Plasma processing device and end point detection method

The plasma processing apparatus uses spectrometer-measured emission intensities in specific wavelength bands to differentiate between silicon oxide and silicon nitride layers, addressing the challenge of end point detection in laminated films, ensuring precise and efficient etching.

WO2024225043A1PCT designated stage expired Publication Date: 2024-10-31TOKYO ELECTRON LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014578
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-25
Filing Date
2024-04-10
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing plasma processing technologies face challenges in efficiently detecting the end point of etching for laminated films with alternating silicon oxide and silicon nitride layers, as conventional methods rely on emission intensities of CO and CN, which are not effective for layered structures.

Method used

A plasma processing apparatus equipped with a spectrometer that measures emission intensities in specific wavelength bands associated with nitrogen and oxygen, allowing for precise detection of etching end points by monitoring changes in emission intensities during plasma processing, enabling efficient differentiation between etching of silicon oxide and silicon nitride layers.

Benefits of technology

This approach allows for accurate and efficient detection of etching end points in both silicon oxide and silicon nitride layers, ensuring appropriate process conditions and preventing over-etching, thereby improving the precision and reliability of plasma processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014578_31102024_PF_FP_ABST
    Figure JP2024014578_31102024_PF_FP_ABST
Patent Text Reader

Abstract

This plasma processing apparatus comprises: a spectrometer that measures emission intensity; and a control unit that controls detection of the end point of etching on the basis of a measurement result obtained by the spectrometer. When a laminated film in which a first layer containing silicon and oxygen and a second layer containing silicon and nitrogen are alternately laminated is etched by means of plasma, the control unit performs: (a) a procedure for acquiring, from the spectrometer, a first emission intensity in a first wavelength band due to the oxygen; (b) a procedure for acquiring, from the spectrometer, a second emission intensity in a second wavelength band due to the nitrogen; and (c) a procedure for detecting an end point of etching in the first layer when the first emission intensity has decreased and the second emission intensity has increased, and detecting an end point of etching in the second layer when the second emission intensity has decreased and the first emission intensity has increased.
Need to check novelty before this filing date? Find Prior Art

Description

Plasma processing apparatus and end point detection method

[0001] The present disclosure relates to a plasma processing apparatus and an endpoint detection method.

[0002] For example, Patent Document 1 discloses a method for selectively etching silicon oxide and silicon nitride. Patent Document 1 discloses that the step of etching silicon oxide is terminated when it is determined that the etching of silicon oxide has been completed based on the emission intensity of CO. Patent Document 1 also discloses that the step of etching silicon nitride is terminated when it is determined that the etching of silicon nitride has been completed based on the emission intensity of CN.

[0003] Japanese Patent Application Laid-Open No. 2018-046185

[0004] The present disclosure provides a technique for efficiently detecting an end point when etching a laminated film in which a first layer and a second layer are stacked.

[0005] According to one aspect of the present disclosure, there is provided a plasma processing apparatus including: a spectrometer that measures an emission intensity during plasma processing; and a controller that controls detection of an etching end point based on measurement results obtained by the spectrometer, wherein the controller performs the following steps when etching a stacked film in which first layers containing silicon and oxygen and second layers containing silicon and nitrogen are alternately stacked using plasma: (a) acquiring from the spectrometer during plasma processing a first emission intensity, which is an emission intensity in a first wavelength band caused by the oxygen; (b) acquiring from the spectrometer during plasma processing a second emission intensity, which is an emission intensity in a second wavelength band caused by the nitrogen, which is different from the first wavelength band; and (c) detecting an etching end point in the first layer when the first emission intensity decreases and the second emission intensity increases, and detecting an etching end point in the second layer when the second emission intensity decreases and the first emission intensity increases.

[0006] The present disclosure provides a technique for efficiently detecting an end point when etching a laminated film in which a first layer and a second layer are stacked.

[0007] FIG. 1 is a diagram illustrating an example of the configuration of a plasma processing system including a plasma processing apparatus according to this embodiment. FIG. 2 is a flow diagram illustrating processing by the plasma processing apparatus according to this embodiment. FIG. 3 is a diagram illustrating an overview of a laminated film processed by the plasma processing apparatus according to this embodiment. FIG. 4 is a diagram illustrating an overview of a laminated film processed by the plasma processing apparatus according to this embodiment. FIG. 5 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 6 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 7 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 8 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 9 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 10 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 11 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment. FIG. 12 is a diagram illustrating an example of an emission spectrum in the plasma processing apparatus according to this embodiment.

[0008] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In this specification and the drawings, substantially identical components are designated by the same reference numerals, and redundant description will be omitted. To facilitate understanding, the scale of each part in the drawings may differ from the actual scale. Directions such as parallel, right-angled, orthogonal, horizontal, vertical, up / down, left / right, and the like are permitted to a degree that does not impair the effects of the embodiments. The shape of corners is not limited to right angles and may be rounded. Parallel, right-angled, orthogonal, horizontal, and vertical may include approximately parallel, approximately right-angled, approximately orthogonal, approximately horizontal, and approximately vertical.

[0009] <Plasma Processing System> An example of the configuration of a plasma processing system will be described below. Fig. 1 is a diagram illustrating an example of the configuration of a plasma processing system including a plasma processing apparatus 1, which is an example of a plasma processing apparatus according to this embodiment.

[0010] The plasma processing system includes a capacitively coupled plasma processing apparatus 1 and a controller 2. The capacitively coupled plasma processing apparatus 1 includes a plasma processing chamber 10, a gas supply 20, a power supply 30, an exhaust system 40, and a spectrometer 60. The plasma processing chamber 10 has at least one gas inlet for supplying at least one process gas into a plasma processing space 10s and at least one gas outlet for exhausting gas from the plasma processing space 10s. The plasma processing chamber 10 also includes a plasma processing space 10s. The plasma processing apparatus 1 also includes a substrate support 11 and an upper electrode showerhead 13. The substrate support 11 is disposed within the plasma processing space 10s. The upper electrode showerhead 13 is disposed above the substrate support 11 and forms at least a portion of the ceiling of the plasma processing chamber 10.

[0011] The substrate support 11 includes a main body 111 and an annular member (edge ​​ring) 112. The main body 111 has a central region (substrate support surface) 111a for supporting a substrate (wafer) W and an annular region (edge ​​ring support surface) 111b for supporting the annular member 112. The annular region 111b of the main body 111 surrounds the central region 111a of the main body 111. The substrate W is disposed on the central region 111a of the main body 111, and the annular member 112 is disposed on the annular region 111b of the main body 111 so as to surround the substrate W on the central region 111a of the main body 111. In one embodiment, the main body 111 includes a base and an electrostatic chuck. The base includes a conductive member (lower electrode). The electrostatic chuck is disposed on the base. The upper surface of the electrostatic chuck has the substrate support surface 111a. Although not shown, in one embodiment, the substrate support 11 may include a temperature control module configured to adjust at least one of the electrostatic chuck and the substrate to a target temperature. The temperature control module may include a heater, a flow path, or a combination thereof. A temperature control fluid such as a coolant or a heat transfer gas flows through the flow path.

[0012] The upper electrode showerhead 13 is configured to introduce at least one process gas from the gas supply unit 20 into the plasma processing space 10s. The upper electrode showerhead 13 has at least one gas inlet 13a, at least one gas diffusion chamber 13b, and multiple gas inlets 13c. The process gas supplied to the gas inlet 13a passes through the gas diffusion chamber 13b and is introduced into the plasma processing space 10s from the multiple gas inlets 13c.

[0013] The gas supply unit 20 may include at least one gas source 21 and at least one flow controller 22. In one embodiment, the gas supply unit 20 is configured to supply at least one process gas from a corresponding gas source 21 through a corresponding flow controller 22 to the upper electrode showerhead 13. Each flow controller 22 may include, for example, a mass flow controller or a pressure-controlled flow controller. Additionally, the gas supply unit 20 may include one or more flow modulation devices to modulate or pulse the flow rate of the at least one process gas.

[0014] The power supply 30 includes an RF power supply coupled to the plasma processing chamber 10. The RF power supply is configured to supply at least one RF signal (RF power), such as a source RF signal and a bias RF signal, to the conductive member of the substrate support 11 and / or the upper electrode showerhead 13. This causes a plasma to be formed from at least one process gas supplied to the plasma processing space 10s. Thus, the RF power supply can function as at least a part of a plasma generating unit configured to generate a plasma from one or more process gases in the plasma processing chamber 10.

[0015] In one embodiment, the RF power supply includes a first RF generator and a second RF generator. The first RF generator is coupled to the conductive member of the substrate support 11 or the upper electrode showerhead 13 and is configured to generate a source RF signal (source RF power) for plasma generation. In one embodiment, the source RF signal has a frequency in a range of 27 MHz to 100 MHz. The generated source RF signal is supplied to the conductive member of the substrate support 11 or the upper electrode showerhead 13. The second RF generator 31b is coupled to the conductive member of the substrate support 11 and is configured to generate a bias RF signal (bias RF power). The generated bias RF signal is supplied to the conductive member of the substrate support 11. In one embodiment, the bias RF signal has a lower frequency than the source RF signal. In one embodiment, the bias RF signal has a frequency in a range of 400 kHz to 13.56 MHz. In various embodiments, the amplitude of at least one of the source RF signal and the bias RF signal may be pulsed or modulated. Amplitude modulation may involve pulsing the RF signal amplitude between an on state and an off state, or between two or more different on states.

[0016] The power supply 30 may also include a DC power supply coupled to the plasma processing chamber 10. The DC power supply includes a bias DC generator. In one embodiment, the bias DC generator is connected to a conductive member of the substrate support 11 and configured to generate a bias DC signal. The generated bias DC signal is applied to the conductive member of the substrate support 11. In one embodiment, the bias DC signal may be applied to another electrode, such as an electrode in an electrostatic chuck. In one embodiment, the bias DC signal may be pulsed. The bias DC generator may also be provided in addition to the RF power supply or instead of the second RF generator.

[0017] The exhaust system 40 may be connected to, for example, an exhaust port 10e provided at the bottom of the plasma processing chamber 10. The exhaust system 40 may include a pressure valve and a vacuum pump. The vacuum pump may include a turbomolecular pump, a roughing pump, or a combination thereof.

[0018] The spectrometer 60 detects the emission spectrum of the plasma in the plasma processing space 10s. The spectrometer 60 detects the emission intensity in a wavelength range from 200 nanometers to 900 nanometers, for example. Note that the wavelength range detected by the spectrometer 60 is not limited to the above, and the spectrometer 60 may also detect the emission intensity in a wavelength range from 200 nanometers to 1100 nanometers, for example.

[0019] The controller 2 processes computer-executable instructions that cause the plasma processing apparatus 1 to perform the various processes described in this disclosure. The controller 2 may be configured to control each element of the plasma processing apparatus 1 to perform the various processes described herein. In one embodiment, part or all of the controller 2 may be included in the plasma processing apparatus 1. The controller 2 may include, for example, a computer 2a. The computer 2a may include, for example, a processing unit (CPU: Central Processing Unit) 2a1, a storage unit 2a2, and a communication interface 2a3. The processing unit 2a1 may be configured to perform various control operations based on programs stored in the storage unit 2a2. The storage unit 2a2 may include a random access memory (RAM), a read-only memory (ROM), a hard disk drive (HDD), a solid state drive (SSD), or a combination thereof. The communication interface 2a3 may communicate with the plasma processing apparatus 1 via a communication line such as a LAN (Local Area Network).

[0020] The process in the plasma processing apparatus according to this embodiment will be described below. By describing the process in the plasma processing apparatus according to this embodiment, the end point detection method executed by the plasma processing apparatus according to this embodiment will be described.

[0021] For example, in a 3D NAND flash memory, a structure has been proposed in which contacts are provided through contact holes of different depths, as opposed to the conventional structure in which contacts are provided in each layer in a stepped manner. For example, when silicon oxide layers and silicon nitride layers are alternately stacked, it is necessary to stop etching at each silicon oxide layer and silicon nitride layer. Therefore, it is important to detect the end point at each silicon oxide layer and silicon nitride layer.

[0022] When etching a laminated film in which first and second layers are alternately stacked, the amount of etchant decreases when etching the first layer and the amount of by-products produced when etching the first layer increases. Similarly, the amount of etchant decreases when etching the second layer and the amount of by-products produced when etching the second layer increases.

[0023] Therefore, the inventors have developed the plasma processing apparatus according to the present embodiment by noting that when the first layer is etched, the amount of light emitted by by-products produced during etching of the first layer increases, and when the second layer is etched, the amount of light emitted by by-products produced during etching of the second layer increases. Furthermore, the inventors have developed the plasma processing apparatus according to the present embodiment by noting that when the first layer and the second layer are etched, the amount of etchant decreases.

[0024] When etching a laminated film in which first and second layers are alternately stacked, the plasma processing apparatus according to this embodiment detects the emission intensities in the wavelength bands caused by the by-products produced when etching the first layer and the by-products produced when etching the second layer. Furthermore, the plasma processing apparatus according to this embodiment detects the end points of the first and second layers based on the emission intensities in the wavelength bands caused by the by-products produced when etching the first layer and the emission intensities in the wavelength bands caused by the by-products produced when etching the second layer. Furthermore, the plasma processing apparatus according to this embodiment detects the emission intensities in the wavelength bands caused by the etchant and corrects the emission intensities caused by the by-products.

[0025] Here, the description will be given using a plasma processing apparatus 1, which is an example of the plasma processing apparatus according to the present embodiment. Fig. 2 is a flow chart illustrating the processing of the plasma processing apparatus 1, which is an example of the plasma processing apparatus according to the present embodiment.

[0026] (Step S10) First, the control unit 2 in the plasma processing apparatus 1 executes a pre-processing step for executing the etching process. Specifically, the control unit 2 controls the loading of a wafer from the outside. Then, the control unit 2 controls the placement of the wafer on the substrate support unit 11.

[0027] Here, a description will be given of the wafer W1 processed by the plasma processing apparatus 1. Fig. 3 is a diagram for explaining an outline of the laminated film SL processed by the plasma processing apparatus 1, which is an example of the plasma processing apparatus according to this embodiment.

[0028] The wafer W1 has a laminated film SL formed on a substrate BS, the laminated film SL including a first layer L1 containing silicon and oxygen, more specifically, a silicon oxide film, and a second layer L2 containing silicon and nitrogen, more specifically, a silicon nitride film, stacked alternately. The wafer W1 also has a mask MK on the laminated film SL.

[0029] The plasma processing apparatus 1 etches the openings of the mask MK in the laminated film SL. When etching the laminated film SL, the plasma processing apparatus 1 alternately etches the first layer L1 and the second layer L2.

[0030] (Step S20) Next, the control unit 2 starts the etching process. Because the wafer W1 has the first layer L1 directly below the mask MK, the control unit 2 sets the process gas, temperature conditions, etc. so as to etch the first layer L1, and generates plasma to start the process.

[0031] In the plasma processing apparatus 1, hydrogen fluoride (HF) gas is used as a processing gas when etching each of the first layer L1 and the second layer L2. The flow rate of the hydrogen fluoride gas in the processing gas may be 70% by volume or more.

[0032] In addition to hydrogen fluoride gas, the processing gas may contain at least one gas selected from the group consisting of a carbon-containing gas, an oxygen-containing gas, a halogen-containing gas, and a phosphorus-containing gas. The carbon-containing gas may contain at least one gas selected from the group consisting of a fluorocarbon gas, a hydrofluorocarbon gas, and a hydrocarbon gas.

[0033] (Step S30) Next, the control unit 2 acquires a reference emission intensity, which is an emission intensity in a reference wavelength band caused by the etchant, from the spectrometer 60. The plasma processing apparatus 1 uses hydrogen fluoride as the etchant. Therefore, the control unit 2 acquires an emission intensity in a wavelength band caused by hydrogen and fluorine contained in the hydrogen fluoride, which is the etchant.

[0034] The emission intensity in a wavelength band may be the emission intensity at a wavelength having a high emission intensity among wavelengths included in the wavelength band, or may be the average or integrated value of the emission intensities at wavelengths included in the wavelength band. The same applies to the emission intensities in the following wavelength bands.

[0035] The wavelength band caused by hydrogen is, for example, at least one of a wavelength band including 483 nanometers and a wavelength band including 656 nanometers. More specifically, the wavelength band caused by hydrogen is, for example, a wavelength band including at least one of the line spectrum of the Balmer series of hydrogen atoms, for example, 656.3, 486.1, 434.1, 410.2, and 397.0 nanometers. The wavelength band caused by fluorine is, for example, at least one of a wavelength band including 704 nanometers and a wavelength band including 713 nanometers. More specifically, the wavelength band caused by fluorine is, for example, a wavelength band including at least one of the line spectrum of fluorine atoms, for example, 720.2, 712.8, 703.7, 696.6, 691.0, 690.2, and 685.6 nanometers.

[0036] (Step S40) Next, the control unit 2 acquires a first emission intensity, which is the emission intensity in a first wavelength band caused by oxygen, from the spectrometer 60. The first layer L1 is a layer containing silicon and oxygen. Therefore, when the first layer L1 is being etched, it is expected that the emission of atoms, molecules, or ions caused by oxygen contained in the first layer L1 will increase. Therefore, the control unit 2 acquires the emission intensity in the wavelength band caused by oxygen.

[0037] The following describes the measurement results of the emission intensity measured in the plasma processing apparatus 1, which is an example of the plasma processing apparatus according to this embodiment. Each of Figures 5 to 12 is a diagram illustrating an example of the emission spectrum measured in the plasma processing apparatus 1, which is an example of the plasma processing apparatus according to this embodiment.

[0038] The horizontal axis in each of Figures 5 to 12 represents wavelength (unit: nanometers). The vertical axis in each of Figures 5 to 12 represents detected emission intensity (unit: arbitrary unit). In each of Figures 5 to 12, the solid line represents the emission intensity when a silicon oxide film is etched, and the dotted line represents the emission intensity when a silicon nitride film is etched.

[0039] Figure 5 shows the results for the wavelength band from 210 nanometers to 250 nanometers. Figure 6 shows the results for the wavelength band from 250 nanometers to 275 nanometers. Figure 7 shows the results for the wavelength band from 285 nanometers to 340 nanometers. Figure 8 shows the results for the wavelength band from 350 nanometers to 365 nanometers. Figure 9 shows the results for the wavelength band from 375 nanometers to 395 nanometers. Figure 10 shows the results for the wavelength band from 410 nanometers to 433 nanometers. Figure 11 shows the results for the wavelength band from 710 nanometers to 750 nanometers. Figure 12 shows the results for the wavelength band from 770 nanometers to 780 nanometers.

[0040] In the plasma processing apparatus according to this embodiment, a wavelength band in which the difference in emission intensity is large when etching a silicon oxide film and a silicon nitride film and the emission intensity is high when etching silicon oxide is adopted as the first wavelength band. Note that one or more of the wavelength bands listed below may be selected as the first wavelength band.

[0041] For example, wavelength bands attributed to oxygen include a wavelength band attributed to oxygen atoms (O) and a wavelength band attributed to hydroxyl radicals (OH). The wavelength band attributed to oxygen atoms is, for example, at least one of a wavelength band including 777 nanometers (see FIG. 12) and a wavelength band including 844 nanometers. More specifically, the wavelength band attributed to oxygen atoms is, for example, a wavelength band including at least one of the line spectra of oxygen atoms, for example, 777.2, 777.4, 794.8, and 844.6. The wavelength band attributed to hydroxyl radicals is, for example, at least one of a wavelength band including 309 nanometers (see FIG. 7) and a wavelength band including 324 nanometers (see FIG. 7). More specifically, the wavelength band attributed to hydroxyl radicals is, for example, at least one of a wavelength band from 306 nanometers to 313 nanometers, including 308.9 nanometers, and a wavelength band from 323 nanometers to 328 nanometers.

[0042] (Step S50) Next, the control unit 2 acquires a second emission intensity, which is the emission intensity in a second wavelength band caused by nitrogen, from the spectrometer 60. The second layer L2 is a layer containing silicon and nitrogen. Therefore, when the second layer L2 is being etched, it is expected that the emission of atoms, molecules, or ions caused by the nitrogen contained in the second layer L2 will increase. Therefore, the control unit 2 acquires the emission intensity in the wavelength band caused by nitrogen.

[0043] In the plasma processing apparatus according to this embodiment, a wavelength band in which the difference in emission intensity is large when etching a silicon oxide film and a silicon nitride film and the emission intensity is high when etching silicon nitride is adopted as the second wavelength band. Note that one or more of the wavelength bands listed below may be selected as the second wavelength band.

[0044] For example, wavelength bands attributed to nitrogen include wavelength bands attributed to nitrogen molecules (N), nitrogen molecule cations (N), nitrogen molecules (N), hydrogen nitride molecules (NH), and carbon nitride molecules (CN). Of the wavelength bands listed below, one wavelength band or multiple wavelength bands may be selected.

[0045] The wavelength band caused by nitrogen molecules is, for example, a wavelength band including at least one of 225 nanometers to 235 nanometers (see FIG. 5), 350 nanometers to 360 nanometers (see FIG. 8), and 375 nanometers to 390 nanometers (see FIG. 9). More specifically, the wavelength band caused by nitrogen molecules is, for example, at least one of 294 nanometers to 298 nanometers, 311 nanometers to 316 nanometers, 352 nanometers to 359 nanometers, and 380 nanometers to 392 nanometers.

[0046] The wavelength band caused by nitrogen molecular cations is, for example, a wavelength band including 388 nanometers (see FIG. 9 ). More specifically, the wavelength band caused by nitrogen molecular cations is, for example, at least one of a wavelength band from 352 nanometers to 359 nanometers and a wavelength band from 380 nanometers to 389 nanometers.

[0047] The wavelength band caused by nitrogen molecules and hydrogen nitride molecules is, for example, a wavelength band including 335 nanometers (see FIG. 7 ). More specifically, the wavelength band caused by nitrogen molecules and hydrogen nitride molecules is, for example, a wavelength band including at least one of 335 nanometers and 337 nanometers. Note that, for example, the wavelength band caused by nitrogen molecules and hydrogen nitride molecules may be a wavelength band including 367 nanometers.

[0048] The wavelength band attributed to carbon nitride molecules is a wavelength band including at least one of 358 nanometers to 359 nanometers (see FIG. 8), 385 nanometers to 388.5 nanometers (see FIG. 9), and 415 nanometers to 428 nanometers (see FIG. 10). More specifically, the wavelength band attributed to carbon nitride molecules is, for example, at least one of 385 nanometers to 388.5 nanometers and 415 nanometers to 421 nanometers.

[0049] (Step S60) Next, the control unit 2 detects the etching end point. Specifically, the control unit 2 detects the etching end point in the first layer L1 when the first emission intensity acquired in step S40 decreases and the second emission intensity acquired in step S50 increases. The control unit 2 also detects the etching end point in the second layer L2 when the second emission intensity acquired in step S50 decreases and the first emission intensity acquired in step S40 increases.

[0050] The control unit 2 may determine whether the first emission intensity is increasing and the second emission intensity is decreasing, or whether the first emission intensity is decreasing and the second emission intensity is increasing, using an equation that combines the first emission intensity and the second emission intensity using a linear equation. Furthermore, the control unit 2 may determine whether the first emission intensity is increasing and the second emission intensity is decreasing, or whether the first emission intensity is decreasing and the second emission intensity is increasing, using a ratio between the first emission intensity and the second emission intensity.

[0051] The criteria by which the control unit 2 determines the end of etching are not limited to the above. For example, the control unit 2 may detect the end point of etching on the first layer L1 when the first emission intensity acquired in step S40 decreases. Alternatively, the control unit 2 may detect the end point of etching on the first layer L1 when the second emission intensity acquired in step S50 increases. In summary, the control unit 2 may detect the end point of etching on the first layer L1 at least when the first emission intensity acquired in step S40 decreases or when the second emission intensity acquired in step S50 increases.

[0052] Furthermore, for example, the control unit 2 may detect the end point of etching in the second layer L2 when the second emission intensity acquired in step S50 decreases. Alternatively, the control unit 2 may detect the end point of etching in the second layer L2 when the first emission intensity acquired in step S40 increases. In summary, the control unit 2 may detect the end point of etching in the second layer L2 at least when the second emission intensity acquired in step S50 decreases or when the first emission intensity acquired in step S40 increases.

[0053] When detecting the etching end point, correction may be made using the emission intensity in the wavelength band due to the etchant. Specifically, the control unit 2 obtains a first corrected emission intensity by dividing the first emission intensity obtained in step S40 by the reference emission intensity obtained in step S30. Furthermore, the control unit 2 obtains a second corrected emission intensity by dividing the second emission intensity by the reference emission intensity obtained in step S30 in step S50. The control unit 2 then detects the etching end point of the first layer when the first corrected emission intensity decreases and the second corrected emission intensity increases. Furthermore, the control unit 2 detects the etching end point of the second layer when the second corrected emission intensity decreases and the first corrected emission intensity increases.

[0054] As described above, the control unit 2 may detect the end point of etching in the first layer L1 when the first corrected emission intensity decreases or when the second corrected emission intensity increases. The control unit 2 may detect the end point of etching in the second layer L2 when the second corrected emission intensity decreases or when the first corrected emission intensity increases.

[0055] (Step S70) Next, in step S60, the control unit 2 determines whether the etching end point of the first layer L1 or the second layer L2 has been detected. If the etching end point has been detected (YES in step S70), the control unit 2 proceeds to step S80. If the etching end point has not been detected (NO in step S70), the control unit 2 returns to step S30 and repeats the process.

[0056] (Step S80) When the etching end point is detected in step S60 (YES in step S70), the control unit 2 stops the etching. Specifically, the control unit 2 stops the supply of the processing gas and stops the generation of plasma.

[0057] (Step S90) Next, the control unit 2 determines whether all layers of the stacked film SL have been etched. If all layers of the stacked film SL have been etched (YES in step S90), the control unit 2 proceeds to step S100. If all layers of the stacked film SL have not been etched, in other words, if the first layer L1 or the second layer L2 to be etched remains in the stacked film SL (NO in step S90), the control unit 2 proceeds to step S110.

[0058] 4 is a diagram illustrating an overview of a laminated film SL processed by a plasma processing apparatus 1, which is an example of a plasma processing apparatus according to this embodiment. Using FIG. 4, a wafer W2 in which all layers of the laminated film SL of the wafer W1 have been etched will be described. As shown in FIG. 4, when all layers of the laminated film SL have been etched (YES in step S90), through-holes TH that penetrate all the way to the substrate BS are formed, as in the wafer W2.

[0059] (Step S100) When all layers of the stacked film SL have been etched (YES in step S90), the control unit 2 executes a post-processing step. Specifically, the control unit 2 controls the processed wafer to be unloaded to the outside.

[0060] (Step S110) If all layers of the stacked film SL have not been etched, in other words, if the first layer L1 or the second layer L2 to be etched remains in the stacked film SL (NO in step S90), the control unit 2 changes the process conditions to etch the next layer. For example, if the first layer L1 has been etched, the process conditions are changed to etch the second layer L2. Also, if the second layer L2 has been etched, the process conditions are changed to etch the first layer L1.

[0061] The wavelength bands shown above are merely examples, and for example, a wavelength band caused by oxygen or a wavelength band caused by nitrogen may be appropriately selected from the wavelength bands shown in FIGS.

[0062] <Summary> The plasma processing apparatus according to this embodiment enables efficient endpoint detection when etching a laminated film having a first layer and a second layer. Furthermore, the plasma processing apparatus according to this embodiment enables endpoint detection for each of the first and second layers during the same etching process. Furthermore, the plasma processing apparatus according to this embodiment uses the emission intensity in the reference wavelength band, thereby suppressing the effects of variations in process conditions when etching each of the first and second layers.

[0063] Furthermore, according to the plasma processing apparatus of this embodiment, it is possible to detect the end point when etching a laminated film in which a first layer and a second layer are stacked, and therefore it is possible to switch the processing so that the processing can be performed under process conditions suitable for etching the first layer and the second layer, respectively.

[0064] The plasma processing apparatus according to the present embodiment disclosed herein should be considered to be illustrative in all respects and not restrictive. The above-described embodiments can be modified and improved in various ways without departing from the spirit and scope of the appended claims. The features described in the above-described embodiments can be configured in other ways as long as they are not inconsistent, and can be combined as long as they are not inconsistent.

[0065] The embodiments disclosed above include, for example, the following aspects: (Supplementary Note 1) A plasma processing apparatus comprising: a spectrometer that measures an emission intensity during plasma processing; and a controller that controls detection of an etching end point based on measurement results obtained by the spectrometer, wherein the controller, when etching a stacked film in which first layers containing silicon and oxygen and second layers containing silicon and nitrogen are alternately stacked using plasma, performs the following steps: (a) acquiring from the spectrometer during plasma processing a first emission intensity, which is an emission intensity in a first wavelength band caused by the oxygen, (b) acquiring from the spectrometer during plasma processing a second emission intensity, which is an emission intensity in a second wavelength band caused by the nitrogen, which is different from the first wavelength band, and (c) detecting the etching end point of the first layer when the first emission intensity decreases and the second emission intensity increases, and detecting the etching end point of the second layer when the second emission intensity decreases and the first emission intensity increases.

[0066] (Supplementary Note 2) The plasma processing apparatus according to Supplementary Note 1, wherein the control unit executes the step (d) of acquiring from the spectrometer during plasma processing a reference emission intensity, which is an emission intensity in a reference wavelength band caused by an etchant; and in the step (c), the control unit executes the steps of: (c-1) determining a first corrected emission intensity by dividing the first emission intensity by the reference emission intensity; (c-2) determining a second corrected emission intensity by dividing the second emission intensity by the reference emission intensity; and (c-3) detecting an end point of etching in the first layer when the first corrected emission intensity decreases and the second corrected emission intensity increases, and detecting an end point of etching in the second layer when the second corrected emission intensity decreases and the first corrected emission intensity increases.

[0067] (Supplementary Note 3) The plasma processing apparatus according to any one of Supplementary Note 1 and Supplementary Note 2, wherein the first wavelength band is a wavelength band caused by at least one of oxygen atoms and hydroxyl radicals.

[0068] (Supplementary Note 4) The plasma processing apparatus according to Supplementary Note 3, wherein the wavelength band caused by oxygen atoms is a wavelength band including at least one of 777.2, 777.4, 794.8, and 844.6 nanometers.

[0069] (Supplementary Note 5) The plasma processing apparatus according to Supplementary Note 3, wherein the wavelength band caused by the hydroxyl radicals is a wavelength band including at least one of 309 nanometers and 324 nanometers.

[0070] (Supplementary Note 6) The plasma processing apparatus according to any one of Supplementary Note 1 to Supplementary Note 5, wherein the second wavelength band is a wavelength band caused by at least one of nitrogen molecules, nitrogen molecule cations, nitrogen molecules and hydrogen nitride molecules, and carbon nitride molecules.

[0071] (Supplementary Note 7) The plasma processing apparatus according to Supplementary Note 6, wherein the wavelength band caused by the nitrogen molecules is a wavelength band including at least one of 294 nanometers to 298 nanometers, 311 nanometers to 316 nanometers, 352 nanometers to 359 nanometers, and 380 nanometers to 392 nanometers.

[0072] (Supplementary Note 8) The plasma processing apparatus according to Supplementary Note 6, wherein the wavelength band caused by the nitrogen molecular cations is a wavelength band including at least one of 352 nanometers to 359 nanometers and 380 nanometers to 389 nanometers.

[0073] (Supplementary Note 9) The plasma processing apparatus according to Supplementary Note 6, wherein the wavelength band caused by the nitrogen molecules and hydrogen nitride molecules is a wavelength band including at least one of 335 nanometers and 337 nanometers.

[0074] (Supplementary Note 10) The plasma processing apparatus according to Supplementary Note 6, wherein the wavelength band caused by the carbon nitride molecules is a wavelength band including at least one of 385 nanometers to 388.5 nanometers and 415 nanometers to 428 nanometers.

[0075] (Supplementary Note 11) An endpoint detection method for detecting an endpoint of etching in each of a first layer and a second layer when etching a laminated film in which first layers containing silicon and oxygen and second layers containing silicon and nitrogen are alternately stacked using plasma, the endpoint detection method comprising: (a) acquiring, during plasma processing, a first emission intensity which is an emission intensity in a first wavelength band caused by the oxygen; (b) acquiring, during plasma processing, a second emission intensity which is an emission intensity in a second wavelength band caused by the nitrogen, which is different from the first wavelength band; and (c) detecting the endpoint of etching in the first layer when the first emission intensity decreases and the second emission intensity increases, and detecting the endpoint of etching in the second layer when the second emission intensity decreases and the first emission intensity increases.

[0076] (Supplementary Note 12) The endpoint detection method according to Supplementary Note 11, comprising the steps of: (d) acquiring a reference emission intensity, which is an emission intensity in a reference wavelength band caused by an etchant, during plasma processing; and in the step (c), comprising: (c-1) determining a first corrected emission intensity by dividing the first emission intensity by the reference emission intensity; (c-2) determining a second corrected emission intensity by dividing the second emission intensity by the reference emission intensity; and (c-3) detecting an endpoint of etching in the first layer when the first corrected emission intensity decreases and the second corrected emission intensity increases, and detecting an endpoint of etching in the second layer when the second corrected emission intensity decreases and the first corrected emission intensity increases.

[0077] (Supplementary Note 13) The endpoint detection method according to Supplementary Note 11 or Supplementary Note 12, wherein the first wavelength band is a wavelength band attributable to at least one of oxygen atoms and hydroxyl radicals.

[0078] (Supplementary Note 14) The endpoint detection method according to Supplementary Note 13, wherein the wavelength band caused by oxygen atoms is a wavelength band including at least one of 777.2, 777.4, 794.8, and 844.6 nanometers.

[0079] (Supplementary Note 15) The endpoint detection method according to Supplementary Note 13, wherein the wavelength band caused by hydroxyl radicals is a wavelength band including at least one of 309 nanometers and 324 nanometers.

[0080] (Supplementary Note 16) The endpoint detection method according to any one of Supplementary Note 11 to Supplementary Note 15, wherein the second wavelength band is a wavelength band caused by at least one of nitrogen molecules, nitrogen molecule cations, nitrogen molecules and hydrogen nitride molecules, and carbon nitride molecules.

[0081] (Supplementary Note 17) The endpoint detection method according to Supplementary Note 16, wherein the wavelength band caused by nitrogen molecules is a wavelength band including at least one of 294 nanometers to 298 nanometers, 311 nanometers to 316 nanometers, 352 nanometers to 359 nanometers, and 380 nanometers to 392 nanometers.

[0082] (Supplementary Note 18) The endpoint detection method according to Supplementary Note 16, wherein the wavelength band caused by the nitrogen molecular cations is a wavelength band including at least one of 352 nanometers to 359 nanometers and 380 nanometers to 389 nanometers.

[0083] (Supplementary Note 19) The endpoint detection method according to Supplementary Note 16, wherein the wavelength band caused by the nitrogen molecules and hydrogen nitride molecules is a wavelength band including at least one of 335 nanometers and 337 nanometers.

[0084] (Supplementary Note 20) The endpoint detection method according to Supplementary Note 16, wherein the wavelength band caused by the carbon nitride molecules is a wavelength band including at least one of 385 nanometers to 388.5 nanometers and 415 nanometers to 428 nanometers.

[0085] (Supplementary Note 21) A plasma processing apparatus comprising: a spectrometer that measures emission intensity during plasma processing; and a control unit that controls detection of an etching end point based on measurement results obtained by the spectrometer, wherein the control unit performs the following steps when etching a stacked film in which first layers containing silicon and oxygen and second layers containing silicon and nitrogen are alternately stacked using plasma: (a) acquiring from the spectrometer during plasma processing a first emission intensity that is emission intensity in a first wavelength band caused by the oxygen; (b) acquiring from the spectrometer during plasma processing a second emission intensity that is emission intensity in a second wavelength band caused by the nitrogen, which is different from the first wavelength band; and (c) detecting an etching end point in the first layer when at least one of the first emission intensity and the second emission intensity decreases, and detecting an etching end point in the second layer when at least one of the second emission intensity and the first emission intensity increases.

[0086] (Supplementary Note 22) An endpoint detection method for detecting an endpoint of etching in each of a first layer and a second layer when etching a laminated film in which first layers containing silicon and oxygen and second layers containing silicon and nitrogen are alternately stacked using plasma, the endpoint detection method comprising: (a) acquiring, during plasma processing, a first emission intensity which is an emission intensity in a first wavelength band caused by the oxygen; (b) acquiring, during plasma processing, a second emission intensity which is an emission intensity in a second wavelength band caused by the nitrogen, which is different from the first wavelength band; and (c) detecting the endpoint of etching in the first layer at least when the first emission intensity decreases or the second emission intensity increases, and detecting the endpoint of etching in the second layer at least when the second emission intensity decreases or the first emission intensity increases.

[0087] This application claims priority from basic patent application No. 2023-071801, filed with the Japan Patent Office on April 25, 2023, the entire contents of which are incorporated herein by reference.

[0088] REFERENCE SIGNS LIST 1 Plasma processing apparatus 2 Control unit 10 Plasma processing chamber 10e Exhaust port 10s Plasma processing space 11 Substrate support unit 13 Upper electrode shower head 20 Gas supply unit 21 Gas source 22 Flow rate controller 30 Power supply unit 40 Exhaust system 60 Spectrometer L1 First layer L2 Second layer MK Mask SL Stacked film W1 Wafer

Claims

1. A plasma processing apparatus comprising: a spectrometer that measures an emission intensity during plasma processing; and a control unit that controls detection of an etching end point based on measurement results obtained by the spectrometer, wherein the control unit performs the following steps when etching a laminated film in which a first layer containing silicon and oxygen and a second layer containing silicon and nitrogen are alternately stacked using plasma: (a) acquiring from the spectrometer a first emission intensity during plasma processing, the first emission intensity being the emission intensity in a first wavelength band caused by the oxygen; (b) acquiring from the spectrometer a second emission intensity during plasma processing, the second emission intensity being the emission intensity in a second wavelength band caused by the nitrogen, the second wavelength band being different from the first wavelength band; and (c) detecting an etching end point in the first layer when the first emission intensity decreases and the second emission intensity increases, and detecting an etching end point in the second layer when the second emission intensity decreases and the first emission intensity increases.

2. The plasma processing apparatus of claim 1, wherein the control unit executes the steps of: (d) acquiring from the spectrometer during plasma processing a reference emission intensity, which is an emission intensity in a reference wavelength band caused by an etchant; and in the step (c), executing the steps of: (c-1) obtaining a first corrected emission intensity by dividing the first emission intensity by the reference emission intensity; (c-2) obtaining a second corrected emission intensity by dividing the second emission intensity by the reference emission intensity; and (c-3) detecting an end point of etching in the first layer when the first corrected emission intensity decreases and the second corrected emission intensity increases, and detecting an end point of etching in the second layer when the second corrected emission intensity decreases and the first corrected emission intensity increases.

3. The plasma processing apparatus according to claim 1, wherein the first wavelength band is a wavelength band caused by at least one of oxygen atoms and hydroxyl radicals.

4. The plasma processing apparatus according to claim 3, wherein the wavelength band caused by the oxygen atoms is a wavelength band including at least any one of 777.2, 777.4, 794.8, and 844.6 nanometers.

5. The plasma processing apparatus according to claim 3, wherein the wavelength band caused by the hydroxyl radicals is a wavelength band including at least one of 309 nanometers and 324 nanometers.

6. A plasma processing apparatus according to claim 1 or claim 2, wherein the second wavelength band is a wavelength band caused by at least one of nitrogen molecules, nitrogen molecule cations, nitrogen molecules and hydrogen nitride molecules, and carbon nitride molecules.

7. The plasma processing apparatus according to claim 6, wherein the wavelength band caused by the nitrogen molecules is a wavelength band including at least any one of 294 nanometers to 298 nanometers, 311 nanometers to 316 nanometers, 352 nanometers to 359 nanometers, and 380 nanometers to 392 nanometers.

8. The plasma processing apparatus according to claim 6, wherein the wavelength band caused by the nitrogen molecular ions is a wavelength band including at least one of 352 nanometers to 359 nanometers and 380 nanometers to 389 nanometers.

9. The plasma processing apparatus according to claim 6, wherein the wavelength band caused by the nitrogen molecules and hydrogen nitride molecules is a wavelength band including at least one of 335 nanometers and 337 nanometers.

10. The plasma processing apparatus according to claim 6, wherein the wavelength band caused by the carbon nitride molecules is a wavelength band including at least one of 385 nanometers to 388.5 nanometers and 415 nanometers to 428 nanometers.

11. A method for detecting an end point of etching in each of a first layer and a second layer when a laminate film in which a first layer containing silicon and oxygen and a second layer containing silicon and nitrogen are alternately stacked is etched with plasma, the method comprising: (a) acquiring a first emission intensity during plasma processing, the first emission intensity being an emission intensity in a first wavelength band caused by the oxygen; (b) acquiring a second emission intensity during plasma processing, the second emission intensity being an emission intensity in a second wavelength band caused by the nitrogen, the second wavelength band being different from the first wavelength band; and (c) detecting an end point of etching in the first layer when the first emission intensity decreases and the second emission intensity increases, and detecting an end point of etching in the second layer when the second emission intensity decreases and the first emission intensity increases.

12. The endpoint detection method according to claim 11, further comprising: (d) a step of acquiring a reference emission intensity, which is an emission intensity in a reference wavelength band caused by an etchant, during plasma processing, wherein in the step (c), the steps of: (c-1) determining a first corrected emission intensity by dividing the first emission intensity by the reference emission intensity; (c-2) determining a second corrected emission intensity by dividing the second emission intensity by the reference emission intensity; and (c-3) detecting an endpoint of etching in the first layer when the first corrected emission intensity decreases and the second corrected emission intensity increases, and detecting an endpoint of etching in the second layer when the second corrected emission intensity decreases and the first corrected emission intensity increases.

13. The endpoint detection method according to claim 11 or 12, wherein the first wavelength band is a wavelength band attributable to at least one of oxygen atoms and hydroxyl radicals.

14. The endpoint detection method according to claim 13, wherein the wavelength band caused by oxygen atoms is a wavelength band including at least one of 777.2, 777.4, 794.8, and 844.6 nanometers.

15. The method for detecting an end point according to claim 13, wherein the wavelength band attributable to hydroxyl radicals is a wavelength band including 309 nanometers or 324 nanometers.

16. The endpoint detection method according to claim 11 or 12, wherein the second wavelength band is a wavelength band caused by at least one of nitrogen molecules, nitrogen molecule cations, nitrogen molecules and hydrogen nitride molecules, and carbon nitride molecules.

17. The endpoint detection method according to claim 16, wherein the wavelength band caused by the nitrogen molecules is a wavelength band including at least one of 294 nanometers to 298 nanometers, 311 nanometers to 316 nanometers, 352 nanometers to 359 nanometers, and 380 nanometers to 392 nanometers.

18. The endpoint detection method according to claim 16, wherein the wavelength band caused by the nitrogen molecular cations is a wavelength band including at least one of 352 nanometers to 359 nanometers and 380 nanometers to 389 nanometers.

19. The endpoint detection method according to claim 16, wherein the wavelength band caused by the nitrogen molecules and hydrogen nitride molecules is a wavelength band including at least one of 335 nanometers and 337 nanometers.

20. The endpoint detection method according to claim 16, wherein the wavelength band attributable to the carbon nitride molecules is a wavelength band including at least one of 385 nanometers to 388.5 nanometers and 415 nanometers to 428 nanometers.

21. A plasma processing apparatus comprising: a spectrometer that measures an emission intensity during plasma processing; and a control unit that controls detection of an end point of etching based on measurement results obtained by the spectrometer, wherein the control unit performs the following steps when etching a laminated film in which a first layer containing silicon and oxygen and a second layer containing silicon and nitrogen are alternately stacked with plasma: (a) acquiring from the spectrometer a first emission intensity that is an emission intensity in a first wavelength band caused by the oxygen during plasma processing; (b) acquiring from the spectrometer a second emission intensity that is an emission intensity in a second wavelength band caused by the nitrogen, different from the first wavelength band; and (c) detecting an end point of etching in the first layer at least when the first emission intensity decreases or when the second emission intensity increases, and detecting an end point of etching in the second layer at least when the second emission intensity decreases or when the first emission intensity increases.

22. A method for detecting an end point of etching in each of a first layer and a second layer when a laminated film in which a first layer containing silicon and oxygen and a second layer containing silicon and nitrogen are alternately stacked is etched with plasma, the method comprising: (a) acquiring a first emission intensity during plasma processing, which is an emission intensity in a first wavelength band caused by the oxygen; (b) acquiring a second emission intensity during plasma processing, which is an emission intensity in a second wavelength band caused by the nitrogen, different from the first wavelength band; and (c) detecting an end point of etching in the first layer at least when the first emission intensity decreases or when the second emission intensity increases, and detecting an end point of etching in the second layer at least when the second emission intensity decreases or when the first emission intensity increases.

Citation Information

Patent Citations

  • Plasma etching device

    JP1988211633A

  • Method of manufacturing mask for extreme ultraviolet exposure

    JP2011187804A

  • Manufacturing method of semiconductor device and method of detecting endpoint of dry etching

    JP2017045871A

  • Method for etching silicon oxide and silicon nitride mutually and selectively

    JP2018046185A

  • Method for manufacturing a thin-film transistor substrate

    WO2011152018A1