Friction joining device and friction joining method
The friction welding device addresses torque-related defects by using current limiting mechanisms to manage torque loads during friction heating, improving bonding accuracy and detecting issues, thus enhancing the overall quality and reliability of the welding process.
Patent Information
- Application Number
- PCT/JP2024/014089
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-10
- Filing Date
- 2024-04-05
- Publication Date
- 2024-10-17
AI Technical Summary
Friction welding processes face defects and equipment failures due to high torque loads during the joining of workpieces, leading to poor bonding and potential damage to the clamp chuck, which existing monitoring methods struggle to detect effectively.
A friction welding device with current limiting means that controls the current flowing through the drive sources during specific phases of the friction heating process, setting different limit values for the initial and subsequent friction heating periods to manage torque loads and prevent workpiece rotation, thereby improving bonding accuracy and detecting potential defects.
This approach effectively suppresses defects in friction welding, enhances the accuracy of determining the welding state, and prevents equipment damage by stabilizing torque loads and monitoring for abnormal droop in the friction heating process.
Smart Images

Figure JP2024014089_17102024_PF_FP_ABST
Abstract
Description
Friction welding device and friction welding method
[0001] The present invention relates to a friction welding device for friction welding two workpieces together.
[0002] A conventional method for effectively utilizing leftover material from workpieces used in machine tools such as automatic lathes is to frictionally weld the leftover material to a new workpiece (see Patent Document 1). That is, when the leftover bar material is too long to be machined into a workpiece, it is frictionally welded to a newly supplied bar material and used as material for the next processing step, thereby reducing material costs and the environmental impact.
[0003] Friction welding involves softening the sliding portions of two workpieces with frictional heat generated at their sliding contact points, and then joining the sliding portions by stopping the relative rotation of the sliding portions while applying pressure, thereby joining the two workpieces together. Specifically, a first workpiece (a new bar material to be used in the next process) held by the main spindle (first spindle) and a second workpiece (a remnant material left over from the previous process) held by the back spindle (second spindle) are rotated relative to each other. The axial distance between the spindles is then narrowed, and the opposing end faces of the first and second workpieces are pressed against each other and slid against each other, generating frictional heat in the sliding portions. Once the joint has been sufficiently softened by friction, the relative rotation between the spindles is stopped while maintaining pressure. When the rotation is stopped and the heat subsides, the sliding portions solidify in a bonded state, and the remnant material and the new material are integrally joined.
[0004] Here, a large torque load is generated in the drive mechanism that drives the spindle when workpieces rotating at high speed come into contact with each other. This large torque load can cause various problems, such as poor workpiece bonding and equipment failure. For example, when the workpieces are rotating relative to each other, the remaining workpiece on the back spindle side, which is stopped, starts to rotate along with the workpiece on the front spindle side, causing the remaining workpiece and the clamp chuck that grips it to seize, resulting in damage to the clamp chuck.
[0005] Patent Literature 2 discloses a method for monitoring whether the active power supplied from an external power supply to a system power supply is within a predetermined numerical tolerance range set for each process, and determining whether an abnormality has occurred and whether the joining condition of the joint is good or bad. In particular, in the latter half of the process, from when the joint melts until rotation stops, the quality of the joint is determined based on a differential signal obtained by subtracting the moving average of the active power output value. However, even if power values are monitored in this manner, it may be difficult to detect the occurrence of the above-mentioned malfunctions.
[0006] JP 2000-202648 A JP 2009-082951 A
[0007] An object of the present invention is to provide a technology that can suppress the occurrence of defects in friction welding and improve the accuracy of determining whether the welding state is good or bad.
[0008] In order to achieve the above object, the friction welding device of the present invention comprises: a first spindle that grips a first workpiece; a second spindle that grips a second workpiece so as to face the first workpiece in the axial direction; a first drive mechanism having a first drive source and moving the first spindle in the axial direction by the drive force of the first drive source; a second drive mechanism having a second drive source and moving the second spindle in the axial direction by the drive force of the second drive source; a rotation drive mechanism that rotates the first workpiece and the second workpiece relatively about a rotation axis along the axial direction; control means that controls the first drive mechanism, the second drive mechanism, and the rotation drive mechanism so as to bring the first workpiece and the second workpiece into contact with each other while rotated relatively, thereby welding the first workpiece and the second workpiece; and current limiting means that limit the current flowing through the first drive source and the second drive source to a predetermined limit value or less. The current limiting means limits the current flowing through the first driving source and the second driving source during a first frictional heating period, which is a predetermined period starting immediately after the first workpiece and the second workpiece come into contact, to a first limit value or less that is smaller than a second limit value for limiting the current flowing through the first driving source and the second driving source during a second frictional heating period after the first frictional heating period has elapsed.
[0009] According to the present invention, it is possible to suppress the occurrence of defects in friction welding and improve the accuracy of determining whether the welding state is good or bad.
[0010] Fig. 4 is an explanatory diagram of the configuration of a friction welding device according to an embodiment of the present invention; Fig. 5 is an explanatory diagram of the friction welding device according to an embodiment of the present invention during friction welding operation; Fig. 6 is a diagram showing a change in load over time during friction welding operation in which a malfunction has occurred; Fig. 7 is a diagram showing a change in load over time during friction welding operation in an embodiment of the present invention; Fig. 8 is a diagram showing a droop related to the relative position of the spindle corresponding to Fig. 4; Fig. 9 is a flow chart of a friction welding process in an embodiment of the present invention;
[0011] Preferred embodiments of the present invention will be described below with reference to the drawings. However, the embodiments described below merely exemplify preferred configurations of the present invention and are not intended to limit the scope of the present invention to those configurations. Furthermore, unless otherwise specified, the hardware and software configurations of the device, manufacturing conditions, component functions, materials, shapes, and relative locations thereof in the following description are not intended to limit the scope of the present invention to those specifics. In addition, identical components are generally designated by the same reference numerals, and repeated explanations will be omitted.
[0012] (Example) Figure 1 is a schematic diagram showing the configuration of a machine tool 1 as a friction joining device according to an example embodiment of the present invention. The machine tool 1 shown in Figure 1 is a so-called automatic lathe device that performs cutting (turning) by rotating a workpiece W, such as a long bar, and applying a cutting tool (machining tool) to the workpiece. The machine tool 1 according to this example embodiment is configured so that it can also be used as a friction joining device that, once it has been able to cut out as much of the machined workpiece as possible from one workpiece W, joins the remaining workpiece W2 to a newly supplied workpiece W1.
[0013] The machine tool 1 generally includes a first spindle mechanism (front spindle mechanism) 100 and a second spindle mechanism (back spindle mechanism) 200, which are arranged opposite each other on a base (not shown), and a tool rest (not shown). The first spindle mechanism 100 has a first spindle (front spindle) 101, and the second spindle mechanism 200 has a second spindle (back spindle) 201, with these two spindles arranged so that their axes are approximately concentric or parallel to each other. The direction of their axes is defined as the Z-axis direction, and among directions perpendicular to the axial directions, a direction parallel to the vertical direction is defined as the X-axis direction, and a direction parallel to the horizontal direction is defined as the Y-axis direction. FIG. 1 is a schematic diagram of the configuration of the machine tool 1 as viewed from above in the Y-axis direction.
[0014] The first spindle mechanism 100 includes a first drive mechanism GZ1 for moving a first headstock 102, which rotatably supports the first spindle 101, in the Z-axis direction on a base. The first drive mechanism GZ is a ball screw drive mechanism that includes a first motor MZ1 (servo motor) as a first drive source, a ball screw, a guide rail, etc. By driving and rotating the ball screw drive mechanism with the first motor MZ1, the first spindle 101 can be moved in the axial direction (Z-axis direction) together with the first headstock 102.
[0015] The second spindle mechanism 200 also includes a second drive mechanism GZ2 for moving a second headstock 202, which rotatably supports the second spindle 201, in the Z-axis direction on a base. The second drive mechanism GZ2 is a ball screw drive mechanism that includes a second motor MZ2 as a second drive source, a ball screw, a guide rail, etc. By driving and rotating the ball screw drive mechanism with the second motor MZ2, the second spindle 201 can be moved in the axial direction (Z-axis direction) together with the second headstock 202.
[0016] The mechanism that enables the first spindle mechanism 100 and the second spindle mechanism 200 to move relatively in the Z-axis direction, which is the direction of the rotation axis of the spindles, is not limited to a specific configuration, and the configuration described above is merely one example. Also, a drive mechanism may be provided that moves the first headstock 102 and the second headstock 202 not only in the Z-axis direction, but also in the Y-axis direction or the X-axis direction.
[0017] The first headstock 102 is configured to have a rotation drive mechanism, such as a first built-in motor MR1 as a rotation drive source, and to rotate the first spindle 101 using the rotation drive force. Similarly, the second headstock 202 is configured to rotate the second spindle 201 using the rotation drive force provided by a second built-in motor MR2 as a rotation drive source. However, when the machine tool 1 is used as a friction welding device (described later), in this embodiment, the friction welding process is performed with the second spindle 201 stationary and not rotating. Note that the configuration is not limited to the above, as long as it can maintain a predetermined relative rotation state between the first workpiece and the second workpiece during friction welding. In other words, both the first spindle 101 and the second spindle 201 may be rotated, or the second spindle 201 may be rotated without rotating the first spindle 101. Furthermore, the power source configuration is not limited to a built-in motor, but may be configured to transmit a rotational driving force from an external power source to rotate the device.
[0018] The first spindle 101 has a hollow structure with a workpiece holding hole for holding or gripping the workpiece W1 as the first workpiece, and is equipped with a first chuck 103 and a chuck sleeve (not shown) for holding the workpiece W1 (a state in which the axial center of the workpiece W1 in the first spindle 101 is determined and axial movement is restricted). The workpiece holding hole opens axially toward the second spindle, and the portion of the workpiece W1 exposed from the opening is the portion that is turned by a cutting tool supported on a tool post (not shown). A guide bush, which is a support structure for the workpiece W1, may be arranged in front of the first spindle 101.
[0019] The first chuck 103 and the chuck sleeve (not shown) are configured such that the chuck sleeve is joined to the first chuck 103, whose axial movement is restricted, from the rear via a tapered surface. The chuck sleeve attempts to move in the axial direction by receiving force from a fluid cylinder (not shown) driven by hydraulic pressure, air, or the like, and applies a force including a component force toward the axis to the first chuck 103, generating a clamping force in the chuck that closes the slits provided in the first chuck 103. This creates a state in which the workpiece W1 is gripped.
[0020] The configuration on the second spindle 201 side is similar to the configuration on the first spindle 101 side, and includes a second chuck 203, a chuck sleeve, etc., and is configured to be able to grip and rotate a workpiece W2 as a second workpiece. The basic configuration is similar to that of a conventionally known back spindle configuration. When the machine tool 1 is used as a friction welding device, the workpiece W2 gripped by the second spindle 201 is a workpiece that is a remnant material remaining after the workpiece is gripped by the first spindle 101 and turned by the cutting tool 301 of the tool rest 300.
[0021] The machine tool 1 includes a tool rest 300 equipped with a cutting tool 301 for cutting, and a drive mechanism 302 that moves the tool rest 300. The tool rest 300 and the cutting tool 301 are configured to be movable at least in the cutting direction (X-axis direction) and the feed direction (Z-axis direction) by driving the drive mechanism 302. When used as a cutting device, the machine tool 1 can perform cutting on the workpiece W by bringing the cutting tool 301 into contact with the workpiece W that is being rotated at a predetermined processing rotation speed corresponding to the cutting.
[0022] The workpieces W to be cut include the first workpiece W1 held by the first spindle 101, the second workpiece W2 held by the second spindle 201, and the third workpiece W3 formed by friction welding the first workpiece W1 and the second workpiece W2 as a remnant material.
[0023] A plurality of cutting tools 301 may be prepared and selectable depending on the type of processing to be performed. That is, the tool rest 300 is provided with a plurality of cutting tools 301, and a selected one of the cutting tools 301 is brought into contact with the workpiece W to perform the desired cutting processing (turning processing) on the workpiece.
[0024] Machine tool 1 includes a control unit 4 as control means for controlling the operations of the various parts that make up machine tool 1, such as spindle mechanisms 100, 200, tool rest 300, and a work supply unit (not shown). Control unit 4 can be configured, for example, by a computer equipped with a processor such as a CPU (Central Processing Unit) and storage means such as a memory.
[0025] A first ammeter 410 serving as a current detection means is connected to the first motor MZ1 of the first drive mechanism GZ1. Based on the current value (first current) of the first motor MZ1 detected by the first ammeter 410, the control unit 4 can detect the drive state of the first drive mechanism GZ1 and the load state (torque) of the first drive mechanism GZ1 during drive.
[0026] Similarly, an ammeter 420 serving as a current detection means is connected to the second motor MZ2 of the second drive mechanism GZ2. Based on the current value (second current) of the second motor MZ2 detected by the ammeter 420, the control unit 4 can detect the drive state of the second drive mechanism GZ2 and the load state (torque) of the second drive mechanism GZ2 during drive.
[0027] Furthermore, a first current limiter (filter circuit) 411 serving as current limiting means is connected to the first motor MZ1 of the first drive mechanism GZ1. The first current limiter 411 is configured to limit the current flowing through the first motor MZ1 to a predetermined limit value or less. This makes it possible to limit the torque generated by the first motor MZ1 to a predetermined torque or less, regardless of the operating status of the first drive mechanism GZ1. The first current limiter 411 is configured to be able to change the magnitude of the current limit value, and in this embodiment, the control unit 4 changes the magnitude of the current limit value set by the first current limiter 411 at a predetermined timing during the friction welding process (details will be described later).
[0028] Similarly, a second current limiter (filter circuit) 421 serving as current limiting means is connected to the second motor MZ2 of the second drive mechanism GZ2. The second current limiter 421 is configured to limit the current flowing through the second motor MZ2 to a predetermined limit value or less, thereby limiting the torque generated by the second motor MZ2 to a predetermined torque or less regardless of the operating status of the second drive mechanism GZ2. The second current limiter 421 is configured to be able to change the magnitude of the current limit value, and in this embodiment, the control unit 4 changes the magnitude of the current limit value set by the second current limiter 421 at a predetermined timing in the friction welding process (details will be described later).
[0029] 2(a) to 2(d) are schematic diagrams showing the state of friction welding of a first workpiece W1 and a second workpiece W2 by a machine tool 1 serving as a friction welding apparatus according to this embodiment. FIG. 2(a) is a diagram showing the state when relative rotation of the first workpiece W1 and the second workpiece W2 begins during friction welding. FIG. 2(b) is a diagram showing the state during the friction heating (friction heat generation) process during friction welding. FIG. 2(c) is a diagram showing the state during the upset pressure process during friction welding. FIG. 2(d) is a diagram showing the state at the end of the upset pressure process, i.e., when the first workpiece W1 and the second workpiece W2 are joined to form a third workpiece W3. Note that some components, such as the control unit 4 shown in FIG. 1, are not shown in FIGS. 2(a) to 2(d).
[0030] The machine tool 1, which serves as a friction welding device, softens the sliding portions of the two workpieces W1, W2 by using frictional heat generated at the sliding portions, and welds the sliding portions by applying pressure and stopping the relative rotation of the sliding portions, thereby integrally joining the two workpieces W1, W2. The workpiece W1 held by the first spindle 101 is a new bar stock prepared as a workpiece for the turning process performed after the friction welding process. On the other hand, the workpiece W2 held by the second spindle 201 is, as described above, a bar stock remaining from the turning process performed before the friction welding process.
[0031] 2(a), the first spindle 101 is rotated with the two workpieces W1 and W2 spaced apart in the Z-axis direction, which is the direction of the rotation axis. Once the rotation speed has stabilized at a predetermined rotation speed, the first spindle 101 is moved by the first drive mechanism GZ1 at a predetermined feed amount (movement amount per unit time) in the Z-axis direction so as to move closer to the second spindle 201. At the same time, the second spindle 201 is also moved by the second drive mechanism GZ2 at a predetermined feed amount in the Z-axis direction so as to move closer to the first spindle 101.
[0032] 2(b), the relative distance in the Z-axis direction between the first spindle 101 and the second spindle 201 is maintained so that the opposing end faces of the first workpiece W1 and the second workpiece W2 are pressed against each other with a predetermined contact pressure, and the first workpiece W1 and the second workpiece W2 are caused to slide. In this frictional heating process, frictional heat is generated in the sliding portions of the first workpiece W1 and the second workpiece W2, causing the sliding portions to become softened.
[0033] The relative rotation between the first workpiece W1 and the second workpiece W2 is not limited to the relative rotation caused by stopping the second workpiece W2 and rotating only the first workpiece W1. The relative rotation may be caused by stopping the first workpiece W1 and rotating only the second workpiece W2. Alternatively, the relative rotation may be caused by rotating the first workpiece W1 and the second workpiece W2 in the same direction but at different rotational speeds. Furthermore, the relative rotation may be caused by rotating the first workpiece W1 and the second workpiece W2 in opposite directions but at different rotational speeds or at the same rotational speed.
[0034] 2(c), the friction sufficiently softens the sliding portion, forming a high-temperature softened portion J between the first workpiece W1 and the second workpiece W2. In this state, the rotation of the first spindle 101 (relative rotation between the spindles) is stopped while maintaining pressure between the first workpiece W1 and the second workpiece W2.
[0035] The rotation of the first spindle 101 is stopped when a position command amount (control amount) for the distance (relative position) in the Z-axis direction between the first headstock 102 and the second headstock 202 reaches a command amount corresponding to a preset position at which rotation of the first spindle 101 is to be stopped. For example, the distance in the Z-axis direction between the headstocks 102 and 202 may be obtained from the drive amount of the first drive mechanism GZ1 and the second drive mechanism GZ2 (ball screw drive mechanism), or the Z-axis positions of the headstocks and spindles may be directly detected using a position sensor or the like. The feed amounts (amount of movement per unit time) of the first headstock 102 and the second headstock 202 and the rotational speed of the first spindle 101 (relative rotational speed with respect to the second spindle 201) are obtained and set in advance through experiments or the like from the viewpoint of forming a softened portion J by the time the rotation stop position is reached.
[0036] Even after the rotation of the first spindle 101 has stopped, pressure continues to be applied between the first workpiece W1 and the second workpiece W2, pushing burrs outward in the softened portion J and performing upset pressure to strengthen the joined state of the first workpiece W1 and the second workpiece W2. In the upset pressure process (joining process), a higher pressure is applied between the first workpiece W1 and the second workpiece W2 than in the friction heating process, and the feed rates of the first spindle 101 and the second spindle 201 are controlled so that this pressurized state is maintained for a predetermined time. The feed rates of the first workpiece W1 and the second workpiece W2 during upset pressure application are set in advance taking into account the allowance (the length shortened by the amount that part of the first workpiece W1 and the second workpiece W2 is released as burrs during joining).
[0037] As shown in Figure 2(d), when the rotation stops, the heat at the joint dissipates and solidifies, resulting in the first workpiece W1 and the second workpiece W2 being joined together. This results in the formation of a third workpiece W3, which is a single bar of material that combines the remaining material and the new material. Any burrs that occur at the joint between the first workpiece W1 and the second workpiece W2 in the third workpiece W3 are removed by cutting using a cutting tool 301.
[0038] Here, in friction welding, a large torque load is generated on the spindle that rotates the workpiece W when the workpieces rotate at high speed come into contact with each other. When the workpieces come into contact with each other with a torque above a certain level, the remaining workpiece on the back spindle side, which is stopped in the relative rotation of the workpieces, starts to rotate along with the workpiece on the front spindle side, and the remaining workpiece and the clamp chuck that grips it may seize, causing damage to the clamp chuck.
[0039] This defect is particularly likely to become a problem when friction welding is performed using a machine tool (using a machine tool as a friction welding device), as in this embodiment. In a configuration in which the back spindle uses a clamp chuck to grip the remnant material, for example, when friction welding hollow metal pipes as workpieces, the workpieces cannot be gripped with a very strong chucking force due to concerns that this may affect the shape of the workpieces. In other words, there are cases in which a limit is set on the chucking force of the clamp chuck of the back spindle. As a result, there is a concern that the workpiece cannot be gripped with sufficient chucking force, resulting in the aforementioned co-rotation.
[0040] Fig. 3 is a time chart showing an example of the change over time in the loads applied to the first drive mechanism GZ1 and the second drive mechanism GZ2 during friction welding in a comparative example in which the motor current limiting control of the present invention, which will be described later, is not implemented. Fig. 3 also shows a time chart showing, as an example of a welding abnormality, the case in which the workpiece rotates together on the back spindle side as described above. In Fig. 3, the current flowing through the first motor MZ1 of the first drive mechanism GZ1 is indicated by a gray solid line, and the current flowing through the second motor MZ2 of the second drive mechanism GZ2 is indicated by a black solid line.
[0041] In Figure 3, time t0 indicates the timing when the first spindle 101 and the second spindle 201 start to move relative to each other in the Z-axis direction, and corresponds to the state shown in Figure 2(a). Time t1 indicates the timing when the opposing end faces of the first workpiece W1 and the second workpiece W2 come into contact with each other, i.e., the timing when the frictional heating process starts, and corresponds to the state shown in Figure 2(b). Time t2 indicates the timing when the relative rotation between the first workpiece W1 and the second workpiece W2 stops, i.e., the timing when the frictional heating process ends and the upset process starts. Times t0 to t2 shown in Figures 4 to 6 are defined in the same way. Each of these timings is preset based on the feed amount set for each process.
[0042] Here, time t2 is the timing when, if the process proceeds normally without the above-mentioned joining abnormality, the machine tool 1 and the workpieces W1 and W2 should be in the state shown in Fig. 2(b). However, in the friction heating process of the comparative example, the second workpiece W2 rotates together with the first workpiece W1, and the sliding portion between the first workpiece W1 and the second workpiece W2 is not melted sufficiently, so that at time t2, a sufficient softened portion J is not formed. Furthermore, as the second workpiece W2 and the second chuck 203 slide against each other due to the rotation, frictional heat is generated in the sliding portion, and depending on the degree of this heat, melting occurs in the sliding portion, resulting in a fused state (seizure state) between the workpieces.
[0043] As shown in FIG. 3 , during the frictional heating process, i.e., from the time when the workpieces W1 and W2 begin to come into contact (time t1) until their relative rotation stops (time t2), multiple peaks P1 to P4 are formed in the current flowing through the motors MZ1 and MZ2. If the frictional heating process proceeds normally, the current flowing through the motors MZ1 and MZ2 reaches its maximum peak immediately after the workpieces W1 and W2 come into contact. As heat is generated at the sliding portions of the workpieces W1 and W2, the current gradually stabilizes. Then, at time t2, the current suddenly drops as the softened portion J forms and the rotation of the first spindle 101 stops. In other words, the peaks P1 to P4 shown in FIG. 3 are abnormal current peaks that would not occur if the process proceeded normally. These peaks indicate the occurrence of, for example, co-rotation of the workpieces W1 and W2 or seizure between the second workpiece W2 and the second chuck 203.
[0044] Fig. 4 is a time chart showing an example of changes over time in the loads applied to the first drive mechanism GZ1 and the second drive mechanism GZ2 during friction welding operation in this embodiment. In Fig. 5, the current flowing through the first motor MZ1 of the first drive mechanism GZ1 is shown by a gray solid line, and the current flowing through the second motor MZ2 of the second drive mechanism GZ2 is shown by a black solid line.
[0045] In this embodiment, in order to suppress the occurrence of problems such as the workpiece dragging on the second spindle 201 (back spindle) side described above, stepwise torque limitation is performed on each of the first drive mechanism GZ1 and the second drive mechanism GZ2 during the friction heating process. That is, the first current limiter 411 controls stepwise the upper limit of the current flowing to the first motor MZ1 of the first drive mechanism GZ1, and the second current limiter 422 controls stepwise the upper limit of the current flowing to the second motor MZ2 of the second drive mechanism GZ2.
[0046] More specifically, in this embodiment, the current limit value IL1 during a predetermined period (t1 to ta) from the start of the friction heating process, i.e., during the predetermined period from when the first workpiece W1 and the second workpiece W2 come into contact, is set to a value smaller than the current limit value IL2 after the predetermined period.
[0047] During the first half period FH of the friction heating step, a large torque load is generated when the first workpiece W1 and the second workpiece W2 come into contact (time t1), and an unstable state occurs where the torque load fluctuates widely for a while thereafter. During the second half period SH, when heating of the sliding portion has progressed, the fluctuation range of the torque load settles to a certain extent (part SS in FIG. 5 ), and a relatively stable sliding state occurs until the relative rotation of the spindle is stopped. Therefore, a predetermined period (t1 to ta) from the start of the first half period FH is defined as a first frictional heating period Tf, and the period after the predetermined period of the first half period FH and the second half period SH are combined to define a second frictional heating period Ts, with the torque limit during the first frictional heating period Tf being set stricter than the torque limit during the second frictional heating period Ts.
[0048] The motor current limit value IL1 (first limit value) during the first frictional heating period Tf is set so that the torque load is suppressed to a level that does not cause the workpiece to rotate as described above. The current limit value IL1 may be set, for example, to a value similar to the peak value of the torque fluctuation portion (SS portion) during the latter half period SH. In this embodiment, the current limit value IL1 of the first motor MZ1 and the second motor MZ2 during the first frictional heating period Tf is set to 15% of their respective maximum rated currents.
[0049] The motor current limit value IL2 (second limit value) during the second frictional heating period Ts is set to a value greater than the current limit value IL1 during the first frictional heating period Tf, so as to efficiently promote frictional heating of the workpiece sliding portion while suppressing excessive torque load. The current limit value IL2 may be set to a value such that the peak value of the torque load fluctuation portion (SS portion) during the latter half period SH is not limited. In this embodiment, the current limit value IL2 of the first motor MZ1 and the second motor MZ2 during the second frictional heating period Ts is set to 20% of their respective maximum rated currents.
[0050] Due to the motor current limitation as described above, during the first frictional heating period Tf, the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a flat torque load (a constant current having the same magnitude as the current limit value IL1) limited by the current limit value IL1. Furthermore, during the second frictional heating period Ts, initially (a predetermined period from the start of the second frictional heating period Ts), the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a flat torque load (a constant current having the same magnitude as the current limit value IL2) limited by the current limit value IL2. Thereafter, as long as the process is proceeding normally, the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a torque load that is not subject to any particular limitation (a current not reaching the same magnitude as the current limit value IL2).
[0051] The motor current limit values shown here are merely examples and are set appropriately from the viewpoint of suppressing the occurrence of the above-mentioned problems and poor connections. The current limit values of the first motor MZ1 and the second motor MZ2 may be the same value or different values.
[0052] At the beginning of the friction heating process (first friction heating period Tf), the first workpiece W1 and the second workpiece W2 are brought into contact with each other with a torque load limited to prevent excessive torque load, and the first workpiece W1 and the second workpiece W2 begin to slide. Then, at a stage (second friction heating period Ts) when heating of the sliding portion has progressed to a certain extent, the torque limit is relaxed. That is, at the beginning of the process, the workpieces W1 and W2 are pressed together with a weak torque to prevent the occurrence of unstable behavior typical of the early stages of the process. After the sliding state stabilizes, the torque load limit is relaxed to promote thermal bonding. This makes it possible to prevent the workpiece W2 on the second spindle 201 (rear spindle) side from rotating together, or to prevent poor bonding.
[0053] In this embodiment, the motor current is detected at the timing of switching from the friction heating process to the upsetting process to detect whether or not droop that occurred during the friction heating process remains. In this embodiment, the first ammeter 410 and the second ammeter 420, which serve as current detection means, function as droop detection means. If droop remains, it is determined that some kind of abnormality has occurred during the friction heating process, a notification is sent to the user, and the subsequent processes are canceled.
[0054] Fig. 5 is a time chart showing an example of the change over time in droop (the difference between the commanded position amount of the spindles and the actual movement amount of the spindles) regarding the relative positions in the Z-axis direction of the first spindle 101 and the second spindle 201 in the friction heating process, and is a detection result in the friction welding operation of this embodiment shown in Fig. 5. In Fig. 6, the droop of the first drive mechanism GZ1 is shown by a gray solid line, and the droop of the second drive mechanism GZ2 is shown by a black solid line.
[0055] During the friction heating process, droop in the relative position of the first spindle 101 and the second spindle 201 in the Z-axis direction gradually accumulates due to the load generated at the sliding portion of the workpieces W1 and W2. However, this droop is resolved when the sliding portion is sufficiently softened. Therefore, as shown in FIG. 5 , if the friction heating process is completed normally without any welding abnormalities, the droop is ultimately resolved by the time the torque fluctuation portion SS shown in FIG. 4 is reached. This droop elimination is also reflected in the current fluctuation shown in FIG. 4 as a drop in the current value (P5) before the torque fluctuation portion SS. In other words, the motor current decreases as the load state is instantly resolved due to sufficient softening of the welded portion. This behavior ultimately results in the spindle position command amount and the actual movement amount of the spindle matching each other.
[0056] Therefore, in this embodiment, if the droop of the first drive mechanism GZ1 and the droop of the second drive mechanism GZ2 remain above a certain threshold value at the timing (time t2) when the relative rotation of the main shafts 101 and 201 stops, it can be determined that the friction welding process is not functioning normally.
[0057] The flow of the friction welding process of this embodiment will be described with reference to Fig. 6. Fig. 6 is a flow diagram of the friction welding process of this embodiment. The control units 4 mainly perform the controls described below.
[0058] The control unit 4 starts rotation of the first spindle 101 using the rotation drive mechanism (S101), and once that rotation has stabilized (S102), starts movement of the first headstock 102 and the second headstock 202 in the Z-axis direction using the drive mechanisms GZ1 and GZ2 (S103). At this time, the control unit 4 sets the current limit value IL1 of the motors MZ1 and MZ2 of each drive mechanism GZ1 and GZ2 to the first limit value described above. The control unit 4 also drives the motors MZ1 and MZ2 using a control target value (first control target value) for the feed rate of the first headstock 102 (the amount of movement in the Z-axis direction per unit time) as the first feed rate (first movement amount) and a control target value (second control target value) for the feed rate of the second headstock 202 as the second feed rate (second movement amount). By driving the drive mechanisms GZ1 and GZ2 and the rotary drive mechanism, the tip surfaces of the workpieces W1 and W2 held by the spindles 101 and 201 are pressed against each other and slide against each other.
[0059] Here, the first feed amount and the second feed amount may be the same or different, and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc.
[0060] During the first frictional heating period Tf, the control unit 4 continues frictional heating by limiting the torque at the first limit value (S104). The end of the first frictional heating period Tf may be determined by the time elapsed since the start of movement of the first headstock 102 and the second headstock 202 in the Z-axis direction reaching a preset end time of the first frictional heating period Tf. Alternatively, the end of the first frictional heating period Tf may be determined by the control amount (position command amount) of the movement of the first headstock 102 and the second headstock 202 in the Z-axis direction by each drive mechanism GZ1, GZ2 reaching a control amount corresponding to the end time of the first frictional heating period Tf.
[0061] When the first frictional heating period Tf ends and the second frictional heating period Ts begins, the control unit 4 changes the current limit values of the motors MZ1, MZ2 of the drive mechanisms GZ1, GZ2 from the first limit value to the above-mentioned second limit value (S105). At this time, the control unit 4 sets the control target value for the feed rate of the first headstock 102 to the third feed rate (third movement amount) and the control target value for the feed rate of the second headstock 202 to the fourth feed rate (fourth movement amount), and drives the motors MZ1, MZ2, respectively.
[0062] Here, the third feed amount and the fourth feed amount may be the same or different, and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc.
[0063] Furthermore, the third feed amount may be the same as or different from the first feed amount. Typically, the third feed amount is set to an amount larger than the first feed amount, but depending on the joining conditions, it may be set to remain the same as the first feed amount or to be smaller than the first feed amount. Similarly, the fourth feed amount may be the same as or different from the second feed amount. Typically, the fourth feed amount is set to an amount larger than the second feed amount, but depending on the joining conditions, it may be set to remain the same as the second feed amount or to be smaller than the second feed amount.
[0064] During the second frictional heating period Ts, the control unit 4 continues frictional heating by limiting the torque at the second limit value (S106). When the sliding portions of the two workpieces have been sufficiently softened by frictional heat, the control unit 4 controls the rotation drive mechanism to stop the relative rotation of the two workpieces, thereby ending the second frictional heating period Ts (S107). The second frictional heating period Ts ends by controlling the timing of the stop of rotation of the first spindle 101 as described above. At this time, it is determined whether the droop at the time of rotation stop is within a predetermined threshold range (S108).
[0065] The determination of whether droop remains when rotation stops may be made, for example, by detecting whether the droop falls below a predetermined threshold value during a predetermined period before and after time t2. For example, the predetermined threshold value may be set to a value of approximately 2 to 3, assuming that the maximum droop value shown in FIG. 5 is 100. Depending on the joining conditions, a value of approximately 5 to 10 may also be used. Furthermore, monitoring for droop detection may be performed only during a predetermined period in the latter half of the frictional heating process. For example, a droop confirmation timer may be started at the timing when the second frictional heating period Ts begins. However, the threshold value is not limited to the above value, and the determination method is not limited to the above method.
[0066] If it is determined that the motor current when the rotation was stopped was normal (S108, YES), the control unit 4 continues the upsetting process (S109). In the upsetting process, the control unit 4 drives the drive mechanisms GZ1 and GZ2 so as to press the workpieces W1 and W2 against each other with a pressure higher than that in the friction heating process, while the rotation of the workpieces W1 and W2 is stopped.
[0067] The control unit 4 sets the control target value for the feed amount of the first headstock 102 to the fifth feed amount (fifth movement amount), and sets the control target value for the feed amount of the second headstock 202 to the sixth feed amount (sixth movement amount), and drives the motors MZ1 and MZ2, respectively.
[0068] Here, the fifth feed amount and the sixth feed amount may be the same or different and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc. Furthermore, the fifth feed amount is typically set to an amount larger than the third feed amount, but may continue to be the same as the third feed amount depending on the joining conditions. Similarly, the sixth feed amount is typically set to an amount larger than the fourth feed amount, but may continue to be the same as the fourth feed amount depending on the joining conditions.
[0069] On the other hand, if it is determined that the droop when rotation stops is not below the threshold value (S108, NO), the control unit 4 will notify the user that there is some kind of abnormality by issuing an alert, etc., assuming that there is some kind of poor joint in the workpieces W1 and W2 or some kind of malfunction in the device (S110).
[0070] As described above, according to the control of the friction welding process of this embodiment, the sliding contact between the workpieces is initiated with a torque load that is suppressed to a level that does not cause the workpieces to rotate together, and the torque limit is controlled to be relaxed once the sliding state has stabilized. This effectively suppresses the occurrence of defects in friction welding, particularly defects that occur early in the friction heating process. Furthermore, by checking whether or not droop remains at the end of the friction heating process, defects that cannot be prevented by limiting the torque load can be detected. In other words, the quality of the welding state can be accurately determined.
[0071] In this embodiment, the explanation is given on the premise that the device configuration is such that a machine tool, which is a cutting device, is converted into a friction welding device, but the present invention may also be applied to a dedicated friction welding device.
[0072] REFERENCE SIGNS LIST 1...machine tool, 100...first spindle mechanism, 101...first spindle, 102...first headstock, 200...second spindle mechanism, 201...second spindle, 202...second headstock, GZ1...first drive mechanism, GZ2...second drive mechanism, MZ1...first motor, MZ2...second motor, 4...control unit, 410...first ammeter, 420...second ammeter, 411...first current limiter, 421...second current limiter, W1...first workpiece, W2...second workpiece
Claims
1. A friction joining device comprising: a first spindle that grips a first workpiece; a second spindle that grips a second workpiece so as to be axially opposed to the first workpiece; a first drive mechanism having a first drive source and moving the first spindle in the axial direction by a drive force of the first drive source; a second drive mechanism having a second drive source and moving the second spindle in the axial direction by a drive force of the second drive source; a rotation drive mechanism that relatively rotates the first workpiece and the second workpiece about a rotation axis line along the axial direction; control means that controls the first drive mechanism, the second drive mechanism, and the rotation drive mechanism so as to join the first workpiece and the second workpiece by bringing them into contact with each other in a relatively rotated state; and current limiting means that limits current flowing through the first drive source and the second drive source to a predetermined limit value or less, the current limiting means limits the current flowing through the first driving source and the second driving source during a first frictional heating period, which is a predetermined period from immediately after the first workpiece and the second workpiece come into contact with each other, to a first limit value or less that is smaller than a second limit value for limiting the current flowing through the first driving source and the second driving source during a second frictional heating period after the first frictional heating period has elapsed.
2. The friction welding device according to claim 1, characterized in that the control means, during the first frictional heating period, controls the first drive source by using a first control target value for the movement amount per unit time of the first workpiece as a first movement amount, and controls the second drive source by using a second control target value for the movement amount per unit time of the second workpiece as a second movement amount, and, during the second frictional heating period, controls the first drive source by using the first control target value as a third movement amount, and controls the second drive source by using the second control target value as a fourth movement amount.
3. The friction welding device according to claim 2, characterized in that the third movement amount is the same as or greater than the first movement amount, and the fourth movement amount is the same as or greater than the second movement amount.
4. The friction welding device according to claim 2, characterized in that the control means controls the rotation drive mechanism to stop the relative rotation of the first workpiece and the second workpiece, thereby terminating the second friction heating period, and in the welding process after the end of the second friction heating period, controls the first drive source with the first control target value as a fifth movement amount, and controls the second drive source with the second control target value as a sixth movement amount.
5. A friction welding device as described in claim 4, further comprising a droop detection means for detecting the droop of the first driving source and the droop of the second driving source, and wherein the control means stops the first driving mechanism and the second driving mechanism and does not perform the welding process if the droop of the first driving source and the droop of the second driving source at the time of stopping the relative rotation exceed respective predetermined threshold values.
6. The friction welding device according to claim 1, characterized in that the rotation drive mechanism rotates the first workpiece but does not rotate the second workpiece.
7. A friction welding device as described in claim 1, characterized in that the current flowing through said first driving source and said second driving source is constant and equal to said first limit value during said first friction heating period.
8. The friction welding device described in claim 1, characterized in that the current flowing through the first driving source and the second driving source is constant at the same magnitude as the second limit value for a predetermined period from the start of the second friction heating period, and does not reach the same magnitude as the second limit value after the predetermined period.
Citation Information
Patent Citations
Friction welding method
JP1997141454A
Dissimilar material joined body, and its manufacturing method
JP2006255749A
Method and apparatus for friction stir welding
JP2008030050A
Machine tool
WO2020017514A1