Spatial light modulator

By deploying a high refractive index micro-nano structure in the first dielectric layer of the spatial light modulator, the crosstalk problem caused by the reduction of pixel spacing and the uncertainty in the orientation of the phase change material layer are solved, and full phase modulation of smaller pixels is achieved. and greater design freedom.

WO2024198746A1PCT designated stage expired Publication Date: 2024-10-03HUAWEI TECH CO LTD +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/076578
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-24
Filing Date
2024-02-07
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

When existing spatial light modulators achieve full phase modulation of small pixels, the reduction in pixel spacing leads to an increase in electrical and optical crosstalk, which limits the design freedom of the pixel layer, and adding micro-nano structures to the phase change material layer will cause orientation uncertainty. properties, limiting the types and properties of available micro-nano structures.

Method used

The micro-nano structure is deployed in the first dielectric layer that does not absorb or rarely absorbs the electromagnetic wave to be modulated, so that it isolates the pixel layer and the phase change material layer, and achieves high reflection through high refractive index, decoupling the light reflection ability and the pixel layer control capabilities, thereby increasing design freedom and avoiding disturbance to the phase change material layer.

Benefits of technology

It achieves full phase modulation capability for smaller pixels, reduces crosstalk between pixels, increases design freedom, eliminates the need to limit the type of micro-nano structures, and improves spatial light modulation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024076578_03102024_PF_FP_ABST
    Figure CN2024076578_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A spatial light modulator, which can be applied to the technical field of electro-optical modulators. The spatial light modulator sequentially comprises, in a first direction, a conductive layer (101), a phase change material layer (102), a first dielectric layer (103) including a micro-nano structure (106), a pixel layer (104) and a circuit control layer (105), wherein the conductive layer (101) is used for regulating electromagnetic waves to be modulated; the phase change material layer (102) is used for performing a reversible transition between different phase states; the first dielectric layer (103) is used for isolating the pixel layer (104) from the phase change material layer (102); the micro-nano structure (106) is used for reflecting the electromagnetic waves to be modulated; each pixel in the pixel layer (104) is used for independently controlling the optical characteristics of the electromagnetic waves that interact with the pixel; and the circuit control layer (105) is used for independently controlling each pixel. The first dielectric layer (103) which does not absorb or absorbs very few electromagnetic waves to be regulated can sufficiently isolate the pixel layer (104) from the phase change material layer (102), and the micro-nano structure (106) has a high refractive index, such that the reflection capability thereof for the electromagnetic waves to be modulated can be improved, and the light reflection capability is fundamentally decoupled from the independent control capability of the pixel layer (104), thereby improving the degree of freedom of the design of the pixel layer (104).
Need to check novelty before this filing date? Find Prior Art

Description

A spatial light modulator

[0001] This application claims priority to the Chinese patent application filed with the State Intellectual Property Office on March 24, 2023, with application number 202310336198.X and invention name “A Spatial Light Modulator”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application relates to the technical field of electro-optical modulators, and in particular to a spatial light modulator. Background Art

[0003] A spatial light modulator (SLM) is a device that can load information onto a one- or two-dimensional optical data field, effectively leveraging the inherent speed, parallelism, and interconnectivity of light. Under the control of a time-varying electrical drive signal or other signal, these devices can change the amplitude, phase, wavelength, and polarization state of the spatial distribution of light, or convert incoherent light into coherent light. An SLM primarily consists of numerous independent units (i.e., pixels) distributed in a one- or two-dimensional array. Each unit can be independently controlled by an optical or electrical signal and changes its optical properties according to the modulation signal, thereby modulating the light waves passing through it.

[0004] The amount of phase that can be adjusted for each pixel of the SLM is determined by phi = d * ΔN * m / λ, where phi is the phase, the unit is radian, d is the thickness of the phase change material layer in the SLM, ΔN is the birefringence index difference of the phase change material (such as liquid crystal) at the working wavelength λ, and m is the number of times the modulated electromagnetic wave propagates through it. To achieve the function of full phase modulation, the value of phi needs to be greater than 2pi. This limitation means that under the same phase change material, d must be greater than d to achieve phi = 2pi. min . The direct result of this is that the electrical and optical crosstalk between pixels will become more and more serious as the pixel pitch p becomes smaller. Experience shows that when d / p>1, the benefits of reducing the size of the pixels are not great. In order to solve the crosstalk problem of small pixels and improve the performance of spatial light modulation, nanoantennas can produce greater phase modulation capabilities through modulation media. While achieving the same modulation amount, the thickness of the phase change material layer can be further reduced, thereby reducing the possible crosstalk between pixels. To achieve the same crosstalk performance, the spacing p between pixels can also be reduced, thereby achieving full phase modulation capabilities of smaller pixels. In this SLM, nanoantennas are realized by adding micro-nano structures to the phase change material layer.

[0005] However, as a modulation layer controlled by an excitation source, the addition of micro-nanostructures to the phase-change material layer can disturb it, causing orientation uncertainty and, consequently, performance loss. To ensure good performance, device design must be restricted, which limits the types of micro-nanostructures that can be used, resulting in limited performance and functionality.

[0006] Summary of the Invention

[0007] The present application provides a spatial light modulator. By deploying a micro-nanostructure in a first dielectric layer that does not absorb or rarely absorbs (i.e., the absorption of the electromagnetic wave to be modulated is less than a first threshold) the electromagnetic wave to be modulated, the first dielectric layer not only isolates the pixel layer and the phase change material layer, but also, due to its high refractive index (i.e., the refractive index is greater than a second threshold), the micro-nanostructure therein can achieve high reflection of the electromagnetic wave to be modulated. This fundamentally decouples the light reflection capability from the independent control capability of the pixel layer, thereby increasing the design freedom of the pixel layer. Furthermore, because the micro-nanostructure is disposed in the first dielectric layer, it does not disturb the phase change material layer, and therefore there is no need to limit the type of micro-nanostructure.

[0008] Based on this, the embodiments of the present application provide the following technical solutions:

[0009] In the first aspect, an embodiment of the present application first provides an SLM, which can be applied to the field of electro-optical modulator technology. The SLM includes: a conductive layer, a phase change material layer, a first dielectric layer, a pixel layer and a circuit control layer in sequence along a first direction, and the first dielectric layer contains a micro-nano structure. The conductive layer is used to modulate the phase or amplitude of the electromagnetic wave to be modulated. The phase change material layer, which may also be referred to as a phase change layer or modulation layer, is used to reversibly transition between different phases. The absorption of the electromagnetic wave to be modulated by the first dielectric layer is less than a first threshold value, the specific value of which can be customized based on the actual application. The first dielectric layer is a dielectric layer that does not absorb or absorbs very little of the electromagnetic wave to be modulated, and is used to isolate the pixel layer from the phase change material layer. The micro-nanostructure is a dielectric layer or metal layer with a patterned structure that does not absorb or absorbs very little of the electromagnetic wave to be modulated. It has a high refractive index and is used to reflect the electromagnetic wave to be modulated. Therefore, the refractive index of the micro-nanostructure is limited to greater than a second threshold value, the specific value of which can be customized based on the actual application. The pixel layer includes multiple pixels, each of which is used to independently control the optical properties of the electromagnetic wave interacting with the pixel, for example, the phase, amplitude, polarization, or other optical properties of the electromagnetic wave (such as light, microwave, THz wave, etc.) interacting with it. The circuit control layer, which may also be referred to as a bottom circuit control layer or control system, is used to independently control each pixel, that is, the circuit control layer can independently control one or more pixels.

[0010] In the above-described embodiment of the present application, by deploying the micro-nanostructure in a first dielectric layer that does not absorb or very little (i.e., the amount of absorption of the electromagnetic wave to be modulated is less than a first threshold) the electromagnetic wave to be modulated, the first dielectric layer not only isolates the pixel layer and the phase change material layer, but also, due to its high refractive index (i.e., a refractive index greater than a second threshold), the micro-nanostructure therein can achieve high reflection of the electromagnetic wave to be modulated, fundamentally decoupling the light reflection capability from the independent control capability of the pixel layer, thereby increasing the design freedom of the pixel layer. Furthermore, because the micro-nanostructure is disposed in the first dielectric layer, it will not disturb the phase change material layer, and therefore there is no need to limit the type of micro-nanostructure.

[0011] In a possible implementation of the first aspect, all of the micro-nano structures are located inside the first dielectric layer.

[0012] In the above embodiment of the present application, the micro-nano structure is entirely located inside the first dielectric layer, which is a device structure of SLM in an application scenario. The purpose is to better shield the phase change material layer above, but allow the micro-nano structure to reflect more electromagnetic waves to be modulated.

[0013] In a possible implementation manner of the first aspect, a portion of the micro-nano structure may be located inside the first dielectric layer, wherein an upper surface of the micro-nano structure is higher than an upper surface of the first dielectric layer by a first height.

[0014] In the above embodiment of the present application, the micro-nano structure is partially located inside the first dielectric layer, which is another device structure of the SLM in another application scenario. The application scenario of this device structure does not require shielding the phase change material layer above, which broadens the application scenario.

[0015] In a possible implementation of the first aspect, the first height is less than one nth of the thickness of the micro-nanostructure, where n≥2, wherein the thickness of the micro-nanostructure is the distance between the upper surface of the micro-nanostructure and the lower surface of the micro-nanostructure.

[0016] In the above embodiment of the present application, the portion of the micro-nanostructure that protrudes above the first dielectric layer is at least less than 1 / n of the thickness of the micro-nanostructure. In this way, most of the micro-nanostructure will be surrounded by the first dielectric layer, and other layers above the micro-nanostructure will further fill the uneven areas caused by the micro-nanostructure and the first dielectric layer, ultimately resulting in a uniform surface.

[0017] In a possible implementation of the first aspect, the thickness of the micro-nanostructure (ie, the distance between the upper surface of the micro-nanostructure and the lower surface of the micro-nanostructure) is less than one m of the wavelength of the electromagnetic wave to be modulated, where m≥2.

[0018] In the above embodiments of the present application, by limiting the size of the micro-nanostructure to a sub-wavelength scale, there will be no diffraction effect within the wavelength range of the electromagnetic wave to be modulated.

[0019] In a possible implementation of the first aspect, the difference in refractive index between the first dielectric layer and the micro-nanostructure within the wavelength range of the electromagnetic wave to be modulated should be greater than 1.

[0020] In the above embodiment of the present application, the difference in refractive index between the first dielectric layer and the micro-nanostructure is greater than 1, which can enable the first dielectric layer to better isolate the phase change material layer and the pixel layer, while improving the reflection efficiency of the micro-nanostructure for the modulated electromagnetic wave.

[0021] In a possible implementation of the first aspect, the size of the micro-nano structure is subwavelength scale, and the micro-nano structure includes at least any one of the following: a one-dimensional periodic structure, a two-dimensional grid structure, wherein the grid structure is periodically distributed along each dimension.

[0022] In the above embodiments of the present application, there can be various types of micro-nano structures, which increases the design freedom of the micro-nano structures.

[0023] In a possible implementation manner of the first aspect, when the micro-nano structure is a one-dimensional periodic structure, the period of the periodic structure is smaller than the wavelength of the electromagnetic wave to be modulated.

[0024] In the above-mentioned embodiment of the present application, the period of the micro-nano structure needs to be smaller than the wavelength of the electromagnetic wave to be modulated. The purpose of this limitation is to improve the reflection ability of the micro-nano structure to the modulated electromagnetic wave, to decouple the electromagnetic wave to be modulated from the pixel layer below, so that the design of the pixel layer can be more diverse.

[0025] In a possible implementation of the first aspect, when the micro-nano structure is a two-dimensional grid structure, the period of the grid structure along each dimension is smaller than the wavelength of the electromagnetic wave to be modulated.

[0026] In the above-mentioned embodiment of the present application, the purpose of such limitation is also to improve the reflection ability of the micro-nano structure to the modulated electromagnetic wave, to decouple the modulated electromagnetic wave from the underlying pixel layer, and to make the design of the pixel layer more diverse.

[0027] In a possible implementation of the first aspect, the conductive layer may include only an electrode layer, and the electrode layer is used to cooperate with the circuit control layer to apply an electrical signal to the SLM to achieve phase or amplitude modulation of the electromagnetic wave to be modulated.

[0028] In the above-mentioned embodiment of the present application, the conductive layer may be only an electrode layer, and the process is simple.

[0029] In a possible implementation of the first aspect, the upper surface of the electrode layer may further include a dielectric reflection layer, where the dielectric reflection layer includes k layers of dielectric films for modulating the phase or amplitude of the electromagnetic wave to be modulated, where k≥1.

[0030] In the above-mentioned embodiment of the present application, the use of the dielectric reflective layer in conjunction with the first dielectric layer and the micro-nano structure can further reduce the lateral size of the pixel, and will not cause performance degradation due to the small pixel size, so an SLM with smaller pixels can be achieved without causing significant performance loss.

[0031] In a possible implementation manner of the first aspect, the thickness of each dielectric film in the k dielectric film layers is smaller than the wavelength of the electromagnetic wave to be modulated.

[0032] In the above embodiments of the present application, the purpose of such limitation is to better achieve the modulation of the phase or amplitude of the electromagnetic wave to be modulated.

[0033] In a possible implementation manner of the first aspect, when k≥2, the refractive index values ​​of adjacent dielectric films in the k-layer dielectric film are different.

[0034] In the above embodiments of the present application, the purpose of such limitation is to increase the modulation range of the phase or amplitude of the electromagnetic wave to be modulated.

[0035] In one possible implementation of the first aspect, the SLM further includes a functional layer located on the upper surface and / or lower surface of the phase change material layer for regulating the orientation of the phase change material layer. In a liquid crystal device, the functional layer can be a photo-alignment layer, an organic alignment layer, or an inorganic alignment layer.

[0036] In the above embodiments of the present application, the added functional layer is used to regulate the phase change material, thereby playing a role in orientation.

[0037] In a possible implementation of the first aspect, when the functional layer is located on the lower surface of the phase change material layer and the micro-nanostructure is entirely located inside the first dielectric layer, the sum of the thickness of the functional layer and the first distance of the micro-nanostructure is greater than one q of the electromagnetic wave to be modulated, the thickness of the functional layer is the distance between the upper surface of the functional layer and the lower surface of the functional layer, the first distance is the distance between the upper surface of the micro-nanostructure and the upper surface of the first dielectric layer, and q≥10.

[0038] In the above embodiments of the present application, the purpose of such limitation is to shield the upper phase change material layer from affecting the functions of the lower first dielectric layer and the micro-nanostructure when being modulated.

[0039] In a possible implementation of the first aspect, when a functional layer is located on the upper surface of the phase change material layer, the SLM further includes a second dielectric layer, the second dielectric layer contains the micro-nano structure, and the second dielectric layer is located between the functional layer and the conductive layer to isolate the functional layer and the conductive layer.

[0040] In the above embodiment of the present application, the second dielectric layer is located between the functional layer and the conductive layer, with the purpose of increasing the amplitude and / or phase of the modulated electromagnetic wave.

[0041] In a possible implementation of the first aspect, the phase change material layer can be a liquid crystal layer, which realizes the phase modulation of the incident light beam through the birefringence of the liquid crystal molecules. The phase change material layer can also be other electro-optical modulation materials. Specifically, this application does not limit the type of phase change material layer.

[0042] In the above-mentioned embodiment of the present application, a typical form of the phase change material layer is specifically described, which has wide applicability.

[0043] In a possible implementation of the first aspect, the upper surface of the conductive layer may be further covered with a substrate (also referred to as a device cover), such as glass, for device packaging.

[0044] In the above embodiments of the present application, a substrate may be provided to package the SLM for ease of application. BRIEF DESCRIPTION OF THE DRAWINGS

[0045] FIG1 is a schematic structural diagram of an SLM provided in an embodiment of the present application;

[0046] FIG2 is another schematic structural diagram of the SLM provided in an embodiment of the present application;

[0047] FIG3 is another structural diagram of the SLM provided in an embodiment of the present application;

[0048] FIG4 is another structural diagram of the SLM provided in an embodiment of the present application;

[0049] FIG5 is a schematic cross-sectional view of a first dielectric layer including a micro-nano structure according to an embodiment of the present application;

[0050] FIG6 is a schematic top view of the structure of a first dielectric layer including a micro-nano structure provided in an embodiment of the present application;

[0051] FIG7 is another schematic top view of the structure of the first dielectric layer including the micro-nano structure provided in an embodiment of the present application;

[0052] FIG8 is another schematic top view of the structure of the first dielectric layer including the micro-nano structure provided in an embodiment of the present application;

[0053] FIG9 is another schematic top view of the structure of the first dielectric layer including the micro-nano structure provided in an embodiment of the present application;

[0054] FIG10 is another schematic top view of the structure of the first dielectric layer including the micro-nano structure provided in an embodiment of the present application;

[0055] FIG11 is a schematic top view of a structure in which all micro-nano structures provided in an embodiment of the present application are located inside the first dielectric layer and the micro-nano structures are a two-dimensional grid structure;

[0056] FIG12 is another schematic structural diagram of an SLM in which a portion of the micro-nano structure is located inside the first dielectric layer according to an embodiment of the present application;

[0057] FIG13 is another schematic cross-sectional view of the first dielectric layer including the micro-nano structure provided in an embodiment of the present application;

[0058] FIG14 is another structural diagram of the SLM provided in an embodiment of the present application;

[0059] FIG15 is another structural diagram of the SLM provided in an embodiment of the present application. DETAILED DESCRIPTION

[0060] The present application provides a spatial light modulator. By deploying a micro-nanostructure in a first dielectric layer that does not absorb or rarely absorbs (i.e., the absorption of the electromagnetic wave to be modulated is less than a first threshold) the electromagnetic wave to be modulated, the first dielectric layer not only isolates the pixel layer and the phase change material layer, but also, due to its high refractive index (i.e., the refractive index is greater than a second threshold), the micro-nanostructure therein can achieve high reflection of the electromagnetic wave to be modulated. This fundamentally decouples the light reflection capability from the independent control capability of the pixel layer, thereby increasing the design freedom of the pixel layer. Furthermore, because the micro-nanostructure is disposed in the first dielectric layer, it does not disturb the phase change material layer, and therefore there is no need to limit the type of micro-nanostructure.

[0061] It should be understood that the terms "upper," "lower," etc. used in this application are used solely for the purpose of distinguishing descriptions and are not to be construed as indicating or implying relative importance or order. Furthermore, for the sake of brevity and clarity, reference numbers and / or letters are repeated in multiple figures of this application. This repetition does not indicate a strict limit relationship between the various embodiments and / or configurations. Furthermore, the terms "first," "second," etc. in the specification and claims of this application and the accompanying figures are used to distinguish similar objects and are not necessarily used to describe a specific order or precedence. It should be understood that the terms used in this manner are interchangeable where appropriate and are merely a means of distinguishing objects of the same attributes when describing the embodiments of this application. Furthermore, the terms "including," "having," and any variations thereof, are intended to cover non-exclusive inclusions, such that a process, method, system, product, or apparatus comprising a series of elements need not be limited to those elements, but may include other elements not explicitly listed or inherent to those processes, methods, products, or apparatuses.

[0062] An SLM is a miniature display consisting of one- or two-dimensionally arranged pixel strips or dots. Each pixel can independently control the phase, amplitude, polarization, or other optical properties of the electromagnetic waves (e.g., light, microwaves, THz waves, etc.) that interact with it. The most commonly used is the amplitude-type SLM, which is widely used in miniature image generators, augmented reality (AR), and virtual reality (VR) portable devices. Applications of phase-type SLM include liquid crystal antennas, adaptive optics, holographic displays, radar, lidar, wavelength selective switches (WSS), and so on. In order to improve the modulation performance of the SLM, the spacing between pixels is designed to be smaller and smaller, but the electrical and optical crosstalk between pixels becomes more serious as the pixel spacing becomes smaller, affecting the design freedom of the pixel layer in the SLM.

[0063] To this end, the present application provides an SLM. FIG1 is a schematic structural diagram of an SLM provided by an embodiment of the present application. As shown in FIG1 , the SLM includes, in sequence along a certain direction (i.e., a first direction), a conductive layer 101, a phase change material layer 102, a first dielectric layer 103, a pixel layer 104, and a circuit control layer 105. The first dielectric layer 103 includes a patterned micro-nano structure (abbreviated as micro-nano in FIG1 ) 106. Each layer is described below in sequence:

[0064] 1. Conductive layer 101

[0065] The conductive layer 101 is used to modulate the phase or amplitude of the electromagnetic wave to be modulated.

[0066] Specifically, in some embodiments of the present application, the conductive layer 101 may only include an electrode layer. For details, please refer to Figure 2, which is another structural schematic diagram of the SLM provided in an embodiment of the present application. The electrode layer 1001 is a specific implementation form of the conductive layer 101. The electrode layer 1001 is used to cooperate with the circuit control layer 105 to apply an electrical signal to the SLM to achieve phase or amplitude modulation of the electromagnetic wave to be modulated. The electrode layer 1001 is both transparent and conductive to the electromagnetic wave to be modulated, and therefore can also be called a conductive transparent layer. For example, the electrode layer 1001 can be indium tin oxide (ITO) or other transparent conductive materials, which is not limited in this application.

[0067] It should be noted that in some other embodiments of the present application, in addition to the electrode layer 1001, the conductive layer 101 may also include a dielectric reflective layer (also referred to as a dielectric reflective control layer). The dielectric reflective layer may be an additional film layer, such as a communication band of 1550nm, and this layer may be composed of silicon. The dielectric reflective layer may also be a dielectric layer containing a micro-nano structure, but the refractive index of the dielectric layer and the refractive index of the micro-nano structure are different from the refractive index of the first dielectric layer 103 and the refractive index of the micro-nano structure 106. Other parameters are similar. For details, please refer to the following description of the first dielectric layer 103 and the micro-nano structure 106, which will not be repeated here. The present application does not limit the specific type of the dielectric reflective layer. Please refer to Figure 3 for details. Figure 3 is another structural schematic diagram of the SLM provided in an embodiment of the present application. The dielectric reflective layer 1002 is located on the upper surface of the electrode layer 1001 and is used to modulate the phase or amplitude of the electromagnetic wave to be modulated to form a cavity. The dielectric reflective layer 1002 is a dielectric layer that has a different refractive index in the electromagnetic spectrum to be modulated than the SLM cover (e.g., glass) and electrode layer 1001, and exhibits low scattering and low absorption losses. The dielectric reflective layer 1002 comprises k (k ≥ 1) layers of dielectric film, i.e., the dielectric reflective layer 1002 is composed of at least one layer of dielectric film.

[0068] It should also be noted that in some embodiments of the present application, the thickness t of each of the k dielectric layers must satisfy the following: t < λ, where λ is the wavelength of the electromagnetic wave to be modulated, i.e., the operating wavelength of the SLM. This is to better modulate the phase or amplitude of the electromagnetic wave to be modulated.

[0069] It should also be noted that in some other embodiments of the present application, if the dielectric reflective layer 1002 is composed of at least two layers of dielectric films (i.e., k≥2), then the refractive index values ​​of the two adjacent dielectric films must be different, the purpose of which is to increase the modulation range of the phase or amplitude of the modulated electromagnetic wave.

[0070] It should be noted that in the embodiments of the present application, since the specific type of dielectric reflective layer 1002 is not limited, the thickness of the phase-change material layer 102 can be reduced when using a dielectric reflective layer 1002 that is selectable and can have multiple variations. This allows for high phase modulation at a much lower thickness than a conventional SLM. In other words, when the thickness of the phase-change material layer 102 is d, a conventional SLM requires a thickness greater than 3 / 2d. However, due to the presence of the dielectric reflective layer 1002, the present application can achieve the same phase modulation amount phi. Furthermore, the use of the dielectric reflective layer 1002 in conjunction with the first dielectric layer 103 and the micro-nanostructure 106 can further reduce the lateral size of the pixel. For example, the current 2.7-micron reflective SLM has essentially reached its limit. This decoupling approach of the present application prevents performance degradation due to smaller pixel sizes, thus enabling SLMs with smaller pixels without significant performance loss.

[0071] It should also be noted that in the embodiment of the present application, the upper surface of the conductive layer 101 may also be covered with a substrate (also referred to as a device cover), such as glass, for device packaging. As an example, FIG4 shows that the conductive layer 101 is also covered with a substrate 100. It should be noted that FIG4 is a substrate 100 added on the basis of FIG1, and FIG4 is for illustration only. In actual applications, the substrate 100 may also be added on the basis of FIG2 and FIG3, which will not be described in detail here.

[0072] 2. Phase Change Material Layer 102

[0073] Phase-change material layer 102, which may also be referred to as a phase-change layer, modulation layer, etc., is configured to reversibly transition between different phases. For example, the phase-change material layer may be a liquid crystal layer, which modulates the phase of an incident light beam through the birefringence of the liquid crystal molecules. The phase-change material layer may also be other electro-optical modulation materials, and this application does not specifically limit the type of phase-change material layer.

[0074] 3. First dielectric layer 103 including micro-nanostructure 106

[0075] The first dielectric layer 103 (refractive index n1) is a layer of medium that absorbs little or no modulated electromagnetic waves. Therefore, this application specifies that the absorption of the modulated electromagnetic waves by the first dielectric layer 103 is less than a first threshold value. The specific value of the first threshold value can be customized based on actual applications. Because the first dielectric layer 103 absorbs little or no modulated electromagnetic waves, it serves to isolate the pixel layer 104 from the phase change material layer 102.

[0076] It should be noted that in the embodiment of the present application, the first dielectric layer 103 also includes a micro-nano structure 106 (refractive index is n2). The micro-nano structure 106 is a dielectric layer or metal layer with a patterned structure. It will not absorb or absorbs very little modulated electromagnetic waves. It has a high refractive index. Therefore, the present application limits the refractive index of the micro-nano structure to be greater than the second threshold value. The specific value of the second threshold value can be customized based on actual applications.

[0077] In addition, in some embodiments of the present application, the first dielectric layer 103 and the micro-nanostructure 106 have a significant difference in optical properties during actual implementation: the refractive index difference between the first dielectric layer 103 and the micro-nanostructure 106 should be greater than 1 within the wavelength range of the electromagnetic wave to be modulated. For example, in the short-wave infrared band, the refractive index of the first dielectric layer 103 is 1.5, and the refractive index of the micro-nanostructure 106 is greater than 2.5. However, it should be noted that in some embodiments, the refractive index of the micro-nanostructure 106 can be greater than the refractive index of the first dielectric layer 103, for example, the refractive index of the micro-nanostructure 106 is 3.5 and the refractive index of the first dielectric layer 103 is 1.5.

[0078] It should also be noted that, in the embodiment of the present application, since the micro-nano structure 106 is disposed in the first dielectric layer 103, the position of the micro-nano structure 106 deployed in the first dielectric layer 103 may be slightly different in different application scenarios. For ease of understanding, the following example is provided to illustrate:

[0079] A. The micro-nano structures 106 are all located inside the first dielectric layer 103 .

[0080] In one possible embodiment, the micro-nanostructure 106 is entirely located within the first dielectric layer 103. For details, please refer to FIG5 , which is a schematic cross-sectional view of the first dielectric layer including the micro-nanostructure provided in the embodiment of the present application. Specifically, FIG5 corresponds to a schematic cross-sectional view of the micro-nanostructure 106 when it is a one-dimensional uniform periodic structure. In the embodiment of the present application, the distance between the upper surface of the micro-nanostructure 106 and the upper surface of the first dielectric layer 103 is a first distance t p The distance between the lower surface of the micro-nano structure 106 and the lower surface of the first dielectric layer 103 is the second distance t b The thickness h of the micro-nanostructure 106 (i.e., the distance between the upper and lower surfaces of the micro-nanostructure 106 ) must be less than one-half m (m ≥ 2) of the wavelength of the electromagnetic wave to be modulated, i.e., h < λ / m. For example, when m = 2, h < λ / 2. By limiting the size of the micro-nanostructure 106 to a subwavelength scale, diffraction effects are eliminated within the wavelength range of the electromagnetic wave to be modulated.

[0081] It should be noted that in the embodiments of the present application, in addition to having a sub-wavelength size, the micro-nano structure may also have a variety of structural types, including but not limited to:

[0082] a. The micro-nano structure 106 is composed of a one-dimensional uniform periodic structure.

[0083] In one possible implementation, the micro-nanostructure 106 may be composed of a one-dimensional uniform periodic structure. FIG5 shows a schematic cross-sectional structure of the micro-nanostructure 106, in which the micro-nanostructure 106 is entirely located within the first dielectric layer 103 and is a one-dimensional uniform periodic structure. Here, w is the line width of the micro-nanostructure material, a is the period of the uniform structure, and h is the thickness of the micro-nanostructure 106. The micro-nanostructure 106 is surrounded by a low-refractive-index medium (i.e., the first dielectric layer 106). The filling medium may include, but is not limited to, dielectric materials such as Al2O3, SiO2, polymethyl methacrylate (PMMA), SU-8, and polydimethylsiloxane (PDMS), as well as optical glue or other materials.

[0084] It should be noted that in some embodiments of the present application, the period a of the micro-nanostructure 106 must also be less than the wavelength λ of the electromagnetic wave to be modulated, that is, a<λ. This limitation is intended to improve the reflectivity of the micro-nanostructure 106 to the electromagnetic wave to be modulated, thereby decoupling the electromagnetic wave to be modulated from the underlying pixel layer 104 and allowing for greater design diversity in the pixel layer 104.

[0085] It should also be noted that, since the phase change material layer is a modulation layer that can be controlled by an excitation source, it requires a certain material quality. For example, the main axes of the anisotropic refractive indices of the liquid crystal need to have consistent directions. Such an orientation is determined by the quality of the contact interface between the phase change material layer and the dielectric layer below it. The unevenness of the contact interface will also affect the quality, and in turn affect the orientation of the liquid crystal. Therefore, if a micro-nano structure is added to the phase change material layer, the micro-nano structure will disturb the phase change material layer, causing uncertainty in orientation, thereby resulting in performance loss. Therefore, the way of adding micro-nano structures to the phase change material layer will limit the types of micro-nano structures that can be used, resulting in limited performance and functions that can be achieved. In this application, since the micro-nano structure is deployed in the first dielectric layer, the type of micro-nano structure can be unrestricted. For ease of understanding, the specific structure of the micro-nano structure 106 of the one-dimensional periodic structure is described below with several specific examples, including but not limited to:

[0086] (1) As an example, please refer to Figure 6. Figure 6 is a schematic diagram of a top view of the structure of the first dielectric layer containing a micro-nano structure provided in an embodiment of the present application. Specifically, Figure 6 corresponds to a schematic diagram of a top view of the structure when the micro-nano structure 106 is a one-dimensional uniform periodic structure. Figure 6 shows a specific structure of the formed micro-nano structure. Each small micro-nano structure has an image structure. Figure 6 shows an elliptical image structure with a structural period of a1 and a2. The line width of the micro-nano structure is w1 and w2. In the embodiment of the present application, a1 and a2 can be different or the same; similarly, w1 and w2 can be different or the same. This is specifically limited by the present application. Figure 6 shows the situation where a1≠a2 and w1≠w2. The purpose of this limitation is to be able to modulate the optical properties of the SLM in two different directions separately, which is a better modulation method.

[0087] (2) As another example, FIG7 shows the specific structure of another group of micro-nanostructures 106 that can be used. Similarly, each small micro-nanostructure has an imaged structure. FIG7 illustrates a triangular imaged structure with a structural period of a3 and a4, and a line width of the micro-nanostructure of w3 and w4. In the embodiment of the present application, a3 and a4 can be different or the same; similarly, w3 and w4 can be different or the same, and this application specifically defines this. FIG7 illustrates the case where a3≠a4 and w3≠w4. The purpose of this limitation is to be able to modulate the optical properties of the SLM in two different directions separately, which is a more optimal modulation method.

[0088] It should be noted that Figures 6 and 7 illustrate only two specific structures of the micro-nanostructure 106. In practical applications, the structure of the micro-nanostructure 106 can be customized based on actual needs. For example, it can be a rectangle as shown in Figure 8, a diamond as shown in Figure 9, or a combination of multiple different shapes as shown in Figure 10. This application does not limit this. Preferably, the micro-nanostructure 106 can have mirror symmetry in the a1 / a3 direction, while symmetry is not required in the other direction a2 / a4.

[0089] b. The micro-nano structure 106 is composed of a two-dimensional grid structure, and the grid structure is periodically distributed along each dimension.

[0090] In a possible implementation, the micro-nano structure 106 may also be composed of a two-dimensional grid structure. FIG11 shows a schematic diagram of a top view of the micro-nano structure 106 located entirely within the first dielectric layer 103 and the micro-nano structure 106 being a two-dimensional grid structure, wherein the periods along the two directions are a and b respectively. 01 and a 02 , the line widths of the micro-nanostructure materials are w 01 and w 02The thickness of the micro-nanostructure 106 is h (h is not shown because FIG. 11 is a top view). The micro-nanostructure 106 is surrounded by a low-refractive-index medium (i.e., the first dielectric layer 106). The filling medium may include, but is not limited to, dielectric materials such as Al2O3, SiO2, PMMA, SU-8, PDMS, and optical glue or materials.

[0091] Similarly, in some embodiments of the present application, the period a of the micro-nanostructure 106 along two directions is 01 and a 02 It also needs to be smaller than the wavelength λ of the electromagnetic wave to be modulated, that is, a 01 <λ and a 02 The purpose of this limitation is also to improve the reflection capability of the micro-nanostructure 106 to the electromagnetic wave to be modulated, to decouple the electromagnetic wave to be modulated from the underlying pixel layer 104, and to allow for greater diversity in the design of the pixel layer 104.

[0092] It should be noted that FIG11 is only a specific two-dimensional grid structure of the micro-nano structure 106. In practical applications, the type of the two-dimensional grid structure can be customized based on needs, and this application does not specifically limit this.

[0093] B. A portion of the micro-nano structure 106 is located inside the first dielectric layer 103, and the upper surface of the micro-nano structure 106 is higher than the upper surface of the first dielectric layer 103 by a first height t. n .

[0094] In another possible embodiment, a portion of the micro-nano structure 106 is located inside the first dielectric layer 103. The characteristic of this device structure is that it does not need to shield the upper phase change material layer 102, and is as close as possible without affecting the phase change material layer 102. Therefore, the micro-nano structure will have a certain contact with the upper layer (such as the phase change material layer 102 or the functional layer 107 described later). Please refer to Figures 12 and 13 for details. Figure 12 is another structural schematic diagram of the SLM provided in an embodiment of the present application, in which a portion of the micro-nano structure is located inside the first dielectric layer. Figure 12 shows the difference in the position of the micro-nano structure in the first dielectric layer relative to Figure 1. Figure 12 is merely a schematic diagram. In actual applications, the position of the micro-nano structure in the first dielectric layer can also be adjusted based on Figures 2 and 3. This will not be described in detail here. Figure 13 is another cross-sectional structural schematic diagram of the first dielectric layer containing the micro-nano structure provided in an embodiment of the present application. Specifically, Figure 13 corresponds to a structural cross-sectional schematic diagram when the micro-nano structure 106 is a one-dimensional uniform periodic structure scenario, wherein w is the line width of the micro-nano structure material, a is the period of the uniform structure, and h is the thickness of the micro-nano structure 106. In the embodiment of the present application, the upper surface of the micro-nano structure 106 is higher than the upper surface of the first dielectric layer 103 by a first height t nThe distance between the lower surface of the micro-nano structure 106 and the lower surface of the first dielectric layer 103 is the second distance t b Similarly, the thickness h of the micro-nano structure 106 should be less than one m (m≥2) of the wavelength of the electromagnetic wave to be modulated, that is, h<λ / m.

[0095] It should be noted that in the embodiments of the present application, in addition to the size of the micro-nano structure being on the subwavelength scale, its structural type can also be diverse, such as the one-dimensional periodic structure or the two-dimensional grid structure mentioned above. For details, please refer to the above description and will not be repeated here.

[0096] It should also be noted that, in the embodiment of the present application, the upper surface of the micro-nano structure 106 is higher than the upper surface of the first dielectric layer 103 by a first height t n It must be less than n (n≥2) times the thickness of the micro-nanostructure 106, that is, 0<t n <h / n, for example, when n=2, then 0<t n <h / 2. Thus, most of the micro-nanostructure 106 will be surrounded by the first dielectric layer 103, and the layers above the micro-nanostructure 106 (such as the phase-change material layer 102 or the functional layer 107 described later) will further fill the uneven areas caused by the micro-nanostructure 106 and the first dielectric layer 103, ultimately resulting in a uniform surface.

[0097] In summary, in the conventional SLM design, the pixel layer below needs to be separated from the phase change material layer by a non-reflective or low-reflective non-conductive material, which will result in the pixel layer being unable to efficiently reflect the electromagnetic waves to be modulated. In the embodiment of the present application, since a sub-wavelength-scale micro-nano structure 106 with a refractive index is deployed in the first dielectric layer 103, a nearly 100% reflection capability for electromagnetic waves can be achieved, and the spectrum that can be covered in the range of 1550nm is >100nm. Moreover, this layer of micro-nano structure 106 will not be affected or will be very little affected by the pixel layer 104 below, so the design of the pixel layer 104 below can also have more options. Fundamentally, the ability to reflect light is decoupled from the ability to individually control pixels.

[0098] 4. Pixel layer 104

[0099] Pixel layer 104 includes a plurality of pixels (as shown in FIG1 ), each of which is configured to independently control the optical properties of electromagnetic waves interacting with the pixel. For example, the pixel layer 104 can independently control the phase, amplitude, polarization, or other optical properties of the electromagnetic waves (e.g., light, microwaves, THz waves, etc.) interacting with the pixel. Pixel layer 104 can be made of metal or other conductive materials, such as ITO. This application does not impose any restrictions on the material type of the pixels, as long as the pixel can reflect the modulated electromagnetic waves.

[0100] It should be noted that, in the embodiment of the present application, the gaps between the pixels may be filled with the same medium as the first medium layer 103 (as shown in FIG. 1 to FIG. 4 ), or may be filled with other mediums, which is not limited in the present application.

[0101] 5. Circuit Control Layer 105

[0102] The circuit control layer 105, which may also be referred to as a bottom circuit control layer, a control system, etc., is used to independently control each pixel. That is, the circuit control layer 105 can independently control one or more pixels. In the embodiment of the present application, the circuit control layer 105 and the electrode layer 1001 act as a pair of electrodes to apply electrical signals to the SLM. The circuit control layer 105 can be a complementary metal oxide semiconductor (CMOS) or a thin film field effect transistor (TFT), which is not limited in this application.

[0103] It should be noted that in some embodiments of the present application, the SLM may further include a functional layer 107. The functional layer 107 may be located on the upper surface and / or lower surface of the phase change material layer 102 to regulate the orientation of the phase change material layer 102. In a liquid crystal device, the functional layer 108 may be a photo-alignment layer, an organic alignment layer, or an inorganic alignment layer. Specifically, please refer to FIG14 , which is another structural schematic diagram of the SLM provided in an embodiment of the present application, wherein the (a) sub-schematic diagram in FIG14 is a structural schematic diagram in which the functional layer is located on the upper surface of the phase change material layer 102, the (b) sub-schematic diagram in FIG14 is a structural schematic diagram in which the functional layer is located on the lower surface of the phase change material layer 102, and the (c) sub-schematic diagram in FIG14 is a structural schematic diagram in which the functional layer is located on both the upper and lower surfaces of the phase change material layer 102. It should be noted that FIG14 is a functional layer 107 added on the basis of FIG1 . FIG14 is for illustrative purposes only. In actual applications, the functional layer 107 may also be added on the basis of FIG2 , FIG3 , FIG4 , and FIG12 . This will not be described in detail here. As an example, if the phase change material layer 102 is a liquid crystal layer, the functional layer 107 can play an orientation role and can be a light orientation layer, such as SD1, which can help the liquid crystal layer to produce a corresponding direction of light orientation through polarized light; this functional layer 107 can also be an inorganic transparent material with extremely small micro-grooves, a texture, or a cross-linked polymer, or a PI material that can guide the liquid crystal layer to produce an orientation after friction. This application specifically defines this. In addition, if the upper and lower surfaces of the phase change material layer 102 have a functional layer 108 (i.e., the schematic diagram (c) in Figure 14), the orientation direction of the functional layer 108 on the upper surface and the orientation direction of the functional layer 108 on the lower surface can be the same or different. Whether the orientation is the same depends on the specific application scenario, and this application does not limit this.

[0104] It should be noted that in the embodiment of the present application, if there is a situation where the functional layer 107 is located on the lower surface of the phase change material layer 102 (i.e., sub-schematic diagrams (b) and (c) in Figure 14), the first dielectric layer 103 containing the micro-nano structure 106 and the upper surface of the functional layer 107 located below the phase change material layer 102 are on the same flat surface, and the flatness of its surface (if there is a functional layer 107, it refers to the flatness of the functional layer 107; if there is no functional layer 107, it refers to the phase change material layer 102) needs to be less than λ / x, where x can be customized, for example, x=20.

[0105] It should also be noted that, in the embodiment of the present application, if the functional layer 107 is located on the lower surface of the phase change material layer 102 and the micro-nano structure 106 is entirely located inside the first dielectric layer 103 (as shown in the schematic diagrams (b) and (c) of FIG14 ), then the corresponding distances will be retained between the upper and lower surfaces of the micro-nano structure 106 and the pixel layer 104 and the functional layer 107. Assuming that the thickness of the functional layer is t 107 (i.e., the distance between the upper surface of the functional layer 107 and the lower surface of the functional layer 107), the first distance between the upper surface of the micro-nano structure 106 and the upper surface of the first dielectric layer 103 is t p , then (t 107 +t p )>λ / q. The purpose of this limitation is to shield the upper phase change material layer 102 from affecting the functions of the lower first dielectric layer 103 and the micro-nano structure 106 when being modulated. Wherein, λ is the wavelength of the electromagnetic wave to be modulated. For example, when q=10, (t 107 +t p )>λ / 10.

[0106] It should also be noted that in other embodiments of the present application, if the functional layer 107 is located on the upper surface of the phase change material layer 102 (as shown in the schematic diagrams (a) and (c) of Figure 14), the SLM may further include a second dielectric layer 108. The second dielectric layer 108 also contains micro-nano structures similar to those of the first dielectric layer 103. The relationship between the second dielectric layer 108 and the micro-nano structures contained therein can be referred to the relationship between the first dielectric layer 103 and the micro-nano structures contained therein, and will not be described in detail here. For details, please refer to Figure 15. The second dielectric layer 108 is located between the functional layer 107 and the conductive layer 101 to isolate the functional layer 107 and the conductive layer 101, with the purpose of increasing the amplitude and / or phase of the modulated electromagnetic wave. It should also be noted that FIG15 shows a second dielectric layer 108 added on the basis of the sub-schematic diagram (c) in FIG14 . FIG15 is for illustration only. In actual applications, the second dielectric layer 108 may be added on the basis of the sub-schematic diagram (a) in FIG14 , or the functional layer 107 and the second dielectric layer 108 may be added on the upper surface of the phase change material layer 102 on the basis of FIG2 , FIG3 , FIG4 , and FIG12 . Details will not be given here.

[0107] In summary, in the embodiments of the present application, the combination of the first dielectric layer 103 containing the micro-nanostructure 106 and the functional layer 107 prevents the properties of the upper phase-change material layer from being altered by changes in the underlying micro-nanostructure structure. For example, the surface topology generated by the liquid crystal and the micro-nanostructure itself can affect the orientation and distribution of the surface liquid crystal molecules, requiring targeted optimization. However, in the present application, if the micro-nanostructure 106 is partially or fully buried, this effect is eliminated. This allows the micro-nanostructure array and its distribution, as described in Figures 6-11, to achieve specialized functions and effects.

[0108] In the application scenarios of the present application, the high-performance phase-type SLM can improve performance after the improvement of the present application. It can be used as a graphic generator in the display to improve the display quality and refresh speed. It can also be used in other scenarios that are sensitive to insertion loss and where increased modulation speed can bring benefits, such as in switching engines used for optical switching in optical communications. In addition, the most critical scenario corresponding to the present application is the optical switching scenario on the backbone optical network, and the core component of the optical switching in the backbone network is WSS. Through analysis, the improved high-performance phase-type SLM can greatly reduce insertion loss and increase switching speed, providing an important input for future large-port optical scheduling. Moreover, further improvements can also expand new application scenarios.

[0109] The above is only a specific implementation method of the present application, but the protection scope of the present application is not limited thereto. Any technician familiar with this technical field can easily think of changes or replacements within the technical scope disclosed in this application, which should be covered by the protection scope of the present application.

Claims

1. A spatial light modulator, characterized in that: The first dielectric layer includes a conductive layer, a phase change material layer, a first dielectric layer, a pixel layer, and a circuit control layer in sequence along the first direction, wherein the first dielectric layer includes a micro-nano structure, wherein: The conductive layer is used to modulate the phase or amplitude of the electromagnetic wave to be modulated; The phase change material layer is used to perform a reversible transition between different phases; The absorption amount of the first dielectric layer to the electromagnetic wave to be modulated is less than a first threshold value, and is used to isolate the pixel layer from the phase change material layer; the refractive index of the micro-nano structure is greater than a second threshold value, and is used to reflect the electromagnetic wave to be modulated; The pixel layer includes a plurality of pixels, each of the pixels being used to independently control the optical properties of the electromagnetic wave interacting with the pixel; The circuit control layer is used to independently control each of the pixels.

2. The spatial light modulator according to claim 1, characterized in that The micro-nano structure contained in the first dielectric layer includes: The micro-nano structures are all located inside the first dielectric layer.

3. The spatial light modulator according to claim 1, characterized in that The micro-nano structure contained in the first dielectric layer includes: A portion of the micro-nano structure is located inside the first dielectric layer, and an upper surface of the micro-nano structure is higher than an upper surface of the first dielectric layer by a first height.

4. The spatial light modulator according to claim 3, characterized in that The first height is less than one nth of the thickness of the micro-nano structure, where n≥2, wherein the thickness of the micro-nano structure is the distance between the upper surface of the micro-nano structure and the lower surface of the micro-nano structure.

5. The spatial light modulator according to any one of claims 1 to 4, characterized in that: The thickness of the micro-nano structure is less than one m of the wavelength of the electromagnetic wave to be modulated, m≥2, wherein the thickness of the micro-nano structure is the distance between the upper surface of the micro-nano structure and the lower surface of the micro-nano structure.

6. The spatial light modulator according to any one of claims 1 to 5, characterized in that: The difference between the refractive index of the first medium layer and the refractive index of the micro-nano structure is greater than 1.

7. The spatial light modulator according to any one of claims 1 to 6, characterized in that: The size of the micro-nano structure is of sub-wavelength scale, and the micro-nano structure includes at least any one of the following: A one-dimensional periodic structure and a two-dimensional grid structure, wherein the grid structure is periodically distributed along each dimension.

8. The spatial light modulator according to claim 7, characterized in that The micro-nano structure is the one-dimensional periodic structure, and the period of the periodic structure is smaller than the wavelength of the electromagnetic wave to be modulated.

9. The spatial light modulator according to claim 7, characterized in that: The micro-nano structure is the two-dimensional grid structure, and the period of the grid structure along each dimension is smaller than the wavelength of the electromagnetic wave to be modulated.

10. The spatial light modulator according to any one of claims 1 to 9, characterized in that: The conductive layer includes an electrode layer, and the electrode layer is used to cooperate with the circuit control layer to apply an electrical signal to the spatial light modulator to achieve modulation of the phase or amplitude of the electromagnetic wave to be modulated.

11. The spatial light modulator according to claim 10, characterized in that A dielectric reflection layer is also included on the upper surface of the electrode layer. The dielectric reflection layer includes k layers of dielectric films for modulating the phase or amplitude of the electromagnetic wave to be modulated, where k≥1.

12. The spatial light modulator according to claim 11, characterized in that The thickness of each dielectric film in the k dielectric films is smaller than the wavelength of the electromagnetic wave to be modulated.

13. The spatial light modulator according to any one of claims 11 to 12, characterized in that: When k≥2, the refractive index values ​​of adjacent dielectric films in the k-layer dielectric films are different.

14. The spatial light modulator according to any one of claims 1 to 13, characterized in that: The spatial light modulator further comprises: a functional layer; The functional layer is located on the upper surface and / or the lower surface of the phase change material layer, and is used to adjust the orientation of the phase change material layer.

15. The spatial light modulator according to claim 14, characterized in that When the functional layer is located on the lower surface of the phase change material layer and the micro-nano structure is entirely located inside the first dielectric layer, the sum of the thickness of the functional layer and the first distance of the micro-nano structure is greater than one qth of the electromagnetic wave to be modulated, the functional layer is located on the lower surface of the phase change material layer and the micro-nano structure is entirely located inside the first dielectric layer. The thickness of the energy layer is the distance between the upper surface of the functional layer and the lower surface of the functional layer, the first distance is the distance between the upper surface of the micro-nano structure and the upper surface of the first dielectric layer, and q≥10.

16. The spatial light modulator according to claim 14, characterized in that When the functional layer is located on the upper surface of the phase change material layer, the spatial light modulator further includes a second dielectric layer, wherein the micro-nano structure is contained in the second dielectric layer; The second dielectric layer is located between the functional layer and the conductive layer, and is used to isolate the functional layer from the conductive layer.

17. The spatial light modulator according to any one of claims 1 to 16, characterized in that: The phase change material layer comprises: Liquid crystal layer.

18. The spatial light modulator according to any one of claims 1 to 17, characterized in that: A substrate is also included on the upper surface of the conductive layer, and the substrate is used to package the spatial light modulator.

Citation Information

Patent Citations

  • Spatial light modulator

    CN118689012A

  • Device and arrangement for controlling an electromagnetic wave, methods of forming and operating the same

    CN108885365A

  • High-diffraction-efficiency phase-type spatial light modulator

    CN110865475A

  • Pure phase spatial light modulator based on metasurface structure anchoring

    CN114791686A

  • Spectrum establishment method and device

    CN115060364A