Nitride semiconductor device
The introduction of an n-type impurity-doped second nitride semiconductor layer between the gate and drain layers in the nitride semiconductor device addresses the issue of high gate leakage current and on-resistance by optimizing electric field distribution and two-dimensional electron gas concentration, resulting in improved performance.
Patent Information
- Application Number
- PCT/JP2024/006385
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-27
- Filing Date
- 2024-02-21
- Publication Date
- 2024-10-03
AI Technical Summary
The existing nitride semiconductor device structure does not adequately relax the electric field between the gate and drain, leading to high gate leakage current and increased on-resistance due to the absence of an n-type nitride semiconductor layer at the gate-side end of the p-type nitride semiconductor layer on the drain side.
Incorporating a second nitride semiconductor layer with a larger band gap than the first nitride semiconductor layer, selectively doped with n-type impurities, positioned between the gate and drain layers, with the end of the n-type impurity-doped region located between the gate and drain layers to reduce electric field strength and enhance two-dimensional electron gas concentration.
This configuration reduces gate leakage current, decreases on-resistance, and increases maximum drain current by optimizing the electric field distribution and two-dimensional electron gas concentration.
Smart Images

Figure JP2024006385_03102024_PF_FP_ABST
Abstract
Description
nitride semiconductor devices
[0001] The present disclosure relates to the structure of a semiconductor device, and more particularly to a device using a semiconductor, particularly a Group III nitride semiconductor, that can be used as a field effect transistor or the like.
[0002] Group III nitride semiconductors have a high breakdown voltage due to their wide band gap. Furthermore, heterostructures such as AlGaN / GaN can be easily formed. The difference in band gap and the piezoelectric charge generated by the difference in lattice constants between AlGaN and GaN can generate a high-mobility, high-concentration electron channel (two-dimensional electron gas) on the GaN layer side of the AlGaN / GaN interface. Controlling this two-dimensional electron gas makes it possible to form a high electron mobility transistor (HEMT). Due to these characteristics of high breakdown voltage, high speed, and large current, Group III nitride semiconductors are being applied to electronic devices such as power field-effect transistors (FETs) and diodes.
[0003] 1 of Patent Document 1, an n-type nitride semiconductor layer is formed between a p-type nitride semiconductor layer on the drain side and a first nitride semiconductor layer. According to Patent Document 1, the formation of the n-type nitride semiconductor layer below the p-type nitride semiconductor layer makes it possible to suppress the expansion of the depletion layer in the p-type nitride semiconductor layer and to suppress a decrease in the concentration of two-dimensional electron gas, thereby suppressing current collapse and reducing the on-resistance of the field-effect transistor even when the drain voltage is low.
[0004] Japanese Patent No. 5903642
[0005] However, in the structure described in Patent Document 1, an n-type nitride semiconductor layer is not formed at the gate-side end of the p-type nitride semiconductor layer on the drain side, where the electric field strength is high. As a result, the electric field relaxation between the gate and drain is insufficient, and there is still room for reduction in gate leakage current.
[0006] Therefore, a nitride semiconductor device according to one aspect of the present disclosure includes a substrate, a first nitride semiconductor layer provided on the substrate, a second nitride semiconductor layer in contact with the first nitride semiconductor layer and having a larger band gap than the first nitride semiconductor layer, a gate layer made of a p-type nitride semiconductor selectively formed on the second nitride semiconductor layer, a drain layer made of a p-type nitride semiconductor provided spaced apart from the gate layer, and a drain electrode electrically connected to both the second nitride semiconductor layer and the drain layer, wherein the second nitride semiconductor layer has a region selectively doped with n-type impurities, and the gate layer side end of the n-type impurity doped region is between the gate layer and the drain layer.
[0007] The semiconductor device according to the present disclosure can increase the drain current, reduce the on-resistance, and reduce the gate leakage current.
[0008]
[0009] Hereinafter, nitride semiconductor devices according to embodiments will be described in detail with reference to the drawings. Note that each of the embodiments described below represents a specific example of the present disclosure. The numerical values, shapes, materials, components, component placement positions, and connection forms shown in the following embodiments are merely examples and are not intended to limit the present disclosure. Furthermore, among the components in the following embodiments, components not recited in independent claims will be described as optional components.
[0010] Furthermore, each figure is a schematic diagram and is not necessarily an exact illustration. Therefore, for example, the scales of the figures do not necessarily match. Furthermore, in each figure, substantially the same components are given the same reference numerals, and redundant explanations are omitted or simplified.
[0011] Furthermore, in this specification, terms indicating the relationship between elements, terms indicating the shape of elements, and numerical ranges are not expressions that only express a strict meaning, but are expressions that also include a substantially equivalent range, for example, a difference of about a few percent.
[0012] Furthermore, in this specification, the terms "above" and "below" do not refer to the upward direction (vertically upward) and downward direction (vertically downward) in absolute spatial recognition, but are used as terms defined by a relative positional relationship based on the stacking order in a stacked configuration. Furthermore, the terms "above" and "below" are applied not only to a case where two components are arranged with a gap between them and another component exists between the two components, but also to a case where two components are arranged closely together and the two components are in contact with each other.
[0013] Furthermore, in this specification, ordinal numbers such as "first" and "second" do not refer to the number or order of components unless otherwise specified, but are used for the purpose of avoiding confusion and distinguishing between components of the same type.
[0014] FIG. 1 shows a cross-sectional structure of a nitride semiconductor device according to an embodiment, in which the gate-side end of an n-type impurity-doped region is located between a gate layer and a drain layer.
[0015] The nitride semiconductor device shown in FIG. 1 has an appropriate buffer layer 2 (e.g., a single layer or multiple layers of a Group III nitride semiconductor such as GaN, AlGaN, AlN, InGaN, InN, or AlInGaN) provided on an appropriate Si substrate 1 (otherwise, for example, a substrate of Sapphire, SiC, GaN, or AlN). The nitride semiconductor device has a first nitride semiconductor layer 3 made of GaN (otherwise, for example, a Group III nitride semiconductor such as InGaN, InN, AlGaN, or AlInGaN) provided on the buffer layer 2. The nitride semiconductor device has a second nitride semiconductor layer 4 made of AlGaN (otherwise, for example, a single layer or multiple layers of a Group III nitride semiconductor such as GaN, InGaN, AlGaN, AlN, or AlInGaN) provided on the first nitride semiconductor layer 3. The second nitride semiconductor layer 4 has a larger band gap than the first nitride semiconductor layer 3, and the two layers are in direct contact with each other. If the second nitride semiconductor layer 4 is made of AlGaN and the first nitride semiconductor layer 3 is made of GaN, a high concentration of two-dimensional electron gas 5 is generated on the first nitride semiconductor layer 3 (channel layer) side near the interface between the second nitride semiconductor layer 4 and the first nitride semiconductor layer 3 due to the piezoelectric charges generated by the difference in lattice constant between AlGaN and GaN and the difference in band gap.
[0016] On the second nitride semiconductor layer 4, selectively formed gate layer 6 (also, for example, Group III nitride semiconductors such as p-InGaN, p-InN, p-AlGaN, p-AlInGaN, etc.) and drain layer 7 (also, for example, Group III nitride semiconductors such as p-InGaN, p-InN, p-AlGaN, p-AlInGaN, etc.) made of p-GaN containing p-type impurities (Mg, Zn, C, etc.) are spaced apart from each other. The concentration of p-type impurities in the gate layer 6 and the drain layer 7 is 1E19 cm -3 Above, if possible, 5E19cm -3 The above is desirable. In addition, when performing normally-off operation, which will be explained later in the operation of this structure, a gate recess 15 may be provided in the second nitride semiconductor layer 4 directly below the gate layer 6, as shown in FIG. 16. Here, "Ek (k is an integer)" represents a power of 10. That is, Ek is 10 kFor example, 1E19 means 1 x 10 19 5E19 is 5 x 10 19 This also applies to FIG. 17 described below.
[0017] Note that a single or multiple nitride semiconductor layers may be present on the second nitride semiconductor layer 4, as shown by the third nitride semiconductor layer 17 in FIG. 16 . The nitride semiconductor layer on the second nitride semiconductor layer 4 has a larger band gap than the first nitride semiconductor layer 3 and is in direct contact with the second nitride semiconductor layer 4. Furthermore, it is desirable that two-dimensional electron gas and two-dimensional hole gas are not formed at the interface between the nitride semiconductor layer and the second nitride semiconductor layer 4 directly below the nitride semiconductor layer, since these gases could cause gate leakage when a field-effect transistor is formed. Therefore, it is desirable that the band gap of this nitride semiconductor layer is equal to or slightly smaller than the band gap of the second nitride semiconductor layer 4. Furthermore, when the nitride semiconductor layer is made of, for example, AlGaN, having a band gap slightly smaller than that of the second nitride semiconductor layer 4 reduces the Al composition, thereby improving crystallinity.
[0018] The second nitride semiconductor layer 4 has a region 8 selectively doped with n-type impurities. The n-type impurity doped region 8 is doped with Si (or Ge, etc.) as an n-type impurity by ion implantation or the like.
[0019] The n-type impurity implanted into the n-type impurity-doped region 8 has two purposes: to obtain a low-resistance n-type nitride semiconductor layer and to reduce the electric field strength between the gate layer 6 and the drain layer 7. Therefore, the ion implantation concentration must be carefully set. Specifically, the n-type impurity concentration in the region 8 must be at least 1E18 cm -3 Above, preferably 3E18cm -3 The n-type impurity concentration in region 8 is preferably 1E21 cm 3 or more so that the ion-implanted crystal does not become a completely amorphous structure due to ion implantation damage. -3 The n-type impurity-doped region 8 is defined as a region where the concentration of n-type impurities is 1E17 cm -3 It is defined as a region having more than this.
[0020] On the second nitride semiconductor layer 4, a source electrode 10 is located on the opposite side of the gate layer 6 from the drain layer 7, spaced apart from the gate layer 6, and a drain electrode 11 is located on the drain layer 7 side, with the gate layer 6 sandwiched between them. The drain electrode 11 may be in direct contact with the drain layer 7 as shown in FIG. 1 , or may be spaced apart from the drain layer 7 (not shown). The source electrode 10 and the drain electrode 11 are made of one or a combination of two or more metals such as Ti, Al, Mo, and Hf, which are in ohmic contact with the nitride semiconductor layer, and are electrically connected to the two-dimensional electron gas 5. The drain electrode 11 is also electrically connected to the drain layer 7.
[0021] A gate electrode 9 is provided on the gate layer 6. The gate electrode 9 may be an electrode made of one or a combination of two or more metals such as Ti, Ni, Pd, Pt, Au, W, WSi, Ta, TiN, Al, Mo, Hf, and Zr. The gate electrode 9 may be in ohmic contact or Schottky contact with the gate layer 6. Because ohmic contact increases the reliability of the gate electrode, it is desirable to use an electrode made of one or a combination of two or more metals with low contact resistance such as Ni, Pt, Pd, Au, Ti, Cr, In, Sn, and Al.
[0022] The structure shown in FIG. 1 (and FIG. 16) is characterized in that the end of the n-type impurity doped region 8 on the gate layer 6 side is located between the gate layer 6 and the drain layer 7.
[0023] The operation of this structure will be described when a gate recess 15 (Figure 16) is included. When no voltage is applied to the electrodes, the gate layer 6 is a p-type nitride semiconductor layer. Because of the gate recess 15 structure, the gate layer 6 is physically close to the two-dimensional electron gas 5, causing the p-n junction to deplete the two-dimensional electron gas 5 directly below the gate layer 6 (off state). In this state, even if a positive voltage is applied to the drain electrode 11 and the source electrode 10 is grounded, no current flows between the drain electrode 11 and the source electrode 10. Next, when a positive voltage is applied to the gate layer 6, the p-n junction is pulled toward the gate electrode 9, the depletion layer becomes smaller, and two-dimensional electron gas 5 is generated directly below the gate layer 6 (on state). In this state, when a positive voltage is applied to the drain electrode 11 and the source electrode 10 is grounded, current flows between the drain electrode 11 and the source electrode 10.
[0024] Although a depletion layer due to the pn junction also exists directly below the drain layer 7, the two-dimensional electron gas 5 cannot be completely depleted because there is no gate recess 15 directly below the drain layer 7, resulting in a low carrier concentration. Therefore, in the on state, a current flows between the drain electrode 11 and the source electrode 10.
[0025] The effects of this structure will now be described. This structure is characterized in that the gate-side end of the n-type impurity-doped region 8 is located between the gate layer 6 and the drain layer 7. This changes the electric field strength at the gate-side end of the drain layer 7, making it possible to lower the maximum electric field strength between the gate and drain, and thus reduce gate leakage current. In addition, the concentration of the two-dimensional electron gas 5 directly below the n-type impurity-doped region 8 between the gate and drain is increased, reducing sheet resistance, which in turn makes it possible to reduce on-resistance and increase the maximum drain current.
[0026] Modifications of the embodiments will be described below. One or more of the modifications described below can be combined as appropriate, as long as no contradictions arise between them. That is, an embodiment realized by combining the following modifications is also realized as one embodiment of the nitride semiconductor device of the present disclosure.
[0027] 2 shows a cross-sectional structure of a nitride semiconductor device according to a first modification of the embodiment, in which the end of the n-type impurity-doped region 8 opposite to the gate layer side is located between the gate layer and the drain layer. In Fig. 2, the end of the n-type impurity-doped region 8 on the drain layer 7 side is located between the gate layer 6 and the drain layer 7, separated from the drain layer 7.
[0028] By using this modified example, in addition to the effects of the embodiment, the electric field strength at the end of the drain layer 7 on the gate layer 6 side can be further changed, the maximum electric field strength between the gate and drain can be lowered, and the gate leakage current can be reduced.
[0029] 3 shows a cross-sectional structure of a nitride semiconductor device according to a second modification of the embodiment, in which an n-type impurity doped region 8 is located closer to the drain layer than a midline 12 between the gate layer and the drain layer. In FIG. 3, n-type impurity doped region 8 is located closer to the drain layer 7 than a midline 12 between the drain layer 7 and the gate layer 6.
[0030] By using this modification, in addition to the effects of the embodiment and the first modification, a high breakdown voltage can be ensured by physically increasing the distance by which the depletion layer of the gate layer 6 extends toward the drain layer 7 due to a high electric field and reaches the region 8 doped with n-type impurities.
[0031] 4 shows a cross-sectional structure of a nitride semiconductor device according to a third modification of the embodiment, in which an n-type impurity-doped region 8 contacts an end of the drain layer 7 on the gate layer 6 side.
[0032] By using this modification, in addition to the effects of the embodiment and the first and second modifications, the electric field strength at the end of the drain layer 7 on the gate layer 6 side can be directly changed, thereby lowering the maximum electric field strength between the gate and drain, and reducing the gate leakage current.
[0033] 1 to 4 show cross-sectional structural views of a nitride semiconductor device according to a fourth modification of the embodiment, in which an n-type impurity-doped region is located on the outermost surface of the second nitride semiconductor layer. In FIGS. 1 to 4, n-type impurity-doped region 8 is located on the outermost surface of the second nitride semiconductor layer 4. In another modification, as shown in FIG. 5, n-type impurity-doped region 8 may be located in a region away from the outermost surface of the second nitride semiconductor layer 4.
[0034] By using this modification, in addition to the effects of the embodiment and the first to third modifications, the electric field strength at the gate side end of the drain layer 7 where the electric field is concentrated can be changed more directly, thereby lowering the maximum electric field strength between the gate and the drain, and reducing the gate leakage current.
[0035] 6 shows a cross-sectional structure of a nitride semiconductor device according to a fifth modification of the embodiment, in which an n-type impurity doped region 8 extends continuously below the drain layer. In this example, the end of n-type impurity doped region 8 on the gate layer 6 side is located between the gate layer 6 and the drain layer 7, and the end on the drain layer 7 side is continuous below the drain layer 7.
[0036] By using this modification, in addition to the effects of the embodiment and the second to fourth modifications, the n-type impurity doped region 8 reaches below the drain layer 7, thereby suppressing the expansion of the depletion layer directly below the drain layer 7 and suppressing a decrease in the concentration of the two-dimensional electron gas 5. This reduces the sheet resistance directly below the drain layer 7, and as a result, it becomes possible to further reduce the on-resistance and increase the maximum drain current.
[0037] 7 shows a cross-sectional structure of a nitride semiconductor device according to a sixth modification of the embodiment, in which an n-type impurity doped region 8 is also located below the drain electrode 11, in addition to being located between the gate layer 6 and the drain layer 7.
[0038] By using this modification, in addition to the effects of the embodiment and the first to fifth modifications, the n-type impurity doped region 8 is located directly below the drain electrode 11, so that the contact resistance between the drain electrode 11 and the second nitride semiconductor layer 4 having the n-type impurity doped region 8 can be reduced, and as a result, the on-resistance can be further reduced and the maximum drain current can be increased.
[0039] 8 shows a cross-sectional structure of a nitride semiconductor device according to a seventh modification of the embodiment, in which an n-type impurity doped region 8 is continuous from below the drain layer to below the drain electrode. In Fig. 8, the end of n-type impurity doped region 8 on the side of gate layer 6 is located between gate layer 6 and drain layer 7, and the end on the side of drain layer 7 is continuous from directly below drain layer 7 to directly below drain electrode 11.
[0040] By using this modification, in addition to the effects of the embodiment and the second to sixth modifications, the n-type impurity doped region 8 is continuously present under the drain layer 7 and under the drain electrode 11, so that the n-type layer directly under the drain layer 7 pushes the p-n junction upward and increases the number of electrons supplied to the two-dimensional electron gas 5, thereby increasing the concentration of the two-dimensional electron gas 5 directly under the drain layer 7. Furthermore, the contact resistance between the drain electrode 11 and the second nitride semiconductor layer 4 having the n-type impurity doped region 8 can be reduced. As a result, it is possible to further reduce the on-resistance and increase the maximum drain current.
[0041] 9 shows a cross-sectional structure of a nitride semiconductor device according to an eighth modification of the embodiment, in which an n-type impurity doped region is also present in the drain layer. In Fig. 9, an n-type impurity doped region 8 is also present in the drain layer 7. In Fig. 9, the n-type impurity doped region 8 in the drain layer 7 is indicated by a hatching pattern consisting of overlapping diagonal lines and dots. The same is true in Fig. 10.
[0042] By using this modification, in addition to the effects of the embodiment and the first to seventh modifications, the n-type impurity-doped region 8 is also present in the drain layer 7, so that the n-type layer in the drain layer 7 pushes the p-n junction further upward, thereby increasing the concentration of the two-dimensional electron gas 5 immediately below the drain layer 7. This makes it possible to further reduce the on-resistance and increase the maximum drain current.
[0043] 10 shows a cross-sectional structure of a nitride semiconductor device according to a ninth modification of the embodiment, in which an n-type impurity-doped region 8 is also present in the surface of the drain layer 7. In FIG.
[0044] By using this modification, in addition to the effects of the embodiment and the first to eighth modifications, the presence of n-type impurity doped region 8 on the surface of drain layer 7 relatively reduces the p-type region of drain layer 7, pushing the p-n junction upward and increasing the concentration of two-dimensional electron gas 5 directly below drain layer 7. This makes it possible to further reduce the on-resistance and increase the maximum drain current.
[0045] 11 shows a cross-sectional structure of a nitride semiconductor device according to a tenth modification of the embodiment, in which an n-type impurity-doped region 8 reaches the first nitride semiconductor layer 3 in the depth direction.
[0046] By using this modification, in addition to the effects of the embodiment and the first to ninth modifications, the n-type impurity doped region 8 reaches the first nitride semiconductor layer 3 in the depth direction, thereby directly increasing the number of electrons supplied to the two-dimensional electron gas 5, thereby further reducing the on-resistance and increasing the maximum drain current.
[0047] 12 shows a cross-sectional structure of a nitride semiconductor device according to an eleventh modification of the embodiment, in which the n-type impurity doped region comprises a damaged region 13 at the center of the n-type impurity doped region and a diffusion region 14 around the damaged region, and the n-type impurity concentration of the diffusion region is lower than that of the damaged region. In FIG. 12, the n-type impurity doped region comprises a damaged region 13 and a diffusion region 14 around the damaged region.
[0048] By using this modification, in addition to the effects of the embodiment and the first to tenth modifications, a higher activation rate of n-type impurities can be obtained and more efficient conversion to n-type can be achieved because no crystal damage caused by ion implantation or the like occurs in the diffusion region 14. This makes it possible to more efficiently increase the number of electrons supplied to the two-dimensional electron gas 5, further reducing the on-resistance and increasing the maximum drain current.
[0049] 13 and 14 show cross-sectional structural views of a nitride semiconductor device according to a twelfth modification of the embodiment, in which the n-type impurity-doped region comprises a damaged region in the center of the n-type impurity-doped region and a surrounding diffusion region, with the diffusion region located below the drain layer. In each of FIGS. 13 and 14, the n-type impurity-doped region comprises a damaged region 13 and a surrounding diffusion region 14. In FIG. 13, the diffusion region 14 is located below the drain layer 7. In FIG. 14 (similar to FIG. 12), the diffusion region 14 is located below the drain layer 7, but the damage region 13 is not located below the drain layer 7. In FIG. 14, the damage region 13 is located on the outermost surface of the second nitride semiconductor layer 4.
[0050] By using this modification, in addition to the effects of the embodiment and the first to eleventh modifications, since the diffusion region 14 is free from crystal damage caused by ion implantation or the like, traps caused by crystal defects at the end of the drain layer 7 on the gate layer 6 side, to which a high electric field is applied, can be suppressed, and the so-called current collapse phenomenon, in which the drain current decreases at high voltage, can be suppressed.
[0051] 15 shows a cross-sectional structure of a nitride semiconductor device according to a thirteenth modification of the embodiment, in which the n-type impurity-doped region comprises a damaged region in the center of the n-type impurity-doped region and a surrounding diffusion region, and the damaged region is located below the drain layer. In Fig. 15, the n-type impurity-doped region comprises a damaged region 13 and a surrounding diffusion region 14, and the damaged region 13 is located below the drain layer 7. In Fig. 15, the damaged region 13 is located on the outermost surface of the second nitride semiconductor layer 4.
[0052] By using this modification, in addition to the effects of the embodiment and the first to twelfth modifications, the damage region 13 has a higher concentration of n-type impurities than the diffusion region 14. This allows the n-type layer directly below the drain layer 7 to more efficiently push the p-n junction upward and increase the electrons supplied to the two-dimensional electron gas 5, thereby increasing the concentration of the two-dimensional electron gas 5 directly below the drain layer 7, reducing the on-resistance and enabling an increase in the maximum drain current.
[0053] (Fourteenth Modification) Next, a nitride semiconductor device according to a fourteenth modification of the embodiment will be described, in which the n-type impurity-doped region extends from the end of the drain layer on the gate layer side to a range of 1 μm or less toward the gate layer. In this modification, the n-type impurity-doped region 8 extends from the end of the drain layer 7 on the gate layer 6 side to a range of 1 μm or less toward the gate layer 6 (see, for example, FIG. 1 ).
[0054] By using this modification, in addition to the effects of the embodiment and the first to thirteenth modifications, a high gate-drain breakdown voltage can be achieved by locating the end of the n-type impurity-doped region 8 on the gate layer 6 side away from the gate layer 6. Conversely, if the end of the n-type impurity-doped region 8 on the gate layer 6 side is close to the gate layer 6, a sufficient breakdown voltage cannot be ensured.
[0055] (Fifteenth Modification) Next, a nitride semiconductor device according to a fifteenth modification of the embodiment will be described, in which the end of the n-type impurity-doped region opposite the gate side is within a range of 1 μm from the gate-side end of the drain layer toward the gate layer. In this modification, the end of the n-type impurity-doped region 8 opposite the gate layer 6 is within a range of 1 μm toward the gate layer 6 from the end of the drain layer 7 on the gate layer 6 side (see, for example, FIG. 2 ).
[0056] By using this modification, in addition to the effects of the embodiment and the first to fourteenth modifications, the n-type impurity doped region 8 is closer to the drain layer 7, so that the electric field at the end of the drain layer 7 on the gate layer 6 side and the electric field at the end of the gate layer 6 on the drain layer 7 side can be more effectively reduced. This makes it possible to achieve a high gate-drain breakdown voltage.
[0057] (Sixteenth Modification) Next, in a nitride semiconductor device according to a sixteenth modification of the embodiment, the n-type impurity concentration in the n-type impurity-doped region is 3E18 cm -3 The nitride semiconductor device described above will now be described. In this modification, the n-type impurity concentration in the n-type impurity-doped region 8 is 3E18 cm -3 That's it (see, for example, FIG. 4).
[0058] 17 shows the results of an electric field simulation for this modification. In this figure, the width of n-type impurity doped region 8 in the gate-drain direction is fixed at 0.5 μm, the end of n-type impurity doped region 8 on the gate layer 6 side is set to 0.5 μm from the end of drain layer 7 on the gate layer 6 side, and the maximum electric field at the end of gate layer 6 on the drain layer 7 side and the end of drain layer 7 on the gate layer 6 side is simulated with a drain voltage of 650 V, a gate voltage of 0 V, and a source voltage of 0 V. The thickness of n-type impurity doped region 8 is set to three levels, 20 nm, 30 nm, and 40 nm from the surface of second nitride semiconductor layer 4, and the impurity concentration of n-type impurity doped region 8 is set to 1E18 cm -3 , 3E18cm -3 , 1E19cm -3 Three levels are calculated:
[0059] As can be seen from FIG. 17, the concentration of n-type impurities is set to 3E18 cm -3 By setting the value to 3E18 cm or more, the maximum electric field at the end of the drain layer 7 on the gate layer 6 side increases, but the maximum electric field at the end of the gate layer 6 on the drain layer 7 side decreases. As a result, although it depends on the depth of the n-type impurity-doped region 8, the n-type impurity concentration can be increased to 3E18 cm -3 By doing so, it is possible to lower the maximum electric field at the end of the gate layer 6 on the drain layer 7 side, thereby making it possible to reduce the gate leakage current.
[0060] By using this modification, in addition to the effects of the embodiment and the first to fifteenth modifications, the maximum electric field at the end of the gate layer 6 on the drain layer 7 side can be reduced, making it possible to reduce the gate leakage current.
[0061] (Seventeenth Modification) Next, a nitride semiconductor device according to a sixteenth modification of the embodiment, in which the thickness of the n-type impurity-doped region 8 is 40 nm or less, will be described. In this modification, the thickness of the n-type impurity-doped region 8 is 40 nm or less (see, for example, FIG. 1 ).
[0062] 17 shows the results of an electric field simulation for this modification. In this figure, the width of n-type impurity doped region 8 in the gate-drain direction is fixed at 0.5 μm, the end of n-type impurity doped region 8 on the gate layer 6 side is set to 0.5 μm from the end of drain layer 7 on the gate layer 6 side, and the maximum electric field at the end of gate layer 6 on the drain layer 7 side and the end of drain layer 7 on the gate layer 6 side is simulated with a drain voltage of 650 V, a gate voltage of 0 V, and a source voltage of 0 V. The depth of n-type impurity doped region 8 is set to three levels, 20 nm, 30 nm, and 40 nm from the surface of second nitride semiconductor layer 4, and the impurity concentration of n-type impurity doped region 8 is set to 1E18 cm -3 , 3E18cm -3 , 1E19cm -3 The three levels are calculated. The n-type impurity-doped region 8 is a region where the n-type impurity concentration is 1E17 cm -3 It is defined as a region having more than this.
[0063] As can be seen from FIG. 17, the impurity concentration of the n-type impurity-doped region 8 is set to 1E19 cm -3 In this case, if the thickness of the n-type impurity doped region 8 is 40 nm or more, the maximum electric field at the end of the drain layer 7 on the gate layer 6 side increases and far exceeds the maximum electric field at the end of the gate layer 6 on the drain layer 7 side. This increases the possibility of dielectric breakdown at the end of the drain layer 7 on the gate layer 6 side. As a result, by setting the thickness of the n-type impurity doped region 8 to 40 nm or less, it is possible to reduce the maximum electric field at the end of the drain layer 7 on the gate layer 6 side.
[0064] By using this modification, in addition to the effects of the embodiment and the first to sixteenth modifications, the maximum electric field at the end of the drain layer 7 on the gate layer 6 side can be reduced, thereby making it possible to ensure the gate-drain breakdown voltage.
[0065] (Manufacturing Method) Next, cross-sectional views showing each step of a manufacturing method for the structure shown in FIG. 16 , in which the source electrode 10 is not shown, are shown in FIGS. 18A to 18F. Note that this manufacturing method describes a minimum configuration, and is not limited to this. Furthermore, the order of steps in this manufacturing method is not limited to this.
[0066] First, an appropriate buffer layer 2 (e.g., a single layer or multiple layers of a Group III nitride semiconductor such as GaN, AlGaN, AlN, InGaN, InN, or AlInGaN) is formed on an appropriate Si substrate 1 (or a substrate of, for example, Sapphire, SiC, GaN, or AlN) using a known epitaxial growth technique such as MOCVD. Next, a first nitride semiconductor layer 3 made of GaN (e.g., a single layer or multiple layers of a Group III nitride semiconductor such as InGaN, InN, AlGaN, or AlInGaN) is formed on the buffer layer 2. Next, a second nitride semiconductor layer 4 made of AlGaN (e.g., a Group III nitride semiconductor such as GaN, InGaN, AlGaN, AlN, or AlInGaN) is formed on the first nitride semiconductor layer 3. The second nitride semiconductor layer 4 has a larger band gap than the first nitride semiconductor layer 3. When the second nitride semiconductor layer 4 is AlGaN and the first nitride semiconductor layer 3 is GaN, piezoelectric charges generated by the difference in lattice constants between AlGaN and GaN and the difference in band gap generate a high concentration of two-dimensional electron gas 5 on the first nitride semiconductor layer 3 side near the interface between the second nitride semiconductor layer 4 and the first nitride semiconductor layer 3. In this structure, since a gate recess structure is provided later to control the threshold voltage (Vth), normally-off operation is possible even if the second nitride semiconductor layer 4 has a film thickness of 40 nm or more when the Al composition of the second nitride semiconductor layer 4 is 15% or more.
[0067] Next, using known photolithography techniques, a resist pattern 16 is formed on the second nitride semiconductor layer 4. Next, ion implantation is performed from the surface side through the resist pattern 16 to form a damaged region 13 (FIG. 18A). The ion implantation involves implanting Si (or Ge, etc.), which is an n-type impurity.
[0068] The n-type impurity ions implanted into the damaged region 13 are implanted for two purposes: to obtain a low-resistance n-type nitride semiconductor layer, and to reduce the electric field strength between the gate layer 6 and the drain layer 7. Therefore, the concentration must be carefully set. Specifically, it is set to a minimum of 1E18 cm -3 Above, preferably 3E18cm -3The above is desirable, and the ion implanted crystal does not become completely amorphous due to ion implantation damage. -3 The ion implantation conditions depend on the thickness of the epitaxial structure used, but are set to 1E13 cm 2 or less with an energy of 10 keV to 50 keV and n-type impurity Si. -2 ~3E15cm -2 As a result, Si is implanted to a depth of about 20 nm to 100 nm at a depth of 1E18 cm -3 ~1E21cm -3 At this point, the crystal lattice of the damaged region 13 is broken due to the damage caused by the ion implantation, and the damaged region 13 becomes amorphous.
[0069] Next, the resist pattern 16 on the second nitride semiconductor layer 4 is completely removed using a known ashing method, organic cleaning method, sulfur-peroxide cleaning, or the like, and high-temperature activation annealing is performed using a known vertical annealing furnace, horizontal annealing furnace, rapid thermal processing (RTA) apparatus, or the like. The activation annealing is performed to activate the ion-implanted n-type impurities. Because this activation annealing is performed at a very high temperature, a silicon oxide film, silicon nitride film, or the like is used as a protective film (not shown) to prevent thermal decomposition of the surface of the second nitride semiconductor layer 4. The activation annealing diffuses the n-type impurities implanted into the damaged region 13 to the surrounding area, forming a diffusion region 14. Next, the protective film, such as a silicon oxide film or silicon nitride film, formed to prevent thermal decomposition of the surface of the second nitride semiconductor layer 4 is removed using a known hydrofluoric acid cleaning method or the like ( FIG. 18B ).
[0070] In order to activate the n-type impurities in the nitride semiconductor and to form a diffusion region 14 around the damaged region 13, activation annealing is usually performed at 1100° C. or higher, preferably 1150° C. or higher, for about 1 to 30 minutes.
[0071] Diffusion region 14 is present in all of the nitride semiconductor layers above, below, left, and right that are in contact with damage region 13. When the lower end of damage region 13 stops midway through second nitride semiconductor layer 4 (FIG. 18A), diffusion region 14 may stop within second nitride semiconductor layer 4 (FIG. 18B), but may also extend from within second nitride semiconductor layer 4 to reach two-dimensional electron gas 5 in first nitride semiconductor layer 3 (not shown).
[0072] The diffusion region 14 is defined as a region in contact with the damage region 13 and into which n-type impurities are diffused from the damage region 13. More specifically, the diffusion region 14 is defined as a region in which the concentration of n-type impurities is 1E17 cm -3 Furthermore, the concentration of n-type impurities in the diffusion region 14 is necessarily lower than that in the damage region 13 because the n-type impurities are diffused from the damage region 13.
[0073] The diffusion region 14 has no or very little ion implantation damage in the downward and lateral directions among the top, bottom, left and right directions that contact the damaged region 13, and has good crystallinity.
[0074] The thickness of the diffusion region 14 may be confined within the second nitride semiconductor layer 4 from the surface side of the second nitride semiconductor layer 4 in the depth direction, as shown in FIG. 18B . Alternatively, as shown in FIG. 11 , the diffusion region 14 may extend as far as the first nitride semiconductor layer 3. However, if the diffusion region 14 is too deep, as shown in the embodiment and its first to seventeenth modifications, the maximum electric field at the end of the drain layer 7 on the gate layer 6 side increases and far exceeds the maximum electric field at the end of the gate layer 6 on the drain layer 7 side. This increases the possibility of dielectric breakdown at the end of the drain layer 7 on the gate layer 6 side. Therefore, by setting the thickness of the n-type impurity-doped region 8 to 40 nm or less, it is possible to reduce the maximum electric field at the end of the drain layer 7 on the gate layer 6 side.
[0075] The n-type impurity doped region 8 shown in FIGS. 1 to 11 can be regarded as the combined region of the diffusion region 14 and the damage region 13 shown in FIGS.
[0076] Next, a resist pattern 16 is formed by a known lithography method, and dry etching is performed using an inductively coupled plasma reactive ion etching (ICP-RIE) method or the like to form a gate recess 15 ( FIG. 18C ). The bottom of the gate recess 15 may penetrate the second nitride semiconductor layer 4 and reach the first nitride semiconductor layer 3 as shown in FIG. 18C , or may stop midway through the second nitride semiconductor layer 4 (not shown).
[0077] Next, the resist pattern 16 is removed and cleaned using a known ashing method, organic cleaning method, sulfur-peroxide cleaning method, or the like, and then a third nitride semiconductor layer 17 made of AlGaN (or other group III nitride semiconductors such as GaN, InGaN, AlGaN, AlN, and AlInGaN) is formed using a known epitaxial growth technique such as MOCVD. Next, a fourth nitride semiconductor layer 18 made of p-GaN containing p-type impurities (such as Mg, Zn, and C) (or other group III nitride semiconductors such as p-InGaN, p-InN, p-AlGaN, and p-AlInGaN) is formed by regrowth on the third nitride semiconductor layer 17 (FIG. 18D). The third nitride semiconductor layer 17 is formed to control the Vth of a field-effect transistor (FET), and therefore the Al composition and film thickness must be appropriately adjusted to ensure normally-off operation of the FET. For example, in order to set Vth to around +1 V, it is necessary to set the Al composition of AlGaN to around 20% and the film thickness to around 20 nm. Furthermore, when the third nitride semiconductor layer 17 is made of a material containing Al, such as AlGaN, the lateral growth rate is slow, so the layer grows along the gate recess 15 without filling the gate recess 15, as shown in FIG. 18D. Conversely, when the fourth nitride semiconductor layer 18 is made of a material not containing Al, such as p-GaN, the lateral growth rate is fast, so the layer grows so as to fill the gate recess 15, as shown in FIG. 18D. The concentration of p-type impurities (Mg, Zn, C, etc.) in the fourth nitride semiconductor layer 18 is set to 1E19 cm in order to make it p-type. -3 Above, if possible, 5E19cm -3 The above is desirable.
[0078] During the process of forming this third nitride semiconductor layer 17, the crystallinity of the damaged region 13 is somewhat restored by supplying group III raw materials such as trimethylgallium (TMG) and trimethylaluminum (TMA), group V raw materials such as ammonia, and carrier gases such as nitrogen and hydrogen from the surface side of the damaged region 13, so that the damaged region 13 has a slightly amorphous-like structure with better crystallinity than a completely amorphous structure. Therefore, the third nitride semiconductor layer 17 that grows directly on the damaged region 13 with restored crystallinity has improved crystallinity and grows epitaxially.
[0079] Since this regrowth process is performed at a very high temperature of around 1000° C., the n-type impurities further diffuse into the surroundings, causing the diffusion region 14 to further expand slightly in all directions, including up and down, left and right, and into the regrown third nitride semiconductor layer 17 (FIG. 18D).
[0080] Next, a resist pattern (not shown) is formed on the fourth nitride semiconductor layer 18 by a known lithography method, and selective dry etching is performed using inductively coupled plasma reactive ion etching (ICP-RIE) or the like to form the gate layer 6 and the drain layer 7. Even when selective dry etching is performed, the selectivity of the dry etching rates of the fourth nitride semiconductor layer 18 and the third nitride semiconductor layer 17 is not infinite, so the third nitride semiconductor layer 17 is overetched by several to several tens of nanometers (not shown). For example, if the regrowth thickness of the third nitride semiconductor layer 17 is about 20 nm, the overetching may be stopped midway through the third nitride semiconductor layer 17 (not shown), or the third nitride semiconductor layer 17 may be overetched by about 20 nm to completely remove it except for the portion directly below the gate layer 6 (not shown). Further overetching may be performed to completely etch down to the second nitride semiconductor layer 4 (not shown).
[0081] When the fourth nitride semiconductor layer 18 made of p-GaN containing p-type impurities (Mg, Zn, C, etc.) is formed continuously after the third nitride semiconductor layer 17 is formed, the p-type impurities diffuse from the surface side of the third nitride semiconductor layer 17, generating a p-type impurity diffusion region (not shown). The p-type impurity concentration in this p-type impurity diffusion region is 5E18 cm -3 If the concentration is too high, such as 5E18 cm or more, the layer will become a p-type nitride semiconductor layer, and the p-type impurity diffusion region will have low resistance. In that case, the surface leakage current will increase when a FET or the like is formed. For this reason, it is recommended that the p-type impurity concentration be 5E18 cm or more. -3 Of the above p-type impurity diffusion regions, it is desirable to remove the regions other than those directly below the gate layer 6 by the above-mentioned over-etching. In other words, the concentration of p-type impurities on the outermost surface side of the p-type impurity diffusion region other than those directly below the gate layer 6 is 5E18 cm -3 The following is desirable:
[0082] Subsequently, the resist pattern is removed and washed using a known ashing method, organic cleaning method, sulfur-peroxide cleaning method, or the like (FIG. 18E).
[0083] Next, activation annealing of the p-type impurities is performed using a known annealing technique in a gas atmosphere such as nitrogen at 700 to 900°C for about 10 to 60 minutes, thereby activating about 1% of the p-type impurities, and the gate layer 6 and the drain layer 7 become p-type.
[0084] Next, a source electrode (not shown) and a drain electrode 11 are formed on the drain layer 7 and the second nitride semiconductor layer 4 using known techniques such as photolithography, vapor deposition, lift-off, sputtering, dry etching, annealing (alloying), ashing, organic cleaning, and sulfur-peroxide cleaning. The drain electrode 11 is made of an electrode made of one or a combination of two or more metals such as Ti, Al, Mo, and Hf, which are in ohmic contact with the nitride semiconductor layer, and is electrically connected to the two-dimensional electron gas 5. Note that the drain electrode 11 may be located on the first nitride semiconductor layer 3, the second nitride semiconductor layer 4, or the third nitride semiconductor layer 17, as long as it is electrically connected to the two-dimensional electron gas 5.
[0085] Finally, a gate electrode 9 is formed using known techniques such as photolithography, vapor deposition, lift-off, sputtering, dry etching, annealing (alloying), ashing, organic cleaning, and sulfur-peroxide cleaning (FIG. 18F). The gate electrode 9 may be an electrode made of one or a combination of two or more metals, such as Ti, Ni, Pd, Pt, Au, W, WSi, Ta, TiN, Al, Mo, Hf, and Zr. While the gate electrode 9 may be in ohmic or Schottky contact with the gate layer 6, ohmic contact provides higher reliability of the gate electrode. Therefore, it is preferable to use an electrode made of one or a combination of two or more metals with low contact resistance, such as Ni, Pt, Pd, Au, Ti, Cr, In, Sn, and Al.
[0086] The effects of this manufacturing method are explained below. By using this manufacturing method, it is possible to change the electric field strength at the gate side end of the drain layer 7, thereby lowering the maximum electric field strength between the gate and drain, and to manufacture a structure that reduces gate leakage current. In addition, it is possible to increase the concentration of the two-dimensional electron gas 5 immediately below the diffusion region 14 between the gate and drain and the damaged region 13, thereby reducing the sheet resistance, and as a result, it is possible to reduce the on-resistance and increase the maximum drain current.
[0087] Next, cross-sectional views of the structure shown in Fig. 16 are shown in Fig. 19A to Fig. 19F, illustrating a manufacturing method in which activation annealing is performed at a different timing than the manufacturing method shown in Fig. 18A to Fig. 18F. Note that this manufacturing method describes a minimum configuration, and is not limited to this. Furthermore, the order of steps in this manufacturing method is not limited to this.
[0088] In this manufacturing method, the gate recess process (FIGS. 19A-19B) and the ion implantation process (FIG. 19C) are performed first. The order in which the gate recess process and the ion implantation process are performed may be either the ion implantation process first as shown in FIGS. 18A-18C, or the gate recess process first as shown in FIGS. 19A-19C. The manufacturing method for each process is the same as that shown in the explanation for FIGS. 18A-18C.
[0089] Next, the resist pattern and the like are completely removed by a known ashing method, organic cleaning method, cleaning with sulfur-peroxide solution, etc., to clean the surface. Thereafter, a known epitaxial growth technique such as MOCVD is used to form a third nitride semiconductor layer 17 made of AlGaN (or other group III nitride semiconductors such as GaN, InGaN, AlGaN, AlN, AlInGaN, etc.).
[0090] During the process of forming this third nitride semiconductor layer 17, the crystallinity of the damaged region 13 is somewhat restored by supplying group III raw materials such as trimethylgallium (TMG) and trimethylaluminum (TMA), group V raw materials such as ammonia, and carrier gases such as nitrogen and hydrogen from the surface side of the damaged region 13, so that the damaged region 13 has a slightly amorphous-like structure with better crystallinity than a completely amorphous structure. Therefore, the third nitride semiconductor layer 17 that grows directly on the damaged region 13 with restored crystallinity has improved crystallinity and grows epitaxially.
[0091] Subsequently, immediately after the formation of the third nitride semiconductor layer 17, activation annealing of Si (or Ge, etc.) as an n-type impurity is carried out continuously at high temperature in the MOCVD chamber (in-situ).
[0092] In order to activate the n-type impurities in the nitride semiconductor and to form a diffusion region 14 around the damaged region 13, activation annealing is usually performed at 1100° C. or higher, preferably 1150° C. or higher, for about 1 to 30 minutes.
[0093] If this in-situ activation annealing is performed before the formation of the third nitride semiconductor layer 17 and the second nitride semiconductor layer 4 does not contain Al, for example, is made of GaN, the second nitride semiconductor layer 4 at the bottom of the gate recess 15 will be etched by a carrier gas such as hydrogen or a source gas such as ammonia, resulting in a deep gate recess 15. Therefore, when in-situ activation annealing is performed, it is desirable to perform it after the formation of the third nitride semiconductor layer 17.
[0094] Furthermore, even when activation annealing is performed after forming the third nitride semiconductor layer 17 containing Al, which is resistant to thermal decomposition, as shown in the present manufacturing method, some thermal decomposition occurs from the surface side of the third nitride semiconductor layer 17, causing the stoichiometry to be lost and the film thickness to be reduced. However, in the present manufacturing method, by forming the fourth nitride semiconductor layer 18 after the activation annealing, the group III and group V elements that have been desorbed by the activation annealing can be resupplied to the third nitride semiconductor layer 17, which has the effect of improving the crystallinity of the third nitride semiconductor layer 17.
[0095] Furthermore, even if the third nitride semiconductor layer 17 is thinned by thermal decomposition during activation annealing, the thinned portion may be regrown (not shown). This additional nitride semiconductor layer, which replaces the thinned portion, has a larger band gap than the first nitride semiconductor layer 3 and is in direct contact with the third nitride semiconductor layer 17. It is desirable that two-dimensional electron gas is not formed at the interface between the third nitride semiconductor layer 17 and the additional nitride semiconductor layer directly below the thinned portion, because this could cause gate leakage current when a field-effect transistor is formed. Therefore, it is desirable that the band gap of this nitride semiconductor layer is equal to or smaller than the band gap of the second nitride semiconductor layer 4. Furthermore, when this nitride semiconductor layer is made of, for example, AlGaN, having a band gap equal to or smaller than that of the third nitride semiconductor layer 17 reduces the Al composition, thereby improving crystallinity.
[0096] The diffusion region 14 is formed in all of the nitride semiconductor layers adjacent to the damaged region 13, above, below, left, and right. If the bottom end of the damaged region 13 stops midway through the second nitride semiconductor layer 4 (FIG. 19C), the diffusion region 14 may stop within the second nitride semiconductor layer 4 (FIG. 19D), or may extend from within the second nitride semiconductor layer 4 to the two-dimensional electron gas 5 in the first nitride semiconductor layer 3 (not shown). Furthermore, since activation annealing is performed after the formation of the third nitride semiconductor layer 17, the diffusion region 14 can also be extended into the third nitride semiconductor layer 17 located above the damaged region 13.
[0097] Furthermore, the diffusion region 14 has no or very little ion implantation damage in the downward and lateral directions among the directions above, below, left and right that contact the damaged region 13, and has good crystallinity.
[0098] The thickness of the diffusion region 14 may be confined within the second nitride semiconductor layer 4 from the surface side of the second nitride semiconductor layer 4 in the depth direction, as shown in FIG. 19D . Alternatively, as shown in FIG. 11 , the diffusion region 14 may extend as far as the first nitride semiconductor layer 3. However, if the diffusion region 14 is too deep, as shown in the first to seventeenth modifications of the embodiment, the maximum electric field at the end of the drain layer 7 on the gate layer 6 side increases and far exceeds the maximum electric field at the end of the gate layer 6 on the drain layer 7 side. This increases the possibility of dielectric breakdown at the end of the drain layer 7 on the gate layer 6 side. Therefore, by setting the thickness of the n-type impurity-doped region 8 to 40 nm or less, it is possible to reduce the maximum electric field at the end of the drain layer 7 on the gate layer 6 side.
[0099] The diffusion region 14 is defined as a region in contact with the damage region 13 and into which n-type impurities are diffused from the damage region 13. More specifically, the diffusion region 14 is defined as a region in which the concentration of n-type impurities is 1E17 cm -3 Furthermore, the concentration of n-type impurities in the diffusion region 14 is necessarily lower than that in the damage region 13 because the n-type impurities are diffused from the damage region 13.
[0100] The n-type impurity doped region 8 shown in FIGS. 1 to 11 can be regarded as the combined region of the diffusion region 14 and the damage region 13 shown in FIGS.
[0101] Subsequently, following the activation annealing, a fourth nitride semiconductor layer 18 (also including, for example, Group III nitride semiconductors such as p-InGaN, p-InN, p-AlGaN, and p-AlInGaN) made of p-GaN containing p-type impurities (e.g., Mg, Zn, and C) is formed by regrowth on the third nitride semiconductor layer 17 ( FIG. 19D ). The third nitride semiconductor layer 17 is formed to control the Vth of a field-effect transistor (FET). Therefore, in order to operate the FET in a normally-off mode, the Al composition and film thickness must be appropriately adjusted. For example, to set the Vth to approximately +1 V, the Al composition of AlGaN must be set to approximately 20% and the film thickness must be set to approximately 20 nm. Furthermore, when the third nitride semiconductor layer 17 is made of a material containing Al, such as AlGaN, its lateral growth rate is slow, and therefore, as shown in FIG. 19D , the layer is grown along the gate recess 15 without filling the gate recess 15. Conversely, when the fourth nitride semiconductor layer 18 is made of a material that does not contain Al, such as p-GaN, the lateral growth rate is fast, and the layer is grown so as to fill the gate recess 15, as shown in FIG. 19D. The concentration of p-type impurities (Mg, Zn, C, etc.) in the fourth nitride semiconductor layer 18 is set to 1E19 cm 3 to impart p-type conductivity. -3 Above, if possible, 5E19cm -3 The above is desirable.
[0102] Since this regrowth process is performed at a very high temperature of around 1000° C., the n-type impurity further diffuses to the surroundings, causing the diffusion region 14 to further expand slightly in all directions. At this time, the diffusion region 14 may further expand from the regrown third nitride semiconductor layer 17 to the fourth nitride semiconductor layer 18, as shown in FIG.
[0103] Subsequently, the process of selectively dry etching the fourth nitride semiconductor layer 18 to form the gate layer 6 and the drain layer 7 ( FIG. 19E ), the activation annealing process of the p-type impurity, the process of forming the source electrode (not shown) and the drain electrode 11, and the process of forming the gate electrode 9 ( FIG. 19F ) are the same as those in FIGS. 18E and 18F .
[0104] The effects of this manufacturing method will now be described. In addition to the effects of the manufacturing method shown in FIGS. 18A to 18F, this manufacturing method allows activation annealing to be performed in situ simultaneously with the regrowth process of the third nitride semiconductor layer 17 and the fourth nitride semiconductor layer 18, thereby simplifying the process. Furthermore, because activation annealing is performed after the formation of the third nitride semiconductor layer 17, the diffusion region 14 can be extended to the third nitride semiconductor layer 17 above the damaged region 13. This allows the n-type layer to be formed further to the outermost surface of the third nitride semiconductor layer 17, more effectively changing the electric field strength at the gate-side end of the drain layer 7 and lowering the maximum electric field strength between the gate and drain, thereby producing a structure that reduces gate leakage current.
[0105] (Summary) The following describes the features of the nitride semiconductor devices described based on the above embodiments.
[0106] A nitride semiconductor device according to a first aspect of the present disclosure comprises: a substrate; a first nitride semiconductor layer provided on the substrate; a second nitride semiconductor layer in contact with and on top of the first nitride semiconductor layer and having a larger band gap than the first nitride semiconductor layer; a gate layer made of a p-type nitride semiconductor selectively formed on the second nitride semiconductor layer; a drain layer made of a p-type nitride semiconductor provided spaced apart from the gate layer; and a drain electrode electrically connected to both the second nitride semiconductor layer and the drain layer, wherein the second nitride semiconductor layer has a region selectively doped with n-type impurities, and a gate-side end of the region doped with n-type impurities is located between the gate layer and the drain layer.
[0107] A nitride semiconductor device according to a second aspect of the present disclosure is the nitride semiconductor device according to the first aspect, wherein an end of the region in which n-type impurities are selectively added in the second nitride semiconductor layer opposite to the gate side is located between the gate layer and the drain layer.
[0108] A nitride semiconductor device according to a third aspect of the present disclosure is the nitride semiconductor device according to the first or second aspect, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is located on the drain layer side of a midline between the gate layer and the drain layer.
[0109] A nitride semiconductor device according to a fourth aspect of the present disclosure is the nitride semiconductor device according to the first or third aspect, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is in contact with an end of the drain layer.
[0110] A nitride semiconductor device according to a fifth aspect of the present disclosure is the nitride semiconductor device according to at least one of the first to fourth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is located on the outermost surface of the second nitride semiconductor layer.
[0111] A nitride semiconductor device according to a sixth aspect of the present disclosure is the nitride semiconductor device according to any one of the first aspect and the third to fifth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is continuous and extends below the drain layer.
[0112] A nitride semiconductor device according to a seventh aspect of the present disclosure is the nitride semiconductor device according to any one of the first aspect and the third to sixth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is also located under the drain electrode.
[0113] A nitride semiconductor device according to an eighth aspect of the present disclosure is the nitride semiconductor device according to any one of the first aspect and the third to seventh aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is continuous across from under the drain layer to under the drain electrode.
[0114] A nitride semiconductor device according to a ninth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to eighth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is also present in the drain layer.
[0115] A nitride semiconductor device according to a tenth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to ninth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is also present in the surface of the drain layer.
[0116] A nitride semiconductor device according to an eleventh aspect of the present disclosure is the nitride semiconductor device according to any one of the first to tenth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities reaches the first nitride semiconductor layer in the depth direction.
[0117] A nitride semiconductor device according to a twelfth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to eleventh aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damage region in the center of the region and a diffusion region surrounding the damage region, and the n-type impurity concentration in the diffusion region is lower than the n-type impurity concentration in the damage region.
[0118] A nitride semiconductor device according to a thirteenth aspect of the present disclosure is a nitride semiconductor device according to any one of the first to twelfth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damaged region in the center of the region and a diffusion region surrounding the damaged region, and the diffusion region is located below the drain layer.
[0119] A nitride semiconductor device according to a fourteenth aspect of the present disclosure is a nitride semiconductor device according to any one of the first to thirteenth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damaged region in the center of the region doped with n-type impurities and a diffusion region surrounding the damaged region, and the damaged region is located below the drain layer.
[0120] A nitride semiconductor device according to a fifteenth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to fourteenth aspects, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is in a range of 1 μm or less from the gate-side end of the drain layer toward the gate layer.
[0121] A nitride semiconductor device according to a sixteenth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to fifteenth aspects, wherein an end of the region in which n-type impurities are selectively added in the second nitride semiconductor layer opposite to the gate layer side is 1 μm or less from the gate side end of the drain layer toward the gate layer.
[0122] A nitride semiconductor device according to a seventeenth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to sixteenth aspects, wherein the n-type impurity concentration in the region selectively doped with n-type impurities in the second nitride semiconductor layer is 3E18 cm -3 That's all.
[0123] A nitride semiconductor device according to an eighteenth aspect of the present disclosure is the nitride semiconductor device according to any one of the first to seventeenth aspects, wherein the thickness of the region in the second nitride semiconductor layer selectively doped with n-type impurities is 40 nm or less.
[0124] While nitride semiconductor devices according to one or more aspects have been described above based on the embodiments, the present disclosure is not limited to these embodiments. As long as they do not deviate from the gist of the present disclosure, various modifications conceivable by those skilled in the art to the present embodiments and configurations constructed by combining components of different embodiments are also included within the scope of the present disclosure.
[0125] Furthermore, various modifications, substitutions, additions, omissions, etc. can be made to the above-described embodiments within the scope of the claims or their equivalents.
[0126] The present disclosure can reduce the on-resistance of a semiconductor device and increase the maximum drain current, thereby improving the performance of the power device.
[0127] REFERENCE SIGNS LIST 1 substrate 2 buffer layer 3 first nitride semiconductor layer 4 second nitride semiconductor layer 5 two-dimensional electron gas 6 gate layer 7 drain layer 8 n-type impurity doped region 9 gate electrode 10 source electrode 11 drain electrode 12 midline 13 damaged region 14 diffusion region 15 gate recess 16 resist pattern 17 third nitride semiconductor layer 18 fourth nitride semiconductor layer
Claims
1. A nitride semiconductor device comprising: a substrate; a first nitride semiconductor layer provided on the substrate; a second nitride semiconductor layer in contact with the first nitride semiconductor layer and having a larger band gap than the first nitride semiconductor layer; a gate layer made of a p-type nitride semiconductor selectively formed on the second nitride semiconductor layer; a drain layer made of a p-type nitride semiconductor provided spaced apart from the gate layer; and a drain electrode electrically connected to both the second nitride semiconductor layer and the drain layer, wherein the second nitride semiconductor layer has a region selectively doped with an n-type impurity, and a gate side end of the region doped with the n-type impurity is between the gate layer and the drain layer.
2. The nitride semiconductor device according to claim 1, wherein an end of said region in said second nitride semiconductor layer selectively doped with n-type impurities opposite to the gate side is located between said gate layer and said drain layer.
3. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with an n-type impurity is located on the drain layer side of a midline between the gate layer and the drain layer.
4. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with an n-type impurity contacts an end of the drain layer.
5. The nitride semiconductor device according to claim 1, wherein the region in which the second nitride semiconductor layer is selectively doped with an n-type impurity is located on the outermost surface of the second nitride semiconductor layer.
6. The nitride semiconductor device according to claim 1, wherein the region in which the second nitride semiconductor layer is selectively doped with an n-type impurity is continuous and extends under the drain layer.
7. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with an n-type impurity is also located under the drain electrode.
8. The nitride semiconductor device according to claim 1, wherein the region in which the second nitride semiconductor layer is selectively doped with an n-type impurity is continuous across from under the drain layer to under the drain electrode.
9. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with an n-type impurity is also present in the drain layer.
10. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with an n-type impurity is also present in the surface of the drain layer.
11. The nitride semiconductor device according to claim 1, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities reaches the first nitride semiconductor layer in the depth direction.
12. A nitride semiconductor device as described in any one of claims 1 to 10, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damage region in the center of the region and a diffusion region surrounding the damage region, and the n-type impurity concentration of the diffusion region is lower than the n-type impurity concentration of the damage region.
13. A nitride semiconductor device according to any one of claims 1 to 11, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damaged region in the center of the region and a diffusion region surrounding the damaged region, the diffusion region being located under the drain layer.
14. A nitride semiconductor device according to any one of claims 1 to 11, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities comprises a damage region in the center of the region doped with n-type impurities and a diffusion region surrounding the damage region, and the damage region is located under the drain layer.
15. A nitride semiconductor device according to any one of claims 1 to 11, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities is in a range of 1 μm or less from the gate side end of the drain layer towards the gate layer.
16. A nitride semiconductor device according to any one of claims 1 to 11, wherein the end of the region in which n-type impurities are selectively added in the second nitride semiconductor layer opposite the gate layer is 1 μm or less from the gate side end of the drain layer towards the gate layer.
17. The n-type impurity concentration in the region in which the n-type impurity is selectively added to the second nitride semiconductor layer is 3E18 cm -3 The nitride semiconductor device according to claim 1 , wherein the nitride semiconductor device is a nitride semiconductor layer.
18. The nitride semiconductor device according to any one of claims 1 to 11, wherein the region in the second nitride semiconductor layer selectively doped with n-type impurities has a thickness of 40 nm or less.
Citation Information
Patent Citations
Field-effect transistor and manufacture thereof
JP1997270522A
Semiconductor device and manufacturing method therefor
JP2013055224A
Semiconductor device and method of manufacturing the same
JP2013207081A
Field effect transistor
JP2013239735A
Semiconductor device and method of manufacturing the same