Wound cell manufacturing method, wound cell and battery

By welding metal sheets to the composite collector electrode ears of the wound battery, forming laminated parts and protrusions, the conductive layers are connected to each other, solving the problem of conductive layer barrier, reducing the internal resistance of the battery cell, and improving the Current conduction capability.

WO2024239623A1PCT designated stage expired Publication Date: 2024-11-28ZHEJIANG LIWINON ENERGY TECHNOLOGY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/139499
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-25
Filing Date
2023-12-18
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing wound cell has a problem of high internal resistance due to the polymer material layer blocking the conductive layer, which causes the conductive layer to be unable to conduct, resulting in a problem of high internal resistance.

Method used

By welding metal sheets to the pole ears of the composite fluid collector, a laminated portion and a protruding portion are formed, and adjacent conductive layers are connected to each other through the laminated portion, and the metal belt pole ears are connected to the protruding portion to achieve conduction.

Benefits of technology

It effectively reduces the internal resistance of the wound cell and improves the current conduction ability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023139499_28112024_PF_FP_ABST
    Figure CN2023139499_28112024_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed in the present invention is a wound cell manufacturing method, which comprises the following steps: using two metal sheets to respectively cover two electrically conductive layers of the same composite current collector and welding the two metal sheets to the two electrically conductive layers; after the two metal sheets respectively cover and are welded to the two electrically conductive layers, respectively cutting the two metal sheets to form a plurality of metal sub-sheets, and then winding the metal sheets and the composite current collector together, such that each metal sub-sheet comprises a stacking portion and a protruding portion, the stacking portions being configured to cover the electrically conductive layers, and the protruding portions protruding out of edges of tab portions; and welding metal strip tabs and all protruding portions that belong to the same composite current collector. By means of the wound cell manufacturing method in the present invention, adjacent electrically conductive layers of the composite current collector can be connected to each other, thereby reducing the internal resistance of a wound cell.
Need to check novelty before this filing date? Find Prior Art

Description

Wound cell manufacturing method, wound cell and battery Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a method for manufacturing a wound battery cell, a wound battery cell and a battery. Background Art

[0002] In related technologies, composite current collectors have the advantages of being lightweight and highly safe. Therefore, when manufacturing some wound battery cells, their core bodies are made of a composite current collector coated with active material.

[0003] The composite current collector comprises a polymer layer and conductive layers on either side of the polymer layer. The polymer layer provides advantages such as lightness and safety. However, the polymer layer also blocks the conductive layers on either side, preventing them from conducting electricity. This prevents all the false tabs in the wound cell from being connected in parallel, resulting in a higher internal resistance.

[0004] Summary of the Invention

[0005] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a method for manufacturing a wound battery cell, which can make adjacent conductive layers of a composite current collector conductive to each other, thereby reducing the internal resistance of the wound battery cell.

[0006] The present invention also provides a wound battery core.

[0007] The present invention also provides a battery.

[0008] According to a first aspect of the present invention, a method for manufacturing a wound battery cell is provided for connecting a wound battery cell to a metal strip tab. The wound battery cell is formed by winding a plurality of composite current collectors. The composite current collectors include tab portions, wherein the plurality of tab portions are spaced apart along the length of the composite current collectors. The tab portions include a stacked polymer material layer and two conductive layers, wherein the two conductive layers are respectively disposed on either side of the polymer material layer.

[0009] The method for manufacturing a wound battery cell comprises the following steps:

[0010] Covering and welding two metal sheets on the two conductive layers of the same composite current collector respectively;

[0011] After the two metal sheets are respectively covered and welded on the two conductive layers, the two metal sheets are respectively cut to form a plurality of sub-metal sheets, and then the metal sheets and the composite current collector are wound together, so that: the sub-metal sheets include a laminated portion and a protruding portion, the laminated portion is used to cover the conductive layer, and the protruding portion protrudes beyond the edge of the electrode ear portion;

[0012] The metal strip tab is welded to all the protrusions belonging to the same composite current collector.

[0013] According to the method for manufacturing a wound battery cell according to an embodiment of the present invention, there are at least the following beneficial effects: after the metal sheet is welded to the pole ear portion of the composite current collector, the laminated portion of the sub-metal sheet is welded on the conductive layer, and the two adjacent sub-metal sheets are welded to each other. Furthermore, the adjacent conductive layers are connected to each other through the laminated portion. After all the protrusions are connected to each other, the metal strip pole ear is connected to the protrusion, which can achieve conduction between the external current and all the conductive layers. In this way, the method for manufacturing a wound battery cell can make the adjacent conductive layers of the composite current collector conductive to each other, thereby reducing the internal resistance of the wound battery cell.

[0014] According to some embodiments of the present invention, the method for manufacturing a wound battery cell, wherein the cutting of the two metal sheets separately further comprises: making the protrusion protrude relative to the pole ear portion along the width direction of the wound battery cell.

[0015] According to some embodiments of the present invention, the method for manufacturing a wound battery cell further includes, before welding the metal strip tab and the protrusion, inserting the metal strip tab between two adjacent protrusions.

[0016] According to a first aspect of the present invention, a method for manufacturing a wound battery cell is provided for connecting a wound battery cell to a metal strip tab. The wound battery cell is formed by winding a plurality of composite current collectors, the composite current collectors comprising a tab portion and a main body portion. The plurality of tab portions are spaced apart along the length of the composite current collectors. The tab portion comprises a stacked polymer material layer and two conductive layers, the two conductive layers being respectively disposed on either side of the polymer material layer. The wound battery cell further comprises a sub-metal sheet, the sub-metal sheet comprising a stacked portion and a protruding portion. The stacked portion is used to cover the conductive layer, and the protruding portion protrudes beyond the edge of the conductive layer.

[0017] The method for manufacturing a wound battery cell comprises the following steps:

[0018] Covering and welding the laminated portion on the conductive layer;

[0019] The metal strip tab is welded to all the protrusions belonging to the same composite current collector.

[0020] According to the method for manufacturing a wound battery cell according to an embodiment of the present invention, there are at least the following beneficial effects: after the metal sheet is welded to the pole ear portion of the composite current collector, the laminated portion of the sub-metal sheet is welded on the conductive layer, and the two adjacent sub-metal sheets are welded to each other. Furthermore, the adjacent conductive layers are connected to each other through the laminated portion. After all the protrusions are connected to each other, the metal strip pole ear is connected to the protrusion, which can achieve conduction between the external current and all the conductive layers. In this way, the method for manufacturing a wound battery cell can make the adjacent conductive layers of the composite current collector conductive to each other, thereby reducing the internal resistance of the wound battery cell.

[0021] According to some embodiments of the present invention, the method for manufacturing a wound battery cell, wherein the cutting of the two metal sheets separately further comprises: making the protrusion protrude relative to the pole ear portion along the width direction of the wound battery cell.

[0022] According to some embodiments of the present invention, the method for manufacturing a wound battery cell further includes, before welding the metal strip tab and the protrusion, inserting the metal strip tab between two adjacent protrusions.

[0023] According to the second aspect of the present invention, the wound battery core is formed by winding a plurality of composite current collectors, and the wound battery core includes:

[0024] The composite current collector includes a tab portion and a main body portion. Along the length direction of the composite current collector, a plurality of tab portions are spaced apart. The tab portion includes a stacked polymer material layer and two conductive layers. The two conductive layers are respectively arranged on both sides of the polymer material layer.

[0025] a sub-metal sheet, comprising a laminated portion and a protruding portion, wherein the laminated portion is used to cover the conductive layer, and the protruding portion protrudes beyond an edge of the conductive layer, wherein all the protruding portions are connected to each other;

[0026] The metal strip tab is welded to the protruding portion.

[0027] The wound battery cell according to the embodiment of the present invention has at least the following beneficial effects: after the metal sheet is welded to the pole ear portion of the composite current collector, the laminated portion of the sub-metal sheet is welded on the conductive layer, and the two adjacent sub-metal sheets are welded to each other. Furthermore, the adjacent conductive layers are interconnected through the laminated portion. After all the protrusions are connected to each other, the metal strip pole ear is connected to the protrusion, which can achieve conduction between the external current and all the conductive layers. In this way, the wound battery cell can make the adjacent conductive layers of the composite current collector conductive to each other, thereby reducing the internal resistance of the wound battery cell.

[0028] According to some embodiments of the wound battery cell of the present invention, the protrusion protrudes relative to the tab portion along a width direction of the wound battery cell.

[0029] According to some embodiments of the wound battery cell of the present invention, the metal strip tab is located between two adjacent protrusions.

[0030] A battery according to an embodiment of a third aspect of the present invention comprises the wound battery cell described in any one of the embodiments of the second aspect.

[0031] The battery according to the embodiment of the present invention has at least the following beneficial effects: after the metal sheet is welded to the pole ear portion of the composite current collector, the stacked portion of the sub-metal sheet is welded on the conductive layer, and the two adjacent sub-metal sheets are welded to each other. Furthermore, the adjacent conductive layers are connected to each other through the stacked portion. After all the protrusions are connected to each other, the metal strip pole ear is connected to the protrusion, which can achieve conduction between the external current and all the conductive layers. In this way, the wound battery cell can make the adjacent conductive layers of the composite current collector conductive to each other, thereby reducing the internal resistance of the wound battery cell. Furthermore, the internal resistance of the battery with the wound battery cell is relatively low.

[0032] Additional aspects and advantages of the present invention will be set forth in part in the description which follows and, in part, will be obvious from the description which follows, or may be learned by practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The present invention will be further described below with reference to the accompanying drawings and embodiments, in which:

[0034] FIG1 is a schematic diagram of a composite current collector in a method for manufacturing a wound battery cell according to a first embodiment of the present invention;

[0035] FIG2 is a schematic diagram of a composite current collector in a method for manufacturing a wound battery cell according to a second embodiment of the present invention;

[0036] 3 is a schematic diagram of a metal sheet connected to a composite current collector in a method for manufacturing a wound battery cell according to a third embodiment of the present invention;

[0037] FIG4 is a schematic diagram of FIG3 from another angle;

[0038] 5 is a cross-sectional view of a metal strip tab connected to a composite current collector in a wound battery cell according to a fourth embodiment of the present invention;

[0039] FIG6 is a schematic diagram of a wound battery cell according to a fifth embodiment of the present invention;

[0040] 7 is a schematic diagram of a composite current collector connected to a metal strip tab in a wound battery cell according to a sixth embodiment of the present invention;

[0041] FIG8 is a side view of a wound battery cell according to a seventh embodiment of the present invention;

[0042] FIG9 is a top view of a wound battery cell according to an eighth embodiment of the present invention;

[0043] FIG. 10 is a top view of a wound battery cell according to a ninth embodiment of the present invention.

[0044] Reference numerals:

[0045] The wound battery cell 100 , the composite current collector 200 , the main body 210 , the tab 220 , the polymer material layer 221 , the conductive layer 222 , the ceramic layer 230 , the metal sheet 300 , the sub-metal sheet 310 , the laminated portion 311 , the protruding portion 312 , and the metal strip tab 400 . DETAILED DESCRIPTION

[0046] The following describes embodiments of the present invention in detail. Examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended only to explain the present invention and are not to be construed as limiting the present invention.

[0047] In the description of the present invention, it should be understood that descriptions involving orientations, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, they cannot be understood as limitations on the present invention.

[0048] In the description of the present invention, "several" means more than one, "plurality" means more than two, "greater than," "less than," and "exceed" are understood to exclude the number itself, while "above," "below," and "within" are understood to include the number itself. The use of "first" and "second" in the description is solely for the purpose of distinguishing technical features and should not be construed as indicating or implying relative importance, implicitly specifying the number of the indicated technical features, or implicitly specifying the order of the indicated technical features.

[0049] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, and connecting should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.

[0050] In the description of the present invention, reference to terms such as "one embodiment," "some embodiments," "illustrative embodiments," "examples," "specific examples," or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the exemplary expressions of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in any one or more embodiments or examples.

[0051] In some embodiments, the method for manufacturing a wound battery cell 100 is used to connect the wound battery cell 100 to a metal strip tab 400. The wound battery cell 100 is formed by winding a plurality of composite current collectors 200. That is, the composite current collectors 200 are stacked and then wound together. Please refer to FIG6 , which illustrates the appearance of the composite current collector 200 after winding. Please refer to FIG1 and FIG2 , which are schematic diagrams of the composite current collector 200 before winding, respectively. The composite current collector 200 includes a main body 210 and a tab 220. The main body 210 is coated with active material, and the tab 220 is connected to one end of the main body 210. Multiple tabs 220 are spaced apart along the length of the composite current collector 200. The tab 220 includes a stacked polymer material layer 221 and two conductive layers 222, with the two conductive layers 222 disposed on either side of the polymer material layer 221.

[0052] The method for manufacturing the wound battery cell 100 includes the following steps:

[0053] S100, covering and welding two metal sheets 300 on two conductive layers 222 of the same composite current collector 200;

[0054] S200: After the two metal sheets 300 are respectively covered and welded on the two conductive layers 222, the two metal sheets 300 are cut to form a plurality of sub-metal sheets 310. The metal sheets 300 and the composite current collector 200 are then wound together, such that: the sub-metal sheets 310 include a laminated portion 311 and a protruding portion 312. The laminated portion 311 is used to cover the conductive layer 222, and the protruding portion 312 protrudes beyond the edge of the tab portion 220.

[0055] S300 , welding the metal strip tab 400 and all the protrusions 312 belonging to the same composite current collector 200 .

[0056] Specifically, please refer to Figures 1, 3, and 4. Figures 1 to 4 show the process diagrams for manufacturing the wound battery cell 100. Among them, Figure 6 is a schematic diagram of the composite current collector 200 after winding. After the metal sheet 300 is welded to the pole ear portion 220 of the composite current collector 200, the stacking portion 311 of the sub-metal sheet 310 is welded on the conductive layer 222, and the two adjacent sub-metal sheets 310 are welded to each other. Furthermore, the adjacent conductive layers 222 are connected to each other through the stacking portion 311. Please refer to Figure 5. After all the protrusions 312 are connected to each other, the metal strip pole ear 400 is connected to the protrusion 312, which can achieve conduction between the external current and all the conductive layers 222. In this way, the manufacturing method of the wound battery cell 100 can make the adjacent conductive layers 222 of the composite current collector 200 conductive to each other, thereby reducing the internal resistance of the wound battery cell 100.

[0057] It should be noted that a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can be to weld the same end of the protrusion 312 of each sub-metal sheet 310 to the same point, and then connect the metal strip tab 400 to this point. In this way, current can enter all the protrusions 312 through the metal strip tab 400. And vice versa. In addition, a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can also be to connect all the protrusions 312 with the help of a metal adapter, and then connect the metal adapter to the metal strip tab 400. In addition, a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can also be to stack and bend all the protrusions 312 and the metal strip tab 400 together, and then concentrate them at the same point, and then weld them. Alternatively, the specific method of welding the metal strip tab 400 and all the protrusions 312 belonging to the same composite current collector 200 can also be to stack all the protrusions 312, weld the metal strip tab 400 to the protrusion 312, and then bend all the protrusions 312 and the metal strip tab 400.

[0058] It should be noted that the welding of the metal strip tab 400 to all protrusions 312 belonging to the same composite current collector 200 can specifically be performed when there are two composite current collectors 200, each coated with different active materials, thereby serving as the positive and negative electrodes of the wound battery cell 100. There are two metal strip tabs 400, each connected to the two composite current collectors 200. That is, one metal strip tab 400 is welded to all protrusions 312 of the positive composite current collector 200, and the other metal strip tab 400 is welded to all protrusions 312 of the negative composite current collector 200.

[0059] Referring to FIG. 4 , a ceramic layer 230 may be further provided between the main body 210 and the tab 220 , thereby improving the safety performance of the wound battery cell 100 .

[0060] Referring to FIG. 6 , in some embodiments, cutting the two metal sheets 300 separately further includes causing the protrusions 312 to protrude relative to the tabs 220 along the width direction of the wound battery cell 100. Specifically, the protrusions 312 may protrude beyond the edges of the tabs 220 along the width direction of the wound battery cell 100 or along the length direction of the wound battery cell 100. When the protrusions 312 protrude relative to the conductive layer 222 along the width direction of the wound battery cell 100, compared to protruding relative to the conductive layer 222 along the length direction of the wound battery cell 100, the protrusions 312 protruding in the length direction extend the length of the wound battery cell 100, whereas the protrusions 312 protruding in the width direction do not increase the length of the wound battery cell 100.

[0061] Referring to FIG. 7 , in some embodiments, before welding the metal tab 400 to the protrusion 312, the process further includes inserting the metal tab 400 between two adjacent protrusions 312. Specifically, the metal tab 400 can be welded to the outside of the protrusion 312 along the thickness direction of the main body 210. However, after the metal tab 400 is connected to the sub-metal sheet 310, the thickness of the weld between the protrusion 312 and the metal tab 400 increases due to the metal tab 400 being connected to the outside of the protrusion 312, thereby exceeding the thickness of the main body 210. When the thickness exceeds the thickness of the main body 210, the energy density of the wound battery cell 100 is reduced, or the wound battery cell 100 is incompatible when placed in an aluminum-plastic film or a steel shell. Therefore, when the metal strip tab 400 is inserted between two adjacent protrusions 312 , welding the metal strip tab 400 to the protrusions 312 does not increase the thickness of the weld, thereby making the wound battery cell 100 more compatible with the aluminum-plastic film or steel shell.

[0062] In addition to the above-mentioned method for manufacturing the wound battery cell 100, there are other methods for manufacturing the wound battery cell 100. Please refer to Figures 1, 3, and 4. Figures 1 to 4 show the process diagrams of manufacturing the wound battery cell 100. Among them, Figure 6 is a schematic diagram of the composite current collector 200 after winding. In some embodiments, the method for manufacturing the wound battery cell 100 is used to connect the wound battery cell 100 and the metal strip tab 400. The wound battery cell 100 is formed by winding multiple composite current collectors 200. The composite current collector 200 includes a main body 210 and a tab 220. The main body 210 is coated with active material, and the tab 220 is connected to one end of the main body 210. Along the length direction of the composite current collector 200, multiple tabs 220 are arranged at intervals. The tab 220 includes a polymer material layer 221 and two conductive layers 222 arranged in a stacked manner. The two conductive layers 222 are respectively arranged on both sides of the polymer material layer 221. The wound battery cell 100 further includes a sub-metal sheet 310 . The sub-metal sheet 310 includes a laminated portion 311 and a protruding portion 312 . The laminated portion 311 is used to cover the conductive layer 222 , and the protruding portion 312 protrudes beyond the edge of the conductive layer 222 .

[0063] The method for manufacturing the wound battery cell 100 includes the following steps:

[0064] S100, covering and welding the laminated portion 311 on the conductive layer 222;

[0065] S200 , welding the metal strip tab 400 and all the protrusions 312 belonging to the same composite current collector 200 .

[0066] Specifically, referring to Figure 6, after the metal sheet 300 is welded to the pole ear portion 220 of the composite current collector 200, the laminated portion 311 of the sub-metal sheet 310 is welded on the conductive layer 222, and the two adjacent sub-metal sheets 310 are welded to each other. Furthermore, the adjacent conductive layers 222 are connected to each other through the laminated portion 311. After all the protrusions 312 are connected to each other, the metal strip pole ear 400 is connected to the protrusion 312, which can achieve conduction between the external current and all the conductive layers 222. In this way, the manufacturing method of the wound battery cell 100 can make the adjacent conductive layers 222 of the composite current collector 200 conductive to each other, thereby reducing the internal resistance of the wound battery cell 100.

[0067] It should be noted that a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can be to weld the same end of the protrusion 312 of each sub-metal sheet 310 to the same point, and then connect the metal strip tab 400 to this point. In this way, current can enter all the protrusions 312 through the metal strip tab 400. And vice versa. In addition, a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can also be to connect all the protrusions 312 with the help of a metal adapter, and then connect the metal adapter to the metal strip tab 400. In addition, a specific method for welding the metal strip tab 400 to all the protrusions 312 belonging to the same composite current collector 200 can also be to stack and bend all the protrusions 312 and the metal strip tab 400 together, and then weld them.

[0068] Referring to FIG. 6 , in some embodiments, cutting the two metal sheets 300 separately further includes causing the protrusions 312 to protrude relative to the tabs 220 along the width direction of the wound battery cell 100. Specifically, the protrusions 312 may protrude beyond the edges of the tabs 220 along the width direction of the wound battery cell 100 or along the length direction of the wound battery cell 100. When the protrusions 312 protrude relative to the conductive layer 222 along the width direction of the wound battery cell 100, compared to protruding relative to the conductive layer 222 along the length direction of the wound battery cell 100, the protrusions 312 protruding in the length direction extend the length of the wound battery cell 100, whereas the protrusions 312 protruding in the width direction do not increase the length of the wound battery cell 100.

[0069] Referring to FIG. 7 , in some embodiments, before welding the metal tab 400 to the protrusion 312, the process further includes inserting the metal tab 400 between two adjacent protrusions 312. Specifically, the metal tab 400 can be welded to the outside of the protrusion 312 along the thickness direction of the main body 210. However, after the metal tab 400 is connected to the sub-metal sheet 310, the thickness of the weld between the protrusion 312 and the metal tab 400 increases due to the metal tab 400 being connected to the outside of the protrusion 312, thereby exceeding the thickness of the main body 210. Exceeding the thickness of the main body 210 can result in a lower energy density of the wound battery cell 100 or make the wound battery cell 100 incompatible when placed in the battery compartment of an electronic device. Therefore, when the metal strip tab 400 is inserted between two adjacent protrusions 312 , welding the metal strip tab 400 to the protrusions 312 does not pose the risk of increasing the thickness of the weld, thereby making the wound battery cell 100 more compatible with the battery compartment.

[0070] The structure of the wound battery cell 100 is described below. Referring to FIG. 6 , in some embodiments, the wound battery cell 100 is formed by winding a plurality of composite current collectors 200. The wound battery cell 100 includes: a composite current collector 200, a sub-metal sheet 310, and a metal strip tab 400. The composite current collector 200 includes a tab portion 220 and a main body portion 210. The main body portion 210 is coated with active material. The tab portion 220 is connected to one end of the main body portion 210. Along the length direction of the composite current collector 200, a plurality of tab portions 220 are spaced apart. The tab portion 220 includes a stacked polymer material layer 221 and two conductive layers 222. The two conductive layers 222 are respectively disposed on both sides of the polymer material layer 221. The sub-metal sheet 310 includes a laminated portion 311 and a protruding portion 312 . The laminated portion 311 is used to cover the conductive layer 222 . The protruding portion 312 protrudes beyond the edge of the conductive layer 222 . All protruding portions 312 are interconnected. The metal strip tab 400 is welded to the protruding portion 312 .

[0071] Specifically, after the metal sheet 300 is welded to the pole ear portion 220 of the composite current collector 200, the laminated portion 311 of the sub-metal sheet 310 is welded on the conductive layer 222, and the two adjacent sub-metal sheets 310 are welded to each other. Furthermore, the adjacent conductive layers 222 are connected to each other through the laminated portion 311. After all the protrusions 312 are connected to each other, the metal strip pole ear 400 is connected to the protrusion 312, which can achieve conduction between the external current and all the conductive layers 222. In this way, the manufacturing method of the wound battery cell 100 can make the adjacent conductive layers 222 of the composite current collector 200 conductive to each other, thereby reducing the internal resistance of the wound battery cell 100.

[0072] Referring to FIG. 6 , in some embodiments, the protrusion 312 protrudes relative to the tab portion 220 along the width direction of the wound battery cell 100. Specifically, the protrusion 312 may protrude beyond the edge of the tab portion 220 along the width direction of the wound battery cell 100 or along the length direction of the wound battery cell 100. When the protrusion 312 protrudes relative to the conductive layer 222 along the width direction of the wound battery cell 100, compared to protruding relative to the conductive layer 222 along the length direction of the wound battery cell 100, the protrusion 312 protruding in the length direction will extend the length of the wound battery cell 100, while the protrusion 312 protruding in the width direction will not increase the length of the wound battery cell 100.

[0073] Referring to Figure 7 , in some embodiments, the metal tab 400 is positioned between two adjacent protrusions 312 . Specifically, the metal tab 400 can be welded to the outside of the protrusion 312 along the thickness of the main body 210 . However, after the metal tab 400 is attached to the sub-metal sheet 310 , the thickness of the weld between the protrusion 312 and the metal tab 400 increases, exceeding the thickness of the main body 210 . Exceeding the thickness of the main body 210 can result in a lower energy density for the wound battery cell 100 or incompatibility when placed in a battery compartment of an electronic device. Therefore, when the metal tab 400 is inserted between two adjacent protrusions 312 , welding the metal tab 400 to the protrusion 312 does not increase the thickness of the weld, thereby improving the compatibility of the wound battery cell 100 with the battery compartment.

[0074] The metal sheet 300 can be made of a highly conductive metal such as copper foil, aluminum foil, or nickel foil. The metal tab 400 can also be made of a highly conductive metal such as copper foil, aluminum foil, or nickel foil. When the metal tab 400 is made of copper foil, its thickness is 3 to 25 μm. When the metal tab 400 is made of aluminum foil, its thickness is 6 to 25 μm.

[0075] Referring to Figure 8 , in some embodiments, the length of the protrusion 312 along the width of the wound battery cell 100 is L1, satisfying the following conditions: 2.5 mm ≤ L1 ≤ 8 mm. When L1 is less than 2.5 mm, and when the protrusion 312 is welded to the metal tab 400, the protrusion 312 is too short, increasing the difficulty for workers to weld the protrusion 312 to the metal tab 400. When L1 is greater than 8 mm, unnecessary material waste occurs.

[0076] Referring to Figures 9 and 10 , in some embodiments, the protrusion 312 protrudes relative to the tab portion 220 along the width direction of the wound battery cell 100. Specifically, the protrusion 312 can protrude inward along the width direction of the wound battery cell 100, as shown in Figure 9 . Furthermore, the protrusion 312 can also protrude outward along the width direction of the wound battery cell 100, as shown in Figure 10 . This allows the wound battery cell 100 to have a wider adaptability.

[0077] In some embodiments, the battery includes the wound cell 100 of any one of the above embodiments. After the metal sheet 300 is welded to the pole ear portion 220 of the composite current collector 200, the laminated portion 311 of the sub-metal sheet 310 is welded on the conductive layer 222, and the two adjacent sub-metal sheets 310 are welded to each other. Furthermore, the adjacent conductive layers 222 are connected to each other through the laminated portion 311. After all the protrusions 312 are connected to each other, the metal strip pole ear 400 is connected to the protrusion 312, which can achieve conduction between the external current and all the conductive layers 222. In this way, the wound cell 100 can make the adjacent conductive layers 222 of the composite current collector 200 conductive to each other, thereby reducing the internal resistance of the wound cell 100. Furthermore, the internal resistance of the battery with the wound cell 100 is small.

[0078] While the embodiments of the present invention have been described in detail above with reference to the accompanying drawings, the present invention is not limited to the embodiments described above. Various modifications may be made within the scope of knowledge possessed by a person skilled in the art without departing from the spirit of the present invention. Furthermore, the embodiments of the present invention and the features thereof may be combined with one another unless there is a conflict.

Claims

1. A method for manufacturing a wound battery cell, characterized in that: Used to connect a wound battery cell and a metal strip pole ear, wherein the wound battery cell is formed by winding a plurality of composite current collectors, wherein the composite current collector comprises a plurality of pole ear portions, and along the length direction of the composite current collector, the plurality of pole ear portions are arranged at intervals, and the pole ear portions comprise a polymer material layer and two conductive layers arranged in a stacked manner, and the two conductive layers are respectively arranged on both sides of the polymer material layer; The method for manufacturing a wound battery core comprises the following steps: Covering and welding two metal sheets respectively on the two conductive layers of the same composite current collector; After the two metal sheets are respectively covered and welded on the two conductive layers, the two metal sheets are respectively cut to form a plurality of sub-metal sheets, and then the metal sheets and the composite current collector are wound together, so that: the sub-metal sheets include a laminated portion and a protruding portion, the laminated portion is used to cover the conductive layer, and the protruding portion protrudes beyond the edge of the pole ear portion; The metal strip tab and all the protrusions belonging to the same composite current collector are welded.

2. The method for manufacturing a wound battery cell according to claim 1, characterized in that: The step of cutting the two metal sheets separately further includes: making the protruding portion protrude relative to the pole ear portion along the width direction of the wound battery core.

3. The method for manufacturing a wound battery cell according to claim 1, characterized in that: Before welding the metal strip electrode tab and the protrusion, the method further includes inserting the metal strip electrode tab between two adjacent protrusions.

4. A method for manufacturing a wound battery cell, characterized in that: Used to connect a wound battery cell and a metal strip pole ear, the wound battery cell is formed by winding a plurality of composite current collectors, the composite current collector comprises a pole ear portion and a main body portion, along the length direction of the composite current collector, a plurality of the pole ear portions are arranged at intervals, the pole ear portion comprises a polymer material layer and two conductive layers arranged in a stacked manner, the two conductive layers are respectively arranged on both sides of the polymer material layer, the wound battery cell further comprises a sub-metal sheet, the sub-metal sheet comprises a stacked portion and a protruding portion, the stacked portion is used to cover the conductive layer, and the protruding portion protrudes beyond the edge of the conductive layer; The method for manufacturing a wound battery core comprises the following steps: Covering and welding the laminated portion on the conductive layer; The metal strip tab and all the protrusions belonging to the same composite current collector are welded.

5. The method for manufacturing a wound battery cell according to claim 4, characterized in that: The step of cutting the two metal sheets separately further includes: making the protruding portion protrude relative to the pole ear portion along the width direction of the wound battery core.

6. The method for manufacturing a wound battery cell according to claim 4, characterized in that: Before welding the metal strip electrode tab and the protrusion, the method further includes inserting the metal strip electrode tab between two adjacent protrusions.

7. A wound battery cell, characterized in that: The wound battery core is formed by winding a plurality of composite current collectors, and the wound battery core comprises: The composite current collector comprises a pole ear portion and a main body portion, and a plurality of pole ear portions are arranged at intervals along the length direction of the composite current collector, and the pole ear portion comprises a polymer material layer and two conductive layers stacked in layers, and the two conductive layers are respectively arranged on both sides of the polymer material layer; a sub-metal sheet, comprising a laminated portion and a protruding portion, wherein the laminated portion is used to cover the conductive layer, and the protruding portion protrudes beyond the edge of the conductive layer, wherein all the protruding portions are connected to each other; The metal strip pole ear is welded to the protruding portion.

8. The wound battery cell according to claim 7, characterized in that: The protruding portion protrudes relative to the pole ear portion along a width direction of the wound battery core.

9. The wound battery cell according to claim 7, characterized in that: The metal strip tab is located between two adjacent protrusions.

10. A battery, characterized in that It comprises the wound battery cell as claimed in any one of claims 7 to 9.

Citation Information

Patent Citations

  • Battery cell and battery

    CN115603006A

  • Winding battery cell manufacturing method, winding battery cell and battery

    CN116759622A

  • Composite current collector cell and lithium battery

    CN217788491U

  • battery

    JP2014167890A