Separable container, and separable container production method and production device

The peelable container design addresses separation issues by introducing a vent mechanism through the lid's rotation, ensuring easy layer separation and cost-effective manufacturing with enhanced container quality.

WO2024225433A1PCT designated stage expired Publication Date: 2024-10-31NISSEI ASB MASCH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/016423
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-27
Filing Date
2024-04-26
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing peelable containers face issues with separating the inner and outer layers during recycling, as the inner layer may unintentionally detach from the cap, and there is a need for an easy method to introduce air between the layers for efficient separation.

Method used

A peelable container design featuring a neck with a thread on the inner layer and a protrusion on the outer layer, allowing air to be introduced by rotating the lid, creating a vent and facilitating easy removal of the inner layer from the outer layer along with the lid.

Benefits of technology

The solution enables easy separation of the inner and outer layers while maintaining the contents' integrity, reducing manufacturing costs by eliminating the need for a preformed vent and improving the aesthetic and physical strength of the container through hot parison blow molding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024016423_31102024_PF_FP_ABST
    Figure JP2024016423_31102024_PF_FP_ABST
Patent Text Reader

Abstract

This separable container comprises: a neck part which is formed from an inner layer and has a mouth at one end thereof and the outer periphery of which has been threaded; and a container main body which is connected to the other end of the neck part and includes an outer layer which is made of a material differing from that of the inner layer and stacked on the outer side of the inner layer. The one end of the container main body which adjoins the neck part has a protrusion having a larger diameter than the neck part, and a cap can be screwed onto the neck part of the inner layer. By rotating the cap in the closing direction and thereby shifting the inner layer with respect to the outer layer in one direction or the circumferential direction, an air-passing opening for leading air to between the inner layer and the outer layer is formed in the one end of the container main body.
Need to check novelty before this filing date? Find Prior Art

Description

Peeling container, method and device for manufacturing the peeling container

[0001] The present invention relates to a stripping container, a method for manufacturing a stripping container, and an apparatus for manufacturing the same.

[0002] Resin containers have been used for a variety of purposes, and various resin containers having multiple resin layers have been put to practical use. For example, peelable resin containers are known that have a two-layer structure consisting of an inner layer and an outer layer, in which the inner layer peels off from the outer layer as the contents are discharged. This type of peelable container is also called an airless bottle and is used, for example, as a container for liquid seasonings such as soy sauce, cosmetic lotions, liquid detergents such as shampoo and hand soap, and liquid chemicals used for disinfection and sterilization.

[0003] In this type of peelable container, the inner layer and the outer layer may be formed using different materials. When the inner layer and the outer layer are made of different materials, it becomes necessary to separate the inner layer container from the outer layer container and separate the inner layer container from the outer layer container by material during recycling. As an example, Patent Document 1 discloses a double container in which a flange portion that engages with a cap is formed at the upper end of the mouth of the inner bag, so that the shrunk inner bag and the cap can be separated from the outer shell.

[0004] Japanese Patent Application Laid-Open No. 2022-51111

[0005] In the container of Patent Document 1, the inner bag is secured to the cap by latching the flange at the top end of the mouth into the cap. Therefore, with the container of Patent Document 1, when the inner bag is being pulled out from the outer shell, the inner bag may unintentionally come off the cap due to a force in the pulling direction, which may cause problems when removing the inner bag from the outer shell.

[0006] Furthermore, the peeling container needs to be provided with a vent hole for introducing air between the outer layer and the inner layer in order to peel the inner layer from the outer layer, and there is a demand for a method for easily providing such a vent hole.

[0007] Therefore, the present invention has been made in consideration of such problems, and aims to provide a peelable container in which an air vent for introducing air between the outer layer and the inner layer can be easily provided, and in which the inner layer together with the lid can be easily removed from the outer layer.

[0008] A peelable container according to one embodiment of the present invention comprises a neck formed from an inner layer, having a mouth on one side and threads formed on the outer periphery, and a container body connected to the other side of the neck, with an outer layer formed of a material different from the inner layer and laminated on the outside of the inner layer. A protrusion having a diameter larger than the diameter of the neck is formed on one side of the container body adjacent to the neck, and a lid can be screwed to the neck of the inner layer. By rotating the lid in the closing direction, the inner layer is displaced to one side or in the circumferential direction relative to the outer layer, and an air vent is formed on one side of the container body to introduce air between the inner and outer layers.

[0009] According to one aspect of the present invention, a peelable container can be provided in which a vent for introducing air between the outer layer and the inner layer can be easily provided and the inner layer can be easily removed from the outer layer together with the lid.

[0010] 1A is a longitudinal cross-sectional view showing an example of the configuration of a preform of this embodiment, and FIG. 1B is a cross-sectional view taken along line A-A in FIG. 1A. FIG. 1B is a cross-sectional view showing an example of the configuration of a peeling container of this embodiment. FIG. 1C is an enlarged view showing the vicinity of the neck when a lid is attached to the peeling container. FIG. 1D is an enlarged view showing the vicinity of the neck when the outer layer and inner layer of the peeling container are separated. FIG. 1E is a diagram showing an example of forming a gap between the outer layer and inner layer of the neck. FIG. 1F is a diagram showing a schematic configuration of a blow molding apparatus of this embodiment. FIG. 1G is a diagram showing an example of the configuration of a first injection molding unit. FIG. 1H is a diagram showing a protruding state of a valve pin in the first injection molding unit. FIG. 1I is a diagram showing an example of the configuration of a second injection molding unit. FIG. 1I is a flowchart showing the steps of a method for manufacturing a container. FIG. 1I is a diagram showing the configuration of protrusions and recesses of a preform (peeling container) according to a first modified example. FIG. 1I is a diagram showing a blow molding process in a blow molding unit according to a second modified example. FIG. 1I is a plan view of the bottom mold shown in FIG. 12. FIG. 1I is a cross-sectional view showing an example of the configuration of a peeling container manufactured in the second modified example.

[0011] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, the same elements will be given the same reference numerals in the drawings. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown schematically and do not represent the actual shapes, dimensions, etc.

[0012] <Configuration example of preform and peeling container> First, a configuration example of a preform for a peeling container according to this embodiment and a configuration example of the peeling container will be described. Fig. 1(a) is a longitudinal cross-sectional view showing a configuration example of a preform 10 according to this embodiment, and Fig. 1(b) is a cross-sectional view taken along line A-A in Fig. 1(a).

[0013] The overall shape of the preform 10 is a cylindrical shape with a bottom, one side of which is open at a mouth 13a and the other side is closed. The preform 10 includes a cylindrical body 14, a bottom 15 that closes the other side of the body 14, and a neck 13 that is formed on one side of the body 14 and includes the mouth 13a.

[0014] The preform 10 has a two-layer structure in which an inner layer 12 is laminated on the inside of an outer layer 11. The outer layer 11 and the inner layer 12 are formed from different thermoplastic resin materials by two-stage injection molding, as described below. The outer layer 11 is made of a synthetic resin with excellent moldability and transparency. On the other hand, the inner layer 12 is made of a synthetic resin with properties (e.g., moisture barrier properties, gas barrier properties, heat resistance, chemical resistance) that enable stable storage of the contents of the container and suppress deterioration (oxidation). The resin material for the outer layer 11 is selected to have a higher melting point than the resin material for the inner layer 12. The inner circumferential surfaces of the outer layer 11 and the inner layer 12 are tapered, with the diameter decreasing downward (toward the other side). The outer circumferential surfaces of the outer layer 11 and the inner circumferential surfaces of the inner layer 12 may also be tapered.

[0015] Hereinafter, the resin material of the outer layer 11 will also be referred to as the "first resin material," and the resin material of the inner layer 12 will also be referred to as the "second resin material." The combination of the first resin material and the second resin material can be selected appropriately depending on the specifications of the peeling container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexanedimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), PLA (polylactic acid), and low-density polyethylene (LDPE).

[0016] As an example, the first resin material is PET, and the second resin material is either PP, LDPE (low-density polyethylene), or L-LDPE (linear low-density polyethylene). PP has a melting point of approximately 160-170°C, while LDPE has a melting point of approximately 105-120°C. Furthermore, L-LDPE has a melting point of approximately 114-126°C. On the other hand, PET has a melting point of approximately 245-260°C, which is higher than the melting points of PP, LDPE, and L-LDPE. Furthermore, L-LDPE has higher tensile strength, impact resistance, and puncture resistance than LDPE.

[0017] The inner layer 12 is formed to form a bottomed tubular shape across the neck 13, body 14, and bottom 15 of the preform. The outer layer 11 covers the outer peripheral side of the inner layer 12 across the body 14 and bottom 15 of the preform 10. The inner layer 12 protrudes to one side beyond the end of the body of the outer layer 11, and the neck 13 of the preform 10 is formed at the part of the inner layer 12 protruding from the outer layer 11. A thread 13b is formed on the outer peripheral surface of the neck 13 part of the inner layer 12. Furthermore, a step 13c having a larger diameter than the lower part of the neck 13 and a circular (or ring-shaped) cross section is formed at the lower end of the neck 13.

[0018] Furthermore, one or more longitudinal ribs 16 are formed on the outer periphery of the inner layer 12, extending in the axial direction from near the boundary between the neck portion 13 and the body portion 14 toward the other side and protruding radially outward from the inner layer 12 in a plane perpendicular to the axial direction. The longitudinal rib 16 of this embodiment is an example of a protrusion formed on the outer periphery of the inner layer 12 and extending in the axial direction, and for example, a plurality of longitudinal ribs 16 are formed at intervals in the circumferential direction of the inner layer 12. Fig. 1(b) shows an example in which six longitudinal ribs 16 are formed on the outer periphery of the inner layer 12, but the number of longitudinal ribs 16 may be one or a number other than six.

[0019] The longitudinal ribs 16 engage with recesses 17 formed at corresponding positions on the inner periphery of the outer layer 11, respectively, and function as anti-rotation portions for the inner layer 12 in the circumferential direction relative to the outer layer 11. When torque centered in the axial direction is applied to the neck portion 13 of the inner layer 12, the longitudinal ribs 16 transmit the torque to the outer layer 11 by engaging with the recesses 17 of the outer layer 11, and suppress misalignment of the inner layer 12 in the rotational direction relative to the outer layer 11. The axial length and radial protrusion amount of the longitudinal ribs 16 are appropriately set so that engagement with the recesses 17 is maintained even when a slight gap is formed between the outer layer 11 and the inner layer 12, for example.

[0020] Furthermore, one or more radially extending grooves 18 that communicate with the outer and inner circumferential sides of the outer layer 11 are formed at one end of the outer layer 11 (the portion adjacent to the neck 13). The grooves 18 are an example of a flow path that introduces air from outside the container toward a vent hole (described below). While FIG. 1( b) shows an example in which two grooves 18 are formed circumferentially at 180-degree intervals around the outer layer 11, the number of grooves 18 may be one or more. Furthermore, a protrusion (first opening) 14b that abuts (adjacent) the underside of the step 13c of the neck 13 is formed at one end of the outer layer 11. The protrusion 14b has a circular cross section (or a ring-shaped cross section, excluding the recess 17), and the inner diameter of the protrusion 14b is smaller than that of the step 13c, so that the upper surface of the protrusion 14b abuts against the lower surface of the step 13c. Furthermore, the outer diameter (diameter) of the protrusion 14b is larger than the outer diameter of the neck 13 (specifically, the outer diameter of the threads 13b and the step 13c of the neck 13).

[0021] In the bottom portion 15 of the preform 10, an opening 15a is formed at the center of the bottom of the outer layer 11, penetrating the outer layer 11. The opening 15a of the outer layer 11 is blocked from the inside by the inner layer 12.

[0022] Next, a structural example of a resin stripping container 20 according to this embodiment will be described with reference to Fig. 2 to Fig. 4. Fig. 2 is a cross-sectional view showing a structural example of the stripping container 20 according to this embodiment. Fig. 3 is an enlarged view showing the vicinity of the neck when the lid 30 is attached to the stripping container 20. Fig. 4 is an enlarged view showing the vicinity of the neck when the outer layer 11 and the inner layer 12 of the stripping container 20 are separated.

[0023] 2, the peel-off container 20 is a bottle-shaped resin container obtained by stretch-blow molding the preform 10, and contains, for example, a seasoning liquid such as soy sauce. Note that the peel-off container 20 may also be used to contain other contents, such as cosmetic lotion.

[0024] Similar to the preform 10, the peeling container 20 has a two-layer structure in which an inner layer 12 is laminated inside an outer layer 11. The peeling container 20 has a neck 13, a cylindrical body 24, a shoulder 24a connecting the neck 13 and one side of the body 24, and a bottom 25 closing the other side of the body 24. In the peeling container 20, the contents are filled into the space inside the inner layer 12. The shoulder 24a, body 24, and bottom 25 are examples of a container body.

[0025] In manufacturing the peeling container 20, the body 14 and bottom 15 of the preform 10 are expanded by stretch blowing, thereby forming the shoulder 24a, body 24, and bottom 25 of the peeling container 20. Note that an opening 25a (non-laminated portion, single-layer portion) penetrating the outer layer 11 is formed at the center of the bottom 25 of the peeling container 20, similar to the preform 10. The opening 25a is filled with the material of the inner layer 12, closing the opening 25a, and the inner layer 12 is exposed outside the outer layer 11 near the opening 25a of the bottom 25 of the peeling container 20.

[0026] On the other hand, the neck 13 of the preform 10 and the upper end portion of the outer layer 11 are held by a neck mold 47b (described later) during blow molding, so that the shape of the preform 10 is maintained as is. Therefore, as shown in Fig. 2, the neck 13 of the peeling container 20 and the upper end portion of the outer layer 11 have the same configuration as the neck 13 of the preform 10 described above. That is, the neck 13 of the peeling container 20 has a step 13c, and the upper end portion of the outer layer 11 (the portion adjacent to the neck 13) has a protrusion 14b. Note that, at the upper end portion of the outer layer 11, a groove 18 and a recess 17 are formed in the outer layer 11, and a vertical rib 16 is formed in the inner layer 12 in that portion.

[0027] 3(a) and 3(b), a lid 30 that seals the inner layer 12 is attached airtight to the neck 13 of the peeling container 20. The lid 30 has a nozzle head 31 equipped with a check valve (not shown) that dispenses a predetermined amount of the contents of the container in response to, for example, an operation of pressing down the top, and a cylindrical cap portion 32 that covers the outside of the neck portion 13. An internal thread 33 that screws into the thread 13b of the neck portion 13 is formed on the inner periphery of the cap portion 32.

[0028] When filling the contents into the peeling container 20 and attaching the lid 30, the cap portion 32 of the lid 30 is placed over the neck portion 13, as shown in Fig. 3(a). Then, as shown in Fig. 3(b), the lid 30 is rotated relative to the neck portion 13, and the internal threads 33 are screwed onto the threads 13b of the neck portion 13, thereby fixing the lid 30 to the neck portion 13 of the peeling container 20. At this time, the cap portion 32 seals the opening portion 13a from the outside air by abutting the upper end of the neck portion 13 with the cap portion 32. Note that an annular sealant (not shown) may be disposed between the cap portion 32 and the neck portion 13, and the opening portion 13a may be sealed by sandwiching the sealant between the cap portion 32 and the neck portion 13.

[0029] After blow molding, the outer layer 11 and the inner layer 12 are in close contact with each other in the peelable container 20. If the lid 30 is further rotated in the closing direction while the threads 13b of the neck 13 and the inner threads 33 are fully engaged (the lid 30 is fixed to the neck 13), a torque in the closing direction acts on the lid 30 and the peelable container 20, and a reaction force against the torque is generated in the outer layer 11, which is held to close the lid 30.

[0030] At this time, the engagement of the recesses 17 and the longitudinal ribs 16 creates resistance to circumferential displacement of the inner layer 12 relative to the outer layer 11, and no circumferential displacement occurs between the outer layer 11 and the inner layer 12. On the other hand, the force applied in the axial direction by the engagement of the threads 13b of the neck 13 with the inner threads 33 guides the longitudinal ribs 16 of the inner layer 12 in the extension direction of the recesses 17, and the inner layer 12 (or the neck 13) is displaced so as to rise to one side.

[0031] Specifically, in a first configuration example, the lower end of the cap portion 32 of the lid body 30 may be brought into contact with the end of the outer layer, and the inner layer 12 (or the neck portion 13) may be displaced so as to be raised relative to the outer layer 11 (specifically, the end (protruding portion 14b) of the outer layer 11) starting from this contact point. This causes the inner layer 12 to shift axially relative to the outer layer 11, opening up between the outer layer 11 and the inner layer 12 at the top end of the container (i.e., the upper surface of the protruding portion 14 of the outer layer 11 separates from the lower surface of the step 13c of the inner layer 12 (or the neck portion 13)), creating a vent through which air can enter between the outer layer 11 and the inner layer 12. Air can enter between the outer layer 11 and the inner layer 12 through this vent, allowing the outer layer 11 and the inner layer 12 of the peeling container 20 to be peeled off.

[0032] At the upper end of the outer layer 11, even if the inner layer 12 peels off from the outer layer 11, it is positioned by the engagement between the recesses 17 and the vertical ribs 16, thereby suppressing rattle of the neck 13. Furthermore, when the lid 30 is displaced so as to lift the neck 13, the portion of the inner layer 12 where the vertical ribs 16 are formed may be stretched and slightly reduced in diameter. This may cause the outer layer 11 and the inner layer 12 to peel off at the lower portion of the neck 13, maintaining the engagement between the vertical ribs 16 and the recesses 17, and forming a gap between the outer peripheral surface of the step 13c and the inner peripheral surface of the protrusion 14b, thereby forming a vent through which air can enter.

[0033] Furthermore, in the example of this embodiment, when the lid 30 is closed, a gap, as an example of a flow path, is formed between the cap portion 32 of the lid 30 and the upper end of the outer layer 11. This allows air from outside to directly flow into the vent between the inner layer 12 and the outer layer 11. As described above, the peeling container 20 may be configured so that the cap portion 32 of the lid 30 and the upper end of the outer layer 11 come into contact with each other when the lid 30 is closed.

[0034] In a second configuration example, a vent may be formed between the outer layer 11 and the inner layer 12 of the neck portion 13 by contact between the vertical rib 16 and the recess 17 in the rotational direction when the lid 30 is closed. In the second configuration example, it is not necessary for the lower end of the cap portion 32 of the lid 30 to abut against the end (protrusion 14b) of the outer layer 11.

[0035] The inner layer 12 (e.g., LDPE, L-LDPE, or PP) is made of a material that is softer than the outer layer 11 (e.g., PET) and has the property of easily returning to its original shape after bending (easily deforming elastically). The lid 30 is turned in a first direction D1 (see FIG. 5 ) along the threads 13b of the neck 13 (inner layer 12) and engages with the neck 13. When the lid 30 is closed, the upper end of the neck 13 abuts airtightly against the inner surface of the lid 30, and the threads 13b engage with the internal threads of the lid, preventing the lid 30 from turning in the first direction D1 relative to the neck 13.

[0036] After the lid 30 is closed, if a small amount of torque is applied to the lid 30 in the first direction D1, the neck 13 elastically deforms slightly relative to the outer layer 11. This causes initial separation between the inner and outer layers at the counter-rotation side (the side opposite to the first direction D1) between the longitudinal rib 16, which functions as a rotation stopper, and the recess 17 (initial separation process). When the torque in the first direction D1 is released, the neck 13 returns to its original position, but the gap 19 between the inner and outer layers formed at the counter-rotation side between the longitudinal rib 16 and the recess 17 is maintained, as shown in FIG. 5 . This allows a vent (gap 19) to be formed between the outer layer 11 and the inner layer 12 on the neck 13 side.

[0037] Furthermore, when torque is applied in the first direction D1, the underside of the step 13c of the neck 13, which is part of the inner layer 11, separates from the protrusion (first opening) 14b, which is part of the outer layer 12, causing initial delamination (initial delamination process). When the torque in the first direction D1 is released, the neck 13 returns to its original position, but the gap between the inner and outer layers formed between the underside of the step 13c and the upper surface of the protrusion (first opening) 14b is maintained. As a result, a gap is formed between the underside of the step 13c and the upper surface of the protrusion (first opening) 14b on the neck 13 side. The gap between the step 13c and the protrusion 14b communicates with the gap 19 between the vertical rib 16 and the recess 17.

[0038] In addition, in the peeling container 20, a groove 18 is formed in part of the circumferential direction at the upper end of the outer layer 11. Even if the cap portion 32 and the outer layer 11 abut, the inside and outside of the cap portion 32 communicate via the space in the groove 18, allowing air to be guided to the upper end side of the peeling container 20. If a gap is secured between the cap portion 32 of the lid body 30 and the upper end of the outer layer 11, the formation of the groove 18 at the upper end of the outer layer 11 may be omitted. Note that, because the mouth portion 13a is sealed by the abutment of the upper end of the neck portion 13 and the cap portion 32, the contents filled in the inner layer 12 do not come into contact with air.

[0039] In the peeling container 20, when the lid 30 is opened and the contents are discharged from the inner layer 12, air introduced into the cap portion 32 through the groove 18 flows into the gap between the outer layer 11 and the inner layer 12 from the upper end side of the container, gradually causing the outer layer 11 and the inner layer 12 to peel off. This allows the volume occupied by the contents in the container to be replaced with air without exposing the contents of the inner layer 12 to air, and allows the contents filled in the inner layer 12 to be discharged outside the container.

[0040] Furthermore, when discarding a used peeling container 20, the inner layer 12 must be removed from the outer layer 11 and separated, since the outer layer 11 and inner layer 12 are made of different materials. As shown in Figure 4(a) , when the peeling container 20 has been used, the contents of the inner layer 12 have been discharged, and the inner layer 12 has been peeled off from the outer layer 11 and shrunk. Meanwhile, the cap portion 32 of the lid 30 is fixed to the neck portion 13 formed on the inner layer 12 by screwing.

[0041] When the lid 30 is pulled in one direction in the state shown in FIG. 4( a), the contracted inner layer 12 can be pulled out of the outer layer 11, as shown in FIG. 4( b), and the inner layer 12 can be removed from the outer layer 11. When the inner layer 12 is pulled out, a force pulling the lid 30 in one direction and a reaction force from the inner layer 12 in the other direction act. When a pulling force is applied to the neck 13 and the lid 30 in one direction, the helically interlocking threads 13b of the neck 13 and the inner threads 33 of the cap portion 32 abut axially, creating high resistance to axial shear. In other words, the neck 13 and the lid 30 are less likely to separate when pulled in one direction, and the pulling force is transmitted to the inner layer 12 without separating the neck 13 and the lid 30. This allows the inner layer 12 to be pulled out of the outer layer 11 together with the lid 30.

[0042] 6 is a diagram schematically illustrating the configuration of a blow molding apparatus 40 according to this embodiment. The blow molding apparatus 40 according to this embodiment is an example of an apparatus for manufacturing the peelable container 20, and employs a hot parison method (also referred to as a one-stage method) in which the peelable container 20 is blow-molded by utilizing the heat (internal heat) retained during injection molding without cooling the preform 10 to room temperature.

[0043] The blow molding apparatus 40 includes a first injection molding unit 41, a first temperature adjustment unit 42, a second injection molding unit 43, a second temperature adjustment unit 44, a blow molding unit 45, a take-out unit 46, and a conveying mechanism 47. The first injection molding unit 41, the first temperature adjustment unit 42, the second injection molding unit 43, the second temperature adjustment unit 44, the blow molding unit 45, and the take-out unit 46 are arranged at positions rotated by the same predetermined angle (e.g., 60 degrees) around the conveying mechanism 47. The blow molding apparatus 40 may be configured without the first temperature adjustment unit 42. In this case, each molding station is arranged at a position rotated by 72 degrees around the conveying mechanism 47. The first injection molding unit 41 and the second injection molding unit 43 are provided with a core mold lifting mechanism (not shown) above the conveying mechanism 47.

[0044] (Transport mechanism 47) The transport mechanism 47 includes a transport plate 47a that rotates around an axis perpendicular to the plane of the paper in Fig. 6. On the transport plate 47a, one or more neck dies 47b (not shown in Fig. 6) that hold the neck portion 13 of the preform 10 (or the peeling container 20) are arranged at predetermined angles.

[0045] In the first injection molding section 41, the neck mold 47b defines the shape of the upper end of the outer layer 11, including the grooves 18. In the second injection molding section 43, the neck mold 47b defines the outer peripheral shape of the neck portion 13 of the inner layer 12.

[0046] The conveying mechanism 47 moves the position of the transfer plate 47a in the rotational direction, thereby conveying the preform 10 (or the peeling container 20) held by the neck mold 47b through the first injection molding section 41, the first temperature adjustment section 42, the second injection molding section 43, the second temperature adjustment section 44, the blow molding section 45, and the removal section 46, in that order. The conveying mechanism 47 can also raise and lower the transfer plate 47a, and also performs operations related to mold closing and mold opening (mold release) in the first injection molding section 41 and the second injection molding section 43.

[0047] (First injection molding unit 41) The first injection molding unit 41 includes a cavity mold 50 and a core mold 51, and cooperates with a neck mold 47b that is transported during molding to manufacture the outer layer 11 of the preform 10. A first injection device 48 that supplies a first resin material via a hot runner mold (not shown) is connected to the first injection molding unit 41. The cavity mold 50 is fixed to the machine base of the blow molding device 40, and the core mold 51 is fixed to a core mold lifting mechanism.

[0048] 7 and 8 are views showing the first injection molding section 41 that molds the outer layer 11 of the preform 10. The cavity mold 50 is a mold that defines the outer peripheral shape of the outer layer 11. A resin supply section 52 that injects a first resin material that has been plasticized (melted) by a first injection device 48 into the cavity mold 50 is connected to the bottom of the cavity mold 50.

[0049] The core mold 51 is a mold that defines the shape of the inner periphery of the outer layer 11, and is inserted from above into the inner periphery of the cavity mold 50. In the core mold 51, in a region that corresponds to the upper end of the outer layer 11, a protrusion 51a that corresponds to the recess 17 of the outer layer 11 is formed along the axial direction.

[0050] The resin supply unit 52 is also provided with a valve pin 53 that is movable in the axial direction to a position close to the core mold 51. The valve pin 53 is a rod-shaped member that opens and closes the resin supply unit 52, and is housed inside so as not to protrude from the resin supply unit 52 until the first resin material is filled into the mold space. After the mold space is filled with the first resin material, the valve pin 53 protrudes to a position close to the core mold 51, as shown in Figure 8. This movement of the valve pin 53 during injection molding allows a thin film portion 11a, in which the thickness of the resin material is thinner than that of the peripheral portion, to be formed in the center of the bottom of the outer layer 11.

[0051] 7 and 8, in the first injection molding section 41, the cavity mold 50, the core mold 51, and the neck mold 47b of the transport mechanism 47 are closed to form a mold space for the outer layer 11. Then, the outer layer 11 of the preform 10 is produced in the first injection molding section 41 by injecting a first resin material from the bottom of the mold space via a resin supply section 52.

[0052] Furthermore, even when the first injection molding section 41 is opened, the neck mold 47b of the transport mechanism 47 does not open, but continues to hold and transport the outer layer 11 of the preform 10. The number of preforms 10 simultaneously molded in the first injection molding section 41 (i.e., the number of peeling containers 20 that can be simultaneously molded in the blow molding device 40) can be set as appropriate.

[0053] (First Temperature Adjustment Unit 42) The first temperature adjustment unit 42 includes a temperature adjustment mold (not shown) (a heating pot or temperature adjustment pot that adjusts the temperature of the outer layer 11 from the outside, and a heating rod or temperature adjustment rod (or air introduction rod) that adjusts the temperature of the outer layer 11 from the inside). The first temperature adjustment unit 42 cools (or heats) the outer layer 11, which is in a high-temperature state after injection molding, by placing it in a temperature adjustment mold that is maintained at a predetermined temperature. The first temperature adjustment unit 42 also has the function of adjusting the temperature distribution of the outer layer 11 to a predetermined state before it is transported to the second injection molding unit 43.

[0054] (Second injection molding unit 43) The second injection molding unit 43 includes a cavity mold 60 and a core mold 61, and cooperates with a neck mold 47b that is transported during molding to injection mold the inner layer 12 on the inner circumferential side of the outer layer 11. A second injection device 49 that supplies a second resin material via a hot runner mold (not shown) is connected to the second injection molding unit 43. The cavity mold 60 is fixed to the machine base of the blow molding device 40, and the core mold 61 is fixed to a core mold lifting mechanism.

[0055] 9 is a diagram showing the second injection molding section 43 that molds the inner layer 12 of the preform 10. The cavity mold 60 is a mold that houses the outer layer 11. A resin supply section 62 that injects a second resin material that has been plasticized (melted) by a second injection device 49 into the cavity mold 60 is connected to the bottom of the cavity mold 60. The core mold 61 is a mold that defines the inner peripheral shape of the inner layer 12 and is inserted into the inner periphery of the cavity mold 60 from above.

[0056] As shown in Fig. 9, the second injection molding section 43 accommodates the outer layer 11 of the preform 10 injection-molded in the first injection molding section 41. When the second injection molding section 43 is closed, a mold space is formed between the inner periphery of the outer layer 11 and the surfaces of the neck mold 47b and the core mold 61. Then, by injecting a second resin material from the bottom of the mold space via a resin supply section 62, the inner layer 12 is laminated on the inner periphery side of the outer layer 11 in the second injection molding section 43, and the preform 10 shown in Fig. 1 is produced.

[0057] (Second temperature adjustment unit 44) The second temperature adjustment unit 44 is equipped with a temperature adjustment mold (a heating pot or temperature adjustment pot that adjusts the temperature of the preform 10 from the outside, and a heating rod or temperature adjustment rod (or air introduction rod) that adjusts the temperature of the preform 10 from the inside) not shown. The second temperature adjustment unit 44 accommodates the preform 10 transported from the second injection molding unit 43 in a mold unit maintained at a predetermined temperature, thereby achieving uniform temperature and eliminating temperature deviation, and adjusting the temperature of the preform 10 to a temperature suitable for the final blow (for example, approximately 90°C to 105°C). The second temperature adjustment unit 44 also has the function of cooling the preform 10 in a high-temperature state after injection molding.

[0058] (Blow molding section 45) The blow molding section 45 performs blow molding on the preform 10 whose temperature has been adjusted in the second temperature adjustment section 44, to manufacture the peeling container 20. The blow molding section 45 includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the peeling container 20, a bottom mold, a stretching rod, and an air introduction member (none of which are shown). The blow molding section 45 blow molds the preform 10 while stretching it. As a result, the preform 10 is shaped into the shape of the blow cavity mold, and the peeling container 20 can be manufactured.

[0059] (Removal Unit 46 ) The removal unit 46 is configured to release the peeled container 20 manufactured in the blow molding unit 45 from the neck mold 47 b and remove the peeled container 20 to the outside of the blow molding device 40 .

[0060] <Explanation of Container Manufacturing Method> Next, a method for manufacturing the peeled container 20 using the blow molding device 40 of this embodiment will be described. Fig. 10 is a flowchart showing steps in the method for manufacturing the peeled container 20.

[0061] 8, in the first injection molding section 41, a first resin material is injected from a first injection device 48 into a mold space formed by a cavity mold 50, a core mold 51, and a neck mold 47b, to produce the outer layer 11 of the preform 10. At this time, a groove 18 is formed in the upper end of the outer layer 11 by the neck mold 47b. In addition, a recess 17 is formed in the inner circumferential surface near the upper end of the outer layer 11 by a protrusion 51a formed on the core mold 51.

[0062] 8, after the outer layer 11 of the preform 10 is molded, a step is carried out in the first injection molding section 41 to project the valve pin 53 to a position close to the core mold 51. As a result, a thin film portion 11a having a thickness thinner than that of the peripheral portion is formed in the center of the bottom of the outer layer 11.

[0063] Thereafter, the mold of the first injection molding section 41 is opened, and the outer layer 11 is released. When the mold of the first injection molding section 41 is opened, the transfer plate 47a of the conveying mechanism 47 moves a predetermined angle in the rotational direction. As a result, the outer layer 11 of the preform 10 held in the neck mold 47b is conveyed to the first temperature adjustment section 42 in a state that includes the heat retained during injection molding.

[0064] (Step S102: First Temperature Adjustment Step) Next, in the first temperature adjustment section 42, the outer layer 11 of the preform 10 is placed in a temperature adjustment mold, and cooling and adjustment of the temperature distribution (temperature uniformization and temperature deviation elimination) of the outer layer 11 are performed. Note that the first temperature adjustment step may be omitted.

[0065] After the first temperature adjustment step (or the first injection molding step), the transfer plate 47 a of the conveying mechanism 47 moves a predetermined angle in the rotational direction, whereby the temperature-adjusted outer layer 11 held in the neck mold 47 b is conveyed to the second injection molding section 43.

[0066] (Step S103: Second Injection Molding Step) Subsequently, the outer layer 11 of the preform 10 is accommodated in the second injection molding section 43, and the inner layer 12 is injection molded.

[0067] 9, in the second injection molding section 43, a mold space is formed between the inner periphery of the outer layer 11, the neck mold 47b, and the surface of the core mold 61 facing these, and a second resin material is injected into the mold space from a second injection device 49. A thin film portion 11a is formed at the bottom of the outer layer 11, but the injection pressure of the second resin material breaks the thin film portion 11a, forming an opening 15a at the bottom, and the second resin material is guided to the inner periphery of the outer layer 11 from the opening 15a.

[0068] In the second injection molding section 43, the neck portion 13 of the inner layer 12 is formed by the neck mold 47b and the core mold 61, and the body portion 14 and the bottom portion 15 of the inner layer 12 are formed by the inner periphery of the outer layer 11 and the core mold 61. In addition, a recess 17 formed in the inner periphery of the outer layer 11 is filled with a second resin material, thereby forming a vertical rib 16 on the outer periphery of the inner layer 12.

[0069] The temperature of the second resin material filled in the second injection molding section 43 is set to a temperature lower than the melting point of the first resin material. Furthermore, the surface temperature of the outer layer 11 when the second resin material is filled in the second injection molding section 43 is cooled to a temperature equal to or lower than the melting point of the second resin material.

[0070] In the second injection molding section 43, the cavity mold 60 faces the outer peripheral side of the outer layer 11, and the shape of the outer layer 11 is maintained from the outer peripheral side by the cavity mold 60. Therefore, in the second injection molding section 43, even if the second resin material comes into contact with the outer layer 11, thermal deformation of the outer layer 11 can be suppressed.

[0071] As described above, the inner layer 12 is laminated on the inner peripheral side of the outer layer 11 by the first injection molding step and the second injection molding step, and the preform 10 shown in FIG. 1 is manufactured.

[0072] Thereafter, the mold of the second injection molding section 43 is opened, and the preform 10 is released. When the mold of the second injection molding section 43 is opened, the transfer plate 47a of the transport mechanism 47 moves a predetermined angle in the rotational direction. As a result, the preform 10 held in the neck mold 47b is transported to the second temperature adjustment section 44 in a state in which it contains the heat retained during injection molding.

[0073] (Step S104: Second temperature adjustment step) Subsequently, in the second temperature adjustment section 44, the preform 10 is housed in a temperature adjustment mold unit, and temperature adjustment is performed to bring the temperature of the preform 10 close to a temperature suitable for final blowing. Thereafter, the transfer plate 47a of the conveying mechanism 47 moves a predetermined angle in the rotational direction. As a result, the temperature-adjusted preform 10 held in the neck mold 47b is conveyed to the blow molding section 45.

[0074] (Step S105: Blow Molding Process) Subsequently, in the blow molding section 45, blow molding of the peeling container 20 is performed. First, the blow cavity mold is closed to accommodate the preform 10 in the mold space, and an air introduction member (blow core) is lowered so that the air introduction member abuts against the neck portion 13 of the preform 10. Then, a stretching rod is lowered to press the bottom portion 15 of the preform 10 from the inner surface, and while vertical axis stretching is performed as necessary, blow air is supplied from the air introduction member, thereby horizontal axis stretching the preform 10. As a result, the preform 10 is bulged and shaped so as to fit closely into the mold space of the blow cavity mold, and is blow molded into the peeling container 20.

[0075] (Step S106: Container Removal Process) When blow molding is completed, the blow cavity mold is opened. This allows the peeled container 20 to be moved from the blow molding section 45. Next, the transfer plate 47a of the conveying mechanism 47 moves a predetermined angle in the rotational direction, and the peeled container 20 is transported to the removal section 46. In the removal section 46, the peeled container 20 is released from the neck mold 47b, and the peeled container 20 is removed to the outside of the blow molding apparatus 40. The manufactured peeled container 20 is sequentially filled with the contents and the lid 30 is attached in a post-processing process not shown.

[0076] This completes one cycle of the manufacturing method for peeled containers. After that, the transfer plate 47a of the conveying mechanism 47 moves a predetermined angle in the rotational direction, and the above steps S101 to S106 are repeated. Note that, when the blow molding device 40 is in operation, six sets of peeled containers 20 are manufactured in parallel, with one step time difference between each step.

[0077] Furthermore, due to the structure of the blow molding device 40, the waiting times for the first injection molding process, the first temperature adjustment process, the second injection molding process, the second temperature adjustment process, the blow molding process, and the container removal process are all the same length. Similarly, the transport times between each process are also the same length.

[0078] The effects of this embodiment will be described below. The peeling container 20 of this embodiment includes a neck 13, a container body (body 14 and bottom 15), and a lid 30. The neck 13 is formed by an inner layer 12, has a mouth 13a on one side, and has threads 13b formed on the outer periphery. The container body is connected to the other side of the neck 13, and an outer layer 11 made of a different material from the inner layer 12 is laminated on the outside of the inner layer 12. The lid 30 is attached to the neck 13 and seals the mouth 13a against air when the container is closed. The lid 30 is screwed onto the neck 13 of the inner layer 12, and the lid 30 and neck 13 generate high resistance to axial shear. Therefore, when separating the inner layer 12 and outer layer 11 of a used peeling container 20, the neck 13 and lid 30 are difficult to separate by pulling force, making it easy to remove the inner layer 12 together with the lid 30 from the outer layer 11. Furthermore, in this embodiment, by rotating the lid 30 in the closing direction to displace the inner layer 12 to one side relative to the outer layer 11, a vent hole for directing air between the inner layer 12 and the outer layer 11 is formed on one side of the container body. Therefore, a vent hole for directing air between the outer layer 11 and the inner layer 12 can be easily provided. Note that, in the configuration of this embodiment, the vent hole can be easily formed when attaching the lid 30, eliminating the need to provide a vent hole in the preform 10 during injection molding. Therefore, there is no need to add a movable mold for forming the vent hole to the injection molding die, thereby reducing the manufacturing cost of the peeling container 20.

[0079] Furthermore, in this embodiment, the outer layer 11 of the preform 10 is molded in a first injection molding process, and the inner layer 12 is injection molded inside the outer layer 11 through the opening 15a of the outer layer 11 in a second injection molding process to produce a two-layer preform 10. The two-layer preform 10 is then stretch-blow molded while retaining the heat from the injection molding process to produce a peelable container 20. Therefore, in this embodiment, a hot parison blow molding method can be used to produce a peelable container 20 with excellent aesthetic appearance and physical strength. Compared to cold parison blow molding, this embodiment does not require cooling the produced preform 10 to near room temperature, and a process of reheating the preform 10 is also unnecessary. Therefore, according to this embodiment, the series of processes from injection molding of the preform 10 to blow molding of the peelable container 20 can be completed in a relatively short time, allowing for mass production of peelable containers 20 in a shorter production cycle.

[0080] 11 shows another example of the configuration of the protrusions and recesses of the preform 10A (peeling container 20) as a first modification of the above embodiment. In the following description of each modification, elements common to the above embodiment are denoted by the same reference numerals, and redundant description will be omitted as appropriate.

[0081] The first modified example is a configuration example in which the protrusions 16a formed on the inner layer 12 of the preform 10A are formed in a ratchet tooth shape. One or more protrusions 16a are formed circumferentially on the outer periphery of the inner layer 12, and preferably a plurality of protrusions 16a are formed at predetermined intervals (e.g., equal intervals). Fig. 11 shows an example in which three protrusions 16a are formed circumferentially on the inner layer 12, but the number of protrusions 16a is not limited to this. Like the longitudinal ribs 16 of the above embodiment, each protrusion 16a extends in the axial direction from near the boundary between the neck portion 13 and the body portion 14 to the other side and protrudes radially outward from the inner layer 12 in a plane perpendicular to the axial direction.

[0082] In addition, the shape of each protrusion 16a increases the radial protrusion amount along the first direction D1 (the closing direction of the lid body 30) in which the lid body 30 is screwed to the neck portion 13, and a ratchet tooth stop surface 16b is formed on the side opposite the first direction D1 in the second direction D2 (the opening direction of the lid body 30).

[0083] On the other hand, in the first modified example, a plurality of recesses 17a corresponding to the shapes of the protrusions 16a are formed at equal intervals in the circumferential direction on the inner periphery of the outer layer 11 of the preform 10A. While Fig. 11 shows an example in which three recesses 17a are formed in the circumferential direction of the outer layer 11, the number of recesses 17a is not limited to the above. The axial length of each recess 17a corresponds to the axial length of the protrusions 16a.

[0084] The shape of each recess 17a is a ratchet tooth shape that matches the protrusion 16a in a plane perpendicular to the axial direction. That is, the shape of the recess 17a is such that the thickness of the outer layer 11 decreases along the first direction D1, and a ratchet tooth stop surface 17b is formed on the second direction D2 side opposite to the first direction D1.

[0085] Even in the peeling container 20 blow-molded from the preform 10A of the first modified example, the neck 13 of the preform 10A and the upper end portion of the outer layer 11 are held by the neck mold 47b during blow molding, so that the shape of the preform 10A is maintained as is. Therefore, the neck 13 and the upper end portion of the outer layer 11 of the peeling container 20 have the same configuration as the neck 13 of the preform 10A described above. In other words, at the upper end portion of the outer layer 11 of the peeling container 20, ratchet-tooth-shaped recesses 17a are formed in the outer layer 11, and ratchet-tooth-shaped protrusions 16a are formed in the inner layer 12 in that portion.

[0086] When attaching the lid body 30 to the peeling container 20 of the first modification, the cap portion 32 of the lid body 30 is placed on the neck portion 13, and the lid body 30 is rotated in the first direction D1 relative to the neck portion 13. This causes the threads 13b of the neck portion 13 to engage with the internal threads 33 of the lid body 30, and the lid body 30 is fixed to the neck portion 13 of the peeling container 20.

[0087] When the lid 30 is screwed onto the threads 13b of the neck 13, the outer layer 11 of the peeling container 20 is held stationary by an operator, while torque in the first direction D1 is applied to the inner layer 12 provided with the neck 13 when the lid 30 is attached. Then, the pawl surfaces 16b of the protrusions 16a of the inner layer 12 facing in the first direction D1 abut against the pawl surfaces 17b of the recesses 17a of the stationary outer layer 11, and the protrusions 16a are caught in and locked with the recesses 17a. Thus, when the lid 30 is screwed onto the threads 13b of the neck 13, the inner layer 12 is prevented from rotating relative to the outer layer 11, and no relative rotation occurs between the outer layer 11 and the inner layer 12.

[0088] On the other hand, when removing the lid 30 from the peeling container 20 of the first modified example, the lid 30 is rotated in the second direction D2 relative to the neck 13. At this time, the outer layer 11 of the peeling container 20 is held stationary by an operator, while a torque in the second direction D2 is applied to the inner layer 12 on which the neck 13 is provided. In this case, the protrusion 16a of the inner layer 12 can move in the second direction D2 without being obstructed by the latching surface 17b of the recess 17a of the outer layer 11. Furthermore, the protrusion 16a moving in the second direction D2 is guided by the inclined surface of the recess 17a and can move freely over the step of the latching surface 17b of the outer layer 11. As a result, when removing the lid 30 from the neck 13, the inner layer 12 can be easily rotated in the second direction relative to the outer layer 11.

[0089] The inner layer 12 may be supported by the outer layer 11 at the opening 25a of the bottom 25. In this case, when torque is applied to the inner layer 12 in the second direction D2 from the neck 13 side, the contracted inner layer 12 is deformed by being twisted around the bottom 25 side as a fulcrum, resulting in a narrowed, easily removable shape. The operator can then remove the inner layer 12 from the outer layer 11 by pulling the lid 30 to one side and pulling the contracted inner layer 12 out of the outer layer 11.

[0090] As described above, according to the first modified example, relative rotation between the outer layer 11 and the inner layer 12 is prevented when the lid 30 is attached to the peeling container 20, while the inner layer 12 can be rotated relative to the outer layer 11 when the lid 30 is removed from the peeling container 20. Therefore, the first modified example further improves the workability when removing and separating the inner layer 12 from the outer layer 11 after use of the peeling container 20.

[0091] The manufacturing method and manufacturing device for the peeled container 20 using the preform 10A of the first modified example differ from those for manufacturing the peeled container 20 using the preform 10 only in the external shape of the core mold (not shown) of the first injection molding part 41. In the core mold (not shown), in a region corresponding to the upper end of the outer layer 11, protrusions corresponding to the recesses 17a of the outer layer 11 (or corresponding to the ratchet tooth-like protrusions 16a of the inner layer 12) are formed along the axial direction.

[0092] (Second Modification) Fig. 12 shows an example of the blow molding step (S105) in the blow molding unit 45 as a second modification of the above embodiment. Fig. 13 is a plan view of the bottom mold 200 shown in Fig. 12. Fig. 14 is a cross-sectional view showing an example of the configuration of a peeling container 20A manufactured in the second modification.

[0093] 12, the blow molding section 45 according to the second modification includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the peeling container 20, a bottom mold 200, a stretch rod 300 extending vertically in the drawing, and an air introduction member (not shown, a member that abuts against the neck portion 13 of the preform 10, 10A to supply and exhaust air). Here, the stretch rod 300 has a lower end portion (tip piece portion) 301 with a larger diameter than the middle portion (hollow rod portion) in order to increase the contact area with the bottom portion 15 of the preform 10 at the lower end side. Note that the blow cavity mold in the blow molding section 45 is omitted from the drawings in FIG. 12.

[0094] The bottom mold 200 has a protrusion 220 extending upward in Fig. 12 at a position corresponding to the opening 15a in the outer layer 11. Figures 13(a) to 13(c) show examples of the shape of the protrusion 220 of the bottom mold 200. As shown in each drawing in Fig. 13, the width of the protrusion 220 (the dimension in the left-right direction in Fig. 12) is formed to be smaller than the width dimension of the opening 15a in the outer layer 11 (the opening 15a is indicated by a dashed line in Fig. 13). Therefore, the protrusion 220 can penetrate the outer layer 11 and be inserted into the opening 15a of the bottom 15, where the inner layer 12 is exposed to the outside.

[0095] The shape of the protrusion 220 may be a circle having a smaller diameter than the opening 15a as shown in Fig. 13(a), a non-circular shape having one or more radially protruding ribs as shown in Fig. 13(b), or a polygonal shape (e.g., a triangular shape) having radially protruding corners as shown in Fig. 13(c). Note that the shape of the protrusion 220 of the bottom mold 200 is not limited to the above. For example, the number of protruding ribs in the protrusion 220 of Fig. 13(b) may be changed arbitrarily, and the protrusion 220 of Fig. 13(c) may be changed to another polygonal shape such as a square or pentagon, or a star shape.

[0096] Figure 12(a) shows the state after the preform 10 (or preform 10A) has been placed in the blow molding section 45, but before the lower end 301 of the stretch rod 300 comes into contact with the bottom 15 of the preform 10. In Figure 12(a), the bottom mold 200 has risen to a molding position where it does not come into contact with the bottom 15 of the preform 10 and is waiting before the blow cavity mold is closed. At this time, the protrusion 220 of the bottom mold 200 is located near the bottom of the opening 15a of the outer layer 11 and is not inserted into the opening 15a of the outer layer 11. Next, the blow cavity mold is closed, and the bottom mold 200 in the molding position blocks the bottom side of the blow cavity mold.

[0097] Fig. 12(b) shows a state in which the stretch rod 300 has been lowered from Fig. 12(a). After the blow cavity mold is closed, the stretch rod 300 is lowered toward the bottom 15 of the preform 10, and as shown in Fig. 12(b), the lower end 301 of the stretch rod 300 comes into contact with the bottom of the inner layer 12, and stretching of the preform 10 in the longitudinal direction begins.

[0098] On the other hand, as the preform 10 is stretched by the stretch rod 300, the protrusions 220 of the bottom mold 200 are inserted into the openings 15a of the outer layer 11, as shown in Fig. 12(b) . As a result, the upper ends of the protrusions 220 come into contact with the inner layer 12 filled in the openings 15a.

[0099] Figure 12(c) shows a state in which the stretch rod 300 has been further lowered from the state in Figure 12(b). When the stretch rod 300 is further lowered from the state in Figure 12(b), an upward reaction force acts from the bottom mold 200 on the inner layer 12 in the opening 15a.

[0100] Furthermore, when the stretch rod 300 starts to descend, or is descending (for example, FIG. 12(b)), or when the stretch rod 300 has finished descending (for example, FIG. 12(c)), the supply of blow air into the preform 10 begins via the air introducing member. As a result, the preform 10 is stretched in the horizontal axis direction by the blow air within the mold space formed by the blow cavity mold and the bottom mold 200, and is shaped into the shape of the peeling container 20. Note that, when blow air is being supplied, it is preferable to maintain a state in which the lower end 301 of the stretch rod 300 does not separate from the bottom inner surface of the inner layer 12, at least until the inner layer 12 and the protrusions 220 come into contact.

[0101] In this type of peeling container, an undercut portion may be provided in the bottom of the inner layer 12, and the undercut portion may be inserted into an opening in the bottom of the outer layer 11 to engage the inner layer 12 with the outer layer 11. A peeling container with the above structure can engage the inner layer 12 and the outer layer 11 relatively strongly, but on the other hand, a large force is required to separate the inner layer 12 and the outer layer 11.

[0102] On the other hand, in the second modified example, the protrusions 220 inserted into the openings 15a of the outer layer 11 press the inner layer 12 from below, and the protrusions 220 apply an upward force to the lower surface of the bottom of the inner layer 12. Also, the lower end 310 of the stretch rod 300 presses the inner layer 12 from above, and a downward force is applied to the upper surface of the bottom of the inner layer 12. In other words, the bottom of the inner layer 12 is pressed from above and below, and the bottom of the inner layer corresponding to the protrusions 220 is thinned. As a result, in the peeling container 20A of the second modified example, as shown in FIG. 14 , the shape of the protrusions 220 of the bottom mold 200 is transferred to the inner layer 12 located within the opening 25a, and a recess 25b recessed toward the inside of the container is formed on the outer surface. By forming a recess 25b in the inner layer 12 within the opening 25a of the bottom 25, the axial thickness of the inner layer 12 placed within the opening 25a is reduced, and the radial thickness of the inner layer 12 located within the opening 25a is also reduced.

[0103] As a result, in the peeling container 20A of the second modification, the rigidity of the inner layer 12 placed at the opening 25a is reduced, and when the inner layer 12 is removed from the outer layer 11 after use of the peeling container 20A, the inner layer 12 is easily detached from the outer layer 11 at the opening 25a. Furthermore, when the inner layer 12 is removed from the outer layer 11, it is less likely that the inner layer 12 will break at the opening 25a and thin pieces of the inner layer 12 will remain on the outer layer 11.

[0104] As described above, in the second modified peeling container 20A, the worker can easily separate the inner layer 12 and the outer layer 11 without having to pull the inner layer 12 strongly, which further improves the workability when removing and separating the inner layer 12 from the outer layer 11 after using the peeling container 20A.

[0105] 13(b) and 13(c), in the second modified example, when the protrusions 220 of the bottom mold 200 have a shape with ribs or corners protruding in the radial direction, the recessed portion 25b of the inner layer 12 may have a portion thinner than other portions or a portion distant from the opening 25a of the outer layer 11. These portions may function as vents that allow air to enter between the inner layer 12 and the outer layer 11 from the bottom 25 side when the peeling container 20A is in use.

[0106] The present invention is not limited to the above-described embodiment and each modification, and various improvements and design changes may be made without departing from the spirit of the present invention. For example, the configuration of the above-described embodiment (including at least one of the first and second configuration examples) may be combined with either the first or second modification, or both the first and second modification may be combined.

[0107] In the above embodiment, as an example of a flow path, a hole penetrating in the radial direction may be formed on the outer periphery of the cap portion 32 so that air can flow in from outside to the vent. In this case, too, the formation of the groove 18 on the upper end of the outer layer 11 can be omitted.

[0108] In this embodiment, the lid 30 is provided with the nozzle head 31 having a pump function, but the lid 30 may be, for example, a cap with a check valve that does not have a pump.

[0109] Furthermore, in the above embodiment, due to the difference in shrinkage rate between the inner layer 12 and the outer layer 11 after blow molding, a gap may be formed between the vertical rib 16 of the inner layer 12 and the recess 17 of the outer layer 11. Similarly, a gap may be formed between the lower surface of the step 13c and the upper surface of the protrusion (first opening) 14b. In this case, when the lid 30 is engaged with the neck 13 of the inner layer 12, the vertical rib 16 and the recess 17, and the step 13c and the protrusion 14b are already spaced apart, making it easier to form a vent hole through which air can enter between the outer layer 11 and the inner layer 12 near the neck 13.

[0110] Furthermore, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not by the above description, and is intended to include all modifications within the meaning and scope of the claims.

[0111] DESCRIPTION OF SYMBOLS 10, 10A...preform, 11...outer layer, 12...inner layer, 13...neck portion, 13a...mouth portion, 13b...thread, 14...body portion, 15...bottom portion, 15a...opening portion, 16...longitudinal rib, 16a...protrusion, 16b...claw surface, 17, 17a...recess, 17b...claw surface, 18...groove, 20, 20A...peel container, 24...body portion, 24a...shoulder portion, 25...bottom portion, 25a...opening portion, 25b...recess portion, 30...lid body, 32...cap portion, 33...internal thread, 40...blow molding apparatus, 41...first injection molding section, 42...first temperature adjustment section, 43...second injection molding section, 44...second temperature adjustment section, 45...blow molding section, 200...bottom mold, 220...protrusion portion, 300...stretch rod

Claims

1. A peel-off container comprising: a neck formed by an inner layer, having a mouth on one side and a thread formed on the outer periphery; and a container body connected to the other side of the neck and having an outer layer formed of a material different from the inner layer and laminated on the outside of the inner layer, wherein a protrusion having a diameter larger than that of the neck is formed on one side of the container body adjacent to the neck, a lid can be screwed to the neck of the inner layer, and an air vent for directing air between the inner layer and the outer layer is formed on one side of the container body by displacing the inner layer to one side or circumferentially relative to the outer layer by rotating the lid in the closing direction.

2. A peeling container as described in claim 1, wherein the container body has a rotation prevention portion that, when the lid is rotated in the closing direction, resists circumferential shifting of the inner layer relative to the outer layer while guiding the inner layer to displace to one side relative to the outer layer.

3. A peeling container as described in claim 2, wherein the anti-rotation portion has a protrusion formed on the outer periphery of the inner layer and extending in the axial direction of the container, and a recess formed on the inner periphery of the outer layer for receiving the protrusion.

4. A peeling container as described in claim 3, wherein the anti-rotation portion has a protrusion that is engaged with the recess when the lid body is rotated in the closing direction, and a protrusion that is freely movable in the opening direction relative to the recess when the lid body is rotated in the opening direction.

5. A peeling container according to any one of claims 1 to 4, wherein the lid or the outer layer further has a flow path for introducing air from outside the container toward the vent hole.

6. A peeling container as described in any one of claims 1 to 4, wherein the container body has an opening at the bottom that penetrates the outer layer and exposes the inner layer to the outside, and the inner layer located within the opening has a recess formed on the outer surface side that is recessed toward the inside of the container.

7. A peel-off container comprising: a neck formed by an inner layer, having a mouth on one side and a thread formed on the outer periphery; and a container body connected to the other side of the neck and having an outer layer formed of a material different from the inner layer and laminated on the outside of the inner layer, wherein a protrusion having a diameter larger than that of the neck is formed on one side of the container body adjacent to the neck, a lid can be screwed onto the neck of the inner layer, and the container body has an anti-rotation portion that resists circumferential misalignment of the outer layer and the inner layer when the lid is rotated in the closing direction.

8. A peeling container as described in claim 7, wherein the anti-rotation portion has a protrusion formed on the outer periphery of the inner layer and extending in the axial direction of the container, and a recess formed on the inner periphery of the outer layer for receiving the protrusion.

9. A peeling container as described in claim 8, wherein the anti-rotation portion engages the protrusion with the recess when the lid is rotated in the closing direction, and the protrusion is freely movable in the opening direction relative to the recess when the lid is rotated in the opening direction.

10. A method for manufacturing a peel-off container comprising: a neck formed by an inner layer, having a mouth on one side and a screw formed on the outer periphery; and a container body connected to the other side of the neck and having an outer layer laminated on the outside of the inner layer, the method comprising: a first injection molding step of injection molding an outer layer of a preform corresponding to the container body with a first resin material; a second injection molding step of injecting a second resin material different from the first resin material and laminating the inner layer corresponding to the neck and the container body on the inside of the outer layer; and a blow molding step of blow molding the preform obtained in the second injection molding step while retaining the heat retained during injection molding, to manufacture the peel-off container.

11. A method for manufacturing a peelable container as described in claim 10, wherein the container body has an anti-rotation portion that resists circumferential misalignment between the outer layer and the inner layer when the lid that is screwed onto the neck portion is rotated in the closing direction.

12. An apparatus for manufacturing a peelable container comprising: a neck portion formed by an inner layer, having a mouth portion on one side and a screw formed on the outer periphery; and a container body portion connected to the other side of the neck portion and having an outer layer laminated on the outside of the inner layer, the apparatus including: a first injection molding section that injection molds an outer layer of a preform corresponding to the container body portion with a first resin material; a second injection molding section that injects a second resin material different from the first resin material and laminates the inner layer corresponding to the neck portion and the container body portion on the inside of the outer layer; and a blow molding section that blow molds the preform obtained in the second injection molding section while retaining heat during injection molding, to manufacture a peelable container.

13. The peelable container manufacturing apparatus described in claim 12, wherein the container body has an anti-rotation portion that resists circumferential misalignment of the outer layer and the inner layer when the lid that is screwed onto the neck portion is rotated in the closing direction.

Citation Information

Patent Citations

  • Preform for molding stack type double structure container and double structure container

    JP2018062146A

  • Peeling container and method for manufacturing peeling container

    WO2021206088A1