Semiconductor structure, manufacturing method for semiconductor structure, and memory
By arranging a protection ring structure perpendicular to the substrate and a first fragile structure in the protection zone of the semiconductor structure, the problem of damage to the semiconductor structure during the cutting process is solved, and the yield and performance are improved.
Patent Information
- Application Number
- PCT/CN2024/084760
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-19
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-24
AI Technical Summary
Semiconductor structures are easily damaged during the cutting process, affecting their yield and performance.
A protective ring structure is provided in a protected area of the semiconductor structure. A first fragile structure is provided in the protective ring structure. The structure extends in a direction perpendicular to the upper surface of the substrate to absorb stress and guide stress to be transmitted in the vertical direction to avoid The stress is transferred to the chip area.
It effectively improves the yield and performance of the semiconductor structure, and reduces the risk of damage in the chip area by buffering stress and guiding stress transfer.
Smart Images

Figure CN2024084760_24102024_PF_FP_ABST
Abstract
Description
Semiconductor structure, method for manufacturing semiconductor structure, and memory
[0001] This disclosure is based on the Chinese patent application with application number 202310437084.4, application date April 19, 2023, and application name “Semiconductor structure, manufacturing method of semiconductor structure and memory”, and claims the priority of the Chinese patent application. The entire content of the Chinese patent application is hereby introduced into the present disclosure as a reference. Technical Field
[0002] The present disclosure belongs to the field of semiconductors, and particularly relates to a semiconductor structure, a method for manufacturing a semiconductor structure, and a memory. Background Art
[0003] The semiconductor structure cutting process typically involves three steps. Step 1: Lamination, for example, laminating the semiconductor structure to the surface of a UV-irradiated adhesive film. Step 2: Laser cutting, which uses a pulsed laser focused on the scribe line area of the semiconductor structure to form a modified layer. The modified layer is a structure with localized melting damage caused by the high temperature of the laser. The modified layer typically extends between the upper and lower surfaces of the semiconductor structure. Step 3: Expansion, which involves uniformly expanding the cut semiconductor structure horizontally to increase the spacing between chips, facilitating subsequent core removal and bonding.
[0004] However, the chip region of the semiconductor structure is easily damaged during the cutting process, thereby affecting the yield and performance of the semiconductor structure.
[0005] Summary of the Invention
[0006] The embodiments of the present disclosure provide a semiconductor structure, a method for manufacturing the semiconductor structure, and a memory, which are at least beneficial to improving the yield and performance of the semiconductor structure.
[0007] According to some embodiments of the present disclosure, on one hand, an embodiment of the present disclosure provides a semiconductor structure, wherein the semiconductor structure includes: a substrate, the substrate including a chip area, a protection area and a dicing area, the protection area is located between the chip area and the dicing area; the protection area has a guard ring structure, the guard ring structure has a first fragile structure inside, and the first fragile structure extends in a direction perpendicular to the upper surface of the substrate.
[0008] According to some embodiments of the present disclosure, on the other hand, an embodiment of the present disclosure further provides a method for manufacturing a semiconductor structure, the manufacturing method comprising: providing a substrate, the substrate comprising a chip area, a protection area and a dicing area, the protection area being located between the chip area and the dicing area; forming a guard ring structure on the protection area; forming a first fragile structure within the guard ring structure, the first fragile structure extending in a direction perpendicular to the upper surface of the substrate.
[0009] According to some embodiments of the present disclosure, another aspect of the present disclosure further provides a memory, the memory comprising: the aforementioned semiconductor structure.
[0010] The technical solution provided by the embodiments of the present disclosure has at least the following advantages: a first fragile structure extending perpendicularly to the upper surface of the substrate within the guard ring structure provides space for deformation of the guard ring structure and guides stress along its extension direction, preventing stress from being transferred to and damaging the chip area. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The accompanying drawings are incorporated into and constitute a part of the specification, illustrate embodiments consistent with the present disclosure, and together with the specification, are used to explain the principles of the present disclosure. Obviously, the drawings described below are only some embodiments of the present disclosure, and those skilled in the art can derive other drawings based on these drawings without inventive effort.
[0012] FIG1 shows a top view of a semiconductor structure provided by an embodiment of the present disclosure;
[0013] 2-3 respectively show different partial top views of the semiconductor structure provided by the embodiments of the present disclosure;
[0014] 4-5 are partial cross-sectional views of different semiconductor structures provided by embodiments of the present disclosure;
[0015] 6 to 11 are schematic structural diagrams corresponding to steps in a method for manufacturing a semiconductor structure provided by an embodiment of the present disclosure;
[0016] 12-15 are schematic structural diagrams corresponding to the steps in another method for manufacturing a semiconductor structure provided by an embodiment of the present disclosure. DETAILED DESCRIPTION
[0017] As we know from the background, the chip area of semiconductor structures is easily damaged during the dicing process. Analysis has found that the main reason is that a guard ring structure can be installed between the dicing lane area and the chip area. The guard ring structure can prevent cracks in the dicing lane area from extending into the chip area, but some stress may still be transferred to the chip area, thereby increasing the damaged area during dicing and affecting the chip yield and performance.
[0018] Embodiments of the present disclosure provide a semiconductor structure comprising: a protection zone located between a chip region and a scribe lane region; a guard ring structure disposed within the protection zone; and a first fragile structure disposed within the guard ring structure, the first fragile structure extending perpendicularly to the upper surface of a substrate. The first fragile structure provides space for deformation of the guard ring structure and also serves as a stress buffer, directing stress transmission perpendicularly to the upper surface of the substrate, thereby preventing damage to the chip region and ensuring chip yield and performance.
[0019] The following describes various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, those skilled in the art will appreciate that many technical details are provided in the various embodiments of the present disclosure to help readers better understand the embodiments of the present disclosure. However, even without these technical details and the various variations and modifications based on the following embodiments, the technical solutions claimed in the embodiments of the present disclosure can be implemented.
[0020] As shown in Figures 1 to 5, an embodiment of the present disclosure provides a semiconductor structure, which includes: a substrate 1, the substrate 1 includes a chip area A, a protection area B and a dicing area C, the protection area B is located between the chip area A and the dicing area C; a protection ring structure 2 is provided on the protection area B, and a first fragile structure 5 is provided in the protection ring structure 2, and the first fragile structure 5 extends in a direction perpendicular to the upper surface of the substrate 1.
[0021] In other words, the first fragile structure 5 has a fragile characteristic and can therefore absorb stress very well. In addition, the extension direction of the first fragile structure 5 is perpendicular to the upper surface of the substrate 1, so that stress can be transmitted in its extension direction and avoid being transmitted to the chip area A, thereby ensuring the yield and performance of the chip area A. It should be noted that due to process reasons, the extension direction of the first fragile structure 5 may not be completely perpendicular to the upper surface of the substrate 1, as long as it is close to a vertical relationship, for example, the angle is between 80° and 100°. The extension direction of the first fragile structure 5 can also be understood as the length direction of the cross section of the first fragile structure 5.
[0022] The semiconductor structure will be described in detail below with reference to the accompanying drawings.
[0023] FIG1 is a top view of a semiconductor structure. Referring to FIG1 , the protection area B and the scribe line area C are disposed around the chip area A. That is, the guard ring structure 2 can be disposed around the chip area A, thereby protecting the chip area A from multiple sides.
[0024] Referring to Figure 2, which is a partially enlarged top view of a semiconductor structure, the guard ring structure 2 includes a peripheral guard ring structure 21 and an inner guard ring structure 22, which are arranged at intervals. The peripheral guard ring structure 21 is located on the side of the inner guard ring structure 22 away from the chip area A. That is, the peripheral guard ring structure 21 is closer to the scribe line area C, and the inner guard ring structure 22 is closer to the chip area A. The peripheral guard ring structure 21 can also be called a scribe line seal ring structure (Scribe line seal ring), and the inner guard ring structure 22 can also be called a main chip seal ring structure (Main die seal ring). The first fragile structure 5 is arranged in the peripheral guard ring structure 21, which can guide the stress further away from the chip area A and avoid damage to the chip area A. In other embodiments, the semiconductor structure can also include only the peripheral guard ring structure 21. The inner guard ring structure 22 can be set through high-level metal grounding to improve the reliability of the semiconductor structure.
[0025] In some embodiments, the guard ring structure 2 is disposed around the chip area A, and the plurality of first fragile structures 5 are spaced apart and arranged circumferentially around the chip area A. For example, the plurality of first fragile structures 5 may be arranged at least once around the chip area A. In this way, the first fragile structures 5 can guide stress transfer around the chip area A, thereby reducing the risk of damage to the chip area A.
[0026] 2-3 , in some embodiments, multiple first fragile structures 5 located on the same side of the chip region A can be arranged in the same row. For example, the arrangement direction of the multiple first fragile structures 5 is parallel to the side of the chip region A. This can improve the uniformity of the semiconductor structure, simplify the manufacturing process, and avoid stress concentration problems.
[0027] In addition, the plurality of first fragile structures 5 may be arranged at equal intervals, so that the first fragile structures 5 are distributed more evenly, thereby better dispersing stress.
[0028] Referring to Figure 2 , the cross-section of the first fragile structure 5, parallel to the upper surface of the substrate 1, is rectangular. The rectangular first fragile structure 5 has a uniform width, which can more evenly guide stress transfer. Furthermore, the rectangular first fragile structure 5 is easier to manufacture.
[0029] Referring to Figure 3, which is a partial top view of another semiconductor structure, the cross-section of the first fragile structure 5 is triangular in a direction parallel to the upper surface of the substrate 1. Triangular shapes offer greater stability and stronger stress resistance. For example, the apex angles of adjacent triangles can be oriented in opposite directions. For example, the apex angle of one triangle faces the chip area A, while the apex angle of the adjacent triangle faces the scribe line area C. Furthermore, the opposing sides of adjacent triangles can be arranged in parallel, allowing the first fragile structure 5 to fully utilize the space within the guard ring structure 2.
[0030] In addition, in the direction parallel to the upper surface of the substrate 1 , the cross-sectional shape of the first fragile structure 5 may also be a circle, a square, a trapezoid, a parallelogram, or other irregular shapes.
[0031] Figures 4 and 5 are different partial cross-sectional views of the semiconductor structure, respectively. Referring to Figure 4, at least one of the upper and lower sides of the first fragile structure 5 has a sharp corner. Sharp corners are more likely to concentrate stress, thereby preventing stress from being transferred toward the chip area A. For example, the upper side of the first fragile structure 5 has a sharp corner protruding upward, and the lower side of the first fragile structure 5 has two sharp corners protruding downward. In other words, the sharp corners on the upper and lower sides protrude roughly in a direction perpendicular to the upper surface of the substrate 1, thereby better guiding the stress to be transferred in this direction. In other embodiments, one of the upper and lower sides of the first fragile structure 5 may have a sharp corner. In addition, referring to Figure 5, the cross-sectional shape of the first fragile structure 5 perpendicular to the upper surface of the substrate 1 may also be rectangular, that is, its upper and lower sides may not have sharp corners.
[0032] The guard ring structure 2 includes a plurality of metal ring structures 210 arranged in a direction parallel to the upper surface of the substrate 1; at least some of the adjacent metal ring structures 210 are spaced apart, and the first fragile structure 5 is located between the spaced metal ring structures 210. Thus, the first fragile structure 5 can provide space for deformation of the metal ring structure 210. In addition, the guard ring structure 2 can also include an interlayer dielectric layer 3, which is located at least between the spaced metal ring structures 210. In other words, with reference to Figures 2 to 5, in a direction parallel to the upper surface of the substrate 1, the guard ring structure 2 as a whole can be a continuous structure with a spacing space inside, in which the interlayer dielectric layer 3 and the first fragile structure 5 can be arranged, and the spacing space divides the guard ring structure 2 into multiple layers of metal ring structures 210.
[0033] For example, referring to FIG3 , the metal ring structure 210 includes a plurality of surrounding metal ring structures 213 and a plurality of connecting metal ring structures 214. The surrounding metal ring structures 213 extend circumferentially around the chip region A and surround the chip region A. The plurality of surrounding metal ring structures 213 are spaced apart in a direction from the chip region A toward the scribe line region C. The connecting metal ring structure 214 can be located between and connected to two adjacent surrounding metal ring structures 213. The first fragile structure 5 can be located in the spacing between adjacent surrounding metal ring structures 213 and between two adjacent connecting metal ring structures 214. Since the spacing between adjacent surrounding metal ring structures 213 also surrounds the chip region A, the plurality of first fragile structures 5 can be arranged circumferentially around the chip region A, thereby guiding stress transfer around the chip region A.
[0034] In some embodiments, referring to Figures 2-4 , the first fragile structure 5 can be a first air gap 51. In other embodiments, referring to Figure 5 , the first fragile structure 5 can also be a first fragile material layer 52, which can include a brittle material such as polysilicon. Compared to the first fragile material layer 52, the first air gap 51 requires fewer steps in the manufacturing process, which helps reduce production costs. Furthermore, the first air gap 51 provides ample space for the guard ring structure 2 to deform, preventing compression of devices within the chip area A.
[0035] In some embodiments, referring to FIG4 , the first fragile structure 5 includes multiple first sub-fragile structures 50 spaced apart in a direction perpendicular to the top surface of the substrate 1. Compared to a continuous first fragile structure 5 of the same height, multiple first sub-fragile structures 50 spaced apart in a direction perpendicular to the top surface of the substrate 1 are more difficult to manufacture and provide greater overall stability for the semiconductor structure, thereby preventing breakage during non-cutting processes. Furthermore, the height of the first sub-fragile structures 50 in a direction perpendicular to the top surface of the substrate 1 can be greater than the width of the first sub-fragile structures 50 in a direction parallel to the top surface of the substrate 1, thereby better guiding stress propagation in a direction perpendicular to the top surface of the substrate 1.
[0036] 4 , the first sub-fragile structure 50 is a first sub-air gap 510 . Referring to FIG5 , the first sub-fragile structure 50 can also be a first sub-fragile material layer 520 .
[0037] In some embodiments, the multiple first sub-fragile structures 50 are of the same type, such as all being air gaps or all being fragile material layers. This facilitates a unified manufacturing process and reduces production costs. In other embodiments, the multiple first sub-fragile structures 50 can be of different types. For example, the first sub-fragile structures 50 located in the lower layer can be a fragile material layer, while the first sub-fragile structures 50 located in the upper layer can be air gaps. This helps improve the stability of the structure.
[0038] In some embodiments, referring to FIG4 , the widths of the multiple first sub-fragile structures 50 can increase sequentially in the direction from substrate 1 toward guard ring structure 2 . This can increase the strength and stability of the semiconductor structure and prevent collapse during non-cutting processes. In other embodiments, referring to FIG5 , the widths of the multiple first sub-fragile structures 50 can also be the same, which can improve the uniformity of the semiconductor structure and simplify the process.
[0039] In some embodiments, referring to Figures 4 and 5 , the guard ring structure 2 includes first sub-metal ring structures 211 and second sub-metal ring structures 212 alternately arranged in a direction perpendicular to the upper surface of the substrate 1. In a direction parallel to the upper surface of the substrate 1, the cross-sectional area of the first sub-metal ring structure 211 is greater than the cross-sectional area of the second sub-metal ring structure 212. The first sub-fragile structure 50 is arranged opposite the first sub-metal ring structure 211.
[0040] This design is because the first sub-metal ring structure 211 is larger and deforms more rapidly. Placing the first sub-fragile structure 50 opposite the first sub-metal ring structure 211 provides ample deformation space for the first sub-metal ring structure 211, thereby releasing stress. Furthermore, in a direction parallel to the upper surface of the substrate 1, the spacing between adjacent first sub-metal ring structures 211 is smaller than the spacing between adjacent second sub-metal ring structures 212. Consequently, the first sub-fragile structure 50 formed between adjacent first sub-metal ring structures 211 has a smaller width-to-length ratio, thereby better guiding stress transmission along the length direction of the first sub-fragile structure 50 (i.e., perpendicular to the upper surface of the substrate 1), thereby reducing the risk of damage to the chip area A. It should be noted that, due to manufacturing process reasons, a portion of the first sub-fragile structure 50 can also be disposed opposite the second sub-metal ring structure 212, but the main portion of the first sub-fragile structure 50 is still disposed opposite the first sub-metal ring structure 211.
[0041] Referring to Figures 4 and 5, the interlayer dielectric layer 3 can surround the first fragile structure 5. In other embodiments, the interlayer dielectric layer 3 and the metal ring structure 210 can jointly surround the first fragile structure 5. For example, referring to Figure 4, when the first fragile structure 5 is a first air gap 51, each first sub-fragile structure 50 is surrounded by the interlayer dielectric layer 3. This is because the first air gap 51 is typically formed in an area with a high aspect ratio. The interlayer dielectric layer 3 can occupy part of the space between adjacent first sub-metal ring structures 211, reducing the width of the remaining space between the first sub-metal ring structures 211, thereby reducing the difficulty of forming the first air gap 51. In other embodiments, referring to Figure 5, when the first fragile structure 5 is a first fragile material layer 52, the metal ring structure 210 can contact at least two opposing sides of the first sub-fragile structure 50. In other words, the first sub-fragile structure 50 can completely fill the space between adjacent first sub-metal ring structures 211. This helps reduce process steps and thus lowers production costs. This will be described in detail later in conjunction with the manufacturing method.
[0042] In other embodiments, the guard ring structure 2 may also be a columnar structure, that is, the cross-sectional shape of the guard ring structure 2 in the direction perpendicular to the upper surface of the substrate 1 may also be a rectangle with a uniform width, which can simplify the production process.
[0043] In some embodiments, referring to Figures 4 and 5 , the semiconductor structure further includes a second fragile structure 8 extending perpendicularly to the top surface of substrate 1; second fragile structure 8 is located within substrate 1 in protected area B and below first fragile structure 5. Second fragile structure 8 can guide stress within substrate 1 in a direction perpendicular to its top surface and provide space for deformation of structures within substrate 1, thereby enhancing protection for chip area A. Furthermore, the alignment of first fragile structure 5 and second fragile structure 8 can better limit the direction of stress transmission.
[0044] In some embodiments, referring to FIG4 , second fragile structure 8 may be a second air gap 83. In other embodiments, referring to FIG5 , second fragile structure 8 may be a second fragile material layer 84, which may comprise a brittle material such as polysilicon. Compared to second fragile material layer 84, second air gap 83 requires fewer steps in the manufacturing process, which helps reduce production costs. Furthermore, second air gap 83 provides ample space for deformation of structures within substrate 1.
[0045] In some embodiments, the first fragile structure 5 and the second fragile structure 8 are of the same type, such as both being air gaps or both being fragile material layers. This facilitates a unified manufacturing process and reduces production costs. In other embodiments, the first fragile structure 5 and the second fragile structure 8 can be of different types, such as the first fragile structure 5 being a first air gap 51 and the second fragile structure 8 being a second fragile material layer 84. This facilitates improved structural stability.
[0046] In some embodiments, the second fragile structure 8 may be a single-layer structure to simplify the production process. In other embodiments, the second fragile structure 8 may also include multiple second sub-fragile structures arranged in a direction perpendicular to the upper surface of the substrate 1 to enhance the stress-guiding effect of the second fragile structure 8 while ensuring the strength of the substrate 1.
[0047] Referring to Figures 4 and 5 , the cross-sectional shape of the second fragile structure 8, perpendicular to the upper surface of the substrate 1, includes a spindle shape. In other words, the dimensions of the second fragile structure 8 at the top and bottom can be smaller than the center. This facilitates stress concentration at the top and bottom of the second fragile structure 8, preventing stress from being transferred to the chip area A.
[0048] In summary, the disclosed embodiment forms a first fragile structure 5 within the guard ring structure 2 to act as a buffer. When external stress is generated and transmitted to the guard ring structure 2, the first fragile structure 5 absorbs the stress and directs it toward the vertical direction, reducing the likelihood of stress transmission into the chip region A, which could cause damage such as cracking. Furthermore, a second fragile structure 8 can be formed within the substrate 1 to enhance the protection of the chip region A.
[0049] As shown in Figures 6 to 15, another embodiment of the present disclosure provides a method for manufacturing a semiconductor structure. This manufacturing method can be used to manufacture the semiconductor structure provided in the aforementioned embodiments. For detailed descriptions of this semiconductor structure, please refer to the aforementioned embodiments and will not be repeated here. It should be noted that, for the purpose of facilitating description and clearly illustrating the steps of the semiconductor structure manufacturing method, Figures 6 to 15 are schematic diagrams of partial structures of the semiconductor structure.
[0050] 6 , a substrate 1 is provided. The substrate 1 may be a silicon substrate, a germanium substrate, or a silicon-germanium substrate. The substrate 1 includes a chip region A, a protection region B, and a scribe lane region C (see FIG1 ). The protection region B is located between the chip region A and the scribe lane region C.
[0051] Referring to Figures 6-11 , a guard ring structure 2 is formed on the protection zone B; a first fragile structure 5 is formed within the guard ring structure 2, extending perpendicularly to the upper surface of the substrate 1. For example, forming the guard ring structure 2 on the protection zone B includes forming a peripheral guard ring structure 21 and an inner guard ring structure 22 (see Figure 2 ) spaced apart on the protection zone B. The peripheral guard ring structure 21 is located on a side of the inner guard ring structure 22 away from the chip zone A, and the first fragile structure 5 is formed within the peripheral guard ring structure 21.
[0052] The steps of forming the protective ring structure 2 and the first fragile structure 5 will be described in detail below.
[0053] 6 to 9 , a plurality of metal ring structures 210 are formed and arranged in a direction parallel to the upper surface of the substrate 1 , and at least some adjacent metal ring structures 210 are spaced apart and surround a first groove 42 .
[0054] Specifically, referring to FIG6 , a first dielectric layer 71, a sacrificial layer 72, a first mask layer 73, a second mask layer 74, and a first photoresist layer 75 are stacked. For example, the first mask layer 73 may be a hard mask layer, and the second mask layer 74 may be an anti-reflective layer. The material of the first dielectric layer 71 may be silicon carbonitride, and the material of the sacrificial layer 72 may be a low-k material such as silicon dioxide or silicon nitride. In other embodiments, the first dielectric layer 71 may not be formed. Alternatively, only a single mask layer may be formed, for example, only one of the first mask layer 73 and the second mask layer 74.
[0055] 7 , using the first photoresist layer 75 as a mask, the first mask layer 73, the second mask layer 74, the first dielectric layer 71, and the sacrificial layer 72 are etched to form a trench 41 penetrating the first dielectric layer 71 and the sacrificial layer 72. Thereafter, the first photoresist layer 75, the first mask layer 73, and the second mask layer 74 are removed.
[0056] 8 , a metal ring structure 210 is formed in the trench 41 . For example, the metal ring structure 210 is formed by an electroplating process.
[0057] 9 , the sacrificial layer 72 is removed to expose the sidewalls of the metal ring structure 210. For example, the sacrificial layer 72 is etched using a dry process, and the etching gas may be ammonia or at least one of hydrogen and nitrogen.
[0058] At this point, the metal ring structure 210 can be formed based on FIG. 6 to FIG. 9 , and the first groove 42 can be formed between adjacent metal ring structures 210 .
[0059] Referring to FIG. 10 , a wrapping layer 76 is formed, covering at least the sidewalls and top surface of the metal ring structure 210. For example, a chemical vapor deposition process or an atomic layer deposition process is used to form the wrapping layer 76 conformally covering the metal ring structure 210. The material of the wrapping layer 76 can be the same as that of the first dielectric layer 71, for example, both can be silicon carbonitride. The wrapping layer 76 can protect the metal ring structure 210 during the subsequent formation of the interlayer dielectric layer 3, thereby preventing the reactive gas from the interlayer dielectric layer 3 from invading and reacting with the metal ring structure 210. In addition, the wrapping layer 76 can also adjust the width of the filling space between adjacent metal ring structures 210, thereby reducing the difficulty of forming the first air gap 51.
[0060] Continuing with FIG10 , an interlayer dielectric layer 3 is formed. The interlayer dielectric layer 3 is located at least on the upper surface of the multiple metal ring structures 210 and closes the top opening of the first groove 42, thereby forming a first air gap 51 at the first groove 42. The first air gap 51 serves as the first fragile structure 5. Furthermore, the interlayer dielectric layer 3 also covers a portion of the upper surface of the wrapping layer 76. Because the interlayer dielectric layer 3 spans across the multiple metal ring structures 210, it has good mechanical strength, which helps ensure structural stability. The guard ring structure 2 includes the interlayer dielectric layer 3 and the metal ring structures 210.
[0061] For example, a chemical vapor deposition process is used to form the interlayer dielectric layer 3. During the chemical vapor deposition process, process parameters need to be adjusted so that the interlayer dielectric layer 3 quickly covers the top opening of the first groove 42 (see FIG. 9 ), thereby reducing the amount of deposited material entering the first groove 42.
[0062] It should be noted that the wrapping layer 76 covering the sidewalls of the metal ring structures 210 is equivalent to reducing the spacing between adjacent metal ring structures 210, thereby preventing excessive deposition of interlayer dielectric material between adjacent metal ring structures 210 due to excessive spacing, thereby avoiding affecting the size of the first air gap 51. In other words, the first air gap 51 can be formed using a self-aligned process without using a new mask.
[0063] Continuing with reference to FIG. 10 , in some embodiments, a stacked lower dielectric layer 31 and an upper dielectric layer 32 are formed to serve together as the interlayer dielectric layer 3. For example, the material of the lower dielectric layer 31 may be silicon oxycarbide or fluorinated silicate glass (FSG). The material of the upper dielectric layer 32 may be silicon oxide or silicon nitride, among others. For example, if the material of the lower dielectric layer 31 is FSG, FSG contains fluorine. The wrapping layer 76 can prevent fluorine from entering the metal ring structure 210 during the high-temperature process, thereby protecting the metal ring structure 210. Fluorine can reduce the dielectric constant and also change the gap-filling capability during thin film deposition. The higher the fluorine content, the stronger the gap-filling capability. Therefore, the fluorine content of the FSG can be set within a relatively small range to prevent excessive FSG from filling the first groove 42. In other embodiments, the interlayer dielectric layer 3 may also be a single-layer structure, i.e., only one of the lower dielectric layer 31 and the upper dielectric layer 32 is formed.
[0064] In other embodiments, the wrapping layer 76 may not be formed before forming the interlayer dielectric layer 3, and the deposition rate may be increased to prevent excessive deposition material from entering the gaps between the metal ring structures 210. Alternatively, the width of the metal ring structure 210 in a direction parallel to the upper surface of the substrate 1 may be increased so that adjacent metal ring structures 210 have a smaller spacing, thereby reducing the difficulty of forming the first air gap 51. Alternatively, another mask may be used to define the pattern of the first air gap 51. For example, after forming the metal ring structure 210, the sacrificial layer 72 is not removed, and thereafter, part of the sacrificial layer 72 between adjacent metal ring structures 210 is etched, thereby transferring the pattern of the mask to the sacrificial layer 72 to form the first groove 42. Thereafter, the interlayer dielectric layer 3 is formed, and the interlayer dielectric layer 3 at least covers the upper surfaces of the metal ring structure 210 and the remaining sacrificial layer 72, and closes the opening of the first groove 42.
[0065] In some embodiments, the width of the first groove 42 is smaller than the height of the metal ring structure 210, that is, the first groove 42 can have a larger aspect ratio, which can reduce the difficulty of forming the first air gap 51 and better guide the stress to be transmitted in a direction perpendicular to the upper surface of the substrate 1.
[0066] In some embodiments, referring to FIG4 , the guard ring structure 2 includes a first sub-metal ring structure 211 and a second sub-metal ring structure 212. The first air gap 51 may include a plurality of first sub-air gaps 510 spaced apart in a direction perpendicular to the upper surface of the substrate 1, that is, the first sub-air gaps 510 serve as the first sub-fragile structure 50. The first sub-air gaps 510 may be arranged opposite to the first sub-metal ring structure 211. For example, the plurality of spaced-apart metal ring structures 210 each include a first sub-metal ring structure 211 and a second sub-metal ring structure 212, and the first sub-air gaps 510 are formed between adjacent first sub-metal ring structures 211 arranged in the same layer. Since the spacing between adjacent first sub-metal ring structures 211 is smaller than the spacing between adjacent second sub-metal ring structures 212, it is easier to form the first sub-air gaps between adjacent first sub-metal ring structures 211.
[0067] For example, a plurality of first sub-metal ring structures 211 spaced apart and a first groove 42 located between adjacent first sub-metal ring structures 211 are first formed, and then an interlayer dielectric layer 3 is formed to cover the plurality of first sub-metal ring structures 211 and close the top opening of the first groove 41, thereby forming a first sub-air gap 510. Thereafter, the interlayer dielectric layer 3 above the first sub-metal ring structure 211 is etched to form a through hole, which exposes a portion of the upper surface of the first sub-metal ring structure 211; and a second sub-metal ring structure 212 is formed to fill the through hole. Thereafter, the aforementioned process steps of forming the first sub-metal ring structure 211, the interlayer dielectric layer 3, the first sub-air gap 510, and the second sub-metal ring structure 212 are repeated. In this way, the first sub-air gap 510 spaced apart in a direction perpendicular to the upper surface of the substrate 1 can be formed.
[0068] Referring to FIG. 11 , in some other embodiments, a first fragile material layer 52 may be formed as the first fragile structure 5. For example, after forming the wrapping layer 76, a chemical vapor deposition process is used to deposit a material such as polysilicon between adjacent metal ring structures 210 to form the first fragile material layer 52. Thereafter, an interlayer dielectric layer 3 is formed above the metal ring structures 210 and the first fragile material layer 52.
[0069] Referring to Figures 12-15 , in some embodiments, before forming the guard ring structure 2, the process further includes forming a second fragile structure 8 within the substrate 1 in the protection area B. The second fragile structure 8 extends perpendicular to the upper surface of the substrate 1, and the first fragile structure 5 is further formed above the second fragile structure 8. The second fragile structure 8 serves as a buffer region within the substrate 1 to enhance protection of the chip area A.
[0070] 12-13 , the substrate 1 is etched in a direction perpendicular to the upper surface of the substrate 1 to form a second groove 85 in the substrate 1 .
[0071] Specifically, referring to FIG12 , a second photoresist layer 81 is formed on the upper surface of the substrate 1, and the second photoresist layer 81 is exposed and developed to pattern the second photoresist layer 81. Referring to FIG13 , using the patterned second photoresist layer 81 as a mask, a dry etching process is used to etch a portion of the thickness of the substrate 1 to form a second groove 85. The second groove 85 can be positioned opposite the first groove 42 to be formed subsequently. Thereafter, the second photoresist layer 81 is removed to expose the upper surface of the substrate 1, and the substrate 1 is cleaned to remove impurities on the surface of the substrate 1.
[0072] It should be noted that the width of the second groove 85 parallel to the upper surface of the substrate 1 can be smaller than the depth of the second groove 85 perpendicular to the upper surface of the substrate 1. For example, the aspect ratio of the second groove 85 can be greater than 2:1, which can reduce the material of the covering layer 82 subsequently deposited into the second groove 85.
[0073] Referring to FIG. 14 , a capping layer 82 is formed to seal the opening at the top of the second groove 85 , thereby forming a second air gap 83 at the second groove 85 . The second air gap 83 serves as the second fragile structure 8 . For example, the capping layer 82 is formed using an epitaxial growth process or a chemical vapor deposition process. Thereafter, a high-temperature annealing process may be performed to repair defects in the substrate 1 . In some embodiments, the material of the capping layer 82 may be the same as that of the substrate 1 , thereby reducing defects at the interface between the capping layer 82 and the substrate 1 .
[0074] In other embodiments, referring to FIG. 15 , a second fragile material layer 84 may be deposited in the second groove 85 as the second fragile structure 8 , and thereafter, a covering layer 82 is formed covering the second fragile material layer 84 and the upper surface of the substrate 1 .
[0075] In summary, the disclosed embodiment forms a first groove 42 between adjacent metal ring structures 210 and an interlayer dielectric layer 3 to seal the opening of the first groove 42, thereby forming a first air gap 51; alternatively, a first fragile material layer 52 is filled in the first groove 42. The first air gap 51 or the first fragile material layer 52, serving as the first fragile structure 5, can limit the direction of stress transmission and prevent damage to the chip area A. Furthermore, a second air gap 83 or a second fragile material layer 84 can be formed within the substrate 1 to enhance the stress guidance effect.
[0076] Another embodiment of the present disclosure further provides a memory, which includes the semiconductor structure provided in the aforementioned embodiment. For detailed descriptions of the semiconductor structure, reference may be made to the detailed descriptions of the aforementioned embodiment. For example, structures such as capacitors, word lines, bit lines, and transistors may also be formed in the chip area. The memory may be a dynamic random access memory (DRAM), a static random access memory (SRAM), or the like.
[0077] In the description of this specification, the reference terms "some embodiments", "exemplarily", etc. mean that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present disclosure. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art can combine and combine different embodiments or examples described in this specification and features of different embodiments or examples without contradiction.
[0078] Although the embodiments of the present disclosure have been shown and described above, it is understood that the above embodiments are illustrative and cannot be understood as limitations on the present disclosure. A person skilled in the art may change, modify, replace and modify the above embodiments within the scope of the present disclosure. Therefore, any changes or modifications made in accordance with the claims and description of the present disclosure shall fall within the scope of the patent of the present disclosure.
Claims
1. A semiconductor structure, characterized in that: include: A substrate (1), the substrate (1) comprising a chip area (A), a protection area (B) and a scribe line area (C), the protection area (B) being located between the chip area (A) and the scribe line area (C); The protection zone (B) has a protection ring structure (2), and the protection ring structure (2) has a first fragile structure (5) inside, and the first fragile structure (5) extends in a direction perpendicular to the upper surface of the substrate (1).
2. The semiconductor structure according to claim 1, characterized in that: The protective ring structure (2) comprises a plurality of metal ring structures (210) arranged in a direction parallel to the upper surface of the substrate (1); at least some of the adjacent metal ring structures (210) are arranged at intervals, and the first fragile structure (5) is located between the spaced metal ring structures (210).
3. The semiconductor structure according to claim 2, characterized in that: The first fragile structure (5) comprises a plurality of first sub-fragile structures (50) arranged at intervals in a direction perpendicular to the upper surface of the substrate (1).
4. The semiconductor structure according to claim 3, characterized in that: The metal ring structure (210) comprises a first sub-metal ring structure (211) and a second sub-metal ring structure (212) which are alternately arranged in a direction perpendicular to the upper surface of the substrate (1); In a direction parallel to the upper surface of the substrate (1), the cross-sectional area of the first sub-metal ring structure (211) is greater than the cross-sectional area of the second sub-metal ring structure (212); The first sub-fragile structure (50) is arranged opposite to the first sub-metal ring structure (211).
5. The semiconductor structure according to claim 1, characterized in that: The protection ring structure (2) is arranged around the chip area (A), and a plurality of the first fragile structures (5) are arranged at intervals in the circumferential direction of the chip area (A).
6. The semiconductor structure according to claim 1, characterized in that In a direction parallel to the upper surface of the substrate (1), the cross-sectional shape of the first fragile structure (5) includes a triangle or a rectangle.
7. The semiconductor structure according to claim 1, characterized in that: At least one of the upper and lower sides of the first fragile structure (5) has a sharp corner.
8. The semiconductor structure according to claim 1, characterized in that: The first fragile structure (5) is a first air gap (51), or the first fragile structure (5) is a first fragile material layer (52), and the material of the first fragile material layer (52) includes polysilicon.
9. The semiconductor structure according to any one of claims 1 to 8, characterized in that: It also includes: a second fragile structure (8) extending in a direction perpendicular to the upper surface of the substrate (1); the second fragile structure (8) is located within the substrate (1) of the protection area (B) and below the first fragile structure (5).
10. The semiconductor structure according to claim 9, characterized in that: The second fragile structure (8) is a second air gap (83), or the second fragile structure (8) is a second fragile material layer (84), and the material of the second fragile material layer (84) includes polysilicon.
11. The semiconductor structure according to claim 9, characterized in that: In a direction perpendicular to the upper surface of the substrate (1), the cross-sectional shape of the second fragile structure (8) includes a spindle shape.
12. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, the substrate (1) comprising a chip area (A), a protection area (B) and a scribe line area (C), wherein the protection area (B) is located between the chip area (A) and the scribe line area (C); forming a protection ring structure (2) on the protection area (B); A first fragile structure (5) is formed in the protection ring structure (2), and the first fragile structure (5) extends in a direction perpendicular to the upper surface of the substrate (1).
13. The method for manufacturing a semiconductor structure according to claim 12, characterized in that: forming a plurality of metal ring structures (210) arranged in a direction parallel to the upper surface of the substrate (1), wherein at least some of the adjacent metal ring structures (210) are arranged at intervals and surround a first groove (42); An interlayer dielectric layer (3) is formed, the interlayer dielectric layer (3) being located at least on the upper surfaces of the plurality of metal ring structures (210) and closing the top opening of the first groove (42) to form a first air gap (51) at the first groove (42), the first air gap (51) serving as the first fragile structure (5); the protection ring structure (2) comprising the interlayer dielectric layer (3) and the metal ring structure (210).
14. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: Before forming the interlayer dielectric layer (3), the method further includes: forming a wrapping layer (76), wherein the wrapping layer (76) at least covers the side wall and the upper surface of the metal ring structure (210); The interlayer dielectric layer (3) also covers a portion of the upper surface of the wrapping layer (76).
15. The method for manufacturing a semiconductor structure according to claim 12, wherein: Before forming the protection ring structure (2), the method further includes: forming a second fragile structure (8) in the substrate (1) of the protection zone (B); the second fragile structure (8) extends in a direction perpendicular to the upper surface of the substrate (1); The first frangible structure (5) is also formed above the second frangible structure (8).
16. The method for manufacturing a semiconductor structure according to claim 15, characterized in that: The step of forming the second fragile structure (8) comprises: Etching the substrate (1) in a direction perpendicular to the upper surface of the substrate (1) to form a second groove (85) in the substrate (1); A covering layer (82) is formed, the covering layer (82) closes the opening at the top of the second groove (85) to form a second air gap (83) at the second groove (85), the second air gap (83) serving as the second fragile structure (8).
17. A memory, characterized in that: include: A semiconductor structure as claimed in any one of claims 1 to 11.
18. The memory according to claim 17, characterized in that: The second fragile structure (8) in the semiconductor structure is at least partially broken.
19. The memory according to claim 17, characterized in that: The first fragile structure (5) in the semiconductor structure is at least partially broken.
20. The memory according to claim 17, characterized in that: There is a crack in the semiconductor structure, and the crack is at least partially arranged in the first fragile structure (5) and / or the second fragile structure (8).
Citation Information
Patent Citations
Semiconductor device
CN101431064A
Semiconductor structure and method of forming the same
CN109309057A
In-chip moat protection structure and manufacturing method thereof
CN111081647A
Scribing structure for memory device
CN115206935A
Chip part and power chip
CN207398113U