength to be diffracted, i.e., 193 nm / 4, i.e., approximately 48 nm, 248 nm / 4, i.e., approximately 62 nm, or 365 nm / 4, i.e., approximately 91 nm. If the structures 1813 are filled with adhesive 1805 as in the example shown in Figure 18, the depth must be divided by the refractive index of the adhesive.An etch stop layer can be used to fabricate the diffractive structure. The material of the etch stop layer should be as transparent as possible at the operating wavelength. For example, the diffractive structure can be fabricated by etching from a silicon dioxide layer with a thickness corresponding to the structure depth to be etched, deposited on an approximately 5 nm to 10 nm thick aluminum layer, which is inert to a reactive etching process.
[0070] List of reference symbols
[0071] 1 VUV lithography device
[0072] 2 Wafer inspection system
[0073] 3 reflective optical element
[0074] 4 reflective optical element
[0075] 5 reflective optical element
[0076] 6 reflective optical element
[0077] 10 Radiation source
[0078] 11 Radiation
[0079] 12 Lighting system
[0080] 13 Mask
[0081] 14 Projection system
[0082] 15 element to be exposed
[0083] 20 Radiation source
[0084] 21 Radiation
[0085] 22 optical system
[0086] 23 Detector
[0087] 25 wafers
[0088] 50 optical element
[0089] 51 Substrat
[0090] 120 lens
[0091] 121 mirrors
[0092] 140 lens
[0093] 141 lens
[0094] 220 mirrors
[0095] 221 mirrors
[0096] 300 optical module
[0097] 301 optical element
[0098] 303 holders
[0099] 305 Glue
[0100] 307 Adhesive protective coating
[0101] 309 UV radiation
[0102] 401 optical element
[0103] 405 Glue
[0104] 407 Adhesive protection coating 71, 47 T higher refractive index layer 73 lower refractive index layer
[0105] 1100 optical module
[0106] 1101 optical element
[0107] 1103 holders
[0108] 1105 Glue
[0109] 1109 UV radiation
[0110] 1110 absorbent layer
[0111] 1111 Adhesive protective coating
[0112] 1112 Anti-reflective coating
[0113] 1210 reflective surface
[0114] 1700 optical module
[0115] 1701 optical element
[0116] 1703 Holder
[0117] 1705 glue
[0118] 1713 Diffraction structure
[0119] 1721 UV radiation
[0120] 1722 UV radiation
[0121] 1723 UV radiation
[0122] 1724 UV radiation
[0123] 1800 optical module
[0124] 1801 optical element
[0125] 1803 Holder
[0126] 1805 glue
[0127] 1813 Diffraction structure
[0128] 1821 UV radiation
[0129] 1822 UV radiation
Claims
Patent claims 1. An optical module comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of irradiation with an adhesive curable at a curing wavelength in the ultraviolet wavelength range, and wherein the module has an adhesive protective coating, characterized in that the adhesive protective coating (307, 407) is designed in multiple layers and is highly reflective and slightly absorbent in the operating wavelength range.
2. Optical module according to claim 1, characterized in that the adhesive protective coating (307, 407) has at least three layers (471, 473).
3. Optical module according to claim 1 or 2, characterized in that the adhesive protective coating (307, 407) has layers (471) made of a material with a higher refractive index at the working wavelength and layers (473) made of a material with a lower refractive index in the working wavelength range, wherein the layers (471) made of material with the higher refractive index and the layers (473) made of material with the lower refractive index are each arranged alternately.
4. Optical module according to one of claims 1 to 3, characterized in that the adhesive protective coating (307, 407) has at least two layers (471) of the material with a higher refractive index at the working wavelength and at least one layer (473) of the material with a lower refractive index at the working wavelength.
5. Optical module according to one of claims 1 to 4, characterized in that the adhesive protective coating (307, 407) comprises between three and sixteen layers (471) of the material with a higher refractive index in the operating wavelength range and between three and sixteen layers (473) of the material with a lower refractive index in the operating wavelength range.
6. Optical module according to one of claims 1 to 5, characterized in that the adhesive protective coating (307, 407) has, on the adhesive side, as the outermost layer, a layer (471) made of the material with a higher refractive index at the working wavelength.
7. Optical module according to claim 6, characterized in that the adhesive protective coating (307, 407) has, on its side facing away from the adhesive, as an outermost layer a layer (471) made of the material with a higher refractive index at the working wavelength.
8. Optical module according to claim 7, characterized in that the thickness of the outermost layer (471 ') facing away from or towards the adhesive is different from that of the remaining layers (471) made of the material with a higher refractive index at the working wavelength.
9. Optical module according to one of claims 3 to 7, characterized in that all layers (471, 473) of a material have the same thickness.
10. Optical module according to one of claims 1 to 9, wherein the working wavelength is not equal to the curing wavelength, characterized in that the adhesive protective coating (307, 407) has a reflection of greater than 70%, preferably greater than 80%, particularly preferably greater than 90% at the working wavelength and a transmission of greater than 90% at the curing wavelength.
11. Optical module according to claim 10, characterized in that it is designed for an operating wavelength of around 193 nm or 248 nm and a curing wavelength of around 365 nm.
12. Optical module according to one of claims 1 to 9, wherein the working wavelength is equal to the curing wavelength, characterized in that the adhesive protective coating (307, 407) has a reflection of greater than 70%, preferably greater than 80%, particularly preferably greater than 90% at the working wavelength and a transmission of greater than 2%, preferably greater than 6% at the curing wavelength.
13. Optical module according to claim 12, characterized in that it is designed for a working wavelength and a curing wavelength around 365 nm.
14. Optical module according to one of claims 1 to 13, characterized in that the adhesive protective coating (307, 407) consists of one, preferably two materials from the Group formed by silicon dioxide, aluminum oxide, hafnium dioxide, tantalum pentoxide, titanium dioxide, zinc sulfide, aluminum fluoride, cryolite, chiolite and magnesium fluoride.
15. Optical module according to claim 14, characterized in that the adhesive protective coating (307, 407) has as material with higher refractive index at the operating wavelength one of the group formed by hafnium dioxide, aluminum oxide, tantalum pentoxide, titanium dioxide and zinc sulfide and as material with lower refractive index at the operating wavelength one of the group formed by silicon dioxide, aluminum fluoride, magnesium fluoride, chiolite and cryolite.
16. An optical module comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is bonded to the holder by means of an adhesive and wherein the module has an adhesive protective coating absorbing at the operating wavelength, characterized in that the adhesive protective coating (1111) has an anti-reflective coating (1112).
17. Optical module according to claim 16, characterized in that the anti-reflection coating (1112) has layers of a material with a higher refractive index at the working wavelength and layers of a material with a lower refractive index in the working wavelength range, wherein the layers of material with the higher refractive index and the layers of material with the lower refractive index are each arranged alternately. 18 Optical module according to claim 16, characterized in that the anti-reflection coating (1112) is designed as a coating with refractive index gradients.
19. Optical module comprising an optical element for an operating wavelength in the ultraviolet wavelength range and a holder, wherein the optical element is glued to the holder by means of an adhesive, characterized in that the module (1700) has a diffractive structure (1713) in the region of the adhesive (1705).
20. Optical module according to claim 19, characterized in that the diffractive structure (1813) has an angle of inclination to the normal of the surface of the optical element (1801).
21. Optical module according to claim 19 or 20, characterized in that it comprises a radiation absorber (1715).
22. Optical module according to one of claims 1 to 21, characterized in that the optical element (301, 1101, 1701, 1801) is designed as a lens (120, 140, 141).
23. Optical system (2, 12, 14) with an optical module according to one of claims 1 to 22.
24. Device with an optical module according to one of claims 1 to 22 or an optical system according to claim 23, wherein it is designed as a UV lithography device (1) or inspection device (2).
Citation Information
Patent Citations
Optical component, useful for a transmission of radiation, comprises a paint-like radiation-protective layer that comprises oxide material including germanium dioxide, antimony pentoxide, aluminum oxide and niobium pentoxide
DE102011080639A1
Optical mount with UV curable adhesive and protective coating
EP0895113A2
Optical mount with UV adhesive and protective layer
US20060033984A1
UV protective coating for lens assemblies
US20150070906A1