Pressure sensor, battery cell, and electrical device

By designing multiple raised structures of different heights in the sensitive layer of the pressure sensor and using conductive particles and interdigital electrodes, the problem of low adaptation of existing pressure sensors is solved, and high sensitivity under multiple pressures is achieved Detection and accurate acquisition of battery internal information.

WO2024239723A1PCT designated stage expired Publication Date: 2024-11-28CONTEMPORARY AMPEREX TECHNOLOGY CO LTD

Patent Information

Application Number
PCT/CN2024/076631
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-19
Filing Date
2024-02-07
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing pressure sensors have low adaptability and are difficult to apply to the detection environment under various pressures. The detection range and sensitivity are insufficient, so they cannot effectively monitor the evolution of the internal structure of the battery and the stress changes.

Method used

A pressure sensor is designed, and its sensitive layer includes raised structures of different heights. By setting up raised structures of different heights, differentiating the pressure sensitive range of each height, increasing the detection range and improving detection sensitivity. Specific measures include setting a plurality of protrusions in the height direction of the protruding structure, reducing the layout complexity using an annular reference line, and improving the conductivity and sensitivity of the sensor through conductive particles and interdigital electrodes.

Benefits of technology

It realizes effective detection of pressure sensors under various pressures, increases the detection range and sensitivity, and can more accurately obtain battery internal information, improving the safety and stability of the battery management system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024076631_28112024_PF_FP_ABST
    Figure CN2024076631_28112024_PF_FP_ABST
Patent Text Reader

Abstract

A pressure sensor (400). The pressure sensor (400) comprises an electrode layer (40) and a sensitive layer (42). At least two protrusion structures (422) of different heights are provided on the sensitive layer (42). Each protrusion structure (422) comprises at least one protrusion. Each protrusion is located on the side of a base layer (420) facing the electrode layer (40), and the contact area between each protrusion and the electrode layer (40) is configured to change along with the change of the pressure applied on the electrode layer (40). In this way, the pressure sensor (400) can be applied to detection environments under various pressures, thereby effectively broadening the detection range of the pressure sensor (400) and improving the detection sensitivity of the pressure sensor (400). Also provided are a battery cell (20) and an electrical device.
Need to check novelty before this filing date? Find Prior Art

Description

Pressure sensors, battery cells and electrical equipment Technical Field

[0001] The present application relates to the field of measurement technology, and in particular to a pressure sensor, a battery cell, and an electrical device. Background Art

[0002] Pressure sensors are components that output applied pressure as an electrical signal. They are characterized by a simple structure, low power consumption, and fast dynamic response. They are widely used in various fields. For example, they can be embedded in batteries to detect internal electrode expansion and other behaviors, reflecting the evolution of the battery's internal structure and providing real-time insights into the battery's operating status. With the development of new energy technologies, battery types are expanding, and the requirements for battery performance are becoming increasingly stringent, leading to an increase in the need for testing. However, existing pressure sensors have a low degree of adaptability. Therefore, there is a need to enhance the adaptability of pressure sensors.

[0003] Summary of the Invention

[0004] The main technical problem solved by this application is to provide a pressure sensor, a battery cell, and an electrical device, which can make the pressure sensor suitable for detection environments under various pressures, thereby effectively increasing the detection range of the pressure sensor and improving the detection sensitivity of the pressure sensor.

[0005] In a first aspect, the present application provides a pressure sensor comprising an electrode layer and a sensitive layer, the sensitive layer comprising a base layer and at least two protrusion structures protruding from the base layer at different heights, each protrusion structure comprising at least one protrusion, each protrusion being located on the side of the base layer facing the electrode layer, and the contact area between each protrusion and the electrode layer being configured to vary with changes in the pressure applied to the electrode layer. By providing two protrusion structures of different heights, the pressure-sensitive range of each protrusion structure is differentiated, enabling the pressure sensor to be adapted for detection environments under a variety of pressures, thereby effectively increasing the detection range of the pressure sensor and improving the detection sensitivity of the pressure sensor.

[0006] In some embodiments of the present application, along the height direction of the protrusion structures, at least some of the relatively low-height protrusion structures are spaced apart from the electrode layer and are configured to contact the electrode layer after the pressure applied to them exceeds a predetermined threshold. Through this approach, after the relatively high-height protrusion structures are compressed to a certain degree, the relatively low-height protrusion structures can be brought into contact with the electrode layer. This effectively staggers the pressure-sensitive ranges of the relatively high-height protrusion structures from those of the relatively low-height protrusion structures, further increasing the detection range and sensitivity.

[0007] In some embodiments of the present application, the tallest protrusions are configured to maintain contact with the electrode layer along their height. By adding microstructures where collapse is evident, the sharp drop in resistance can be effectively slowed, thereby increasing the sensor's range. By utilizing the tallest protrusions to provide support for the sensitive layer, the adverse effects of sensitive layer collapse can be effectively mitigated.

[0008] In some embodiments of the present application, the highest raised structures are located in the middle and / or corner regions of the sensitive layer. These regions are more susceptible to collapse, particularly when the sensitive layer is large. By placing the higher raised structures in the corners and middle regions, which are more susceptible to collapse, more effective support can be provided for the sensitive layer.

[0009] In some embodiments of the present application, the protrusion has a cross-section perpendicular to the height direction of the protrusion, and the cross-section of the protrusion gradually decreases in the direction from the substrate layer to the electrode layer. Through this arrangement, when the protrusion is compressed by pressure, the contact area with the electrode layer gradually changes, which can effectively improve the sensitivity of the contact area of ​​the protrusion to pressure. When the higher-level microstructure reaches the compression limit under pressure, the lower-level microstructure adds a contact electrode. Through the hierarchical pressure division of the microstructure, the sensitivity of the sensor within a large range can be greatly improved, and pressure changes can be better distinguished.

[0010] In some embodiments of the present application, the protrusion is configured in the shape of a spherical segment. Through this configuration, the sensitivity of the contact area of ​​the protrusion to pressure can be further effectively increased by utilizing the arc-shaped characteristics of the outer surface of the spherical segment.

[0011] In some embodiments of the present application, each protrusion structure includes multiple protrusions, and the multiple protrusions of the same protrusion structure are spaced apart and arranged on a circular reference line centered at a predetermined reference point. By arranging protrusions of the same height on the circular reference line, the design process can use the circular reference line as a unit for design considerations, reducing the complexity of the protrusion arrangement.

[0012] In some embodiments of the present application, the preset reference point is set at the area of ​​maximum deformation of the sensitive layer under pressure. By setting the maximum deformation area at the center of the annular reference line and using the deformation pattern of the sensitive layer relative to the maximum deformation area to set an appropriate annular reference line, the complexity of the arrangement of the protrusion structure can be further reduced.

[0013] In some embodiments of the present application, the preset reference point is set in the middle area of ​​the sensitive layer. By setting the preset reference point in the middle area of ​​the sensitive layer, more space can be reserved around it for setting the circular reference line, thereby further reducing the complexity of the arrangement of the protrusion structure.

[0014] In some embodiments of the present application, each protrusion structure includes multiple protrusions, and the multiple protrusions of the same protrusion structure are spaced apart to form multiple groups of ring structures, with the multiple protrusions in each group of ring structures located on a ring reference line. By grouping protrusions of the same height and planning them using the ring reference line as a unit, grouping can further reduce the complexity of the protrusion structure arrangement, especially when the sensitive layer area is large and the number of protrusion structures is large.

[0015] In some embodiments of the present application, the number of protrusions at the same height on the same annular reference line is not less than three. This arrangement increases the gradient of the contact area, which is beneficial for improving the sensitivity of the pressure sensor.

[0016] In some embodiments of the present application, protrusion structures of different heights are located on different annular reference lines. Different annular reference lines are used to plan the protrusion structures of different heights, thereby reducing the complexity of the arrangement of the protrusion structures.

[0017] In some embodiments of the present application, at least some of the protrusions are configured to overlap with protrusions at other heights after moving along the annular reference line. This arrangement helps increase the density of the protrusion structure and thus improve the sensitivity of the pressure sensor.

[0018] In some embodiments of the present application, the annular reference line includes one of a circle, an ellipse, and a polygon. By utilizing the equidistance between the graphics and the center, the layout complexity can be reduced.

[0019] In some embodiments of the present application, the protrusions have a cross-section perpendicular to their height, and the maximum cross-sectional dimension of a protrusion with a relatively small height is smaller than the maximum cross-sectional dimension of a protrusion with a relatively large height. This allows the protrusion with a relatively small height to deform more easily, making changes in the contact area more sensitive to pressure, thereby improving the sensitivity of the contact between the protrusion with a relatively small height and the electrode layer.

[0020] In some embodiments of the present application, the number of relatively small protrusions is greater than the number of relatively large protrusions. By increasing the number of relatively small protrusions, the pressure shared by the relatively small protrusions can be increased, while also increasing the rate of change of the contact area of ​​the relatively small protrusions with pressure. This can improve detection sensitivity.

[0021] In some embodiments of the present application, the multiple raised structures have at least three different heights. By using the raised structures to divide pressure, the sensitivity of the sensor can be significantly improved over a wide range, enabling better resolution of pressure changes. By providing multiple heights, both the range and sensitivity can be increased.

[0022] In some embodiments of the present application, in two adjacent heights of at least two different heights, the ratio of the difference between the relatively larger height and the relatively smaller height to the relatively larger height is 0.3-0.8. This arrangement can improve the continuity of the contact area change and increase sensitivity.

[0023] In some embodiments of the present application, the height of the plurality of raised structures is 5-200 μm; alternatively, the height of the plurality of raised structures is 10-50 μm. By setting the height within this range, the relatively large raised structures are prevented from sharing too much pressure, and the pressure sensitivity of the contact area of ​​the relatively small raised structures is increased, thereby enabling the pressure sensor to have a higher range.

[0024] In some embodiments of the present application, the material of the sensitive layer includes a flexible substrate and conductive particles dispersed in the flexible substrate, which can make the protruding structure conductive and elastic, and have better deformation recovery ability.

[0025] In some embodiments of the present application, the conductive particles include graphite particles and carbon nanotube particles. The selected particles have high conductivity and can be nanoscale, with more uniform dispersion and higher sensitivity.

[0026] In some embodiments of the present application, the electrode layer includes a first electrode and a second electrode arranged in an interdigitated manner. The use of interdigitated coplanar electrodes can effectively reduce the thickness of the sensor while maintaining the ability of the sensitive layer to deform under pressure, thereby achieving sensitive resistance change acquisition capabilities.

[0027] In some embodiments of the present application, the first electrode includes a plurality of first electrode strips arranged side by side and spaced apart, and the second electrode includes a plurality of second electrode strips arranged side by side and spaced apart, with at least some of the first electrode strips disposed within the spacing regions between the second electrode strips. The width of the first and second electrode strips is 10-200 μm, and the spacing between adjacent first and second electrode strips is 5-200 μm. Alternatively, the width of the first and second electrode strips is 50-150 μm, and the spacing between adjacent first and second electrode strips is 20-80 μm. By properly setting the width and spacing of the electrode strips, the raised structures facilitate forming a conductive network between the first and second electrodes, thereby improving the detection sensitivity of the sensor.

[0028] In some embodiments of the present application, the raised structure has a cross-section perpendicular to the height direction of the raised structure, and the maximum cross-sectional dimension of the raised structure is greater than or equal to 1.5 times the spacing distance. This configuration facilitates the use of a single raised structure to directly form an electrical connection with adjacent first and second electrode strips.

[0029] In a second aspect, the present application provides a battery cell, comprising a housing and a pressure sensor according to any one of the above embodiments, wherein the pressure sensor is disposed inside the housing, so as to obtain information about the battery's internal structure, and the obtained data is more accurate.

[0030] In a third aspect, the present application provides an electrical device including the aforementioned battery cell, which can acquire internal information of the battery, and the acquired data is more accurate.

[0031] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present application. Those skilled in the art can also derive other drawings based on these drawings without inventive work, among which:

[0033] FIG1 is a schematic cross-sectional view of a pressure sensor according to one or more embodiments of the present application;

[0034] FIG2 is a schematic cross-sectional view of a pressure sensor under different pressure states according to one or more embodiments of the present application;

[0035] FIG3 is a schematic cross-sectional view of a pressure sensor according to one or more embodiments of the present application;

[0036] FIG4 is a schematic planar structural diagram of a sensitive layer of a pressure sensor according to one or more embodiments of the present application;

[0037] FIG5 is a schematic plan view of the structure of a pressure sensor according to one or more embodiments of the present application;

[0038] FIG6 is a schematic diagram of an exploded structure of a battery according to one or more embodiments;

[0039] FIG7 is a schematic diagram of the exploded structure of a battery cell according to one or more embodiments;

[0040] FIG8 is a schematic diagram of the structure of a vehicle according to one or more embodiments.

[0041] In the attached figure:

[0042] 1000, vehicle; 300, motor; 200, controller; 100, battery; 10, housing; 11, first part; 12, second part; 20, battery cell; 21, end cap; 21a, electrode terminal; 22, housing; 23, electrode assembly;

[0043] 400, pressure sensor; 40, electrode layer; 42, sensitive layer; 420, substrate layer; 422, protrusion structure; 4221, protrusion; 42211, protrusion; 4222, protrusion; 42221, protrusion; 4223, protrusion; 401, first electrode; 402, second electrode; 403, electrode base; 44, corrosion-resistant protective layer; 46, insulating layer; 48, sensitive layer adhesive; 49, insulating layer adhesive. DETAILED DESCRIPTION

[0044] The following will be combined with the accompanying drawings in the embodiments of this application to clearly and completely describe the technical solutions in the embodiments of this application. Obviously, the embodiments described are only part of the embodiments of this application, not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.

[0045] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned figure descriptions are intended to cover non-exclusive inclusions.

[0046] In the description of the embodiments of the present application, the technical terms "first" and "second" are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, unless otherwise clearly and specifically defined, the term "multiple" refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).

[0047] References herein to "embodiments" mean that a particular feature, structure, or characteristic described in connection with the embodiments may be included in at least one embodiment of the present application. The appearance of this phrase in various places in the specification does not necessarily refer to the same embodiment, nor does it constitute an independent or alternative embodiment that is mutually exclusive of other embodiments. It is understood, both explicitly and implicitly, by those skilled in the art that the embodiments described herein may be combined with other embodiments.

[0048] In the description of the embodiments of this application, the term "and / or" is simply a description of the association relationship between associated objects, indicating that three relationships can exist. For example, A and / or B can represent the following three situations: A exists alone, A and B exist simultaneously, and B exists alone. In addition, the character " / " in this document generally indicates that the associated objects are in an "or" relationship.

[0049] In the description of the embodiments of the present application, the technical terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the embodiments of the present application.

[0050] In the description of the embodiments of the present application, unless otherwise expressly specified or limited, technical terms such as "installed," "connected," "connected," and "fixed" should be understood in a broad sense. For example, they can refer to fixed connections, detachable connections, or integration; mechanical connections or electrical connections; direct connections or indirect connections through an intermediate medium; internal connections between two components or interactions between two components. Those skilled in the art can understand the specific meanings of the above terms in the embodiments of the present application based on specific circumstances.

[0051] Amounts, ratios, and other numerical values ​​are presented herein in a range format. It should be understood that such range format is used for convenience and brevity and should be interpreted flexibly to include not only the values ​​explicitly specified as range limits, but also all individual values ​​or sub-ranges encompassed within the range, as if each value and sub-range were explicitly specified.

[0052] With the widespread application of electrochemical devices (e.g., lithium-ion batteries), people have increasingly higher requirements for their performance, especially battery safety, stability, and capacity. They expect batteries to have good comprehensive performance in all aspects. Lithium batteries are complex systems in which chemical energy, thermal energy, and electrical energy are highly coupled in (electro)chemical reactions. Real-time understanding of the internal working state of the battery is key to the development and design of new batteries and their efficient and safe operation. At the microscopic level, lithium de-lithiation and lithium insertion reactions during the charge and discharge process of lithium batteries cause the electrode materials to expand, increasing internal stress in the battery and easily leading to electrode delamination and increased SEI film thickness. Studies have shown that the expansion of graphite electrodes can reach 10%, while that of graphite-silicon composite electrodes can reach 280%. Under long-term cycling, the internal electrode sheets will experience irreversible expansion and associated problems such as electrolyte consumption, capacity reduction, and lithium dendrites due to changes in the battery potential, resulting in decreased battery performance and shortened battery life. At a macroscopic level, the combined expansion of multiple layers of wound electrode sheets causes the cell to expand in volume, which in turn compresses against the battery casing, causing deformation. This synergistic mechanical-thermal coupling significantly alters the internal and external stresses and heat generation behavior of the battery, with uncontrollable factors increasing with age. Electrode expansion behavior reflects the evolution of the internal structure and contains a wealth of information. Obtaining information on battery expansion behavior is crucial for a comprehensive and in-depth understanding of lithium-ion battery operating modes, optimizing battery material selection, monitoring battery energy conversion status, gaining a deeper understanding of the battery's internal operating mechanisms, and establishing more accurate digital twin models of the battery cell. This information can provide crucial information to battery management systems (BMS), further improving the safety, efficiency, and stability of lithium-ion batteries during operation.

[0053] To obtain more accurate and reliable information from the battery's interior, embedded sensors can be used to measure temperature, stress, and other parameters. However, most current sensors collect a single physical quantity, limiting their applicability. The development and design of high-performance embedded sensors is lacking.

[0054] In order to solve the above technical problems, the present application provides a pressure sensor. Please refer to Figure 1, which is a schematic cross-sectional structure diagram of a pressure sensor according to one or more embodiments of the present application. The pressure sensor 400 includes an electrode layer 40 and a sensitive layer 42. The sensitive layer 42 includes a base layer 420 and at least two protrusion structures 422 protruding from the base layer 420 at different heights. Each protrusion structure 422 includes at least one protrusion. Each protrusion is located on the side of the base layer 420 facing the electrode layer 40, and the contact area between each protrusion and the electrode layer 40 is configured to change as the pressure on the electrode layer 40 changes.

[0055] The pressure sensor 400 is a component that outputs the applied pressure in the form of an electrical signal. The pressure sensor 400 may be a resistive sensor that converts the measured pressure into an electrical signal that is related to the pressure by using a change in resistance.

[0056] Pressure sensor 400 can be a thin-film sensor. It can be fabricated using metals, semiconductors, and polymers to form temperature, pressure, and strain sensors. These sensors can be embedded within batteries to measure temperature and stress. This enables in-situ detection of internal electrode expansion pressure signals and temperature under various operating conditions. This provides critical data for the construction of accurate battery numerical models and battery management systems, and serves as a crucial tool for the industrialization of a new generation of safe and efficient lithium-ion batteries.

[0057] Specifically, the electrode layer 40 is used to collect changes in the electrical signal of the sensitive layer 42, and forms a conductive network in contact with the sensitive layer 42, thereby converting the pressure signal into an electrical signal. The sensitive layer 42 is used to form a contact resistance with the electrode layer 40, so that the pressure sensor 400 can detect the pressure applied based on the contact resistance between the sensitive layer 42 and the electrode layer 40. In other words, it can be a resistive pressure sensor, which mainly relies on the deformation of the sensitive layer under the action of external force, causing the internal conductive network to break or reconstruct, resulting in a change in resistance, thereby reflecting the magnitude of the applied external force.

[0058] In some embodiments of the present application, the electrode layer 40 includes a first electrode 401 and a second electrode 402 arranged in a forked manner. The forked electrodes are electrodes with a periodic pattern in a finger-like or comb-like surface. The first electrode 401 and the second electrode 402 are located on the same side of the sensitive layer 42, that is, the first electrode 401 and the second electrode 402 are coplanar electrodes. Due to the narrow internal space of the battery, if the sensor is too thick, when the sensor is placed inside the battery, it may cause damage to the battery electrode material and lithium deposition due to stress concentration at a single point. In this embodiment, the use of coplanar electrodes based on forked electrodes can effectively reduce the thickness of the sensor without affecting the deformation ability of the sensitive layer under pressure, thereby obtaining sensitive resistance change acquisition capabilities.

[0059] In some embodiments of the present application, the first electrode 401 includes a plurality of first electrode strips arranged side by side and spaced apart, and the second electrode 402 includes a plurality of second electrode strips arranged side by side and spaced apart, with at least some of the first electrode strips disposed within the spacing between the second electrode strips. The width of the first and second electrode strips is 10-200 μm, and the spacing between adjacent first and second electrode strips is 10-200 μm. The width of the electrode strips and the spacing between the electrode strips are measured along the electrode arrangement direction; the distance from one edge of an electrode strip to the other edge is measured using a micrometer to obtain the width of the electrode strip; and the spacing between the electrode strips is measured from the edge of a first electrode strip closest to the second electrode strip to the edge of a second electrode strip closest to the first electrode strip using a micrometer to obtain the spacing between the electrode strips. The greater the number of interdigitated fingers per unit area, the better the sensor's performance output. However, if the electrode strips are too thin or the spacing between the electrode strips is too small, this may lead to unstable solder joints and the occurrence of thickness mutation points, thereby reducing performance. In this embodiment, by comprehensively considering performance requirements and rationally setting the width and spacing of the electrode strips, the raised structure facilitates the formation of a conductive network between the first and second electrodes, thereby improving the sensor's detection sensitivity.

[0060] In some embodiments of the present application, the width of the first electrode strips and the second electrode strips is 50-150 μm, and the spacing between adjacent first electrode strips and the second electrode strips is 20-80 μm. For example, the width of the first electrode strips and the second electrode strips is 50 μm, 80 μm, 100 μm, 120 μm, 150 μm, etc. If the width of the electrode strips is too small (less than 50 μm), defects such as broken wires are likely to occur, resulting in unstable solder joints. If the width of the electrode strips is too large (greater than 150 μm), the electrode arrangement density will decrease within the limited space, the number of electrodes will decrease, and the sensitivity of the sensor will be reduced. The spacing between adjacent first electrode strips and the second electrode strips is 20 μm, 35 μm, 50 μm, 60 μm, 80 μm, etc. If the spacing between the electrode strips is too small (less than 20μm), short circuits and sudden changes in weld thickness are likely to occur. If the spacing between the electrode strips is too large (greater than 80μm), the electrode arrangement density will decrease within the limited space, reducing the number of electrodes and lowering the sensor sensitivity. By further optimizing the electrode strip width and spacing, it is possible to utilize the raised structure to directly form an electrical connection with two adjacent first and second electrode strips.

[0061] In some embodiments of the present application, the interdigitated electrodes can be unconnected metal wires fabricated on an insulating substrate using a circuit etching process. The interdigitated electrodes can be fabricated using a copper plate circuit process based on an FPC (flexible printed circuit) board, with a PI film (polyimide) as the substrate and copper wires formed on the substrate to form the interdigitated electrodes. To enhance the conductivity between the sensitive layer and the electrode and accurately capture resistance changes, a 10nm layer of gold (Au) can also be deposited on the surface of the copper wire.

[0062] In some embodiments of the present application, the material of the sensitive layer 42 includes a flexible substrate and conductive particles dispersed in the flexible substrate.

[0063] The flexible substrate is used to enable the sensitive layer 42 to deform under pressure and recover after pressure is released. The conductive particles form a conductive network when in contact with the electrode layer 40. The flexible substrate can be made of a polymer material such as polyurethane, while the conductive particles can be made of materials such as graphite and carbon nanotubes.

[0064] In some embodiments of the present application, the sensitive layer 42 has a microstructure, specifically including at least two protruding structures 422 of different heights. The protruding structure 422 contacts two electrodes that are not connected to each other in the electrode layer 40, constructing a conductive network and forming a contact resistance. Wherein, the height direction is along the direction from the substrate layer 420 to the electrode layer 40 (the X direction shown in the figure), and the height of the protruding structure 422 can be measured under a scanning electron microscope. As the pressure gradually increases, the contact area between the protruding structure 422 and the electrode gradually increases, and the contact resistance gradually decreases. The change in the contact area of ​​the protruding structure 422 is caused by the compression deformation of the protruding structure 422 caused by the pressure and the support of the electrode layer 40.

[0065] Please refer to Figure 2, which is a schematic diagram of the cross-sectional structure of a pressure sensor under different pressure states of one or more embodiments of the present application. Among them, Figure 2 (a) is a schematic diagram of the cross-sectional structure of the pressure sensor under the first pressure state of one or more embodiments of the present application, Figure 2 (b) is a schematic diagram of the cross-sectional structure of the pressure sensor under the second pressure state of one or more embodiments of the present application, and Figure 2 (c) is a schematic diagram of the cross-sectional structure of the pressure sensor under the third pressure state of one or more embodiments of the present application. As the pressure increases further, the protruding structure 422 that was not originally involved in the construction of the conductive network contacts the electrode and is incorporated into the conductive network, which is equivalent to connecting a new resistor in parallel to the original conductive network, thereby further reducing the overall resistance at both ends of the electrode to reflect the change in pressure value. In this embodiment, three protruding structures 422 of different heights are included, wherein the protrusion 4221 is a protrusion of the protruding structure of the first height, the protrusion 4222 is a protrusion of the protruding structure of the second height, and the protrusion 4223 is a protrusion of the protruding structure of the third height. The height of protrusion 4223 is greater than the height of protrusion 4221, and the height of protrusion 4221 is greater than the height of protrusion 4222. As shown in Figure 2 (a), under the first pressure state, protrusion 4221 and protrusion 4223 are in contact with the first electrode 401 and the second electrode 402 of electrode layer 40, respectively, to form a conductive network. At this time, the contact area between the protrusion structure 422 and the electrode is small. As the pressure increases, as shown in Figure 2 (b), under the second pressure (the second pressure is greater than the first pressure) state, the contact area between protrusion 4221 and protrusion 4223 and the electrode increases. As the pressure continues to increase, as shown in Figure 2 (c), under the third pressure (the third pressure is greater than the second pressure) state, protrusion 4222 that was not originally in contact with the electrode begins to contact the electrode, and protrusion 4222 is in contact with the first electrode 401 and the second electrode 402 at the same time, forming a new conductive network. From state (a) to state (c) in Figure 2, the contact area between protrusion 4221 and first electrode 401 gradually increases. From state (a) to state (b) in Figure 2, the contact area between protrusion 4223 and second electrode 402 gradually increases. However, from state (b) to state (c) in Figure 2, the contact area between protrusion 4223 and second electrode 402 does not increase significantly. This is because after protrusion 4223 is compressed to a certain extent, it reaches its deformation limit and no longer changes significantly. In other words, when the compression amount of the protrusion is within a certain range (i.e., the pressure sensitive range), the contact area changes relatively significantly, thereby effectively detecting pressure. However, outside this range, the contact area changes little or nothing, thereby failing to effectively detect pressure or degrading sensitivity. In this embodiment, by providing two protrusion structures of different heights, the pressure sensitive range of each protrusion structure is differentiated, enabling the pressure sensor to be suitable for detection environments under various pressures, thereby effectively obtaining the range and sensitivity of the pressure sensor.For example, from state (b) to state (c) in Figure 2, the contact area between the protrusion 4223 and the second electrode 402 does not increase significantly, but at this time, the protrusion 4222 begins to contact the electrode to form a new conductive network, that is, a new resistor is incorporated, and the resistance change continues to be more sensitive, thereby improving the range and sensitivity.

[0066] In some embodiments of the present application, at least a portion of the relatively low-height protrusions 422 are spaced apart from the electrode layer 40 along the height direction of the protrusion structures and are configured to contact the electrode layer 40 when subjected to a pressure greater than a predetermined threshold. As shown in FIG2 , the height of protrusion 4223 is greater than that of protrusion 4221, which in turn is greater than that of protrusion 4222. In a first pressure state, protrusion 4222 is spaced apart from the electrode layer 40, protrusion 4221 is just in contact with the electrode layer 40, and protrusion 4223 is in contact with the electrode layer 40 and compressed to a certain degree. When the pressure increases to a second pressure, protrusion 4222 is spaced apart from the electrode layer 40, and protrusions 4221 and 4223 contact the electrode layer 40 and are further compressed. When the pressure increases to a third pressure, the degree of compression of protrusion 4223 remains essentially unchanged compared to the second pressure state, protrusion 4221 is further compressed, and protrusion 4222 begins to contact the electrode layer 40. Through the above method, after the relatively high protrusion structure is compressed to a certain extent, the relatively low protrusion structure can be made to contact the electrode layer, so that the pressure sensitive range of the relatively high protrusion structure and the pressure sensitive range of the relatively low protrusion structure can be effectively staggered, thereby further increasing the range and sensitivity.

[0067] In some embodiments of the present application, along the height direction of the raised structures, the raised structure with the highest height is configured to always be in contact with the electrode layer 40. Continuing to refer to Figures 1 and 2, the protrusion 4223 can be kept in contact with the electrode layer 40 at all times in the natural state and under pressure. The natural state is a state in which the pressure sensor is placed in an atmospheric pressure environment and is not affected by other pressures. The sensitive layer will collapse due to the application of pressure, and the collapse will cause the resistance of the sensor to drop significantly and prematurely. By adding microstructures at locations where the collapse is obvious, the sharp drop in resistance can be effectively delayed, thereby improving the range of the sensor. The ability to use the raised structure with the highest height to provide support for the sensitive layer can effectively reduce the adverse effects of the collapse of the sensitive layer. Specifically, if the sensitive layer collapses, it will cause abnormal contact between the raised structure and the electrode layer, which will in turn cause the change in the contact area of ​​the raised structure to be inconsistent with the design expectations, affecting the measurement accuracy.

[0068] In some embodiments of the present application, the highest raised structure is arranged in the middle area and / or corner area of ​​the sensitive layer 42. The middle area is the area near the middle of the sensitive layer, which is the internal area relative to the edge. If the sensitive layer is a regular shape, such as a circle, rectangle, ellipse, etc., the middle area is the area close to the geometric center of the shape; if the sensitive layer is an irregular shape and there is no clear geometric center of the shape, the sensitive layer is equivalent to the closest regular shape to determine the middle area. In other words, the middle area is the internal area away from the edge area. The corner area is the area near the edge of the sensitive layer. The middle area and the corner area are areas that are relatively easy to collapse. In particular, when the area of ​​the sensitive layer is large, the fixed traction force on the middle area is small and it is easier to collapse. By arranging the raised structures with higher heights in the corners and middle areas that are relatively easy to collapse, more effective support can be provided for the sensitive layer.

[0069] In some embodiments of the present application, the protrusion of the protrusion structure 422 has a cross section perpendicular to the height direction of the protrusion, and the cross section of the protrusion gradually decreases in the direction from the base layer 420 to the electrode layer 40.

[0070] Among them, the so-called gradually decreasing cross-section of the protrusion can be understood as that, in the direction from the base layer 420 to the electrode layer 40, the protrusion of the protrusion structure 422 is in a shape with a large bottom and a small head, for example, it can be a cone or a frustum that gradually becomes thinner from the bottom to the top; it can also be a spherical segment with an arc-shaped change.

[0071] Please refer to Figure 3, which is a schematic diagram of the cross-sectional structure of the pressure sensor of one or more embodiments of the present application. Taking the protrusion as a spherical segment as an example, cross sections are made at different heights to obtain the radii r1, r2 and r3 of different cross sections; along the direction from the base layer 420 to the electrode layer 40 (the X direction shown in the figure), the radius of the cross section gradually becomes smaller. Through this arrangement, when the protrusion is compressed by pressure, the contact area with the electrode layer 40 gradually changes, which can effectively improve the sensitivity of the contact area of ​​the protrusion to pressure. When the higher-level microstructure reaches the compression limit under the action of pressure, the lower-level microstructure adds a contact electrode. Through the microstructure grading and pressure division, the sensitivity of the sensor within a large range can be greatly improved, and the pressure changes can be better distinguished.

[0072] In some embodiments of the present application, the protrusions of the protrusion structure 422 are arranged in a spherical segment shape. This arrangement can further effectively improve the sensitivity of the contact area of ​​the protrusion structure to pressure by utilizing the arc-shaped characteristics of the outer surface of the spherical segment.

[0073] In some embodiments of the present application, the protrusion has a cross-section perpendicular to the height direction of the protrusion, and the maximum cross-sectional dimension of the protrusion is greater than or equal to 1.5 times the spacing between adjacent first and second electrode strips. This arrangement facilitates the use of a single protrusion to directly form an electrical connection with adjacent first and second electrode strips. As shown in Figure 2(c), the protrusion 4222 can contact the first electrode 401 and the second electrode 402 to form a conductive network.

[0074] In some embodiments of the present application, each protrusion structure includes multiple protrusions, and the multiple protrusions of the same protrusion structure are spaced apart on a circular reference line centered at a preset reference point, which can be arranged at equal intervals or at unequal intervals.

[0075] Please refer to Figures 4a and 4b. Figure 4a illustrates the arrangement design of the protrusion structures of the sensitive layer of a pressure sensor according to one or more embodiments of the present application. Figure 4b illustrates the arrangement of the protrusion structures of the sensitive layer of a pressure sensor sample according to one or more embodiments of the present application. In this embodiment, three protrusion structures 422 are provided, each having a different height: protrusion 4221, a protrusion of a first height; protrusion 4222, a protrusion of a second height; and protrusion 4223, a protrusion of a third height. Protrusion 4223 is greater than protrusion 4221, which is greater than protrusion 4222. As shown in Figure 4a, multiple protrusions 4221 are spaced apart along annular reference line 1 centered on a predetermined reference point A; multiple protrusions 4222 are spaced apart along annular reference line 2 centered on a predetermined reference point A; and multiple protrusions 4223 are spaced apart along annular reference line 3 centered on a predetermined reference point A. By arranging protrusions of the same height on the annular reference line, the annular reference line can be used as a unit for design considerations during the design process, thereby reducing the complexity of the arrangement of the protrusion structure.

[0076] In some embodiments of the present application, the preset reference point is set at the maximum deformation area of ​​the sensitive layer 42 under pressure.

[0077] The maximum deformation zone refers to the theoretical maximum deformation zone of the sensitive layer 42 under pressure, ignoring the support provided by the protruding structures 422. Once the maximum deformation zone is determined, the deformation of other regions of the sensitive layer 42 exhibits a certain regularity relative to the maximum deformation zone, using the maximum deformation zone as a reference. By setting the maximum deformation zone at the center of the annular reference line and using the regularity of the deformation of the sensitive layer 42 relative to the maximum deformation zone to set appropriate annular reference lines, the layout complexity of the protruding structures 422 can be further reduced.

[0078] In some embodiments of the present application, the preset reference point is set in the middle area of ​​the sensitive layer 42. The middle area is the area near the middle of the sensitive layer, which is the internal area relative to the edge. If the sensitive layer is a regular shape, such as a circle, rectangle, ellipse, etc., the middle area is the area close to the geometric center of the shape; if the sensitive layer is an irregular shape and there is no clear geometric center of the shape, the sensitive layer is equivalent to the closest regular shape to determine the middle area. In other words, the middle area is the internal area away from the edge area. By setting the preset reference point in the middle area of ​​the sensitive layer 42, more space can be reserved around to set the annular reference line. This can further reduce the arrangement complexity of the raised structure.

[0079] In some embodiments of the present application, the protrusions of the protrusion structure 422 of the same height are divided into at least two groups, and the protrusions of different groups are located on different annular reference lines. In other words, each protrusion structure includes multiple protrusions, and the multiple protrusions of the same protrusion structure are arranged at intervals to form multiple groups of annular structures, and the multiple protrusions of each group of annular structures are located on a single annular reference line.

[0080] Continuing with Figure 4a, there are multiple protrusions 4222, which are organized into multiple groups. As shown in Figure 4a, the first group of protrusions 4222 is arranged along annular reference line 2a, the second group of protrusions 4222 is arranged along annular reference line 2b, and the third group of protrusions 4222 is arranged along annular reference line 2c. In this embodiment, by grouping protrusions of the same height and planning them using the annular reference line as a unit, grouping can further reduce the complexity of the protrusion arrangement, especially when the sensitive layer area is large and the number of protrusion structures is large.

[0081] In some embodiments of the present application, the number of protrusions at the same height on the same annular reference line is no less than three. As shown in Figure 4a, the annular reference line 1 is provided with six protrusions 4221 of the protrusion structure. This arrangement increases the contact area variation gradient, which helps improve the sensitivity of the pressure sensor.

[0082] In some embodiments of the present application, raised structures 422 of different heights are located on different annular reference lines. In other words, multiple reference lines do not cross or overlap. By using different annular reference lines to plan raised structures of different heights, the complexity of the arrangement of the raised structures is reduced.

[0083] In some embodiments of the present application, at least some of the protrusions of protrusion structure 422 are configured to overlap with protrusions of other protrusion structures at different heights after moving along the annular reference line. As shown in Figure 4a, if protrusion 42221 is moved clockwise along reference line 2, it will partially overlap with protrusion 42211 when passing it. This arrangement helps increase the density of the protrusion structures, thereby improving the sensitivity of the pressure sensor.

[0084] In some embodiments of the present application, the annular reference line includes one of a circle, an ellipse, and a polygon. By utilizing the equidistance between the circumference or regular shape and the center, the layout complexity can be reduced.

[0085] In some embodiments of the present application, the protrusions of the protrusion structures 422 have cross-sections perpendicular to the height direction of the protrusions, and the maximum cross-sectional dimension of the protrusions of the relatively smaller protrusion structures 422 is smaller than the maximum cross-sectional dimension of the protrusions of the relatively larger protrusion structures 422. For example, the maximum cross-sectional dimension of the protrusions 4222 may be smaller than the maximum cross-sectional dimension of the protrusions 4223. Since the relatively larger protrusions 4223 share some of the pressure, the maximum cross-sectional dimension of the relatively smaller protrusions 4222 is set relatively small, making them more susceptible to deformation. Consequently, changes in the contact area are more sensitive to pressure, thereby improving the sensitivity of the relatively smaller protrusion structures when in contact with the electrode layer.

[0086] In some embodiments of the present application, the number of relatively small protrusions is greater than the number of relatively large protrusions. As shown in Figure 4a, the number of protrusions 4222 is greater than the number of protrusions 4221, and the number of protrusions 4221 is greater than the number of protrusions 4223. Since the relatively large protrusions share some of the pressure, increasing the number of relatively small protrusions can increase the overall pressure shared by the relatively small protrusions, while also increasing the rate of change of the contact area of ​​the relatively small protrusions with pressure. This can improve detection sensitivity.

[0087] In some embodiments of the present application, the multiple raised structures 422 have at least three different heights. When a higher-level raised structure reaches its compression limit under pressure, a lower-level raised structure is added as a contact electrode. This hierarchical pressure distribution of the raised structures significantly improves the sensor's sensitivity over a wide range, enabling better discrimination of pressure changes. By providing multiple heights, both the range and sensitivity can be increased.

[0088] In some embodiments of the present application, in two adjacent heights of at least two different heights, the ratio of the difference between the relatively larger height and the relatively smaller height to the relatively larger height is 0.3-0.8. For example, the ratio of the height difference between protrusion 4223 and protrusion 4221 to the height of protrusion 4223 is 0.3-0.8. Specifically, the height ratio can be 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, etc. If the height ratio of the two is too small (such as less than 0.3), the contact process between the different protrusion structures and the electrode will lack span, making it easier for the two protrusion structures to reach the compression limit at the same time, making the detection range too small; if the height ratio of the two is too large (such as greater than 0.8), the contact process between the different protrusion structures and the electrode will have too large a span, making it easier for resistance mutations to occur, affecting detection sensitivity. By setting the height ratio to 0.3-0.8, the continuity of the contact area change can be improved, thereby improving sensitivity.

[0089] In some embodiments of the present application, the height of the protrusions of the multiple protrusion structures 422 is 5-200 μm. The height direction is along the direction from the base layer 420 to the electrode layer 40 (the X direction shown in the figure), and the height of the protrusion structure 422 can be measured under a scanning electron microscope. Optionally, the height of the protrusions of the multiple protrusion structures 422 is 10-50 μm. For example, the heights of the three different protrusion structures can be 10 μm, 30 μm, and 50 μm; that is, three different heights of protrusion structures with heights of 10 μm, 30 μm, and 50 μm can be set simultaneously in a sensitive layer. Specifically, the height can be 5 μm, 15 μm, 25 μm, 50 μm, 70 μm, 90 μm, 110 μm, 130 μm, 150 μm, etc. If the height is too small (e.g., less than 5μm), the manufacturing difficulty will increase, and the setting range of different heights will be small, making the height ratio of different protrusion structures difficult to control. If the height is too large (e.g., greater than 200μm), the sensitive layer will easily collapse. When the height is between 10-50μm, the heights of different protrusion structures are relatively even, and the height is easier to control. By setting the height within the above range, the relatively large protrusion structures are prevented from sharing too much pressure, and the pressure sensitivity of the contact area of ​​the relatively small protrusion structures is increased, so that the pressure sensor can have a higher range.

[0090] In some embodiments of the present application, a mold can be used for reverse molding to form a sensitive layer. The mold used for reverse molding of the sensitive layer can be composed of an acrylic plate outer layer and a PDMS (polydimethylsiloxane) inner layer, PDMS is the main body of the mold, and the acrylic outer frame is used to support PDMS. The PDMS solution is mixed with a curing agent, the mass ratio of PDMS solution to curing agent is 10:1, the mixture is placed in a vacuum box for 30 minutes to remove all bubbles, and then heated at 80°C for 1 hour to fully cross-link and cure. After molding, an infrared / ultraviolet laser is used to perform microstructure processing and groove processing on the PDMS mold. Specifically, an infrared laser can be used to process corresponding pits on the PDMS surface according to the designed structural pattern. The depth and diameter of the microstructure can be adjusted by changing the processing power, number of dot counts and processing frequency of the laser. The sensitive layer solution is scraped into the processed groove to achieve reverse molding preparation to obtain a sensitive layer.

[0091] Please refer to Figure 5, which is a schematic diagram of the planar structure of a pressure sensor according to one or more embodiments of the present application. The pressure sensor 400 also includes a corrosion-resistant protective layer 44, which is used to resist corrosion from the main electrolyte inside the lithium battery; a sensitive layer 42 for sensing external forces, and the sensitive layer 42 includes a base layer 420 and at least two protruding structures 422 protruding from the base layer 420 at different heights; the electrode layer 40 and the sensitive layer 42 are encapsulated by a sensitive layer adhesive 48, and the two together constitute a key circuit that responds to pressure; the electrode layer 40 includes an electrode base 403, and a first electrode 401 and a second electrode 402 arranged in an interdigitated manner. The electrode base 403 is used to support membrane structures such as the sensitive layer 42. An insulating layer 46 is located between the sensitive layer 42 and the corrosion-resistant protective layer 44 to protect the sensitive layer 42 from being affected or damaged during the processing and manufacturing of the corrosion-resistant protective layer 44. The insulating layer 46 is connected to the electrode base 403 via an insulating layer adhesive 49. The pressure sensor 400 is a piezoresistive sensor based on the change of contact resistance between the microstructure of the sensitive layer and the coplanar interdigitated electrodes.

[0092] In the above embodiments, the sensing function relies primarily on the change in contact resistance between the conductive sensitive layer and the electrode as pressure changes. Fabricating specific microstructures on the sensitive layer that contact the electrode, such as pyramidal or dome-shaped structures, can alter the contact characteristics between the sensitive layer and the electrode, thereby improving or regulating the sensor's piezoresistive properties. The introduction of specifically shaped microstructures can, to a certain extent, enhance the pressure sensor's performance, including sensitivity and range.

[0093] In some embodiments of the present application, a pressure sensor can be used to detect the internal pressure of a battery. That is, the present application provides a battery cell, which includes a housing and a pressure sensor according to any of the above embodiments, wherein the pressure sensor is disposed inside the housing.

[0094] The embodiments of the present application are applicable to batteries of various systems, such as lithium batteries and sodium batteries. There is no particular limitation on the shape of the battery, which can be cylindrical, square, or any other shape.

[0095] In some embodiments, the battery 100 of the present application includes a housing 10 and a battery cell 20, with the battery cell 20 housed within the housing 10. See FIG6 , which is a schematic diagram of the exploded structure of a battery according to one or more embodiments. The housing 10 provides a storage space for the battery cell 20 and can have various structures. In some embodiments, the housing 10 can include a first portion 11 and a second portion 12, which overlap each other and together define a storage space for the battery cell 20. The second portion 12 can be a hollow structure with one end open. The first portion 11 can be a plate-like structure, with the first portion 11 overlapping the open side of the second portion 12, so that the first portion 11 and the second portion 12 together define a storage space. Alternatively, the first portion 11 and the second portion 12 can each be a hollow structure with one end open, with the open side of the first portion 11 overlapping the open side of the second portion 12. Of course, the housing 10 formed by the first portion 11 and the second portion 12 can have various shapes, such as a cylinder or a rectangular parallelepiped.

[0096] In the battery 100, there may be multiple battery cells 20, and the multiple battery cells 20 may be connected in series, in parallel, or in a hybrid connection. A hybrid connection refers to a combination of series and parallel connections among the multiple battery cells 20. The multiple battery cells 20 may be directly connected in series, in parallel, or in a hybrid connection, and then the entire battery cell 20 may be housed within the housing 10. Alternatively, the battery 100 may be constructed by first connecting multiple battery cells 20 in series, in parallel, or in a hybrid connection to form a battery module, which is then connected in series, in parallel, or in a hybrid connection to form a complete battery module, and then housed within the housing 10. The battery 100 may also include other structures, such as a busbar assembly for electrically connecting the multiple battery cells 20.

[0097] Each battery cell 20 may be a secondary battery, such as a lithium-ion battery, a sodium-ion battery, a magnesium-ion battery, or an aluminum-ion battery, but is not limited thereto. The battery cell 20 may be cylindrical, flat, rectangular, or have other shapes.

[0098] Battery manufacturing methods include laminated and wound types. Laminated batteries offer uniform current collection, low internal resistance, and high specific power. However, to ensure accuracy, they require extremely high mold precision, high equipment investment, and a complex process, resulting in low production efficiency. Wound batteries are simple to manufacture, with moderate equipment precision requirements during the production and assembly processes. They offer high production efficiency and low costs. In terms of performance, wound batteries offer excellent high and low temperature performance, very fast charging, an extremely long lifespan, a stable high output voltage, a sturdy structure, and strong shock resistance.

[0099] Please refer to Figure 7, which is a schematic diagram of the exploded structure of a battery cell 20 in one or more embodiments. A battery cell 20 is the basic unit within a battery that converts chemical energy into electrical energy. The battery cell 20 includes an end cap 21, a housing 22, an electrode assembly 23, and other functional components.

[0100] The end cap 21 refers to a component that covers the opening of the shell 22 to isolate the internal environment of the battery cell 20 from the external environment. Without limitation, the shape of the end cap 21 can be adapted to the shape of the shell 22 to match the shell 22. Optionally, the end cap 21 can be made of a material with a certain hardness and strength (such as aluminum alloy). In this way, the end cap 21 is not easily deformed when squeezed or collided, so that the battery cell 20 can have a higher structural strength and improved safety performance. Functional components such as electrode terminals 21a can be provided on the end cap 21. The electrode terminal 21a can be used to electrically connect to the electrode assembly 23 for outputting or inputting electrical energy of the battery cell 20. In some embodiments, the end cap 21 can also be provided with a pressure relief mechanism for releasing internal pressure when the internal pressure or temperature of the battery cell 20 reaches a threshold. The material of the end cap 21 can also be various, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc. In some embodiments, an insulating member may be provided inside the end cap 21 to isolate the electrical connection components in the housing 22 from the end cap 21 to reduce the risk of short circuit. For example, the insulating member may be made of plastic, rubber, or the like.

[0101] The housing 22 is a component that cooperates with the end cap 21 to form the internal environment of the battery cell 20, wherein the formed internal environment can be used to accommodate the electrode assembly 23, electrolyte, and other components. The housing 22 and the end cap 21 can be independent components. An opening can be provided in the housing 22, and the end cap 21 is closed at the opening to form the internal environment of the battery cell 20. The end cap 21 and the housing 22 can also be integrated. Specifically, the end cap 21 and the housing 22 can form a common connection surface before other components are inserted into the housing. When the interior of the housing 22 needs to be encapsulated, the end cap 21 is closed to the housing 22. The housing 22 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylindrical shape, a hexagonal prism, etc. Specifically, the shape of the housing 22 can be determined according to the specific shape and size of the electrode assembly 23. The housing 22 can be made of various materials, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc.

[0102] The electrode assembly 23 is a component in the battery cell 20 where electrochemical reactions occur. One or more electrode assemblies 23 may be contained in the housing 22. The electrode assembly 23 is mainly formed by winding or stacking cathode sheets and anode sheets, and a separator is usually provided between the cathode sheets and the anode sheets. The parts of the cathode sheets and the anode sheets with active materials constitute the main body of the electrode assembly, and the parts of the cathode sheets and the anode sheets without active materials each constitute a tab 23a. The cathode tab and the anode tab may be located together at one end of the main body or respectively at both ends of the main body. During the charge and discharge process of the battery, the cathode active material and the anode active material react with the electrolyte, and the tab 23a connects the electrode terminals to form a current loop.

[0103] The cathode electrode generally includes a cathode current collector and a cathode film layer arranged on the cathode current collector.

[0104] The cathode current collector generally adopts a conventional metal foil or a composite current collector (a metal material can be disposed on a polymer substrate to form a composite current collector). As an example, the cathode current collector can adopt aluminum foil.

[0105] The cathode film layer includes cathode active materials as well as a binder, a conductive agent and other optional additives.

[0106] As an example, the cathode active material may include one or more of lithium transition metal oxides, lithium phosphates with an olivine structure and their respective modified compounds, transition metal oxides, polyanionic compounds, and Prussian blue analogs. Examples of lithium transition metal oxides may include one or more of lithium cobalt oxide, lithium nickel oxide, lithium manganese oxide, lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide, lithium nickel cobalt aluminum oxide, and their modified compounds. Examples of lithium phosphates with an olivine structure may include one or more of lithium iron phosphate, a composite material of lithium iron phosphate and carbon, lithium manganese phosphate, a composite material of lithium manganese phosphate and carbon, lithium manganese iron phosphate, a composite material of lithium manganese iron phosphate and carbon, and their modified compounds. The modified compounds of the above materials may be doping modification and / or surface coating modification of the materials. These materials can all be obtained through commercial channels.

[0107] As an example, the conductive agent may be one or more of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, Super P (SP), graphite, and carbon nanofibers.

[0108] As an example, the binder can be one or more of styrene-butadiene rubber (SBR), water-based acrylic resin, polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene-vinyl acetate copolymer (EVA), polyacrylic acid (PAA), carboxymethyl cellulose (CMC), polyvinyl alcohol (PVA) and polyvinyl butyral (PVB).

[0109] As an example, other optional auxiliary agents may be thickening and dispersing agents (such as sodium carboxymethyl cellulose CMC-Na), and PTC thermistor materials.

[0110] The anode plate generally includes an anode current collector and an anode film layer disposed on the anode current collector.

[0111] The anode current collector may be a conventional metal foil or a composite current collector (for example, a metal material may be disposed on a polymer substrate to form a composite current collector). As an example, the anode current collector may be a copper foil.

[0112] The anode film layer includes an anode active material, a binder, a conductive agent and other optional additives.

[0113] The anode active material may include one or more of silicon-based materials, silicon-carbon materials, carbon materials, and selenium-based materials. Specifically, it includes one or more of artificial graphite, natural graphite, hard carbon, soft carbon, silicon-based materials and selenium-based materials. Silicon-based materials can be selected from one or more of elemental silicon, silicon oxide compounds (such as silicon monoxide), silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. Selenium-based materials can be selected from one or more of elemental selenium, selenium oxide compounds, and selenium alloys. These materials can all be obtained through commercial channels. In some embodiments of the present application, the design concept of active density is also applicable to sodium batteries, or in other words, the type of battery is not limited. The present application does not limit the selection and matching of electrode materials. Different combinations of anode and cathode materials may have different active density control standards.

[0114] As an example, the conductive agent may be one or more of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphite, and carbon nanofibers.

[0115] As an example, the binder may be one or more of styrene-butadiene rubber (SBR), water-based acrylic resin, polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene-vinyl acetate copolymer (EVA), polyvinyl alcohol (PVA) and polyvinyl butyral (PVB).

[0116] As an example, other optional auxiliary agents may be thickening and dispersing agents (such as sodium carboxymethyl cellulose CMC-Na), and PTC thermistor materials.

[0117] In one embodiment, the cathode active material, the anode active material, the binder, and the conductive agent are mixed in proportion to obtain cathode slurry and anode slurry, and then the cathode slurry and anode slurry are coated on the corresponding current collectors respectively, and dried after coating to obtain cathode and anode pole pieces.

[0118] Furthermore, the battery cell also includes a separator and an electrolyte.

[0119] The separator is placed between the cathode and anode electrodes. As an insulating layer, it effectively prevents contact between the cathode and anode electrodes, which could cause an internal short circuit, while allowing electrolyte ions to pass smoothly. The performance of the separator determines the battery's interface structure and internal resistance, directly affecting the battery's mechanical strength and safety.

[0120] The specific type of separator material is not limited. Any material known in the art for battery separators can be used, and those skilled in the art can select the material based on their needs. For example, the separator material can include one or more of polyolefins, fluoropolymers, cellulose, and fiberglass. Polyolefins can include, but are not limited to, one or more of polypropylene and polyethylene. All of these materials are commercially available.

[0121] In some embodiments, the isolation membrane includes a base membrane and a coating located on one side / both sides of the base membrane, and the coating includes a filler. The filler may include an inorganic material, a polymer adhesive, and a dispersant. The inorganic material includes one or more of boehmite and silica, the polymer adhesive material includes one or more of PVDF (polyvinylidene fluoride) and polystyrene-acrylate; the dispersant material includes polyvinyl alcohol, etc. By providing a coating on one side / both sides of the isolation membrane, the performance of the isolation membrane can be improved and regulated. The performance of the isolation membrane can be regulated by regulating the type of filler. For example, a filler with heat insulation and heat resistance can be added to improve the heat resistance of the isolation membrane. The specific type of the base membrane material is not limited, and may include but is not limited to one or more of polyethylene, polypropylene and glass fiber. These materials can all be obtained through commercial channels.

[0122] The electrolyte plays the role of conducting ions between the cathode electrode and the anode electrode, and may include electrolyte salts and solvents.

[0123] As an example, the electrolyte salt can be selected from one or more of lithium hexafluorophosphate (LiPF6), lithium tetrafluoroborate (LiBF4), lithium perchlorate (LiClO4), lithium hexafluoroarsenate (LiAsF6), lithium bis(fluorosulfonyl)imide (LiFSI), lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), lithium trifluoromethanesulfonate (LiTFS), lithium difluorooxalatoborate (LiDFOB), lithium dioxalatoborate (LiBOB), lithium difluorophosphate (LiPO2F2), lithium difluorobis(oxalatophosphate) (LiDFOP) and lithium tetrafluorooxalatophosphate (LiTFOP).

[0124] As an example, the solvent may be selected from ethylene carbonate (EC), propylene carbonate (PC), methyl ethyl carbonate (EMC), diethyl carbonate (DEC), dimethyl darbonate (DMC), dipropyl carbonate (DPC), methyl propyl carbonate (MPC), ethyl propyl carbonate (EPC), butylene carbonate (BC), fluoroethylene carbonate (FEC), methyl formate (MF), methyl acetate (MA), ethyl acetate (EA), n-propyl acetate (PA), methyl propionate (MP), ethyl propionate (EP), n-propyl propionate (NP), propylene glycol (PEG), propylene glycol (PP), propylene glycol (C1), propylene glycol (C2), propylene glycol (C3), propylene glycol (C4), propylene glycol (C5), propylene glycol (C6), propylene glycol (C7), propylene glycol (C8), propylene glycol (C9), propylene glycol (D1), propylene glycol (D2), propylene glycol (D3), propylene glycol (D4), propylene glycol (D5), propylene glycol (D6), propylene glycol (D7), propylene glycol (D8), propylene glycol (D9), propylene glycol (D10), propylene glycol (D11), propylene glycol (D12), propylene glycol (D13), propylene glycol (D14), propylene glycol (D15), propylene glycol (D16), propylene glycol (D17), propylene glycol (D18), propylene glycol (D19), propylene glycol (D20), propylene glycol (D21), propylene glycol (D22), propylene glycol (D23), propylene glycol (D24), propylene glycol (D25), propylene glycol (D26), propylene glycol (D27), propylene glycol (D28), propylene glycol (D29), propylene glycol (D31), propylene glycol (D32), propylene glycol (D33), propylene glycol (D34), propylene glycol (D35), propylene glycol (D36), propylene glycol (D37), propylene glycol (D38), propylene glycol (D39), propylene One or more of the group consisting of propionate (PP), methyl butyrate (Methyl Butyrate MB), ethyl butyrate (Ethyl Butyrate, EB), 1,4-butyrolactone (1,4-Butyrolactone, GBL), tetramethylene sulfone (SF), dimethyl sulfone (Methyl Sulfone, MSM), methyl ethyl sulfone (Methyl Ethyl Sulfone, EMS) and diethyl sulfone (Diethyl Sulfone, ESE).

[0125] In some embodiments, the electrolyte further includes additives. For example, the additives may include anode film-forming additives, cathode film-forming additives, or additives capable of improving certain battery properties, such as additives that improve battery overcharge performance, additives that improve battery high-temperature performance, and additives that improve battery low-temperature performance.

[0126] The battery disclosed in the embodiments of the present application can be used in electrical devices that use the battery as a power source or various energy storage systems that use the battery as an energy storage element. The electrical devices may be, but are not limited to, mobile phones, tablets, laptops, electric toys, power tools, battery cars, electric cars, ships, spacecraft, and the like. Among them, electric toys may include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, and the like, and spacecraft may include airplanes, rockets, space shuttles, and spacecraft, and the like.

[0127] The energy storage system can be a hydropower, thermal, wind power, solar power station or other energy storage power supply system.

[0128] For the convenience of description, the following embodiments are described by taking a vehicle 1000 as an example of an electrical device according to an embodiment of the present application.

[0129] Please refer to Figure 8, which is a schematic structural diagram of a vehicle 1000 in some embodiments of the present application. The vehicle 1000 can be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle can be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 100 is provided inside the vehicle 1000, and the battery 100 can be provided at the bottom, head or tail of the vehicle 1000. The battery 100 can be used to power the vehicle 1000. For example, the battery 100 can serve as an operating power source for the vehicle 1000. The vehicle 1000 may also include a controller 200 and a motor 300. The controller 200 is used to control the battery 100 to power the motor 300, for example, for starting, navigating and driving the vehicle 1000.

[0130] In some embodiments of the present application, the battery 100 can serve not only as an operating power source for the vehicle 1000, but also as a driving power source for the vehicle 1000, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000.

[0131] The above-mentioned electrical equipment and energy storage systems are also within the protection scope of this application.

[0132] The above description is only an implementation method of the present application and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the description and drawings of this application, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A pressure sensor, wherein: The pressure sensor comprises: Electrode layer; A sensitive layer, wherein the sensitive layer comprises a base layer and at least two protrusion structures protruding from the base layer at different heights, each of the protrusion structures comprises at least one protrusion, each of the protrusions is located on a side of the base layer facing the electrode layer, and a contact area between each of the protrusions and the electrode layer is configured to change with a change in the pressure applied to the electrode layer.

2. The pressure sensor according to claim 1, wherein: Along the height direction of the protruding structures, at least a portion of the protruding structures with relatively low heights are spaced apart from the electrode layer, and are configured to contact the electrode layer after the pressure applied is greater than a predetermined threshold.

3. The pressure sensor according to claim 1 or 2, wherein: Along the height direction of the protruding structures, the protruding structure with the highest height is configured to always be in contact with the electrode layer.

4. The pressure sensor according to claim 3, wherein: The protruding structure with the highest height is arranged in the middle area and / or corner area of ​​the sensitive layer.

5. The pressure sensor according to any one of claims 1 to 4, wherein: The protrusions have a cross section perpendicular to a height direction of the protrusions, and the cross section of each of the protrusions gradually becomes smaller in a direction from the base layer to the electrode layer.

6. The pressure sensor according to claim 5, wherein: The protrusion is arranged in a spherical segment shape.

7. The pressure sensor according to any one of claims 1 to 6, wherein: Each type of the protrusion structure includes a plurality of the protrusions, and the plurality of protrusions of the same type of the protrusion structure are arranged at intervals on a circular reference line centered at a preset reference point.

8. The pressure sensor according to claim 7, wherein: The preset reference point is set at the maximum deformation area of ​​the sensitive layer under pressure.

9. The pressure sensor according to claim 7 or 8, wherein: The preset reference point is set in the middle area of ​​the sensitive layer located inside the edge area.

10. The pressure sensor according to any one of claims 7 to 9, wherein: Each type of the protrusion structure includes a plurality of the protrusions, and the plurality of the protrusions of the same type of the protrusion structure are arranged at intervals to form a plurality of groups of annular structures, and the plurality of the protrusions of each group of annular structures are located on one of the annular reference lines.

11. The pressure sensor according to any one of claims 7 to 10, wherein: The number of the protrusions at the same height on the same annular reference line is not less than three.

12. The pressure sensor according to any one of claims 7 to 11, wherein: The protruding structures of different heights are located on different annular reference lines.

13. The pressure sensor according to any one of claims 7 to 12, wherein: At least part of the protrusions are configured to be able to overlap with protrusions at other heights after moving along the annular reference line where the protrusions are located.

14. The pressure sensor according to any one of claims 7 to 13, wherein: The annular reference line includes one of a circle, an ellipse, and a polygon.

15. The pressure sensor according to any one of claims 1 to 14, wherein: The protrusion has a cross section perpendicular to the height direction of the protrusion, and the maximum cross-sectional dimension of the protrusion of the protrusion structure with a relatively smaller height is smaller than the maximum cross-sectional dimension of the protrusion of the protrusion structure with a relatively larger height.

16. The pressure sensor according to any one of claims 1 to 15, wherein: The number of the protruding structures with relatively smaller heights is greater than the number of the protruding structures with relatively larger heights.

17. The pressure sensor according to any one of claims 1 to 16, wherein: The plurality of protruding structures have at least three different heights.

18. The pressure sensor according to any one of claims 1 to 17, wherein: In two adjacent heights of the at least two different heights, the ratio of the difference between the relatively larger height and the relatively smaller height to the relatively larger height is 0.3-0.

8.

19. The pressure sensor according to any one of claims 1 to 18, wherein: The height of the plurality of protruding structures is 5-200 μm.

20. The pressure sensor according to any one of claims 1 to 19, wherein: The material of the sensitive layer includes a flexible substrate and conductive particles dispersed in the flexible substrate.

21. The pressure sensor according to claim 20, wherein: The conductive particles include graphite particles and carbon nanotube particles.

22. The pressure sensor according to any one of claims 1 to 21, wherein: The electrode layer includes a first electrode and a second electrode arranged in an interdigitated manner.

23. The pressure sensor according to claim 22, wherein: The first electrode includes a plurality of first electrode strips arranged side by side and at intervals, the second electrode includes a plurality of second electrode strips arranged side by side and at intervals, at least some of the first electrode strips are arranged in the spacing area between the second electrode strips, the width of the first electrode strips and the second electrode strips is 10-200 μm, and the spacing distance between adjacent first electrode strips and second electrode strips is 5-200 μm.

24. The pressure sensor according to claim 22 or 23, wherein: The width of the first electrode strips and the second electrode strips is 50-150 μm, and the interval between adjacent first electrode strips and second electrode strips is 20-80 μm.

25. The pressure sensor according to claim 23 or 24, wherein: The protrusion has a cross section perpendicular to the height direction of the protrusion, and the maximum cross-sectional dimension of the protrusion is greater than or equal to 1.5 times the spacing distance.

26. A battery cell, wherein: The battery cell comprises a housing and a pressure sensor as claimed in any one of claims 1 to 25, wherein the pressure sensor is arranged inside the housing.

27. An electrical device, wherein: The electric device comprises the battery cell as claimed in claim 26.

Citation Information

Patent Citations

  • Pressure sensor

    CN109997021A

  • Resistance-type flexible pressure sensor and preparation method thereof

    CN111060238A

  • Piezoresistive flexible three-dimensional force sensor array and preparation method thereof

    CN111537115A

  • Flexible pressure sensor with microstructure

    CN112033582A

  • Flexible pressure sensor with pressure-sensitive structure

    CN112378554A

Cited By

  • Flexible pressure sensor and preparation method thereof

    CN119880206A