Ceramic scintillator, photon counting type x-ray detector, and method for manufacturing ceramic scintillator
A ceramic scintillator using a garnet compound with Pr optimizes decay time and light emission to address high counting rate challenges in X-ray detectors, enabling efficient and accurate energy measurement and improved imaging.
Patent Information
- Application Number
- PCT/JP2024/015837
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-25
- Filing Date
- 2024-04-23
- Publication Date
- 2024-10-31
AI Technical Summary
Current X-ray detectors, both direct and indirect types, face challenges in handling high counting rates, leading to signal pile-up and inaccurate energy measurement, and existing scintillators cannot support the required counting rates for fast imaging applications like X-ray CT, resulting in decreased throughput and temporal resolution.
A ceramic scintillator made of a garnet compound containing Pr, with a specific absorption rate and light emission characteristics, is developed to handle high counting rates by optimizing the decay time constant and light emission amount, enabling accurate energy measurement and improved imaging capabilities.
The ceramic scintillator with a decay time constant of 17 ns or less and light emission of 10,000 ph/MeV or more effectively prevents signal pile-up, allowing for high counting rate handling and improved imaging performance, including enhanced S/N ratio and energy resolution.
Smart Images

Figure JP2024015837_31102024_PF_FP_ABST
Abstract
Description
Ceramic scintillator, photon counting X-ray detector, and method for manufacturing ceramic scintillator
[0001] FIELD Embodiments of the present invention relate to a ceramic scintillator, a photon-counting X-ray detector, and a method for manufacturing a ceramic scintillator.
[0002] Imaging systems using radiation, for example, X-rays, are widely used in industrial applications such as baggage inspection and non-destructive testing, and in medical applications such as X-ray diagnostic devices and X-ray CT (Computed Tomography) devices. The current mainstream detection method in X-ray imaging systems is the energy integration type, which generally consists of a combination of a luminescent material and a photodetector.
[0003] However, energy-integrating detectors have the drawbacks of being unable to obtain X-ray energy information and of resulting in a large amount of radiation exposure. In recent years, development of X-ray detectors that employ the photon-counting method has been progressing to solve these problems. Photon-counting X-ray detectors are also called photon detectors or photon-counting detectors.
[0004] The photon counting method is characterized by performing pulse signal processing on each incident X-ray photon. Photon counting methods are further classified into direct types, which use semiconductors such as CdTe to directly convert X-rays into electrical signals, and indirect types, which use luminescent materials to convert X-rays into light, which is then converted into electrical signals by a photodetector.
[0005] Among photon counting methods, direct photon counting can measure the energy of X-ray photons from the number of carriers, while indirect photon counting can measure the energy of X-ray photons from the number of emitted photons. Furthermore, because noise components can be easily removed, data with a high S / N ratio can be obtained. These advantages are expected to lead to new functional diagnostics and reduced radiation exposure through low-dose measurements in medical applications. The mainstream of research and development in photon counting is the direct photon counting method, which can achieve high energy resolution. However, the direct photon counting method faces challenges such as the high cost of semiconductor materials such as CdTe, the difficulty in obtaining uniform characteristics and the difficulty in manufacturing large-area detectors, and the signal pile-up phenomenon caused by the slow response speed of the material.
[0006] On the other hand, photomultiplier tubes with high multiplication factors are generally used as photodetectors in indirect photon counting systems. However, the large size of photomultiplier tubes and the difficulty of configuring pixels in narrow gaps have been issues with indirect systems. Silicon photomultipliers (Si-PMs), which are Si-based photodetectors that operate in Geiger mode and have been developed in recent years, have solved the issues mentioned above with photomultiplier tubes, have a multiplication factor close to that of photomultiplier tubes, and are low-cost. For this reason, it is expected that the use of silicon photomultipliers in indirect systems will expand in the future.
[0007] JP 2018-2974 A JP 2010-235388 A
[0008] A common technical issue for both direct and indirect detectors is their inability to handle high counting rates. The counting rate indicates the number of X-ray photons incident on a unit area and unit time, and corresponds to the intensity of the X-rays.
[0009] When taking a large amount of images in a short time using photon counting X-ray measurement, a detector that can handle a high count rate is required. This situation is necessary in X-ray CT, and the required count rate is 10 8 [cps / mm 2 This means that the X-ray photon is 1 [mm 2] at an average interval of 10 [nsec]. If the counting rate exceeds the capacity of the detector, overlapping of pulse signals occurs, making it difficult to measure the correct X-ray photon energy.
[0010] On the other hand, long-term measurements at a reduced count rate result in longer imaging times, which can lead to problems such as reduced throughput and reduced time resolution.Since the count rate that a detector can handle is primarily determined by the response speed of the material, improvements are expected.
[0011] An object of the present invention is to provide a ceramic scintillator that can accommodate a high counting rate, a photon-counting X-ray detector, and a method for manufacturing the ceramic scintillator.
[0012] A ceramic scintillator according to an embodiment is made of a garnet compound containing Pr, and has an absorptance at a wavelength of 320 nm relative to a wavelength of 280 nm of 0.15 or less.
[0013] 1A is a schematic diagram showing the configuration of a photon-counting X-ray detector according to an embodiment; FIG. 1B is an enlarged cross-sectional view of a partial region shown in FIG. 1A in a photon-counting X-ray detector according to an embodiment; FIG. 1C is a diagram showing, in a table form, the relationship between the absorptance at a wavelength of 320 [nm] relative to the absorptance at a wavelength of 280 [nm] (320 nm absorptance / 280 nm absorptance) and the relative light emission amount relative to the relative decay time constant (relative light emission amount / relative decay time constant) in an example; FIG. 1D is a diagram showing, in a graph form, changes in absorption spectrum in an example; and FIG. 1E is a diagram showing, in a table form, the relationship between the absorptance at a wavelength of 320 [nm] relative to the absorptance at a wavelength of 280 [nm] (320 nm absorptance / 280 nm absorptance) and the relative light emission amount relative to the relative decay time constant (relative light emission amount / relative decay time constant) in a comparative example. Embodiment
[0014] Hereinafter, embodiments of a ceramic scintillator, a photon-counting X-ray detector, and a method for manufacturing a ceramic scintillator will be described in detail with reference to the drawings.
[0015] (Photon-counting X-ray detector) Figures 1A to 1C are schematic diagrams showing the configuration of a photon-counting X-ray detector according to an embodiment. Figure 1A is a top view of the photon-counting X-ray detector according to an embodiment. Figure 1B is a side view showing the channel direction CH of the photon-counting X-ray detector according to an embodiment. Figure 1C is a side view showing the slice direction SL of the photon-counting X-ray detector according to an embodiment.
[0016] 1A to 1C show a photon-counting X-ray detector (hereinafter simply referred to as an "X-ray detector") 1 according to an embodiment. Also, 1B and 1C show a collimator device 3 in addition to the X-ray detector 1. 1C shows an X-ray tube 2 in addition to the X-ray detector 1.
[0017] The X-ray detector 1 is provided on a rotating frame of a gantry. The X-ray detector 1 has n (n: plural) X-ray detection elements 1n. The X-ray detection elements 1n are arranged two-dimensionally in a matrix in a channel direction and a slice direction SL. The channel direction refers to the direction in which the fan beam X-rays emitted from the X-ray tube 2 spreads, and the slice direction refers to the thickness direction of the fan beam X-rays.
[0018] The X-ray incident surface of the X-ray detector 1 is formed by the X-ray incident surfaces of the X-ray detection elements 1n. For example, about 1000 X-ray detection elements 1n are arranged in the channel direction CH and 64 in the slice direction SL.
[0019] The X-ray tube 2 is provided on a rotating frame of the gantry device so as to face the X-ray detector 1. The X-ray tube 2 is a vacuum tube that generates X-rays by applying a high voltage and irradiating thermions from a cathode (filament) to an anode (target). For example, the X-ray tube 2 may be a rotating anode type X-ray tube that generates X-rays by irradiating a rotating anode with thermions.
[0020] The collimator device 3 has multiple collimator plates that absorb scattered X-rays. The multiple collimator plates are made up of plates extending in the slice direction SL and erected to divide the X-ray detection elements 1n in the channel direction CH (a one-dimensional collimator). Alternatively, the multiple collimator plates are made up of plates extending in the slice direction SL and erected to divide the X-ray detection elements 1n in the channel direction CH, and plates extending in the channel direction CH and erected to divide the X-ray detection elements 1n in the slice direction SL (a two-dimensional collimator). The inclination of the collimator plate surfaces is adjusted so that they are parallel to the X-ray irradiation direction E, which is the direction in which X-rays from the X-ray focal point F of the X-ray tube 2 are irradiated. FIG. 1C shows a case in which the collimator device 3 is a one-dimensional collimator. Note that a combination of the X-ray detector 1 and the collimator device 3 is sometimes called a "photon-counting X-ray detector."
[0021] The X-ray detector 1 may be configured by modularizing a predetermined number of X-ray detection elements among the X-ray detection elements 1n and arranging a plurality of detector modules. Similarly, the collimator device 3 may be configured by modularizing a predetermined number of collimator plates and arranging a plurality of collimator modules.
[0022] FIG. 2 is an enlarged cross-sectional view of a partial region R shown in FIG. 1B in the X-ray detector 1. As shown in FIG.
[0023] The X-ray detection elements 1n are provided on a ceramic substrate 4. Each of the X-ray detection elements 1n includes a ceramic scintillator 11 and a photoelectric conversion element 12.
[0024] The ceramic scintillator 11 is an element that converts incident X-rays into photons and emits them. X-rays typically have a predetermined X-ray energy distribution. X-rays with a specific X-ray energy can be considered as a cluster of X-ray particles, the number of which corresponds to the magnitude of the X-ray energy. The ceramic scintillator 11 converts the X-ray particles into photons with a predetermined probability while maintaining the cluster of X-ray particles. In other words, when X-rays are incident on the ceramic scintillator 11, the ceramic scintillator 11 approximately simultaneously emits a number of photon groups corresponding to the X-ray energy, depending on the X-ray energy.
[0025] The ceramic scintillator 11 is a light conversion element having a substantially rectangular or cubic shape. The ceramic scintillator 11 is arranged so that its X-ray incident surface is approximately perpendicular to the X-ray irradiation direction, i.e., the X-ray incident direction E, and so that its side surface parallel to the X-ray incident direction E is approximately parallel to the channel direction CH and the slice direction SL.
[0026] The photoelectric conversion element 12 has a substantially rectangular plate-like shape, converts incident photons into an electrical signal, and outputs the electrical signal. The electrical signal is an electrical pulse signal corresponding to each incident photon. When a group of photons is simultaneously incident on the photoelectric conversion element 12, the photoelectric conversion element 12 outputs a pulse signal with a pulse height corresponding to the number of photons constituting the photon group. The photoelectric conversion element 12 is a semiconductor device suitable for so-called photon counting, such as a silicon photomultiplier (Si-PM). A silicon photomultiplier is a high-performance semiconductor photodetector capable of photon counting measurement and also applicable to analog measurement such as scintillation detection. A silicon photomultiplier is an element in which multiple avalanche photodiode (APD) pixels operating in Geiger mode are connected in parallel.
[0027] The photoelectric conversion element 12 receives photons emitted from the ceramic scintillator 11 and outputs a pulsed electrical signal. When the intensity of X-rays transmitted through the subject is sufficiently low, photon groups for each X-ray energy are emitted from the ceramic scintillator 11 in a state scattered along the time axis. At this time, the photoelectric conversion element 12 outputs pulse signals with pulse heights corresponding to the magnitude of the X-ray energy for each X-ray energy, the number of which corresponds to the dose of X-rays having that X-ray energy, scattered along the time axis. Therefore, by counting the pulse signals output within a certain period of time by pulse height, it is possible to determine the dose of X-rays transmitted through the subject for each X-ray energy. Furthermore, by counting all pulse signals output within a certain period of time regardless of pulse height, it is possible to determine the total dose of X-rays transmitted through the subject.
[0028] Conductor patterns (not shown) formed on the ceramic substrate 4 are connected to the photoelectric conversion elements 12. Electrical signals from the photoelectric conversion elements 12 are output to an external processing device (not shown) through these conductor patterns. The electrical signals output from the photoelectric conversion elements 12 are used to collect projection data using a photon counting method.
[0029] Detectors used in photon counting generally have very high X-ray detection sensitivity. High sensitivity means that a detector can obtain a signal with a sufficient S / N ratio even when the X-ray dose is low and the number of photons emitted from the scintillator is small. However, when the X-ray dose is high, pulse signals overlap, causing a phenomenon known as pile-up, which makes it impossible to resolve the signal in the time axis direction.
[0030] Indirect photon counting systems have the same problem of counting rate as direct systems. Counting rate refers to the number of X-ray photons incident on a unit area and unit time. To achieve imaging using a photon counting X-ray detector, a detector capable of a high counting rate is required. For example, the counting rate required for an X-ray CT device is 10 8 [cps / mm 2 This means that the X-ray photon is 1 [mm 2 This means that the photons are incident on an area of 1000 nm at intervals of 10 nsec on average. Currently, there are no practical scintillators that can handle such high counting rates. If the counting rate exceeds the capacity of the scintillator, pile-up occurs, making it difficult to measure the correct photon energy. On the other hand, long-term measurements with a suppressed counting rate cause problems such as reduced throughput and reduced time resolution.
[0031] The counting rate of a scintillator is primarily determined by the response speed of the material, so there is an urgent need to develop scintillator materials with improved response speeds to avoid long measurement times and pile-ups.
[0032] (Ceramic scintillator and its manufacturing method) The main factor that determines the response speed of the indirect type is the decay time constant of the scintillator's luminescence. 8 [cps / mm 2 In order to achieve this, it is particularly important to control the decay time constant of the scintillator's luminescence, and it is preferable that the decay time constant of the luminescence is approximately 17 nsec or less. By setting the decay time constant of the luminescence to 17 nsec or less, pileup can be prevented and practical imaging can be achieved, as described above. Therefore, experiments were conducted with the aim of setting the decay time constant of the scintillator's luminescence to approximately 17 nsec or less. As a result, it was found that the luminescence dose should be 10,000 ph / MeV or more. This is because an luminescence dose of 10,000 ph / MeV or more provides no problems with the S / N ratio or energy resolution, and a detector with higher accuracy can be obtained.
[0033] In other words, it is desirable for the decay time constant to be 17 nsec or less and for the luminescence intensity to be 10,000 ph / MeV or more. To this end, the fluorescent material of the ceramic scintillator 11 used as the light conversion element is made of a garnet compound containing Pr. The fluorescent material of the ceramic scintillator 11 must satisfy the following condition: Condition 1: The absorptance at a wavelength of 320 nm relative to the absorptance at a wavelength of 280 nm is 0.15 or less. Here, the decay time constant is defined as the time it takes for the luminescence intensity generated by irradiation with a short pulse of radiation to decrease to 1 / e (=0.3679) of the maximum luminescence intensity, assuming that the time at which the luminescence intensity reaches its maximum is zero. For example, the decay time constant can be calculated from the recorded change in luminescence intensity by performing time-correlated single photon counting (TCSPC) using a pulsed X-ray tube. Furthermore, the absorptance is the absorptance of the absorption spectrum measured by absorption spectroscopy. The above condition 1 is expressed as a ratio of the absorptance at a wavelength of 320 nm, which is the peak of the emission wavelength, to the absorptance at a wavelength of 280 nm, which has a relatively high absorptance in the absorption spectrum of each fluorescent material.
[0034] The ceramic scintillator 11 is a garnet compound having a composition formula of R 3 M 5 O 12 and it is more preferable that the composition satisfies the following condition 2 or 3. Condition 2: The element R in the composition contains Pr and at least one of Y, La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu, and the element M in the composition contains Al and Ga. Condition 3: The element R in the composition contains Pr, and the element M in the composition contains Al and Ga and at least one of Sc, Si, Ge, and Sn.
[0035] Next, we will explain the results of investigating the characteristics of the light emission amount and the light emission decay time constant of fluorescent materials according to examples that have compositions that satisfy the above-mentioned condition 1, and fluorescent materials according to comparative examples that do not satisfy the above-mentioned condition 1. The fluorescent materials according to the examples and the fluorescent materials according to the comparative examples were produced through the following process.
[0036] First, in the first step, a powder mixture (oxide powder) of an oxide of element R and an oxide of element M is filled into an alumina container and mixed. In the second step, the mixed powder is fired at a temperature of 1300°C or higher. In the third step, the product obtained in the second step is filled into an alumina container and fired at a temperature of 1200°C or higher in a nitrogen / hydrogen mixed atmosphere. In the fourth step, the product obtained in the third step is molded. In the fifth step, the product obtained in the fourth step is sintered to produce a ceramic scintillator.
[0037] Sintering is performed in one step. By performing sintering in one step, unlike when sintering is performed in two or more steps, it is possible to obtain a ceramic scintillator with little deviation in composition and good crystallinity, and also to suppress volatilization of Ga, thereby obtaining a ceramic scintillator with a small decay time constant.
[0038] The fluorescent material is composed of the elements contained in the above composition and contains no other elements except for unavoidable impurities. Because the decay time constant of luminescence varies depending on the elements contained, containing a large amount of impurities can increase the decay time constant. Note that the material may contain impurities in amounts of 100 ppm or more as long as it satisfies the required luminescence intensity and / or the required decay time constant of luminescence. Here, when Si functions as a sintering aid, it remains as an impurity in the grain boundaries of the finished ceramic scintillator. Therefore, if Si remains in the grain boundaries, it can be determined that it has been added as a sintering aid, and if it is present in the base material, it can be determined that it has been added as a raw material. In the ceramic scintillator according to the embodiment, except when present at tens of ppm as an impurity, Sn, Si, Ge, or a compound containing at least one of them is not present in the grain boundaries, and the base material is a garnet compound containing Si, Ge, or Sn.
[0039] (Conditions 1 to 3) The relationship between the absorptance at a wavelength of 320 nm relative to the absorptance at a wavelength of 280 nm (320 nm absorptance / 280 nm absorptance) and the relative luminescence amount relative to the relative decay time constant (relative luminescence amount / relative decay time constant) depending on the types of elements R and M in the composition of the garnet compound will be described with reference to FIGS. 3 to 5. Here, the relative luminescence amount refers to the percentage [%] of the luminescence amount when the luminescence amount in Example 1 is set as the reference (100). Furthermore, the relative decay time constant refers to the percentage of the decay time constant when the decay time constant in Example 1 is set as the reference (100).
[0040] Referring to FIG. 3, FIG. 3 shows Examples 1 to 16 in which the elements R and M in the composition satisfy the above-mentioned condition 2, and Examples 17 to 20 in which the elements M satisfy the above-mentioned condition 3. For example, Example 1 shows a garnet compound containing Lu and Pr as the element R in a mass ratio of 0.998:0.002, and Al and Ga as the element M in a mass ratio of 0.9:0.1. Examples 1 to 20 satisfy condition 1, i.e., the 320 nm absorptance / 280 nm absorptance is 0.15 or less. Generally, there is a trade-off between the luminescence decay time constant and the luminescence output, so whether the characteristics are excellent or not is determined based on the relative luminescence output relative to the relative decay time constant (relative luminescence output / relative decay time constant). In Examples 1 to 20, the relative luminescence output / relative decay time constant is 0.9 or greater. In this case, the decay time constant is approximately 17 nsec or less, and the luminescence output is 10,000 ph / MeV or greater, which falls within the preferable range of characteristics. Comparing Examples 17 to 20, when element M contains a tetravalent element (Examples 18 to 20), the 320 nm absorptance / 280 nm absorptance is smaller and the relative emission amount / relative decay time constant is larger than when element M does not contain a tetravalent element (Example 17). In other words, it is preferable that element M contains a tetravalent element.
[0041] In the condition 3, the element M in the composition may contain one or more of tetravalent elements Si, Ge, and Sn. 3+ and Pr 4+ does not emit light but absorbs visible light. 4+ The presence of Pr is a factor that reduces the light emission amount and decay time constant characteristics of the scintillator. 3+ Since it replaces Pr 3+ However, Pr 4+ Here, when a divalent element is added, Pr tends to become tetravalent in order to maintain the charge balance, and the absorption rate at a wavelength of 320 [nm] increases (as shown in Figure 4). 2+ , Sr 2+ , Mg 2+), the light emission amount and decay time constant characteristics of the scintillator are further deteriorated. On the other hand, when a tetravalent element is added, Pr tends to become trivalent in order to maintain charge balance, and the absorptance at a wavelength of 320 [nm] is reduced (Si 4+ Ge 4+ , Sn 4+ (similar), Pr 4+ By suppressing the residue of Pr 3+ However, the element M in the composition is not limited to a tetravalent element.
[0042] Referring to Figure 5, Figure 5 shows Comparative Examples 1 to 15 in which the elements R and M in the composition do not satisfy either condition 2 or condition 3 (Comparative Examples 1 to 15 do not satisfy condition 2 because the element M contains elements other than Al and Ga). In Comparative Examples 1 to 15, the 320 nm absorptance / 280 nm absorptance is 0.17 or greater. In Comparative Examples 1 to 15, condition 1 is not satisfied either; that is, the relative light emission amount / relative decay time constant is less than 0.90. In this case, it is difficult for the characteristics to fall within the preferred range.
[0043] The ceramic scintillator made of the Pr-containing garnet compound described above can provide a fluorescent material with a short decay time constant of luminescence. Furthermore, by applying this fluorescent material as a ceramic scintillator in a medical X-ray detector, it is possible to meet the required reactivity.
[0044] According to at least one of the embodiments described above, it is possible to provide a ceramic scintillator that can handle a high counting rate, a photon-counting X-ray detector including the same, and a method for manufacturing the ceramic scintillator.
[0045] The ceramic scintillator 11 is not limited to being applied to a photon-counting X-ray detector equipped with a silicon photomultiplier in an X-ray CT device. For example, the ceramic scintillator 11 may be applied to an X-ray detector equipped with a photodiode in an X-ray CT device. The ceramic scintillator 11 may also be applied to a flat panel detector (FPD) equipped with a complementary metal oxide semiconductor (CMOS) in an X-ray diagnostic device. Furthermore, the ceramic scintillator 11 may be applied to a photon-counting detector equipped with a silicon photomultiplier in a PET (Positron Emission Tomography) device. The ceramic scintillator 11 may also be applied to imaging for industrial purposes such as baggage inspection and non-destructive testing.
[0046] Although several embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included within the scope and spirit of the invention, as well as within the scope of the invention described in the claims and their equivalents.
Claims
1. A ceramic scintillator made of a garnet compound containing Pr, wherein the absorptance at a wavelength of 320 nm relative to the absorptance at a wavelength of 280 nm is 0.15 or less.
2. The composition formula of the garnet compound is R 3 M 5 O 12 2. The ceramic scintillator according to claim 1, wherein an element R in the composition of the garnet compound includes Pr and at least one of Y, La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu, and an element M in the composition includes Al and Ga.
3. The composition formula of the garnet compound is R 3 M 5 O 12 2. The ceramic scintillator according to claim 1 , wherein an element R in the composition of the garnet compound includes Pr, and an element M in the composition includes Al, Ga, and at least one of Sc, Si, Ge, and Sn.
4. A photon-counting X-ray detector comprising: the ceramic scintillator according to any one of claims 1 to 3; and a silicon photomultiplier.
5. A method for producing the ceramic scintillator according to any one of claims 1 to 3, comprising the steps of: forming a garnet compound having a composition formula R 3 M 5 O 12 a first step of filling an alumina container with a mixture of oxide powders of elements R and M in the composition and mixing the mixture; a second step of firing the mixed mixture at a temperature of 1300°C or higher; a third step of filling an alumina container with a product obtained in the second step and firing the product in a nitrogen / hydrogen mixed atmosphere at a temperature of 1200°C or higher; a fourth step of molding the product obtained in the third step; and a fifth step of sintering the product obtained in the fourth step to produce the ceramic scintillator.
Citation Information
Patent Citations
Luminescence material, ceramic scintillator and radiation detector, and manufacturing method of luminescence material
JP2018002974A
Transparent ceramic, method of manufacturing the same and device using the transparent ceramic
JP2010235388A
Phosphor material, and scintillator and radiation detector by using the same
JP2011153200A
Garnet type crystal for scintillator and radiation detector using the same
JP2013040274A
Ceramic scintillator, photon counting-type x-ray detector, and ceramic scintillator manufacturing method
WO2022050417A1