Optical circuit
The optical circuit configuration simplifies the manufacturing and packaging of optical modulators by integrating electrodes within the SiPh circuit, addressing the complexity and cost issues of existing LN thin film on SiPh circuit designs, and enabling efficient miniaturization and high-density packaging.
Patent Information
- Application Number
- PCT/JP2023/020700
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-06-02
- Publication Date
- 2024-12-05
AI Technical Summary
The manufacturing process of optical modulators with a lithium niobate (LN) thin film on a silicon photonic (SiPh) circuit is complex and costly due to the need for additional photolithography steps and incompatible electrode heights, limiting miniaturization and packaging efficiency.
An optical circuit configuration where the silicon substrate, cladding layer, and ferroelectric thin film are arranged in order, with electrodes formed within the SiPh circuit to modulate the refractive index of the LN thin film, eliminating the need for additional photolithography and allowing flip-chip mounting.
This configuration simplifies the manufacturing process, enables all electrodes to be formed at the same height, and facilitates high-density packaging, improving the manufacturability and packaging efficiency of optical modulators.
Smart Images

Figure JP2023020700_05122024_PF_FP_ABST
Abstract
Description
optical circuit
[0001] The present invention relates to optical circuits, and more particularly to the structure of optical circuits including ferroelectric thin films.
[0002] With the spread of IoT and 5G (fifth generation mobile communication system) services, there is a demand for even faster speeds in the optical communication networks that support them. Research and development is ongoing to achieve higher performance, smaller size, and lower power consumption in optical modulators, which are one of the key devices.
[0003] LN optical modulators are optical modulators that utilize the refractive index change due to the Pockels effect of LiNbO3 (hereinafter referred to as LN) crystals, and are one of the core devices in optical communications. They are used as external modulators to modulate CW light from DFB lasers and other sources, and are capable of high-speed modulation exceeding 100 GHz. They are also expected to be used as optical modulators in optical modules such as the high-bandwidth coherent driver modulator (HB-CDM) proposed by the Optical Internetworking Forum (OIF). To achieve smaller size and lower cost, optical modulators with thin-film LN attached to a Si waveguide are expected to be developed due to their high efficiency and wide bandwidth.
[0004] FIG. 1 is a schematic diagram showing the configuration of an LN thin-film SiPh hybrid optical modulator (see Non-Patent Document 1). The optical modulator 700 has a hybrid configuration of an LN thin-film and SiPh circuit, in which an LN thin-film 12 is attached to a silicon photonic (SiPh) circuit, which has a SiO layer and a core layer formed on a Si substrate 10. The branched core layer forms a Mach-Zehnder interferometer (MZI) including two interference optical waveguides 21. High-frequency electrodes 22 are further formed on the top surface of the LN thin-film 12, sandwiching each of the interference waveguides 21. The core, the surrounding SiO cladding, and the LN thin-film 12 adjacent to the core function together as an optical waveguide. Light is not only confined by the core, but also seeps into and propagates through the LN, functioning as a composite optical waveguide in which the ferroelectric LN and Si core are integrated.
[0005] By modulating the refractive index of the attached thin film LN with a high-frequency electrical signal applied to the modulating electrode 22, the interference conditions of the MZI change, turning on / off the combined optical output of the two interference optical waveguides. By combining thin film LN with SiPh circuits, it is expected that the optical module including the optical modulator will be significantly miniaturized and highly efficient.
[0006] Weigel, Peter O., et al. "Hybrid silicon photonic-lithium niobate electro-optic Mach-Zehnder modulator beyond 100 GHz bandwidth." arXiv preprint arXiv:1803.10365 (2018)
[0007] However, the optical modulator configured with an LN thin film bonded to a SiPh circuit as shown in Figure 1 has problems with its manufacturability and assembly. The modulating electrode 22, to which an electrical signal for refractive index modulation is applied, is formed on the LN thin film 12. Typically, the process of bonding the LN thin film to the SiPh circuit must be performed as an independent process after the photolithography process for fabricating the SiPh circuit has been completed. As a result, the photolithography process for forming the high-frequency electrode 22 must be performed twice. This manufacturing process for an optical modulator is complex and expensive. Furthermore, the height of the pad relative to the other electrodes fabricated in the SiPh circuit process differs from the height of the pad relative to the modulating electrode 22. The subsequent process of assembling the fabricated optical modulator chip into an optical module, etc., also limits flip-chip mounting for miniaturization.
[0008] The present invention has been made in view of the above-mentioned problems, and provides an optical circuit configuration that combines a ferroelectric thin film and a SiPh circuit, with improved manufacturability and mountability.
[0009] One embodiment of the present invention is an optical circuit comprising a silicon substrate, a cladding layer, and a ferroelectric thin film arranged in that order, the optical circuit comprising a core formed within the cladding layer, and one or more electrodes formed along the core for applying an electric field to the ferroelectric thin film.
[0010] The present invention provides an optical circuit that combines a ferroelectric thin film and a SiPh circuit, with improved manufacturability and mountability.
[0011] FIG. 1 is a schematic diagram showing the configuration of an LN thin-SiPh hybrid optical modulator; FIG. 2 is a diagram schematically showing the configuration of a hybrid optical modulator of the prior art; FIG. 3 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 1; FIG. 4 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 2; FIG. 5 is a diagram showing the configuration of a mode converter between a SiN core and a Si core; FIG. 6 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 3; FIG. 7 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 4; FIG. 8 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 5; and FIG. 9 is a diagram schematically showing the configuration of the top surface and side cross section of an optical circuit of embodiment 6.
[0012] The optical circuit disclosed herein provides a novel configuration that combines a ferroelectric thin film and a SiPh circuit, improving manufacturability and mountability. As an example, a novel configuration suitable for an LN-Si hybrid optical modulator is presented. Electrodes to which an electrical signal that modulates the refractive index of the LN thin film is applied are formed within the SiPh circuit. Because all electrodes in the optical circuit are formed during the fabrication process of the SiPh circuit, additional photolithography is not required after attaching the LN thin film. It is possible to fabricate high-frequency electrodes and other electrodes, such as those for bias, at the same height, enabling flip-chip mounting of the fabricated optical modulator chip in a subsequent process. This improves the manufacturability and mountability of devices that utilize the electro-optic effect of LN, including optical modulators.
[0013] Below, we will first use an optical modulator as an example to clarify the configuration of optical circuits in the prior art and their problems. Next, we will explain in detail the basic configuration, modifications, and manufacturing process of the optical circuit disclosed herein. In the following description, a hybrid optical modulator refers to a Mach-Zehnder modulator (MZM) that combines an LN thin film and a SiPh circuit. All drawings of the optical circuit structure described below are schematic diagrams and are not drawn to scale. The substrate thickness direction (z direction) is significantly enlarged. Please also note that the relative relationships between elements, such as the height and width, are not necessarily accurately depicted.
[0014] In the following description, the optical circuit of the present disclosure will be described as being applied to a hybrid optical modulator. However, the optical circuit configuration of the present disclosure can also be applied to other optical circuits configured with a ferroelectric thin film attached to a SiPh circuit. Ferroelectric materials are not limited to lithium niobate (LN) and include lithium tantalate (LT) and barium titanate, as long as they can change the refractive index of the optical waveguide through the electro-optic effect. Furthermore, optical devices utilizing refractive index modulation of a ferroelectric thin film near the core can also include, in addition to optical modulators, polarization controllers and phase shifters that can be used to compensate for polarization mode dispersion.
[0015] FIG. 2 is a schematic diagram illustrating the configuration of a conventional hybrid optical modulator. FIG. 2(a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), and FIG. 2(b) is a side cross-sectional view (y-z plane) taken along line IIb-IIb and perpendicular to the substrate surface and the light propagation direction. FIG. 2(c) is a side cross-sectional view taken along line IIc-IIc and perpendicular to the substrate surface and the light propagation direction. In the conventional MZ-type hybrid optical modulator 700 shown in FIG. 1, the portion of one optical waveguide 21 of the two interference optical waveguides, including modulation electrodes 22a and 22b, that functions as a refractive index modulation region is schematically illustrated. Referring to the two side cross-sectional views of FIG. 2(b) and (c), the SiPh circuit in the optical modulator 700 includes a SiO layer 11 formed on a Si substrate 10 and a rectangular Si core 12.
[0016] The SiPh circuit includes, for example, an electrode 23 formed inside SiO2, which functions as a cladding layer. The electrode 23 can be a high-frequency electrode through which the modulation signal of the optical modulator propagates, or it can be an electrode for other circuits, such as an electrical circuit, integrated with the optical modulator. The electrode 23 is shown schematically as a different configuration from the modulation electrode 22, and its position on the top surface of the optical circuit 700 is not important. Furthermore, its height position in the cross-sectional view is not limited to the position shown in Figure 2(c). This SiPh circuit can be fabricated by forming each layer on a Si substrate and patterning the core and electrodes using photolithography. Alternatively, the SiPh circuit can be fabricated by processing an SOI (silicon-on-insulator) substrate, on which a Si layer and a SiO2 layer, which function as the core, have already been formed.
[0017] An LN thin film 12 is attached to the SiPh circuit. The LN thin film is attached by activating the surface of the LN thin film and SiO2 layer, which have been pre-formed to the required size, with an argon beam, bringing them into contact, and then applying pressure and heat. Because the LN thin film 12 is formed by bonding the LN thin film, a physical attachment process separate from the Si photolithography process is required. To create a refractive index change in the LN thin film 12, which serves as part of the optical waveguide for light leaking from the Si core 12, modulation electrodes 22a, 22b, for example, gold electrodes, are formed on the LN thin film 12. Connection pads 24a, 24b are formed at the ends of the electrodes. Forming these modulation electrodes 22a, 22b requires a second photolithography process after attaching the LN thin film 12, which complicates the manufacturing process of the optical modulator 700 and increases costs.
[0018] 2(b) and 2(c), the height of the modulation electrodes 22a and 22b is different from the height of the electrode 23 of the SiPh circuit. In terms of the circuit configuration of the optical circuit, if the electrode heights are different, high-density packaging technology using ball grid arrays (BGA) cannot be used. The inability to use effective BGA technology in optical modulators, which require miniaturization and high-density packaging, is a major obstacle to the miniaturization of optical modules and optical transmission devices. The optical circuit disclosed herein solves the problems of manufacturability and packaging, which were shown in the optical modulator 700 described above.
[0019] [Embodiment 1] FIG. 3 is a diagram schematically illustrating the top and side cross-sectional configurations of an optical circuit according to Embodiment 1. This diagram also illustrates the configuration of a hybrid optical modulator as an example of the optical circuit 100 of this embodiment. Similar to FIG. 2, FIG. 3(a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), FIG. 3(b) is a side cross-sectional view (x-y plane) taken along line IIIb-IIIb, and FIG. 3(c) is a side cross-sectional view (x-y plane) taken along line IIIc-IIIc, perpendicular to the substrate surface and the light propagation direction. FIG. 3 is a schematic diagram illustrating a portion of one optical waveguide 31 of two interference optical waveguides in an MZ-type optical modulator, including modulation electrodes 30a and 30b, which functions as a refractive index modulation region. The configuration of the core 31 of the optical waveguide is similar to that of the core 21 of the conventional optical circuit 700 shown in FIG. 2. The following description focuses on the differences from the conventional optical circuit 700.
[0020] The optical circuit 100 differs from conventional configurations in that the modulating electrodes 30a, 30b are formed within the SiO cladding region in a plane perpendicular to the SiPh circuit substrate, whereas the electrodes are formed on an LN thin film outside the SiPh circuit. The PADs 34a, 34b connected to the modulating electrodes 30a, 30b do not contribute to the refractive index modulation of the LN thin film and are not included in the refractive index modulation region. The modulating electrodes 30a, 30b each have PADs 34a, 34b at both ends via vias. The PADs are connected to electrical circuits, electrical signal sources, etc., that supply electrical signals via some means. They may be wire-bonded or connected to other electrical elements or driver circuits via BGA. Alternatively, the modulating electrodes may be directly connected to an electrical circuit integrated on the same Si substrate as the optical modulator, without the PAD. In the optical modulator, the modulating electrodes serve as high-frequency electrodes to which high-frequency electrical signals are applied.
[0021] 3, for the purpose of indicating the input points of the modulation signals, the PADs 34a and 34b are shown as being generally adjacent to the LN thin film 12. The modulating electrodes 30a and 30b may be extended, and the PADs may be formed at positions away from the region of the LN thin film 12. It should be noted that the positions of the PADs 34a and 34b in FIG. 3 are merely examples.
[0022] Because the modulating electrodes 30a and 30b are formed in the SiO2 clad region in a plane perpendicular to the SiPh circuit substrate, the modulating electrodes, like all other electrodes, can be fabricated in the same photolithography process for the SiPh circuit. This eliminates the need for an additional photolithography process after the LN thin film 12 attachment process, as in the prior art. Furthermore, it is possible to form the pads of all electrodes, including the modulating electrodes, at the same height. This allows for flip-chip mounting using BGA or bumps.
[0023] Therefore, the optical circuit of the present invention can be implemented as an optical circuit in which a silicon substrate 10, a cladding layer 11, and a ferroelectric thin film 12 are arranged in this order, and which includes a core 31 formed within the cladding layer, and one or more electrodes 30a, 30b formed along the core for applying an electric field to the ferroelectric thin film.
[0024] 3(b) and 3(c), the modulating electrodes 30a and 30b are shown as having the same bottom surface height as the Si core 31 in the substrate thickness direction (z direction), but this is not limited thereto. As long as the modulating electrodes 30a and 30b are formed within the SiO2 layer 11 in a plane perpendicular to the substrate of the SiPh circuit, the modulating electrodes are fabricated in the same photolithography process as all other electrodes of the SiPh circuit. Electrodes other than the modulating electrodes may be fabricated at different heights.
[0025] [Embodiment 2] Figure 4 is a diagram showing the top and side cross-sectional configurations of an optical circuit according to Embodiment 2. The configuration of a hybrid optical modulator is also shown as an example of the optical circuit 200 of this embodiment. Figure 4(a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), Figure 4(b) is a side cross-sectional view (x-y plane) taken along line IVb-IVb, and Figure 4(c) is a side cross-sectional view (x-y plane) taken along line IVc-IVc, perpendicular to the substrate surface and the light propagation direction. Figure 4 is a schematic diagram showing the portion of one optical waveguide 32 of the two interference optical waveguides in an MZ-type optical modulator 200, which includes modulation electrodes 30a and 30b and functions as a refractive index modulation region. The differences from the optical circuit 100 of Embodiment 1 are as follows.
[0026] In the optical circuit 100 of the first embodiment described above, the optical waveguide whose refractive index is modulated comprises a Si core 31, a surrounding SiO cladding, and an LN thin film 12 adjacent to the core in the refractive index modulation region, forming a composite waveguide. The Si core 31, together with the surrounding SiO cladding, forms a continuous optical waveguide both inside and outside the refractive index modulation region having a hybrid configuration with the LN thin film. In contrast, in the optical circuit 200 of this embodiment, the optical waveguide whose refractive index is changed by an electrical signal is composed of a silicon nitride (SiN) core 32 located closer to the LN thin film 12 than the Si core. Outside the refractive index modulation region having a hybrid configuration with the LN thin film, the optical waveguide is composed of the Si core 31, separate from the SiN core. In the thickness direction (z direction) of the substrate, the SiN core 32 can be formed higher than the Si core 31 and closer to the LN thin film 12. This allows for efficient refractive index modulation of the LN thin film 12 by an electrical signal. The SiN core 32 and the Si core 31, which are different in height, can be optically connected by the mode converter 40 formed near the boundary of the LN thin film 12 in FIG. 4(a).
[0027] FIG. 5 illustrates the configuration of a mode converter between a SiN core and a Si core. FIG. 5(a) is a top view of the optical circuit 200, looking at the Si substrate surface (x-y plane), showing only the two types of cores 32 and 31 near the mode converter 40. FIG. 5(b) is a side cross-sectional view (x-z plane) of the mode converter 40, taken along the substrate surface and the light propagation direction, passing through the center line (Vb-Vb) of the core. Referring to FIG. 5(a), the mode converter 40 has a first taper at the tip of the SiN core 32, where the core width gradually narrows, and a second taper at the tip of the Si core 31, where the core width gradually widens. Referring to FIG. 5(b), two tapered sections overlap above and below within the region of the mode converter 40 in the SiO cladding layer 11, providing efficient optical coupling between optical waveguides of different heights. The mode converter is not limited to the one illustrated in FIG. 5; other configurations can be used as long as they are capable of optical mode conversion.
[0028] 4, the mode converter 40 is shown as being located near the end of the LN thin film 12, but it may be located within the region of the LN thin film 12 or outside the region of the LN region 12. The position of the mode converter 40 is not important as long as the SiN core 32 can produce a sufficient electro-optic effect (e.g., a change in refractive index) with the adjacent modulating electrodes 30a and 30b.
[0029] Therefore, the optical circuit of the present invention can be implemented as a core including a first core 32 of silicon nitride formed on the side of the ferroelectric thin film 12 in the thickness direction (z direction) of the substrate within the region where the ferroelectric thin film 12 is formed on the substrate surface (xy plane), and a second core 31 of silicon formed on the side of the substrate closer to the first core in the thickness direction, and the first core and the second core are optically coupled.
[0030] According to the optical circuit 200 of the second embodiment, an additional photolithography process is not required after the process of attaching the LN thin film 12, and it is possible to form the PADs of all electrodes, including the modulation electrodes, at the same height. The SiN core in the refractive index modulation region where the LN thin film is attached can also be formed within the series of manufacturing processes for the SiPh circuit. Because the SiN core 32 and the LN thin film 12 can be placed close to each other, applying the configuration of the optical circuit 200 to an optical modulator can efficiently generate refractive index modulation.
[0031] 4(b) and 4(c), the modulating electrodes 30a and 30b are shown as being located midway between the SiN core 32 and the Si core 31 in the substrate thickness direction (z direction), but this is not limiting. As long as the modulating electrodes 30a and 30b are formed within the SiO layer 11 in a plane perpendicular to the substrate of the SiPh circuit, the modulating electrodes are fabricated in the same photolithography process as all other electrodes of the SiPh circuit. Electrodes other than the modulating electrodes may be fabricated at different heights.
[0032] [Embodiment 3] Figure 6 is a diagram showing the top and side cross-sectional configurations of an optical circuit according to Embodiment 3. It is a diagram showing the configuration of a hybrid optical modulator as an example of an optical circuit 300 according to this embodiment. Figure 6(a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), Figure 6(b) is a side cross-sectional view (x-y plane) taken along line VIb-VIb, and Figure 6(c) is a side cross-sectional view (x-y plane) taken along line VIc-VIc, perpendicular to the substrate surface and the light propagation direction. Figure 6 is a diagram showing a portion of one optical waveguide 31 of two interference optical waveguides in an MZ-type optical modulator 300, including modulation electrodes 30a and 30b, which functions as a refractive index modulation region. The differences from the optical circuit 100 according to Embodiment 1 are as follows.
[0033] In the optical circuit 100 of the first embodiment described above, the LN thin film 12 is configured exclusively in the refractive index modulation region where the MZI including the two interference optical waveguides 21 is configured. The ends of the modulation electrodes 30a and 30b to which an electric signal is applied are provided with PADs to which bonding wires or the like from an electric signal source are connected, so it is essential to align the LN thin film so that it does not cover the PADs. Furthermore, when multiple optical modulators are fabricated on one wafer, a process of aligning the multiple LN thin films and attaching them to each other is required.
[0034] The optical circuit 300 of this embodiment differs from Embodiments 1 and 2 in that the PADs 35a and 35b of the modulating electrodes 30a and 30b are configured on the back surface of the Si substrate opposite to the LN thin film 12. The PADs 35a and 35b are formed on the surface of the Si substrate 10 opposite to the surface to which the LN thin film 12 is attached. The modulating electrodes 30a and 30b are connected to the PADs 35a and 35b by through-silicon vias (TSVs) 36a and 36b, respectively.
[0035] Since the external electrical signal source and the PADs 35a and 35b can be connected to the surface of the Si substrate opposite to the LN thin film 12, there is no need to limit the position of the LN thin film 12, and the accuracy of the attachment position can be low. For multiple optical modulator chips, one LN thin film can be attached to the entire surface of the SiO2 layer 11.
[0036] 6(b) and 6(c), the modulating electrodes 30a and 30b are shown as having the same bottom surface height as the Si core 31 in the substrate thickness direction (z direction), but this configuration is not limited to this. As long as the modulating electrodes 30a and 30b are configured within the SiO2 layer 11 in a plane perpendicular to the SiPh circuit substrate, the modulating electrodes can be fabricated in the same photolithography process as all other electrodes in the SiPh circuit. Electrodes other than the modulating electrodes may be fabricated at different heights.
[0037] [Embodiment 4] Figure 7 is a diagram showing the top and side cross-sectional configurations of an optical circuit according to Embodiment 4. The configuration of a hybrid optical modulator is also shown as an example of an optical circuit 400 according to this embodiment. Figure 7(a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), Figure 7(b) is a side cross-sectional view (x-y plane) taken along line VIIb-VIIb, and Figure 7(c) is a side cross-sectional view (x-y plane) taken along line VIIc-VIIc, perpendicular to the substrate surface and the light propagation direction. Figure 6 is a schematic diagram showing a portion of one of two interference optical waveguides in an MZ-type optical modulator 400, including modulation electrodes 30a and 30b, which functions as a refractive index modulation region. The differences between the optical circuits 100, 200, and 300 of the above-described embodiments and the optical circuit 400 are as follows.
[0038] In the optical modulator using the optical circuit 400 of this embodiment, the core is composed of a SiN 32 core in the refractive index modulation region and a Si core 31 outside the refractive index modulation region, similar to the optical modulator 200 of the second embodiment. It also includes a mode converter 40 between the SiN core and the Si core, as shown in FIG. 5 . The modulating electrodes 33a and 33b differ from the electrodes of the other embodiments described above in that they extend along the core in the x-direction and have a wall-like shape standing in the z-direction. The TSV can be considered to be continuously formed in the x-direction. In other words, the high-frequency electrodes serving as modulating electrodes are wall-like electrodes 33a and 33b that are continuously formed in the thickness direction of the substrate 10, penetrating from the height of the core 32 to the surface opposite the cladding layer 11 of the substrate.
[0039] As mentioned above, FIG. 7 is a schematic diagram, and the scales are not consistent in each direction. The substrate thickness direction (z direction) is significantly enlarged, and the cross sections (y-z planes) of the modulating electrodes 30a and 30b in Embodiments 1 to 3 are actually rectangular with their horizontal lengths in the y direction. On the other hand, the cross sections (y-z planes) of the modulating electrodes 33a and 33b in Embodiment 4 shown in FIG. 7(b) can be rectangular with their vertical lengths in the z direction, as well as horizontal lengths in the y direction, allowing for significant changes in electrode shape. It should be noted that the characteristic impedance as a transmission path for high-frequency electrical signals can also be calculated using different parameter values. Compared to the modulating electrodes of Embodiments 1 to 3, the same characteristic impedance can be obtained with electrodes 33a and 33b that are narrower in the y direction parallel to the substrate surface. Therefore, by narrowing the electrode width, the wall-shaped modulating electrodes 33a and 33b of Embodiment 4 shown in FIG. 7(b) are more suitable for high-density integration.
[0040] It does not matter if the positional accuracy when attaching the LN thin film 12 is low, and it is also possible to attach one LN thin film to the entire surface of the SiO2 layer 11 for a plurality of optical modulator chips.
[0041] [Embodiment 5] Figure 8 is a diagram showing the top and side cross-sectional configurations of an optical circuit according to Embodiment 5. The configuration of a hybrid optical modulator is shown as an example of the optical circuit 500 of this embodiment. Figure 8 (a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), Figure 8 (b) is a side cross-sectional view (x-y plane) taken along line VIIIb-VIIIb, and Figure 8 (c) is a side cross-sectional view (x-y plane) taken along line VIIIc-VIIIc, perpendicular to the substrate surface and the light propagation direction. Figure 8 also shows a schematic diagram of a portion of one optical waveguide 31 of two MZ-type interference optical waveguides in an MZ-type optical modulator, which includes modulation electrodes 37a and 37b and functions as a refractive index modulation region.
[0042] The optical circuit 500 of this embodiment has the same configuration as the optical circuit 300 of Embodiment 3 shown in FIG. 6 in terms of the optical waveguide and modulating electrodes. The difference from the configuration of Embodiment 3 is that the modulating electrodes 37a and 37b are made of Si doped with impurities by ion implantation or the like, rather than metals such as aluminum, copper, or gold. By using ion-implanted Si as the material for the high-frequency electrodes, the high-frequency electrodes can be formed in the same layer as the Si core 31. According to the configuration of the optical circuit 500 of this embodiment, the modulating electrodes 37a and 37b can be formed directly beside the Si core 31 at the same height, which facilitates electric field concentration within the LN thin film 12. Applying the configuration of the optical circuit 500 to an optical modulator enables efficient refractive index modulation.
[0043] 8 shows an example in which modulating electrodes 37a, 37b made of impurity-doped Si are combined with PADs 35a, 35b formed on the backside of a Si substrate. However, the present invention can also be applied to cases in which PADs 34a, 34b are formed on the top surface of the SiO2 layer 11, as in the first and second embodiments shown above. In this case, however, the LN thin film must be attached only to the top side of the modulating electrodes.
[0044] [Embodiment 6] Figure 9 is a diagram showing the top and side cross-sectional configurations of an optical circuit according to Embodiment 6. As an example, it is a diagram showing the configuration of a hybrid optical modulator 600. Figure 9 (a) is a top view of the SiPh circuit, looking at the Si substrate surface (x-y plane), Figure 9 (b) is a side cross-sectional view (x-y plane) taken along line IXb-IXb, and Figure 9 (c) is a side cross-sectional view (x-y plane) taken along line IXc-IXc, perpendicular to the substrate surface and the light propagation direction. Figure 9 is a diagram showing a portion of one of two interference optical waveguides in an MZ-type optical modulator 600, which includes a modulation electrode and functions as a refractive index modulation region.
[0045] Like the optical circuit 200 of the second embodiment, the optical circuit 600 has an optical waveguide structure in which the SiN core 32 and the Si core 31 are coupled by the mode conversion section 40. Since the SiN core 32 and the LN thin film 12 can be brought into close proximity, like the optical circuit 200, refractive index modulation can be efficiently generated.
[0046] The optical circuit 600 of this embodiment differs from the optical circuit of embodiment 2 in that the positions of the modulating electrodes 30a, 30b in the substrate thickness direction (z direction) are at the same height as the SiN core 32. Furthermore, PADs 35a, 35b to which bonding wires or the like from an electric signal source are connected for applying electric signals to the modulating electrodes are formed on the back surface of the Si substrate 10 on the side opposite to the LN thin film 12, as in embodiments 3 to 5. The modulating electrodes 30a, 30b and the PADs 35a, 35b are connected by TSVs 36a, 36b, respectively.
[0047] According to the configuration of the optical circuit 600 of this embodiment, by forming the modulating electrodes 30a and 30b directly beside the SiN core at the same height, the electric field tends to concentrate inside the LN thin film 12. Applying the configuration of the optical circuit 600 to an optical modulator enables efficient refractive index modulation. Since the external electrical signal source and the PADs 35a and 35b can be connected on the side opposite the LN thin film 12, there is no need to limit the position of the LN thin film 12, and the accuracy of the attachment position can be low. For multiple optical modulator chips, a single LN thin film can also be attached to the entire surface of the SiO layer 11.
[0048] The optical circuit 600 in Figure 9 shows an example in which PADs 35a and 35b are formed on the back side of the Si substrate, and the positions of the modulating electrodes 30a and 30b in the substrate thickness direction are at the same height as the SiN core 32. However, this can also be applied to the case in which PADs 34a and 34b are formed on the upper surface of the SiO2 layer 11 in the previously shown embodiment 2. In this case, however, the LN thin film needs to be attached only to the upper side of the modulating electrodes. Furthermore, the optical circuit 600 of this embodiment can also be combined with a modulating electrode 3 made of Si to which impurities have been added by ion implantation or the like, as in embodiment 5.
[0049] The above-described embodiments have been described using hybrid optical modulators that combine an LN thin film and a SiPh circuit as examples. However, ferroelectric materials such as lithium tantalate (LT) and barium titanate can also be used instead of the LN thin film. Furthermore, optical devices that utilize the electro-optic effect of ferroelectric thin films are not limited to optical modulators. For example, polarization controllers that arbitrarily control the polarization state of light and phase shifters that arbitrarily change the phase state of light can be realized. When used as a polarization controller or phase shifter, it should be noted that a low-frequency control signal, a constant DC signal, or the like can be applied to the electrodes that apply an electric field to the above-described ferroelectric thin film, rather than a modulation signal. Furthermore, when the polarization controller is operated as a polarization scrambler, a signal of approximately several GHz may be applied.
[0050] As described above in various embodiments, the optical circuit of the present invention can improve the manufacturability and mountability of an optical circuit that combines a ferroelectric thin film and a SiPh circuit.
[0051] The present invention can be used in optical communications.
Claims
1. An optical circuit comprising a silicon substrate, a cladding layer, and a ferroelectric thin film, arranged in that order, the optical circuit comprising: a core formed within the cladding layer; and one or more electrodes formed along the core for applying an electric field to the ferroelectric thin film.
2. The optical circuit described in claim 1, wherein the core includes a first core of silicon nitride formed on the side of the ferroelectric thin film in the thickness direction of the substrate within a region of the substrate where the ferroelectric thin film is formed, and a second core of silicon formed on the side of the substrate closer to the first core in the thickness direction, and the first core and second core are optically coupled.
3. The optical circuit according to claim 2, wherein said one or more electrodes are formed at the same height as said first core in said thickness direction.
4. An optical circuit as claimed in any one of claims 1 to 3, wherein the one or more electrodes are wall-shaped electrodes formed continuously in the thickness direction of the substrate, penetrating from the height of the core to the surface of the substrate opposite the cladding layer.
5. An optical circuit according to any one of claims 1 to 3, wherein said one or more electrodes are made of silicon doped with impurities.
6. An optical circuit according to any one of claims 1 to 3, wherein a PAD is formed on the surface of the substrate opposite to the clad layer at an end of the electrode via a through silicon via (TSV).
7. An optical circuit according to any one of claims 1 to 3, wherein a PAD is formed on the upper surface of said cladding layer at the end of said electrode through a via.
8. An optical circuit as claimed in any one of claims 1 to 3, wherein the cladding layer is made of SiO2, the ferroelectric thin film is any one of lithium niobate (LN), lithium tantalate (LT) and barium titanate, and the one or more electrodes are supplied with an electrical signal that produces an electro-optic effect in the ferroelectric thin film.
Citation Information
Patent Citations
Multilayered photoelectron substrate with electrical intercoupling and optical intercoupling, and manufacture thereof
JP2000114581A
Spot size converter and manufacturing method thereof
JP2016018191A
Method and system for forming stabilized tetragonal barium titanate
JP2023500463A
Heterogeneously integrated electro-optic modulator
US10788689B1
Organic thin-film optical integrated circuit
WO2017130744A1