Nanoparticle array and method for the manufacture and use thereof
The multi-channel SECCM method addresses the limitations of existing nanoparticle synthesis by enabling high-throughput and spatially controlled electrodeposition of metal alloy nanoparticles, improving their catalytic performance for electrocatalytic reactions.
Patent Information
- Application Number
- PCT/US2024/029566
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-29
- Filing Date
- 2024-05-16
- Publication Date
- 2024-12-05
AI Technical Summary
Current methods for synthesizing nanoparticles lack high-throughput and spatial control, particularly for metal alloy nanoparticles, which are crucial for electrocatalytic applications due to their sensitive composition and arrangement-dependent properties.
A multi-channel scanning electrochemical cell microscopy (SECCM) method using a dual-channel pipette to electrodeposition metal alloy nanoparticles with controlled composition and spatial arrangement on a substrate, where the bias potential and current control the electrophoretic diffusion of metal precursors to form nanoparticles with varying compositions and patterns.
Enables the high-throughput synthesis of metal alloy nanoparticles with precise control over composition and spatial arrangement, enhancing their catalytic activity and selectivity for electrocatalytic reactions, such as CO2 reduction and hydrogen evolution.
Smart Images

Figure US2024029566_05122024_PF_FP_ABST
Abstract
Description
NANOPARTICLE ARRAY AND METHOD FOR THE MANUFACTURE AND USETHEREOFCROSS REFERENCE TO RELATED APPLICATIONThis application claims priority to U.S. Provisional Patent Application No. 63 / 469,526, filed on May 29, 2023, the contents of which are hereby incorporated by reference in their entirety.BACKGROUND
[0001] Controlled placement of nanostructures (e.g., nanoparticles) onto a substrate is of interest for a variety of applications. Previous methods for achieving the controlled placement of nanostructures include self-assembly onto lithographically patterned substrates, dip-pen lithography, or optical trapping. Such methods suffer from significant limitations, for example throughput and controlling the composition of the nanostructures in addition to controlling the placement on the substrate.
[0002] It would therefore be advantageous to provide a method for producing an array of nanostructures on a substrate having controlled placement. It would be a further advantage to provide arrays with varying nanostructure composition using a single deposition method.SUMMARY
[0003] An aspect of the present disclosure is a method of fabricating a metal alloy nanoparticle array, the method comprising: contacting a multi-channel pipette with a substrate at a first point, wherein the multi-channel pipette comprises a first metal precursor solution in a first channel, and a second metal precursor solution in a second channel; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof; applying a first electrical bias or a first current between the first channel and the second channel of the multi-channel pipette; forming a metal alloy nanoparticle by electrodeposition; and repeating the method across a plurality of points on the substrate to provide the metal alloy nanoparticle array.
[0004] Another aspect is a metal alloy nanoparticle array made by the method.
[0005] Another aspect is a metal alloy nanoparticle array comprising a plurality of discrete portions of metal alloy nanoparticles on a substrate, wherein each of the plurality of discrete portions has a predetermined shape; wherein each of the plurality of discrete portions comprises a plurality of individual metal alloy nanoparticles arranged in a pattern; and whereineach of the plurality of discrete portions of metal alloy nanoparticles on the substrate comprise metal alloy nanoparticles that are different from the metal alloy nanoparticles of an adjacent portion.
[0006] Another aspect is a device comprising the metal nanoparticle array.100071 The above described and other features are exemplified by the following figures and detailed description.BRIEF DESCRIPTION OF THE DRAWINGS
[0008] The following figures represent exemplary embodiments.
[0009] FIG. 1 is a schematic illustration of on-demand deposition of a nanoparticle array according to an aspect of the disclosure.
[0010] FIG. 2 shows concentration gradients of copper (Cu) and silver (Ag) when the bias potential of -0.1, 0, and 0.1 volts (V) is applied in a finite element simulation of electrochemical deposition of bimetals in a dual barrel pipette.
[0011] FIG. 3 shows simulated flux fraction of copper (Cu) and silver (Ag) at the substrate as a function of Vbias in a finite element simulation of electrochemical deposition of bimetals in a dual barrel pipette.
[0012] FIG. 4 shows cyclic voltammograms for the deposition and stripping of Cu-Ag bimetallic particles in scanning electrochemical cell microscopy (SECCM) at Vbias of -0.6 V, -0.2 V, 0 V, 0.2 V, and 0.6 V, and the molar fraction of Cu and Ag in the particle calculated from the charge in the anodic stripping peaks in the reverse scan at different Vbias. Error bars represent the standard deviation from triplicate.
[0013] FIG. 5 shows electrodeposition of bimetallic nanoparticles under constant potential at different voltage biases between the pipettes (Vbias). The working electrode is held at -0.7 V for 0.2 s, followed by the stripping voltammogram.
[0014] FIG. 6 shows i-VwE curves observed during nanoparticle stripping after deposition when Vbias is -0.2 V, 0.1 V, and 0.2 V.
[0015] FIG. 7 shows molar fraction of Cu-Ag nanoparticles from stripping of nanoparticle deposits by reverse voltage sweep when Vbias = -0.1 to 0.2 V.
[0016] FIG. 8 shows scanning transmission electron microscopy (STEM) images and energy dispersive spectroscopy (EDS) elemental maps of Cu-Ag nanoparticles fabricated by SECCM and having continuously varying composition of 99: 1 Cu:Ag, 76:24 Cu: Ag, 48:52 Cu:Ag, and 7:93 Cu:Ag.
[0017] FIG. 9 shows molar fraction (atomic percentage) of Cu-Ag nanoparticles obtained from EDS analyses as a function of Vbias-
[0018] FIG. 10 shows cyclic voltammogram of Cu-Pt by SECCM (condition: channel 1 - 2mM Cu(C104)2+ 2 mM HC1O4, channel 2 - 2mM H2PtCl6+ 2mM HC1O4, scan rate - 0.5 V / s).
[0019] FIG. 11 shows a scanning electron microscope (SEM) image and EDS elemental maps Cu-Pt nanoparticles fabricated by SECCM when VWE = -0.8 V and Vbias = -0.4 V, showing 99: 1 Cu:Pt, 82:18 Cu:Pt, and 1:99 Cu:Pt.
[0020] FIG. 12 shows the atomic percentage (molar fraction) of Cu-Pt nanoparticles observed by EDS.
[0021] FIG. 13 shows scanning transmission electron microscopy (STEM) images and energy dispersive spectroscopy (EDS) elemental maps of Au-Pt nanoparticles.
[0022] FIG. 14 shows scanning transmission electron microscopy (STEM) images and energy dispersive spectroscopy (EDS) elemental maps of Cu-Pb nanoparticles.
[0023] FIG. 15 shows scanning transmission electron microscopy (STEM) images and energy dispersive spectroscopy (EDS) elemental maps of Co-Ni nanoparticles.
[0024] FIG. 16 shows SEM image (left) and EDS map (right) of Cu-rich or Ag-rich nanoparticles fabricated on the substrate by one dual-channel pipette (scale bar: 10 pm). Each elemental deposition was performed with varying the bias potential.
[0025] FIG. 17 shows (top) SEM image of a Cu-Ag nanoparticle array synthesized with different Vbias- The inset image depicts the location of droplets during electrochemical mapping, (middle) current heat map at -1.161 V vs standard hydrogen electrode (SHE) of the Cu-Ag particle array; and (bottom) current density of Cu-Ag nanoparticles as a function of mole fractions, corresponding to the applied bias potential ranging from -0.2 to 0.2 V. Error bars represent the standard deviation from triplicates.DETAILED DESCRIPTION
[0026] Metallic nanoparticles have unique physical and chemical properties that enable their wide usage in many fields, including electrocatalysis, optics, and biomedicine. Precision nanoparticle synthesis to control the size, shape, facet, and ligand has provided fundamental understanding of the structure-function relationship of nanoparticles as electrocatalysts for a number of reactions, including hydrogen evolution reaction, oxygen reduction reaction, and CO2reduction reaction. However, the sensitive dependence of the catalytic activity of the nanoparticles on their size, structure, spatial arrangement presents significant challenge in finding the optimal nanoparticles for specific reactions due to the exponential increase in the number of permutations compared with limited throughput of synthesis. The problem is further compounded in metal nanoparticle alloys, which can have better electrocatalytic properties thanindividual mono-metallic counterpart. Alloy particles introduce further complexity in the atomic composition. Additionally, even with the same atomic composition, the variation in atomic arrangement can lead to structures from intermetallic compounds to alloys, and heterogeneously structured nanoparticles, which can exhibit different properties. In addition, the spatial arrangement between nanoparticles is promising in designing tandem catalytic systems, which offers control of the efficiency and selectivity in electrocatalytic reactions with multiple potential products, like CO2 reduction. Conventional methods of nanoparticle synthesis have intrinsically low throughput and no spatial control of the particles, for example on an electrode. There remains a continuing need in the art for a high-throughput synthesis with continuous compositional control and sufficient spatial control of the particles.
[0027] Previous methods for high-throughput synthesis include dip-pen nanolithography (DPN) using a pre-made metal precursor ink, combinatorial sputtering, and optical ablation. However, a high degree of control over the spatial positioning of nanoparticles has been limited to multi-step methods such as lithographic techniques or manipulation of pre-synthesized nanoparticles by sharp probes. Also, the use of a ligand to stabilize the nanoparticles adds another layer of complexity to existing methods.
[0028] Electrochemistry has been found to be an effective method to challenge the intricacies involved in alloy nanoparticle synthesis. In electrodeposition, the driving force can be readily controlled in real-time by adjusting electrode potentials, while the rate of electrodeposition can be monitored by the current. This allows quantitative control of the nucleation and growth processes during nanoparticles synthesis. Furthermore, the use of ligand can be avoided, which can often block the active sites of the electrocatalysts. Additionally, directly depositing nanoparticles on the electrode surfaces offers improved attachment. However, to date, using electrodeposition to control nanoparticle synthesis has faced challenges. For example, spatial control of nanoparticles through electrodeposition can be challenging due to the distribution of the nucleation sites and the stochastic nature of nucleation. In addition, the throughput of electrodeposition to form nanoparticles is intrinsically low.
[0029] Scanning electrochemical cell microscopy (SECCM) has emerged as a promising method for electrodeposition of metallic nanoparticles with high spatial resolution and precise control over their size and shape. A glass capillary with a nanoscopic opening, referred to as a nanopipette, can be filled with metal precursor solution and brought to the surface of a substrate to make a droplet in contact with the surface. The reduction of the precursor in the nanodroplet cell results in the nucleation and growth of nanoparticles. Despite the great success in localized electrodeposition of single nanoparticles, synthesis of alloy nanoparticles with various compositions has yet to be reported.
[0030] The present inventors have advantageously developed a high through-put method for the preparation of nanoparticles (i.e. , metal alloy nanoparticles) having varying composition, size, and shape, and controlled spatial arrangement on a substrate. Specifically, the present inventors have developed a multi-channel (e.g., dual channel) SECCM method to synthesize metal alloy (e.g., bimetallic) nanoparticles with control of the elemental compositions and location of the nanoparticles on the surface of a substrate. Each barrel of the nanopipette can be filled with different metal precursors (e.g., copper (Cu) precursors, silver (Ag) precursors, and the like) to be reduced on the electrode surface. Control of the alloy composition of the nanoparticles can be achieved by fluidic control in a droplet cell. The bias potential controls electroosmosis and electrophoresis in the droplet between the pipette and the substrate, which provides varied concentration and flux of each metal precursor at the substrate surface. Furthermore, the catalytic activity of the spatially and compositionally controlled alloy nanoparticles can be screened by single-channel SECCM. By carefully controlling the composition of the metal precursor solution and the deposition potential, well-defined metal nanoparticles can be provided for numerous applications such as catalyst, electronics, and sensors, where precise control over their properties is crucial. A significant improvement is therefore provided by the present disclosure.[00311 Accordingly, an aspect of the present disclosure is a method for fabricating a metal alloy nanoparticle array. The term “metal alloy nanoparticle” as used herein refers to a nanoparticle comprising at least two metals. A “nanoparticle” as used herein refers to a nanostructure having a maximum diameter of 1000 nanometers (nm). The nanoparticle can be of any suitable shape, and is preferably spherical or semi-spherical. When the nanoparticle has an irregular shape, it will be understood that the longest dimension is 1000 nm or less.
[0032] The method described herein utilizes a multi-channel nanopipette (also referred to herein as “the pipette” for simplicity). The multi-channel nanopipette has at least two channels or barrels, each capable of containing and dispensing a solution. The multi-channel pipette has a nanoscale pipette tip though which the solutions present in the channels can be dispensed. In an aspect, the nanopipette tip can have an opening that is 100 nm to 50 micrometers (pm) in diameter. Within this range, the tip can have an opening that is 500 nm to 50 m, or 500 nm 30 pm, or 1 to 50 pm, or 10 to 50 pm, or 1 to 25 pm, or 1 to 20 pm, or 1 to 10 pm. In a specific aspect, the tip can have an opening that is 1 to 10 pm, or 1 to 5 pm. As will be understood by the skilled person, the size of the opening can be controlled by the pulling process to prepare the capillary. An exemplary pipette tip of a multi-channel pipette is shown schematically in FIG. 1. As shown in FIG. 1, each channel has an outlet at the pipette tip.
[0033] In an aspect, the multi-channel pipette comprises at least two channels. While a multi-channel pipette having two channels is shown in FIG. 1, multi-channel pipettes having more than two channels are also contemplated by the present disclosure. For example, a multichannel pipette can have two or more channels, for example two channels, or three channels, or four channels, or five channels. The number of channels can be selected based on the desired number of metals to be included in the metal alloy nanoparticle. For example, a pipette having two channels can be useful for forming a metal alloy nanoparticle including two metals (i.e., a bimetallic nanoparticle), and a pipette having three channels can be useful for forming a metal alloy nanoparticle including three metals (i.e., a trimetallic nanoparticle).
[0034] The multi-channel pipette comprises a first metal precursor solution in a first channel, and a second metal precursor solution in a second channel. It will be understood that when three channels are present, the multi-channel pipette can comprise a first metal precursor solution in a first channel, a second metal precursor solution in a second channel, and a third metal precursor solution in a third channel. Stated another way, each channel of the multichannel pipette comprises a metal precursor solution. The metal precursors present in each channel are different from one another.
[0035] Each metal precursor solution comprises a metal precursor and a solvent. The solution should have a composition such that nanoparticles of a desired composition may be electrochemically reduced to yield solids of the desired materials. For example, dissolved metals, metal ions, or various salt solutions may be used.
[0036] Suitable metal precursors can be selected based on the desired metals in the metal alloy nanoparticle product. A metal precursor for any metal that can be electrodeposited from an aqueous solution can generally be used, for example a precursor to a transition metal of Groups 3-12 of the Periodic Table. For example, the precursor can be a Pt precursor, a Ru precursor, a Au precursor, a Co precursor, a Cr precursor, a Fe precursor, a Cu precursor, a Ni precursor, a Zn precursor, a Rh precursor, a Pd precursor, a Sn precursor, a Re precursor, a Os precursor, a Ir precursor, a Cd precursor, a Ag precursor, a Mn precursor, a Se precursor, a Tc precursor, an In precursor, a Sb precursor, a Te precursor, a Hg precursor, a T1 precursor, a Pb precursor, or a Bi precursor. In an aspect, the precursor can be to a Group 10 or Group 11 metal. In a specific aspect, the first metal precursor solution and the second metal precursor solution can each independently comprise a copper precursor, a gold precursor, a silver precursor, a platinum precursor, a lead precursor, a cobalt precursor, or a nickel precursor, provided that the first and second metal precursor solutions are not the same. Exemplary precursors can include, for example, a metal perchlorate (e.g., copper (II) perchlorate, silver perchlorate, lead perchlorate,and the like), metal halide (e.g., copper (II) chloride, cobalt chloride, nickel chloride, and the like), and metal complexes (e.g., chloroplatinic acid, chloroauric acid, and the like).
[0037] In an aspect, the first metal precursor solution can comprise a copper precursor, and the second metal precursor solution can comprise a silver precursor or a platinum precursor. In an aspect, the first metal precursor solution can comprise a platinum precursor, and the second metal precursor solution can comprise a silver precursor or a gold precursor. In an aspect, the first metal precursor solution can comprise a copper precursor, and the second metal precursor solution can comprise a lead precursor. In an aspect, the first metal precursor solution can comprise a cobalt precursor, and the second metal precursor solution can comprise a nickel precursor.
[0038] The metal precursor solutions comprise a solvent. The solvent is not particularly limited provided that it is capable of dissolving or dispersing the selected metal precursor. The solvent should not react with the nanoparticles or the substrate. In an aspect, the metal precursor solutions can be aqueous solutions (i.e., the solvent can be water). For example, the metal precursor solutions can comprise the metal precursor dissolved or dispersed in water. In an aspect, the solvent can comprise an organic solvent. Exemplary organic solvents can include acetonitrile, dimethyl sulfoxide, dimethyl formamide, and the like, or a combination thereof. Combinations of the aforementioned aqueous and organic solvents are also contemplated. When a combination of an aqueous and an organic solvent are used, it can be preferable that the aqueous and organic solvents are miscible (i.e., do not provide a phase-separated solution).
[0039] In some aspects, additional reagents including but not limited to emulsifiers, polymers, organic solvents, wetting agents, complexing agents, and ligands can be excluded from the metal precursor solutions.
[0040] In an aspect, the metal precursor solutions can be acidic solutions, for example comprising aqueous solutions of sulfuric acid (H2SO4), nitric acid (HNO3), perchloric acid (HCIO4), hydrochloric acid (HC1), or acetic acid (CH3COOH). The acidic solution can offer efficient ion conductivity during electrodeposition. In a specific aspect, the solution can comprise perchloric acid. The concentration of the acid in the solution can be, for example, 0.01 millimolar (mM) to 100 mM, for example 0.5 mM to 5 mM, or 1 mM to 5 mM, or 1 to 2 mM.
[0041] The concentration of the metal precursor in the solution can be, for example 0.01 mM to 5 mM, for example 0.5 mM to 5 mM, or 1 mM to 5 mM, or 1 mM to 2 mM.
[0042] The tip of the multi-channel pipette is contacted with a surface of a substrate at a first point. It is noted that the tip may be in direct contact with the substrate, but it need not be. Rather, it will be understood that the tip must only be close enough to the substrate so that a meniscus forms, bridging the gap between the tip and the substrate, for example as shown inFIG. 1. Thus, the tip is “in contact” with the substrate when it is close enough that this meniscus forms. A droplet is therefore formed on the surface of the substrate at the first point, and said droplet forms a meniscus between the tip and the substrate. The droplet remains in contact with both the tip and the substrate, for example as shown in FIG. 1. The initial droplet (i.e., prior to applying any electrical bias) comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof.
[0043] The size of the droplet can determine the maximum size of the final nanoparticle. In an aspect, the droplet can have a volume of, for example 100 to 500 attoliters. The attoliter droplet can provide nanoparticles having diameters of 1000 nm or less, for example 500 nm or less, for example 10 to 500 nm, or 50 to 500 nm.
[0044] When the droplet is in contact with the surface of the substrate, a first electrical bias or a first current is applied between the first channel and the second channel of the multichannel pipette, for example as shown in FIG. 1. As further described in the working example below, the voltage bias can cause electrophoretic diffusion of either the first or the second metal precursor into the droplet (depending on the applied bias). For example, in an aspect, the first electrical bias or the first current can be selected to favor electrophoresis of the first metal precursor into the droplet, while the second metal precursor will electrophoretically diffuse away from the droplet (i.e., into the pipette channel, away from the substrate). Under such an electrical bias or current, the resulting metal nanoparticle will comprise a major amount of a metal derived from the first metal precursor. Conversely, the first electrical bias or first current can be selected to favor electrophoresis of the second metal precursor into the droplet, while the first metal precursor will electrophoretically diffuse away from the droplet (i.e., into the pipette channel, away from the substrate). Under such an electrical bias or current, the resulting metal nanoparticle will comprise a major amount of a metal derived from the second metal precursor. The composition of the metal alloy nanoparticle can therefore be controlled based on the voltage bias or current applied to the channels of the pipette. As further explained below and in the working examples of the present application, the electrical bias or current can be selected based on the chemical identity of the first and second metal precursors, as well as the desired composition of the nanoparticle. In an aspect, the electrical bias can be -0.75 to 0.75 V, or -0.7 to 0.7 V, or -0.6 to 0.6 V, or -0.5 to 0.5 V, or -0.4 to 0.4 V.
[0045] In an aspect, a negative electrical bias can be applied to the nanopipette, and the first metal precursor will diffuse into the droplet, while the second metal precursor will diffuse away from the droplet. The droplet will therefore comprise a majority of the first metal precursor, and the resulting nanoparticles will comprise a majority of a metal derived from the first metal precursor. In an aspect, the first metal precursor can be a copper precursor, and thesecond metal precursor can be a silver precursor. In an aspect, the first metal precursor can be a copper precursor, and the second metal precursor can be a platinum precursor. In an aspect, the first metal precursor can be a gold precursor and the second metal precursor can be a platinum precursor. In an aspect, the first metal precursor can be a copper precursor and the second metal precursor can be a lead precursor. In an aspect, the first metal precursor can be a cobalt precursor and the second metal precursor can be a nickel precursor.
[0046] In an aspect, a positive electrical bias can be applied to the nanopipette, and the second metal precursor will diffuse into the droplet, while the first metal precursor will diffuse away from the droplet. The droplet will therefore comprise a majority of the second metal precursor, and the resulting nanoparticles will comprise a majority of a metal derived from the second metal precursor. In an aspect, the first metal precursor can be a copper precursor, and the second metal precursor can be a silver precursor. In an aspect, the first metal precursor can be a copper precursor, and the second metal precursor can be a platinum precursor. In an aspect, the first metal precursor can be a gold precursor and the second metal precursor can be a platinum precursor. In an aspect, the first metal precursor can be a copper precursor and the second metal precursor can be a lead precursor. In an aspect, the first metal precursor can be a cobalt precursor and the second metal precursor can be a nickel precursor.
[0047] In an aspect, the nanoparticle provided by the method can be a core-shell nanoparticle. In an aspect, the core-shell nanoparticle can include a core formed from the first metal precursor and a shell encapsulating the core formed from the second metal precursor. In an aspect, the core-shell nanoparticle can include a core formed from the second metal precursor and a shell encapsulating the core formed from the first metal precursor. The size of the core can be determined by the size of the droplet during deposition as discussed above. The thickness of the shell encapsulating the core can similarly be controlled to provide core-shell nanoparticles having varying thicknesses of the core and / or the shell.
[0048] In an aspect, an electrical bias can be applied to provide a nanoparticle having a molar ratio of the first metal (i.e., derived from the first metal precursor) to the second metal (i.e., derived from the second metal precursor) of 40:60 to 60:40, or 45:55 to 55:45, or 50:50. In an aspect, such an electrical bias can be 0.1 to 0.3 V, or 0.15 to 0.25 V, or 0.18 to 0.22 V. In addition to voltage, the composition of the nanoparticle can alternatively be controlled by controlling the current through the barrels of the pipette.
[0049] The metal alloy nanoparticle is formed by electrodeposition, wherein the deposition is controlled by current or voltage. That is, after applying the electrical bias to the multi-channel pipette to tune the composition of the nanoparticle, the metal precursors present in the droplet can be reduced by an electrical current passing through the substrate (i.e., theelectrons provided at the substrate reduce the metal ions). To stop electrodeposition, either the nanopipette tip can be removed, the current supplied to the substrate may be shut off, or both. The proper period for electrodeposition can differ depending on the desired size of the nanoparticles. The electrochemical reduction of the metal precursors can be at a temperature of 0 to 200°C, preferably 10 to 100 °C, or 10 to 50 °C.
[0050] Advantageously, no additional reagents are required to enable reduction of the precursors and formation of the metal alloy nanoparticles. Rather it is the electric current passed through the substrate that reduces the dissolved metal precursors to provide the metal alloy nanoparticles. In an additional advantageous feature, no further processing steps are required.
[0051] Accordingly, the substrate is capable of conducting an electrical current. The substrate can therefore comprise a conductive substrate, a substrate having a conductive coating disposed thereon (e.g., ITO-coated glass), or a semiconducting substrate. In an aspect the substrate can comprise a metal (e.g., gold, silver, aluminum, copper, platinum, palladium, and the like), a metal oxide (e.g., an oxide of Al, Ti, Fe, Ag, Zn, Zr, In, Sn, Cu, and the like), a semiconducting metal (e.g., Si, CdSe, CdS, CdS coated with ZnS, and the like). Exemplary substrates can include silicon substrates, glassy carbon substrates, and highly oriented pyrolytic graphite (HOPG) substrates. The substrate can be of any size and shape. Methods of making suitable substrates are generally known. Suitable substrates can also be obtained commercially from, for example, Digital Instruments (gold), Molecular Imaging (gold), Park Scientific (gold), Electronic Materials, Inc. (semiconductor wafers), Silicon Quest, Inc. (semiconductor wafers), MEMS Technology Applications Center, Inc. (semiconductor wafers), Crystal Specialties, Inc. (semiconductor wafers), or Siltronix, Switzerland (silicon wafers).
[0052] In an aspect, the substrate has a substantially smooth surface. In an aspect, the surface of the substrate has not been patterned (e.g., lithographically).
[0053] The method can further comprise repeating the contacting the pipette with a preselected point on the substrate, forming a droplet, applying a bias, and forming the metal alloy nanoparticle by electrodeposition across a plurality of points on the surface of the substrate to provide the metal alloy nanoparticle array. An “array” as used herein is an arrangement of the nanoparticles in a pattern on the substrate.
[0054] The metal alloy nanoparticles can be arranged in a pattern to form the array, and the plurality of points for forming the nanoparticles can be predetermined. The pattern can generally be any pattern and can be simple or complex. For example, the pattern can be a line, a cross, a geometric shape (e.g., a triangle, a square, or a circle), combinatorial arrays (e.g., a square array of rows and columns of nanoparticles), an electronic circuit, or a combination of any of the foregoing. A “combinatorial array” is an array wherein each sample area or a smallgroup of replicate sample areas (usually 2-4) contain(s) a sample which is different (i.e., nanoparticles having different compositions) than that found in other sample areas of the array.
[0055] Accordingly, in an advantageous feature, the method described herein can be used to provide an array of metal alloy nanoparticles, wherein the composition of the metal nanoparticles can vary by location on the substrate. Stated another way, the present inventors have advantageously discovered that metal alloy nanoparticle composition can be tuned based on the electrical bias or the current that is applied across the channels of the multi-channel pipette during deposition of each nanoparticle. Accordingly, the method described herein can enable preparation of metal alloy nanoparticle arrays having varying composition across the surface of the substrate. In some aspects, at least a portion of the metal alloy nanoparticles of the array can be core-shell nanoparticles.
[0056] The method can further comprise moving the multi-channel pipette to a second location on the substrate and forming a droplet on a surface of the substrate. The droplet again comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof. A second electrical bias (or current) can be applied between the first channel and the second channel of the multi-channel pipette, wherein the second electrical bias (or current) is different from the first electrical bias (or current). Selection of a different electrical bias (or current) applied to the pipette can result in a different nanoparticle composition. For example, the first electrical bias (or current) can be selected to favor electrophoretic migration of the first metal precursor to the droplet in contact with the substrate, and the second electrical bias (or current) can be selected to favor electrophoretic migration of the second metal precursor to the droplet in contact with the substrate.
[0057] The metal alloy nanoparticle is formed on the surface of the substrate by electrodeposition. The method can further include repeating the method across a plurality of points on the substrate. Accordingly, a metal alloy nanoparticle array can be provided which comprises a first portion of metal alloy nanoparticles, and a second portion of metal alloy nanoparticles, wherein the first portion and the second portion are spatially separated on the substrate, and wherein the metal alloy nanoparticles of the first portion have a composition that is different from the metal alloy nanoparticles of the second portion. The first portion and the second portion can be of any shape (e.g., various geometric shapes) and can be arranged in any patterns (e.g., rows and columns of discrete sample areas).
[0058] In an aspect, the first portion of metal alloy nanoparticles comprises a plurality of metal alloy nanoparticles comprising greater than 50 mole percent of the first metal (derived from the first metal precursor), and the second portion of metal alloy nanoparticles comprises aplurality of metal alloy nanoparticles comprising greater than 50 mole percent of the second metal (derived from the second metal precursor).
[0059] Metal alloy nanoparticles having a different composition can refer to metal alloy nanoparticles comprising the same metals, but in different ratios. For example, the metal alloy nanoparticles of the first portion described above can be Cu-Ag nanoparticles that have a majority of Cu (e.g., greater than 50 mole percent Cu), and the metal alloy nanoparticles of the second portion described above can be Cu-Ag nanoparticles that have a majority of Ag (e.g., greater than 50 mole percent Ag).
[0060] A metal alloy nanoparticle array made by the method described herein represents another aspect of the present disclosure. As noted above, an advantageous feature of the presently disclosed method is the ability to provide patterned nanoarrays having varying metal compositions across the surface of the substrate. In an aspect, a metal alloy nanoparticle array can comprise a plurality of discrete portions of metal alloy nanoparticles on a substrate, wherein each of the plurality of discrete portions has a predetermined shape. Each of the plurality of discrete portions comprises a plurality of individual metal alloy nanoparticles arranged in a pattern. Furthermore, each of the plurality of discrete portions of metal alloy nanoparticles on the substrate comprise metal alloy nanoparticles that are different from the metal alloy nanoparticles of an adjacent portion.
[0061] In an aspect, the metal alloy nanoparticle array can comprise two discrete portions of metal alloy nanoparticles. The first portion of the metal alloy nanoparticles have a first metal alloy composition. The second portion of the metal alloy nanoparticles have a second metal alloy composition different from the first metal alloy composition. For example, the metal alloy nanoparticles of the first portion can be Cu-Ag nanoparticles that have a majority of Cu (e.g., greater than 50 mole percent Cu), and the metal alloy nanoparticles of the second portion can be Cu-Ag nanoparticles that have a majority of Ag (e.g., greater than 50 mole percent Ag).
[0062] In an aspect, the first portion of the metal alloy nanoparticles and the second portion of the metal alloy nanoparticles each independently comprise copper-silver nanoparticles, copper-platinum nanoparticles, platinum- silver nanoparticles, platinum gold nanoparticles, copper-lead nanoparticles, or cobalt-nickel nanoparticles. Other metal alloy nanoparticle compositions are also contemplated by the present disclosure, and the exemplary embodiments of copper-silver nanoparticles, copper-platinum nanoparticles, platinum-silver nanoparticles, platinum gold nanoparticles, copper-lead nanoparticles, or cobalt-nickel nanoparticles should not be construed as limiting.
[0063] In an aspect, a variation of the method of the present disclosure can be used to deposit metallic alloy lines on a surface (i.e., as opposed to discrete nanoparticles in an array).For example, such a method can comprise contacting the tip of the multi-channel pipette with a surface of a substrate at a first point. The size of the initial droplet can determine the maximum height of the metallic alloy line. For example, as described above, the droplets provided by the nanopipette can provide lines having an average height of 1000 nm or less, for example 500 nm or less, for example 10 to 500 nm, or 50 to 500 nm.
[0064] Once the droplet is in contact with the substrate, a first electrical bias or a first current is applied between the first channel and the second channel of the multi-channel pipette, causing electrophoretic diffusion of either the first or the second metal precursor into the droplet (depending on the applied bias or current). The composition of the metallic alloy line can therefore be controlled based on the voltage bias or current applied to the channels of the pipette. The method further comprises reducing the metal precursors present in the droplet by an electrical current passing through the substrate (i.e., the electrons provided at the substrate reduce the metal ions). The tip of the pipette can be moved along the surface of the substrate, wherein the tip of the pipette maintains contact with the surface, and the solution deposited by the pipette (e.g., the first metal precursor solution, the second metal precursor solution, or a combination thereof) maintains contact with the initial droplet to provide the line.
[0065] All variations for the metal precursors, solvents, the substrate, and electrodeposition conditions described above can also be applied to the method of forming the lines.
[0066] The lines may generally form any shape or pattern on the surface of a substrate, and may be continuous or have noncontinuous segments. In an aspect, a metallic alloy line can comprise a first portion having a first metal alloy composition and a second portion having a second metal alloy composition. In an aspect the metallic alloy line can comprise a compositional gradient transitioning from the first portion to the second portion. As described herein, the metal composition of the line can be adjusted depending on the bias or current applied across the pipette during deposition. For example, a first electrical bias (or current) can be selected to favor electrophoretic migration of the first metal precursor to the droplet in contact with the substrate, and a second electrical bias (or current) can be selected to favor electrophoretic migration of the second metal precursor to the droplet in contact with the substrate. Though a first and second bias or current are specifically mentioned, it is noted that the present disclosure is not limited to the use of two biases or currents. Rather, a plurality of biases or currents can be selected and utilized in the preparation of the lines and arrays described herein, and can be selected by the skilled person guided by the present disclosure, depending on the desired composition(s) of the final nanoparticles, arrays thereof, or lines and shapes.
[0067] The metal alloy nanoparticle arrays described herein can be useful for various applications. Arrays and methods of using them are known in the art. For instance, such arrays can be used for biological and chemical screenings to identify and / or quantitate a biological or chemical material. Arrays of nanoparticles can be used for a variety of purposes including, for example, analysis of catalytic activity and studying particle-particle and particle-substrate interactions.
[0068] The nanoparticles arrays can also find use in various devices, particularly where well-defined patterns of single nanoparticles are needed. Accordingly, a device comprising the nanoparticle array represents another aspect of the present disclosure. Exemplary devices can include but are not limited to microfluidic devices, sensors, fuel cells, solid-state batteries, or energy storage devices. In an aspect, the nanoparticle array can be used in an energy storage application, for example a liquid fuel cell (e.g., formic acid, methanol, ethanol, or the like). In an aspect, the nanoparticle array can be used in an environmental remediation application, for example removing contaminants from environmental media. In an aspect, the nanoparticle array can be used in biological applications (e.g., antimicrobial applications, bio-imaging, sensors, or drug delivery).
[0069] This disclosure is further illustrated by the following examples, which are nonlimiting.EXAMPLES
[0070] SECCM is used for depositing metal alloy nanoparticles because of its ability to confine the deposition locally, allowing deposition with high spatial resolution and high throughput. As illustrated in FIG. 1, a dual barrel pipette filled with solutions containing metal precursors, e.g., Ag+or Cu2+, is used as the probe. Once the droplet / nanopipette is moved to the surface and forms a meniscus, the droplet cell defines the area where the electrodeposition can occur. After deposition at each location, the nanopipette can be controlled to move to a new location for a new deposition. The process can be repeated at a few hundred to a few thousand locations, allowing for synthesizing an extensive library of nanoparticles for electrocatalytic screening. Alloy particles can be synthesized when multiple precursors are used in the solution. It is noted that the examples provided herein focus on bimetallic particles, however the method can be extended to multi-element particles, including high-entropy alloys.
[0071] Controlling composition in electrodeposition is achieved by fluidic control in the dual-barrel pipette SECCM. Cu-Ag bimetallic particles were used as an example. Each of the barrels of the pipette was filled with different solutions. For example, the left barrel (shown in the inset of FIG. 1) was filled with 2 mM Cu(C104)2 in 2 mM HCIO4, while the right barrel wasfilled with 2 mM AgClCU in 2 mM HCIO4. A quasi-reference counter electrode (QRCE) was inserted in each barrel, and the one inserted in the Cu2+-containing barrel was connected to the ground. The potential bias between the two QRCEs (Vbias) controls the ratio of Cu2+and Ag+in the droplet. When no bias is applied, Cu2+and Ag+are expected to mix in the solution by diffusion. When Vbias < 0 is applied (i.e., the Ag+barrel is more negative), the cation is expected to move from the left to the right barrel by migration. For the example in FIG. 1 , Cu2+will move into the right barrel through the droplet, while Ag+is expected to move further into the right barrel. The net result is an enrichment of Cu and depletion of Ag in the droplet. Accordingly, electrodeposition under this condition was expected to result in particles enriched with Cu. Similarly, when Vbias > 0 is applied, the droplet is expected to be enriched with Ag, creating a condition to deposit Ag-enriched nanoparticles. In addition, the enrichment of one element versus the other is expected to be sensitively influenced by Vbias, allowing continuous nanoparticle composition variation. It is noted that electroosmotic flow can also affect the flux of each ion, but its contribution is expected to be small in 2 mM HCIO4 because it is close to the lower end of the range of pH for silica.
[0072] To validate the concept of the control of the composition of the electrodeposited nanoparticles, a finite element simulation was used to simulate the concentration profile and the ionic flux in a dual-barrel pipette. A 3D model was constructed in COMSOL Multiphysics, which solves the Nernst-Plank equation with bulk neutrality considering electroosmotic flow. As shown in FIG. 2, at -0.1 V, an enrichment of Cu and depletion of Ag in the droplet and right barrel was observed. Similarly, enrichment of Ag and depletion of Cu in the droplet was observed at +0. 1 V. Another simulation was performed under the same condition, except that the concentration at the electrode surface was set to 0 to simulate the diffusion-limited depositions of metal ions. The resulting flux of Ag and Cu as a function of Vbias is shown in FIG. 3. Enrichment of Cu and Ag was observed at negative and positive bias, respectively.
[0073] The Cu-Ag system was also explored experimentally. Cyclic voltammograms showing the cathodic deposition and anodic stripping of the two metals at different bias are shown in FIG. 4. At Vbias=-0.6 V (FIG. 4, top left), the working electrode potential was first scanned negatively, starting from 0.5 V (versus Pt QRCE). The current was observed to increase as the potential becomes more negative than -0.5 V, corresponding to the electrochemical reduction of Cu2+precursors to metallic Cu. In the reverse scan, a single stripping peak was observed at approximately -0.3 V, which is assigned to the anodic stripping of deposited Cu in the previous forward scan. At Vbias = -0.2 V (FIG. 4, top middle), similar voltammetric behavior was observed, except that the anodic stripping peak was smaller than Vbias=-0.6 V, and the deposition current at the negative going scan was also smaller. At Vbias =0 V (FIG. 4, top right),the anodic stripping peak was further decreased. In addition, the base of the peak became wider, potentially due to the emergence of another stripping peak. As Vbias was increased to 0.2 V (FIG. 4, bottom left), two anodic stripping peaks were observed, one centered at approximately -0.4 V, with the other centered at approximately 0 V. The peak with more negative potential was assigned to the anodic stripping of Cu, while the peak at 0 V was assigned to the anodic stripping of Ag. The difference is similar to the difference of E0 for Ag / Ag+(0.799 V) and Cu / Cu2+(0.34x V). As the bias was further increased to 0.6 V (FIG. 4, bottom middle), the peak corresponding to Cu was almost invisible, while the peak for Ag increases significantly. The fraction of deposited Cu vs Ag can be readily calculated by integrating the charge associated with each peak, which is subsequently converted to moles using Faraday’s law of electrolysis. The measured mole fraction of Ag and Cu based on the anodic stripping peaks at different Vbias is shown in FIG. 4 (bottom right). At negative bias, deposition was observed to be dominated by Cu. As Vbias, increased, the fraction of deposited Cu decreases while that of Ag increased. This trend is in agreement with the finite element simulation. It is noted that the point where the mole ratio reaches 1:1 occurs at Vbias close to 0.2 V, not precisely at 0 V. Without wishing to be bound by theory, this is believed to be due to the difference in the mobility of the ions and the asymmetry of the pipette.[00741 Deposition conditions under constant potential were also explored. A working electrode potential of -0.7 V was applied for 0.2 seconds, followed by stripping voltammetry at 1 V / s, and the waveform is illustrated in FIG. 5. This procedure can quantify the amount of Cu and Ag in the deposit. FIG. 6 shows the stripping voltammogram of the deposition under the same constant working electrode potential at different Vbias. At Vbias = -0.2 V (FIG. 6, left), only one peak was observed, due to the stripping of Cu. At intermediate bias (Vbias = 0.1 V (FIG. 6, middle)), two peaks were observed, similar to the voltammetric results observed in FIG. 4. The presence of two peaks suggests the deposition of a bimetallic particle. At positive bias, i.e., 0.2 V (FIG. 6, right), only one stripping peak was observed, corresponding to Ag. The mole fraction of deposited Cu and Ag as a function of Vbias is summarized in FIG. 7. This trend in the constant voltage experiment is similar to that observed in the CV experiment in FIG. 3.
[0075] The stripping voltammograms in FIG. 4 and 6 demonstrated that the composition of the deposit could be changed by changing the Vbias- To verify the structure and composition of the deposited particles, scanning transmission electron microscopy (STEM) and energy- dispersive X-ray spectroscopy (EDX) images were taken for the nanoparticles deposited at the same working electrode potential but with different Vbias, as shown in FIG. 8. As shown in FIG. 7, the deposited nanoparticle at -0.1 V bias indeed shows an enrichment in Cu (~ 99% mole fraction based on EDX). The EDX images show that Ag is uniformly mixed with Cu, suggestingthe particle is a Cu-Ag alloy. The mole fraction of Cu decreased further as Vbias increased, reaching 76% at 0 V (FIG. 7), and 48 % at 0.05 V (FIG. 7). Similarly, the EDX map shows that Cu and Ag are uniformly mixed in the particle. At Vt>ias=0.2 V, the mole fraction of Cu in the particle decreased to 7%, while the mole fraction of Ag reached 93%. Overall, the particles are approximately 90 nanometers in radius, which does not depend sensitively on Vbias- The morphology seems to be affected by Vbias, or the composition of the element. At lower Vbias and lower Ag mole fraction, the particle comprises aggregates of small secondary particles (e.g., less than < 10 nm). These secondary particles seem more rounded when Ag is enriched at Vbias =0.2 V. However, the spatial distribution of each element in the particles is uniform regardless of the deposition conditions and the final particle morphology. The general trend of increasing Ag and decreasing Cu in the nanoparticle as the Vbias increases as determined by EDX is summarized in FIG. 9.
[0076] The generality of the method to control the composition was further demonstrated by electrodeposition of copper-platinum (Cu-Pt) particles using a single nanopipette with various compositions. Cu-Pt nanoparticles have shown to be good catalysts for methanol oxidation reactions. To this end, the right barrel of the dual-barrel pipette was filled 2 mM H2PtCle in 2 mM HCIO4, while the left barrel was the same Cu solution used in the previous example (i.e., 2 mM). FIG. 10 shows an SECCM voltammogram for the deposition at Vbias = 0 V. In the forward scan (negative going), multiple voltametric waves for electrochemical reduction are observed when VWE is lower than -0.5 V, corresponding to the reduction of Pt and Cu. FIG. 11 shows the SEM images of the deposited particles and the corresponding EDS maps, which were used to estimate the mole fraction of Cu and Pt.
[0077] Similar to the results for Cu-Ag particles, at low Vbias, e.g., Vbias=-0.4 V, the particle is enriched with Cu. Overall, the mole fraction of Pt and Cu decreases and increases respectively as Vbias increases, as shown in the EDS maps of FIG. 11. The mole fraction of Cu and Pt in the particles measured from EDS as a function of Vbias is summarized in FIG. 12.
[0078] The versatility of the method in depositing bimetallic nanoparticles is further showcased through different elemental combinations by changing the metal precursor solutions. As shown in FIGs. 13-15, Au-Pt, Cu-Pb, and Co-Ni were deposited, and the elemental maps show a homogeneous mixing of each element in the nanoparticle. In addition, the elemental composition in the particles can be tuned by Vbias under the same principle of fluidic control as that demonstrated for Cu-Ag and Cu-Pt.
[0079] To further demonstrate the ability to control the spatial distribution of the particles and the elemental composition in each particle, nanoparticles were deposited into an array created in the image of a longhorn. As can be seen in the SEM image shown in FIG. 16,the nanoparticles are faithfully deposited, and the 150 pixels form an image of a longhorn. Each pixel contains nanoparticles of approximately 100 nanometers in radius. The EDS mapping also demonstrates that the composition can be controlled. The horns of the longhorn are purposely deposited for particles enriched with Ag using the same nanopipette. The ability to deposit multiple elements using the same pipette allows precision fabrication of nanoparticle architecture with high throughput which is useful in additive fabrication and fabrication of architectures for cascade catalysis.
[0080] Finally, the alloy particle arrays synthesized in accordance with the present disclosure were demonstrated for use in direct screening of catalytic activity. Cu-Ag was chosen to screen for their electrocatalytic activity in the hydrogen evolution reaction (HER) because it is of high interest for electrochemical CO2 reduction where the HER is the most important competing reaction. Five different compositions of Cu-Ag nanoparticle alloys were synthesized via different bias potentials ranging from -0.2 to 0.2 V, as depicted in FIG. 17. The fraction of Cu in the Cu-Ag nanoparticles decreases from left to right, while the particles in the same column were deposited under the same conditions and shared similar compositions. An approximately 3 pm diameter single barrel pipette containing 50 mM HCIO4 was used as an SECCM probe to voltammetrically screen the activity of the HER. A hopping voltammetric scan mode was used with a 2 pm stepping distance. The local voltammograms are visualized by plotting the current at -1.161 V vs the standard hydrogen electrode (SHE) as a heat map, as shown in FIG. 17 (middle). Each pixel in the map corresponds to a single local voltametric measurement, and the local current was higher at the nanoparticles compared to that on the GC substrate. To validate the composition-activity correlation of Cu-Ag nanoparticles, the composition was determined by EDS, while the current was normalized to the current density using the surface area of the particles determined by atomic force microscopy. As shown in FIG. 17 (bottom), the HER current density on the Cu-Ag nanoparticles first increases and then decreases as the mole fraction of Cu decreases, and the maximum activity is reached with nanoparticles containing 80% Cu and 20% Ag. Furthermore, Cu-rich nanoparticles exhibited HER activity higher than that of Ag-rich particles.
[0081] Accordingly, the present inventors have developed a dual-channel nanopipette method that enables precise synthesis of bimetallic nanoparticle libraries of continuous variation in composition. Nanofluidic control by the voltage bias in the dual-channel nanopipette allows precise control of the electrodeposition rate of each element, creating bimetallic nanoparticles with precise composition. The control of composition was demonstrated by various bimetallic nanoparticles, including Cu-Ag, Cu-Pt, Au-Pt, Cu-Pb, and Co-Ni. On-demand nanoparticle alloy synthesis is further demonstrated by surface patterning from nanoparticles, where thecomposition can be controlled at the single-pixel level. The synthesized bimetallic nanoparticle arrays with varying compositions were further shown to be suitable for screening the electrocatalytic activity via SECCM. The ability to synthesize libraries of nanoparticle arrays with gradient compositions is important for the accelerated discovery of materials in electrocatalysis and beyond. While the method was demonstrated using dual-barrel pipettes for the electrodeposition of bimetallic nanoparticles, the same concept of in situ composition control can be further extended to include multiple elements by increasing the number of barrels, potentially enabling the high-throughput synthesis of a library of high-entropy alloys with different compositions. The ability of sub-micrometer and nanoscale patterning can further benefit the development of nanoscale additive manufacturing, as well as creating architectures for tandem catalysis.
[0082] A significant improvement is therefore provided by the present disclosure.
[0083] This disclosure further encompasses the following aspects, which are nonlimiting.
[0084] Aspect 1: A method of fabricating a metal alloy nanoparticle array, the method comprising: contacting a multi-channel pipette with a substrate at a first point, wherein the multi-channel pipette comprises a first metal precursor solution in a first channel, and a second metal precursor solution in a second channel; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof; applying a first electrical bias or a first current between the first channel and the second channel of the multi-channel pipette; forming a metal alloy nanoparticle by electrodeposition; and repeating the method across a plurality of points on the substrate to provide the metal alloy nanoparticle array.
[0085] Aspect 2: The method of aspect 1, wherein the multi-channel pipette comprises two channels.
[0086] Aspect 3: The method of aspect 1 or 2, wherein the metal alloy nanoparticle is a bimetallic nanoparticle.
[0087] Aspect 4: The method of any of aspects 1 to 3, wherein the metal alloy nanoparticle is a bimetallic nanoparticle.
[0088] Aspect 5: The method of any of aspects 1 to 4, wherein the first electrical bias or the first current is selected to favor electrophoresis of the first metal precursor to the droplet in contact with the substrate.
[0089] Aspect 6: The method of any of aspects 1 to 5, wherein the first electrical bias or the first current is selected to favor electrophoresis of the second metal precursor to the droplet in contact with the substrate.
[0090] Aspect 7: The method of any of aspects 1 to 6, wherein the substrate is a conductive substrate.
[0091] Aspect 8: The method of any of aspects 1 to 7, wherein forming the metal nanoparticle comprises reducing the first metal precursor, the second metal precursor, or both in the droplet to form the metal alloy nanoparticle.
[0092] Aspect 9: The method of any of aspects 1 to 8, further comprising moving the multi-channel pipette to a second location on the substrate; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof; applying a second electrical bias or a second current between the first channel and the second channel of the multi-channel pipette, wherein the second electrical bias or the second current is different from the first electrical bias; forming a metal alloy nanoparticle by electrodeposition; and repeating the method across a plurality of points on the substrate in the second location to provide the metal alloy nanoparticle array having a first portion of metal alloy nanoparticles, and a second portion of metal alloy nanoparticles, wherein the first portion and the second portion are spatially separated on the substrate, and wherein the metal alloy nanoparticles of the first portion have a composition that is different from the metal alloy nanoparticles of the second portion.
[0093] Aspect 10: The method of aspect 9, wherein the first electrical bias or the first current is selected to favor electrophoresis of the first metal precursor to the droplet in contact with the substrate; and the second electrical bias or the second current is selected to favor electrophoresis of the second metal precursor to the droplet in contact with the substrate.
[0094] Aspect 11: The method of aspect 9 or 10, wherein the first portion of metal alloy nanoparticles comprises a plurality of metal alloy nanoparticles comprising greater than 50 weight percent of the first metal; and the second portion of metal alloy nanoparticles comprises a plurality of metal alloy nanoparticles comprising greater than 50 weight percent of the second metal.
[0095] Aspect 12: The method of any of aspects 1 to 11, wherein the first metal precursor solution and the second metal precursor solution each independently comprises copper, gold, silver, platinum, lead, cobalt, or nickel, provided that the first and second metal precursor solutions are not the same.
[0096] Aspect 13: The method of any of aspects 1 to 12, wherein the first metal precursor solution comprises a copper precursor.
[0097] Aspect 14: The method of aspect 13, wherein the second metal precursor solution comprises a silver precursor or a platinum precursor.
[0098] Aspect 15: The method of any of aspects 1 to 12, wherein the first metal precursor solution comprises a platinum precursor.
[0099] Aspect 16: The method of aspect 15, wherein the second metal precursor solution comprises a silver precursor or a gold precursor.101001 Aspect 17: The method of any of aspects 1 to 12, wherein the first metal precursor solution comprises a copper precursor.
[0101] Aspect 18: The method of aspect 17, wherein the second metal precursor solution comprises a lead precursor.
[0102] Aspect 19: The method of any of aspects 1 to 12, wherein the first metal precursor solution comprises a cobalt precursor.
[0103] Aspect 20: The method of aspect 19, wherein the second metal precursor solution comprises a nickel precursor.
[0104] Aspect 21: A metal alloy nanoparticle array made by the method of any of aspects 1 to 20.
[0105] Aspect 22: A metal alloy nanoparticle array comprising a plurality of discrete portions of metal alloy nanoparticles on a substrate, wherein each of the plurality of discrete portions has a predetermined shape; wherein each of the plurality of discrete portions comprises a plurality of individual metal alloy nanoparticles arranged in a pattern; and wherein each of the plurality of discrete portions of metal alloy nanoparticles on the substrate comprise metal alloy nanoparticles that are different from the metal alloy nanoparticles of an adjacent portion.
[0106] Aspect 23: The metal alloy nanoparticle array of aspect 22, comprising two discrete portions of metal alloy nanoparticles, wherein a first portion of the metal alloy nanoparticles have a first metal alloy composition; and a second portion of the metal alloy nanoparticles have a second metal alloy composition different from the first metal alloy composition.
[0107] Aspect 24: The metal alloy nanoparticle array of aspect 22 or 23, wherein the substrate is a conductive substrate.
[0108] Aspect 25: The metal alloy nanoparticle array of aspect 23 or 24, wherein the first portion of the metal alloy nanoparticles and the second portion of the metal alloy nanoparticles each independently comprise copper-silver nanoparticles, copper-platinum nanoparticles, platinum-silver nanoparticles, platinum-gold nanoparticles, copper-lead nanoparticles, or cobalt-nickel nanoparticles, provided that the metal alloy nanoparticles of the first portion and the metal alloy nanoparticles of the second portion of the metal alloy nanoparticles are not the same.
[0109] Aspect 26: A method of fabricating a metal alloy line, the method comprising: contacting a multi-channel pipette with a substrate at a first point, wherein the multi-channel pipette comprises a first metal precursor solution in a first channel, and a second metal precursor solution in a second channel; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof; applying a first electrical bias or a first current between the first channel and the second channel of the multi-channel pipette; forming a metal alloy by electrodeposition; and moving the multi-channel pipette along the surface of the substrate to provide the metal alloy line,
[0110] Aspect 27: The method of aspect 26, wherein the multi-channel pipette comprises two channels.
[0111] Aspect 28: The method of aspect 26 or 27, wherein the metal alloy line is a bimetallic line.
[0112] Aspect 29: The method of any of aspects 26 to 28, wherein the first electrical bias or the first current is selected to favor electrophoresis of the first metal precursor to the droplet in contact with the substrate.
[0113] Aspect 30: The method of any of aspects 26 to 29, wherein the first electrical bias or the first current is selected to favor electrophoresis of the second metal precursor to the droplet in contact with the substrate.
[0114] Aspect 31: The method of any of aspects 26 to 30, wherein the substrate is a conductive substrate.
[0115] Aspect 32: The method of any of aspects 26 to 31, wherein forming the metal alloy comprises reducing the first metal precursor, the second metal precursor, or both in the droplet to form the metal alloy.
[0116] Aspect 33: The method of any of aspects 26 to 32, wherein moving the multichannel pipette along the surface of the substrate comprises maintaining contact of the multichannel pipette with the substrate, wherein the first metal precursor solution, the second metal precursor solution, or both are deposited continuously, maintaining contact with the initial droplet to form the line,
[0117] Aspect 34: A metal alloy line on a surface of a substrate made by the method of any of aspects 26 to 33.
[0118] Aspect 35: The metal alloy line of aspect 34, wherein the metal alloy line is continuous.
[0119] Aspect 36: The metal alloy line of aspect 34 to 35, wherein the metal alloy line has a first portion having a first metal alloy composition and a second portion having a second metal alloy composition.
[0120] Aspect 37: The metal alloy line of any of aspects 34 to 36, wherein the line has a gradient composition.
[0121] Aspect 38: A device comprising the metal nanoparticle array of any of aspects 21 to 25 or the metal nanoparticle array made by the method of any of aspects 1 to 20 or the metal alloy line of any of aspects 26 to 33, or the metal alloy line made by the method of any of aspects 34 to 37.
[0122] Aspect 39: The device of aspect 38, wherein the device is a microfluidic device, a sensor, a fuel cell, a solid-state battery, or an energy storage device.
[0123] The compositions, methods, and articles can alternatively comprise, consist of, or consist essentially of, any appropriate materials, steps, or components herein disclosed. The compositions, methods, and articles can additionally, or alternatively, be formulated so as to be devoid, or substantially free, of any materials (or species), steps, or components, that are otherwise not necessary to the achievement of the function or objectives of the compositions, methods, and articles.
[0124] All ranges disclosed herein are inclusive of the endpoints, and the endpoints are independently combinable with each other. “Combinations” is inclusive of blends, mixtures, alloys, reaction products, and the like. The terms “first,” “second,” and the like, do not denote any order, quantity, or importance, but rather are used to distinguish one element from another. The terms “a” and “an” and “the” do not denote a limitation of quantity, and are to be construed to cover both the singular and the plural, unless otherwise indicated herein or clearly contradicted by context. “Or” means “and / or” unless clearly stated otherwise. Reference throughout the specification to “an aspect” means that a particular element described in connection with the aspect is included in at least one aspect described herein, and may or may not be present in other aspects. The term “combination thereof’ as used herein includes one or more of the listed elements, and is open, allowing the presence of one or more like elements not named. In addition, it is to be understood that the described elements may be combined in any suitable manner in the various aspects.
[0125] Unless specified to the contrary herein, all test standards are the most recent standard in effect as of the filing date of this application, or, if priority is claimed, the filing date of the earliest priority application in which the test standard appears.
[0126] Unless defined otherwise, technical and scientific terms used herein have the same meaning as is commonly understood by one of skill in the art to which this applicationbelongs. All cited patents, patent applications, and other references are incorporated herein by reference in their entirety. However, if a term in the present application contradicts or conflicts with a term in the incorporated reference, the term from the present application takes precedence over the conflicting term from the incorporated reference.101271 Compounds are described using standard nomenclature. For example, any position not substituted by any indicated group is understood to have its valency filled by a bond as indicated, or a hydrogen atom. A dashthat is not between two letters or symbols is used to indicate a point of attachment for a substituent. For example, -CHO is attached through carbon of the carbonyl group.
[0128] While particular embodiments have been described, alternatives, modifications, variations, improvements, and substantial equivalents that are or may be presently unforeseen may arise to applicants or others skilled in the art. Accordingly, the appended claims as filed and as they may be amended are intended to embrace all such alternatives, modifications variations, improvements, and substantial equivalents.
Claims
CLAIMS1. A method of fabricating a metal alloy nanoparticle array, the method comprising: contacting a multi-channel pipette with a substrate at a first point, wherein the multichannel pipette comprises a first metal precursor solution in a first channel, and a second metal precursor solution in a second channel; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof; applying a first electrical bias or a first current between the first channel and the second channel of the multi-channel pipette; forming a metal alloy nanoparticle by electrodeposition; and repeating the method across a plurality of points on the substrate to provide the metal alloy nanoparticle array.
2. The method of claim 1, wherein the multi-channel pipette comprises two channels.
3. The method of claim 1, wherein the metal alloy nanoparticle is a bimetallic nanoparticle.
4. The method of claim 1, wherein the metal alloy nanoparticle is a core-shell nanoparticle.
5. The method of claim 1, wherein the first electrical bias or first current is selected to favor electrophoresis of the first metal precursor to the droplet in contact with the substrate.
6. The method of claim 1, wherein the first electrical bias or first current is selected to favor electrophoresis of the second metal precursor to the droplet in contact with the substrate.
7. The method of claim 1, wherein the substrate is a conductive substrate.
8. The method of claim 1, wherein forming the metal nanoparticle comprises reducing the first metal precursor, the second metal precursor, or both in the droplet to form the metal alloy nanoparticle.
9. The method of claim 1, further comprising moving the multi-channel pipette to a second location on the substrate; forming a droplet on a surface of the substrate, wherein the droplet comprises the first metal precursor solution, the second metal precursor solution, or a combination thereof;applying a second electrical bias or second current between the first channel and the second channel of the multi-channel pipette, wherein the second electrical bias or second current is different from the first electrical bias; forming a metal alloy nanoparticle by electrodeposition; and repeating the method across a plurality of points on the substrate in the second location to provide the metal alloy nanoparticle array having a first portion of metal alloy nanoparticles, and a second portion of metal alloy nanoparticles, wherein the first portion and the second portion are spatially separated on the substrate, and wherein the metal alloy nanoparticles of the first portion have a composition that is different from the metal alloy nanoparticles of the second portion.
10. The method of claim 9, wherein the first electrical bias or first current is selected to favor electrophoresis of the first metal precursor to the droplet in contact with the substrate; and the second electrical bias or second current is selected to favor electrophoresis of the second metal precursor to the droplet in contact with the substrate.
11. The method of claim 9, wherein the first portion of metal alloy nanoparticles comprises a plurality of metal alloy nanoparticles comprising greater than 50 weight percent of the first metal; and the second portion of metal alloy nanoparticles comprises a plurality of metal alloy nanoparticles comprising greater than 50 weight percent of the second metal.
12. The method of claim 1, wherein the first metal precursor solution and the second metal precursor solution each independently comprises copper, gold, silver, platinum, lead, cobalt, or nickel, provided that the first and second metal precursor solutions are not the same.
13. The method of claim 1, wherein the first metal precursor solution comprises a copper precursor and the second metal precursor solution comprises a silver precursor or a platinum precursor; or the first metal precursor solution comprises a platinum precursor and the second metal precursor solution comprises a silver precursor or a gold precursor; orthe first metal precursor solution comprises a copper precursor and the second metal precursor solution comprises a lead precursor; or the first metal precursor solution comprises a cobalt precursor and the second metal precursor solution comprises a nickel precursor.
14. A metal alloy nanoparticle array made by the method of claim 1.
15. A metal alloy nanoparticle array comprising a plurality of discrete portions of metal alloy nanoparticles on a substrate, wherein each of the plurality7of discrete portions has a predetermined shape; wherein each of the plurality of discrete portions comprises a plurality of individual metal alloy nanoparticles arranged in a pattern; and wherein each of the plurality of discrete portions of metal alloy nanoparticles on the substrate comprise metal alloy nanoparticles that are different from the metal alloy nanoparticles of an adjacent portion.
16. The metal alloy nanoparticle array of claim 15, comprising two discrete portions of metal alloy nanoparticles, wherein a first portion of the metal alloy nanoparticles have a first metal alloy composition; and a second portion of the metal alloy nanoparticles have a second metal alloy composition different from the first metal alloy composition.
17. The metal alloy nanoparticle array of claim 15, wherein the substrate is a conductive substrate.
18. The metal alloy nanoparticle array of claim 16, wherein the first portion of the metal alloy nanoparticles and the second portion of the metal alloy nanoparticles each independently comprise copper-silver nanoparticles, copper-platinum nanoparticles, platinum-silver nanoparticles, platinum-gold nanoparticles, copper-lead nanoparticles, or cobalt-nickel nanoparticles, provided that the metal alloy nanoparticles of the first portion and the metal alloy nanoparticles of the second portion of the metal alloy nanoparticles are not the same.
19. A device comprising the metal nanoparticle array of claim 15.
20. The device of claim 19, wherein the device is a microfluidic device, a sensor, a fuel cell, a solid-state battery, or an energy storage device.