3D NAND flash memory device and manufacturing method therefor

By positioning the electron capture layer structure close to the channel structure in 3D NAND flash memory devices, the problem of charge diffusion after programming is solved, and data retention capability and storage life are improved.

WO2024244378A1PCT designated stage expired Publication Date: 2024-12-05UNITED MEMORY TECHNOLOGY (JIANGSU) LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/137799
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-01
Filing Date
2023-12-11
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

In NAND flash memory devices, charge diffusion of the electron capture layer after programming causes the threshold voltage of the memory cell to decrease, the data retention capability becomes poor, and the data retention life is short.

Method used

In the production method of a 3D NAND flash memory device, the electron capture layer structure is positioned close to the channel structure, thereby avoiding charge diffusion after a period of programming operation and maintaining the threshold voltage of the memory cell stable.

Benefits of technology

It effectively improves data retention capabilities, extends the storage life of data, and prevents the threshold voltage of the memory cell from falling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023137799_05122024_PF_FP_ABST
    Figure CN2023137799_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of semiconductor storage devices, and specifically relates to a 3D NAND flash memory device and a manufacturing method therefor. The manufacturing method comprises: first, providing a semiconductor substrate layer, and forming unit isolation structures, channel structures and source electrode lead-out spaces on the semiconductor substrate layer, wherein the unit isolation structures are stacked structures which comprise unit isolation layers and storage unit occupation spaces; then sequentially depositing first dielectric layers and second dielectric layers, wherein the first dielectric layers at least cover exposed surfaces of the unit isolation structures; then etching the second dielectric layers, removing all second dielectric layers located on lateral faces, removing at least some second dielectric layers located on second surfaces, retaining all the second dielectric layers located on first surfaces, and forming electron capturing layers of storage unit structures by using the remaining second dielectric layers; and finally, manufacturing the storage unit structures and electrode structures of a flash memory device. The portions of electron capturing layer structures of the flash memory device that extend to the positions of source electrodes are eliminated, such that the data retention capability can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

3D NAND flash memory device and manufacturing method thereof Technical Field

[0001] The present application relates to the technical field of semiconductor memory devices, and in particular to a 3D NAND flash memory device and a manufacturing method thereof. Background Art

[0002] Data in NAND flash memory devices is stored in the form of electric charge. The amount of stored charge represents the data in the device. Typically, when the charge level in a NAND flash memory cell is in the majority state, it indicates the data stored in the cell is "1," while when it is in the minority state, it indicates the data stored in the cell is "0." The amount of stored charge depends on the voltage applied to the gate.

[0003] During programming of a memory cell, charge flows from the substrate into the electron-trapping layer of the memory cell through the tunneling effect, causing the charge in the electron-trapping layer to be in a majority state. However, over time, due to external influences such as temperature changes, the charge moves a certain distance in the electron-trapping layer.

[0004] Figure 1 shows a schematic diagram of the charge state in the electron capture layer of a memory cell in the related art immediately after a programming operation is completed. As can be seen from Figure 1, the charge distribution in the electron capture layer 1 is relatively concentrated immediately after the programming operation is completed. Figure 2 shows a schematic diagram of the charge state in the electron capture layer of a memory cell in the related art some time after the programming operation is completed. As can be seen from Figure 2, the charge in the electron capture layer 1 diffuses some time after the programming operation is completed.

[0005] Since the distribution of charge in the electron capture layer affects the threshold voltage of the memory cell, when the charge concentration state in FIG1 changes to the charge diffusion state shown in FIG2 , the threshold voltage of the memory cell becomes lower after programming, resulting in a deterioration in the data retention capability of the memory cell, that is, a shortened data retention life. Summary of the Invention

[0006] The present application provides a 3D NAND flash memory device and a method for manufacturing the same, which can solve the problem in related technologies that charge diffuses in the electron capture layer some time after the programming operation is completed, resulting in a decrease in the threshold voltage of the storage cell and a deterioration in data retention capability.

[0007] In order to solve the technical problem described in the background technology, the first aspect of the present application provides a method for manufacturing a 3D NAND flash memory device, wherein the method for manufacturing a 3D NAND flash memory device comprises the following steps performed in sequence:

[0008] A semiconductor substrate layer is provided, on which a plurality of cell isolation structures spaced apart in the horizontal direction and a channel structure penetrating the cell isolation structures in the vertical direction are formed, wherein the spacing between the cell isolation structures serves as a source lead-out space; each cell isolation structure comprises a plurality of cell isolation layers spaced apart in the vertical direction, the spacing within the cell isolation structure serves as a memory cell occupied space, and the sidewalls of the channel structure are exposed at the location of the memory cell occupied space;

[0009] Depositing a first dielectric layer and a second dielectric layer in sequence, wherein the second dielectric layer covers the first dielectric layer, and the first dielectric layer covers at least the surface exposed by the cell isolation structure; the exposed surface of the cell isolation structure includes: the surface of each memory cell occupied space and the side surface of each cell isolation layer close to the source lead space; the surface of the memory cell occupied space includes: the first surface of the channel structure exposed from the memory cell occupied space, and the second surface of the cell isolation layer located in the memory cell occupied space;

[0010] Etching the second dielectric layer to remove all of the second dielectric layer on the side surface, remove at least a portion of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface, with the remaining second dielectric layer forming an electron capture layer of the memory cell structure;

[0011] The memory cell structure and electrode structure of the flash memory device are manufactured.

[0012] Optionally, the step of etching the second dielectric layer to remove all of the second dielectric layer on the side surface, remove at least a portion of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface includes:

[0013] Coating a photosensitive layer, wherein the photosensitive layer fills the space occupied by the storage unit and the source electrode lead-out space;

[0014] removing the photosensitive layer located in the source lead-out space and retaining the photosensitive layer located in the space occupied by the storage unit;

[0015] Using the remaining photosensitive layer as an etching stop, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove at least a portion of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface;

[0016] Remove the remaining photosensitive layer.

[0017] Optionally, the step of etching the second dielectric layer using an etching solution using the remaining photosensitive layer as a barrier to retain the second dielectric layer on the surface of the channel structure exposed from the space occupied by the storage unit to form the electron capture layer structure includes:

[0018] Using the remaining photosensitive layer as an etching stop, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove all of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface;

[0019] The remaining second dielectric layer forms an electron capture layer of the memory cell structure.

[0020] Optionally, the step of etching the second dielectric layer using an etching solution using the remaining photosensitive layer as a barrier to retain the second dielectric layer on the surface of the channel structure exposed from the space occupied by the storage unit to form the electron capture layer structure includes:

[0021] Using the remaining photosensitive layer as an etching stop, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove a portion of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface;

[0022] The remaining second dielectric layer forms the electron capture layer of the memory cell structure. The remaining second dielectric layer on the second surface forms an extension of the electron capture layer. The remaining second dielectric layer on the first surface forms a main body of the electron capture layer.

[0023] Optionally, the channel structure includes a channel hole, and a channel polysilicon layer and a channel dielectric layer that fill the channel hole;

[0024] The channel hole extends into the semiconductor substrate layer, the channel polysilicon layer covers the inner wall of the channel hole, and the channel polysilicon layer surrounds the outer periphery of the channel dielectric layer;

[0025] The extension portion extends from both ends of the main portion along the second surface to a first length.

[0026] Optionally, the step of removing the photosensitive layer located in the source lead-out space and retaining the photosensitive layer located in the space occupied by the storage unit includes:

[0027] Using ultraviolet rays to irradiate the photosensitive layer filled in the source lead-out space through a mask;

[0028] The photosensitive layer filled in the source lead-out space is removed using a developing solution, and the photosensitive layer located in the space occupied by the storage unit is retained.

[0029] Optionally, in the step of manufacturing the memory cell structure and the electrode structure of the flash memory device, the step of manufacturing the memory cell structure of the flash memory device includes:

[0030] Etching the first dielectric layer to remove the first dielectric layer covering the side surface and retaining the first dielectric layer covering the surface of the space occupied by the memory unit, with the remaining first dielectric layer forming an electron tunneling layer of the memory unit structure;

[0031] Manufacturing an oxide isolation layer and a high dielectric thin film layer of the memory cell structure;

[0032] The oxidized isolation layer is located in the space occupied by the memory cell and covers the exposed surface of the electron tunneling layer and the exposed surface of the electron capture layer;

[0033] The high dielectric film layer is located in the space occupied by the memory cell and covers the exposed surface of the oxide isolation layer;

[0034] The high dielectric thin film layer surrounds and forms a gate-occupied space, and the gate-occupied space is used to form a gate electrode.

[0035] Optionally, in the step of providing a semiconductor substrate layer, forming a plurality of unit isolation structures spaced apart in the horizontal direction and a channel structure penetrating the unit isolation structure in the vertical direction on the semiconductor substrate layer, and the spacing space on both sides of the unit isolation structure being the source lead-out space, the bottom layer of each of the unit isolation structures is the space occupied by the storage unit, and the top layer of each of the unit isolation structures is the unit isolation structure.

[0036] Optionally, the step of providing a semiconductor substrate layer, forming a plurality of cell isolation structures spaced apart in a horizontal direction and a channel structure vertically penetrating the cell isolation structures on the semiconductor substrate layer, wherein the spacing between the cell isolation structures is a source lead-out space, includes:

[0037] Providing a semiconductor substrate layer, and forming a composite layer structure on the semiconductor substrate layer, wherein the composite layer structure includes multiple sacrificial dielectric layers and multiple cell isolation dielectric layers alternately stacked in sequence;

[0038] forming a channel structure in the composite layer structure, wherein the channel structure vertically penetrates the composite layer structure and extends into the semiconductor substrate layer;

[0039] forming a source lead-out space in the composite layer structure, wherein the end of the sacrificial dielectric layer and the upper surface of the semiconductor substrate layer are exposed in the source lead-out space;

[0040] The sacrificial dielectric layer is removed by etching to form the memory cell occupied space, and the remaining cell isolation dielectric layer forms a cell isolation layer.

[0041] In order to solve the technical problem described in the background technology, the second aspect of the present application provides a 3D NAND flash memory device, and the 3D NAND flash memory device is manufactured by the 3D NAND flash memory device described in the first aspect of the present application.

[0042] The technical solution of the present application includes at least the following advantages: the present application locates the electron capture layer structure for storing electrons in each memory cell structure close to the channel structure, thereby avoiding the problem of charge diffusion in the electron capture layer after a period of programming operation, thereby avoiding the reduction of the memory cell threshold voltage and improving the data retention capability. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the following is a brief introduction to the drawings required for use in the specific implementation methods or the description of the prior art. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.

[0044] FIG1 is a schematic diagram showing the charge state in the electron capture layer of a memory cell in the related art when the programming operation has just been completed;

[0045] FIG2 is a schematic diagram showing the charge state in the electron capture layer of a memory cell after a period of time after the memory cell completes a programming operation in the related art;

[0046] FIG3 shows a schematic diagram of a partial cross-sectional structure of a device after step S1 of a method for manufacturing a 3D NAND flash memory device according to an embodiment of the present application is completed;

[0047] FIG4 shows a schematic cross-sectional structure diagram of the semiconductor substrate layer provided in step S1;

[0048] FIG5 is a schematic cross-sectional view of the device after the semiconductor substrate layer shown in FIG4 forms a composite layer structure and a channel structure;

[0049] FIG6 is a schematic diagram of a cross-sectional structure of a device after a source lead-out space is formed in the composite layer structure shown in FIG5 ;

[0050] FIG7 shows a schematic diagram of a partial cross-sectional structure of a device after step S2 of a method for manufacturing a 3D NAND flash memory device according to an embodiment of the present application is completed;

[0051] FIG8 is a schematic diagram of a cross-sectional structure of the device after the photosensitive layer has completely filled the space occupied by the storage unit and the source lead-out space in the structure shown in FIG7 ;

[0052] FIG9 is a schematic cross-sectional view of the device structure in which the photosensitive layer located in the source lead-out space is removed based on FIG8 , and the remaining photosensitive layer is filled in the space occupied by the storage unit;

[0053] FIG10 shows a schematic cross-sectional structure diagram of the device after the second dielectric layer is partially etched away based on the remaining photosensitive layer in FIG9 ;

[0054] FIG11 shows a structure formed after the step of etching the second dielectric layer using an etching solution with the remaining photosensitive layer as an etching stop is completed;

[0055] FIG12 shows another structure formed after the step of etching the second dielectric layer using the remaining photosensitive layer as an etching stop is completed;

[0056] FIG13 shows a schematic cross-sectional structural diagram of a 3D NAND flash memory device provided in an embodiment of the present application;

[0057] FIG14 shows an enlarged structural schematic diagram of part A in FIG13 ;

[0058] FIG15 shows a flowchart of a method for manufacturing a 3D NAND flash memory device according to an embodiment of the present application. DETAILED DESCRIPTION

[0059] The following is a clear and complete description of the technical solutions in this application in conjunction with the accompanying drawings. Obviously, the embodiments described are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making any creative efforts are within the scope of protection of this application.

[0060] In the description of this application, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings and are intended solely to facilitate the description of this application and simplify the description. They do not indicate or imply that the devices or components referred to must have a specific orientation, be constructed, or operate in a specific orientation. Therefore, they should not be construed as limitations on this application. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0061] In the description of this application, it should be noted that, unless otherwise expressly specified or limited, the terms "installed," "connected," and "connected" should be understood in a broad sense. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to mechanical connections or electrical connections; they can refer to direct connections or indirect connections through an intermediate medium; they can refer to internal connections between two components; they can refer to wireless connections or wired connections. Those skilled in the art will understand the specific meanings of the above terms in this application based on the specific circumstances.

[0062] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0063] FIG15 shows a flow chart of a method for manufacturing a 3D NAND flash memory device according to an embodiment of the present application. As can be seen from FIG15 , the method for manufacturing a 3D NAND flash memory device includes the following steps S1 to S4 which are performed in sequence.

[0064] Step S1: Providing a semiconductor substrate layer. A plurality of horizontally spaced cell isolation structures and a channel structure vertically extending through the cell isolation structures are formed on the semiconductor substrate layer. The spacing between the cell isolation structures serves as source lead-out space for forming a source lead-out structure. Each cell isolation structure includes multiple vertically spaced cell isolation layers. The spacing within each cell isolation structure serves as a memory cell occupying space for forming a memory cell. The sidewalls of the channel structure are exposed at the locations of the memory cell occupying spaces.

[0065] Referring to Figure 3, it shows a schematic diagram of a partial cross-sectional structure of the device after step S1 of the present application is completed. As can be seen from Figure 3, step S1 forms a plurality of unit isolation structures 210 on the semiconductor substrate layer 100, and a channel structure 220 is formed in each unit isolation structure 210. The channel structure 220 penetrates the corresponding unit isolation structure 210 in the vertical direction, and the bottom ends of all the channel structures 220 extend into the semiconductor substrate layer 100.

[0066] In addition, two adjacent cell isolation structures 210 are spaced apart in the horizontal direction to form a spacing space. The spacing spaces on both sides of each cell isolation structure 210 are source extraction spaces 230 for forming source extraction structures in subsequent steps.

[0067] Each cell isolation structure 210 includes multiple vertically spaced cell isolation layers 211. The space within each cell isolation structure 210 serves as a memory cell occupying space 212, which will be used to form memory cells in subsequent steps. The sidewalls of the channel structure 220 are exposed at the location of the memory cell occupying space 212.

[0068] Illustratively, the bottom layer of each cell isolation structure 210 is the memory cell occupied space 212 , that is, the space between the semiconductor substrate layer 100 and the adjacent cell isolation layer 211 is the memory cell occupied space 212 . In addition, the top layer of each cell isolation structure 210 is the cell isolation structure 211 .

[0069] The cell isolation layer 211 may be made of silicon dioxide. The channel structure 220 includes a channel hole, a channel polysilicon layer 221 filling the channel hole, and a channel dielectric layer 222. The channel hole extends into the semiconductor substrate layer 100, and the channel polysilicon layer 221 covers the inner wall of the channel hole and surrounds the outer periphery of the channel dielectric layer 222.

[0070] FIG4 to FIG6 show a schematic diagram of a cross-sectional structure of a device formed after each step of an embodiment of step S1 is completed. An achievable embodiment of step S1 is described below in conjunction with FIG4 to FIG6 :

[0071] 4 , a semiconductor substrate layer 100 as shown in FIG. 4 is provided, and a composite layer structure 200 is formed on the semiconductor substrate layer 100 . The composite layer structure 200 includes multiple sacrificial dielectric layers 110 and multiple cell isolation dielectric layers 120 that are alternately stacked in sequence.

[0072] 5 , a channel structure 220 is formed in the composite layer structure 200 . The channel structure 220 passes through the composite layer structure 200 in a vertical direction and extends into the semiconductor substrate layer 100 .

[0073] The steps of making the channel structure 220 include: first etching to form a channel hole, wherein the channel hole extends into the semiconductor substrate layer 100; then forming a channel polysilicon layer 221 and a channel dielectric layer 222 in the channel hole, wherein the channel polysilicon layer 221 covers the inner wall of the channel hole, and the channel polysilicon layer 221 surrounds the outer periphery of the channel dielectric layer 222.

[0074] 6 , a source lead-out space 230 is formed in the composite layer structure 200 , and the end of the sacrificial dielectric layer 110 and the upper surface of the semiconductor substrate layer 100 are exposed in the source lead-out space 230 .

[0075] Then, based on the structure shown in FIG. 6 , the sacrificial dielectric layer 110 is etched away to form the memory cell occupying space 212 shown in FIG. 3 , and the remaining cell isolation dielectric layer 120 forms the cell isolation layer 211 shown in FIG. 3 .

[0076] Step S2: depositing a first dielectric layer and a second dielectric layer in sequence, wherein the second dielectric layer covers the first dielectric layer, and the first dielectric layer at least covers the exposed surface of the cell isolation structure.

[0077] Referring to Figure 7 , which shows a schematic diagram of a partial cross-sectional structure of the device after step S2 is completed, it can be seen from Figure 7 that the deposited second dielectric layer 320 covers the first dielectric layer 310, and the first dielectric layer 310 covers the exposed surface of the cell isolation structure 210. The exposed surface of the cell isolation structure 210 includes: the surface of each memory cell occupied space 212 and the side surface 30c of each layer of cell isolation layer 211 near the source lead-out space 230, as shown in Figure 3 ; the surface of the memory cell occupied space 212 includes: the first surface 30a of the channel structure 220 exposed from the memory cell occupied space 212, and the second surface 30b of the cell isolation layer 211 located in the memory cell occupied space 212, as shown in Figure 3 . In this embodiment, the first dielectric layer 310 and the second dielectric layer 320 also cover the upper surface of the semiconductor substrate layer 100.

[0078] The first dielectric layer 310 is used to form an electron tunneling layer in a subsequent step, and its material may be silicon dioxide. The second dielectric layer 320 is used to form an electron capture layer in a subsequent step, and its material may be silicon nitride.

[0079] Step S3: etching the second dielectric layer to remove all of the second dielectric layer on the side surface and at least a portion of the second dielectric layer on the second surface, while retaining all of the second dielectric layer on the first surface. The remaining second dielectric layer forms an electron capture layer of the memory cell structure.

[0080] FIG8 to FIG10 show a schematic diagram of a cross-sectional structure of a device formed after each step of an embodiment of step S3 is completed. The following describes an achievable embodiment of step S3 in conjunction with FIG7 to FIG10 :

[0081] A photosensitive layer is first coated, and the photosensitive layer fills the storage unit occupied space and the source lead space.

[0082] 8 , the coated photosensitive layer 400 completely fills the memory cell occupying space 212 and the source lead-out space 230 in the structure shown in FIG. 7 .

[0083] Then, the photosensitive layer located in the source lead-out space is removed, and the photosensitive layer located in the space occupied by the storage unit is retained.

[0084] 9 , the photosensitive layer 400 located in the source lead-out space 230 is removed, and the remaining photosensitive layer 400 is filled in the memory cell occupying space 212 .

[0085] For example, the photosensitive layer can be an organic polymer that undergoes a chemical reaction under ultraviolet light. Ultraviolet light can be irradiated through a mask onto the photosensitive layer 400 filling the source lead-out space 230. A developer can then be used to remove the photosensitive layer 400 filling the source lead-out space 230. The photosensitive layer 400 filling the memory cell occupied space 212 is not exposed to ultraviolet light and, therefore, remains insoluble in the developer.

[0086] 9 , after the photosensitive layer 400 in the source lead-out space 230 is removed, the second dielectric layer 320 on the side surface 30 c (as shown in FIG. 3 ) is exposed, and the second dielectric layer 320 at the connection position between the second surface 30 b (as shown in FIG. 3 ) and the side surface 30 c is exposed.

[0087] Then, the remaining photosensitive layer is used as an etching stop, and the second dielectric layer is etched with an etching solution to remove the entire second dielectric layer on the side surface, remove at least a portion of the second dielectric layer on the second surface, and retain the entire second dielectric layer on the first surface.

[0088] Referring to Figure 10 , the remaining photosensitive layer 400 fills the memory cell occupied space 212. Due to the etch-stop effect of the photosensitive layer 400, the second dielectric layer 320 located on the first surface 30a shown in Figure 3 is not etched and remains during step S5. That is, the second dielectric layer 320 on the first surface 30a where the channel structure 220 is exposed from the memory cell occupied space 212 is not etched and remains. The remaining second dielectric layer 320 serves as the electron capture layer structure 600 in the memory cell. The second dielectric layer 320 located on the side surface 30c is completely etched away due to its exposure. Since the second dielectric layer 320 at the junction of the second surface 30b and the side surface 30c is also exposed, the etching solution can gradually etch away all or part of the second dielectric layer 320 located on the second surface 30b starting from this junction.

[0089] Finally, remove the remaining photosensitive layer.

[0090] Figure 11 shows a structure formed after the step of etching the second dielectric layer using the remaining photosensitive layer as an etch stop using an etchant is completed. Figure 12 shows another structure formed after the step of etching the second dielectric layer using the remaining photosensitive layer as an etch stop using an etchant is completed. The following describes the step of etching the second dielectric layer using the remaining photosensitive layer as an etch stop using an etchant, in conjunction with Figures 11 and 12.

[0091] Referring to FIG. 11 , the remaining photosensitive layer 400 can be used as an etching stopper to etch the second dielectric layer 320 using an etching solution. The entire second dielectric layer 320 on the side surface 30 c is removed, and the entire second dielectric layer 320 on the second surface 30 b is removed. The entire second dielectric layer 320 on the first surface 30 a is retained. The remaining second dielectric layer 320 forms the electron capture layer 600 of the memory cell structure.

[0092] 12 , the remaining photosensitive layer 400 can be used as a barrier to etch the second dielectric layer 320 using an etching solution to remove the entire second dielectric layer 320 on the side surface 30 c and the portion of the second dielectric layer 320 on the second surface 30 b , while retaining the entire second dielectric layer 320 on the first surface 30 a .

[0093] The remaining second dielectric layer 320 forms the electron capture layer 600 of the storage unit structure. The remaining second dielectric layer 320 located on the second surface 30b forms an extension portion 620 of the electron capture layer 600. The remaining second dielectric layer 320 located on the first surface 30a forms a main body portion 610 of the electron capture layer 600. The extension portion 620 extends from both ends of the main body portion 610 along the second surface 30b by a first length L, and the first length L is less than or equal to half the length of the space occupied by the storage unit.

[0094] Exemplarily, the material of the second dielectric layer 320 may be silicon nitride, and the etching solution includes phosphoric acid.

[0095] Step S4: manufacturing the memory cell structure and electrode structure of the flash memory device.

[0096] Among the steps of manufacturing the memory cell structure and the electrode structure of the flash memory device, the step of manufacturing the memory cell structure of the flash memory device includes:

[0097] The first dielectric layer is first etched to remove the first dielectric layer covering the side surface, and the first dielectric layer covering the surface of the space occupied by the storage unit is retained. The remaining first dielectric layer forms the electron tunneling layer of the storage unit structure.

[0098] Then, an oxidation isolation layer and a high dielectric film layer of the memory cell structure are manufactured.

[0099] The oxide isolation layer is located in the memory cell occupied space and covers the exposed surface of the electron tunneling layer and the exposed surface of the electron capture layer. The high dielectric thin film layer is located in the memory cell occupied space and covers the exposed surface of the oxide isolation layer. The high dielectric thin film layer surrounds a gate occupied space, and the gate occupied space is used to form a gate electrode.

[0100] The present application also provides a 3D NAND flash memory device, which is manufactured based on the 3D NAND flash memory device manufacturing method shown in Figure 15. Figure 13 is a schematic cross-sectional view of the 3D NAND flash memory device formed after the 3D NAND flash memory device manufacturing method shown in Figure 15 is completed. The structure of the 3D NAND flash memory device in this embodiment is described below in conjunction with Figure 13.

[0101] 13 , the 3D NAND flash memory device includes a semiconductor substrate layer 100 forming a plurality of stacked structures 700 . The stacked structure 700 is a structure formed after the cell isolation structure 210 shown in FIG. 3 undergoes steps S2 to S4 shown in FIG. 15 .

[0102] Each stacked structure 700 includes at least one channel structure 220. The channel structure 220 vertically penetrates the stacked structure 700, and the bottom of the channel structure 220 extends into the semiconductor substrate layer 100. Exemplarily, the channel structure 220 includes a channel hole, a channel polysilicon layer 221 that fills the channel hole, and a channel dielectric layer 222. The channel hole extends into the semiconductor substrate layer 100, and the channel polysilicon layer 221 covers the inner wall of the channel hole. The channel polysilicon layer 221 surrounds the outer periphery of the channel dielectric layer 222.

[0103] A source lead-out structure 710 is formed between two adjacent stacked structures 700. A source doped region 720 is formed in the semiconductor substrate layer 100 at the bottom of the source lead-out structure 710. The source lead-out structure 710 is connected to the source doped region 720 and is used to lead the source doped region 720 out. The source lead-out structure 710 includes a source electrode 711 and a source insulating layer 712 located on both sides of the source electrode 711. The source insulating layer 712 isolates the source electrode 711 from the adjacent stacked structures 700. The top of the source electrode 711 is connected to the bit line of the flash memory device.

[0104] Each stacked structure 700 includes a memory cell structure 730 and a cell isolation layer 211 alternately stacked in a vertical direction. For example, the bottom layer of the stacked structure 700 is the memory cell structure 730, and the top layer of the stacked structure 700 is the cell isolation layer 211. The memory cell structure 730 is formed after the memory cell occupied space 212 shown in FIG. 3 undergoes steps S2 to S4 shown in FIG. 15 .

[0105] FIG14 is an enlarged schematic diagram of the structure of section A in FIG13 . Combining FIG13 and FIG14 , it can be seen that the memory cell structure 730 includes an electron tunneling layer 731, an electron capture layer 600, an oxide isolation layer 732, a high dielectric thin film layer 733, and a gate electrode 734, stacked sequentially from the outside to the inside. The electron tunneling layer 731 is a structure formed after the first dielectric layer 310 shown in FIG7 undergoes steps S3 and S4, and the electron capture layer 600 is a structure formed after the second dielectric layer 320 shown in FIG7 undergoes steps S3 and S4.

[0106] The electron tunneling layer 731 covers a portion of the surface of the adjacent channel structure 220, ie, the first surface 30a shown in Figure 3. The electron tunneling layer 731 also covers the surface of the adjacent cell isolation layer 211, ie, the second surface 30b shown in Figure 3.

[0107] The electron capture layer 600 covers the electron tunneling layer 731 at the first surface 30a. Optionally, the electron capture layer 600 includes a main portion 610 and an extension portion 620, wherein the main portion 610 covers the electron tunneling layer 731 at the first surface 30a, and the extension portion 620 extends from both ends of the main portion 610 along the second surface 30b by a first length L that is less than or equal to half the length of the space occupied by the memory cell.

[0108] The flash memory device formed by the above steps in this embodiment includes a memory cell structure stacked in a vertical direction. The electron capture layer structure for storing electrons in each memory cell structure is located near the channel structure, so that after a period of programming operation, the problem of charge diffusion in the electron capture layer is avoided, thereby avoiding the reduction of the memory cell threshold voltage and improving data retention capability.

[0109] Obviously, the above embodiments are merely examples for clarity of explanation and are not intended to limit the implementation methods. Those skilled in the art will appreciate that other variations or modifications can be made based on the above description. It is not necessary and impossible to enumerate all implementation methods here. Obvious variations or modifications arising therefrom remain within the scope of protection of this application.

Claims

1. A method for manufacturing a 3D NAND flash memory device, characterized in that: The method for manufacturing the 3D NAND flash memory device comprises the following steps performed in sequence: A semiconductor substrate layer is provided, on which a plurality of cell isolation structures spaced apart in the horizontal direction and a channel structure penetrating the cell isolation structure in the vertical direction are formed, wherein the spacing spaces on both sides of the cell isolation structure are source lead-out spaces; each of the cell isolation structures comprises a plurality of cell isolation layers spaced apart in the vertical direction, the spacing spaces inside the cell isolation structures are memory cell occupied spaces, and the sidewalls of the channel structures are exposed at the locations of the memory cell occupied spaces; Depositing a first dielectric layer and a second dielectric layer in sequence, wherein the second dielectric layer covers the first dielectric layer, and the first dielectric layer at least covers the exposed surface of the cell isolation structure; The exposed surface of the cell isolation structure includes: the surface of each of the memory cell occupied spaces and the side of each layer of the cell isolation layer close to the source lead-out space; the surface of the memory cell occupied space includes: the first surface of the channel structure exposed from the memory cell occupied space, and the second surface of the cell isolation layer located in the memory cell occupied space; Etching the second dielectric layer to remove all of the second dielectric layer on the side surface, remove at least part of the second dielectric layer on the second surface, retain all of the second dielectric layer on the first surface, and the remaining second dielectric layer forms an electron capture layer of the storage unit structure; The memory cell structure and the electrode structure of the flash memory device are manufactured.

2. The method for manufacturing a 3D NAND flash memory device according to claim 1, wherein: The step of etching the second dielectric layer, removing all of the second dielectric layer on the side, removing at least part of the second dielectric layer on the second surface, and retaining all of the second dielectric layer on the first surface comprises: Coating a photosensitive layer, wherein the photosensitive layer fills the space occupied by the storage unit and the source electrode lead-out space; Removing the photosensitive layer located in the source lead-out space, and retaining the photosensitive layer located in the space occupied by the storage unit; Using the remaining photosensitive layer as an etching stop, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove at least a portion of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface; Remove the remaining photosensitive layer.

3. The method for manufacturing a 3D NAND flash memory device according to claim 2, wherein: The step of using the remaining photosensitive layer as a barrier, etching the second dielectric layer with an etching solution, and retaining the second dielectric layer on the surface of the channel structure exposed from the space occupied by the storage unit to form an electron capture layer structure comprises: Using the remaining photosensitive layer as an etching barrier, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove all of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface; The remaining second dielectric layer forms an electron capture layer of the memory cell structure.

4. The method for manufacturing a 3D NAND flash memory device according to claim 2, wherein: The step of using the remaining photosensitive layer as a barrier, etching the second dielectric layer with an etching solution, and retaining the second dielectric layer on the surface of the channel structure exposed from the space occupied by the storage unit to form an electron capture layer structure comprises: Using the remaining photosensitive layer as an etching stop, etching the second dielectric layer with an etching solution to remove all of the second dielectric layer on the side surface, remove part of the second dielectric layer on the second surface, and retain all of the second dielectric layer on the first surface; The remaining second dielectric layer forms the electron capture layer of the memory cell structure, the remaining second dielectric layer on the second surface forms an extension of the electron capture layer, and the remaining second dielectric layer on the first surface forms a main body of the electron capture layer.

5. The method for manufacturing a 3D NAND flash memory device according to claim 4, wherein: The channel structure includes a channel hole, and a channel polysilicon layer and a channel dielectric layer that fill the channel hole; The channel hole extends into the semiconductor substrate layer, the channel polysilicon layer covers the inner wall of the channel hole, and the channel polysilicon layer surrounds the outer periphery of the channel dielectric layer; The extension portion extends from both ends of the main portion along the second surface to a first length.

6. The method for manufacturing a 3D NAND flash memory device according to claim 2, wherein: The step of removing the photosensitive layer in the source lead-out space and retaining the photosensitive layer in the space occupied by the storage unit comprises: Using ultraviolet rays to irradiate the photosensitive layer filled in the source lead-out space through a mask; The photosensitive layer filled in the source lead-out space is removed by using a developing solution, and the photosensitive layer located in the space occupied by the storage unit is retained.

7. The method for manufacturing a 3D NAND flash memory device according to claim 1, wherein: The step of manufacturing the memory cell structure and the electrode structure of the flash memory device comprises: Etching the first dielectric layer to remove the first dielectric layer covering the side surface, retaining the first dielectric layer covering the surface of the space occupied by the storage unit, and the remaining first dielectric layer forms an electron tunneling layer of the storage unit structure; Manufacturing an oxide isolation layer and a high dielectric film layer of the memory cell structure; The oxide isolation layer is located in the space occupied by the storage unit and covers the exposed surface of the electron tunneling layer and the exposed surface of the electron capture layer; The high dielectric film layer is located in the space occupied by the memory cell and covers the exposed surface of the oxide isolation layer; The high dielectric thin film layer surrounds and forms a gate-occupied space, and the gate-occupied space is used to form a gate electrode.

8. The method for manufacturing a 3D NAND flash memory device according to claim 1, wherein: In the step of providing a semiconductor substrate layer, forming a plurality of unit isolation structures spaced apart in the horizontal direction and a channel structure penetrating the unit isolation structure in the vertical direction on the semiconductor substrate layer, wherein the spacing space on both sides of the unit isolation structure is a source lead-out space, the bottom layer of each unit isolation structure is the space occupied by the storage unit, and the top layer of each unit isolation structure is the unit isolation structure.

9. The method for manufacturing a 3D NAND flash memory device according to claim 1, wherein: The step of providing a semiconductor substrate layer, forming a plurality of cell isolation structures spaced apart in a horizontal direction and a channel structure penetrating the cell isolation structures in a vertical direction on the semiconductor substrate layer, wherein the spacing spaces on both sides of the cell isolation structures are source lead-out spaces, comprises: Providing a semiconductor substrate layer, forming a composite layer structure on the semiconductor substrate layer, wherein the composite layer structure includes multiple sacrificial dielectric layers and multiple unit isolation dielectric layers alternately stacked in sequence; forming a channel structure in the composite layer structure, wherein the channel structure penetrates the composite layer structure in a vertical direction and extends into the semiconductor substrate layer; A source lead-out space is formed in the composite layer structure, wherein the end of the sacrificial dielectric layer and the upper surface of the semiconductor substrate layer are exposed in the source lead-out space; The sacrificial dielectric layer is removed by etching to form the storage unit occupied space, and the remaining unit isolation dielectric layer forms a unit isolation layer.

10. A 3D NAND flash memory device, characterized in that: The 3D NAND flash memory device is manufactured by the 3D NAND flash memory device according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Method of manufacturing semiconductor devices

    CN109801918A

  • Three-dimensional memory device and method of forming the same

    CN111557049A

  • Three-dimensional memory device and method for forming same

    CN113924646A

  • 3D NAND flash memory device and manufacturing method thereof

    CN116528589A

  • Nonvolatile Memory Devices And Methods Of Fabricating The Same

    US20150194440A1