Analysis device

The integration of a protective layer within the porous base material of analytical devices prevents plasticizer leakage, maintaining sensitivity and stability, addressing the challenge of long-term storage stability in analytical devices.

WO2024232292A1PCT designated stage expired Publication Date: 2024-11-14CANON KK
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/016378
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-10
Filing Date
2024-04-26
Publication Date
2024-11-14

AI Technical Summary

Technical Problem

Analytical devices using porous substrates face challenges in maintaining measurement sensitivity and stability over long-term storage, particularly due to the leakage and diffusion of plasticizers from the ion-selective membrane, which affects ion concentration responsiveness and sensitivity, especially in high-temperature environments.

Method used

Incorporating a protective layer made of materials like polyimide resins or fluororesins within the porous base material to inhibit the penetration of plasticizers, preventing their diffusion into the substrate and maintaining the ion-selective membrane's integrity.

Benefits of technology

The protective layer effectively suppresses plasticizer leakage and diffusion, ensuring consistent measurement sensitivity and stability even after long-term storage, regardless of temperature conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024016378_14112024_PF_FP_ABST
    Figure JP2024016378_14112024_PF_FP_ABST
Patent Text Reader

Abstract

To provide an analysis device capable of maintaining good measurement sensitivity even after long-term storage and obtaining a proper potential with respect to selected ions. Provided is an analysis device comprising: a porous substrate; an electrode formed on the inside, on the surface, or from the inside to the surface of the porous substrate; an ion selective film covering the electrode; and a protective layer. The ion selective film contains a plasticizer. The protective layer is formed inside the porous substrate so as to be close to at least a part of the ion selective film, and contains a component that inhibits permeation of the plasticizer.
Need to check novelty before this filing date? Find Prior Art

Description

analytical devices

[0001] The present invention relates to an analytical device in which a flow path region is formed inside a porous substrate.

[0002] In recent years, analytical devices that utilize small microchannels to efficiently perform biochemical analysis within a single chip have been attracting attention in a wide range of fields. Specifically, small analytical devices have been attracting attention not only in biochemical research but also in fields such as medicine, drug discovery, healthcare, the environment, and food.

[0003] In the early 1990s, photolithography and molds were used to form micrometer-sized fine channels on glass or silicon, and microanalysis chips were developed that could perform sample pretreatment, stirring, mixing, reaction, and detection on a single chip. As a result, miniaturization of testing systems, rapid analysis, and reductions in specimen and waste liquid volumes were realized.

[0004] Electrochemical analysis, which measures the concentration of a target substance by measuring the potential between electrodes immersed in the sample to be analyzed, is widely used in fields such as medicine and the environment. Conventional electrochemical analysis is performed by technicians using sophisticated equipment, which limits the fields and resources available for measurement. However, there is a need for inexpensive, easy-to-use, and disposable microanalysis chips for electrochemical analysis, such as for medical treatment in developing countries, remote areas, and disaster sites where medical facilities are inadequate, as well as for use in airports and other locations where the spread of infectious diseases must be prevented at the border.

[0005] Patent Literature 1 proposes a device including a microanalytical chip capable of measuring potential differences using a porous substrate, enabling electrochemical measurements at low cost, with easy handling and disposal. This device describes a configuration including one or more working electrodes and one reference electrode on a porous substrate, with an ion-selective membrane used as the working electrode, for measuring potential differences between the ion-selective electrode and the reference electrode. Furthermore, the ion-selective membrane of this device typically contains a lipophilic ion receptor (ionophore) and a lipophilic ion exchanger in an optimized molar ratio, both of which are incorporated into a polymer membrane matrix such as plasticized poly(vinyl chloride) (PVC). Potential differences can be measured using this ion-selective membrane.

[0006] Furthermore, Non-Patent Document 1 proposes a filter paper-based measurement device for measuring the concentrations of Na ions and K ions. This device has a dispensing section for dispensing a sample, and the dispensed sample permeates from the dispensing section into the working electrode and reference electrode, electrically connecting the two electrodes and enabling potential difference measurement. The ion-selective membrane of this device is prepared using an ionophore, an anion scavenger, PVC, and DOS and NPOE as plasticizers for Na ions and K ions, respectively. The use of such an ion-selective membrane enables potential difference measurement.

[0007] Furthermore, Non-Patent Document 1 describes depositing KCl ion crystals on the reference electrode to obtain a stable potential at the reference electrode. This allows KCl to dissolve in the sample during measurement, maintaining a high concentration of Cl ions in the reference electrode region and obtaining a stable reference electrode potential. Furthermore, Non-Patent Document 1 describes an ion-selective membrane formed to cover the working electrode, which selects only the ions to be measured, allowing measurement to be performed without being affected by other ions.

[0008] US Patent Application Publication No. 2016 / 033438

[0009] Nipapan Ruecha, Orawon Chailapakul, Koji Suzuki and Daniel Citterio “Fully Inkjet-Printed Paper-Based Potentiometric Ion-Sensing Devices” Analytical chemistry August 29, 2017 Published, 89, pp.10608-10616

[0010] However, analytical devices using porous substrates as described above may not be able to maintain their performance during long-term storage. Specifically, analytical devices using porous substrates have electrodes and an ion-selective membrane formed on the porous substrate, with the ion-selective membrane partially in contact with the porous substrate. The ion-selective membrane also contains a plasticizer, a lipophilic ion exchanger, which transports ionophores during measurement. This plasticizer is typically liquid during measurement (above room temperature) and can flow through the ion-selective membrane. Therefore, the plasticizer oozes out of the ion-selective membrane during long-term storage. When the oozing plasticizer comes into contact with the porous substrate, the capillary action of the porous substrate accelerates the oozing of the plasticizer, which can further diffuse toward the porous substrate. This reduces the amount of plasticizer in the ion-selective membrane, preventing the proper material ratio within the ion-selective membrane from being maintained. As a result, the responsiveness to the ion concentration of the analyte, i.e., the measurement sensitivity, changes, and the potential on the working electrode side may change even for the same analyte concentration.

[0011] This problem is particularly likely to occur during long-term storage in a high-temperature environment, as it is affected by the fluidity of the plasticizer within the ion-selective membrane. Therefore, the extent of the problem can be reduced by setting the storage environment of the analytical device at a low temperature, such as 10°C or below. However, storing analytical devices at low temperatures requires storage equipment and power supply facilities, which may be unusable in some medical settings, such as POCT. Therefore, there is a demand for chips that can perform more stable analysis even after long-term storage, even if they are not stored at low temperatures.

[0012] In view of the above, an object of the present invention is to provide an analytical device for measuring electrolyte concentrations that maintains good measurement sensitivity even after long-term storage and that can obtain an appropriate potential for selected ions.

[0013] According to one aspect of the present invention, there is provided an analytical device having a porous substrate, an electrode formed inside, on the surface, or from the inside to the surface of the porous substrate, an ion-selective membrane covering the electrode, and a protective layer, wherein the ion-selective membrane contains a plasticizer, and the protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion-selective membrane and contains a component that inhibits penetration of the plasticizer.

[0014] According to the present invention, it is possible to provide an analytical device for measuring the concentration of an electrolyte that maintains good measurement sensitivity even when stored for a long period of time and that can obtain an appropriate potential for a selected ion.

[0015] FIG. 1B is a schematic diagram illustrating the analytical device of Example 1. FIG. 1A is a cross-sectional view taken along the dotted line in FIG. 1A. FIG. 2A is a schematic diagram illustrating an analytical device of a modified example of Example 1. FIG. 2A is a cross-sectional view taken along the dotted line in FIG. 2A. FIG. 1B is a schematic diagram illustrating the analytical device of Example 1. FIG. 2C is a cross-sectional view taken along the dotted line in FIG. 2A. FIG. 1C is a schematic diagram illustrating the analytical device of Example 1. FIG. 3C is a schematic diagram illustrating an example of potential difference measurement of the analytical device. FIG. 3D is a schematic diagram illustrating the state when a sample is dispensed into the analytical device. FIG. 3E is a schematic diagram illustrating an analytical device of a comparative example of the present invention. FIG. 5A is a cross-sectional view taken along the dotted line in FIG. 5A. FIG. 5D is a schematic diagram illustrating analytical devices of Examples 2 and 4. FIG. 6A is a cross-sectional view taken along the dotted line in FIG. 6A. FIG. 6E is a schematic diagram illustrating an analytical device of a modified example of Example 3. FIG. 7A is a cross-sectional view taken along the dotted line in FIG. 7A. FIG. 8A is a cross-sectional view taken along the dotted line in FIG. 8A. FIG. 9A is a schematic diagram illustrating a state of measuring a sample using the analytical device of Example 5. FIG. 9D is a cross-sectional view taken along the dotted line in FIG. 9A. FIG. 9E is a schematic diagram illustrating a modified example of the analytical device.

[0016] One embodiment of the present invention provides an analytical device having a porous substrate, electrodes formed inside, on the surface, or from the inside to the surface of the porous substrate, an ion-selective membrane covering the electrodes, and a protective layer, wherein the ion-selective membrane contains a plasticizer, and the protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion-selective membrane and contains a component that inhibits penetration of the plasticizer.

[0017] The analytical device may have a flow path region (sometimes simply referred to as a flow path) surrounded by a flow path wall formed inside the porous substrate. In this case, the electrodes, ion-selective membrane, and protective layer are formed in the flow path region. The flow path region includes a first flow path chamber, a second flow path chamber, and a flow path connecting them. The electrodes, ion-selective membrane, and protective layer are formed in the first flow path chamber, and the second flow path chamber may include a reference electrode.

[0018] The ion-selective membrane can be formed within, on, or in and on the surface of the porous substrate and includes a plasticizer.

[0019] The protective layer is formed in close proximity to at least a portion of either the back surface or the periphery of the ion selective membrane. The back surface refers to the surface opposite the front surface. In this specification, "close" and "close to" refer to either adjacent or nearby, even if not adjacent. The protective layer is formed in close proximity to at least a portion of the ion selective membrane, such as the electrode or the bottom surface and periphery of the ion selective membrane. The protective layer inhibits the penetration of the plasticizer contained in the ion selective membrane and suppresses the plasticizer in the ion selective membrane from seeping out and diffusing into the porous substrate through the voids in the porous substrate or the fibers that make up the porous substrate. Therefore, the protective layer is preferably made of a material that is incompatible with the plasticizer. The protective layer preferably contains a resin, and examples of such resins include polyimide resins and fluorine-based resins. The polyimide resin is preferably a resin made of a polymer compound containing an imide bond (-CO-NR-CO-). The fluorine-based resin is a resin containing a fluoroalkylene structure, such as -(CF)- or -(CF 2)- repeating structure is preferable. Alternatively, the protective layer can be formed by printing and further heating resin particles. In this case, a preferable example of the resin particles is toner particles.

[0020] Examples and comparative examples of the present invention will be described below with reference to the drawings. Note that the following examples are illustrative and do not limit the present invention to the contents of the embodiments. Furthermore, in the following drawings, components that are not necessary for explaining the embodiments are omitted from the drawings.

[0021] Example 1 The configuration of the analytical device of this example will be described using the drawings. FIGS. 1A and 1B show an analytical device 100 of Example 1. The analytical device 100 has a flow path region 3 surrounded by a flow path wall 2 provided inside a porous substrate 1. The analytical device 100 had a horizontal width L1 of 22 mm and a vertical width H1 of 17 mm. The flow path region 3 includes a first flow path chamber 3a, a second flow path chamber 3b, each 6 mm square, and a third flow path chamber 3c and a fourth flow path chamber 3d, each 6 mm square and 3 mm high, as contact portions with the base electrode. The flow path region 3 also includes a 6 mm wide, 4 mm high flow path connecting the first flow path chamber 3a and the second flow path chamber 3b, and a 2 mm wide, 3 mm high flow path connecting the first flow path chamber 3a and the third flow path chamber 3c, and the second flow path chamber 3b and the fourth flow path chamber 3d. The third flow path chamber 3c and the fourth flow path chamber 3d can be provided from the viewpoint of adhesion between the substrate and the electrodes, but are not necessary. A working electrode 4 is disposed in the first flow chamber 3a. The working electrode 4 is composed of a 2 mm square base electrode 5 connected to the third flow chamber and a 4 mm square ion selective membrane 6 covering the base electrode 5. A plasticizer 7 is contained within the ion selective membrane 6. A protective layer 8 is disposed on the back surface of the working electrode 4, at the portion of the analytical device 100 where the ion selective membrane 6 is present. In this embodiment, the protective layer 8 is actually located on the back surface of the ion selective membrane 6 and therefore cannot be seen from above, but for convenience, the protective layer 8 is shown in FIG. 1A. FIG. 1B is a cross-sectional view of the analytical device 100 taken along the dotted line in FIG. 1A.

[0022] The specific configuration and manufacturing method of the analytical device of this example will be described. In this example, filter paper with a thickness of 100 μm and a porosity of 50% was used as the porous substrate 1. By using filter paper as the porous substrate, capillary action can be generated in the liquid, allowing the sample to be measured to flow through the flow path even in an electrically uncharged environment.

[0023] In this example, filter paper was used as the porous substrate, but the porous substrate is not limited to this and may be any material that generates capillary action in a liquid. For example, the porous substrate may have a porous structure such as a mesh structure, such as open cells or nanofibers, or may be resin, glass, an inorganic substrate, fabric, metal paper, or the like.

[0024] Furthermore, while the thickness of the porous substrate 1 used here is 100 μm, it is not limited to this and can be selected appropriately depending on the purpose, and a thickness of approximately 20 μm to 300 μm is often used. If the thickness is less than 20 μm, the strength of the substrate may not be maintained. If the thickness is more than 300 μm, materials such as the ion-selective membrane 6 and protective layer 8 may easily diffuse into the analytical device, which may result in a deterioration in dimensional accuracy. However, depending on the application, a thick porous substrate 1 of approximately 600 μm may be used by adjusting the arrangement within the analytical device.

[0025] The flow path region 3 was formed by the method described in JP 2021-37612 A. Specifically, a desired flow path pattern was formed in an unfixed state on a porous substrate by electrophotography using flow path wall forming particles T1 (toner) characterized by meltability, and then heated in an oven or heater, etc. The flow path wall 2 was formed by penetrating the flow path pattern into the porous substrate, and the flow path region 3 was formed.

[0026] In this example, particles T1 having a number average particle size of 6.5 μm, which were produced by the following production method, were used as particles for forming the flow path walls. The production method of particles T1 will be described below.

[0027] <Production of Particles T1> [Preparation of Polymerizable Monomer Composition] The following components were mixed and then dispersed in a ball mill for 3 hours. Styrene 70.0 parts n-butyl acrylate 30.0 parts divinylbenzene 0.1 parts polyester resin 5.0 parts (polycondensate of propylene oxide-modified bisphenol A and isophthalic acid (glass transition point 65°C, weight average molecular weight (Mw) 10,000, number average molecular weight (Mn) 6,000)) The resulting dispersion was transferred to a reactor equipped with a propeller stirring blade and heated to 60°C while stirring at a rotation speed of 300 rpm. Thereafter, 3.0 parts of 2,2'-azobis(2,4-dimethylvaleronitrile) was added and dissolved to prepare a polymerizable monomer composition.

[0028] [Preparation of Aqueous Dispersion Medium] 710 parts of ion-exchanged water and 450 parts of a 0.1 mol / L aqueous solution of sodium phosphate were added to a 2 L four-neck flask equipped with a high-speed stirring device, T. K. Homomixer (manufactured by Primix Corporation), and the mixture was heated to 60°C while stirring at a rotation speed of 12,000 rpm. 68.0 parts of a 1.0 mol / L aqueous solution of calcium chloride was added to the flask to prepare an aqueous dispersion medium containing calcium phosphate (a poorly water-soluble dispersion stabilizer).

[0029] [Granulation and Polymerization] The polymerizable monomer composition was added to the aqueous dispersion medium, and while maintaining a rotation speed of 12,000 rpm, 10 parts of a polymerization initiator, t-butyl peroxypivalate, was added and granulated for 15 minutes. The high-speed agitator was then replaced with a propeller agitator, and the internal temperature was maintained at 60°C to continue the polymerization reaction for 5 hours. The internal temperature was then increased to and maintained at 80°C, and the polymerization reaction was continued for another 3 hours. After completion of the polymerization reaction, the remaining monomer was distilled off at 80°C under reduced pressure, and the mixture was cooled to 30°C to obtain a polymer microparticle dispersion.

[0030] [Washing] The polymer microparticle dispersion was transferred to a washing container, and while stirring, dilute hydrochloric acid was added to adjust the pH to 1.5. The dispersion was stirred for 2 hours, and then subjected to solid-liquid separation using a filter to obtain polymer microparticles. This was then added to 1,200 parts of ion-exchanged water and stirred to form a dispersion again, and then subjected to solid-liquid separation using a filter. This operation was repeated three times to obtain base particles of particles T1.

[0031] [External Addition] Furthermore, 1.0 part of a flowability improver (silica having a number average particle diameter of 7 nm) surface-treated with hexamethyldisilazane was dry-mixed with 100.0 parts of the obtained base particles for 5 minutes using a Henschel mixer to obtain flow path pattern image-forming particles T1 having a number average particle diameter D1 of 6.5 μm.

[0032] The method for forming the flow paths is not limited to the method of this embodiment, and any other method may be used as long as the flow path pattern can be formed, such as a method of cutting the porous substrate 1 so that only the flow path shape remains, or a method of forming the flow path walls 2 with a wax printer.

[0033] Next, the protective layer, a feature of the present invention, will be described. In this example, flow path wall-forming particles T1 (toner) were used as the material for the protective layer 8. As with the flow path wall-forming process described above, the protective layer was produced by electrophotographically drawing a pattern of flow path walls 2 on the ion selective membrane 5-forming portion of the porous substrate 1. Here, it is preferable for the protective layer portion to have as many flow path wall-forming particles as possible penetrate into the porous substrate from the viewpoint of sealing the porous substrate. Therefore, the flow path wall pattern drawing formation process using electrophotography and the penetration process into the porous substrate using an oven or heater were repeated four times so that the amount of flow path wall 2 patterned in the protective layer 8 portion was greater than the amount of flow path wall 2 drawn in the flow path wall-forming process. That is, the protective layer contained approximately four times as many flow path wall-forming particles as the flow path walls. The formed protective layer pattern is shown in FIGS. 1A and 1B.

[0034] In this example, the protective layer forming step was performed after the flow path wall forming step, but the pattern formation in the flow path wall forming step and the pattern formation in the protective layer forming step may be performed simultaneously. In this case, since there is a limit to the amount of flow path wall-forming particles that can be transferred to the porous substrate, the protective layer forming step may be additionally performed as necessary, as in this example, to increase the amount of drawing in the protective layer portion.

[0035] In this embodiment, toner, which is a particle for forming the flow path wall, was used as the material for the protective layer 8, but this is not limited thereto. It is sufficient that the protective layer 8 seals the area where the ion selective membrane 6 and the porous substrate 1 are adjacent. An analytical device according to a modified example of Example 1 is shown in FIGS. 2A and 2B. For example, as shown in the cross-sectional view of FIG. 2B, a known toner that does not penetrate the porous substrate 1 much can be pre-placed as a protective layer at the area where the ion selective membrane 6 and the porous substrate 1 contact. By turning the porous substrate 1 upside down and forming a base electrode 5 and an ion selective membrane 6 on it, a configuration such as that shown in FIG. 8B can be obtained. Furthermore, by locally drawing the toner, a protective layer can be formed around the ion selective membrane, as shown in FIG. 7B. Furthermore, by locally increasing or decreasing the amount of drawing, a protective layer can be formed on the back surface and periphery of the ion selective membrane, as shown in FIG. 6B, for example. The thickness of the protective layer (thickness perpendicular to the surface of the device) is preferably 10 μm or more when the protective layer is placed on the back surface of the ion selective membrane, with no particular upper limit. If it is 10 μm or less, it may not be possible to sufficiently inhibit the penetration of the plasticizer. When the protective layer is placed around the ion selective membrane, it is desirable to adjust the width of the protective layer so that the analyte dropped on the ion selective membrane can move to the porous substrate. As shown in FIG. 10, when the ion selective membrane is formed inside the porous substrate, the width of the protective layer (thickness in the surface direction of the device) is preferably 1 mm or less. When the ion selective membrane is located on the surface of the substrate, as shown in FIG. 4B, the analyte moves by utilizing the height difference between the ion selective membrane and the porous substrate, so the upper limit of the width of the protective layer can be 2 mm.

[0036] In this embodiment, as shown in Figure 1B, a protective layer was placed inside the porous substrate in the ion-selective membrane-forming portion, but this is not limited to this. As in the embodiments described below, by filling the area where the ion-selective membrane 6 and the porous substrate 1 are in contact with each other with a protective layer, it is possible to reduce the diffusion of the plasticizer 7 contained in the ion-selective membrane 6 into the porous substrate 1.

[0037] Next, the working electrode 4 was formed on the flow path pattern 3 formed above by screen printing, an ink jet device, a dispenser, or the like.

[0038] 1A, an Ag / AgCl electrode was printed by screen printing on the flow path pattern 3 as the base electrode 5 of the working electrode. Next, an intermediate layer of NaCl (not shown) was formed on the base electrode 5 by an inkjet method, and then an ion-selective membrane 6 having selectivity for target ions was laminated thereon to form a solid-contact ion-selective electrode as the working electrode 4. In this example, the ion-selective electrode used Na ions as the target ions.

[0039] The base electrode 5 may be made of any known material, such as Ag / AgCl, carbon, or PEDOT / PSS, without any particular limitation. For the preparation of an electrode using Ag / AgCl or carbon, see, for example, Patent Document 1. For the preparation of an electrode using PEDOT / PSS, see, for example, Non-Patent Document 1. For the base electrode, an electrode suited to the required characteristics of the device, such as cost and performance, may be selected. In this example, an Ag / AgCl electrode was used as the base electrode 5.

[0040] The intermediate layer may be made of a commonly used electrolyte such as NaCl or KCl, and in this example, was made by applying an aqueous NaCl solution by inkjet printing.

[0041] The ion selective membrane 6 may be any commonly used membrane, as long as it has sensitivity to the target ions and sufficient selectivity to interfering ions.

[0042] The material used for the ion-selective membrane may be any commonly used material. The ion-selective membrane preferably contains an ionophore and an anion filter that exhibit ion selectivity. An example of the ionophore is 12-crown 4-ether, which has a crown ether structure, and an example of the anion filter is sodium tetraphenylborate (NaTPB). The above materials were used in this example. Any known material can be used for the ion-selective membrane. For examples of such materials, see pages 138 to 140 of "Measuring Ion Concentration with an Electrode" by Dojindo Laboratories, Ltd.

[0043] Furthermore, to maintain the structure of the ion-selective membrane, the ion-selective membrane contains a polymeric agent. Examples of the polymeric agent include polyvinyl chloride (abbreviated as PVC) and a copolymer of vinyl chloride and vinyl acetate. In this example, polyvinyl chloride was used.

[0044] The ion-selective membrane also contains a plasticizer 7 to activate the ionophore. While known plasticizers can be used as the plasticizer 7, lipophilic ion exchange materials that act as lipophilic ion exchangers in the ion-selective membrane are more preferred. Examples of known plasticizers include 2-nitrophenyl octyl ether (abbreviation: NPOE), bis(2-ethylhexyl) sebacate (abbreviation: DOS), bis(2-ethylhexyl) adipate (abbreviation: DOA), and di-n-octylphenylphosphonate (abbreviation: DOPP). In this example, DOS was used as the plasticizer 7.

[0045] The ion-selective membrane 6 can be produced by mixing appropriate amounts of each of the above-mentioned components, dissolving or dispersing them in a solvent such as THF or cyclohexanone, and applying the resulting liquid by an inkjet method onto a base electrode (Ag / AgCl electrode) on which an intermediate layer such as NaCl is laminated.

[0046] The method for applying the ion selective membrane 6 is not limited to the inkjet method, and a dispenser, screen printing, or the like may also be used as appropriate. The viscosity of the solution may be adjusted according to the respective application method, and then the ion selective membrane 6 may be laminated on the base electrode 5.

[0047] In this example, the configuration and fabrication method of the working electrode according to the present invention have been described. However, in order to measure the electrolyte of a sample, a configuration may be used in which a reference electrode 9 is provided in addition to the working electrode 4, and measurement is performed using the potential difference between the two electrodes, as shown in FIG. 3. In this figure, the reference electrode is shown as consisting of only an electrode. The configuration and fabrication method of the reference electrode are well known, so a description thereof will be omitted.

[0048] Next, a method for measuring the electrolyte concentration of a sample using the analytical device of the present invention will be described. In this example, in order to focus only on the performance of the working electrode, a commercially available reference electrode 10 was placed on one side of the analytical device where the reference electrode was formed, as shown in Figure 4A, and the reference electrode 10 and working electrode 4 were connected via the sample, and the potential difference between the two electrodes was measured.

[0049] In this example, a sample was dispensed onto the surface of the working electrode 4 and then measured. As shown in Figures 4A and 4B, the sample 11 is dispensed onto the surface of the ion selective membrane 6 in the first flow channel chamber 3a, then flows by capillary action, passes through a channel connecting the first flow channel chamber 3a and the second flow channel chamber 3b, and reaches the reference electrode portion in the second flow channel chamber 3b. As a result, the reference electrode 10 and the working electrode 4 are electrically connected by the sample 11, and the potential difference is measured.

[0050] In this embodiment, the Na concentration of the sample 11 to be dispensed is set to 10 -5 Measurements were carried out while varying the concentration from 0.1 mol / L to 1 mol / L, and the potential difference between the reference electrode 10 and the working electrode 4 was plotted, and the slope of the plot was calculated as the sensitivity.

[0051] Next, a method for evaluating the long-term storage performance of an analytical device will be described. In this example, as an accelerated test for long-term storage, the analytical device was stored in a constant temperature and humidity chamber at 55°C and 30% humidity for 3 months, and the change in sensitivity to Na ions before and after storage was evaluated.

[0052] The evaluation results of the accelerated test were evaluated as follows: if the absolute value of the rate of change in sensitivity before and after storage was less than 1%, it was rated as "good", if it was 1% or more but less than 2%, it was rated as "passable", and if it was 2% or less, it was rated as "fail". The absolute value of the rate of change in sensitivity was calculated using the following formula (1): 100 x |Sensitivity after storage - Sensitivity before storage| / Sensitivity before storage Formula (1)

[0053] Furthermore, to compare the effects of this example with those of the analytical device 200 shown in Figures 5A and 5B, a similar evaluation was carried out as a comparative example. The analytical device 200 of the comparative example had the same configuration as that of Example 1, except that it did not have the protective layer 8. The evaluation results are shown in Table 1.

[0054] When the analytical device 200 of the comparative example was used, the sensitivity increased significantly after storage, but when the analytical device 100 of Example 1 was used, it was found that the change in sensitivity was suppressed.

[0055] The analytical device of Example 1 has a configuration in which a protective layer 8 is disposed inside the porous substrate 1 on the back surface of the portion where the ion selective membrane 6 is formed, thereby reducing the area where the ion selective membrane 6 and the porous substrate 1 come into direct contact. Furthermore, since the inside of the porous substrate 1 is filled and sealed with the protective layer 8, the plasticizer 7 in the ion selective membrane 6 acts to suppress seeping and diffusion into the porous substrate 1 through the voids in the porous substrate 1 or the fibers that make up the porous substrate 1.

[0056] The contact angle of the protective layer of this example with water was measured using a contact angle meter (DropMaster, manufactured by Kyowa Interface Science Co., Ltd.). The results are shown in Table 1.

[0057] The contact angle of water of the protective layer 8 of the analytical device 100 of Example 1 was increased compared to the analytical device 200 of the comparative example without a protective layer. The surface free energy of the protective layer 8 portion was reduced, which acted to reduce the wettability of the plasticizer 7 to the porous substrate 1, and therefore the penetration of the plasticizer 7 into the porous substrate 1 in the protective layer 8 portion was able to be reduced.

[0058] [Example 2] In this example, instead of the flow path wall-forming particles used in Example 1, a polyimide resin was filled into the inside of the porous substrate where the ion selective membrane was disposed and around it to form a protective layer.

[0059] In this example, as shown in Figures 6A and 6B, a flow path pattern 3 was formed on the porous substrate 1 in the same manner as in Example 1, and then a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed. Then, on the back surface of the porous substrate 1 on which the ion selective membrane 6 was arranged (the position shown by diagonal lines in Figure 6B), a polyimide varnish (a varnish obtained by dissolving KPI-MX300F manufactured by Kawamura Sangyo Co., Ltd. in methyl ethyl ketone) was drawn using an inkjet method and dried at 150 ° C. to form a polyimide film inside the porous substrate 1 on which the porous ion selective membrane 6 was arranged and in the vicinity thereof, which was used as a protective layer 8. The evaluation results of this example are shown in Table 1.

[0060] [Example 3] In this example, instead of the polyimide used in Example 2, a fluorine-based resin was filled in the vicinity of the ion-selective membrane of the porous substrate to form a protective layer.

[0061] In this example, as shown in Figures 7A and 7B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 in the same manner as in Example 2. Thereafter, a fluorine-based resin (SF Coat: SFE-B002H manufactured by AGC Seimi Chemical Co., Ltd.) was drawn by an inkjet method at the position indicated by diagonal lines in Figure 7B of the porous substrate on which the ion selective membrane 6 was arranged, that is, in the vicinity of the ion selective membrane 6 of the porous substrate 1, and then naturally dried at room temperature to form a fluoropolymer membrane, which was used as a protective layer 8. The evaluation results of this example are shown in Table 1.

[0062] [Example 4] In this example, instead of the polyimide used in Example 2, a fluorine-based resin was filled in the inside of the porous substrate where the ion-selective membrane was disposed and in the vicinity thereof to form a protective layer.

[0063] In this example, as shown in Figures 6A and 6B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 by the same method as in Example 2. Thereafter, a fluorine-based resin (Somaflon AF manufactured by Somar) was drawn by an inkjet method at the position indicated by diagonal lines in Figure 6B of the porous substrate 1 where the ion selective membrane 6 was arranged, and then naturally dried at room temperature to form a fluoropolymer membrane, which served as a protective layer. The evaluation results of this example are shown in Table 1.

[0064] [Example 5] This example differs from Example 4 in the arrangement of the protective layer, in that the protective layer is formed by filling a fluorine-based resin inside the porous substrate where the ion-selective membrane is arranged.

[0065] In this example, as shown in Figures 8A and 8B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 by the same method as in Example 2. Thereafter, a fluororesin (Somaflon AF manufactured by Somar) was applied by an inkjet method to the position of the porous substrate 1 where the ion selective membrane 6 was disposed, which is indicated by diagonal lines in Figure 8B, and then allowed to dry naturally at room temperature to form a fluoropolymer membrane as a protective layer, which was used as the protective layer.

[0066] In this example, as shown in Figures 9A and 9B, a sample was dispensed onto the surface of the flow path between the working electrode and the reference electrode, and measurements were performed. After being dispensed into the flow path connecting the first flow path chamber 3a and the second flow path chamber 3b, the sample 11 flows by capillary action and reaches the side of the working electrode 4 in the first flow path chamber 3a and the reference electrode in the second flow path chamber 3b. This connects the commercially available reference electrode 10 and the working electrode 4 via the sample 11, and the potential difference is measured. The evaluation results of this example are shown in Table 1.

[0067]

[0068] Each example will be explained using Table 1. In comparison with the comparative example in which there was no protective layer in the region adjacent to the ion-selective membrane, the contact angle of the protective layer in each example was higher than the contact angle of the porous substrate. In other words, it can be seen that the contact angle at the protective layer increased and the surface free energy decreased.

[0069] Furthermore, in Example 3, since a protective layer is not provided on the back surface of the ion selective membrane, which is the contact area between the ion selective membrane and the porous substrate, the degree of diffusion of the plasticizer into the porous substrate increases, and the rate of sensitivity change is larger than in Examples 2 and 4. However, it can be seen that a configuration in which a protective layer is provided at least in the vicinity thereof can provide the effect of suppressing the outflow of plasticizer from the ion selective membrane. Therefore, the arrangement of the protective layer is not limited to the position shown in this example, and it may be in a nearby area, such as the periphery or back surface of the ion selective membrane.

[0070] In the adjacent region, it is more preferable to place a protective layer at the contact area between the ion-selective membrane and the porous substrate, since by placing a protective layer to further reduce the contact area between the ion-selective membrane and the porous substrate, it is possible to prevent the plasticizer that has flowed out from the ion-selective membrane from penetrating and diffusing into the porous substrate due to capillary action.

[0071] In addition, the material of the protective layer is not limited to the materials shown in this embodiment, and known materials can be used. By arranging the protective layer, the pores in the porous substrate are sealed, the contact angle of the porous substrate is increased, and the surface free energy is reduced, thereby further suppressing the penetration of the plasticizer, which is preferable. The contact angle of the protective layer is preferably higher than the contact angle of the porous substrate 1. More specifically, from the viewpoint of reducing the surface free energy, it is preferably 80 ° or more, and more preferably 100 ° or more.

[0072] Furthermore, although there are no particular regulations regarding the thickness of the protective layer, when a protective layer is placed around the ion selective membrane in the vicinity thereof as in Example 4, it is more preferable to set the thickness of the protective layer so that the height of the protective layer is lower than the height of the ion selective membrane, so that the measurement sample can be easily connected between the ion selective membrane and the flow path during measurement. However, the ion selective membrane does not necessarily have to be on the surface of the porous substrate; as shown in Figure 10, it may be placed inside the porous substrate and the protective layer may be placed around it. In such cases, the width of the surrounding protective layer is preferably 1 mm or less, so that the measurement sample can be easily connected between the ion selective membrane and the flow path.

[0073] The present invention is not limited to the above-described embodiments, and various modifications and variations can be made without departing from the spirit and scope of the present invention. Therefore, the following claims are appended to apprise the public of the scope of the present invention.

[0074] This application claims priority based on Japanese Patent Application No. 2023-078162, filed on May 10, 2023, the entire contents of which are incorporated herein by reference.

[0075] REFERENCE SIGNS LIST 1 Porous substrate 2 Channel wall 3 Channel region (channel pattern) 4 Working electrode 5 Base electrode 6 Ion-selective membrane 7 Plasticizer 8 Protective layer 9 Reference electrode 10 Commercially available reference electrode 11 Sample 100 Analytical device

Claims

1. An analytical device having a porous substrate, an electrode formed inside, on a surface, or from inside to a surface of the porous substrate, an ion selective membrane covering the electrode, and a protective layer, wherein the ion selective membrane contains a plasticizer, and the protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion selective membrane and contains a component that inhibits penetration of the plasticizer.

2. The analytical device according to claim 1, which has a flow path region surrounded by a flow path wall formed inside the porous substrate.

3. The analytical device according to claim 2, wherein the electrodes, the ion selective membrane, and the protective layer are formed in the flow path region.

4. The analytical device according to any one of claims 1 to 3, wherein the plasticizer is a lipophilic ion exchange material.

5. The analytical device according to any one of claims 1 to 4, wherein the protective layer contains at least a resin.

6. The analytical device according to any one of claims 1 to 5, wherein the protective layer is made of a material incompatible with the plasticizer.

7. The analytical device according to any one of claims 1 to 6, wherein the protective layer contains at least a fluorine-based resin.

8. An analytical device according to any one of claims 1 to 7, wherein the contact angle of the protective layer is higher than the contact angle of the porous substrate.

Citation Information

Patent Citations

  • Manufacturing method for micro-passage device

    JP2021037612A

  • Techniques for communicating synchronization signal block index in physical broadcast channel payload

    JP2023078162A

  • Microanalysis chip, electrolyte concentration measurement system, and electrolyte concentration measurement method

    JP2023048923A

  • Micro analysis chip

    JP2023156182A

  • Micro analysis chip

    JP2023160684A