Analysis method
The method simplifies solid sample analysis by using a regression equation based on signal intensities from standard sample films to calculate analyte concentrations in solid samples, addressing the complexity and reproducibility issues of existing techniques.
Patent Information
- Application Number
- PCT/JP2024/008246
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-12-07
- Filing Date
- 2024-03-05
- Publication Date
- 2024-10-03
AI Technical Summary
Current methods for analyzing solid samples, such as LA-ICP-OES and LA-ICP-MS, require complex pretreatment processes like mixing resin powder with the sample, heating, and molding, which are time-consuming and prone to component segregation, affecting reproducibility, especially for powder samples.
The method involves creating a regression equation based on signal intensity values from standard sample films irradiated with a laser, allowing for direct analysis of solid samples without pretreatment by forming an analytical laminate and varying the concentration or thickness of the standard sample membrane to calculate the analyte concentration in the sample.
This approach simplifies the analysis process, improves reproducibility, and eliminates the need for complex pretreatment, enabling easy analysis of a wide range of solid samples, including powders, by directly calculating analyte concentrations through laser-induced signal intensities.
Smart Images

Figure JPOXMLDOC01-APPB-T000001 
Figure JPOXMLDOC01-APPB-T000002 
Figure JPOXMLDOC01-APPB-T000003
Abstract
Description
Analysis method
[0001] The present invention relates to an analytical method.
[0002] The method of irradiating a sample with laser light and analyzing it is known as a method for qualitative and quantitative analysis of solid samples. When a high-intensity laser light is incident on a solid sample, it produces light emission specific to the elements contained in the solid sample, or it evaporates part of the solid sample from the sample surface, generating gas or fine particles derived from the solid sample. Examples of methods for analyzing solid samples that utilize phenomena that occur when laser light is incident include laser-induced breakdown spectroscopy (LIBS), laser ablation inductively coupled plasma optical emission spectrometry (LA-ICP-OES), and laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS). In LA-ICP-OES and LA-ICP-MS, gas or particles generated from a solid sample by irradiation with laser light are introduced into an inductively coupled plasma, and analyzed using a photodetector and a mass analyzer, respectively. These analytical methods enable qualitative and quantitative analysis of solid samples.
[0003] While LA-ICP-OES and LA-ICP-MS are applicable to solid samples, the introduction of gas or particles derived from the solid sample into the inductively coupled plasma is required for powder samples to ensure analytical reproducibility. A common approach is to compact the powder sample into a powder compact. In this regard, Patent Document 1 describes an invention in which a fine resin powder and the powder sample are mixed, heated above the melting point of the resin, and then cooled to form a sample disk for laser ablation. It is described that this invention ensures analytical reproducibility.
[0004] JP 2013-238455 A
[0005] In the analysis of solid samples, there is a demand for a simpler method that does not require pretreatment, etc. In the method described in Patent Document 1, in order to obtain a sample for measurement, it is necessary to mix a resin powder with a powder sample to obtain a mixture, and then heat the mixture, cool it, and mold it, which is far from being a simple method, and therefore an improvement has been demanded.
[0006] Therefore, an object of the present invention is to provide an analytical method that can easily analyze an analyte in a solid sample.
[0007] The present inventors have conducted extensive research to solve the above problems and have completed the present invention. That is, they have found that the above problems can be solved by the following configuration.
[0008] [1] An analytical method comprising performing any one of the following operations 1 to 4, creating a regression equation based on the signal intensity value obtained and the amount of the analyte contained in a standard sample film removed by laser light irradiation, and using the regression equation to calculate the amount of the analyte in a solid analytical sample containing the analyte removed by laser light irradiation.Operation 1: Placing the standard sample film containing the analyte on the solid analytical sample containing the analyte to obtain an analytical laminate, irradiating the analytical laminate with laser light, and performing operation X, which detects signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample, two or more times while changing the concentration of the analyte in the standard sample film.Operation 2: Performing operation X at least once and operation Y, which irradiates the analytical sample with laser light and detects signal intensities derived from the analyte in the analytical sample. Operation 3: Performing at least the following steps: Operation X at least once; and Operation Z, in which a reference sample film not containing the analyte is placed on the analytical sample to obtain a reference laminate, and the reference laminate is irradiated with laser light to detect the signal intensity derived from the analyte in the analytical sample. Operation 4: Performing Operation X at least twice while changing the number or thickness of the standard sample films stacked. [2] The analytical method according to [1], further comprising a step of calculating the concentration of the analyte in the analytical sample based on the amount of the analyte in the analytical sample removed by laser light irradiation. [3] The analytical method according to [1] or [2], in which the removed volume of the analytical sample removed by laser light irradiation is determined by shape measurement, and the volume concentration of the analyte in the analytical sample is calculated based on the removed volume. [4] The analytical method according to any one of [1] to [3], in which the signal intensity is a signal intensity obtained by mass spectrometry.
[0009] According to the present invention, an analytical method can be provided that can easily analyze an analyte in a solid sample.
[0010] FIG. 1 is a schematic cross-sectional view illustrating a part of operation X performed in the present invention. FIG. 2 is a schematic top view and a schematic cross-sectional view of an analytical laminate used in the examples. FIG. 3 is a top view of a perforated adhesive tape used in an embodiment in which the number of stacked standard sample membranes is changed in the fourth embodiment of the present invention. FIG. 4 is a schematic cross-sectional view illustrating an embodiment in which the number of stacked standard sample membranes is changed in the fourth embodiment of the present invention. FIG. 5 is a schematic cross-sectional view illustrating an embodiment in which the number of stacked standard sample membranes is changed in the fourth embodiment of the present invention. FIG. 6 is a diagram illustrating an embodiment of an adhesive tape that may be used in the fourth embodiment of the present invention.
[0011] The present invention will be described in detail below. The following description of the components may be based on representative embodiments of the present invention, but the present invention is not limited to such embodiments.
[0012] The following describes the meaning of each description in this specification.
[0013] In this specification, a numerical range expressed using "to" means a range that includes the numerical values before and after "to" as the lower and upper limits.
[0014] <Analysis Method> The analysis method of the present invention involves performing any one of the following procedures 1 to 4, creating a regression equation based on the signal intensity value obtained and the amount of the analyte contained in a standard sample film removed by laser light irradiation, and using the regression equation to calculate the amount of the analyte in a solid analytical sample containing the analyte removed by laser light irradiation. Procedure 1: A standard sample film containing the analyte is placed on a solid analytical sample containing the analyte to obtain an analytical laminate, and procedure X, in which the analytical laminate is irradiated with laser light and signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample are detected, is performed two or more times while changing the concentration of the analyte in the standard sample film. Procedure 2: Procedure X is performed at least once, and at least procedure Y, in which the analytical sample is irradiated with laser light and signal intensities derived from the analyte in the analytical sample are detected. Operation 3: Perform operation X at least once, and at least operation Z, in which a reference sample film not containing the analyte is placed on the analytical sample to obtain a reference laminate, and the reference laminate is irradiated with laser light to detect the signal intensity derived from the analyte in the analytical sample.Operation 4: Perform operation X at least twice while varying the number or thickness of the standard sample films stacked.In other words, operation 4 corresponds to operation W, in which a plurality of analytical laminates are obtained by stacking the standard sample film containing the analyte on the solid analytical sample containing the analyte, with varying numbers or thicknesses of layers, and the plurality of analytical laminates are irradiated with laser light to detect the signal intensity derived from the analyte in the standard sample film and the analyte in the analytical sample, respectively.The regression equation is created using the value of the obtained signal intensity as the dependent variable and the amount of the analyte contained in the standard sample film removed by the laser light irradiation as the independent variable.
[0015] In the analytical method of the present invention, a standard sample film is simply placed on the analytical sample in Procedures X and W, and a reference sample film is simply placed on the analytical sample in Procedure Z, so pretreatment is not required and measurements can be performed easily. Furthermore, since no pretreatment is required in Procedure Y, measurements can be performed easily. Furthermore, in the analytical method of the present invention, even if the analytical sample is a powder sample, there is no need to mix it with a resin powder, and there is no need to heat the resin powder to melt it. Therefore, in the analytical method of the present invention, heating does not cause any chemical reactions to proceed, and the analytical sample does not melt, so the analysis of a wide range of samples can be easily performed. Furthermore, since pretreatment does not cause segregation of components in the solid sample, it is believed that the reproducibility of measurements is also improved.
[0016] The analytical method of the present invention will be described in detail below. In the following, the case where operation 1 is performed will be referred to as the first embodiment, the case where operation 2 is performed will be referred to as the second embodiment, the case where operation 3 is performed will be referred to as the third embodiment, and the case where operation 4 is performed will be referred to as the fourth embodiment.
[0017] <First Embodiment> In a first embodiment of the analytical method of the present invention, the following procedure 1 is carried out, a regression equation is created based on the obtained signal intensity value and the amount of the analyte contained in the standard sample film removed by laser light irradiation, and the regression equation is used to calculate the amount of the analyte in the solid analytical sample containing the analyte removed by laser light irradiation. Procedure 1: A standard sample film containing the analyte is placed on a solid analytical sample containing the analyte to obtain an analytical laminate, and laser light is irradiated onto the analytical laminate to detect signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample. This procedure X is carried out two or more times while changing the concentration of the analyte in the standard sample film. Below, we will first explain procedure X.
[0018] [Procedure X] In procedure X, a standard sample film containing an analyte is placed on a solid analytical sample containing the analyte to obtain an analytical laminate, and laser light is irradiated onto the analytical laminate to detect signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample. Note that the signal intensities are those obtained by the analytical means described below. Procedure X will be described in detail below.
[0019] (Analyte) The standard sample film and the analytical sample contain an analyte. The analyte is not particularly limited as long as it can provide a signal intensity by the analytical means described below. Examples of the analyte include a specific element, a specific group, and a specific organic molecule.
[0020] The specific element is preferably a metal element. Examples of the metal element include metal elements in Groups 1 to 16 of the periodic table. Metal elements in Group 13 include aluminum (Al), gallium (Ga), indium (In), and thallium (Tl). Metal elements in Group 14 include germanium (Ge), tin (Sn), and lead (Pb). Metal elements in Group 15 of the periodic table include antimony (Sb) and bismuth (Bi). Metal elements in Group 16 of the periodic table include polonium (Po). As the metal element, lithium (Li), sodium (Na), potassium (K), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), zirconium (Zr), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), manganese (Mn), iron (Fe), nickel (Ni), palladium (Pd), cobalt (Co), copper (Cu), silver (Ag), zinc (Zn), cadmium (Cd), mercury (Hg), aluminum (Al), gallium (Ga), thallium (Tl), and lead (Pb) are preferred. The specific elements as described above can be analyzed by, for example, mass spectrometry, emission spectrometry, and absorption spectrometry to obtain the signal intensity.
[0021] The specific group may be a group containing carbon atoms or a group not containing carbon atoms. The specific group may be a monovalent group or a divalent or higher valent group. Examples of the specific group include hydrocarbon groups. Examples of the hydrocarbon group include alkyl groups, alkynyl groups, alkenyl groups, and aryl groups, as well as groups formed by combining these groups. A linking group containing a carbon atom (for example, -CH 2 The groups (-, -CH=, etc.) may be substituted with a linking group as described later. Furthermore, the hydrogen atoms of the hydrocarbon groups may be substituted with a substituent as described later. Furthermore, the specific group may be a substituent as described later.
[0022] Examples of the substituent include an aldehyde group (-CHO), a carboxy group (-COOH) and its salts, a cyano group (-CN), a hydroxy group (-OH), an amino group (-NR T 2 ), nitro group (-NO 2 ), sulfo group (—SO 3 H) and its salts, phosphate group (-PO 4 H 2 ) and salts thereof, halogen atoms (e.g., F, Cl, Br and I). T each independently represents a hydrogen atom or a hydrocarbon group which may have a substituent. Examples of the linking group include an ether bond (-O-), a sulfide bond (-S-), an azo group (-N=N-), a carbonyl group (-CO-), an ester bond (-COO-), an amide bond (-CONR T -), urethane bond (-NH-COO-), and siloxane bond (-SiR T 2 -O-) n ) can be mentioned. Teach independently represents a hydrogen atom or a hydrocarbon group which may have a substituent, and n represents an integer of 1 or greater. The specific group may be a group related to an environmentally regulated substance. Such specific groups are not particularly limited, but examples thereof include halogenated alkyl groups (e.g., fluorinated alkyl groups) and groups containing a phthalate ester structure. The above-mentioned specific groups can be analyzed, for example, by mass spectrometry to obtain signal intensities. In mass spectrometry, the specific group may be detected as an ion of the specific group itself, or as one or more fragment ions derived from the specific group.
[0023] Examples of the specific organic molecule include organic molecules containing the specific group. The specific organic molecule can be analyzed by mass spectrometry, for example, to obtain signal intensities. In mass spectrometry, the specific organic molecule may be detected as an ion of the specific organic molecule itself, or as one or more fragment ions derived from the specific organic molecule.
[0024] The analyte is contained in the analytical sample and the standard sample film, and its chemical state etc. will be described later.
[0025] (Analytical Sample) The analytical sample is solid and contains the analyte described above. The analyte contained in the analytical sample may be one type or two or more types. The material constituting the analytical sample is not particularly limited as long as it is solid, and may be inorganic, organic, or a composite of an inorganic and an organic substance. Examples of inorganic substances include metals, semiconductors, metal oxides, metal nitrides, semiconductor oxides, semiconductor nitrides, composite oxides, composite nitrides, metal oxynitrides, and semiconductor oxynitrides. Examples of organic substances include resins and molecular organic compounds. The form of the analytical sample is also not particularly limited. Examples of the form of the analytical sample include powder, film, plate, and block. Alternatively, a method can be used in which a solution containing the analyte is placed on a standard sample film and the solvent component is removed to form a film or block. Alternatively, a method can be used in which a standard sample film-forming composition (described later) is placed on the analyte and the solvent component is removed to form a film or block. When the analytical sample does not have a flat surface, it is preferable to process the analytical sample to create a flat surface before obtaining the analytical laminate described below. For example, when the analytical sample is in a powder form, it is preferable to compact the powder so as to have a flat surface.
[0026] The analyte may be contained in the analytical sample, and the chemical state of the analyte contained in the analytical sample is not particularly limited. When the analyte is a specific element, examples of the chemical state of the specific element include a metallic state, an oxide state, a nitride state, a state bonded to an organic molecule, a metal salt state, and an ionized state. When the analyte is a specific group, examples of the chemical state of the specific group include a non-ionized state and an ionized state. Note that the specific group is usually contained in at least one of a molecular organic compound and a resin. When the analyte is a specific organic molecule, examples of the chemical state of the specific organic molecule include a non-ionized state and an ionized state.
[0027] (Standard sample membrane) The standard sample membrane contains an analyte, which will be described in detail later. The standard sample membrane contains an analyte contained in the analytical sample, or an analyte corresponding to the analyte contained in the analytical sample. An analyte corresponding to the analyte contained in the analytical sample refers to an analyte that has a different chemical state from the analyte contained in the analytical sample, and refers to an analyte that can obtain a signal similar to that of the analyte contained in the analytical sample using the analytical means described later. In operation X, a standard sample membrane with a known analyte content is used. The analyte content in the standard sample membrane can be measured using known means. When the standard sample membrane is produced using the means described later, the content of each component, such as the analyte, may be calculated from the amount of each component charged.
[0028] The standard sample film may contain an analyte contained in the analytical sample or an analyte corresponding to the analyte contained in the analytical sample, and the chemical state of the analyte contained in the standard sample film is not particularly limited. When the analyte is a specific element, the chemical state of the specific element may be, for example, a metallic state, an oxide state, a nitride state, a state bonded to an organic molecule, a metal salt state, or an ionized state, with the metal salt state being preferred. When the analyte is a specific group, the chemical state of the specific group may be, for example, a non-ionized state or an ionized state. Note that the specific group is usually contained in at least one of a molecular organic compound and a resin. When the analyte is a specific organic molecule, the chemical state of the specific organic molecule may be, for example, a non-ionized state or an ionized state.
[0029] The standard sample membrane is not particularly limited as long as it contains the analyte, but it is preferable that it contains a polymer as a component other than the analyte. The standard sample membrane may also contain a hydrocarbon. Preferred embodiments of the standard sample membrane are described below.
[0030] The standard sample membrane preferably contains a polymer. The type of polymer contained in the standard sample membrane is not particularly limited, but examples include water-insoluble polymers and water-soluble polymers. A water-soluble polymer is a polymer that dissolves in an amount of 1 g or more when dried at 105°C for 2 hours and then dissolved in 100 g of water at 25°C. A water-insoluble polymer refers to a polymer other than the water-soluble polymers described above. As will be described later, when preparing a standard sample membrane, it is preferable to use a water-soluble polymer when water is used, and it is preferable to use a water-insoluble polymer when an organic solvent is used.
[0031] Examples of polymers include (meth)acrylic polymers, styrene polymers, olefin polymers, polyester polymers, polyamide polymers, and cellulose polymers. (Meth)acrylic polymers are a general term for acrylic polymers and methacrylic polymers. The (meth)acrylic polymers, styrene polymers, olefin polymers, polyester polymers, and polyamide polymers exemplified above are often water-insoluble polymers.
[0032] A styrene-based polymer is a polymer that contains the largest amount of repeating units derived from styrene in terms of mass ratio among all repeating units. The content of repeating units derived from styrene in a styrene-based polymer is preferably 50% by mass or more, more preferably 70% by mass or more, and even more preferably 90% by mass or more, based on the total repeating units contained in the styrene-based polymer, in order to further suppress the variation in signal intensity depending on the measurement position of the standard sample film. The upper limit is not particularly limited, but may be 100% by mass.
[0033] A (meth)acrylic polymer is a polymer that contains repeating units derived from an alkyl acrylate and / or an alkyl methacrylate in the largest amount by mass of all repeating units. The (meth)acrylic polymer preferably contains repeating units derived from an alkyl (meth)acrylate having an alkyl group having 1 to 14 carbon atoms, in order to further suppress variation in signal intensity. The number of carbon atoms in the alkyl (meth)acrylate is preferably 2 to 14, more preferably 3 to 10, and even more preferably 3 to 8, in order to further suppress variation in signal intensity. The alkyl (meth)acrylate is a general term for alkyl acrylate and alkyl methacrylate.
[0034] Examples of the (meth)acrylic acid alkyl ester include methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, isopropyl (meth)acrylate, n-butyl (meth)acrylate, sec-butyl (meth)acrylate, 1,3-dimethylbutyl acrylate, pentyl (meth)acrylate, isopentyl (meth)acrylate, hexyl (meth)acrylate, 2-ethylbutyl (meth)acrylate, heptyl (meth)acrylate, n-octyl (meth)acrylate, isooctyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, n-nonyl (meth)acrylate, isononyl (meth)acrylate, n-decyl (meth)acrylate, isodecyl (meth)acrylate, n-dodecyl (meth)acrylate, n-tridecyl (meth)acrylate, and n-tetradecyl (meth)acrylate.
[0035] The content of repeating units derived from a (meth)acrylic acid alkyl ester having an alkyl group having 1 to 14 carbon atoms in the (meth)acrylic polymer is preferably 50% by mass or more, more preferably 70% by mass or more, and even more preferably 90% by mass or more, based on the total repeating units contained in the (meth)acrylic polymer, in order to further suppress variations in signal intensity. The upper limit is not particularly limited, but may be 100% by mass.
[0036] Olefin polymers are polymers that contain the largest amount of olefin-derived repeating units by mass among all repeating units. Examples of olefins include ethylene and propylene. Polyester polymers are polymers synthesized by dehydration condensation of polycarboxylic acids (dicarboxylic acids) and polyalcohols (diols) to form ester bonds. Examples of polyester polymers include polyethylene terephthalate, polyethylene naphthalate, and polybutylene terephthalate. Polyamide polymers are polymers formed by bonding multiple monomers via amide bonds. Examples of polyamide polymers include nylon 6 and nylon 6,6. Cellulose polymers are polymers with a cellulose skeleton. Examples of cellulose polymers include diacetyl cellulose and triacetyl cellulose.
[0037] The water-soluble polymer is preferably a polymer containing a repeating unit having at least one structure selected from the group consisting of a structure containing a hydroxy group, a structure containing a pyrrolidone ring, and a structure containing an oxyalkylene group.
[0038] Examples of water-soluble polymers containing hydroxy groups include gum arabic, soy gum, carboxymethyl cellulose, hydroxymethyl cellulose, hydroxyethyl cellulose, polyhydroxyethylated cellulose, hydroxypropyl cellulose, hydroxypropyl methylcellulose, glyoxalated hydroxypropyl methylcellulose, hydroxypropyl methylcellulose phthalate, methylcellulose, and polyvinyl alcohol.
[0039] Examples of water-soluble polymers containing a pyrrolidone ring include polyvinylpyrrolidone and copolymers of vinylpyrrolidone and vinyl acetate. Examples of water-soluble polymers containing an oxyalkylene group include polyalkylene glycols such as polyethylene glycol and polyoxyethylene polyoxypropylene glycol (also called polyoxyethylene-polyoxypropylene condensates), and polyoxyalkylene monoalkyl or aryl ethers such as poly(ethylene glycol) methyl ether and poly(ethylene glycol) phenyl ether.
[0040] Among these, the water-soluble polymer is preferably a water-soluble polymer or polysaccharide containing a pyrrolidone ring, more preferably a water-soluble polymer containing a pyrrolidone ring, and even more preferably polyvinylpyrrolidone. Examples of the polysaccharide include polysaccharides, polysaccharide derivatives, and alkali metal salts thereof. The cellulose-based polymer is preferably a compound in which at least a portion of the hydroxyl groups of cellulose are substituted with at least one selected from the group consisting of alkyl groups and hydroxyalkyl groups.
[0041] The content of the polymer in the standard sample film is not particularly limited, but in order to further suppress the variation in signal intensity, it is preferably 40% by mass or more, more preferably 60% by mass or more, even more preferably 80% by mass or more, and particularly preferably 90% by mass or more, relative to the total mass of the standard sample film. The upper limit is not particularly limited, but it is often less than 99% by mass, preferably 98% by mass or less, more preferably 97% by mass or less. The polymer may be used alone or in combination of two or more types. When two or more types of polymers are used in combination, it is preferable that the total content of the polymers is within the above range.
[0042] The standard sample film may contain a hydrocarbon. The type of hydrocarbon is not particularly limited, and examples include known hydrocarbons. The hydrocarbon may be a saturated hydrocarbon or an unsaturated hydrocarbon, with saturated hydrocarbons being preferred in that the variation in signal intensity depending on the measurement position on the standard sample film is further suppressed. The hydrocarbon may be an aliphatic hydrocarbon or an aromatic hydrocarbon, with aliphatic hydrocarbons being preferred in that the variation in signal intensity is further suppressed. The hydrocarbon may be linear or branched. It may also have a cyclic structure. The number of carbon atoms in the hydrocarbon is not particularly limited, but is preferably 5 or more, more preferably 10 or more, even more preferably 15 or more, and particularly preferably 20 or more, in that the variation in signal intensity is further suppressed. The upper limit is not particularly limited, but is often 40 or less, more often 30 or less.
[0043] As the hydrocarbon, aliphatic saturated hydrocarbons are preferred, aliphatic saturated hydrocarbons having 10 or more carbon atoms are more preferred, and paraffin is even more preferred, in that they further suppress variations in signal intensity. In this specification, paraffin means aliphatic saturated hydrocarbons having 15 or more carbon atoms.
[0044] The SP value of the hydrocarbon is not particularly limited, but a value of 14 to 18 MPa is preferred in order to further suppress the variation in signal intensity. 1/2 is preferable, and 15 to 17 MPa 1/2 The SP value is calculated as follows: Using a calculation program (HSPiP, ver. 4.1.07), the molecular structure of each material is input, and the HSP value (δ D , δ P , δ H ) is calculated. Next, the SP value is calculated using the following formula: SP value = (δ D 2 +δ P 2 +δ H 2 ) 1/2
[0045] The content of hydrocarbons in the standard sample film is not particularly limited, but in order to further suppress variations in signal intensity, it is preferably 1 to 60 mass % relative to the total mass of the standard sample film, more preferably 1 to 40 mass %, even more preferably 1 to 20 mass %, and particularly preferably 1 to 10 mass %. The hydrocarbons may be used alone or in combination of two or more. When two or more hydrocarbons are used in combination, it is preferable that the total content of the hydrocarbons is within the above range.
[0046] When the standard sample film contains hydrocarbons, the absolute value of the difference between the SP value of the polymer contained in the standard sample film and that of the hydrocarbon is 3.5 MPa. 1/2 The specific polymer may be a polymer having a SP value within 2.5 MPa (hereinafter, simply referred to as "specific polymer"). The specific polymer can be said to have good compatibility with hydrocarbons. The absolute value of the difference between the SP value of the specific polymer and the SP value of the hydrocarbon is 2.5 MPa or less, in terms of further suppressing the variation in signal intensity. 1/2 Preferably within 2.0 MPa 1/2 More preferably, within 1.5 MPa 1/2 Within 1.0 MPa is particularly preferred. 1/2 The lower limit of the absolute value of the difference is not particularly limited, but is preferably 0. The SP value of the specific polymer preferably satisfies the range of the absolute value of the difference, but is preferably 15 to 19 MPa in order to further suppress the variation in signal intensity. 1/2 is preferable, and 16 to 17 MPa 1/2 The SP value is calculated as follows: Using a calculation program (HSPiP, ver. 4.1.07), the molecular structure of each material (the structure of the repeating unit in a specific polymer) is input, and the HSP value (δ) is calculated using the HSP value (Hansen Solubility Parameter) calculation function included in the program. D , δ P , δ H ) is calculated. Next, the SP value is calculated using the following formula: SP value = (δ D 2 +δ P 2 +δ H 2 ) 1/2In addition, when the specific polymer contains a plurality of repeating units, the SP value of the specific polymer is calculated by multiplying the SP value of each repeating unit by the molar ratio of that repeating unit to all repeating units, and then summing the products. A Repeating unit A and SP B and repeating unit B, the molar ratio of repeating unit A to all repeating units is 0.2, and the molar ratio of repeating unit B to all repeating units is 0.8, the SP value of the specific polymer is calculated as follows: SP value of specific polymer=(SP A × 0.2) + (SP B ×0.8)
[0047] When the analyte contained in the analytical sample is a specific element, the standard sample film preferably contains a salt of the specific element. The salt of the specific element is preferably a metal salt, more preferably a metal salt of an inorganic acid or a metal salt of an organic acid, and even more preferably a metal salt of an organic acid. The salt of the specific element may also be a complex salt, as described below. When the analyte contained in the analytical sample is a specific element, the standard sample film may contain a complex containing the specific element. When the analyte contained in the analytical sample is a specific element, the standard sample film may contain solid particles containing the specific element.
[0048] A metal salt of an organic acid is a salt containing an organic acid and a metal element. Examples of organic acids contained in metal salts of organic acids include compounds having an acid group selected from the group consisting of a sulfonic acid group, a carboxylic acid group, a phosphoric acid group, a phenolic hydroxyl group, and a thiol group. Among these, compounds having a sulfonic acid group are preferred. The organic acid preferably has a hydrocarbon group (an aliphatic hydrocarbon group or an aromatic hydrocarbon group), more preferably an aliphatic hydrocarbon group, and even more preferably an alkyl group. The number of carbon atoms in the hydrocarbon group (an aliphatic hydrocarbon group or an alkyl group) is not particularly limited, but is preferably 5 or more. The organic acid may have both an aliphatic hydrocarbon group and an aromatic hydrocarbon group. As the organic acid, hydrocarbons having the acid group are preferred, and alkylarylsulfonic acids are more preferred, in terms of further suppressing variations in signal intensity. Preferred metal elements contained in metal salts include the metal elements listed as specific elements.
[0049] A metal salt of an inorganic acid is a salt containing an inorganic acid and a metal element. Examples of inorganic acids contained in the metal salt of an inorganic acid include hydrochloric acid, nitric acid, sulfuric acid, and phosphoric acid. Preferred examples of the metal element contained in the metal salt of an inorganic acid include the metal elements described above.
[0050] When the standard sample film contains a salt of a specific element, the content of the salt of the specific element is not particularly limited, but in order to further suppress variations in signal intensity, the concentration of the specific element derived from the salt of the specific element is preferably 0.1 to 1000 ppm by mass, more preferably 0.1 to 300 ppm by mass, relative to the total mass of the standard sample film. The concentration of the specific element derived from the salt of the specific element in the standard sample film means the concentration of the specific element contained in the salt of the specific element in the standard sample film. The salt of the specific element may be used alone, or two or more types may be used in combination. When two or more types of salts of specific elements with different types of specific elements are used in combination, it is preferable that the concentration of the specific element derived from each salt of the specific element be within the above range.
[0051] The complex containing the specific element is a compound containing the specific element and a ligand. Examples of the complex include, but are not limited to, aqua complexes, sulfide complexes, halide (e.g., fluoro, chloro, bromide, and iodide) complexes, hydride complexes, cyanate complexes, azide complexes, thiocyanate complexes, isothiocyanate complexes, nitro complexes, nitrite complexes, ammine complexes, amine complexes, diamine complexes, triamine complexes, tetramine complexes, pyridine complexes, diimine complexes, triimine complexes, porphyrin complexes, phthalocyanine complexes, phosphine complexes, and crown ether complexes. The complex containing the specific element may also bond with other ions to form a complex salt.
[0052] The solid particles containing the specific element are not particularly limited, but are preferably nanoparticles or nanofibers. In this specification, nanoparticles refer to particles having an average particle diameter of 1000 nm or less. In this specification, nanofibers refer to fibers having an average fiber diameter of 1000 nm or less and a ratio of average fiber length to average fiber diameter of 2 or more. The nanoparticles and nanofibers may contain the specific element, and may also contain elements other than the specific element. In other words, the nanoparticles and nanofibers may be made of compounds. Furthermore, the nanoparticles and nanofibers may have unevenly distributed elements, such as a core-shell structure. Specific examples of solid particles containing a specific element include, but are not limited to, copper particles, silver particles, gold particles, iron oxide particles, titanium oxide particles, zinc oxide particles, aluminum oxide (alumina) particles, indium tin oxide particles, cerium oxide (ceria) particles, cerium oxide-zirconium oxide (ceria-zirconia) particles, silicon particles, germanium particles, tin oxide particles, cadmium sulfide particles, zinc sulfide particles, cadmium sulfide-zinc sulfide particles, indium phosphide particles, copper sulfide-indium sulfide particles, lead sulfide particles, cadmium selenide particles, cadmium telluride particles, and silicon dioxide (silica) particles. The solid particles may be nanoparticles. Furthermore, among the solid particles containing a specific element, those that are semiconductor materials, have a core-shell structure, and have a particle size controlled to approximately several tens of nanometers are sometimes referred to as quantum dots. Examples of quantum dots include InP / ZnS, CdSe / ZnS, CdS / ZnS, and CdZnS / ZnS (described in the form of core material / shell material). As described above, the solid particles containing a specific element may be nanofibers. Examples of nanofibers include zinc oxide nanofibers, aluminum oxide nanofibers, and cerium oxide-zirconium oxide nanofibers.
[0053] When the analyte contained in the analytical sample is a specific group, the standard sample film preferably contains a compound having the specific group. The compound having the specific group may be a compound having a repeating unit or a compound without a repeating unit. As described above, the specific group may be a group related to an environmentally regulated substance, and the analyte may be an environmentally regulated substance. Environmentally regulated substances are not particularly limited, but examples include halogenated alkane compounds (e.g., fluorinated alkane compounds), halogenated alkyl ether compounds (e.g., fluorinated alkyl ether compounds), and phthalate ester compounds. The compound having the specific group preferably has good compatibility with other components contained in the standard sample film. When the standard sample film contains a compound having the specific group, the content of the compound having the specific group is not particularly limited. However, in order to further suppress variation in signal intensity, the content of the specific element in the compound having the specific group is preferably 0.1 to 10,000 ppm by mass, and more preferably 0.1 to 300 ppm by mass, relative to the total mass of the standard sample film.
[0054] Furthermore, the standard sample film preferably contains a component that functions as an internal standard. By including an internal standard in the standard sample film, fluctuations in sensitivity during measurement can be detected. The internal standard is preferably a component that generates a signal that does not interfere with the analyte in the analytical means described below. Furthermore, the internal standard is preferably a component that exhibits the same behavior as the analyte in the analytical means described below. For example, when the analyte is a specific element, an element that is not the analyte is preferably used as the internal standard. Specific examples of elements preferred as the internal standard include Bi (bismuth), Ho (holmium), In (indium), Rh (rhodium), Sc (scandium), Tb (terbium), and Y (yttrium). When the internal standard is an element, its chemical state is not particularly limited, and it may, for example, be ionized within the standard sample film.
[0055] The content of the internal standard in the standard sample film is not particularly limited, but is preferably 0.01 to 100 ppm by mass, more preferably 0.1 to 10 ppm by mass, relative to the total mass of the standard sample film. For example, when the internal standard is a specific metal element, the content of the metal element is preferably in the above range.
[0056] The standard sample film may contain a surfactant. When the standard sample film contains a surfactant, the type of surfactant is not particularly limited, and known surfactants may be used. Examples of surfactants include hydrocarbon surfactants, fluorine-based and / or silicon-based surfactants (specifically, fluorine-based surfactants, silicon-based surfactants, and surfactants having both fluorine atoms and silicon atoms), with fluorine-based and / or silicon-based surfactants (specifically, fluorine-based surfactants, silicon-based surfactants, and surfactants having both fluorine atoms and silicon atoms) being preferred. By including a surfactant in the standard sample film, coating defects (cissing, coating streaks, surface unevenness) can be suppressed when the film is formed by coating over a large area. Examples of hydrocarbon surfactants include acetylene-based surfactants such as Olfine D-10A, D-10PG, E1004, E1010, E1020, E1030W, PD-001, PD-002W, PD-004, PD-005, EXP. 4001, EXP. 4200, EXP. 4123, EXP. 4300, WE-001, WE-002, and WE-003 (manufactured by Nissin Chemical Industry Co., Ltd.). Examples of fluorine-based and / or silicone-based surfactants include those described in paragraph
[0276] of U.S. Patent Application Publication No. 2008 / 0248425. Surfactants other than the fluorine-based and / or silicone-based surfactants described in paragraph
[0280] of U.S. Patent Application Publication No. 2008 / 0248425 can also be used.Further, for example, Megafac F-251, F-253, F-410, F-477, F-551, F-552, F-553, F-554, F-555, F-556, F-557, F-558, F-559, F-560, F-561, F-562, F-563, F-565, F-568, F-569, F-570, F-572, F-575, F-576, R-40, R-40-LM, R-41 (manufactured by DIC Corporation), FC4432 (manufactured by Sumitomo 3M Limited), Surflon S-221, S-231, S-232, S-233, S S-241, S-242, S-243, S-420, S-431, S-386, S-611, S-647, S-651, S-653, S-656, S-693 (manufactured by AGC Seimi Chemical Co., Ltd.), PF-136A, PF-156A, PF-151N (manufactured by OMNOVA), Ftergent 100, 100C, 150, 150CH, 251, 212M, 215M, 250, 222F, 245F, 208G, DFX-18, 710FL, 710FM, 710FS, 610FM, 683 (manufactured by Neos Co., Ltd.) can also be used. These surfactants may be used alone or in combination of two or more. When the standard sample film contains a surfactant, the content of the surfactant is preferably 0.0001 to 2% by mass, more preferably 0.0005 to 1% by mass, relative to the standard sample film.
[0057] It is also preferable that the maximum height difference in the film thickness of the standard sample film is 0.50 μm or less. The maximum height difference in the film thickness of the standard sample film is more preferably 0.30 μm or less, even more preferably 0.20 μm or less, and particularly preferably 0.10 μm or less, in order to further suppress variations in signal intensity. There is no particular lower limit, but it is often 0.001 μm or more. The maximum height difference in the film thickness of the standard sample film is measured using the following method. The film thickness of the standard sample film is calculated using a stylus-type step gauge. The measurement distance is 3 mm, and the scanning speed is 0.02 mm / sec. The 3 mm straight line on which the first measurement was performed is designated as scanning line 1, and the second measurement is performed at a location 0.2 mm or more away from scanning line 1 in a direction perpendicular to scanning line 1. Similar measurements are then repeated, for a total of 10 measurements. Ten measurements (scans) are performed to determine the maximum and minimum film thickness values for each scan, and the difference (value A - value B) between the largest value A among the ten maximum values obtained by the ten scans and the smallest value B among the ten smallest values obtained by the ten scans is defined as the maximum film thickness difference.
[0058] The average thickness of the standard sample film is not particularly limited, but is preferably 3.5 μm or less, more preferably 2.5 μm or less, and even more preferably 2.0 μm or less, in order to further suppress variations in signal intensity. The lower limit of the average thickness is not particularly limited, but is preferably 0.05 μm or more, more preferably 0.1 μm or more, in terms of measurement accuracy. The average thickness is determined by measuring the thickness at any 20 points using a stylus profilometer and taking the arithmetic average.
[0059] The standard sample film may be subjected to the above-mentioned operation X while being laminated with a substrate, as described below. Examples of the substrate include those described below. Among these, an organic substrate made of an organic material is preferred, and a resin film is more preferred, in terms of facilitating improved measurement accuracy. When the standard sample film is subjected to operation X while being laminated with a substrate, it is preferable that the substrate does not contain the analyte described above or contains only a small amount of it. When the standard sample film is subjected to operation X while being laminated with a substrate, the total film thickness of the standard sample film and the substrate is preferably 100 μm or less, more preferably 50 μm or less, even more preferably 25 μm or less, particularly preferably 20 μm or less, particularly preferably 15 μm or less, even more preferably 10 μm or less, and most preferably 8 μm or less, in terms of further improving analytical accuracy. When the average value of the total film thickness of the standard sample film and the substrate (average film thickness) is within the above-mentioned preferred range, it is believed that the amount of ablation of the standard sample film during irradiation with laser light, as described below, is less likely to be uneven, thereby further improving analytical accuracy. Furthermore, from the viewpoint of ease of handling when the standard sample film is used in a laminated state with the substrate, the average value of the total film thickness of the standard sample film and the substrate (average film thickness) is preferably 0.1 μm or more, more preferably 0.2 μm or more, even more preferably 0.5 μm or more, particularly preferably 1.2 μm or more, particularly preferably 1.3 μm or more, even more preferably 2.0 μm or more, significantly preferably 3.0 μm or more, and most preferably 3.5 μm or more. The average film thickness can be measured in the same manner as for the standard sample film.
[0060] (Method for Producing Standard Sample Film) The method for producing a standard sample film is not particularly limited. When the analyte is a specific element and a metal salt of an organic acid is used as the salt of the specific element, an example of a method includes preparing a standard sample film-forming composition containing a polymer (particularly a water-insoluble polymer), a metal salt of an organic acid, other components used as needed (e.g., an internal standard, a hydrocarbon, and a surfactant), and an organic solvent, and applying the resulting standard sample film-forming composition to a substrate to form a standard sample film. When a metal salt of an inorganic acid is used as the salt of the specific element, an example of a method includes preparing a standard sample film-forming composition containing a polymer (particularly a water-soluble polymer), a metal salt of an inorganic acid, other components used as needed (e.g., an internal standard and a surfactant), and water or an aqueous solution containing an inorganic acid, and applying the resulting standard sample film-forming composition to a substrate to form a standard sample film. That is, an example of a method includes applying a standard sample film-forming composition containing at least a polymer, a source of a metal element, an internal standard, and a solvent to a substrate to form a standard sample film.
[0061] Among these, in terms of being able to produce standard sample films with good productivity, the absolute value of the difference between the SP values of hydrocarbons, metal salts of organic acids, and the hydrocarbons is 3.5 MPa. 1/2 The method for producing a standard sample film preferably includes a step of forming a standard sample film by applying a composition for forming a standard sample film containing a polymer having a molecular weight of 100 or less, an internal standard, and a solvent. The hydrocarbon and organic acid metal salts, and the internal standard are as described above.
[0062] The absolute value of the difference with the SP value of hydrocarbon is 3.5 MPa 1/2 The polymer (specific polymer) having a molecular weight of 1.0 or less is compatible with hydrocarbons. The specific polymer is as described above.
[0063] The content of the specific polymer contained in the standard sample film-forming composition is preferably adjusted to match the content of the polymer in the above-mentioned standard sample film. The content of the metal salt of an organic acid contained in the standard sample film-forming composition is preferably adjusted to match the content of the metal element in the above-mentioned standard sample film. The content of the internal standard contained in the standard sample film-forming composition is preferably adjusted to match the content of the internal standard in the above-mentioned standard sample film. The content of the hydrocarbon contained in the standard sample film-forming composition is preferably 1 to 60 mass%, more preferably 1 to 40 mass%, even more preferably 1 to 20 mass%, and particularly preferably 1 to 10 mass%, based on the total amount of the specific polymer, the metal salt of an organic acid, and the hydrocarbon.
[0064] The solvent contained in the standard sample film-forming composition may be any solvent capable of dissolving the various components described above. Examples of the solvent include organic solvents and water, with organic solvents being preferred. Examples of organic solvents include ketone solvents, alcohol solvents, ether solvents, hydrocarbon solvents, and ester solvents, with ketone solvents and ester solvents being preferred. Specific examples of the solvent include methyl ethyl ketone, butyl acetate, toluene, hexane, acetone, and chloroform. The solvent concentration in the standard sample film-forming composition is not particularly limited. However, in order to obtain a film with a highly uniform thickness, the solvent content relative to the total weight of the composition is preferably 60 to 99% by weight, more preferably 70 to 99% by weight.
[0065] The method for applying the standard sample film-forming composition onto the substrate is not particularly limited, and examples thereof include known methods (e.g., spin coating, dip coating, inkjet printing, etc.). The type of substrate is not particularly limited, and examples thereof include quartz, glass substrates, and silicon wafers, which have excellent flatness. Furthermore, resin films (e.g., polyethylene terephthalate films, polyethylene naphthalate films, polypropylene films, etc.) may be used as the substrate in terms of ease of handling. After applying the standard sample film-forming composition to the substrate, a drying treatment may be carried out, if necessary, to remove the solvent in the coating film. Examples of drying methods include heating. During the drying treatment, hydrocarbons may be removed by volatilization.
[0066] The substrate may be a temporary support. When the substrate is a temporary support, a transfer film is formed having the temporary support and the standard sample film placed on the temporary support. The standard sample film can be placed on the object to be transferred by contacting the standard sample film on the temporary support of this transfer film with the object to be transferred and then peeling off the temporary support. By using such a transfer film, the standard sample film can be placed on objects to be transferred of various shapes.
[0067] Examples of temporary supports include supports whose surfaces are treated with a release agent (e.g., a silicone-based release agent) and supports that themselves have releasability. A polymer substrate is preferred as the temporary support. Examples of materials constituting the temporary support include cellulose-based polymers, (meth)acrylic polymers, styrene-based polymers, olefin-based polymers, polyester-based polymers, and polyamide-based polymers. The water contact angle on the side of the temporary support on which the standard sample film is placed is not particularly limited, but is preferably 100 degrees or more in terms of better transferability of the standard sample film. Examples of methods for measuring the water contact angle include the sessile drop method described in JIS R 3257:1999. Specifically, the water contact angle is measured using a contact angle meter FTA1000 (software Fta32) (manufactured by First Ten Angstroms) at room temperature of 25°C and humidity of 50%. More specifically, 1.5 μl of pure water was dropped onto the surface of a temporary support kept horizontal, and after 30 seconds, the radius r and height h of the pure water droplet on the surface of the temporary support were determined, and the water contact angle θ was calculated using the formula θ = 2 arctan(h / r).
[0068] (Analytical Laminate) The analytical laminate is obtained by placing a standard sample membrane on a solid analytical sample containing an analyte. The method for placing the standard sample membrane on the analytical sample is not particularly limited, as long as the standard sample membrane is placed on the analytical sample. Specific methods for placing the standard sample membrane include a method of laminating the standard sample membrane on the analytical sample, a method of pressing and holding the standard sample membrane with a jig, and a method of placing the analytical sample on the standard sample. In the analytical laminate, it is preferable that the analytical sample and the standard sample membrane are placed in direct contact with each other. The analytical laminate may also be obtained by the method described in the fourth embodiment below (see Figures 3 and 4(a) to 4(d)).
[0069] The analytical laminate may contain a substrate (e.g., a resin substrate) used in preparing the standard sample film. When the analytical laminate contains the substrate used in preparing the standard sample film, the substrate is preferably disposed on the opposite side of the standard sample film from the analytical sample side.
[0070] The analytical laminate may be obtained in a state where it is held in a sample holder. Examples of sample holders include a support substrate having a recess into which an analytical sample is filled and an adhesive layer disposed on the surface of the recess except for the recess. Other examples include a support substrate having a through-hole into which an analytical sample is filled (see pellet frame 16 in FIG. 2 ) and an adhesive layer disposed on the surface except for the through-hole (see double-sided tape 18 in FIG. 2 ). In such a sample holder, the analytical sample is held in the recess or through-hole of the support substrate, and the adhesive layer holds the standard sample film in contact with the analytical sample.
[0071] The material constituting the support substrate of the sample holder is not particularly limited as long as it can hold the analytical sample, and known materials can be used. Examples of materials constituting the support substrate include paper, cellulose, plastic materials, metal, and glass. The shape of the recess or through-hole in the support substrate is not particularly limited and may be rectangular or circular. The shape of the recess or through-hole in the support substrate refers to the shape when observed from the normal direction of one surface of the support substrate. The size of the recess or through-hole in the support substrate is not particularly limited as long as it is wider than the area irradiated with laser light. When the recess or through-hole in the support substrate is circular, its diameter is, for example, 0.1 to 5.0 mm. Furthermore, the recess or through-hole in the support substrate preferably has a constant area in the thickness direction of the support substrate. By adopting the above-described embodiment, when the analytical sample is a powder sample, the powder sample can be easily compressed to a uniform density and held in the sample holder. The shape, size, and thickness of the support substrate can be selected appropriately.
[0072] The adhesive layer in the sample holder is not particularly limited as long as it can hold the standard sample film. In particular, it is preferable that the peel strength of the adhesive layer on the side in contact with the support substrate is greater than the peel strength of the side in contact with the standard sample film. By employing the adhesive layer of the above embodiment, the standard sample film can be easily peeled and removed from the sample holder after laser light irradiation, as described in detail below, and the volume of the analytical sample removed by laser light irradiation, as described in detail below, can be easily measured. Furthermore, by employing the adhesive layer of the above embodiment, the standard sample film can be easily reattached, resulting in excellent handleability. The peel strength of the adhesive layer on the side in contact with the standard sample film is preferably, for example, 0.1 N / 25 mm or less. The peel strength is measured by measuring the force required to peel a 25 mm wide film attached to an acrylic resin substrate in a 180-degree direction at a speed of 1200 mm / min. The material constituting the adhesive layer is not particularly limited, and for example, a material having known adhesive and pressure-sensitive adhesive properties can be employed. Examples of materials constituting the adhesive layer include acrylic resin, silicone resin, urethane resin, natural rubber, and synthetic rubber, with silicone resin being preferred because it easily satisfies the above-mentioned peel strength. For example, commercially available double-sided tape can also be used as the adhesive layer.
[0073] (Laser Light Irradiation) In operation X, the analytical laminate is irradiated with laser light. The laser light irradiation may be performed from the side of the analytical laminate where the standard sample film is placed, or from the side of the analytical laminate where the analytical sample is placed. The laser light irradiation is performed so that the standard sample film is ablated by the laser light and the analytical sample is also ablated by the laser light, in order to obtain signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample. That is, when the laser light irradiation is performed from the side of the analytical laminate where the standard sample film is placed, the laser light irradiation is performed so that the standard sample film is ablated to form a through-hole, and the laser light is irradiated through the through-hole to ablate the analytical sample. When the laser light irradiation is performed from the side of the analytical laminate where the analytical sample is placed, the laser light irradiation is performed so that the standard sample is ablated to form a through-hole, and the laser light is irradiated through the through-hole to ablate the standard sample film.
[0074] FIG. 1 illustrates laser light irradiation when the laser light is irradiated from the side of the analytical laminate where the standard sample film is placed. FIGS. 1(a) and 1(b) are schematic cross-sectional views of an analytical laminate 20, in which a standard sample film 12 and an analytical sample 14 are stacked. First, as shown in FIG. 1(a), laser light 30 is irradiated from the side of the analytical laminate 20 where the standard sample film 12 is placed. The irradiation of the laser light 30 ablates the standard sample film 12 and the analytical sample 14, creating a through-hole in the standard sample film 12 as shown in FIG. 1(b). Furthermore, a portion of the analytical sample 14 is removed, generating an ablated sample 22. For example, when the analytical means described below is LA-ICP-MS, the ablated sample 22 is introduced into the detector of the analytical means. Laser light irradiation may also be performed from the side of the analytical laminate where the analytical sample is placed, and can be performed in a similar manner to the method described above.
[0075] The method of irradiating the standard sample film with laser light is not particularly limited, but it is preferable to repeatedly irradiate the same area with pulsed laser light to ablate the analytical sample. The wavelength of the irradiated laser light is not particularly limited, but is preferably 200 to 300 nm, more preferably 230 to 260 nm, in order to further suppress variations in signal intensity. The pulse intensity of the irradiated laser light is not particularly limited, but is preferably 5.0 to 20.0 J / cm in order to further suppress variations in signal intensity. 2 is preferred, and 12.0 to 18.0 J / cm 2 is more preferable. The pulse width of the irradiated laser light is not particularly limited, but is preferably 200 to 300 fs, more preferably 230 to 250 fs, in terms of further suppressing variations in signal intensity. The frequency of the irradiated laser light is not particularly limited, but is preferably 5000 to 20000 Hz, more preferably 8000 to 12000 Hz, in terms of further suppressing variations in signal intensity. The irradiation time of the laser light is not particularly limited, but is preferably 0.5 to 3.0 seconds, more preferably 1.5 to 2.5 seconds, in terms of further suppressing variations in signal intensity. The irradiation area of the laser light is not particularly limited, but is often an area of 0.1 to 1.0 mm in length and 0.1 to 1.0 mm in width.
[0076] Laser light irradiation may be performed on a plurality of positions on the analytical laminate, the signal intensity at each position may be obtained, and the signal intensity obtained may be arithmetically averaged to obtain the signal intensity detected in operation X. When laser light irradiation is performed on a plurality of positions on the analytical laminate, it is preferable that the regions irradiated with the laser light are spaced apart from each other by approximately the length of one side of the irradiated region. Furthermore, when laser light irradiation is performed on a plurality of positions on the analytical laminate, the number of irradiated positions is not particularly limited, but is usually 5 to 20.
[0077] (Signal Intensity) In operation X, the analytical laminate is irradiated with laser light, and the signal intensity derived from the analyte in the standard sample film and the analyte in the analytical sample is detected. The signal intensity can be obtained by various analytical means. Examples of analytical means include a method of analyzing the light emission generated by laser light irradiation using a spectroscopic analyzer, a method of analyzing the light emission generated when gas or particles derived from the standard sample film and analytical sample ablated by laser light irradiation are introduced into inductively coupled plasma using a spectroscopic analyzer, and a method of introducing the gas or particles derived from the standard sample film and analytical sample ablated by laser light irradiation into inductively coupled plasma, ionizing them, and analyzing them with a mass spectrometer. The method of analyzing the light emission generated by laser light irradiation using a spectroscopic analyzer is also called laser-induced breakdown spectroscopy (LIBS). The method of analyzing the light emission generated when gas or particles derived from the standard sample film and analytical sample ablated by laser light irradiation are introduced into inductively coupled plasma using a spectroscopic analyzer is also called laser ablation inductively coupled plasma optical emission spectroscopy (LA-ICP-OES). The method of introducing gases or particles derived from a standard sample film and an analytical sample, which are ablated by laser irradiation, into an inductively coupled plasma, ionizing them, and analyzing them with a mass spectrometer is also called laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS).
[0078] With LIBS, the luminescence intensity derived from the analyte is obtained as the signal intensity. With LA-ICP-OES, the luminescence intensity derived from the analyte is obtained as the signal intensity. With LA-ICP-MS, the ion intensity derived from the analyte is obtained as the signal intensity. In the above-mentioned analysis means, analysis is performed continuously for a time period corresponding to the time of laser light irradiation, and the average value per time is taken as the signal intensity. Furthermore, when the standard sample film contains an internal standard, the signal intensity derived from the analyte may be corrected based on the signal intensity derived from the internal standard. For example, a value obtained by dividing the signal intensity derived from the analyte by the signal intensity derived from the internal standard may be used as the signal intensity value obtained in Operation 1 described below to create a regression equation. The above-mentioned signal intensity is preferably a signal intensity obtained by mass spectrometry. More specifically, the above-mentioned signal intensity is preferably a signal intensity obtained by LA-ICP-MS.
[0079] When the analytical laminate contains two or more types of analytes, the signal intensities from the two or more types of analytes may be obtained simultaneously, or the signal intensities from the analytes may be obtained one by one.
[0080] [Operation 1 and Creation of Regression Equation] As described above, in the first embodiment of the analytical method of the present invention, the following operation 1 is performed. Operation 1: A standard sample film containing an analyte is placed on a solid analytical sample containing the analyte to obtain an analytical laminate, and operation X, in which laser light is irradiated onto the analytical laminate and signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample are detected, is performed two or more times while changing the concentration of the analyte in the standard sample film. That is, operation X is performed on two or more analytical laminates containing different concentrations of the analyte in the standard sample film, and signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample are detected. In operation 1, the number of analytical laminates containing standard sample films containing different concentrations of the analyte for which operation X is performed is two or more, but the number of analytical laminates containing standard sample films containing different concentrations of the analyte for which operation X is performed can be adjusted depending on the desired analytical accuracy. The number of analytical laminates for which operation X is performed, which contain standard sample films with different concentrations of the analyte, is preferably 3 to 20, more preferably 5 to 20, and even more preferably 5 to 10, from the viewpoint of analytical accuracy.
[0081] Next, a regression equation is created based on the signal intensity value obtained in operation 1 and the amount of analyte contained in the standard sample film removed by laser light irradiation. The amount of analyte contained in the standard sample film removed by laser light irradiation can be calculated from the volume of the standard sample film removed by laser light irradiation and the known content of the analyte in the standard sample film. The volume of the standard sample film removed by laser light irradiation can be calculated from the previously measured film thickness of the standard sample film and the area of the region of the standard sample film removed by laser light irradiation. The method for measuring the film thickness of the standard sample film is as described above. The area of the region of the removed standard sample film can be calculated, for example, by measuring the shape. The shape measurement can be performed on the analytical laminate after laser light irradiation, and can be performed using, for example, an optical microscope, an optical interferometer, or a stylus profilometer. The content of the analyte in the standard sample film can be controlled by the amount of analyte added during the formation of the standard sample film. The content of the analyte in the standard sample film used can be adjusted appropriately depending on the content of the analyte in the analytical sample.
[0082] In operation 1, when the content of the analyte in the standard sample film is plotted on the horizontal axis and the signal intensity on the vertical axis, two or more plots are drawn, and a regression equation can be created based on these plots. The regression equation can be created, for example, by linear regression. For example, when the regression equation is created by linear regression, the absolute value of the value at the intersection of the regression equation line and the horizontal axis is the amount of the analyte in the analytical sample removed by laser light irradiation. Note that if operation X is performed three or more times in operation 1, the regression equation can be created by determining coefficients, etc., using the above plots by the least squares method, etc.
[0083] Furthermore, the concentration of the analyte in the analytical sample can be calculated from the amount of the analyte in the analytical sample removed by laser light irradiation and the amount of the analytical sample removed by laser light irradiation. For example, the volume of the analytical sample removed by laser light irradiation can be used as the amount of the analytical sample removed by laser light irradiation, and the volume density of the analyte in the analytical sample can be calculated. The volume of the analytical sample removed by laser light irradiation can be calculated by performing the shape measurement method described above on the analytical laminate after laser light irradiation. Furthermore, by calculating the volume density of the analyte in the analytical sample and then separately measuring the density of the analytical sample, the mass density of the analyte in the analytical sample can be calculated. Known methods can be used to measure density.
[0084] The coefficients and the like in the regression equation obtained by the above procedure may be corrected by the amount of analytical sample removed by laser light irradiation. A specific procedure, for example, is to first determine the coefficients and the like in the regression equation without correcting for the amount of analytical sample removed by laser light irradiation. Next, the determined amount of the analyte in the analytical sample removed by laser light irradiation is compared with the amount of analytical sample ablated in the analytical sample, and the signal intensity on the vertical axis is corrected. The coefficients and the like in the regression equation are again determined based on the corrected signal intensity. Note that the correction for the amount of analytical sample removed by laser light irradiation may be performed by a method other than the above.
[0085] When the analytical laminate contains two or more analytes, a regression equation is created for each analyte using the above procedure, and the amount of each analyte in the analytical sample is calculated.
[0086] <Second Embodiment> In a second embodiment of the analytical method of the present invention, the following operation 2 is carried out, a regression equation is created based on the obtained signal intensity value and the amount of the analyte contained in the standard sample film removed by laser light irradiation, and the regression equation is used to calculate the amount of the analyte in a solid analytical sample containing the analyte removed by laser light irradiation. Operation 2: Operation X is carried out at least once, and at least operation Y, in which the analytical sample is irradiated with laser light and the signal intensity derived from the analyte in the analytical sample is detected. Operation X is as described in the first embodiment, so a description thereof will be omitted. Operation Y will be described below.
[0087] [Procedure Y] In procedure Y, the analytical sample is irradiated with laser light to detect the signal intensity derived from the analyte in the analytical sample. The analytical sample and the analyte are as described in the first embodiment. Procedure Y differs from procedure X in that the analytical sample is directly irradiated with laser light, in which the analytical laminate is irradiated with laser light, but is otherwise similar to procedure X. The preferred conditions for laser light irradiation are the same as those in procedure X. Furthermore, the preferred mode for detecting the signal intensity is also the same as procedure X.
[0088] [Operation 2 and Creation of Regression Equation] As described above, in the second embodiment of the analytical method of the present invention, the following operation 2 is performed. Operation 2: Operation X is performed at least once, and at least operation Y, in which the analytical sample is irradiated with laser light and the signal intensity derived from the analyte in the analytical sample is detected. That is, in operation 2, operation X is performed one or more times on the analytical laminate, and operation Y is performed on the analytical sample. In operation X, the signal intensity derived from the analyte in the standard sample film and the analyte in the analytical sample is detected, and operation Y, in which the signal intensity derived from the analyte in the analytical sample is detected. In operation 2, operation X is performed on one or more analytical laminates, but operation X may also be performed on two or more analytical laminates in which the standard sample film has a different analyte concentration. The number of analytical laminates in which operation X is performed on the standard sample film has a different analyte concentration can be adjusted depending on the desired analytical accuracy. The number of analytical laminates with different concentrations of the analyte in the standard sample membranes for performing operation X is preferably 3 to 20, more preferably 5 to 20, and even more preferably 5 to 10, from the viewpoint of analytical accuracy.
[0089] Next, a regression equation is created based on the signal intensity value obtained in operation 2 and the amount of analyte contained in the standard sample film removed by laser light irradiation. The amount of analyte contained in the standard sample film removed by laser light irradiation can be calculated in the same manner as in operation 1. Here, the amount of analyte contained in the standard sample film removed by laser light irradiation in operation Y is set to 0. The content of the analyte in the standard sample film can be controlled by the amount of analyte added when forming the standard sample film. The content of the analyte in the standard sample film used can be adjusted appropriately depending on the content of the analyte in the analytical sample.
[0090] In operation 2, when the content of the analyte in the standard sample film is plotted on the horizontal axis and the signal intensity on the vertical axis, two or more plots are drawn, and a regression equation can be created based on these plots. The regression equation can be created, for example, by linear regression. When the regression equation is created by linear regression, the absolute value of the value at the intersection of the regression equation line and the horizontal axis is the amount of the analyte in the analytical sample removed by laser light irradiation. Note that if operation X is performed two or more times in operation 2, the regression equation can be created by determining coefficients, etc., using the above plots by the least squares method, etc.
[0091] Furthermore, the concentration of the analyte in the analytical sample can be calculated from the amount of the analyte in the analytical sample removed by laser light irradiation and the amount of the analytical sample removed by laser light irradiation. For example, the volume of the analytical sample removed by laser light irradiation can be used as the amount of the analytical sample removed by laser light irradiation, and the volume density of the analyte in the analytical sample can be calculated. The volume of the analytical sample removed by laser light irradiation can be calculated by performing the shape measurement method described above on the analytical laminate after laser light irradiation. Furthermore, by calculating the volume density of the analyte in the analytical sample and then separately measuring the density of the analytical sample, the mass density of the analyte in the analytical sample can be calculated. Known methods can be used to measure density.
[0092] The coefficients in the regression equation obtained by the above procedure may be corrected based on the amount of the analytical sample removed by laser light irradiation. The correction method may be the same as that in the first embodiment.
[0093] When the analytical laminate contains two or more analytes, a regression equation is created for each analyte using the above procedure, and the amount of each analyte in the analytical sample is calculated.
[0094] <Third Embodiment> In a third embodiment of the analytical method of the present invention, the following operation 3 is performed, a regression equation is created based on the obtained signal intensity value and the amount of the analyte contained in the standard sample film removed by laser light irradiation, and the regression equation is used to calculate the amount of the analyte in the solid analytical sample containing the analyte removed by laser light irradiation. Operation 3: Operation X is performed at least once, and at least operation Z is performed in which an analyte-free reference sample film is placed on the analytical sample to obtain a reference laminate, and the reference laminate is irradiated with laser light to detect the signal intensity derived from the analyte in the analytical sample. Operation X is as described in the first embodiment, so a description thereof will be omitted. Operation Z will be described below.
[0095] [Operation Z] In operation Z, a reference sample film not containing the analyte is placed on the analytical sample to obtain a reference laminate, and the reference laminate is irradiated with laser light to detect the signal intensity derived from the analyte in the analytical sample. The analytical sample and analyte are as described in the first embodiment. Operation Z differs from operation X in that the reference laminate is irradiated with laser light, but is otherwise similar to operation X. The preferred conditions for laser light irradiation are the same as in operation X. Furthermore, the preferred mode for detecting the signal intensity is also the same as operation X.
[0096] (Reference Laminate) The reference laminate is similar to the analytical laminate except that a reference sample film is used instead of the standard sample film, and therefore a description thereof will be omitted.
[0097] (Reference sample membrane) The reference sample membrane used to obtain the reference laminate is the same as the standard sample membrane described above, except that it is substantially free of the analyte. Note that in the reference sample membrane, being substantially free of the analyte means that in a method for detecting signal intensity, no signal intensity derived from the analyte is detected. Preferred aspects of the reference sample membrane are the same as the preferred aspects of the standard sample membrane, except that it does not contain the analyte. Note that the reference sample membrane may be produced without adding the analyte in the production method for the standard sample membrane described above.
[0098] [Operation 3 and Creation of Regression Equation] As described above, in the third embodiment of the analytical method of the present invention, the following operation 3 is performed. Operation 3: Operation X is performed at least once, and at least operation Z is performed in which an analyte-free reference sample film is placed on an analytical sample to obtain a reference laminate, and laser light is irradiated onto the reference laminate to detect the signal intensity derived from the analyte in the analytical sample. That is, in operation 3, operation X is performed one or more times on the analytical laminate, and operation Z is performed on the reference laminate. In operation X, signal intensities derived from the analyte in the standard sample film and the analyte in the analytical sample are detected, and operation Z detects the signal intensity derived from the analyte in the analytical sample. In operation 3, operation X is performed on one or more analytical laminates, but operation X may also be performed on two or more analytical laminates with different analyte concentrations in the standard sample film. The number of analytical laminates with different analyte concentrations in the standard sample film to which operation X is performed can be adjusted depending on the desired analytical accuracy. The number of analytical laminates with different concentrations of the analyte in the standard sample membranes for performing operation X is preferably 3 to 20, more preferably 5 to 20, and even more preferably 5 to 10, from the viewpoint of analytical accuracy.
[0099] Next, a regression equation is created based on the signal intensity value obtained in operation 3 and the amount of analyte contained in the standard sample film removed by laser light irradiation. The amount of analyte contained in the standard sample film removed by laser light irradiation can be calculated in the same manner as in operation 1. Here, the amount of analyte contained in the standard sample film removed by laser light irradiation in operation Z is set to 0. The content of the analyte in the standard sample film can be controlled by the amount of analyte added when forming the standard sample film. The content of the analyte in the standard sample film used can be adjusted appropriately depending on the content of the analyte in the analytical sample.
[0100] In operation 3, when the content of the analyte in the standard sample film is plotted on the horizontal axis and the signal intensity on the vertical axis, two or more plots are drawn, and a regression equation can be created based on these plots. The regression equation can be created, for example, by linear regression. When the regression equation is created by linear regression, the absolute value of the value at the intersection of the regression equation line and the horizontal axis is the amount of the analyte in the analytical sample removed by laser light irradiation. Note that if operation X is performed two or more times in operation 3, the regression equation can be created by determining the coefficients using the least squares method or the like using each of the above plots.
[0101] Furthermore, the concentration of the analyte in the analytical sample can be calculated from the amount of the analyte in the analytical sample removed by laser light irradiation and the amount of the analytical sample removed by laser light irradiation. For example, the volume of the analytical sample removed by laser light irradiation can be used as the amount of the analytical sample removed by laser light irradiation, and the volume density of the analyte in the analytical sample can be calculated. The volume of the analytical sample removed by laser light irradiation can be calculated by performing the shape measurement method described above on the analytical laminate after laser light irradiation. Furthermore, by calculating the volume density of the analyte in the analytical sample and then separately measuring the density of the analytical sample, the mass density of the analyte in the analytical sample can be calculated. Known methods can be used to measure density.
[0102] The coefficients in the regression equation obtained by the above procedure may be corrected based on the amount of the analytical sample removed by laser light irradiation. The correction method may be the same as that in the first embodiment.
[0103] When the analytical laminate contains two or more analytes, a regression equation is created for each analyte using the above procedure, and the amount of each analyte in the analytical sample is calculated.
[0104] <Fourth Embodiment> In a fourth embodiment of the analytical method of the present invention, the following procedure 4 is carried out, a regression equation is created based on the obtained signal intensity value and the amount of the analyte contained in the standard sample film removed by laser light irradiation, and the regression equation is used to calculate the amount of the analyte in the solid analytical sample containing the analyte removed by laser light irradiation. Procedure 4: The above procedure X is carried out two or more times while changing the number or thickness of the stacked standard sample films. Procedure X is as explained in the first embodiment, so its explanation is omitted.
[0105] [Operation 4 and Creation of Regression Equation] As described above, in the fourth embodiment of the analytical method of the present invention, the following operation 4 is performed. Operation 4: The above operation X is performed two or more times while changing the number of stacked standard sample membranes or the thickness of the standard sample membrane. That is, operation X is performed for two or more analytical laminates having different numbers of stacked standard sample membranes or different thicknesses, and signal intensities derived from the analyte in the standard sample membrane and the analyte in the analytical sample are detected. In operation 4, the number of analytical laminates having different numbers of stacked standard sample membranes or different thicknesses for which operation X is performed is two or more, but the number of analytical laminates having different numbers of stacked standard sample membranes or different thicknesses for which operation X is performed can be adjusted depending on the desired analytical precision. The number of analytical laminates having different concentrations of the analyte contained therein for which operation X is performed is preferably 3 to 20, more preferably 5 to 20, and even more preferably 5 to 10, from the viewpoint of analytical precision.
[0106] Next, a regression equation is created based on the signal intensity value obtained in operation 4 and the amount of analyte contained in the standard sample film removed by laser light irradiation. The amount of analyte contained in the standard sample film removed by laser light irradiation can be calculated from the volume of the standard sample film removed by laser light irradiation and the known content of the analyte in the standard sample film. The volume of the standard sample film removed by laser light irradiation can be calculated from the previously measured film thickness of the standard sample film and the area of the region of the standard sample film removed by laser light irradiation. The method for measuring the film thickness of the standard sample film is as described above. The area of the region of the removed standard sample film can be calculated, for example, by measuring the shape. The shape measurement can be performed on the analytical laminate after laser light irradiation, and can be performed using, for example, an optical microscope, an optical interferometer, or a stylus profilometer. The content of the analyte in the standard sample film can be controlled by the number of standard sample films stacked or the thickness of the standard sample film. Changing the number of stacked standard sample films or the thickness of the standard sample film changes the amount of analyte contained per unit area of the standard sample film, making it possible to control the amount of analyte contained in the standard sample film removed by laser light irradiation. That is, in operation 4, it is preferable to obtain an analytical laminate so that the amount of analyte contained per unit area of the standard sample film varies. Furthermore, as explained in the first embodiment, the content of the analyte in the standard sample film can be controlled by the amount of analyte added during film formation of the standard sample film. The content of the analyte in the standard sample film used can be adjusted appropriately depending on the content of the analyte in the analytical sample.
[0107] In step 4, when the analytical laminate is obtained by varying the number of standard sample films stacked, the analytical laminate may be obtained by stacking standard sample films with different analyte concentrations and / or different thicknesses. For example, standard sample films with the same thickness and analyte concentration may be stacked, or standard sample films with the same thickness but different analyte concentrations may be stacked. Furthermore, standard sample films with different thicknesses but the same analyte concentration may be stacked, or standard sample films with different thicknesses and analyte concentrations may be stacked. Laminating standard sample films with the same thickness and analyte concentration is simpler and more preferable because only one type of standard sample film needs to be prepared. The number of standard sample films stacked is not particularly limited, but 2 to 10 films is preferred. The amount of analyte contained per unit area of the standard sample film can be controlled by the number of standard sample films stacked, the analyte concentration in the standard sample film to be stacked, and the thickness of the standard sample film. In operation 4, the concentration of the analyte in the standard sample film and the preferred thickness of the standard sample film are the same as the preferred ranges for the standard sample film explained in the first embodiment.
[0108] In operation 4, when laminating the standard sample film, the standard sample film may be laminated on a substrate, as described in the first embodiment. Alternatively, the standard sample film may be placed on the analyte with the standard sample film and substrate (temporary support) laminated together, and the substrate (temporary support) may be peeled off before laminating another standard sample film. Alternatively, the standard sample film may be laminated using perforated adhesive tape according to the following procedure. An example of the procedure for laminating standard sample films will be described below with reference to the drawings. Figure 3 is a top view of a perforated adhesive tape 52 used in one embodiment in which the number of laminated standard sample films is varied. The perforated adhesive tape 52 in Figure 3 is an adhesive tape with an adhesive layer disposed on one side and has a circular hole H. Known adhesive tapes can be used as the perforated adhesive tape 52, and commercially available products can also be used. The shape of the hole H in the perforated adhesive tape 52 is not particularly limited and may be rectangular or have other shapes. 3, there is only one hole H, but multiple holes may be provided. The size of hole H is preferably larger than the area irradiated with laser light in operation X. The area irradiated with laser light is as described in the first embodiment. Hole H can be formed by a known method, for example, by punching with a blade, or by cutting out a part of the adhesive tape with a cutter or the like.
[0109] Figure 4 is a cross-sectional schematic diagram showing one embodiment of a procedure for changing the number of stacked standard sample films. First, as shown in Figure 4(a), a standard sample film 12c is placed on one surface of a temporary support 12d, and a perforated adhesive tape 52 is attached to the surface of the standard sample film 12c opposite the temporary support 12d. After the perforated adhesive tape 52 is attached to the standard sample film 12c, as shown in Figure 4(b), the perforated adhesive tape 52 is pulled in the direction opposite the temporary support 12d, and peeled off at the interface between the standard sample film 12c and the temporary support 12d. When the standard sample film 12c is peeled off at the interface between the standard sample film 12c and the temporary support 12d, the standard sample film 12c and the perforated adhesive tape 52 are laminated together (see Figure 4(c)). Next, the laminate of the standard sample film 12c and the perforated adhesive tape 52 is attached to the analytical sample 14c. The laminate is attached so that the standard sample film 12c and the analytical sample 14c come into contact (see FIG. 4(d)). The lamination of the laminate results in an analytical laminate 20a that can be used in operation X. After the analytical laminate 20a shown in FIG. 4(d) is obtained, the above-mentioned laminate (a laminate comprising the standard sample film 12c and the perforated adhesive tape 52) is further laminated to obtain an analytical laminate 20b with the standard sample film 12c laminated thereon (see FIG. 4(e)). Repeated lamination of the above-mentioned laminates allows for the number of standard sample films to be varied. Furthermore, in the resulting analytical laminate (analytical laminate 20a or analytical laminate 20b), laser light can be irradiated directly onto the standard sample film 12c through the holes in the perforated adhesive tape 52. The lamination of the above-mentioned laminate onto the analytical laminate 20a shown in FIG. 4(d) may be performed after removing the perforated adhesive tape 52. When removing the perforated adhesive tape 52, it is preferable to make cuts in the standard sample film 12c along the shape of the holes in the perforated adhesive tape 52 (see hole H in Figure 3), so that the standard sample film 12c having the same shape as the holes in the perforated adhesive tape 52 is laminated on the analytical sample 14c.
[0110] In addition, in FIG. 4(e), the standard sample film 12c on the side to be laminated and the standard sample film 12c on the side laminated on the analytical sample 14c are arranged so that they completely overlap when viewed in the thickness direction. However, the standard sample films 12c may be arranged so that only a portion of the film overlaps when viewed in the thickness direction. Arranging the standard sample films 12c so that only a portion of the film overlaps can form areas where two standard sample films 12c overlap and areas where the standard sample films 12c do not overlap. Furthermore, the standard sample films may be laminated using perforated adhesive tape with holes of different shapes. More specifically, as shown in FIG. 5, the standard sample film 12e may be laminated on the analytical sample 14c using a perforated adhesive tape 52a with two holes, and then the standard sample film 12c may be laminated using a perforated adhesive tape 52 with one hole to obtain the analytical laminate 20c. When the standard sample films are laminated in the manner shown in Fig. 5, two standard sample films (standard sample film 12e and standard sample film 12c) are laminated in the region on the right side of Fig. 5, and one standard sample film (standard sample film 12e) is present in the region on the left side of Fig. 5. With such an analytical laminate 20c, operation 4 can be easily performed by changing the region to be irradiated with laser light. Note that the analytical laminate 20c shown in Fig. 5 is an embodiment obtained by laminating the standard sample film 12c without removing the perforated adhesive tape 52a, but the analytical laminate may also be obtained by removing the perforated adhesive tape 52a.
[0111] The perforated adhesive tape 52 used in the procedure described with reference to FIG. 4 may have other configurations. For example, instead of the perforated adhesive tape 52, the adhesive tapes shown in FIGS. 6(a) to 6(d) may be used. The adhesive tape 54a shown in FIG. 6(a) has adhesive tape in a region of a predetermined width from three sides of a rectangular area from which the standard sample film is to be peeled. When the standard sample film is peeled using the adhesive tape 54a shown in FIG. 6(a), the standard sample film is peeled off with the region A1, which is the region surrounded by the solid and dotted lines, exposed. The adhesive tape 54b shown in FIG. 6(b) has adhesive tape in a region of a predetermined width from two sides of a rectangular area from which the standard sample film is to be peeled. When the standard sample film is peeled off using adhesive tape 54b shown in Fig. 6(b), the standard sample film is peeled off in area A2, which is the area surrounded by the solid and dotted lines. When the area from which the standard sample film is peeled off is rectangular, adhesive tape 54c shown in Fig. 6(c) has adhesive tape in an area of a predetermined width from one side of the rectangle. When the standard sample film is peeled off using adhesive tape 54c shown in Fig. 6(c), the standard sample film is peeled off in area A3, which is the area surrounded by the solid and dotted lines.
[0112] Although the regions A1 to A3 of the standard sample film that are peeled off by the adhesive tapes 54a to 54c are rectangular in shape in Fig. 6, they may have shapes other than those shown in Fig. 6. Examples of the shapes of the regions include a rectangle with one or more rounded corners, a polygon, a semicircle, a sector, and an ellipse.
[0113] The adhesive tape 54d shown in Fig. 6(d) is an embodiment in which, when the region from which the standard sample film is to be peeled is rectangular, the adhesive tape is provided in a region of a predetermined width on a part of one side of the rectangle. When the standard sample film is peeled using the adhesive tape 54d shown in Fig. 6(d), the standard sample film is peeled from the region A4, which is the region surrounded by the solid line and the dotted line.
[0114] Although the adhesive tape 54d has a rectangular shape, it may have a shape other than that shown in Fig. 6. Examples of shapes of the adhesive tape other than those described above include a rectangular shape with one or more rounded corners, a polygonal shape, a circle, an ellipse, a semicircle, and a fan shape.
[0115] Furthermore, the adhesive tape used to peel off the standard sample membrane (for example, the perforated adhesive tape 52, perforated adhesive tape 52a, and adhesive tapes 54a to 54d) may have an area that does not come into contact with the standard sample membrane. If the area that does not come into contact with the standard sample membrane is provided, the standard sample membrane can be easily peeled off from the support by gripping that area.
[0116] Furthermore, in operation 4, when the thickness of the standard sample film is changed to obtain an analytical laminate, the concentration of the analyte in the standard sample film may be different. The amount of the analyte contained per unit area of the standard sample film can be controlled by the concentration of the analyte in the standard sample film and the thickness of the standard sample film. In operation 4, the preferred thickness of the standard sample film is the same as the preferred thickness of the standard sample film described in the first embodiment.
[0117] In operation 4, when the content of the analyte in the standard sample film is plotted on the horizontal axis and the signal intensity on the vertical axis, two or more plots are drawn, and a regression equation can be created based on these plots. The regression equation can be created, for example, by linear regression. For example, when the regression equation is created by linear regression, the absolute value of the value at the intersection of the regression equation line and the horizontal axis is the amount of the analyte in the analytical sample removed by laser light irradiation. Note that if operation X is performed three or more times in operation 4, the regression equation can be created by determining coefficients, etc., using the above plots by the least squares method, etc.
[0118] Furthermore, the concentration of the analyte in the analytical sample can be calculated from the amount of the analyte in the analytical sample removed by laser light irradiation and the amount of the analytical sample removed by laser light irradiation. For example, the volume of the analytical sample removed by laser light irradiation can be used as the amount of the analytical sample removed by laser light irradiation, and the volume density of the analyte in the analytical sample can be calculated. The volume of the analytical sample removed by laser light irradiation can be calculated by performing the shape measurement method described above on the analytical laminate after laser light irradiation. Furthermore, by calculating the volume density of the analyte in the analytical sample and then separately measuring the density of the analytical sample, the mass density of the analyte in the analytical sample can be calculated. Known methods can be used to measure density.
[0119] The coefficients and the like in the regression equation obtained by the above procedure may be corrected by the amount of analytical sample removed by laser light irradiation. A specific procedure, for example, is to first determine the coefficients and the like in the regression equation without correcting for the amount of analytical sample removed by laser light irradiation. Next, the determined amount of the analyte in the analytical sample removed by laser light irradiation is compared with the amount of analytical sample ablated in the analytical sample, and the signal intensity on the vertical axis is corrected. The coefficients and the like in the regression equation are again determined based on the corrected signal intensity. Note that the correction for the amount of analytical sample removed by laser light irradiation may be performed by a method other than the above.
[0120] When the analytical laminate contains two or more analytes, a regression equation is created for each analyte using the above procedure, and the amount of each analyte in the analytical sample is calculated.
[0121] In addition, in the fourth embodiment, when creating a regression equation, at least one of the above-mentioned operations Y and Z may be performed, and the resulting plot may be added to the plot when creating the regression equation in the fourth embodiment.
[0122] The present invention will be described in more detail below with reference to examples. The materials, amounts used, ratios, treatment details, treatment procedures, etc. shown in the following examples can be changed as appropriate without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be construed as being limited by the examples shown below.
[0123] <Preparation of Standard Sample Film> Polybutyl methacrylate and a metal dispersion (CONOSTAN STD S-21, manufactured by SCP Sciences) were added to butyl acetate and dissolved to obtain a composition for forming a standard sample film. The concentration of polybutyl methacrylate was 10% by mass relative to the total mass of the composition. The metal dispersion also contained multiple alkylarylsulfonates of different metal species and paraffin. The amount of metal dispersion added was adjusted so that the aluminum atom content relative to the total weight of the standard sample film described below was 100 ppm by mass. The metal dispersion also contained boron atoms, sodium atoms, magnesium atoms, silicon atoms, phosphorus atoms, calcium atoms, titanium atoms, vanadium atoms, chromium atoms, manganese atoms, iron atoms, nickel atoms, copper atoms, zinc atoms, molybdenum atoms, silver atoms, cadmium atoms, tin atoms, barium atoms, and lead atoms, each of which was equal in mass to the aluminum atom. In addition, a reference sample film-forming composition that did not contain a metal dispersion was also prepared for blank measurement (for preparing a reference sample film to be used in the above-mentioned operation Z). Except for not containing a metal dispersion, the reference sample film-forming composition was prepared under the same conditions as the standard sample film-forming composition.
[0124] The obtained standard sample film-forming composition was spin-coated (rotation speed: 2000 rpm, time: 20 seconds) onto a PET (polyethylene terephthalate) film (2.5 cm long, 2.5 cm wide, average film thickness 4.6 μm) and dried. A standard sample film (thickness of standard sample film: 0.5 μm) was prepared on the PET film and used as a standard sample sheet. The paraffin content relative to the total mass of the standard sample film excluding the PET film was 8 mass%, and the polybutyl methacrylate content consisted of the remainder of the paraffin and components derived from the metal dispersion (e.g., alkylarylsulfonium salt). The average film thickness of the standard sample sheet (average value of the total film thickness of the PET film and the standard sample film) was 5.1 μm. Using the same procedure, the reference sample film-forming composition was spin-coated onto the PET film to prepare a reference sample film (average film thickness of the standard sample film: 0.5 μm) and use as a reference sample sheet.
[0125] <Preparation of analytical laminate> A rock ashed sample (hereinafter also referred to as the "ash sample") was used as an unknown sample for element content quantification. The ash sample was pelletized using a pellet frame (Clear Disk, manufactured by Jusco Engineering, 20 mm diameter, pellet hole 5 mm diameter, thickness 1.2 mm) and a handy press. Double-sided tape (FIXFILM, manufactured by Fujicopian) was attached to one side of the pellet frame as a support layer for attaching the standard sample film. The standard sample sheet and the pellet frame were attached so that the side of the pellet frame with the double-sided tape facing the standard sample film side of the standard sample sheet, thereby obtaining an analytical laminate (Example analytical laminate). Note that the double-sided tape had different peel strengths on one side and the other side. When obtaining the analytical laminate, the double-sided tape was attached so that the side with the higher peel strength faced the pellet frame, and the side with the lower peel strength faced the standard sample sheet. In the obtained laminate for analysis, the standard sample sheet could be peeled off from the double-sided tape and could also be reattached.
[0126] The structure of the analytical laminate obtained by the above procedure will be described with reference to FIG. 2. Note that for purposes of illustration, the size ratio in FIG. 2 may differ from the actual size ratio. FIG. 2(a) is a top view of the obtained analytical laminate 40 of the example. FIG. 2(b) is a schematic cross-sectional view of the analytical laminate 40 of the example taken along line AA in FIG. 2(a). As shown in FIG. 2(b), the analytical laminate 40 of the example comprises a cylindrical pellet frame 16 with double-sided tape 18 disposed on one side thereof, and through-holes formed in the pellet frame 16 and the double-sided tape 18. The through-hole is filled with an analytical sample 14b from the side of the pellet frame 16 where the double-sided tape 18 is disposed to the side of the double-sided tape 18 opposite the pellet frame 16 side. A standard sample film 12a is disposed so as to contact the side of the analytical sample 14b facing the double-sided tape 18, and a PET film 12b is disposed on the surface of the standard sample film 12a opposite the analytical sample 14b side. The analytical laminate 40 of the example shown in FIG. 2 corresponds to the analytical laminate described above.
[0127] In addition, an Example Reference Laminate was obtained in the same manner as the Example Analytical Laminate, except that the standard sample sheet was replaced with the above-mentioned reference sample sheet. That is, an Example Reference Laminate having the analytical sample, the reference sample film, and the PET film in this order from the analytical sample side was obtained.
[0128] <Analysis Method> [Analysis Conditions by LA-ICP-MS] Femtosecond laser ablation inductively coupled plasma mass spectrometry was carried out using the obtained Example analytical laminate and Example reference laminate. That is, the Example analytical laminate and Example reference laminate were irradiated with laser light, respectively, and analyzed by LA-ICP-MS to obtain signal intensity, in accordance with the above-mentioned operation X and operation Z. The femtosecond laser ablation device used was a Jupiter solid nebulizer (manufactured by ST Japan). The various conditions were as follows. (Device conditions such as laser conditions) Laser device: LPS MultiProbe Laser wavelength: 260 nm Laser power (fluence): 5.0 to 15.0 J / cm 2ICP-MS conditions: Laser pulse width: 247 fs, Laser frequency: 10,000 Hz, Irradiation time: approximately 2 seconds, Irradiation area: 1 mm length x 1 mm width, Carrier gas: He gas 0.6 L / min in the sample chamber, Ar gas 1.1 L / min added immediately after passing through the sample chamber (ICP-MS conditions), MS measurement device: iCAP TQ (Thermo Fisher Scientific), RF power: 1,550 W, Cooling gas flow rate: 14 L / min, Auxiliary gas flow rate: 0.8 L / min
[0129] [Measurement of Mass of Ablated Analytical Sample] After LA-ICP-MS measurement, the analytical laminate of the example and the reference laminate of the example were observed using a morphological observation microscope to determine the ablation area of the standard sample film and the depth of the ablation mark of the ash sample (analytical sample). The volume was calculated by multiplying the obtained ablation mark depth by the ablation area, and the ablation mass (M) was calculated by multiplying this by the density of the ash sample calculated by the gravimetric method.
[0130] [Quantification of element content] Elemental quantification was performed using the following procedure. The following values of Y0, Y1, and X1 were obtained by LA-ICP-MS measurement, and X2 was calculated. Y0: ICP-MS signal intensity of the analyte of the Example Reference Laminate; Y1: ICP-MS signal intensity of the analyte of the Example Analytical Laminate; X1: mass of the analyte contained in a standard sample film of the analyte of the Example Analytical Laminate (ablation area of the standard sample film) × 0.5 μm; X2: absolute value of the x-axis intercept of the line connecting (x, y) = (0, Y0) and (x, y) = (X1, Y1), where the x-axis represents the mass of the analyte contained in (ablation area of the standard sample film) × 0.5 μm and y represents the signal intensity. The mass concentration of the analyte in each ash sample was calculated by dividing the obtained X2 value by the mass of the ablated ash sample.
[0131] <Results> The analytes were nickel, vanadium, chromium, molybdenum, and cadmium, and the mass concentrations of the analytes contained in the ash samples were calculated using the method described above. The results are shown in the table below. To confirm reproducibility, the same ash samples were used to repeat the above measurements and procedures, and the mass concentrations of the analytes were determined again. In both measurements, the mass concentrations obtained were such that the error ranges of the respective measurements overlapped. The error ranges were calculated by ablating a 1 mm x 1 mm area within the same analytical sample, with the signal intensities measured three times without overlapping each other, and then performing the above procedure.
[0132]
[0133] The results shown in Table 1 confirm that the analytical method of the present invention allows for easy analysis of an analyte in a solid sample.
[0134] In the examples, the method of the third embodiment in which the above-mentioned operation 3 is performed is shown, but the methods shown in the first embodiment in which operation 1 is performed and the second embodiment in which operation 2 is performed can also be used to easily analyze the analyte in a solid sample. More specifically, in the above-mentioned example, a standard sample film with a different metal content than the above is prepared, an analytical laminate is obtained using the same procedure, a signal is acquired by LA-ICP-MS, and a regression equation is created using the above-mentioned method, whereby a value corresponding to the above X2 can be calculated (first embodiment). Also, in the above-mentioned example, when a sample without a reference sample film is irradiated with laser light and a signal is acquired by LA-ICP-MS, a value corresponding to the above Y0 is obtained, and a value corresponding to the above X2 can be calculated (second embodiment).
[0135] In addition, standard sample sheets were prepared by varying the thickness of the PET film used to obtain the standard sample sheet in the above procedure, and the analytes in the solid samples were analyzed using these standard sample sheets in the same manner as above. PET film thicknesses of 19 μm, 20 μm, 1 μm, and 0.5 μm were prepared, and standard sample sheets were prepared for each and analyzed. That is, the average film thicknesses of the standard sample sheets (the average value of the total film thickness of the PET film and the standard sample film) were 19.5 μm, 20.5 μm, 1.5 μm, and 1.0 μm, respectively. The results are shown in Table 2.
[0136]
[0137] The results in Table 2 confirmed that the analytical method of the present invention allows for easy analysis of analytes in solid samples. Comparing the results in Table 2 with those in Table 1 confirmed that when the average thickness of the standard sample sheet (the average value of the total thickness of the PET film and the standard sample film) is 20 μm or less (preferably 15 μm or less, more preferably 10 μm or less, and even more preferably 8 μm or less), the error range is small and analytical accuracy is excellent. Comparing the results in Table 2 with those in Table 1 confirmed that when the average thickness of the standard sample sheet (the average value of the total thickness of the PET film and the standard sample film) is 1.2 μm or more (preferably 2.0 μm or more, more preferably 3.0 μm or more, and even more preferably 3.5 μm or more), the error range is small and analytical accuracy is excellent. This is thought to be because when the average thickness of the standard sample sheet is within the above range, the standard sample sheet is easy to handle, and can be laminated more smoothly without generating wrinkles or the like.
[0138] Separately from the above examples, a standard sample film was prepared and analyzed according to the following procedure.
[0139] <Preparation of Standard Sample Film> Polybutyl methacrylate, a metal dispersion (CONOSTAN STD, manufactured by SCP Sciences), and a surfactant (MEGAFAC R-41, manufactured by DIC Corporation) were added to butyl acetate and dissolved to obtain a solution. The concentration of polybutyl methacrylate was 15 mass% relative to the total mass of the solution, and the concentration of the surfactant was 0.05 mass% relative to the total mass of the solution. The metal dispersion was added after adjusting the concentration of each element in the standard sample film to 100 mass ppm. The obtained solution was spin-coated onto a disk-shaped silicon wafer (4.0 inches in diameter x 0.5 mm thick) and baked on a hot plate at 200°C for 5 minutes to form a 3 μm-thick standard sample film on the silicon wafer.
[0140] <Preparation of analytical laminate> First, a 6 mm diameter hole was formed in the width center of a 10 mm wide adhesive tape using a punching machine. Next, the silicon wafer with the standard sample film was cleaved into approximately 1 cm square pieces. An adhesive tape with a hole formed in it was attached to the cleaved silicon wafer with the standard sample film so that the hole roughly coincided with the center of the silicon wafer, and the adhesive tape was peeled off. When the adhesive tape was peeled off, peeling occurred at the interface between the silicon wafer and the standard sample film, and the standard sample film migrated to the adhesive tape side. By the above procedure, only the standard sample film was present in the hole of the adhesive tape.
[0141] Next, certified reference material NIST SRM 612 was prepared as the analytical sample. After polishing the surface of the analytical sample, a standard sample film attached to adhesive tape was attached to the analytical sample so that the standard sample film and the polished surface of the analytical sample were in contact with each other. The standard sample film was attached to two locations on the polished surface of the analytical sample. In addition, another standard sample film was attached to one of the standard sample films in a layered manner. At this time, the adhesive tape was attached so that the holes in the tape roughly aligned, resulting in an analytical laminate. On the polished surface of the analytical sample in the analytical laminate, there were areas where one standard sample film was attached and areas where two standard sample films were attached in a layered manner.
[0142] <Analysis Method> [Analysis Conditions by LA-ICP-MS] The analytical laminate obtained by the above procedure was irradiated with laser light and analyzed by LA-ICP-MS to obtain signal intensity. Specifically, laser light was irradiated under the following conditions to the area of the analytical laminate where no standard sample film was attached, the area where one standard sample film was attached, and the area where two standard sample films were attached, and analysis was performed by LA-ICP-MS. That is, the above operation Y was performed once, and operation X was performed twice while changing the number of stacked standard sample films. (Apparatus Conditions, such as Laser Conditions) Laser output: 50 mW Irradiation area: 0.5 mm length x 0.5 mm width All other conditions were the same as those described above.
[0143] [Measurement of Mass of Ablated Analytical Sample] After LA-ICP-MS measurement, the analytical laminate was observed using a morphological observation microscope to determine the ablation area of the standard sample film and the depth of the ablation mark of the analytical sample. The volume was calculated by multiplying the obtained ablation mark depth by the ablation area, and the ablation mass (M) was calculated by multiplying this by the density of the analytical sample.
[0144] [Quantification of element content] Elemental quantification was performed according to the following procedure. The following values of Y3, Y4, Y5, X3, X4, and X5 were obtained by LA-ICP-MS measurement, and a calibration curve was created. Y3: ICP-MS signal intensity of the analyte in a region of the analytical laminate where no standard sample film was attached Y4: ICP-MS signal intensity of a region of the analytical laminate where one standard sample film was attached Y5: ICP-MS signal intensity of a region of the analytical laminate where two standard sample films were attached X3: 0 X4: Mass of the analyte contained in the standard sample film of the analyte of the example analytical laminate (ablation area of the standard sample film) × 3 μm X5: Twice the value of the mass of the analyte contained in the standard sample film of the analyte of the example analytical laminate (ablation area of the standard sample film) × 3 μm A regression equation was created by linear regression from the plots of (X3, Y3), (X4, Y4), and (X5, Y5) above. Specifically, a calibration curve was created by fitting using the least squares method, and the X-intercept of the calibration curve was determined. The mass concentration of the analyte in each analytical sample was calculated by dividing the X-intercept value of the obtained calibration curve by the mass of the ablated analytical sample. Note that the signal intensity was corrected using the signal intensity of antimony as an internal standard, assuming that antimony is uniformly dispersed in the analytical sample.
[0145] <Results> The analytes were titanium, chromium, manganese, barium, and lead, and the mass concentrations of the analytes contained in the analytical samples were calculated using the method described above. Calibration curves with high coefficients of determination were obtained for each element. The results and NIST-certified values are shown in Table 3 below. In Table 3, "quantitative value" refers to the mass concentration of the analyte calculated using the method described above.
[0146]
[0147] From the results shown in Table 3, the analytical values obtained by the analytical method of the present invention are close to the NIST-certified values, and it has been confirmed that the present invention allows for the easy analysis of analytes in solid samples. In the above example, the fourth embodiment method in which the above-mentioned operation 4 is performed is shown, but the methods shown in the first to third embodiments in which the above-mentioned operations 1 to 3 are performed, respectively, also allow for the easy analysis of analytes in solid samples.
[0148] In addition, in the procedure for obtaining the above-mentioned standard sample film by spin-coating it onto a silicon wafer, the amount of paraffin contained in the standard sample film and the film thickness were adjusted to form the standard sample film. The formed standard sample film was then peeled from the silicon wafer using adhesive tape with holes to confirm whether the resulting film was obtained with only the standard sample film present in the holes of the adhesive tape. More specifically, the amount of paraffin added was adjusted so that the paraffin content relative to the total mass of the standard sample film was the amount shown in Table 4 below, and the solution concentration and coating amount were adjusted to form the standard sample film with the thickness shown in Table 4 below. In Table 4, the tape peeling column indicates that the film obtained with only the standard sample film present in the holes of the adhesive tape when peeled using the adhesive tape with holes is marked "A." Furthermore, the film obtained with only the standard sample film present in the holes of the adhesive tape when peeled using the adhesive tape with holes is marked "B."
[0149] The solution used to obtain the standard sample film was prepared by adding paraffin to the solution used in the procedure for obtaining the standard sample film by spin-coating it onto a silicon wafer. The paraffin content was 0.1 to 3.0 mass% relative to the total mass of the solution, and the polybutyl methacrylate content was 6 to 15 mass% relative to the mass of the solution. The paraffin content in the standard sample film was determined by dissolving two standard sample films of the same area, prepared under the same conditions except for whether or not they were baked, in deuterated THF and 1The paraffin content in the standard sample film was calculated by H NMR measurement. More specifically, the peak area derived from paraffin was normalized by the peak area derived from the polymer (polybutyl methacrylate), and the peak areas derived from paraffin were compared between two standard sample films to calculate the amount of paraffin volatilized during the baking process. The amount of paraffin remaining after baking was calculated from the paraffin charge amount in the solution and the volatilized amount, and the paraffin content in the standard sample film was calculated by dividing the calculated amount by the mass of the standard sample film remaining after baking.
[0150]
[0151] From the results shown in Table 4 above, it can be seen that for all standard sample films, when peeled off using adhesive tape with holes, only the standard sample film remained in the holes of the adhesive tape.
[0152] In addition, in the procedure for obtaining the above-mentioned standard sample films by spin-coating them onto silicon wafers, the surfactant used was changed to the following surfactants to prepare standard sample films. The surfactants used were KL-400HF, Polyflow KL-401, Polyflow KL-402, Polyflow KL-700, LE-302N, and LE-304. The preparation of standard sample films was carried out under the same conditions as above, except for the surfactants used. Regardless of which surfactant was used, similar standard sample films were obtained, and they could be peeled off using tape with holes.
[0153] 12, 12a, 12c, 12e Standard sample film 12b PET film 12d Temporary support 14, 14b, 14c Analysis sample 16 Pellet frame 18 Double-sided tape 20, 20a, 20b, 20c Laminate for analysis 22 Ablation sample 30 Laser light 40 Example analysis laminate 52, 52a Perforated adhesive tape 54a, 54b, 54c, 54d Adhesive tape
Claims
1. An analytical method comprising carrying out any one of the following operations 1 to 4, creating a regression equation based on the signal intensity value obtained and the amount of the analyte contained in a standard sample film removed by laser light irradiation, and using the regression equation to calculate the amount of the analyte in a solid analytical sample containing the analyte removed by laser light irradiation. Operation 1: The standard sample film containing the analyte is placed on the solid analytical sample containing the analyte to obtain an analytical laminate, and an operation X of irradiating the analytical laminate with laser light and detecting signal intensities originating from the analyte in the standard sample film and the analyte in the analytical sample is carried out two or more times while changing the concentration of the analyte in the standard sample film. Operation 2: At least the operation X is carried out at least once, and an operation Y of irradiating the analytical sample with laser light to detect signal intensities originating from the analyte in the analytical sample. Operation 3: Perform at least the operation X at least once, and an operation Z of arranging a reference sample film not containing the analyte on the analytical sample to obtain a reference laminate, irradiating the reference laminate with laser light, and detecting the signal intensity derived from the analyte in the analytical sample. Operation 4: Perform the operation X two or more times while changing the number or thickness of the stacked standard sample films.
2. The analytical method according to claim 1, further comprising the step of calculating the concentration of the analyte in the analytical sample based on the amount of the analyte in the analytical sample removed by irradiation with laser light.
3. An analytical method as described in claim 1 or 2, in which the volume of the analytical sample removed by irradiating laser light is determined by measuring the shape, and the volume concentration of the analyte in the analytical sample is calculated based on the removed volume.
4. The analytical method according to claim 1 or 2, wherein the signal intensity is a signal intensity obtained by mass spectrometry.
Citation Information
Patent Citations
Powder sample disk for quantitative analysis using laser ablation, manufacturing method thereof, and apparatus for the same
JP2013238455A
Positive resist composition and pattern-forming method
US20080248425A1
Analysis of germanium alloy composition
JP1991218444A
Standard sample film, manufacturing method for standard sample film, standard sample, sample set, quantitative analysis method, and transfer film
WO2021157407A1
System and method for performing laser-induced breakdown spectroscopy measurements on molten metal samples
WO2023037392A2
Cited By
Method for representing thickness of thin film of superconducting cavity of accelerator