Friction stir spot welding tool
The friction stir spot welding tool with a step-shaped pin tip surface addresses the high pressure requirements in joining fiber-reinforced materials by actively scraping and extruding material, resulting in lower pressing forces and more economical equipment.
Patent Information
- Application Number
- PCT/JP2024/009545
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-22
- Filing Date
- 2024-03-12
- Publication Date
- 2024-11-28
AI Technical Summary
Friction stir spot welding tools require high welding pressure, especially when joining fiber-reinforced thermoplastic resin members, leading to larger and more expensive equipment due to the need for high rigidity and large arms to manage reaction forces.
A friction stir spot welding tool with a cylindrical pin and shoulder, where the pin is press-fitted into the overlapping portion while the shoulder is retracted, featuring a step-shaped portion on the pin's tip surface to reduce welding pressure by actively scraping and extruding material, thereby reducing the required pressing force.
The step-shaped portion on the pin's tip surface allows for lower welding pressure, reducing equipment size and cost by efficiently cutting continuous fibers and extruding material, enabling effective friction stir spot welding with reduced pressing force.
Smart Images

Figure JP2024009545_28112024_PF_FP_ABST
Abstract
Description
Friction stir spot welding tools
[0001] The present disclosure relates to a friction stir spot welding tool having a pin and a shoulder.
[0002] Friction stir welding is known as a method for joining two or more overlapping members, such as metal members and fiber-reinforced thermoplastic resin members. For friction stir welding, a friction stir spot welding tool equipped with a pin and a shoulder having a hollow portion for accommodating the pin is sometimes used. For example, in a shoulder-first process, the shoulder is protruded and pressed into the overlapping portion of the members to be joined, while the pin is retracted to accommodate overflow material (see, for example, Patent Document 1). On the other hand, in a pin-first process, the pin is pressed into the overlapping portion while the shoulder is retracted.
[0003] In the pin-first process, when a high welding pressure is required for the friction stir spot welding of the overlapping portions, the equipment, including the welding tool, becomes large and expensive. For example, when joining overlapping portions of fiber-reinforced thermoplastic resin members, a large welding pressure is required to cut the continuous fibers contained therein. In this case, in order to reduce the amount of deflection due to the reaction force of the welding pressure, the arms to which the welding tool is attached must be large and highly rigid.
[0004] JP 2015-186869 A
[0005] The present disclosure aims to reduce the welding pressure applied to overlapping portions of members to be joined in a friction stir spot welding tool that employs a pin-first process.
[0006] A friction stir spot welding tool according to one aspect of the present disclosure comprises a cylindrical pin that rotates around an axis, a shoulder having a hollow portion through which the pin is inserted, and a drive unit that drives the pin to rotate while pressing it into objects to be joined, and drives the shoulder to retract relative to the objects to be joined, and at least a portion of the tip surface of the pin is provided with a step-shaped portion that forms a step in the rotational direction of the pin.
[0007] According to the present disclosure, it is possible to provide a friction stir spot welding tool that employs a pin-first process and that can reduce the welding pressure applied to the overlapping portions of the workpieces to be joined.
[0008] FIG. 1 is a schematic diagram showing the configuration of a friction stir spot welding apparatus including a friction stir spot welding tool according to an embodiment of the present disclosure. FIG. 2 is a diagram showing the configuration of a first member and a second member to be friction stir spot welded. FIG. 3 is a diagram showing a joining procedure using a pin-first process using a friction stir spot welding tool. FIG. 4 is a perspective view and a side view showing the shape of a pin and its tip surface of a friction stir spot welding tool according to an embodiment of the present disclosure, along with a comparative example. FIG. 5 is a graph showing the relationship between the press-fit amount of the pin into a test piece and the joining time for an embodiment and a comparative example. FIG. 6 is a graph showing the relationship between the press-fit amount and the joining time when the pin of the embodiment is pressed into the test piece by changing the pressure applied to the pin. FIG. 7(A) is a diagram showing the behavior of the stirring material in the shoulder-first process, and FIG. 7(B) is a diagram showing the behavior of the stirring material in the pin-first process. FIGS. 8(A) to 8(C) are perspective views showing other examples of pin tip shapes for a friction stir spot welding tool. FIGS. 9(A) to 9(F) are plan views showing modified shapes of the pin tip surface shown in FIG. 4.
[0009] The following describes in detail embodiments of the present disclosure with reference to the drawings. A friction stir spot welding apparatus equipped with a friction stir spot welding tool according to the present disclosure can be used to manufacture various joined structures formed by spot welding two or more overlapping structural members, such as plates, frames, exterior materials, or columns made of metal, resin, or thermoplastic resin molded bodies containing fibrous materials. The joined structures thus manufactured are components for structures such as aircraft, railway vehicles, and automobiles.
[0010] [Configuration of Friction Stir Spot Welding Apparatus] Figure 1 is a schematic diagram showing the configuration of a friction stir spot welding apparatus M according to one embodiment of the present disclosure. The friction stir spot welding apparatus M includes a double-action friction stir spot welding tool 1, a tool drive unit 2 that drives the tool 1 to rotate and elevate, and a controller 20 that controls the operation of each part of the friction stir spot welding apparatus M. Note that although Figure 1 includes directional indications of "up" and "down," this is for ease of explanation and is not intended to limit the actual direction in which the tool 1 is used.
[0011] The tool 1 is supported by various tool fixing parts. For example, the tool fixing part is the tip of an articulated robot. A backup 15 is arranged facing the lower end surface of the tool 1. The workpiece 3 to be welded is arranged between the tool 1 and the backup 15. The workpiece 3 to be welded is formed by overlapping at least two members. FIG. 1 shows an example in which an overlapping portion 30, in which a part of a first member 31 made of a flat plate and a part of a second member 32 also made of a flat plate overlap in the vertical direction, is arranged as the workpiece 3 to be welded between the tool 1 and the backup 15.
[0012] The tool 1 includes a pin 11, a shoulder 12, a clamp 13, and a spring 14. The pin 11 is a cylindrical member and is arranged so that its axis extends in the vertical direction. The pin 11 is rotatable about the axis R, and is also movable up and down along the rotation axis R. When the tool 1 is in use, the rotation axis R is aligned with the spot joining position W at the overlapping portion 30.
[0013] The shoulder 12 is a cylindrical member having a hollow portion through which the pin 11 is inserted. The axis of the shoulder 12 is coaxial with the axis of the pin 11, i.e., the rotation axis R. The shoulder 12 is rotatable about the rotation axis R and can move up and down along the rotation axis R. The tool 1 of this embodiment is a double-acting tool in which the pin 11 and the shoulder 12 move independently in the axial direction. That is, the shoulder 12 and the pin 11 inserted in the hollow portion can both rotate about the rotation axis R and move relatively in the direction of the rotation axis R. Specifically, the pin 11 and the shoulder 12 can not only simultaneously move up and down along the rotation axis R, but also independently move, with one descending while the other ascends.
[0014] The clamp 13 is a cylindrical member having a hollow portion into which the shoulder 12 is inserted. The axis of the clamp 13 is also coaxial with the rotation axis R. The clamp 13 does not rotate around its axis, but moves up and down along the rotation axis R, that is, moves forward and backward. The clamp 13 serves to surround the outer periphery of the pin 11 or the shoulder 12 when they perform friction stirring. The enclosure by the clamp 13 prevents the friction stir material from scattering, and enables the friction stir spot welded portion to be finished smoothly.
[0015] The spring 14 is attached to the upper end side of the clamp 13 and urges the clamp 13 downward toward the overlapping portion 30. The clamp 13 is attached to the tool fixing portion via the spring 14. The backup 15 has a flat surface that abuts against the underside of the overlapping portion 30 to be joined. The backup 15 is a backing member that supports the overlapping portion 30 when the pin 11 or shoulder 12 is press-fitted into the overlapping portion 30. The clamp 13, urged by the spring 14, presses the overlapping portion 30 against the backup 15.
[0016] The tool driving unit 2 includes a rotation driving unit 21, a pin driving unit 22, a shoulder driving unit 23, and a clamp driving unit 24. The rotation driving unit 21 includes a motor, a drive gear, etc., and drives the pin 11 and the shoulder 12 to rotate about the rotation axis R. The pin driving unit 22 is a mechanism that moves the pin 11 back and forth along the rotation axis R. The pin driving unit 22 drives the pin 11 to press the pin 11 into the overlapping portion 30 and retract it from the overlapping portion 30. The shoulder driving unit 23 is a mechanism that moves the shoulder 12 back and forth along the rotation axis R, causing the shoulder 12 to press into and retract from the overlapping portion 30. The clamp driving unit 24 is a mechanism that moves the clamp 13 back and forth along the rotation axis R. The clamp driving unit 24 moves the clamp 13 toward the overlapping portion 30 and presses the overlapping portion 30 against the backup 15. At this time, the biasing force of the spring 14 acts.
[0017] The controller 20 is comprised of a microcomputer or the like, and executes a predetermined control program to control the operation of the tool driving unit 2. Specifically, the controller 20 controls the rotation driving unit 21 to cause the pin 11 and the shoulder 12 to perform a required rotational movement. The controller 20 also controls the pin driving unit 22, the shoulder driving unit 23, and the clamp driving unit 24 to cause the pin 11, the shoulder 12, and the clamp 13 to perform a required forward / backward movement movement.
[0018] 2 is a diagram showing the configuration of a first member 31 and a second member 32 to be friction stir spot welded. Here, an overlapping portion 30 is shown, in which a portion of a plate-shaped first member 31 and a portion of a plate-shaped second member 32 are overlapped vertically. The overlapping portion 30 may be an overlapping portion between a plate and a frame or a columnar material, or an overlapping portion between frames. The overlapping portion 30 has a mating surface BD, in which a joining surface 31A on the lower surface of the first member 31 and a joining surface 32A on the upper surface of the second member 32 are in direct contact with each other. One or more other plates may be interposed between the first member 31 and the second member 32.
[0019] FIG. 2 shows an example in which the first member 31 and the second member 32 are formed by laminating multiple layers of prepregs, each of which is made of a continuous fiber array impregnated with a thermoplastic resin. FIG. 2 also shows a portion of the sheet stack 33 constituting the first member 31. The sheet stack 33 includes a first sheet layer 33A, a second sheet layer 33B, and a third sheet layer 33C, each of which is made of a sheet of a continuous fiber array impregnated with a thermoplastic resin. The first sheet layer 33A is a sheet approximately 0.1 mm to 0.5 mm thick, in which a large number of continuous fibers 34 are aligned in a predetermined alignment direction and the array is impregnated with a thermoplastic resin to form an integrated structure. The second sheet layer 33B and the third sheet layer 33C are similar to the above, but the alignment directions of the continuous fibers 34 are mutually different. The second member 32 is also a plate made of a multilayer laminate of sheets similar to the first member 31.
[0020] When friction stir spot welding of the overlapping portion 30 is performed using the tool 1, the tool 1 is pressed in to cut the continuous fibers 34 while friction stirring the thermoplastic resin of the impregnating material. The prepreg molded body is an example of the constituent material of the first member 31 and the second member 32. For example, the overlapping portion 30 may be formed using two or more metal plates such as aluminum or steel. As an example, the first member 31, which is the side into which the tool 1 is first pressed in, may be made of an aluminum alloy, and the second member 32 may be made of high-tensile steel.
[0021] [Method of Using the Tool] Next, a method of using the tool 1 exemplified in this embodiment will be described. Methods of using the friction stir spot welding apparatus M can be roughly divided into a pin-first process in which the pin 11 of the tool 1 is first pressed into the overlapping portion 30 of the workpieces 3, and a shoulder-first process in which the shoulder 12 is first pressed into the overlapping portion 30. In this embodiment, the controller 20 drives the tool 1 to operate in the pin-first process.
[0022] 3 is a diagram showing processes P11 to P14 of the friction stir spot welding method using the pin-first process. Here, the process for friction stir spot welding of an overlapping portion 30 of a first member 31 and a second member 32 is shown in simplified form. Process P11 shows a preheating step for the overlapping portion 30. With the lower end of the tool 1 in contact with the surface of the first member 31, the pin 11 and shoulder 12 are rotated around their axis at a predetermined high speed.
[0023] Process P12 shows the step of press-fitting the pin 11. As indicated by the outline arrow in the figure, the pin 11 is rotated around its axis and lowered to press-fit it into the overlapping portion 30, while the shoulder 12 is retracted upward. This action agitates the material in the press-fit region of the pin 11. Furthermore, the overflowing material OF that overflows from the overlapping portion 30 due to the press-fitting is released into the annular region between the pin 11 and the clamp 13, which is created by the retraction of the shoulder 12 (see arrow a1).
[0024] Process P13 shows a backfilling process of the overflowed material OF. In the backfilling process, the pin 11 is raised and retracted, while the shoulder 12 is lowered. By lowering the shoulder 12, the overflowed material OF that has escaped to the annular region is backfilled into the press-fit region of the pin 11, as shown by arrow a2.
[0025] Process P14 represents a smoothing step. The lower end surfaces of the pin 11 and shoulder 12 are returned to the same height as the surface of the first member 31, and then both are rotated to smooth the spot-bonded portion. Note that if the first member 31 is made of a thermoplastic resin, the pin 11 and shoulder 12 may not be rotated in process P14, and the spot-bonded portion may simply be pressed. Through the above process, the stir-welded portion 4a is formed, and the first member 31 and the second member 32 are spot-bonded at the overlapping portion 30.
[0026] [Embodiment of Tool Pin] Figure 4 is a perspective view and a side view showing the shape of the pin 11 and its tip portion 11T of the friction stir spot welding tool 1 according to an example of the present disclosure, along with a comparative example. Conventionally, the tip portion 11T of the pin 11 has a circular tip surface 50 made of a flat surface, as shown in the <Comparative Example> section. In other words, the tip surface 50 is a flat surface without any steps or the like. When a pin-first process is performed using a tool 1 equipped with a pin 11 having such a tip surface 50, a high welding pressure may be required.
[0027] An example of a welding process requiring a high welding pressure is when the workpieces 3 are composed of a sheet stack 33 made of thermoplastic resin prepreg reinforced with continuous fibers 34, such as thermoplastic CFRP, as shown in FIG. 2 , and at least the first member 31 is formed from the sheet stack 33. In the case of such a first member 31, the pin 11 is pressed into the workpiece 31 while cutting the continuous fibers 34 during friction stirring. To cut the continuous fibers 34, a large pressure must be applied to the tool 1. Experiments conducted by the present inventors have shown that approximately 60% of the total pressure applied to the tool 1 is used to cut the continuous fibers of the thermoplastic CFRP. The remaining approximately 40% of the total pressure is used exclusively to push the overflow material OF into the annular region around the pin 11.
[0028] When a high welding pressure is required, measures to deal with the reaction force are necessary. For example, when the tool 1 is mounted on the tip of a robot arm, the rigidity of the robot arm needs to be set high so that bending deformation or the like does not occur due to the reaction force. Increasing the rigidity requires increasing the size of the robot arm or using a high-strength arm material, which results in an increase in the size and cost of the friction stir spot welding apparatus M including the tool 1.
[0029] The tip portion 11T of the pin 11 according to the present disclosure has a tip surface 5 shaped to suppress the joining pressure force. As shown in the <Example> section of Figure 4 , the tip surface 5 is circular when viewed in the axial direction, as in the conventional case, but the tip surface 5 is provided with a stepped portion 51 that forms a step in the rotational direction F of the pin 11. The step of the stepped portion 51 is a radial step extending radially from the center point CP of the circular tip surface 5 to the outer periphery of the circle. A plurality of stepped portions 51 are arranged in the circumferential direction of the tip surface 5. Figure 4 shows an example in which eight radial steps are arranged at equal intervals in the circumferential direction of the tip surface 5.
[0030] The stepped portion 51 is shallowest at the center point C of the tip surface 5 and deepest at the outer periphery of the tip surface 5. In other words, the stepped portion 51 has a shape in which the step height h gradually increases from the center point C toward the radially outer side of the tip surface 5. As a result of forming eight such stepped portions 51 at equal intervals, eight fan-shaped surfaces 52 of the same size are lined up in the circumferential direction on the tip surface 5. These fan-shaped surfaces 52 are surfaces with an inclination corresponding to the step height h of the stepped portion 51.
[0031] Referring also to the side view of Figure 4, the fan surface 52 is inclined such that the front end 521 is higher and the rear end 522 is lower in the rotation direction F of the pin 11. The "high" front end 521 means that, assuming the tip end surface 5 is the lower end surface of the pin 11, the front end 521 protrudes downward more than the rear end 522. The line Ho shown in the side view is a horizontal line perpendicular to the axis of the pin 11. The fan surface 52 has an inclination relative to this line Ho determined by the step height h. The step height h is maximum at the outer periphery of the tip end surface 5. The height of the front end 521 is the same as the height of the center point CP. Meanwhile, the height of the rear end 522 is the same as the center point CP at the position of the center point CP, but is lower by the maximum step height h at the outer periphery of the tip end surface 5.
[0032] As can be seen from the above-described shape characteristics, the center point CP of the tip surface 5 does not protrude downward. In other words, even though the stepped portion 51 is machined, the flatness of the tip surface 5 is ensured from a macroscopic perspective. This is because, as described above, process P14 in FIG. 3 includes a step in which the tip surface 5 of the pin 11 is pressed against the surface of the stir welded portion 4 to perform finishing, and it is considered that the shape of the tip surface 5 is transferred to the surface of the stir welded portion 4 in this step. In other words, if there are significant protrusions on the tip surface 5, corresponding recesses will be formed on the surface of the stir welded portion 4, making it impossible to ensure the flatness of the workpieces 3. To avoid this, it is desirable that there are no significant protrusions on the tip surface 5.
[0033] The stepped portion 51 has a stepped surface based on the difference in height between the front end 521 and the rear end 522 of a pair of circumferentially adjacent fan surfaces 52. This stepped surface is a surface that extends in a direction perpendicular to the rotation direction F. The stepped surface and the right-angled edge of the front end 521 form a blade-like shape that serves to cut the materials to be joined. Such a blade not only improves the agitation properties of the materials to be joined and the ability to push the agitation material outward in the radial direction, but also contributes to cutting the continuous fibers 34 described above.
[0034] The step height h of the stepped portion 51 may be set as appropriate, but if it is too high, the press-fit resistance will increase, and if it is too low, the effect as a "blade" will be reduced. The step height h can be determined based on the diameter φ of the pin 11. For example, the step height h can be set so that the maximum height difference between the front end 521 and the rear end 522 is in the range of 1% to 10% of the diameter φ of the pin 11, and preferably in the range of 1.5% to 7%.
[0035] The step surface of the stepped portion 51 may be a vertical surface parallel to the axis Zo of the pin 11, or may be a surface having an inclination angle θ with respect to the axis Zo as shown in Figure 4. The step surface of the stepped portion 51 in the illustrated example is a surface that intersects at a right angle with a sector surface 52 that is inclined with respect to the line Ho. The inclination angle θ can be selected, for example, from the range of 2 to 7 degrees.
[0036] [Press-Fit Test Example] <Test 1> Using a tool 1 having the tip surface 5 according to the <Example> in FIG. 4 at the tip portion 11T of the pin 11 and a tool 1 having the tip surface 50 according to the <Comparative Example>, the pressure required to achieve the same pin press-fit amount on the same test piece was investigated. An overlapping portion 30 consisting of two 2.5 mm thick thermoplastic CFRP resin sheets was prepared as the test piece for the joining target 3. In both the Example and Comparative Example, the pin 11 had a diameter φ of 9 mm. The maximum height difference of the step height h of the stepped portion 51 on the tip surface 5 of the Example was 0.28 mm, and the inclination angle θ of the stepped surface was 5 degrees. The tip surface 50 of the Comparative Example was a flat horizontal surface.
[0037] The pin 11 was press-fitted into the overlapping portion 30 using the tool 1 of the example and the comparative example, with a target press-fit value of 3.87 mm. In both the example and the comparative example, the pin 11 was press-fitted to achieve the target press-fit value. However, the pressing force required to achieve the target press-fit value was 4 kN in the example and 9 kN in the comparative example, confirming that the tool 1 of the example can perform friction stir spot welding of the overlapping portion 30 with a pressing force significantly lower than that of the comparative example.
[0038] <Test 2> A test was conducted in which the pin 11 was press-fitted into the same metal sample at the same pressure using a tool 1 having the same tip surface 5 of the example as in Test 1 and a tool 1 having the tip surface 50 of the comparative example. The metal sample used was a 1 mm thick sample of A7075 aluminum alloy specified in JIS-H-4040 that had been subjected to T6 treatment. The target value for pressing the pin 11 into the sample was set to 0.5 mm, and the pressure was set to 5.5 kN, and the pin 11 of the tool 1 of the example and the comparative example was press-fitted into the metal sample.
[0039] FIG. 5 is a graph showing the relationship between the amount of press-fitting (mm) of the pin 11 into the metal sample and the welding time (seconds) for the example and the comparative example. Characteristic A1 shows the behavior of the pin 11 being pressed into the metal sample using the tool 1 of the example. It can be seen that the target press-fitting value was achieved approximately 2.5 seconds after the start of pressing the pin 11 into the metal sample. On the other hand, characteristic B1 shows the behavior of the pin 11 being pressed into the metal sample using the tool 1 of the comparative example. As a result, the pin 11 could not be pressed into the metal sample to achieve the target press-fitting value at the set pressure of 5.5 kN. Characteristic B2 shows the behavior of the pin 11 being pressed into the metal sample using the tool 1 of the comparative example, when a pressure of 8.7 kN, which can be set by the test device used in Test 2, was applied to the tool 1 of the comparative example. As shown in characteristic B2, the tool 1 of the comparative example was only able to press into the metal sample by approximately 0.2 mm, even when a pressure of approximately 60% greater than the set pressure was applied, and the target press-fitting value was not achieved.
[0040] <Test 3> The relationship between the pin press-fit amount and joining time was investigated using overlapping portion 30 formed from the thermoplastic CFRP resin sheet used in Test 1 and tool 1 having the tip surface 5 of the example. In Test 1, it was confirmed that the target press-fit value of 3.87 mm could be achieved with a pressure of 4 kN for tool 1, but an investigation was conducted to determine whether press-fitting at a lower pressure was possible.
[0041] 6 is a graph showing the relationship between the pin press-in amount (mm) and the welding time (seconds) when the pin 11 is pressed into the overlapping portion 30 while varying the pressure applied to the tool 1 of the embodiment. The characteristics A11, A12, A13, and A14 shown in the graph represent the press-in behavior when the pin 11 is pressed into the overlapping portion 30 at pressures of 4 kN, 3.5 kN, 3 kN, and 2 kN, respectively. As can be seen from this graph, it was confirmed that the target press-in value can be achieved even when the pressure is reduced to 2 kN by reducing the press-in speed of the pin 11 and thereby lengthening the welding time. Incidentally, with the tool 1 of the comparative example, the target press-in value could not be achieved with a pressure of 4 kN, no matter how much the pin 11 press-in speed was reduced.
[0042] The above tests 1 to 3 confirmed that the stepped portion 51 contributes to reducing the welding pressure when joining objects by pressing the pin 11 in the pin-first process. In the pin-first process, in which the pin 11 is pressed in while the shoulder 12 is retracted, as described in process P12 of FIG. 3 , the material directly below the pin 11 is agitated and fluidized, and then pushed out into the annular space created by the retraction of the shoulder around the outer periphery of the pin 11. The stepped portion 51 on the tip surface 5 of the pin 11 forms a step in the rotation direction F of the pin 11. Therefore, when the pin 11 is pressed into the objects 3 while rotating around its axis, the stepped portion 51 actively cuts the material directly below the pin 11. Even when the objects 3 are a sheet stack 33 as illustrated in FIG. 2 , the stepped portion 51 acts as a blade to cut the continuous fibers 34, thereby reducing the welding pressure.
[0043] Furthermore, the stepped portion 51 contributes to actively pushing the material scraped directly below the pin 11 into the shoulder retraction space. That is, the stepped portion 51 has a stepped surface extending in a direction perpendicular to the rotation direction F of the pin 11, i.e., in the radial direction. As the pin 11 rotates, the stepped surface functions to push the stirring material radially outward. This function cannot be achieved with the pin 11 of the comparative example, which has only a flat tip surface 50. When used with the pin 11 of the embodiment, which has the above-described stepped portion 51 that actively scrapes and pushes the stirring material, the stirring of the material directly below the pin 11 and the flow of the stirring material radially outward from the pin 11 are smoothed. Therefore, the pressure applied by the pin 11 to the workpiece 3 during friction stir spot welding, i.e., the welding pressure that must be applied to the tool 1, can be reduced.
[0044] Based on the above confirmation results, it is also possible to adopt a shoulder-first process instead of the pin-first process and provide a stepped portion similar to the stepped portion 51 of this embodiment on the tip surface of the shoulder 12. However, adopting the pin-first process and providing the stepped portion 51 on the tip surface 5 of the pin 11 has many advantages over the shoulder-first process. This point will be explained using FIG. 7.
[0045] Figure 7(A) shows the behavior of the stirred material in the shoulder-first process, and Figure 7(B) shows the behavior of the stirred material in the pin-first process. In the tool 100 employing the shoulder-first process, as indicated by arrow a3, it is assumed that the overflow material OF will escape into the space within the shoulder 120 created by the rise of the pin 110. However, if a stepped portion is provided on the tip surface of the shoulder 120, thereby increasing the flow of the stirred material, the overflow material OF will have no escape route, and as indicated by arrow a4, the material may flow radially outward from the shoulder 120 below the clamp 130. Such material leakage can easily cause dents in the friction stir spot weld. In contrast, in the pin-first process, as indicated by arrow a5, the overflow material OF is originally designed to escape radially outward from the pin 11. Therefore, even if the flow of the stirring material increases due to the application of the stepped portion 51, the overflowing material OF easily returns to the stirring area, and no dents are formed in the friction stir spot welded portion.
[0046] Furthermore, when the joint diameter Ws in the shoulder-first process and the joint diameter Wp in the pin-first process are the same, the volume of overflow material OF is larger in the pin-first process. For example, when the diameter φ of the pin 11 is 9 mm, the overflow material OF when the pin-first process is used is 1.8 times that of the shoulder-first process. Thus, in the pin-first process, where more material needs to be extruded during mixing, the significance of forming the stepped portion 51 on the tip surface 5 of the pin 11 to increase the extrusion force is greater than in the shoulder-first process.
[0047] 8A to 8C are perspective views showing other examples of the shape of the tip portion 11T of the pin 11 of the friction stir spot welding tool 1. In Fig. 8A to 8C, examples are shown in which the steps of the stepped portion are formed by cutting out portions of the outer circumferential edges of the pin tip surfaces 5A, 5B, and 5C. These steps are formed by groove-shaped cutouts.
[0048] The distal end surface 5A of the distal end portion 11T shown in FIG. 8A has multiple oblique grooves 53 formed therein. The oblique grooves 53 are recessed grooves formed in the distal end surface 5A, extending linearly from the outer periphery of the distal end surface 5A toward the radially inward direction of the distal end surface 5A. The oblique grooves 53 are inclined toward the outer periphery with respect to an imaginary line corresponding to the diameter of the circular distal end surface 5A. The inclination orients the oblique grooves 53 in a direction following the rotational direction F of the pin 11. The formation of such oblique grooves 53 creates a stepped shape near the outer periphery of the distal end surface 5A. FIG. 8A shows an example in which eight short oblique grooves 53 are evenly spaced along the outer periphery of the distal end surface 5A. The length, radius, depth, arrangement pitch, and inclination of the oblique grooves 53 can be changed as appropriate.
[0049] The tip portion 11T shown in Fig. 8(B) has a plurality of spiral grooves 54 formed therein, starting from the tip surface 5B and extending in the axial direction of the pin 11. The spiral grooves 54 are recessed grooves formed in the side peripheral surface of the tip portion 11T, and extend spirally from the outer circumferential edge of the tip surface 5B upstream in the rotation direction F. A stepped shape is formed near the outer circumferential edge of the tip surface 5B by cutting out the spiral grooves 54 radially inward. The spiral grooves 54 in Fig. 8(B) are just an example, and the length, radius, depth, arrangement pitch, helical angle, etc. of the spiral grooves 54 can be changed as appropriate.
[0050] The tip end portion 11T shown in FIG. 8(C) is formed with an axial groove 55 that extends linearly in the axial direction of the pin 11, starting from the tip end surface 5C. The axial groove 55 is a recessed groove formed in the circumferential side surface of the tip end portion 11T and extends a predetermined length in the axial direction of the pin 11 from the outer circumferential edge of the tip end surface 5B. In a pin 11 equipped with a tip end portion 11T having the axial groove 55, both the clockwise and counterclockwise directions can be set as the rotation direction FA. A stepped shape is formed near the outer circumferential edge of the tip end surface 5C by cutting out the axial groove 55 inward in the radial direction. The axial groove 55 shown in FIG. 8(C) is an example, and the length, radius, depth, and arrangement pitch of the axial groove 55 can be changed as appropriate.
[0051] As illustrated above, a step can be formed by cutting away part of the outer periphery of the tip end surface of the pin through the formation of the oblique groove 53, the spiral groove 54, and the axial groove 55. This step can also promote the cutting away of the material directly below the pin 11 and the extrusion of the material into the shoulder retraction space, thereby reducing the joining pressure of the tool 1.
[0052] 9A to 9F show various modified examples of forming the stepped portion 51 shown in Fig. 4 on the tip surface of the pin 11. Fig. 9A shows a tip surface 5D that includes only one stepped portion 51. Similar to the example in Fig. 4, the stepped portion 51 extends linearly from the center point C toward the outer periphery of the tip surface 5D, and has a shape in which the step height gradually increases toward the radially outer side.
[0053] FIG. 9(B) shows a distal end surface 5E having two stepped portions 51. The two stepped portions 51 are aligned linearly with a center point C in between. As a result, two semicircular surfaces exist on the distal end surface 5E. These semicircular surfaces are inclined according to the steps of the stepped portions 51. FIG. 9(C) shows a distal end surface 5F having four stepped portions 51. The four stepped portions 51 are arranged at equal intervals of 90 degrees in the circumferential direction. Four fan-shaped surfaces of the same size are arranged circumferentially on the distal end surface 5F. FIG. 9(D) shows a distal end surface 5G in which the four stepped portions 51 are arranged at random intervals in the circumferential direction. As in the example of FIG. 9(D), the stepped portions 51 do not have to be arranged at equal intervals in the circumferential direction.
[0054] FIG. 9(E) shows a tip end surface 5H having four stepped portions 51 each having a curved portion 51A. In the above example, the stepped portions 51 extend linearly in the radial direction. However, the tip end surface 5H may have the curved portion 51A as shown in FIG. 9(E). The curved portion 51A is a portion of the stepped portion 51 near the outer periphery of the tip end surface 5H that is curved to follow the rotation direction F. FIG. 9(F) also shows a tip end surface 5I having four stepped portions 51 each having a curved portion 51B. The curved portion 51B here is a portion of the stepped portion 51 near the outer periphery of the tip end surface 5H that is curved in the direction opposite to the rotation direction F. Providing the tip end surfaces 5D to 5I shown above on the pin 11 also reduces the welding pressure of the tool 1.
[0055] [Summary of the Disclosure] The specific embodiments described above include disclosures having the following configurations.
[0056] A friction stir spot welding tool according to a first aspect of the present disclosure comprises a cylindrical pin that rotates around an axis, a shoulder having a hollow portion through which the pin is inserted, and a drive unit that drives the pin to rotate while pressing it into objects to be joined and drives the shoulder to retract from the objects to be joined, and at least a portion of the circular tip surface of the pin is provided with a step-shaped portion that forms a step in the rotational direction of the pin.
[0057] According to the first aspect, the stepped portion contributes to reducing the welding pressure when joining workpieces by press-fitting a pin. That is, in a pin-first process in which the pin is pressed in while the shoulder is retracted, the material directly below the pin is pushed into the shoulder retraction space located on the outer periphery of the pin. The stepped portion forms a step in the direction of rotation of the pin. Therefore, when the pin is pressed into the workpieces while rotating around its axis, the stepped portion actively scrapes and pushes the material directly below the pin into the shoulder retraction space. This facilitates the stirring of the material directly below the pin and the smooth flow of the stirred material radially outward from the pin. Therefore, the pin pressure applied to the workpieces during friction stir spot welding, i.e., the welding pressure that must be applied to the tool, can be reduced. Reducing the welding pressure also suppresses the reaction force, making it possible to install a friction stir spot welding tool on a small robot or a small dedicated device. This makes it possible to avoid the need for larger equipment including friction stir spot welding tools and increased costs.
[0058] A friction stir spot welding tool according to a second aspect is the tool of the first aspect, wherein the step of the stepped portion is a radial step extending radially from the center point of the tip surface to the outer circumferential edge.
[0059] According to the second aspect, the step is a radial step, so that the material can be efficiently pushed out in the direction of the outer periphery of the pin when stirring by press-fitting the pin.
[0060] A friction stir spot welding tool according to a third aspect is the tool of the second aspect, wherein a plurality of the radial steps are arranged in the circumferential direction of the tip end surface of the pin.
[0061] According to the third aspect, since multiple radial steps are arranged in the circumferential direction, the force of pushing the material outward from the pin can be increased, and the pressure applied by the pin can be reduced.
[0062] A friction stir spot welding tool according to a fourth aspect is the tool of the third aspect, wherein the plurality of radial steps are arranged at equal intervals in the circumferential direction of the tip end surface.
[0063] According to the fourth aspect, since a plurality of radial steps are arranged at equal intervals, it is possible to perform the cutting of material directly below the pin and the pushing of that material toward the outer periphery of the pin in a well-balanced manner.
[0064] The friction stir spot welding tool of the fifth aspect is the tool of the first to fourth aspects, wherein the maximum height difference of the step of the stepped portion is set in the range of 1% to 10% of the diameter of the pin.
[0065] According to the fifth aspect, the step height of the stepped portion can be optimized.
[0066] A friction stir spot welding tool according to a sixth aspect is the tool of the first aspect, wherein the step of the stepped portion is a step formed by cutting away a part of the outer circumferential edge of the tip surface.
[0067] According to the sixth aspect, even if there is a step due to a cutout in part of the outer peripheral edge, it is possible to promote the cutting of material directly below the pin and the extrusion of said material into the shoulder retreat space, thereby reducing the joining pressure of the tool.
[0068] DESCRIPTION OF SYMBOLS 1 Tool (friction stir spot welding tool) 11 Pin 12 Shoulder 13 Clamp 2 Tool drive unit (drive unit) 3 Joint 3 4 Stir welded portion 5, 5A to 5I Tip surface 51 Step-shaped portion 53 Oblique groove (step-shaped portion) 54 Spiral groove (step-shaped portion) 55 Axial groove (step-shaped portion) F Rotation direction M Friction stir spot welding device R Rotation axis (axis)
Claims
1. A friction stir spot welding tool comprising: a cylindrical pin that rotates about an axis; a shoulder having a hollow portion through which the pin is inserted; and a drive unit that drives the pin to rotate while pressing it into objects to be joined, and drives the shoulder to retract from the objects to be joined, wherein at least a portion of the tip surface of the pin is provided with a step-shaped portion that forms a step in the rotational direction of the pin.
2. A friction stir spot welding tool as claimed in claim 1, wherein the step of the stepped portion is a radial step extending radially from the centre point of the tip surface to the outer periphery.
3. A friction stir spot welding tool as claimed in claim 2, wherein the radial steps are arranged in a plurality in the circumferential direction on the tip surface of the pin.
4. A friction stir spot welding tool as claimed in claim 3, wherein the plurality of radial steps are arranged at equal intervals in the circumferential direction of the tip surface.
5. A friction stir spot welding tool according to any one of claims 1 to 4, wherein the maximum height difference of the step of the step-shaped portion is set in the range of 1% to 10% of the diameter of the pin.
6. A friction stir spot welding tool as claimed in claim 1, wherein the step of the stepped portion is a step formed by cutting out a part of the outer circumferential edge of the tip surface.
Citation Information
Patent Citations
Bonding method
JP2015186869A
Lap spot welding method for metallic foil
JP2015123488A
Friction stirring joining tool and friction stirring joining method
JP2017200702A
Friction stir joining method for aluminum alloy plate and steel plate
JP2021164943A
Friction stir spot welding device and method for operating same
WO2020138326A1