An electrode comprising n-doped conductive polymer

The use of a polymeric electrode with an intrinsically doped n-type conductive polymer and a polymeric cation in optoelectronic devices addresses the challenge of achieving high conductivity and stability for low-work function applications, achieving record-high efficiencies and stability in optoelectronic devices.

WO2024236186A1PCT designated stage expired Publication Date: 2024-11-21WESTRA MATERIALS AB

Patent Information

Application Number
PCT/EP2024/063781
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-17
Filing Date
2024-05-17
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Current optoelectronic devices face challenges in achieving high conductivity and stability for low-work function polymeric electrodes, particularly in organic solar cells, where existing materials like PEDOT:PSS suffer from reduced conductivity and stability issues when modified for low-work function applications.

Method used

A low-work function polymeric electrode comprising a first film layer of intrinsically doped n-type conductive polymer and a second film layer of polymeric cation, such as PEIE-modified PBFDO, which maintains high conductivity and stability by minimizing conductivity reduction at the interface, enabling efficient electron transport and optical properties.

Benefits of technology

The solution achieves high power conversion efficiencies comparable to traditional ITO electrodes, with record-high efficiencies of >15.1% under indoor lighting conditions and maintains stability across multiple bending tests, demonstrating a viable alternative for flexible and efficient optoelectronic devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024063781_21112024_PF_FP_ABST
    Figure EP2024063781_21112024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to a low-work function polymeric electrode for an optoelectronic device, comprising: a first film layer comprising an intrinsically doped n-doped conductive polymer; and5 a second film layer comprising a polymeric cation.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] AN ELECTRODE COMPRISING N-DOPED CONDUCTIVE POLYMER TECHNICAL FIELD The present invention relates to a low-work function transparent polymeric electrode for an optoelectronic device. Further, the present invention relates to a method for manufacturing such an electrode. BACKGROUND OF THE INVENTION Both high- and low-work-function (WF) electrodes are vital units in state-of- the-art optoelectronic devices. Conducting polymers are potential candidates for such electrodes due to their high conductivity, flexibility, and solution-processibility. The poly(3,4-ethylenedioxythiophene) doped with polystyrene sulfonate (PEDOT:PSS), being the most common p-type conducting polymer, is widely used as high-WF electrode in solar cells, photodiodes, and light-emitting diodes. Although PEDOT:PSS can be used as low-WF electrode after surface modification with an amine group, such a modification will typically reduce conductivity of the polymer and impair stability of the device. Therefore, low-WF polymeric electrode with high conductivity for high performance optoelectronic devices is still a challenge. Transparent electrodes (TEs) play a crucial role in optoelectronic devices, facilitating the in- and out-coupling of light and charges. Indium tin oxide (ITO) stands out as a benchmark TE in both academic research and industrial applications, owing to its exceptional conductivity and transmittance. Despite its effectiveness, the increasing demand and cost associated with the rare element indium motivate the search for alternative TEs with optimized electrode characteristics and enhance device efficiencies. Various metal oxides, such as zinc oxide (ZnO) and tin oxide (SnO2) have been explored as partial substitutes for ITO electrodes in specific applications. However, these metal-oxide electrodes face limitations for the development of flexible devices due to their mechanical fragility and the requirement for a high-temperature sintering process. In response to these challenges, metallic nanostructures like metal grids and metal nanowires, along with carbon-based materials such as carbon nanotubes and graphene, have emerged as promising alternatives. These materials enable the fabrication of thin and flexible films with low sheet resistance and high transparency. However, their suitability for large-scale applications is hindered by the high surface roughness and intricate synthetic routes. Siedel et al. “Single step formation of a low WF cathode interlayer and n-type bulk doping from semiconducting polymer / polyethyleneimine blend solution”, Applied material and interfaces, vol. 12, no. 25, 2020-05-28 discloses a study on thin films formed by spin-coating blended solutions of PEI and poly{[N,N'-bis(2- octyldodecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-5,5'-(2,2'- bithiophene)} [P(NDI2OD-T2)] on indium tin oxide. Vertical phase separation was observed in such films, where PEI accumulates at the bottom and the top, sandwiching the semiconductor layer, thus forming a self-organized low WF cathode interlayer. Although bulk conductivity of the material is increased by four orders of magnitude, the conductivity is still very low (2·10-3S / cm), making the material unsuitable as an electrode. For such an application, the conductivity should be as high as possible, but at least 100 S / cm. Conducting polymers are highly promising materials for TEs, combining the advantageous features of both polymers (such as solution processability, mechanical flexibility, lightweight, and chemical versatility) and metals (electrical conductivity). Although the several conducting polymers achieved high conductivity over 1000 S cm–1which is close to that of ITO, their applicability in TE is severely restricted by the precisely doping process and lack of stability. Owning to its high stability under high doping level and solution-processibility, poly(3,4- ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS) is widely utilized as the TE in various optoelectronic devices like solar cells and light-emitting diodes, primarily serving as a high work function (WF) electrode to extract / inject holes from the active layer due to its suitable WF. When a PEDOT:PSS electrode is used to inject / extract electrons, an additional low-WF modifier or interlayer is needed to reduce its WF. However, these modifiers or interface layers often contain amine groups, such as poly(ethyleneimine) (PEI), polyethylenimine ethoxylated (PEIE), and ethanolamine- based sol-gel ZnO precursors, leading to the chemical reduction of PEDOT:PSS (i.e., low doping level) during the modifier / interlayer deposition process. This de-doping process increases its sheet resistance and decreases transparency in the visible region, resulting in poor device performance. While various strategies, such as passivation of amine by metal chelation and novel precursor engineering, can mitigate this undesirable interface reaction, there is still a pressing need to explore chemically stable conducting polymers to act as low-WF electrodes. Recently, an n-type conducting polymer poly(benzodifurandione) (PBFDO) was developed by an innovative combination of oxidative polymerization and in situ reductive doping processes. PBFDO exhibit a high conductivity of 2000 S cm–1due to its high doping level, comparable to commercial p-type PEDOT:PSS formulations and was successfully applied in thermoelectric devices and as active channel material in organic electrochemical transistors. Besides, its solution-processibility and excellent stability in air and harsh acid or base conditions make it an alternative as TE in multijunction devices. However, its mismatched work function, e.g., 4.4-4.7 eV, diminishes its efficiency in extracting electrons from commonly used organic solar cell (OSC) materials, hampering its application as low WF electrode in diode based devices. SUMMARY OF THE INVENTION In view of the above, the present invention aims to solve the problems of the prior art. To this end, the present invention relates to a low-work function polymeric electrode for an optoelectronic device, the electrode comprising: a first film layer comprising an intrinsically doped n-type conductive polymer; and a second film layer comprising a polymeric cation. In order for the n-type conducting polymer to be useful in organic solar cells, it should fulfil three criteria: high bulk conductivity, low work function and high transparency. The conductivity of the intrinsically doped n-type conducting polymer should be at least 100 S / cm. When the intrinsically doped n-type conducting polymer comes in contact with the polymeric cation, the conductivity of the n-type conductive polymer is reduced. Therefore, applying the n-type conductive polymer and the polymeric cation polymeric cation as two distinct layers offers the advantage of minimizing thus drawback. In other words, conductivity of the n-type conducting polymer is reduced only at the interface between the first and the second layer, while bulk conductivity of the entire electrode remains unaltered. It has been shown that treating intrinsically non-doped n-type conducting polymer with a polymeric cation, e.g. an amine-based polymeric cation, yields high conductivity. However, the inevitable electron transfer between the polymeric cation and the n-type conducting polymer also leads to a chemical reduction of the latter (i.e. increased doping level), which forces the n-type conducting polymer out of their thermodynamic equilibrium, thus affecting their ambient stability. The use of a polymeric cation on intrinsically doped n-type conducting polymers, such as the recently reported (PBFDO), would not alter their charge carrier density, and thus intrinsic electrical conductivity and optical properties, but would instead only influences their energetics, thus enabling the development of a low WF transparent electrode with ideal and stable electrical, optical, and electronic properties. The second film layer may be deposited on the first film layer to lower the work function of the electrode. Further, at least one additional layer may be present between the first and the second film layers. Such an additional layer may be an n- type inorganic oxide such as ZnO, SnO2, TiO2 or mixtures thereof. The thickness of the first film layer may be in the range from 10 nm to 1 μm, depending on the deposition technology used during manufacturing of the electrode. In particular, the thickness of the first film layer may be in the range from 20 nm to 50 nm. The thickness of the second film layer should be kept at a minimum due to its poor conductivity. In particular, the thickness of the second layer may be in the range from 0.1 nm to 50 nm, preferably from 1 nm to 30 nm. It should be noted that the polymeric electrode according to the present invention offers the advantage of comprising a two-in-one electron transport layer (ETL) and TE, based on films of an intrinsically doped n-type conductive polymer modified with a polymeric cation. The conductivity of the n-type conductive polymer may be at least 500 S / cm, more preferably at least 1000 S / cm, and most preferably at least 1500 S / cm. In particular, polyethylenimine ethoxylated (PEIE) may be used to modify poly(benzodifurandione) (PBFDO). These PEIE-modified PBFDO layers exhibit a unique combination of properties, including low sheet resistance (130 Ω sq–1), low work function (4.2 eV), and high optical transparency (>85% in the UV-Vis-NIR range). In contrast to commonly used poly(3,4- ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS), the doping level of the n-type conductive polymer remains unaffected by the treatment with the polymeric cation, as verified through UV-Vis-NIR absorption and X-ray photoelectron spectroscopy measurements. When employed as a two-in-one ETL / TE in organic solar cells, the polymeric electrode of the present invention exhibits performance comparable to conventional ITO electrodes. Moreover, the inventors demonstrate all- plastic solar cells with record-high power conversion efficiencies of >15.1% under indoor lighting conditions. The monomer in the n-type conductive polymer may be in the form of a heterocyclic moiety having a central symmetrical benzene ring fused with at least one, preferably at least two rings, preferably five-membered rings. The monomer further comprises an active hydrogen and at least one electron-withdrawing group at the benzylic position. In particular, the monomer may be 3,7-dihydrobenzo[1,2-b:4,5- b']difuran-2,6-dione (HBFDO), 5,7-dihydropyrrolo[2,3-f]indole-2,6(1H,3H)-dione, or 3,7-dihydrobenzo[1,2-b:4,5-b']dithiophene-2,6-dione. In particular, the monomer is 3,7-dihydrobenzo[1,2-b:4,5-b’]difuran-2,6-dione (HBFDO). In such an embodiment, the n-type conducting polymer is poly(benzodifurandione) (PBFDO), having the following structure: The n-type conductive polymer may comprise from 2 to 10000, more preferably from 6 to 1000, even more preferably from 3 to 100, most preferably from 5 to 50 repetitive units. The polymeric cation according to the present invention is preferably linear polyethyleneimine (PEIlin), branched PEI (PEIbra), ethoxylated PEI (PEIE) or mixtures thereof. The number of repetitive units in the polymeric cation may be from 5 to 10000, preferably from 10 to 1000, more preferably from 20 to 100 repetitive units. When the polymeric cation is branched PEI, a, b, c and d are positive integers, such that the sum of these integers is from 5 to 10000, preferably from 10 to 1000, more preferably from 50 to 100. When the polymeric cation is ethoxylated PEI, x, y and z are positive integers, such that the sum of these integers is from 5 to 10000, preferably from 10 to 1000, more preferably from 50 to 100. According to the present invention, the polymeric cation modifies the work function of the n-type conductive polymer. In other words, the conductivity of the first film layer is negligibly affected by addition of the second film layer since the n-type conductive polymer of the first film layer already has high conductivity. The first film layer may have a work function in the range from 3 to 6 eV, preferably about 5 eV. Further, the first film layer may have a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm. The electrode may have a work function in the range from 2 to 5 eV, preferably about 4 eV. Further, the electrode may have a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm. The present invention further relates to an organic solar cell comprising an electrode as described above. The organic solar cell may have a structure comprising a cathode, an electron transport layer (ETL), an active layer, a hole transport layer (ETL) and an anode. In particular, the low WF polymeric electrode as described above may act as cathode or as a two-in-one TE and ETL. The inventors demonstrate all- plastic solar cells with record-high power conversion efficiencies of >15.1% under indoor lighting conditions, as will be described in greater detail below. The present invention further relates to a method for manufacturing a low- work function polymeric electrode for an optoelectronic device, the method comprising the steps of: a) depositing a first solution comprising an intrinsically doped n-type conductive polymer on a substrate, thus obtaining a first film layer; b) depositing a second solution comprising a polymeric cation on the first film layer thus obtaining a second film layer. The substrate may be rigid or flexible. By the term “rigid” is understood as being deficient in or devoid of flexibility. By the term “flexible” is understood as being supple enough to bend freely or repeatedly without breaking. Further, the substrate may be transparent or opaque. By the term “transparent” is understood as having the property of transmitting light without appreciable scattering so that bodies lying beyond are seen clearly. By the term “opaque” is understood as blocking the passage of radiant energy and especially light. In particular, the substrate may be manufactured of glass, polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethersulfone (PES) or mixtures thereof. It should be mentioned that there should be at least one transparent electrode in a solar cell in order to allow the solar radiation to enter the solar cell. The concentration of the n-type conductive polymer in the first solution may be from 0.1 to 500 mg / mL, preferably from 1 to 100 mg / mL. The solvent used for preparing the first solution may be a polar aprotic solvent, a polar protic solvent or a mixture thereof. In particular, the solvent may be DMSO, DMF, water or mixture thereof. The concentration of the polymeric cation in the second solution may be from 0.01 to 100 mg / mL, preferably from 0.1 to 10 mg / mL. The second solution may comprise a polar protic or aprotic solvent. The polar protic solvent may be water, alcohol or mixture thereof. The alcohol may be selected from the group consisting of methanol, ethanol, propan-1-ol, propan-2-ol (IPA), butan-1-ol, 2-methylpropan-1-ol, 2-methylpropan-2-ol, 2-methylbutan-2-ol, ethane-1,2-diol, 2-methoxyethan-1-ol, and 1-methoxypropan-2-ol or mixtures thereof, as illustrated below. In particular, the alcohol is ethanol, IPA, methanol or mixtures thereof. According to the present invention, the first solution and / or the second solution may be deposited by a solution-processed technology, such as spin-coating, drop-casting, spray-coating, inkjet-printing and screen-printing. The first and / or the second solutions of the present invention may be deposited in air and ambient temperature, forming the film having thickness of from 10 nm to 1 μm. The thermal annealing may be performed at temperatures from 40°C to 200 °C for periods from 1 min to 1200 min. Preferably, thermal annealing is performed at 50°C for 20 min or 150 °C for 10 min. The method according to the present invention may further comprise a step of: a´) obtaining the first solution comprising an intrinsically doped n-type conductive polymer by means of oxidative polymerization and in situ reductive doping in a polar protic or aprotic solvent. The oxidative polymerization may be performed according to the following reaction scheme using duroquinone (TMQ) as catalyst, as disclosed in CN115651448: The polar protic solvent in step a´) may be water, alcohol, or mixtures thereof. The polar aprotic solvent may be N,N-dimethylformamide, dimethyl sulfoxide, or mixtures thereof. The alcohol may be selected from the group consisting of methanol, ethanol, propan-1-ol, propan-2-ol (IPA), butan-1-ol, 2-methylpropan-1-ol, 2-methylpropan-2-ol, 2-methylbutan-2-ol, ethane-1,2-diol, 2-methoxyethan-1-ol, and 1-methoxypropan-2-ol or mixtures thereof, as illustrated below. Preferably, the non-halogenated polar solvent is ethanol, IPA, methanol or mixtures thereof. The TMQ or AQ act as a catalyst. The surfactant may be selected from polyethylene glycol (PEG), polyvinylpyrrolidone (PVP), polyvinyl alcohol (PVA), sodium polystyrene sulfonate (PSSNa), poly(styrene sulfonate) acid (PSSH), sodium dodecylbenzenesulfonate (DBSNa), polyquaternium-4 (PQ-4), polyquaternium-10 (PQ-10), polydiallyldimethylammonium chloride (PDADMAC), polydiallyldiethylammonium chloride (PDADEAC), TWEEN® 20, TWEEN® 80, κ - Carrageenan, PEG-PPG-PEG, Polyoxyethylene (10) tridecyl ether, Triton™ X-100 or combination thereof.

[0002] The base may be MOH, wherein M is selected from Li+, Na+, K+, Me4N+, Bu4N+ or combination thereof. Alternatively, the n-type conductive polymer may be manufactured using a quinone comprising a branched side chain having at least one chiral center, as disclosed in PCT / EP2023 / 063322: PBFDO n=6 to 10000, 0<m<n BRIEF DESCRIPTION OF THE DRAWINGS Embodiments of the invention will now be described by way of example with reference to the accompanying drawings, of which: Fig.1 shows (a) Chemical structures of PEDOT:PSS, PBFDO, and PEIE. (b) Secondary electron cutoff spectra of PEDOT:PSS and PBFDO films before and after PEIE treatment. Current-voltage characteristics of (c) PEDOT:PSS and (d) PBFDO films modified by PEIE solution with different concentrations; Fig. 2 illustrates work function of PEDOT:PSS and PBFDO films with and without PEIE surface modification as measured by Kelvin probe in ambient. The error bars indicate SD based on 30 measurements; Fig.3 depicts UPS spectra for (a) PEDOT:PSS and (b) PBFDO films before and after deposition of the ethanolamine based ZnO precursor. Current-voltage curves of (c) PEDOT:PSS and (d) PBFDO films before and after deposition of the ethanolamine-based ZnO precursor; Fig 4 shows sheet resistance of (a) PEDOT:PSS and (b) PBFDO film modified by PEIE solution (with different concentrations), as extracted from the current-voltage curves in Fig.1c-d; Fig.5 illustrates absorption spectra of (a) PEDOT:PSS and (b) PBFDO films before and after treatment with 1 wt% PEIE solution. The absorption was obtained from transmittance and reflectance in Figure 6. Photographs of the corresponding films are shown in the insets. (c) S(2p) XPS spectra of PEDOT films and (d) O(1s) XPS spectra of PBFDO films before and after modification with PEIE; Fig.6 shows transmittance and reflectance spectra of PEDOT:PSS (a-b) and PBFDO (c-d) films before and after modification with PEIE (1 wt%); Fig. 7 illustrates XPS N(1s) spectra of (a) PEIE, (b) PEIE-modified PEDOT:PSS, and (c) PEIE-modified PBFDO films. The peak of protonated amine increased after PEIE modification, indicating the interaction between PEIE and conducting polymer; Fig. 8 depicts EPR spectra of (a) PEDOT:PSS and (b) PBFDO films at different concentrations of PEIE; Fig.9 illustrates AFM images of (a) PBFDO and (b) PEIE-modified PBFDO films on glass substrate. The scale bar is 200 nm; Fig.10 depicts AFM images of PBFDO films on flexible PET substrate without (a) bending and with (b) 100-times bending and (c) 1000-times bending. AFM images of PEIE-modified PBFDO films on flexible PET substrate without (d) bending and with (e) 100-times bending and (f) 1000-times bending. The scale bar is 400 nm and the bending radius is 2.5 mm @ 180o; Fig.11 shows the conductivity of PBFDO and PEIE-modified PBFDO films on PET substrate after bending test. The bending radius is 2.5 mm @ 180o; Fig.12 depicts 2D GIWAXS patterns of (a) PBFDO, (b) PBFDO / PEIE, and (c) PEIE. In-plane (d) and out-of-plane (e) GIWAXS line cuts of PBFDO, PEIE, and PBFDO / PEIE films; Fig. 13 shows the contact angle of water droplet on (a) PBFDO, (b) PEIE- modified PBFDO film and (c) ZnO ETL; Fig.14 shows the thermogravimetric analysis (TGA) of (a) PBFDO, (b) PEIE- modified PBFDO and (c) PEIE; Fig.15 depicts the differential scanning calorimetry of (a) PBFDO, (b) PEIE- modified PBFDO and (c) PEIE; Fig.16 illustrates (a) Chemical structures of the active layer materials and (b) device configurations used in this work. Current density-voltage characteristics of (c) rigid OSCs under AM 1.5G and (d) all-plastic solar cells under 552 lux illumination; Fig.17 shows the J-V curve of PEIE-modified PBFDO as two-in-one electrode with different PEIE concentrations; Fig.18 depicts J-V characteristics of the rigid OSCs with polymeric TE and sol-gel ZnO as ETL under AM 1.5 G; Fig. 19 illustrates EQE spectra of OSCs with PBFDO as the transparent electrode. The integrated JSC is consistent with the JSC extracted from Figure 16c; Fig.20 shows fraction of light absorbed as calculated using the transfer matrix formalism incorporated in an in-house script based on the work of Burkhard et al. The simulated device stack consisted of glass / PBFDO (50 nm) / PEIE (5 nm) / PM6:Y6 (100 nm) / MoO3 (10 nm) / Ag (100 nm). The n and k value of material were obtained from literature; Fig.21 shows J-V curves of the device under AM 1.5G condition. The device structure is glass / PBFDO / PM6:Y6 / MoO3 / Ag; Fig.22 illustrates J-V curves of the reference device under AM 1.5G condition. The structure of the reference device is glass / ITO / PEIE or ZnO / PM6:Y6 / MoO3 / Ag; Fig.23 depicts the transmittance of PEIE-modified ITO and PBFDO electrode; Fig.24 illustrates photon flux (black line) and integrated current density (red line) of the LED lamp used in this work. The illuminance was obtained at about 552 lux by integrating spectral power; Fig. 25 shows stability of the all-plastic devices under 70oC and indoor conditions. The devices were stored in N2-filled glovebox without encapsulation; Fig. 26 depicts the mechanical stability of all-plastic devices, where the bending radius is 4.0 mm @ 180°. DETAILED DESCRIPTION OF THE INVENTION As mentioned above, the present invention provides a low-work function polymeric electrode for an optoelectronic device, the electrode comprising: a first film layer comprising an intrinsically doped n-type conductive polymer; and a second film layer comprising a polymeric cation. In the embodiment illustrated in the figures, the monomer is 3,7- dihydrobenzo[1,2-b:4,5-b’]difuran-2,6-dione (HBFDO). In such an embodiment, the n- type conducting polymer is poly(benzodifurandione) (PBFDO), having the following structure: The polymeric cation in the embodiments described below is linear polyethyleneimine (PEIlin), branched PEI (PEIbra), or ethoxylated PEI (PEIE). The n-type PBFDO and p-type PEDOT:PSS films were deposited on pre- cleaned glass by spin-coating and annealing in the air. Then the PEI solution was spin- coated on the polymeric films at 5000 rpm for 1 minute to tailor their WF. The WF was measured by Kelvin probe in the air. The conductivity (σ) of the films was calculated ^ from the equation of ^ =s where the sheet resistance R was measured by four- probe and the thickness (d) was measured by profilometer. PEDOT:PSS (CleviosTM PH 1000) was purchased from Heraeus. 5% ethylene glycol was added to PEDOT:PSS to further improve the conductivity. PBFDO was synthesized from dimethyl sulfoxide (DMSO) solution following a procedure reported previously. PEIE was purchased from Sigma-Aldrich, and the active layer materials in OSCs were purchased from 1-Material Inc. UPS and XPS spectra were acquired using a Scienta ESCA 200 system equipped with a SES 200 electron analyzer in a vacuum of 1 × 10-10 mbar. A monochromatic Al Ka X-ray source (1486.6 eV) and a helium discharge lamp (21.22 eV) were used for XPS and UPS measurements. All spectra were collected at normal emission and were calibrated by a sputter-cleaned Au film with the Fermi level at 0 eV and the Au 4f peak at 84.0 eV. Kelvin probe measurements were performed using a scanning Kelvin Probe (SKP5050) in ambition conditions. The samples were spin-coated on a clean glass substrate and a highly ordered pyrolytic graphite with a WF of 4.6 eV was used for calibration. The statistical results are calculated from 30 measurements. Transmittance (T%) and reflectance (R%) spectra were measured with a UV- Vis-NIR spectrophotometer (PerkinElmer Lambda 950) with a step of 2 nm, respectively. The absorption (A%) spectrum was calculated with the equation of A = 100-T-R. Quantitative EPR measurements were performed with SPINSCAN X in dark conditions at room temperature. The PEDOT:PSS and PBFDO film were drop-casted on a quartz substrate and then loaded into sealed quartz tubes. Electrical characterization: Electrical conductivity measurements were performed by four probe techniques in ambient conditions. The I-V curves were recorded by a Keithley 4200-SCS semiconductor characterization system. Thin-film morphology characterization: The AFM images were obtained by a Bruker Dimension Icon XR in tapping mode using a silicon nitride cantilever with a spring constant of 40 N m-1. The GIWAXS diffraction patterns were collected at a photon energy of 11.08 eV at an incidence angle of 0.12oat Beamline 9A in the Pohang Accelerator Laboratory (South Korea). All samples were characterized in vacuum, and the exposure time was 10 s. Thermal analysis: The thermal gravity analyses (TGA) were measured by a TA Instrument Q500 analyzer under N2with the heating rate of 10oC min−1. The differential scanning calorimetry (DSC) analyses were measured by TA Instruments Discovery DSC250 under N2. The samples were heated and cooled between 20 and 250oC at a heating / cooling rate of 10oC min−1. The materials were drop-cast on the glass substrate and peeled off for measurement. OSC fabrication and characterization: The rigid OSCs were fabricated in a configuration of glass / PEIE-modified polymeric TE / PM6:Y6 / MoO3 / Ag. The polymeric electrode was deposited on pre-cleaned glass substrates via off-center spin-coating. The PEDOT:PSS electrode was annealed at 150 °C for 10 min, while the PBFDO electrode was annealed at 50 °C for 20 min and 150 °C for 10 min. The thickness of PEDOT:PSS and PBFDO is about 120 and 40 nm, respectively, measured by stylus profilers (Dektak XT Bruker). The optical transmittance of PBFDO films as a function of film thickness is shown in Figure S25. The PEIE (0.1 wt% in H2O) solution was then spin-coated on the polymeric electrode and annealed at 150 °C for 10 min. For the sol-gel-based device, the deposition of the ZnO layer was performed following the previous reports. The active layer was then spin-coated from PM6:Y6 solution (7:8.4 mg ml-1 in chloroform with 0.5 vol% of 1-chloronaphthalene as additive) at 2500 r.p.m. and annealed at 100oC for 10 minutes in the N2-filled glovebox. Finally, MoO3 (10 nm) / Ag (100 nm) electrode was evaporated under a vacuum of 5 × 10-7Torr. The effective area of the device is about 4.3 mm2, confirmed by a shadow mask. The all-plastic devices were fabricated via solution processing and lamination technology following previous reports, except for the PEIE-modified PBFDO as the cathode electrode, which was deposited as described above. For the devices illuminated under AM 1.5G, the J-V curves were recorded by a Paios platform in the N2-filled glovebox with a step voltage of 0.02 V. The light intensity (100 mW cm-2) was determined by a standard silicon photodiode. For indoor devices, the J-V curves were acquired using a Keithley 2400 source meter while the devices were under cool LED irradiation at room temperature. The LED source's emission spectra and irradiance were measured using a high-precision fiber optics spectrometer (QE-Pro, Ocean Optics) and a Hamamatsu silicon photodiode (S1133- 01). By integrating the corresponding emission spectrum obtained from the specific device location, the illuminance, power density, and current density were calculated as 552 lux, 148 µW / cm2, and 67 µA / cm2, respectively. The EQE spectrum was recorded by a Newport Merlin lock-in amplifier. PBFDO has recently emerged as a notable example of n-type conducting polymers, boasting an impressive electrical conductivity that exceeds 2000 S cm–1, comparable to commercial p-type PEDOT:PSS formulations. Similar to PEDOT:PSS, PBFDO is transparent in the visible spectrum and possesses a high WF exceeding 5 eV, rendering it stable in ambient conditions. However, while this high WF is advantageous in stability, it diminishes its efficiency in extracting electrons from commonly used OSC materials, hampering its application as ETL. To address this limitation, an ultrathin layer (< 10 nm) of PEIE was deposited on top of PBFDO to induce a shift of the WF toward lower energies. This shift was confirmed through ultraviolet photoemission spectroscopy (UPS, Figure 1b) and Kelvin probe measurements conducted in ambient conditions (Figure 2), which indicated a transition from 5.03 eV for pristine PBFDO to 4.21 eV for PEIE-modified PBFDO. For comparison, the application of an ultrathin layer of PEIE on PEDOT:PSS yields a similar WF shift, with the WF changing from 5.14 eV for pristine PEDOT:PSS to 3.97 eV for PEIE-modified PEDOT:PSS (Figure 1b). A similar trend is observed when coating commonly used sol-gel ethanolamines-based ZnO precursors containing ethanolamines on top of PEDOT:PSS and PBFDO films, with their WF shifting from ~5.0 eV to ~3.9 eV for both polymers upon treatment (Figure 3a-b). In stark contrast to PEDOT:PSS, the application of PEIE on top of PBFDO does not induce any change in sheet resistance, which instead remains relatively constant at around 138.7 ± 5.5 Ω sq–1regardless of the PEIE concentration (i.e., PEIE film thickness), as shown in Figure 1c-d and Figure 4. Similarly, applying the sol-gel ethanolamines-based ZnO precursors to coat both PEDOT:PSS and PBFDO films induces a 10× increase in sheet resistance of PEDOT:PSS, while that of PBFDO remains constant (Figure 3c-d). Since the electrical properties of conducting polymers are intricately tied to their optical characteristics, the absorption properties of PEDOT:PSS and PBFDO before and after PEIE treatment were measured to investigate the effect of PEIE on their doping level. As illustrated in Figure 5a, the absorption spectrum of pristine PEDOT:PSS films features a broad absorption band extending far into the infrared region, attributed to polaron / bipolaron absorptions. Upon depositing PEIE on PEDOT:PSS, the absorption band in the region 500-1100 nm increases while the extended absorption band at wavelengths larger than 1200 nm decreases. The alteration is visually apparent in the optical photograph reported as an inset to Figure 5a, where the color of the PEDOT:PSS films transitions from light blue to dark blue, providing clear evidence of dedoping. Conversely, PBFDO films exhibit negligible changes in absorption and color after PEIE modification (Figure 5b), suggesting that the doping level of PBFDO remains largely unaltered. The corresponding transmittance and reflectance spectra are reported in Figure 6 for a detailed analysis. Dedoping is observed for PEDOT:PSS films after PEIE modification: the transmittance decreases in the range of 400-1100 nm and increases at wavelengths >1100 nm. In stark contrast, the transmittance of PEIE-modified PBFDO films increases in the visible-infrared range, as shown in (c). We attributed this shift to the differences in the refractive indices of PBFDO (0.6 to 1.4) and PEIE (about 1.6). PEIE acts as an anti- reflective layer (reflectance spectra in d), having a similar effect to the commonly used dielectric-metal-dielectric transparent electrode. The refractive index of PEDOT:PSS is about 1.5-1.6, on par with that of PEIE. Next, X-ray photoelectron spectroscopy (XPS) studies were conducted to gain a deeper understanding of how the PEIE treatment affects the reduction / oxidation state of PBFDO and PEDOT:PSS films. As shown in Figure 5c, the S(2p) signal in the pristine PEDOT:PSS film can be divided into two components. The first at lower binding energy (167-163 eV) originates from the thiophene group in the PEDOT chain, while the second at higher binding energy (171-167 eV) arises from the sulphonate group in the PSS chain. Deconvolution of the PEDOT component reveals a strong asymmetric doublet, characterized by a tail extending toward higher binding energies. This asymmetry is indicative of the presence of positive charges delocalized over the PEDOT chains, resulting in a change in the electronic environment near the sulfur atom. Following PEIE modification, the signal of the PEDOT component decreases compared to that of the PSS component, and the asymmetric tail becomes weaker. These changes suggest a significant decrease in the oxidation (doping) level of PEDOT upon PEIE treatment. The N(1s) signal, presented in Figure 7, exhibits a prominent peak at around 402.3 eV, attributed to positively charged amines formed during the de-doping process. The de-doping of PEDOT:PSS is further confirmed by electron paramagnetic resonance (EPR) spectroscopy measurements (Figure 8), showing a gradual decrease of the EPR signal with increasing PEIE concentration. For PBFDO, the O(1s) signal originates from the lactone group. In the n- doped PBFDO, protons are expected to compensate for the negative charges on the polymer backbone, causing the O(1s) signal from the carbonyl group to shift toward higher binding energies. The reduction level of PBFDO can be evaluated by assessing the peak area of the protonated carbonyl group at 534.5 eV and the pristine carbonyl group at 531.3 eV. As shown in Figure 5d, the signal ratio of two carbonyl groups remains nearly unchanged after PEIE modification, indicating that the reduction level of PBFDO film does not change with the treatment. The EPR signal of PBFDO films is not affected by the PEIE treatment and remains independent of the PEIE concentration (Figure 8). The morphology and microstructure of PEIE-modified PBFDO films were also examined. Atomic force microscopy (AFM) images, presented in Figures 9 and 10, reveal that both PBFDO and PEIE-modified PBFDO films exhibit a smooth and uniform surface, which is advantageous for the fabrication of multi-layer thin-film devices. After 1000-times bending test, the roughness of the film will slightly increase (Figure 10) and maintain over 90% of the conductivity (Figure 11). Grazing-incidence wide-angle X-ray scattering (GIWAXS) reveals that PBFDO chains primarily adopt an edge-on orientation with respect to the substrate in pristine films (Figure 12), with a strong lamellar (100) peak at Qz = 0.579 Å-1(d-spacing = 10.839 Å) and a π–π stacking (010) peak at Qxy = 1.877 Å-1(d-spacing = 3.347 Å). This tightly packed microstructure is attributed to the absence of side chains and the high planarity of the PBFDO polymer backbone. Following PEIE treatment, the PBFDO / PEIE bilayer largely maintains the diffraction pattern of the original PBFDO. Note that the diffraction pattern of pure PEIE shows a broad ring, characteristic of a disordered system (Figure 10). The wettability of PBFDO and PEIE-modified PBFDO films was presented in Figure 13 and the thermal analysis of PBFDO and PEIE-modified PBFDO were presented in Figure 14 and 15. The contact angle decreases from 32.93oof PBFDO to 10.91oof PEIE- modified PBFDO indicated the successful surface modification of PBFDO due to the hydrophilicity of PEIE (Fig.13 a and b). As a comparison, the contact angle of water droplet of the (c) common-used ZnO ETL is about 39.07o. Although PEIE-modified PBFDO show a poorer thermal stability than PBFDO due to the quick decomposition of PEIE between 260-350o. But all of them show nearly no mass loss below 200oC, which is compatible with most of flexible substrate (e.g., 140oC for PET and 170-180oC for PEN, Fig.14). The heating rate is 10oC min−1. As is evident from Fig.15, no obvious exothermic or endothermic behavior was observed in the range of 20 - 250oC at heating / cooling rates of 10 / 10oC min−1. The high electrical conductivity, transparency in the visible range, and low- WF of PEIE-modified PBFDO enable it to function simultaneously as an ETL and a TE. The application of PEIE-modified PBFDO as a two-in-one electrode in OSCs having the active layer and device structures presented in Figure 16a-b was investigated. Rigid solar cells with structure glass / PEIE-modified PBFDO / PM6:Y6 / MoO3 / Ag were fabricated following the procedure outlined above. The current density-voltage (J-V) characteristics, tested under 100 mW cm−2AM 1.5G illumination and reported in Figure 16c, reveal a PCE of 12.1% (VOC = 0.81 V, JSC = 22.46 mA cm-2, and FF = 0.66). The performance of devices with different PEIE concentration were present in the Figure 17. Similar results are achieved when PBFDO is modified with sol-gel amine-based ZnO precursors, yielding OSCs with PCE of 13.35% (VOC = 0.83 V, JSC = 22.65 mA cm-2, and FF = 0.71, see Figure 18). The JSC was further confirmed by external quantum efficiency (EQE) measurements (Figure 19) and optical modeling (Figure 20). For comparison, devices featuring pure PBFDO (without PEIE) as the TE exhibit no photovoltaic behavior, a phenomenon we attributed to the relatively high WF of PBFDO itself (see Figure 21). Additionally, we compared the device characteristics of identical OSCs comprising PEIE-modified PEDOT:PSS as the TE and observed PCE < 2% (Figure 16c). The inventors attributed this to the de-doped PEIE-modified PEDOT:PSS. The J-V characteristics of reference devices with ITO electrodes are presented in Figure 22 and show PCEs of about 13.99% (VOC = 0.81 V, JSC = 25.40 mA cm-2, and FF = 0.69) for PEIE-modified ITO electrodes and 15.40% (VOC = 0.83 V, JSC = 25.42 mA cm-2, and FF = 0.73) for ZnO-modified ITO electrodes. The device’s photovoltaic parameters are summarized in 1. While the ITO-based device shows a higher JSC due to its relatively higher transmittance (Figure 23), the similar VOC and FF suggest that the sheet resistance of PEIE-modified PBFDO electrode is sufficiently low to effectively extract electrons from the active layer.

[0003] Table 1. The photovoltaic parameters of OSCs in this work. The devices were illuminated under AM 1.5G. The values in parentheses are the statistical results from 16 devices. VOC JSC PCE Structure FF (V) (mA cm-2) (%) 0.83 25.42 0.73 15.40 Glass / ITO / ZnO / PM6:Y6 / MoO3 / Ag (0.82±0.01) (24.96±0.41) (0.70±0.02) (14.67±0.56) 0.81 25.40 0.68 13.99 Glass / PEIE-modified ITO / PM6:Y6 / MoO3 / Ag (0.80±0.01) (24.67±0.45) (0.66±0.02) (13.23±0.63) 0.83 22.65 0.71 13.35 Glass / PBFDO / ZnO / PM6:Y6 / MoO3 / Ag (0.81±0.02) (22.14±0.57) (0.68±0.03) (12.58±0.69) 0.81 22.46 0.66 12.07 Glass / PEIE-modified PBFDO / PM6:Y6 / MoO3 / Ag (0.79±0.02) (21.78±0.65) (0.61±0.04) (11.21±0.83) Glass / PEDOT:PSS / ZnO / PM6:Y6 / MoO3 / Ag0.69 13.33 0.21 1.93Glass / PEIE-modified PEDOT:PSS / PM6:Y6 / MoO3 / Ag0.67 8.17 0.24 1.315 The present invention thus demonstrates flexible, all-organic solar cells using the lamination approach described in the Experimental Section (Figure 16b). In brief, PEIE-modified PBFDO was deposited on a PET foil and used as the low-WF electrode, while PEDOT:PSS deposited on another PET foil, served as the high-WF electrode. A 10 blend of PTQ10:PC61BM was utilized as the active layer and deposited on each PET sheet before the two were laminated on top of each other. PTQ10 and PC61BM were chosen for their high stability and potentially low-cost upscale fabrication. Besides, their absorbance matches the spectrum of indoor LED emission (Figure 24). The resulting all-organic solar cells exhibited a PCE of 15.1% (VOC= 0.78 V, JSC= 42.7715μA cm-2, and FF = 0.67) under 552 lux illumination conditions (Figure 16d). Remarkably, the all-organic solar cells retained close to 90% of their initial efficiency after 264 hours at 70 °C and indoor conditions (Figure 25) and could be bent 1000 times to a bending radius of 4.0 mm without any performance loss (Figure 26). These figures of merit are among the highest reported for all-organic solar cells tested under20 indoor lighting conditions (see Table 2 for a survey of the field). Table 2. The summary of all-organic devices PC Structure substrate illumination E (%) PEIE-modified PBFDO / PTQ10:PC61BM / PEDOT:PSS PET 552 lux 15.1 H3PO4−PEDOT: PSS / PEI / P3HT: ICBA / EG-PEDOT: PSS PES 100 mW cm−23.3 PEDOT:PSS / PEI / P3HT:ICBA / PEDOT:PSS 100 mW cm−22.8 PH1000 / PEI / P3HT:ICBA / PEDOT:PSS-m13 / PEI / PTB7- PES 100 mW cm−26.1 Th:PC61BM / PEDOT:PSS PEDOT: PSS / P3HT: ICBA: PEI / PEDOT: PSS PES 100 mW cm−23.3 HC-PEDOT: PSS / PEI / P3HT: ICBA / EG-PEDOT: PSS PES 100 mW cm−24.05 PH1000 / PEI / P3HT:ICBA / PEDOT PES 100 mW cm−23.0 PH1000 / PEIE / P3HT: IDT-2BR PES 100 mW cm−22.88 PEDOT:PSS / PEIx / TQ1:PC61BM / PEDOT:PSS PET 100 mW cm−21.70 low-WF PEDOT:PSS / P3HT:ICBA / high-WF PEDOT:PSS Glass 100 mW cm−24.0 low-WF PEDOT:PSS / P3HT:ICBA / high-WF PEDOT:PSS Glass 100 mW cm−23.1 hc-PEDOT:PSS-TBA / PM6:IT-4F / PEDOT:PSS Glass 100 mW cm−27.82 H2SO4 / EG-PEDOT:PSS / PM6:Y6 / PDINO / PEDOT:PSS Glass 100 mW cm−28.93 In conclusion, it has been demonstrated that treating the n-type conducting polymer, e.g. PBFDO, with an ultrathin layer of polymeric cation, e.g. PEIE, maintain the high doping level and highest conductivity (close to 2000 S cm-1) as well as low WF (4.2 eV). These unique features allow us to make transparent (>85% in the UV- Vis-NIR spectral region) two-in-one electrode with low sheet resistance (130 Ω sq–1) outperforming conventional polymeric ETL materials. Importantly, the doping level of PBFDO is not affected by PEIE treatment, ensuring stable and reliable performance. Utilizing the PEIE-modified PBFDO electrode as a two-in-one ETL / TE in OSCs yields results comparable to those obtained with traditional ITO electrodes. On the other hand, the low WF of the electrode can eliminate the need for using ETL. Through a facile lamination approach, it has been demonstrated the fabrication of all-organic solar cells, achieving a record-high power conversion efficiency (>15.1%) under indoor lighting conditions. This innovative approach offers a compelling alternative to traditional ITO electrodes in solar cells and holds promise for the development of efficient and cost-effective optoelectronic devices. Although the present invention has been described with reference to various embodiments, those skilled in the art will recognize that changes may be made without departing from the scope of the invention. It is intended that the detailed description be regarded as illustrative and that the appended claims including all the equivalents are intended to define the scope of the invention.

Claims

CLAIMS 1. A low-work function polymeric electrode for an optoelectronic device, said electrode comprising: a first film layer comprising an intrinsically doped n-type conductive polymer; and a second film layer comprising a polymeric cation.

2. The electrode according to claim 1, wherein said n-type conductive polymer is poly(benzodifurandione) (PBFDO).

3. The electrode according to claim 1 or 2, wherein said n-type conductive polymer comprises from 2 to 10000, more preferably from 6 to 1000, even more preferably from 3 to 100, most preferably from 5 to 50 repetitive units.

4. The electrode according to any one of the preceding claims, wherein said polymeric cation is poly(ethyleneimine) (PEI), ethoxylated PEI (PEIE) or mixtures thereof.

5. The electrode according to claim 4, wherein said PEI is linear or branched.

6. The electrode according to any one of the preceding claims, wherein said polymeric cation comprises from 5 to 10000, preferably from 10 to 1000, more preferably from 20 to 100 repetitive units.

7. The electrode according to any one of the preceding claims, wherein said first film layer has a work function in the range from 3 to 6 eV, preferably about 5 eV, and wherein said first film layer further has a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm.

8. The electrode according to any one of the preceding claims, wherein said electrode has a work function in the range from 2 to 5 eV, preferably about 4 eV, and wherein said electrode further has a conductivity in the range from 100 to 2500 S / cm, preferably from 500 to 2500 S / cm, more preferably from 1000 to 2500 S / cm.

9. An organic solar cell comprising an electrode according to any one of claims 1-8.

10. A method for manufacturing a low-work function polymeric electrode for an optoelectronic device, said method comprising the steps of: a) depositing a first solution comprising an n-type conductive polymer on a substrate, thus obtaining a first film layer; b) depositing a second solution comprising a polymeric cation on said first film layer thus obtaining a second film layer.

11. The method according to claim 10, wherein the concentration of said n-type conductive polymer in said first solution is from 0.1 to 500 mg / mL, preferably from 1 to 100 mg / mL.

12. The method according to any one of claims 10-11, wherein the concentration of said polymeric cation in said second solution is from 0.01 to 100 mg / mL, preferably from 0.1 to 10 mg / mL.

13. The method according to any one of claims 10-12, wherein said first solution and / or said second solution is deposited by a solution-processed technology.

14. The method according to any one of claims 10-13, wherein said second solution comprises a polar protic or aprotic solvent.

15. The method according to any one of claims 10-14, wherein said method further comprises a step of: a´) obtaining said first solution comprising an n-type conductive polymer by means of oxidative polymerization and in situ reductive doping in a polar protic or aprotic solvent.

Citation Information

Patent Citations

  • A one-step method for obtaining an ink comprising an n-type conducting polymer

    WO2024235468A1

  • Rigid conjugated polymer based on benzodifurandione and derivatives thereof as well as preparation and application of rigid conjugated polymer

    CN110862517A

  • Conductive ink with n-type conductivity and preparation and application thereof

    CN115651448A

  • Copolycondensates of the polyindophenine type

    DE3618838A1

  • Materials and methods for improving corner and edge coverage of solid electrolytic capacitors

    US20120206859A1

Cited By

  • Preparation method of silicon negative electrode of conductive binder containing side-chain-free n-type high-conductivity polymer material PBFDO

    CN120033211A