A low work-function electrode comprising n-type conductive polymer
The use of an n-type conductive polymer and polymeric cation in a layered structure addresses the challenge of maintaining high conductivity and stability in low-work function polymeric electrodes for optoelectronic devices, achieving a low work function and suitable conductivity for high-performance applications.
Patent Information
- Application Number
- PCT/EP2023/063341
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-17
- Publication Date
- 2024-11-21
AI Technical Summary
Current low-work function polymeric electrodes for optoelectronic devices face challenges in maintaining high conductivity and stability due to surface modifications required for p-type conducting polymers like PEDOT:PSS, which reduce their performance.
A low-work function polymeric electrode comprising a first film layer of n-type conductive polymer and a second film layer of n-type polymeric cation, with optional additional n-type inorganic oxide layers, where the n-type conductive polymer is based on heterocyclic moieties like 3,7-dihydrobenzo[1,2-b:4,5-b']difuran-2,6-dione and the n-type polymeric cation is linear or branched polyethyleneimine, ethoxylated, to achieve a low work function without compromising conductivity.
The solution effectively lowers the work function of the electrode to 2-5 eV while maintaining conductivity in the range of 100-2500 S/cm, suitable for high-performance optoelectronic devices like organic solar cells, without impairing the stability and conductivity of the first film layer.
Smart Images

Figure EP2023063341_21112024_PF_FP_ABST
Abstract
Description
[0001]A LOW WORK-FUNCTION ELECTRODE COMPRISING N-TYPE CONDUCTIVE POLYMER TECHNICAL FIELD The present invention relates to a low-work function polymeric electrode for an optoelectronic device. Further, the present invention relates to a method for manufacturing such an electrode. BACKGROUND OF THE INVENTION Both high- and low-work-function (WF) electrodes are vital units in state-of- the-art optoelectronic devices. Conducting polymers are potential candidates for such electrodes due to their high conductivity, flexibility, and solution-processibility. The poly(3,4-ethylenedioxythiophene) doped with polystyrene sulfonate (PEDOT:PSS), being the most common p-type conducting polymer, is widely used as high-WF electrode in solar cells, photodiodes, and light-emitting diodes. Although PEDOT:PSS can be used as low-WF electrode after surface modification with an amine group, such a modification will typically reduce conductivity of the polymer and impair stability of the device. Therefore, low-WF polymeric electrode with high conductivity for high performance optoelectronic devices is still a challenge. SUMMARY OF THE INVENTION In view of the above, the present invention aims to solve the problems of the prior art. To this end, the present invention relates to a low-work function polymeric electrode for an optoelectronic device, the electrode comprising: a first film layer comprising an n-type conductive polymer; and a second film layer comprising an n-type polymeric cation. The second film layer may be deposited on the first film layer to lower the work function of the electrode. Further, at least one additional layer may be present between the first and the second film layers. Such an additional layer may be an n- type inorganic oxide such as ZnO, SnO2, TiO2or mixtures thereof. The thickness of the first film layer may be in the range from 10 nm to 1 μm, depending on the deposition technology used during manufacturing of the electrode. In particular, the thickness of the first film layer may be in the range from 20 nm to 50 nm. The thickness of the second film layer should be kept at a minimum due to its poor conductivity. In particular, the thickness of the second layer may be in the range from 0.1 nm to 50 nm, preferably from 1 nm to 30 nm. The monomer in the n-type conductive polymer may be in the form of a heterocyclic moiety having a central symmetrical benzene ring fused with at least one, preferably at least two rings, preferably five-membered rings. The monomer further comprises an active hydrogen and at least one electron-withdrawing group at the benzylic position. In particular, the monomer may be 3,7-dihydrobenzo[1,2-b:4,5- b']difuran-2,6-dione (HBFDO), 5,7-dihydropyrrolo[2,3-f]indole-2,6(1H,3H)-dione, or 3,7-dihydrobenzo[1,2-b:4,5-b']dithiophene-2,6-dione. In particular, the monomer is 3,7-dihydrobenzo[1,2-b:4,5-b’]difuran-2,6-dione (HBFDO). In such an embodiment, the n-type conducting polymer is poly(benzodifurandione) (PBFDO), having the following structure: The n-type conductive polymer may comprise from 2 to 10000, more preferably from 6 to 1000, even more preferably from 3 to 100, most preferably from 5 to 50 repetitive units. The n-type polymeric cation according to the present invention is preferably linear polyethyleneimine (PEIlin), branched PEI (PEIbra), ethoxylated PEI (PEIE) or mixtures thereof. The number of repetitive units in the n-type polymeric cation may be from 5 to 10000, preferably from 10 to 1000, more preferably from 20 to 100 repetitive units. When the n-type polymeric cation is branched PEI, a, b, c and d are positive integers, such that the sum of these integers is from 5 to 10000, preferably from 10 to 1000, more preferably from 50 to 100. When the n-type polymeric cation is ethoxylated PEI, x, y and z are positive integers, such that the sum of these integers is from 5 to 10000, preferably from 10 to 1000, more preferably from 50 to 100. According to the present invention, the n-type polymeric cation modifies the work function of the n-type conductive polymer. In other words, the conductivity of the first film layer is negligibly affected by addition of the second film layer, since the n- type conductive polymer of the first film layer already has high conductivity. The first film layer may have a work function in the range from 3 to 6 eV, preferably about 5 eV. Further, the first film layer may have a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm. The electrode may have a work function in the range from 2 to 5 eV, preferably about 4 eV. Further, the electrode may have a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm. The present invention further relates to an organic solar cell comprising an electrode as described above. The organic solar cell may have a structure comprising a cathode, an electron transport layer (ETL), an active layer, a hole transport layer (ETL) and an anode. In particular, the low WF polymeric electrode as described above may act as cathode. The present invention further relates to a method for manufacturing a low- work function polymeric electrode for an optoelectronic device, the method comprising the steps of: a) depositing a first solution comprising an n-type conductive polymer on a substrate, thus obtaining a first film layer; b) depositing a second solution comprising an n-type polymeric cation on the first film layer thus obtaining a second film layer. The substrate may be rigid or flexible. By the term “rigid” is understood as being deficient in or devoid of flexibility. By the term “flexible” is understood as being supple enough to bend freely or repeatedly without breaking. Further, the substrate may be transparent or opaque. By the term “transparent” is understood as having the property of transmitting light without appreciable scattering so that bodies lying beyond are seen clearly. By the term “opaque” is undersood as blocking the passage of radiant energy and especially light. In particular, the substrate may be manufactured of glass, polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethersulfone (PES) or mixtures thereof. It should be mentioned that there should be at least one transparent electrode in a solar cell in order to allow the solar radiation to enter the solar cell. The concentration of the n-type conductive polymer in the first solution may be from 0.1 to 500 mg / mL, preferably from 1 to 100 mg / mL. The solvent used for preparing the first solution may be a polar aprotic solvent, a polar protic solvent or a mixture thereof. In particular, the solvent may be DMSO, DMF, water or mixture thereof. The concentration of the n-type polymeric cation in the second solution may be from 0.01 to 100 mg / mL, preferably from 0.1 to 10 mg / mL. The second solution may comprise a polar protic or aprotic solvent. The polar protic solvent may be water, alcohol or mixture thereof. The alcohol may be selected from the group consisting of methanol, ethanol, propan-1-ol, propan-2-ol (IPA), butan-1-ol, 2-methylpropan-1-ol, 2-methylpropan-2-ol, 2-methylbutan-2-ol, ethane-1,2-diol, 2-methoxyethan-1-ol, and 1-methoxypropan-2-ol or mixtures thereof, as illustrated below. In particular, the alcohol is ethanol, IPA, methanol or mixtures thereof. According to the present invention, the first solution and / or the second solution may be deposited by a solution-processed technology, such as spin-coating, drop-casting, spray-coating, injet-printing and screen-printing. The first and / or the second solutions of the present invention may be deposited in air and ambient temperature, forming the film having thickness of from 10 nm to 1 μm. The thermal annealing may be performed at temperatures from 40°C to 200°C for periods from 1 min to 1200 min. Preferably, thermal annealing is performed at 50°C for 20 min or 150 °C for 10 min. The method according to the present invention may further comprise a step of: a´) obtaining the first solution comprising an n-type conductive polymer by means of oxidative polymerization and in situ reductive doping in a polar protic or aprotic solvent. The oxidative polymerization may be performed according to the following reaction scheme: The polar protic solvent in step a´) may be water, alcohol, or mixtures thereof. The polar aprotic solvent may be N,N-dimethylformamide, dimethyl sulfoxide, or mixtures thereof. The alcohol may be selected from the group consisting of methanol, ethanol, propan-1-ol, propan-2-ol (IPA), butan-1-ol, 2-methylpropan-1-ol, 2-methylpropan-2-ol, 2-methylbutan-2-ol, ethane-1,2-diol, 2-methoxyethan-1-ol, and 1-methoxypropan-2-ol or mixtures thereof, as illustrated below. Preferably, the non-halogenated polar solvent is ethanol, IPA, methanol or mixtures thereof. The TMQ or AQ act as a catalyst. The surfactant may be selected from polyethylene glycol (PEG), polyvinylpyrrolidone (PVP), polyvinyl alcohol (PVA), sodium polystyrene sulfonate (PSSNa), poly(styrene sulfonate) acid (PSSH), sodium dodecylbenzenesulfonate (DBSNa), polyquaternium-4 (PQ-4), polyquaternium-10 (PQ-10), polydiallyldimethylammonium chloride (PDADMAC), polydiallyldiethylammonium chloride (PDADEAC), TWEEN® 20, TWEEN® 80, κ - The base may be MOH, wherein M is selected from Li+, Na+, K+, Me4N+, Bu4N+ or combination thereof. As mentioned above, the low WF polymeric electrode according to the present invention may be used in an optoelectronic device, such as an organic solar cell. BRIEF DESCRIPTION OF THE DRAWINGS Embodiments of the invention will now be described by way of example with reference to the accompanying drawings, of which: Fig.1 shows the work function and conductivity of n-type PBFDO and p-type PEDOT:PSS with and without PEI modifications; Fig. 2 illustrates current density-voltage curve of the organic solar cell with PBFDO or PBFDO / PEIE as cathode. DETAILED DESCRIPTION OF THE INVENTION As mentioned above, the present invention provides a low-work function polymeric electrode for an optoelectronic device, the electrode comprising: a first film layer comprising an n-type conductive polymer; and a second film layer comprising an n-type polymeric cation. In the embodiment illustrated in the figures, the monomer is 3,7- dihydrobenzo[1,2-b:4,5-b’]difuran-2,6-dione (HBFDO). In such an embodiment, the n- type conducting polymer is poly(benzodifurandione) (PBFDO), having the following structure: The n-type polymeric cation in the embodiments described below is linear polyethyleneimine (PEIlin), branched PEI (PEIbra), or ethoxylated PEI (PEIE). The n-type PBFDO and p-type PEDOT:PSS films were deposited on pre- cleaned glass by spin-coating and annealing in the air. Then the PEI solution was spin- coated on the polymeric films at 5000 rpm for 1 minute to tailor their WF. The WF was measured by Kelvin probe in the air. The conductivity (σ) of the films was calculated ^ from the equation of ^ = where the sheet resistance Rswas measured by four- probe and the thickness (d) was measured by profilometer. Fig.1 illustrates WF and conductivity of n-type PBFDO with and without the second film layer comprising PEI. As may be seen in Fig.1, the WF and conductivity of the first film layer is about 5.30 eV and 700 S / cm, respectively. After the second film layer is provided on the first layer, the WF drops to about 3.98 eV with an insignificant change in conductivity (about 740 S / cm). For comparison, the WF of p-type PEDOT:PSS is reduced from 5.07 to 4.08 eV while the conductivity reduced from about 500 S / cm to 170 S / cm after PEI modification. Such a decrease in conductivity makes PEDOT:PSS unsuitable for application in low WF electrodes. Fig.2 shows current density-voltage curve of an organic solar cell comprising PBFDO / PEIE can act as cathode in organic solar cells. The organic solar cell has the structure cathode / PM6:Y6 / MoO3 / Ag. The PBFDO was deposited on the pre-cleaned glass at 1500 rpm for 2 minutes and annealed at 50oC for 20 minutes. Then the PEIE solution was spin-coated on the PBFDO film at 5000 rpm for 1 minute. The PM6:Y6 solution was prepared by dissolving in chloroform (with 0.5 vol% of 1- chloronaphthalene as additive) with the weight ratio of 7:8.4 mg / ml. Finally, the 10 nm / 100 nm MoO3 / Ag electrode was thermally evaporated with a shadow mask under a vacuum of 1 × 10-6Torr. The effective area of the device was about 4.43 mm2. J-V characteristics of the device were performed by a Paios platform under AM 1.5G illumination (100 mW cm-2) from a solar simulator in the N2-filled glovebox. The devices were measured with a step voltage of 0.02 V. The light intensity was determined by a standard silicon photodiode. As shown in Figure 2, the device with PBFDO / PEIE shows a rectification characteristic under light while the device with PBFDO show a symmetric curve due to its mismatch energy level. Although the present invention has been described with reference to various embodiments, those skilled in the art will recognize that changes may be made without departing from the scope of the invention. It is intended that the detailed description be regarded as illustrative and that the appended claims including all the equivalents are intended to define the scope of the invention.
Claims
CLAIMS 1. A low-work function polymeric electrode for an optoelectronic device, said electrode comprising: a first film layer comprising an n-type conductive polymer; a second film layer comprising an n-type polymeric cation.
2. The electrode according to claim 1, wherein said n-type conductive polymer is poly(benzodifurandione) (PBFDO).
3. The electrode according to claim 1 or 2, wherein said n-type conductive polymer comprises from 2 to 10000, more preferably from 6 to 1000, even more preferably from 3 to 100, most preferably from 5 to 50 repetitive units.
4. The electrode according to any one of the preceding claims, wherein said n- type polymeric cation is poly(ethyleneimine) (PEI), ethoxylated PEI (PEIE) or mixtures thereof.
5. The electrode according to claim 4, wherein said PEI is linear or branched.
6. The electrode according to any one of the preceding claims, wherein said n- type polymeric cation comprises from 5 to 10000, preferably from 10 to 1000, more preferably from 20 to 100 repetitive units.
7. The electrode according to any one of the preceding claims, wherein said first film layer has a work function in the range from 3 to 6 eV, preferably about 5 eV, and wherein said first film layer further has a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm.
8. The electrode according to any one of the preceding claims, wherein said electrode has a work function in the range from 2 to 5 eV, preferably about 4 eV, and wherein said electrode further has a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm.
9. An organic solar cell comprising an electrode according to any one of claims10. A method for manufacturing a low-work function polymeric electrode for an optoelectronic device, said method comprising the steps of: a) depositing a first solution comprising an n-type conductive polymer on a substrate, thus obtaining a first film layer; b) depositing a second solution comprising an n-type polymeric cation on said first film layer thus obtaining a second film layer.
11. The method according to claim 10, wherein the concentration of said n-type conductive polymer in said first solution is from 0.1 to 500 mg / mL, preferably from 1 to 100 mg / mL.
12. The method according to any one of claims 10-11, wherein the concentration of said n-type polymeric cation in said second solution is from 0.01 to 100 mg / mL, preferably from 0.1 to 10 mg / mL.
13. The method according to any one of claims 10-12, wherein said first solution and / or said second solution is deposited by a solution-processed technology.
14. The method according to any one of claims 10-13, wherein said second solution comprises a polar protic or aprotic solvent.
15. The method according to any one of claims 10-14, wherein said method further comprises a step of: a´) obtaining said first solution comprising an n-type conductive polymer by means of oxidative polymerization and in situ reductive doping in a polar protic or aprotic solvent.
Citation Information
Patent Citations
N-type conductive composition comprising a rigid conjugated polymer
WO2022106018A1