Semiconductor structure and forming method therefor

By adding an insulating structure to the formation method of a three-dimensional semiconductor memory device, reliability problems caused by parasitic capacitance and leakage channels in traditional methods are solved, and the stability and performance of the semiconductor structure are improved.

WO2024212854A1PCT designated stage expired Publication Date: 2024-10-17RUILI INTEGRATED CIRCUIT CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/085731
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-14
Filing Date
2024-04-03
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

The reliability of traditional three-dimensional semiconductor memory devices is affected by parasitic capacitance and leakage channels, causing reliability problems in the development of miniaturization.

Method used

In the method of forming the semiconductor structure, an alternating stacked structure of dielectric layers and semiconductor layers is formed on the substrate, and a word line opening extending along the third direction is formed in the isolation structure, and an insulation structure is added to increase the distance between the word line structure and the substrate. distance between the bases to reduce coupling effects and parasitic capacitance.

Benefits of technology

The reliability of the semiconductor structure is effectively improved, leakage channels between the word line structure and the substrate are avoided, and the performance of the three-dimensional semiconductor memory device is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024085731_17102024_PF_FP_ABST
    Figure CN2024085731_17102024_PF_FP_ABST
Patent Text Reader

Abstract

A semiconductor structure and a forming method therefor. The forming method for a semiconductor structure comprises: on a substrate, forming a stacked structure in which dielectric layers and semiconductor layers are alternately stacked; forming a plurality of isolation structures, which extend in a first direction, penetrate through the stacked structure and extend into the substrate, wherein the isolation structures partition the stacked structure into a plurality of stacked sub-structures, which are arranged in a second direction; forming, in the isolation structures, a word-line opening which extends in a third direction, wherein a bottom surface of the word-line opening is lower than a bottom surface of the semiconductor layer which is closest to the substrate, and the word-line opening is located between the stacked sub-structures and the isolation structures; forming an insulating structure between the word-line opening and the substrate; and forming a word-line structure in the word-line opening.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor structure and method for forming the same

[0001] Cross-references

[0002] This disclosure claims priority to the Chinese invention patent application with application number 202310422720.6, filed on April 14, 2023, and application name “Semiconductor structure and method for forming the same”. The entire contents of this Chinese invention patent application are incorporated by reference into this disclosure. Technical Field

[0003] The present disclosure relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for forming the same. Background Art

[0004] The integration level of two-dimensional semiconductor memory devices is primarily determined by the area occupied by the memory cells, and is therefore significantly influenced by the level of fine patterning technology. To overcome this limitation, three-dimensional semiconductor memory devices have recently been proposed, including memory cells arranged in three dimensions.

[0005] However, conventional three-dimensional semiconductor memory devices and their formation methods still have certain defects. How to further improve the reliability of three-dimensional semiconductor memory devices has become an urgent problem that needs to be solved.

[0006] Summary of the Invention

[0007] In view of this, embodiments of the present disclosure provide a semiconductor structure and a method for forming the same in order to solve at least one problem existing in the prior art.

[0008] To achieve the above objectives, the technical solution of the embodiment of the present disclosure is implemented as follows:

[0009] In a first aspect, an embodiment of the present disclosure provides a method for forming a semiconductor structure, comprising:

[0010] forming a stack structure in which dielectric layers and semiconductor layers are alternately stacked on a substrate;

[0011] forming a plurality of isolation structures extending along a first direction and penetrating the stack structure and extending into the substrate; the isolation structures separate the stack structure into a plurality of sub-stack structures arranged along a second direction; the first direction is perpendicular to the second direction, and both are perpendicular to a third direction, which is a thickness direction of the substrate;

[0012] forming a word line opening extending along the third direction in the isolation structure; wherein a bottom surface of the word line opening is lower than a bottom surface of the semiconductor layer closest to the substrate, and the word line opening is located between the sub-stack structure and the isolation structure;

[0013] forming an insulating structure between the wordline opening and the substrate;

[0014] A word line structure is formed in the word line opening.

[0015] In some embodiments, the isolation structure includes a support structure extending along the first direction and insulating layers located on two opposite sides of the support structure along the second direction; and forming a word line opening extending along the third direction in the isolation structure includes:

[0016] performing a first etching on the insulating layer along the third direction to form an initial opening exposing a portion of the sidewall of the support structure and the sidewall of the sub-stack structure; wherein a bottom surface of the initial opening is lower than a bottom surface of the sub-stack structure;

[0017] forming a barrier layer on the sidewalls of the initial opening;

[0018] The insulating layer is subjected to a second etching along the third direction through the initial opening to form the word line opening; the sidewalls of the word line opening expose the substrate; the bottom surface of the word line opening is higher than the bottom surface of the isolation structure and lower than the bottom surface of the semiconductor layer of the sub-stack structure closest to the substrate.

[0019] In some embodiments, forming an insulating structure between the word line opening and the substrate includes:

[0020] The substrate exposed by the sidewalls of the word line opening is doped to form the insulating structure; the insulating structure protrudes from the sidewalls of the word line opening toward the interior of the substrate.

[0021] In some embodiments, the sidewalls of the wordline opening expose the substrate; the bottom surface of the wordline opening is higher than the bottom surface of the isolation structure and lower than the bottom surface of the sub-stack structure; the isolation structure includes a support structure extending along the first direction and insulating layers located on opposite sides of the support structure along the second direction; and forming an insulating structure between the wordline opening and the substrate includes:

[0022] Etching the substrate exposed by the sidewall of the word line opening to form a groove protruding from the word line opening into the interior of the substrate;

[0023] The groove is filled with an insulating material to form the insulating structure.

[0024] In some embodiments, forming a word line opening extending along the third direction in the isolation structure and forming an insulating structure between the word line opening and the substrate includes:

[0025] Etching the isolation structure along the third direction to form a word line opening exposing a sidewall of the sub-stack structure, wherein a bottom surface of the word line opening is higher than a bottom surface of the sub-stack structure;

[0026] When the word line opening is formed, the isolation structure between the bottom of the word line opening and the substrate constitutes the insulation structure.

[0027] In some embodiments, doping the substrate exposed by the sidewalls of the word line opening comprises: performing angled nitrogen doping on the substrate exposed by the sidewalls of the word line opening using a plasma nitriding process.

[0028] In some embodiments, forming a word line structure in the word line opening includes:

[0029] A gate dielectric layer and a gate layer are sequentially formed in the word line opening; the gate dielectric layer is located between the gate layer and the semiconductor layer.

[0030] In some embodiments, the method for forming a semiconductor structure further includes:

[0031] An active structure is formed in the semiconductor layer of the sub-stack structure; the active structure and the word line structure constitute a transistor structure.

[0032] In a second aspect, an embodiment of the present disclosure provides a semiconductor structure, including:

[0033] A substrate and a stacked structure located on the substrate; the stacked structure comprises alternately stacked dielectric layers and semiconductor layers;

[0034] an isolation structure extending along a first direction, penetrating the stack structure, and extending into the substrate; the isolation structure divides the stack structure into a plurality of sub-stack structures arranged along a second direction; the first direction is perpendicular to the second direction, and both are perpendicular to a third direction, which is a thickness direction of the substrate;

[0035] a word line structure extending along the third direction; a bottom surface of the word line structure being lower than a bottom surface of the semiconductor layer closest to the substrate, and the word line structure being located between the sub-stack structure and the isolation structure;

[0036] An insulating structure is located between the word line structure and the substrate.

[0037] In some embodiments, the isolation structure includes a support structure extending along the first direction and an insulating layer located on opposite sides of the support structure along the second direction; the word line structure is located between the support structure and the sub-stack structure and above the insulating layer; the bottom surface of the word line structure is higher than the bottom surface of the isolation structure and lower than the bottom surface of the semiconductor layer of the sub-stack structure closest to the substrate.

[0038] In some embodiments, the insulating layer contacts a bottom end of the insulating structure.

[0039] In some embodiments, a bottom surface of the word line structure is higher than a bottom surface of the isolation structure and lower than a bottom surface of the semiconductor layer of the sub-stack structure closest to the substrate.

[0040] In some embodiments, the insulating structure is located between a sidewall of the word line structure and the substrate; and the insulating structure protrudes from the sidewall of the word line structure toward the interior of the substrate.

[0041] In some embodiments, along the second direction, in a direction from the word line structure toward the substrate, a size of the insulation structure in the third direction decreases.

[0042] In some embodiments, a bottom surface of the word line structure is higher than a bottom surface of the sub-stack structure; and the insulating structure is located between the bottom surface of the word line structure and the substrate.

[0043] In some embodiments, constituent elements of the insulating structure include nitrogen and / or oxygen.

[0044] In some embodiments, the word line structure includes a gate dielectric layer and a gate layer; the gate dielectric layer is located between the gate layer and the semiconductor layer.

[0045] In some embodiments, the semiconductor layer includes an active structure; the active structure and the word line structure constitute a transistor structure.

[0046] In some embodiments, the insulating structure is located below the sub-stack structure, and a top of the insulating structure contacts a bottom surface of the dielectric layer closest to the substrate in the sub-stack structure.

[0047] In some embodiments, a bottom end of the insulating structure is lower than a bottom surface of the word line structure.

[0048] In the embodiments provided in the present disclosure, a word line opening is formed in an isolation structure that separates a stacked structure, and an insulating structure is formed between the word line opening and the substrate before a word line structure is formed in the word line opening. The insulating structure can increase the distance between the gate layer and the substrate in the word line structure, reduce the coupling effect between the word line structure and the substrate, reduce the parasitic capacitance between the word line structure and the substrate, avoid the generation of a leakage channel between the word line structure and the substrate, and effectively improve the reliability of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] FIG1 is a schematic flow chart of a method for forming a semiconductor structure according to an embodiment of the present disclosure;

[0050] 2a to 2i are schematic structural diagrams of a semiconductor structure forming process according to an embodiment of the present disclosure;

[0051] 3a to 3d are schematic structural diagrams of a semiconductor structure forming process according to another embodiment of the present disclosure;

[0052] 4a to 4c are schematic structural diagrams of a semiconductor structure forming process provided by yet another embodiment of the present disclosure. DETAILED DESCRIPTION

[0053] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the specific embodiments described herein. Instead, these embodiments are provided to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0054] In the following description, numerous specific details are provided to provide a more thorough understanding of the present disclosure. However, it will be apparent to those skilled in the art that the present disclosure can be practiced without one or more of these details. In other instances, certain technical features known in the art are not described to avoid confusion with the present disclosure; that is, all features of actual embodiments are not described herein, nor are well-known functions and structures described in detail.

[0055] In the drawings, like reference numerals refer to like elements throughout.

[0056] It should be understood that spatial relationship terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used herein for convenience of description to describe the relationship of one element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the drawings is turned over, then the elements or features described as "under the other elements" or "under it" or "under it" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" can include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial description terms used herein are interpreted accordingly.

[0057] The purpose of the terms used herein is only to describe specific embodiments and is not intended to limit the present disclosure. When used herein, the singular forms "a", "an", and "the" are intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "comprising" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0058] In the currently proposed method for forming a three-dimensional semiconductor structure, a wordline opening is directly formed in the stacked structure, and a wordline structure including a gate layer and a gate dielectric layer is directly formed in the wordline opening. With the trend of miniaturization of semiconductor devices, the thickness of the gate dielectric layer is getting smaller and smaller, which may cause the distance between the ultimately formed gate layer and the substrate to be too close, resulting in a large parasitic capacitance between the wordline structure and the substrate, and even a leakage channel, seriously affecting the reliability of the three-dimensional semiconductor structure.

[0059] Therefore, it is necessary to further improve the reliability of three-dimensional semiconductor structures. To this end, the present disclosure proposes the following embodiments.

[0060] The present disclosure provides a method for forming a semiconductor structure. FIG1 is a flow chart of the method for forming a semiconductor structure provided by the present disclosure. As shown in FIG1 , the method for forming a semiconductor structure includes the following steps:

[0061] Step 101: forming a stack structure of alternating dielectric layers and semiconductor layers on a substrate;

[0062] Step 102: forming a plurality of isolation structures extending along a first direction, penetrating the stack structure, and extending into the substrate; the isolation structures separate the stack structure into a plurality of sub-stack structures arranged along a second direction;

[0063] Step 103: forming a word line opening extending along a third direction in the isolation structure; a bottom surface of the word line opening is lower than a bottom surface of the semiconductor layer closest to the substrate, and the word line opening is located between the sub-stack structure and the isolation structure;

[0064] Step 104: forming an insulating structure between the word line opening and the substrate;

[0065] Step 105 : forming a word line structure in the word line opening.

[0066] 2a to 2i are schematic diagrams of a semiconductor structure forming process according to an embodiment of the present disclosure. The method for forming a semiconductor structure according to an embodiment of the present disclosure will be described in detail below with reference to FIG1 and FIG2a to 2i.

[0067] 2 a , step 101 is performed to form a stack structure in which dielectric layers 201 and semiconductor layers 202 are alternately stacked on a substrate 200 .

[0068] In some embodiments, the substrate 200 can be a single semiconductor material substrate (for example, a silicon substrate, a germanium substrate, etc.), a compound semiconductor material substrate (for example, a germanium silicon substrate, etc.), or a silicon-on-insulator (SOI) substrate, a germanium-on-insulator (GeOI) substrate, etc.

[0069] In some embodiments, the dielectric layer 201 and the semiconductor layer 202 can be formed by a deposition process, first forming a dielectric layer 201 on the substrate 200, then forming a semiconductor layer 202 on the dielectric layer 201, and repeating the process to form a stacked structure in which the dielectric layer 201 and the semiconductor layer 202 are alternately stacked.

[0070] It should be noted that the number of dielectric layers 201 and semiconductor layers 202 shown in FIG. 2 a is only an example, and the present disclosure does not limit the specific number of dielectric layers 201 and semiconductor layers 202 in the stacked structure.

[0071] In some embodiments, the material of the dielectric layer 201 can be one of dielectric materials such as silicon oxide, silicon nitride, silicon oxynitride, and silicon carbide nitride; the material of the semiconductor layer 202 can be one of semiconductor materials such as silicon, germanium, and indium gallium zinc oxide.

[0072] In the embodiments of the present disclosure, the deposition process includes but is not limited to chemical vapor deposition (CVD), low pressure chemical vapor deposition (LPCVD), plasma enhanced chemical vapor deposition (PECVD), physical vapor deposition (PVD) and atomic layer deposition (ALD).

[0073] 2 b , step 102 is performed to form a plurality of isolation structures 220 extending along a first direction, penetrating the stack structure, and extending into the substrate 200 ; the isolation structures 220 separate the stack structure into a plurality of sub-stack structures 210 arranged along a second direction.

[0074] In the embodiment of the present disclosure, the first direction is the X direction, the second direction is the Y direction, and the third direction is the Z direction, and the third direction is the thickness direction of the substrate 200 .

[0075] In some embodiments, the specific steps of forming the isolation structure 220 include: forming a patterned mask layer 203 on the stacked structure, and etching the stacked structure using the patterned mask layer 203 as a mask to form a plurality of grooves in the stacked structure extending along a first direction and penetrating the stacked structure and extending into the substrate 200.

[0076] In some specific examples, the material of the patterned mask layer 203 includes, but is not limited to, silicon nitride.

[0077] In an embodiment of the present disclosure, referring to Figure 2b, after the groove is formed, the remaining patterned mask layer 203 is not removed, and a support structure 221 extending along the first direction and an insulating layer 222 located on opposite sides of the support structure 221 along the second direction are formed in the groove. The support structure 221 and the insulating layer 222 constitute an isolation structure 220, and the top surface of the isolation structure 220 is flush with the top surface of the patterned mask layer 203.

[0078] In the embodiment of the present disclosure, the materials of the support structure 221 and the insulating layer 222 are different, and the material of the insulating layer 222 has a large etching selectivity ratio with the material of the support structure 221 .

[0079] In a specific example, the material of the support structure 221 is silicon nitride, and the material of the insulating layer 222 is silicon oxide.

[0080] It should be noted that in the embodiment of the present disclosure, the isolation structure 220 separates the stacking structure into multiple sub-stack structures 210 arranged along the second direction. The number of isolation structures 220 and sub-stack structures 210 in Figure 2b is only an example, and the present disclosure does not limit the specific number of isolation structures 220 and sub-stack structures 210.

[0081] 2 c to 2 e , step 103 is performed to form a word line opening 233 extending along a third direction in the isolation structure 220 ; the bottom surface of the word line opening 233 is lower than the bottom surface of the semiconductor layer 202 closest to the substrate 200 , and the word line opening 233 is located between the sub-stack structure 210 and the isolation structure 220 .

[0082] Referring to FIG. 2 c , a wordline opening 233 extending along a third direction is formed in the isolation structure 220 . This includes performing a first etching of the insulating layer 222 along the third direction to form an initial opening 231 that exposes a portion of the sidewalls of the support structure 221 and the sidewalls of the sub-stack structure 210 . The bottom surface of the initial opening 231 is lower than the bottom surface of the semiconductor layer 202 of the sub-stack structure 210 that is closest to the substrate 200 . In the embodiment of the present disclosure, a dry etching process can be used to perform the first etching of the insulating layer 222 . Here, the dry etching process can be an etching process with good directionality, such as plasma etching, sputtering etching, ion beam etching, reactive ion etching, etc., to minimize the impact on the sub-stack structure 210 .

[0083] 2 d , a word line opening 233 extending along a third direction is formed in the isolation structure 220 , and the process further includes forming a barrier layer 232 on a sidewall of the initial opening 231 .

[0084] In the embodiment of the present disclosure, the material of the insulating layer 222 and the material of the blocking layer 232 have a large etching selectivity ratio, and the blocking layer 232 can prevent the dielectric layer 201 and the semiconductor layer 202 in the sub-stack structure 210 from being affected by subsequent process steps.

[0085] In some specific examples, the material of the barrier layer 232 includes, but is not limited to, silicon nitride.

[0086] In some specific examples, the method of forming the barrier layer 232 includes, but is not limited to, an ALD process.

[0087] Referring to Figure 2e, a word line opening 233 extending along a third direction is formed in the isolation structure 220, and the process also includes: performing a second etching on the insulating layer 222 along the third direction through the initial opening 231 to form the word line opening 233; the sidewalls of the word line opening 233 expose the substrate 200; the bottom surface of the word line opening 233 is higher than the bottom surface of the isolation structure 220 and lower than the bottom surface of the sub-stack structure 210, and a portion of the insulating layer 222 is retained between the bottom surface of the word line opening 233 and the substrate 200.

[0088] Here, a portion of the insulating layer 222 is retained between the bottom surface of the word line opening 233 and the substrate 200, so that after the word line structure is subsequently formed in the word line opening 233, a certain distance is maintained between the word line structure and the substrate 200, and the material of the insulating layer 222 can be a low dielectric constant material, thereby improving the coupling effect between the word line structure and the substrate 200, reducing the parasitic capacitance between the word line structure and the substrate 200, and avoiding the generation of a leakage channel between the word line structure and the substrate 200.

[0089] In the embodiment of the present disclosure, a wet etching process can be used to perform a second etching on the insulating layer 222 to etch the insulating layer 222 located at the bottom of the initial opening 231. During this process, the barrier layer 232 can protect the sub-stack structure 210 and prevent the sub-stack structure 210 from being etched. In the embodiment of the present disclosure, two wordline openings 233 extending along the third direction need to be formed in the isolation structure 220. The isolation structure 220 includes a support structure 221 and an insulating layer 222. The material of the insulating layer 222 has a large etching selectivity ratio with the material of the support structure 221. During the formation of the wordline openings 233, a maskless etching process can be used to perform a second etching only on the insulating layer 222. The support structure 221 serves to separate the two wordline openings. After the wordline structure is formed in the wordline opening 233 in a subsequent process, the support structure 221 can be used to isolate the two adjacent wordline structures, thereby reducing the mutual influence between the two adjacent wordline structures.

[0090] 2 f , step 104 is performed to form an insulating structure 240 between the word line opening 233 and the substrate 200 .

[0091] In the embodiment of the present disclosure, forming an insulating structure 240 between the word line opening 233 and the substrate 200 includes: doping the substrate 200 exposed by the sidewalls of the word line opening 233 to form an insulating structure 240, wherein the insulating structure 240 protrudes from the sidewalls of the word line opening 233 toward the interior of the substrate 200, and the bottom end of the insulating structure 240 contacts the insulating layer 222.

[0092] In some specific examples, a plasma nitriding process is used to perform angled nitrogen doping on the substrate 200 exposed by the wordline opening 233. As shown in FIG2f , the doped region extends from the surface of the substrate 200 exposed by the wordline opening 233 into the interior of the substrate 200, thereby forming an insulating structure 240 that protrudes from the sidewalls of the wordline opening 233 into the interior of the substrate 200. During the doping process of the substrate 200, the barrier layer 232 on the sidewalls of the sub-stack structure 210 can block the plasma, thereby reducing the impact on the sub-stack structure 210.

[0093] In other specific examples, a high-temperature vapor-phase doping process can be used to dope the substrate 200 exposed by the sidewalls of the wordline openings 233. The doping gas can contact the substrate 200 through the wordline openings 233 and dope the substrate 200 at a high temperature, thereby forming an insulating structure 240 that protrudes from the sidewalls of the wordline openings 233 into the interior of the substrate 200. During the doping process of the substrate 200, the barrier layer 232 on the sidewalls of the sub-stack structure 210 can block the doping gas, so that the semiconductor layer 202 in the sub-stack structure 210 is not doped.

[0094] In some other embodiments of the present disclosure, the substrate 200 exposed by the sidewalls of the word line opening 233 may be doped by an ion implantation process.

[0095] In the embodiment of the present disclosure, the doping element may be nitrogen and / or oxygen, that is, the constituent elements of the insulating structure 240 include nitrogen and / or oxygen. After the substrate 200 is doped, the insulation of the doped region is significantly improved compared to the substrate 200.

[0096] In the embodiment of the present disclosure, the material of the dielectric layer 201 of the sub-stack structure 210 is different from the material of the insulating layer 222. After the insulating layer 222 is first etched along the third direction, the bottom surface of the initial opening 231 is lower than the bottom surface of the semiconductor layer 202 closest to the substrate 200 in the sub-stack structure 210, and is slightly higher than the bottom surface of the sub-stack structure 210. After the blocking layer 232 is formed, the bottom of the blocking layer 232 is higher than the top surface of the substrate 200. Thus, the blocking layer 232 will not block the doping gas from contacting the substrate 200. The top of the insulating structure 240 formed by doping can contact the bottom surface of the sub-stack structure 210, thereby further avoiding the generation of a leakage channel between the subsequently formed word line structure and the substrate 200.

[0097] In other embodiments, the material of the dielectric layer 201 of the sub-stack structure 210 is the same as the material of the insulating layer 222. After the insulating layer 222 is first etched along the third direction, the bottom surface of the initial opening should be slightly lower than the bottom surface of the sub-stack structure 210, so that the barrier layer formed in the subsequent steps completely covers the side wall of the sub-stack structure 210, thereby preventing the dielectric layer 201 from being etched when the insulating layer 222 is etched for the second time.

[0098] In some embodiments, referring to FIG. 2 f and FIG. 2 g , after the insulating structure 240 is formed, the barrier layer 232 may be removed by an etching process.

[0099] Referring to Figure 2g, when the blocking layer 232 is removed by the etching process, a portion of the insulating structure 240 exposed by the side wall of the word line opening 233 will also be etched away, so that the size of the portion of the word line opening 233 below the top surface of the substrate 200 in the second direction is larger than the size of the portion of the word line opening 233 above the top surface of the substrate 200 in the second direction.

[0100] 2h and 2i , step 105 is performed to form a wordline structure 250 in the wordline opening 233. The process of forming the wordline structure 250 includes sequentially forming a gate dielectric layer 251 and a gate layer 252 in the wordline opening 233. The gate dielectric layer 251 is located between the gate layer 252 and the semiconductor layer 202. The bottom surface of the wordline structure 250 is lower than the bottom surface of the sub-stack structure 210 and higher than the bottom surface of the isolation structure 220.

[0101] In some embodiments, as shown in FIG. 2i , the gate layer 252 includes not only a portion extending along the third direction but also a portion located on the sub-stack structure 210 , which connects the word line structures 250 located on opposite sides of the sub-stack structure 210 along the second direction.

[0102] In some embodiments, the gate dielectric layer 251 is formed by a deposition process. The material of the gate dielectric layer 251 may be at least one of a high-k dielectric material, silicon oxide, silicon nitride, and silicon oxynitride. The high-k dielectric material may be at least one of hafnium oxide, hafnium silicon oxide, lanthanum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, lithium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.

[0103] In some specific examples, the gate dielectric layer 251 is formed by an ALD process. Referring to FIG. 2 h , the gate dielectric layer 251 covers the bottom and sidewalls of the word line opening 233 .

[0104] In some other specific examples, the gate dielectric layer is formed by an in-situ steam generation (ISSG) process, and the gate dielectric layer is only formed on the sidewalls of the semiconductor layer 202 exposed by the word line opening 233 .

[0105] In some embodiments, a conductive material is filled in the word line opening 233 by a deposition process to form a gate layer 252. The conductive material can be at least one of a doped semiconductor material (for example, doped polysilicon, doped germanium, etc.), a conductive metal nitride (for example, titanium nitride, tantalum nitride, etc.), a metal material (for example, tungsten, titanium, tantalum, etc.) and a metal semiconductor compound (for example, tungsten silicide, cobalt silicide, titanium silicide, etc.).

[0106] In the embodiment of the present disclosure, in combination with reference to Figure 2g and Figure 2i, since the size of the portion of the word line opening 233 below the top surface of the substrate 200 in the second direction is larger than the size of the portion of the word line opening 233 above the top surface of the substrate 200 in the second direction, after the word line structure 250 is formed in the word line opening 233, the size of the portion of the word line structure 250 below the top surface of the substrate 200 in the second direction is larger than the portion of the word line structure 250 above the top surface of the substrate 200. Therefore, the resistance of the portion of the word line structure 250 below the top surface of the substrate 200 can be reduced, and the voltage drop caused by this portion during actual operation can be reduced, thereby improving the reliability of the semiconductor structure.

[0107] In some embodiments, the method for forming a semiconductor structure further includes: forming an active structure (not shown in the figure) in the semiconductor layer 202 of the sub-stack structure 210 through an ion implantation process, the active structure including a source region, a channel region, and a drain region arranged along a first direction, and the word line structure 250 is located on opposite sides of the channel region along a second direction, forming a transistor structure with the active structure.

[0108] In the embodiment of the present disclosure, a wordline opening 233 is formed in the isolation structure 220 that penetrates the stack structure, and a portion of the insulating layer 222 is retained between the bottom of the wordline opening 233 and the substrate 200. Then, an insulating structure 240 is formed between the wordline opening 233 and the substrate 200, and then a wordline structure 250 is formed in the wordline opening 233. That is, the insulating structure 240 is formed between the wordline structure 250 and the substrate 200. The insulating structure 240 protrudes from the sidewall of the wordline structure 250 into the interior of the substrate 200, thereby increasing the distance between the sidewall of the gate layer 252 and the substrate 200. The insulating layer 222 increases the distance between the bottom of the wordline structure 250 and the substrate 200. As a result, the coupling effect between the wordline structure 250 and the substrate 200 can be reduced, the parasitic capacitance between the wordline structure 250 and the substrate 200 can be reduced, and the generation of a leakage channel between the wordline structure 250 and the substrate 200 can be avoided, thereby effectively improving the reliability of the semiconductor structure.

[0109] Figures 3a to 3d are schematic diagrams of a semiconductor structure forming process according to another embodiment of the present disclosure. Below, the differences between the semiconductor structure forming method according to another embodiment of the present disclosure and the semiconductor structure forming method shown in Figures 2a to 2i will be described in conjunction with Figures 1 and 3a to 3d.

[0110] In the embodiment of the present disclosure, after executing steps 101 to 103, a structure as shown in Figure 3a is obtained, which includes a sub-stack structure 310 arranged along the second direction, an isolation structure 320, a word line opening 333 located between the isolation structure 320 and the sub-stack structure 310, and a blocking layer 332 formed on the side wall of the word line opening 333, the isolation structure 320 includes a support structure 321 and an insulating layer 322, the bottom surface of the word line opening 333 is lower than the bottom surface of the semiconductor layer 302 of the sub-stack structure 310 closest to the substrate 300, and is higher than the bottom surface of the isolation structure 320, and the side wall of the word line opening 333 exposes the substrate 300.

[0111] 3b and 3c, step 104 is performed to form an insulating structure 340 between the word line opening 333 and the substrate 300. The specific process is as follows: the substrate 300 exposed on the sidewall of the word line opening 333 is etched to form a groove 334 protruding from the word line opening 333 to the inside of the substrate 300. As shown in FIG3b, the maximum dimension of the groove 334 in the second direction is smaller than half of the dimension of the sub-stack structure 310 in the second direction, so that part of the substrate 300 is retained between the two grooves 334 under one sub-stack structure 310, thereby avoiding the collapse of the sub-stack structure 310; and insulating material is filled in the groove 334 to form an insulating structure 340.

[0112] In the embodiment of the present disclosure, the substrate 300 with the exposed sidewalls of the word line opening 333 is etched by a wet etching process to form a groove 334 protruding from the word line opening 333 toward the interior of the substrate 300. During this process, the blocking layer 332 can serve as a sacrificial layer and be removed while etching the substrate 300, thereby reducing the impact on the sub-stack structure 310.

[0113] In some embodiments, a dry etching process may be used to etch the exposed sidewalls of the wordline opening 333 on the substrate 300 to form the recess 334. Here, the dry etching process includes but is not limited to plasma etching, sputter etching, ion beam etching, and reactive ion etching.

[0114] In the disclosed embodiment, an insulating material is deposited into the recess 334. For example, after depositing the insulating material into the wordline opening 333 and the recess 334, the insulating material in the wordline opening 333 is removed. In one specific example, the insulating material filling the recess 334 is silicon oxide; in another specific example, the insulating material filling the recess 334 is silicon nitride. In the disclosed embodiment, the insulating structure 340 protrudes from the sidewalls of the wordline opening 333 toward the interior of the substrate 300, and the bottom of the insulating structure 340 contacts the insulating layer 322.

[0115] 3 d , step 105 is performed to form a word line structure 350 in the word line opening 333 . The word line structure 350 includes a gate dielectric layer 351 and a gate layer 352 .

[0116] In the embodiment of the present disclosure, a word line opening 333 is formed in the isolation structure 320 that penetrates the stack structure, and a portion of the insulating layer 322 is retained between the bottom of the word line opening 333 and the substrate 300. Then, a groove 334 is formed between the word line opening 333 and the substrate 300, which protrudes from the word line opening 333 to the inside of the substrate 300. The groove 334 is then filled to form an insulating structure 340. Then, a word line structure 350 is formed in the word line opening 333, that is, an insulating junction is formed between the word line structure 350 and the substrate 300. The insulating structure 340 protrudes from the sidewall of the word line structure 350 toward the inside of the substrate 300, thereby increasing the distance between the sidewall of the gate layer 352 and the substrate 300. The insulating layer 322 increases the distance between the bottom of the word line structure 350 and the substrate 300. As a result, the coupling effect between the word line structure 350 and the substrate 300 can be reduced, the parasitic capacitance between the word line structure 350 and the substrate 300 can be reduced, and the leakage channel between the word line structure 350 and the substrate 300 can be avoided, thereby effectively improving the reliability of the semiconductor structure.

[0117] Figures 4a and 4c are schematic diagrams of a semiconductor structure forming process according to another embodiment of the present disclosure. The following describes the differences between the semiconductor structure forming method according to another embodiment of the present disclosure and the semiconductor structure forming method shown in Figures 2a to 2i, in conjunction with Figures 1, 4a, and 4c.

[0118] In an embodiment of the present disclosure, after executing step 101 and step 102, a structure as shown in Figure 4a is obtained, which includes a sub-stack structure 410 and an isolation structure 420 arranged along the second direction, and the isolation structure 420 includes a support structure 421 extending along the first direction and an insulating layer 422 located on opposite sides of the support structure 421 along the second direction.

[0119] 4 b , steps 103 and 104 are performed to form a word line opening 431 extending along a third direction in the isolation structure 420, and to form an insulating structure 423 between the word line opening 431 and the substrate 400. The specific process is as follows: the isolation structure 420 is etched along the third direction to form a word line opening 431 exposing the side wall of the sub-stack structure 410, wherein the bottom surface of the word line opening 431 is lower than the bottom surface of the semiconductor layer 402 closest to the substrate 400 and higher than the bottom surface of the sub-stack structure 410; when the word line opening 431 is formed, the insulating layer remaining between the bottom surface of the word line opening 431 and the substrate 400 constitutes the insulating structure 423.

[0120] Here, since the thickness of the dielectric layer 401 in the sub-stack structure 410 is generally thin, when forming the word line opening 431, the etching time and etching uniformity can be controlled so that the bottom surface of the word line opening 431 is lower than the bottom surface of the semiconductor layer 402 closest to the substrate 400 and higher than the bottom surface of the sub-stack structure 410.

[0121] 4 c , step 105 is performed to form a word line structure 440 in the word line opening 431 . The word line structure 440 includes a gate dielectric layer 441 and a gate layer 442 .

[0122] In the embodiment of the present disclosure, a bottom surface of the word line structure 440 is lower than a bottom surface of the semiconductor layer 402 closest to the substrate 400 , and is higher than a bottom surface of the sub-stack structure 410 .

[0123] In the embodiment of the present disclosure, the insulating structure 423 is located between the bottom surface of the word line structure 440 and the substrate 400, thereby increasing the distance between the bottom of the word line structure 440 and the substrate 400. As a result, the coupling effect between the word line structure 440 and the substrate 400 can be reduced, the parasitic capacitance between the word line structure 440 and the substrate 400 can be reduced, and the generation of a leakage channel between the word line structure 440 and the substrate 400 can be avoided, thereby effectively improving the reliability of the semiconductor structure.

[0124] Based on the same technical concept as the aforementioned method for forming a semiconductor structure, an embodiment of the present disclosure provides a semiconductor structure. Figures 2i, 3d, and 4c are cross-sectional views of the semiconductor structure provided in the ZY plane according to an embodiment of the present disclosure, wherein the semiconductor structure shown in Figure 2i is obtained by the method for forming the semiconductor structure shown in Figures 1 and 2a to 2i, the semiconductor structure shown in Figure 3d is obtained by the method for forming the semiconductor structure shown in Figures 1 and 3a to 3d, and the semiconductor structure shown in Figure 4c is obtained by the method for forming the semiconductor structure shown in Figures 1 and 4a to 4c.

[0125] As shown in Figure 2i, the semiconductor structure includes: a substrate 200 and a stacking structure located on the substrate 200, the stacking structure including alternating dielectric layers 201 and semiconductor layers 202; an isolation structure 220, the isolation structure 220 extends along a first direction and penetrates the stacking structure and extends into the substrate 200, the isolation structure 220 separates the stacking structure into a plurality of sub-stack structures 210 arranged along a second direction; a word line structure 250, the word line structure 250 extends along a third direction and is located between the sub-stack structure 210 and the isolation structure 220, the bottom surface of the word line structure 250 is lower than the bottom surface of the semiconductor layer 202 closest to the substrate 200; and an insulating structure 240, the insulating structure 240 is located between the word line structure 250 and the substrate 200.

[0126] In some embodiments, the substrate 200 can be a single semiconductor material substrate (for example, a silicon substrate, a germanium substrate, etc.), a compound semiconductor material substrate (for example, a germanium silicon substrate, etc.), or a silicon-on-insulator (SOI) substrate, a germanium-on-insulator (GeOI) substrate, etc.

[0127] In some embodiments, the material of the dielectric layer 201 can be one of dielectric materials such as silicon oxide, silicon nitride, silicon oxynitride, and silicon carbide nitride; the material of the semiconductor layer 202 can be one of semiconductor materials such as silicon, germanium, and indium gallium zinc oxide.

[0128] In the embodiment of the present disclosure, the first direction is the X direction, the second direction is the Y direction, and the third direction is the Z direction, and the third direction is the thickness direction of the substrate 200 .

[0129] In the embodiment of the present disclosure, the isolation structure 220 includes a support structure 221 extending along a first direction and an insulating layer 222 located on opposite sides of the support structure 221 along a second direction, and the insulating layer 222 is in contact with the bottom end of the insulating structure 240; the word line structure 250 is located between the support structure 221 and the sub-stack structure 210, and is located above the insulating layer 222; the bottom surface of the word line structure 250 is higher than the bottom surface of the isolation structure 220, and lower than the bottom surface of the semiconductor layer 202 of the sub-stack structure 210 closest to the substrate 200.

[0130] In a specific example, the material of the support structure 221 is silicon nitride, and the material of the insulating layer 222 is silicon oxide.

[0131] In the embodiment of the present disclosure, the insulating structure 240 is located between the side wall of the word line structure 250 and the substrate 200. As shown in Figure 2i, the insulating structure 240 protrudes from the side wall of the word line structure 250 toward the interior of the substrate 200. In the direction from the word line structure 250 toward the substrate 200, the size of the insulating structure 240 in the third direction decreases.

[0132] In the embodiment of the present disclosure, the insulating structure 240 is composed of nitrogen and / or oxygen, and the insulating structure 240 has a higher insulating property than the substrate 200 .

[0133] In the embodiment of the present disclosure, the size of the portion of the word line structure 250 below the top surface of the substrate 200 in the second direction is larger than the size of the portion of the word line structure 250 above the top surface of the substrate 200 in the second direction. Thus, the resistance of the portion of the word line structure 250 below the top surface of the substrate 200 can be reduced, and the voltage drop caused by this portion during actual operation can be reduced, thereby improving the reliability of the semiconductor structure.

[0134] In the embodiment of the present disclosure, the word line structure 250 includes a gate dielectric layer 251 and a gate layer 252 ; the gate dielectric layer 251 is located between the gate layer 252 and the semiconductor layer 202 .

[0135] In some embodiments, the material of the gate dielectric layer 251 may be at least one of a high-k dielectric material, silicon oxide, silicon nitride, and silicon oxynitride. The high-k dielectric material may be at least one of hafnium oxide, hafnium silicon oxide, lanthanum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, lithium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.

[0136] In some embodiments, the material of the gate layer 252 can be at least one of a doped semiconductor material (e.g., doped polysilicon, doped germanium, etc.), a conductive metal nitride (e.g., titanium nitride, tantalum nitride, etc.), a metal material (e.g., tungsten, titanium, tantalum, etc.), and a metal semiconductor compound (e.g., tungsten silicide, cobalt silicide, titanium silicide, etc.).

[0137] In the embodiment of the present disclosure, the semiconductor layer 202 in the sub-stack structure 210 includes an active structure, which includes a source region, a channel region, and a drain region arranged in sequence along a first direction. The word line structure 250 is located on opposite sides of the channel region along a second direction, and constitutes a transistor structure with the active structure.

[0138] In the semiconductor structure provided by the embodiment of the present disclosure, an insulating structure 240 is arranged between the word line structure 250 and the substrate 200. The insulating property of the insulating structure 240 is higher than that of the substrate 200. The insulating structure 240 protrudes from the side wall of the word line structure 250 toward the inside of the substrate 200. The distance between the side wall of the gate layer 252 and the substrate 200 is large, which can avoid the generation of large parasitic capacitance and leakage channel between the word line structure 250 and the substrate 200. Therefore, the semiconductor structure has high reliability.

[0139] As shown in Figure 3d, the semiconductor structure includes: a substrate 300 and a stacking structure located on the substrate 300, the stacking structure including alternating dielectric layers 301 and semiconductor layers 302; an isolation structure 320, the isolation structure 320 extends along a first direction and penetrates the stacking structure and extends into the substrate 300, the isolation structure 320 separates the stacking structure into a plurality of sub-stack structures 310 arranged along a second direction; a word line structure 350, the word line structure 350 extends along a third direction and is located between the sub-stack structure 310 and the isolation structure 320, the bottom surface of the word line structure 350 is lower than the bottom surface of the semiconductor layer 302 closest to the substrate 300; and an insulating structure 340, the insulating structure 340 is located between the word line structure 350 and the substrate 300.

[0140] In the embodiment of the present disclosure, the isolation structure 320 includes a support structure 321 extending along a first direction and an insulating layer 322 located on opposite sides of the support structure 321 along a second direction, and the insulating layer 322 is in contact with the bottom end of the insulating structure 340; the word line structure 350 is located between the support structure 321 and the sub-stack structure 310, and is located above the insulating layer 322; the bottom surface of the word line structure 350 is higher than the bottom surface of the isolation structure 320, and lower than the bottom surface of the semiconductor layer 302 of the sub-stack structure 310 closest to the substrate 300.

[0141] In the embodiment of the present disclosure, the insulating structure 340 is located between the side wall of the word line structure 350 and the substrate 300. As shown in Figure 3d, the insulating structure 340 protrudes from the side wall of the word line structure 350 toward the interior of the substrate 300. In the direction from the word line structure 350 toward the substrate 300, the size of the insulating structure 340 in the third direction decreases.

[0142] In the embodiment of the present disclosure, the material of the insulating structure 340 is silicon oxide and / or silicon nitride.

[0143] In the embodiment of the present disclosure, the word line structure 350 includes a gate dielectric layer 351 and a gate layer 352 ; the gate dielectric layer 351 is located between the gate layer 352 and the semiconductor layer 302 .

[0144] In the embodiment of the present disclosure, the semiconductor layer 302 in the sub-stack structure 310 includes an active structure, which includes a source region, a channel region, and a drain region arranged in sequence along a first direction. The word line structure 350 is located on opposite sides of the channel region along a second direction, and constitutes a transistor structure with the active structure.

[0145] In the semiconductor structure provided by the embodiment of the present disclosure, an insulating structure 340 is arranged between the word line structure 350 and the substrate 300. The insulating property of the insulating structure 340 is higher than that of the substrate 300. The insulating structure 340 protrudes from the side wall of the word line structure 350 toward the inside of the substrate 300. The distance between the side wall of the gate layer 352 and the substrate 300 is large, which can avoid the generation of large parasitic capacitance and leakage channel between the word line structure 350 and the substrate 300. The semiconductor structure has high reliability.

[0146] As shown in Figure 4c, the semiconductor structure includes: a substrate 400 and a stacking structure located on the substrate 400, the stacking structure including alternating dielectric layers 401 and semiconductor layers 402; an isolation structure 420, the isolation structure 420 extends along a first direction and penetrates the stacking structure and extends into the substrate 400, the isolation structure 420 separates the stacking structure into a plurality of sub-stack structures 410 arranged along a second direction; a word line structure 440, the word line structure 440 extends along a third direction and is located between the sub-stack structure 410 and the isolation structure 420, the bottom surface of the word line structure 440 is lower than the bottom surface of the semiconductor layer 402 closest to the substrate 400; and an insulating structure 423, the insulating structure 423 is located between the word line structure 440 and the substrate 400.

[0147] In the embodiment of the present disclosure, the word line structure 440 includes a gate dielectric layer 441 and a gate layer 442 , and the gate dielectric layer 441 is located between the gate layer 442 and the semiconductor layer 402 .

[0148] In the embodiment of the present disclosure, the bottom surface of the word line structure 440 is higher than the bottom surface of the sub-stack structure 410 ; the insulating structure 423 is located between the bottom surface of the word line structure 440 and the substrate 400 .

[0149] In the semiconductor structure provided in the embodiment of the present disclosure, an insulating structure 423 is arranged between the bottom surface of the word line structure 440 and the substrate 400. The distance between the bottom surface of the word line structure 440 and the substrate 400 is large, which can avoid the generation of large parasitic capacitance and leakage channels between the word line structure 440 and the substrate 400. Therefore, the semiconductor structure has high reliability.

[0150] The embodiments of the present disclosure provide a semiconductor structure and a method for forming the same, which effectively improve the reliability of the semiconductor structure.

[0151] In the disclosed embodiment, a plurality of isolation structures are first formed in the stack structure, extending along a first direction, penetrating the stack structure, and extending into the substrate. The isolation structures separate the stack structure into a plurality of sub-stack structures arranged in a second direction. Then, wordline openings extending along a third direction are formed in the isolation structures. An insulating structure is formed between the wordline openings and the substrate, and a wordline structure is formed in the wordline openings, thereby forming an insulating structure between the wordline structure and the substrate. The provision of the insulating structure increases the distance between the gate layer in the wordline structure and the substrate, thereby reducing the coupling effect between the wordline structure and the substrate, avoiding the generation of large parasitic capacitance and leakage channels between the wordline structure and the substrate, and improving the reliability of the semiconductor structure.

[0152] The methods disclosed in the several method embodiments provided in this disclosure can be arbitrarily combined without conflict to obtain new method embodiments.

[0153] The features disclosed in the several device embodiments provided in this disclosure can be arbitrarily combined without conflict to obtain new device embodiments.

[0154] The above description is merely a specific embodiment of the present disclosure, but the scope of protection of the present disclosure is not limited thereto. Any changes or substitutions that can be easily conceived by a person skilled in the art within the technical scope disclosed in this disclosure should be included in the scope of protection of the present disclosure. Therefore, the scope of protection of the present disclosure should be based on the scope of protection of the claims.

Claims

1. A method for forming a semiconductor structure, comprising: A stacking structure (101) in which dielectric layers (201, 301, 401) and semiconductor layers (202, 302, 402) are alternately stacked is formed on a substrate (200, 300, 400); A plurality of isolation structures (220, 320, 420) extending along a first direction (X) and penetrating the stacking structure and extending into the substrate (200, 300, 400) are formed; the isolation structures (220, 320, 420) separate the stacking structure into a plurality of sub-stacking structures (210, 310, 410) (102) arranged along a second direction (Y); the first direction (X) is perpendicular to the second direction (Y), and both are perpendicular to a third direction (Z), and the third direction (Z) is the thickness direction of the substrate (200, 300, 400); A word line opening (233, 333, 431) extending along the third direction (Z) is formed in the isolation structure (220, 320, 420); a bottom surface of the word line opening (233, 333, 431) is lower than a bottom surface of the semiconductor layer (202, 302, 402) closest to the substrate (200, 300, 400), and the word line opening (233, 333, 431) is located between the sub-stack structure (210, 310, 410) and the isolation structure (220, 320, 420) (103); forming an insulating structure (240, 340, 423) (104) between the word line opening (233, 333, 431) and the substrate (200, 300, 400); A word line structure (250, 350, 440) (105) is formed in the word line opening (233, 333, 431).

2. The method for forming a semiconductor structure according to claim 1, wherein: The isolation structure (220, 320, 420) comprises a support structure (221, 321, 421) extending along the first direction (X) and an insulating layer (222, 322, 422) located on two opposite sides of the support structure (221, 321, 421) along the second direction (Y); a word line opening (233, 333, 431) extending along the third direction (Z) is formed in the isolation structure (220, 320, 420), comprising: Performing a first etching on the insulating layer (222) along the third direction (Z) to form an initial opening (231) exposing a portion of the sidewalls of the support structure (221) and the sidewalls of the sub-stack structure (210); the bottom surface of the initial opening (231) is lower than the bottom surface of the semiconductor layer (202) of the sub-stack structure (210) closest to the substrate (200); forming a barrier layer (232) on the sidewall of the initial opening (231); The insulating layer (222) is secondly etched along the third direction (Z) through the initial opening (231) to form the word line opening (233); the side wall of the word line opening (233) exposes the substrate (200); the bottom surface of the word line opening (233) is higher than the bottom surface of the isolation structure (220) and lower than the bottom surface of the sub-stack structure (210).

3. The method for forming a semiconductor structure according to claim 2, wherein: The insulating structure (240, 340, 423) is formed between the word line opening (233, 333, 431) and the substrate (200, 300, 400), comprising: The substrate (200) exposed by the sidewall of the word line opening (233) is doped to form the insulating structure (240); the insulating structure (240) protrudes from the sidewall of the word line opening (233) toward the inside of the substrate (200).

4. The method for forming a semiconductor structure according to claim 1, wherein: The sidewall of the word line opening (333) exposes the substrate (300); the bottom surface of the word line opening (333) is higher than the bottom surface of the isolation structure (320) and lower than the bottom surface of the sub-stack structure (310); the isolation structure (220, 320, 420) comprises a support structure (221, 321, 421) extending along the first direction (X) and an insulating layer (222, 322, 422) located on two opposite sides of the support structure (221, 321, 421) along the second direction (Y); the insulating structure (240, 340, 423) is formed between the word line opening (233, 333, 431) and the substrate (200, 300, 400), comprising: Etching the substrate (300) exposed by the sidewall of the word line opening (333) to form a groove (334) protruding from the word line opening (333) toward the inside of the substrate (300); The groove (334) is filled with an insulating material to form the insulating structure (340).

5. The method for forming a semiconductor structure according to claim 1, wherein: The method comprises forming a word line opening (233, 333, 431) extending along the third direction (Z) in the isolation structure (220, 320, 420) and forming an insulating structure (240, 340, 423) between the word line opening (233, 333, 431) and the substrate (200, 300, 400), comprising: Etching the isolation structure (420) along the third direction (Z) to form a word line opening (431) exposing the side wall of the sub-stack structure (410), wherein the bottom surface of the word line opening (431) is higher than the bottom surface of the sub-stack structure (410); When the word line opening (431) is formed, the isolation structure (420) between the bottom of the word line opening (431) and the substrate (400) constitutes the insulation structure (423).

6. The method for forming a semiconductor structure according to claim 3, wherein: The step of doping the substrate (200) exposed by the sidewall of the word line opening (233) comprises: using a plasma nitriding process to perform angled nitrogen doping on the substrate (200) exposed by the sidewall of the word line opening (233).

7. The method for forming a semiconductor structure according to any one of claims 1 to 5, wherein: The word line structure (250, 350, 440) is formed in the word line opening (233, 333, 431), comprising: A gate dielectric layer (251, 351, 441) and a gate layer (252, 352, 442) are sequentially formed in the word line opening (233, 333, 431); the gate dielectric layer (251, 351, 441) is located between the gate layer (252, 352, 442) and the semiconductor layer (202, 302, 402).

8. The method for forming a semiconductor structure according to any one of claims 1 to 5, wherein: The method for forming the semiconductor structure further includes: An active structure is formed in the semiconductor layer (202, 302, 402) of the sub-stack structure (210, 310, 410); the active structure and the word line structure (250, 350, 440) form a transistor structure.

9. A semiconductor structure comprising: A substrate (200, 300, 400) and a stacked structure located on the substrate (200, 300, 400); the stacked structure comprises alternately stacked dielectric layers (201, 301, 401) and semiconductor layers (202, 302, 402); An isolation structure (220, 320, 420), the isolation structure (220, 320, 420) extending along a first direction (X) and penetrating the stacking structure and extending into the substrate (200, 300, 400); The isolation structure (220, 320, 420) separates the stack structure into a plurality of sub-stack structures (210, 310, 410) arranged along the second direction (Y); The first direction (X) is perpendicular to the second direction (Y), and both are perpendicular to a third direction (Z), and the third direction (Z) is the thickness direction of the substrate (200, 300, 400); A word line structure (250, 350, 440), the word line structure (250, 350, 440) extending along the third direction (Z); a bottom surface of the word line structure (250, 350, 440) is lower than a bottom surface of the semiconductor layer (202, 302, 402) closest to the substrate (200, 300, 400), and the word line structure (250, 350, 440) is located between the sub-stack structure (210, 310, 410) and the isolation structure (220, 320, 420); An insulating structure (240, 340, 423) is located between the word line structure (250, 350, 440) and the substrate (200, 300, 400).

10. The semiconductor structure according to claim 9, wherein: The isolation structure (220, 320, 420) comprises a support structure (221, 321, 421) extending along the first direction (X) and an insulating layer (222, 322, 422) located on two opposite sides of the support structure (221, 321, 421) along the second direction (Y); the word line structure (250, 350, 440) is located between the support structure (221, 321, 421) and the sub-stack structure (210, 310, 410), and is located on the insulating layer (222, 322, 422).

11. The semiconductor structure according to claim 10, wherein: The insulating layer (222, 322) contacts the bottom end of the insulating structure (240, 340).

12. The semiconductor structure according to claim 9, wherein: The bottom surface of the word line structure (250, 350, 440) is higher than the bottom surface of the isolation structure (220, 320, 420) and lower than the bottom surface of the semiconductor layer (202, 302, 402) of the sub-stack structure (210, 310, 410) closest to the substrate (200, 300, 400).

13. The semiconductor structure according to claim 12, wherein: The insulating structure (240, 340) is located between the side wall of the word line structure (250, 350) and the substrate (200, 300); the insulating structure (240, 340) protrudes from the side wall of the word line structure (250, 350) into the interior of the substrate (200, 300).

14. The semiconductor structure according to claim 13, wherein: Along the second direction (Y), in a direction from the word line structure (250, 350) toward the substrate (200, 300), the size of the insulating structure (240, 340) in the third direction (Z) decreases.

15. The semiconductor structure according to claim 9, wherein: The bottom surface of the word line structure (440) is higher than the bottom surface of the sub-stack structure (410); and the insulating structure (423) is located between the bottom surface of the word line structure (440) and the substrate (400).

16. The semiconductor structure according to claim 9, wherein: The constituent elements of the insulating structure (240, 340, 423) include nitrogen and / or oxygen.

17. The semiconductor structure according to any one of claims 9 to 16, wherein: The word line structure (250, 350, 440) comprises a gate dielectric layer (251, 351, 441) and a gate layer (252, 352, 442); the gate dielectric layer (251, 351, 441) is located between the gate layer (252, 352, 442) and the semiconductor layer (202, 302, 402).

18. The semiconductor structure according to any one of claims 9 to 16, wherein: The semiconductor layer (202, 302, 402) includes an active structure; the active structure and the word line structure (250, 350, 440) form a transistor structure.

19. The semiconductor structure according to any one of claims 9 to 14, wherein: The insulating structure (240, 340) is located below the sub-stack structure (210, 310), and the top of the insulating structure (240, 340) contacts the bottom surface of the dielectric layer (201, 301) closest to the substrate (200, 300) in the sub-stack structure (210, 310).

20. The semiconductor structure of claim 19, wherein: The bottom end of the insulating structure (240, 340) is lower than the bottom surface of the word line structure (250, 350).

Citation Information

Patent Citations

  • Vertical memory devices having charge storage layers and method for manufacturing same

    CN105845689A

  • Three-dimensional memory and method for forming three-dimensional memory

    CN110349965A

  • Semiconductor structure and forming method thereof

    CN114975286A

  • Three-dimensional memory device containing inter-select-gate electrodes and methods of making the same

    US20210305384A1