Composition for manufacture of a dielectric substrate and method for producing a foil-clad dielectric material

The use of fusible copolymers and quartz fillers in a hot pressing process addresses the high dielectric losses and adhesion issues of PTFE substrates, achieving low dielectric constants and thermal expansion in printed circuit boards for frequencies above 20 GHz, with improved adhesion and reduced processing costs.

WO2024248651A1PCT designated stage expired Publication Date: 2024-12-05OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOSTYU SINTEZ PROEKT +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/RU2023/000158
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-06-01
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Existing polymer dielectric substrates for printed circuit boards experience high dielectric losses and coefficient of linear thermal expansion at frequencies above 20 GHz, and polytetrafluoroethylene (PTFE) substrates require complex surface preparation due to low adhesion with most adhesives and high thermal expansion coefficients.

Method used

A foil dielectric composition using fusible copolymers of perfluorinated ethylene and propylene with quartz fillers and metal foils, processed by hot pressing without additional adhesives, ensuring impregnation and adhesion at elevated pressures and temperatures, utilizing copolymers like hexafluoropropylene and tetrafluoroethylene (FEP) as the fluoropolymer matrix, which offers lower processing temperatures and efficient filler impregnation.

Benefits of technology

The solution achieves minimal dielectric losses and low dielectric constants below 2.5, along with reduced coefficient of linear thermal expansion, across a wide frequency range including above 20 GHz, and provides strong adhesion without pre-treatment, enabling the production of dielectric materials with thicknesses of 50 to 150 μm and improved thermal stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

A composition and method for manufacturing thin (150 μm or less) polymeric dielectric substrates with low dielectric losses (less than 0.001) at superhigh frequencies (5G, 6G), which are foil clad with an electrically conductive layer on one or two sides. The claimed polymer substrate composition consists of an injection moldable fluoroplastic and a quartz filler. The fluoroplastic is selected from among F-4MB grade perfluorinated copolymers of ethylene and propylene, or analogs thereof, namely Teflon FEP, Neoflon FEP, Dyneon FEP. The quartz filler can consist of continuous fibers (yarns or tows, or fabrics) and / or dispersed fillers (discontinuous fibers, powders, flakes and the like). The proposed technology for producing a foil-clad dielectric material does not entail the use of a special adhesive layer between the foil and the polymer substrate and consists in hot pressing three separate components – a polymer film, a quartz filler and a foil, i.e. in a single operation, the filler is impregnated with a molten fluoroplastic and the dielectric material is bonded to a metal foil.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] COMPOSITION FOR MANUFACTURING A DIELECTRIC SUBSTRATE AND A METHOD FOR PRODUCING A FOIL-COATED DIELECTRIC

[0002] The invention relates to the field of radio engineering and electronics industry, namely to the technology of manufacturing dielectric substrates for printed circuit boards.

[0003] For printed circuit boards of microcircuits operating at frequencies above 20 GHz (5G, 6G), it is preferable to use materials with minimal dielectric losses (no more than 0.001) and minimal dielectric constant (no more than 2.5) as dielectric materials. Such materials may be ceramic materials (not considered in this application, since they belong to a different class of materials and have a much narrower scope of application and higher cost) and polymeric materials.

[0004] Many polymeric materials traditionally used in printed circuit boards at frequencies below 10-20 GHz have too high dielectric loss values ​​(more than 0.001) at frequencies above 20 GHz. Polymeric materials from a number of polyolefins and fluorinated polyolefins remain suitable for use in the frequency range above 20 GHz. Polyolefins do not meet the heat resistance requirements, so the only class of polymers suitable for the above-mentioned tasks are fluorinated polyolefins.

[0005] Most existing polymer dielectric substrates of printed circuit boards are made on the basis of polytetrafluoroethylene (hereinafter referred to as PTFE), since this polymer has low dielectric loss values ​​(less than 0.001) in the widest frequency range, has excellent chemical resistance and heat resistance. Among the disadvantages, firstly, it can be noted that PTFE has too high a coefficient of linear thermal expansion (hereinafter referred to as CLTE), therefore, to obtain dielectric substrates of printed circuit boards, it is filled with continuous or dispersed ceramic fillers, most often based on glass materials. However, for use in the frequency range above 20 GHz, filling fluoropolymers with such ceramic materials or glass materials is not permissible, since it leads to an increase (more than 0.001) in dielectric losses Df.The second significant disadvantage of PTFE from the point of view of applicability to the production of foil-clad dielectrics is its extremely low adhesion to most adhesives, which requires complex and expensive preparation of the PTFE surface before gluing, for example, treatment with melts of alkali metals or their complexes.

[0006] The closest analogue to the present invention is the international application for invention EP 0 695 1 16 A1 of Rogers Corporation, where the composite material described in the application includes at least two types of ceramic fillers in order to be able to independently regulate the dielectric constant Dk (within the range from 3 to 20) and the CTE of the composite. However, this application did not pursue the goal of obtaining a material with dielectric losses Df less than 0.001 at frequencies above 20 GHz (communication generations 5G, 6G), therefore, in all examples of the invention, glass fabric or non-woven fabric is used, which makes it possible to reduce the CTE, or a very high (~ 60%) filling of the dielectric material with dispersed filler fused amorphous silicon dioxide, which leads to a high (2.9 and more) Dk value.Polytetrafluoroethylene (PTFE) is most preferred as the matrix, but one or a combination of the following fluoropolymers may also be present: tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA), hexafluoropropylene-tetrafluoroethylene copolymer (FEP), ethylene-tetrafluoroethylene copolymer, and polyvinylidene fluoride.

[0007] The claimed composition and technology are free from the above-mentioned disadvantages and allow obtaining a material with minimal dielectric losses (no more than 0.001) and a minimal dielectric constant (no more than 2.5) at frequencies, including those above 20 GHz. The present invention consists of the following: to obtain a foil-clad dielectric, films based on fusible copolymers of perfluorinated ethylene and propylene, quartz fillers and metal foils are used as a polymer material, while the finished material is obtained in one step by hot pressing without using additional adhesive compositions and does not require preliminary processing of the polymer film, quartz filler and foil. Impregnation of the filler and adhesion to the foil are ensured by increased pressure and temperature in the range from 290 to 330 °C.The fluoropolymer matrix was chosen to be hexafluoropropylene and tetrafluoroethylene (FEP) copolymers because, compared to polytetrafluoroethylene (PTFE): 1) a lower processing temperature is required (lower energy costs, cheaper auxiliary tooling and heat-pressing equipment) and 2) a lower melt viscosity allows for more efficient impregnation of reinforcing fillers. The present invention allows for producing foil dielectrics with a dielectric material thickness of at least 50 to 150 μm and higher, with dielectric constant values ​​below 2.5 and a dielectric loss tangent of less than 0.001, including at frequencies from 20 to 200 GHz. In addition, the resulting materials have low CLTE values ​​in the XY plane due to quartz fillers. The invention is illustrated by the following examples.

[0008] Example 1. Foiled dielectric based on quartz threads and F-4MB film.

[0009] A copper foil of 18 μm thickness was placed on the flat forming tool, then a film of F-4MB of 50 μm thickness, then a quartz thread was wound first in the X direction with a step of 1 mm, then in the perpendicular direction Y with a step of 0.5 mm (equivalent to two passes with a step of 1 mm) and again in the X direction with a step of 1 mm. Then it was covered with a layer of F-4MB film of 50 μm thickness and copper foil of 18 μm thickness. The assembly was placed in a plane-parallel press mold and heated under pressure from 1 t to 10 t to a temperature of 300 °C, cooled to room temperature, unloaded and the foil-clad dielectric was removed from the press mold. The obtained material had the following characteristics: Dk / Df = 2.61 / 0.00086 at 28 GHz, 2.59 / 0.00063 at 60 GHz, the adhesion of copper foil to the dielectric substrate was 2.81 N / mm when peeled off at an angle of 90 °, the coefficient of thermal expansion in the temperature range from 30 to 150 °C in the X and Y directions = 10.9x10' 6 TO 1 , the thickness of the dielectric layer is 150 microns.

[0010] Example 2. Foiled dielectric based on quartz non-woven material and Teflon FEP film.

[0011] On the flat forming tool we placed copper foil with a thickness of 18 µm, then Teflon FEP film with a thickness of 35 µm, then a quartz veil of 10 g / m 2 50 μm thick, bonded with a polyimide compound, and again with copper foil 18 μm thick. The assembly was placed in a plane-parallel press mold and heated under pressure from 1 t to 10 t to a temperature of 310 °C, cooled to room temperature, unloaded and removed the foil-clad dielectric from the press mold. The resulting material had the following characteristics: Dk / Df = 2.02 / 0.00064 at 28 GHz, 2.00 / 0.00059 at 60 GHz, the adhesion of the copper foil to the dielectric substrate was 1.83 N / mm when peeling at an angle of 90 °, CLTE in the temperature range from 30 to 150 ° C in the X and Y directions = 26.7 x 10 ' 6 TO' 1 , thickness of the dielectric layer -

[0012] 64 µm. Example 3. Foiled dielectric based on quartz non-woven material and F-4MB film.

[0013] On the flat forming tooling we placed copper foil with a thickness of 18 microns, then F-4MB film with a thickness of 35 microns, then a quartz veil of 8 g / m 2 50 μm thick, bonded with epoxy composition, and again with copper foil 35 μm thick. The assembly was placed in a plane-parallel press mold and heated under pressure from 1 t to 10 t to a temperature of 310 °C, cooled to room temperature, unloaded and removed the foil-clad dielectric from the press mold. The resulting material had the following characteristics: Dk / Df = 2.05 / 0.00070 at 28 GHz, 2.03 / 0.00062 at 60 GHz, the adhesion of the copper foil to the dielectric substrate was 1.51 N / mm when peeling at an angle of 90 °, CLTE in the temperature range from 30 to 150 °C in the X and Y directions = 30.5x10' 6 TO' 1 , the thickness of the dielectric layer is 60 microns.

[0014] Example 4. Foiled dielectric based on quartz threads and Neoflon FEP film.

[0015] A copper foil of 18 μm thickness was placed on a flat forming tool, then a Neoflon FEP film of 50 μm thickness, then a quartz thread was wound first in the X direction with a step of 2 mm, then in the perpendicular Y direction with a step of 1 mm (equivalent to two passes with a step of 2 mm) and again in the X direction with a step of 2 mm. Then it was covered with a layer of Neoflon FEP film of 50 μm thickness and copper foil of 18 μm thickness. The assembly was placed in a plane-parallel press mold and heated under pressure from 1 t to 10 t to a temperature of 300 °C, cooled to room temperature, unloaded and the foil-clad dielectric was removed from the press mold. The obtained material had the following characteristics: Dk / Df = 2.20 / 0.00065 at 28 GHz, 2.20 / 0.00062 at 60 GHz, the adhesion of copper foil to the dielectric substrate was 2.95 N / mm when peeled off at an angle of 90 °, the coefficient of thermal expansion in the temperature range from 30 to 150 °C in the X and Y directions = 17.0x10' 6 TO 1 , thickness of the dielectric layer -

[0016] 125 microns.

Claims

CLAUSES OF THE INVENTION 1. A composition for the production of polymer dielectric substrates with dielectric losses of less than 0.001 at ultra-high frequencies, including generations 5G, 6G, consisting of a polymer material of copolymers of perfluorinated ethylene and propylene with a quartz filler in the form of continuous fibers and / or dispersed particles.

2. A method for producing foil-clad dielectrics without a special adhesive layer between the foil and the dielectric substrate, carried out by hot pressing together polymer films, quartz fillers and foil. 5

Citation Information

Patent Citations

  • Method for manufacture of multilayer construction and printed circuit board substrate based on multilayer construction

    RU2139792C1

  • Organic / inorganic laminates for high frequency printed circuit board applications

    US20210068249A1

  • Low signal loss bonding ply for multilayer circuit boards

    US6783841B2

  • Method of manufacturing an electronic circuit device through a direct write technique