Photovoltaics effectively leveraging triplet excitons
By integrating a singlet fission layer and organic semiconductor layers with a silicon semiconductor, the architecture effectively transfers triplet excitons, overcoming the Shockley-Queisser limit and enhancing the efficiency of silicon photovoltaic cells.
Patent Information
- Application Number
- PCT/US2024/054697
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-11-06
- Filing Date
- 2024-11-06
- Publication Date
- 2025-05-15
AI Technical Summary
Crystalline silicon (c-Si) solar cells, the current industry standard for photovoltaics, are approaching the Shockley-Queisser limit, necessitating new developments to enhance efficiency beyond this theoretical limit.
The implementation of a device architecture that includes a singlet fission layer, an organic semiconductor layer, a passivation layer, and a base semiconductor, which facilitates the generation and transfer of triplet excitons to a silicon semiconductor, thereby increasing photocurrent and efficiency.
This approach enables the transfer of triplet excitons to silicon photovoltaic materials, leading to enhanced photoconversion efficiency and the potential for exceeding the conventional single-junction limit in solar cell performance.
Smart Images

Figure US2024054697_15052025_PF_FP_ABST
Abstract
Description
[0001]PHOTOVOLTAICS EFFECTIVELY LEVERAGING TRIPLET EXCITONS RELATED APPLICATIONS This application claims priority under 35 U.S.C. § 119(e) to U.S. Provisional Patent Application No.63 / 596,585, filed November 6, 2023, and entitled “SILICON SOLAR CELL DESIGN FOR TRIPLET EXCITON SENSITIZATION” which is incorporated herein by reference in its entirety for all purposes. STATEMENT REGARDING FEDERALLY SPONSORED RESEARCH OR DEVELOPMENT This invention was made with government support under DE-FG02-07ER46474 awarded by the U.S. Department of Energy. The government has certain rights in the invention. TECHNICAL FIELD Devices and / or methods for generating and transferring triplet excitons to a semiconductor are generally described BACKGROUND The efficiencies of crystalline silicon (c-Si) solar cells, the current industry standard for photovoltaics, are approaching the Shockley-Queisser limit. New developments are urgently needed. SUMMARY This Summary introduces a selection of concepts in simplified form that are described further below in the Detailed Description. This Summary neither identifies key or essential features, nor limits the scope, of the claimed subject matter. In one set of embodiments, a device includes a singlet fission layer; an organic semiconductor layer; a passivation layer; and a base semiconductor. In some embodiments, the organic semiconductor layer is between the singlet fission layer and the passivation layer. In certain embodiments, the passivation layer is between the organic semiconductor layer and the base semiconductor. In another set of embodiments, a device includes an outer singlet fission layer; an electron donating layer or an electron accepting layer; a passivation layer; an n-type emitter layer or a p-type emitter layer; and a p-type base layer or an n-type base layer. In some embodiments, the electron donating layer or the electron accepting layer is between the outer singlet fission layer and the passivation layer. In certain embodiments, the passivation layer is between the electron donating layer or the electron accepting layer and the n-type emitter layer or the p-type emitter layer. In yet another set of embodiments, a method is included. The method may include exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons. The method may include transferring, to a base semiconductor, either an electron or a hole, without simultaneously transferring the other to the silicon semiconductor thereby creating current in the base semiconductor. In accordance with some embodiments, a method includes exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons. In some embodiments, the method includes transferring, to a base hotovoltaic material, either an electron or a hole, without simultaneously transferring the other to the base photovoltaic material thereby increasing the photoconversion efficiency of the base photovoltaic material. In accordance with certain embodiments, a method includes exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons. In certain embodiments, the method includes transferring at least some triplet excitons to a semiconductor. In some embodiments, the method includes transferring an electron or holes to a base semiconductor thereby creating current in the semiconductor from the formation of triplet excitons. The following Detailed Description references the accompanying drawings which form a part of this application, and which show, by way of illustration, specific example implementations. Other implementations may be made without departing from the scope of the disclosure. BRIEF DESCRIPTION OF THE DRAWINGS Non-limiting embodiments of the present disclosure will be described by way of example with reference to the accompanying figures, which are schematic and are not intended to be drawn to scale unless otherwise indicated. In the figures, each identical or nearly identical component illustrated is typically represented by a single numeral. For purposes of clarity, not every component is labeled in every figure, nor is every component of each embodiment of the disclosure shown where illustration is not necessary to allow those of ordinary skill in the art to understand the disclosure. The figures illustrate various embodiments and / or examples that fall within this disclosure, but do not represent the full scope of the disclosure or claims. In the figures: Figs.1A and 1B shows a device comprising a singlet fission layer and additional layers. Figs.2A and 2B shows device configurations involving to a radial junction. Fig 3 shows a schematic diagram for operating a device, where a charge is transferred. Fig.4 shows a schematic diagram for operating a device, where the opposite charge is transferred. Fig.5 shows a schematic diagram with reduced recombination processes. Fig.6 shows EQE spectra of singlet fission material and associated devices. Fig.7 shows a microscopy image of an array of microwire, device architectures, and related properties. Figs.8A and 8B show device architectures for photovoltaic applications. Figs.9A and 9B show EQE spectra of certain device configurations. Figs.10A and 10B show energy level diagrams of device configurations. Figs.11A and 11B show junction depth on a microwire device. DETAILED DESCRIPTION This disclosure involves, in one set of embodiments, an approach to address and go beyond the Shockley-Queisser limit by sensitizing a semiconductor using molecules, optionally organic molecules, that can perform singlet exciton fission (SF), a carrier multiplication process that creates two triplet excitons (electron-hole pairs) from a single photon. Successful transfer of these two triplet excitons to c-Si can result in increased photocurrent and improved efficiencies. The present disclosure involves harvesting singlet fission excitons in photovoltaic devices, photodetectors, and related methods. Some embodiments involve a singlet fission layer configured to generate triplet excitons in the presence of electromagnetic radiation and transfer the excitons to a base semiconductor (the base semiconductor is exemplified as a silicon semiconductor in many embodiments, although other types of semiconductors can be used as those of ordinary skill in the art are equipped to do based on this disclosure). Improved device architectures and configurations involving semiconductors are also described. Efforts directed towards maximizing the efficiency of silicon photovoltaics have led to devices nearing the theoretical limit of 29%. Nonetheless, traditional silicon photovoltaics (i.e., devices where photoconversion occurs in silicon layers) have been understood to be limited by the production of one charge per incident photon. One alternative approach involves carrier multiplication, in which, absorption of one high energy photon leads to creation of more than one electron-hole pair (also referred to herein as an exciton). One way to generate two or more excited states per absorbed photon is singlet exciton fission (also referred to herein as singlet fission) which can occur in some materials (e.g., some aggregates of organic molecules, e.g., tetracene) in which a singlet exciton energy is equal to roughly double a triplet exciton energy of the material. A distinct advantage of singlet exciton fission is that major potential loss for a down-conversion process is spin-forbidden: a singlet exciton cannot convert to one triplet exciton. It may be that only conversion of a singlet exciton into two triplet excitons (also referred to herein as triplets) via a correlated triplet-triplet pair state is spin-allowed. Indeed, this process may be employed in organic photovoltaics (OPV), where internal and external quantum efficiencies in excess of 100% may be achieved. But singlet exciton fission may also cut the maximum achievable open circuit voltage in half, so that in isolation, photoconversion efficiency gain may not be realized. In order to boost power efficiencies, singlet fission materials may be associated with low bandgap inorganic semiconductors including, for example, silicon. As highlighted above, a present, long-standing challenge is to successfully and effectively transfer triplet excitons to silicon photovoltaic materials, such that more than one charge carrier per photon can be collected. The inventors of this disclosure have recognized that certain interfaces and configurations in a device can allow the transfer of fission-generated carriers from a singlet fission layer to a silicon semiconductor, such that carrier multiplication can be achieved. To achieve this, in one set of embodiments, a singlet fission layer is disposed on an organic semiconductor layer, in a way that, in the presence of electromagnetic radiation, the singlet fission layer can generate triplet excitons. The organic semiconductor layer can provide several advantages, as described later herein, such as facilitating the transfer of excitons from the singlet fission layer. In certain aspects, a passivation layer is described, which can be configured to reduce recombination of charges, among several other advantages. In addition, in some embodiments, a silicon semiconductor, which can comprise an emitter layer and a base layer forming a photovoltaic cell, is configured to receive singlet fission-generated excitons in the presence of electromagnetic radiation. Part of the disclosure describes device configurations or device architectures that may be beneficial for successfully transferring triplet excitons. In one set of embodiments, the device can have a shallow junction depth (e.g., diffusion length of less than or equal to 1000, 800, 600, 400, 200, 100, or less than 75 micrometers), which may reduce recombination losses in a photovoltaic device. It has been recognized that the presence of a shallow junction depth, including those found in some device architectures (e.g., microwires), can further reduce recombination (e.g., bulk recombination) of carriers in photovoltaic devices. In much of this disclosure, a singlet fission layer is described and can be configured to operate with other components. In certain embodiments, a singlet fission layer can generate two triplet excitons per photon in the presence of electromagnetic radiation via singlet fission. The singlet fission layer can be configured to operate with a silicon semiconductor, such that at least some triplet excitons are transferred to the silicon semiconductor. In some cases, a singlet fission layer capable of generating triplet excitons may be configured to operate in a silicon photovoltaic device, such that at least a portion of the photogenerated current is generated in the singlet fission layer. In such way, the singlet fission layer may be configured to enhance the efficiency of a silicon photovoltaic device, as described later herein. The singlet fission layer may be positioned or configured in different ways. One embodiment is described with reference to Fig.1A, which shows device 100 having singlet fission layer 102, organic semiconductor layer 104, passivation layer 106, and silicon semiconductor layer 108. According to certain embodiments, the singlet fission layer comprises an outer singlet fission layer. In such cases, the outer singlet fission layer may be directly exposed to electromagnetic radiation, such that singlet fission may occur. As also shown in Fig. 1A, singlet fission layer 102 can be adjacent to, disposed on, or otherwise positioned on organic semiconductor layer 104. This disclosure involves new devices and methods. In many embodiments the devices are new arrangements of components, some or all of which will be understandable to those of ordinary skill in the art. Those of ordinary skill can select various materials based on knowledge in the art, in combination with the content of this disclosure, without undue experimentation. Certain embodiments include a singlet fission material that can produce triplet excitons in the presence of electromagnetic radiation, where such excitons may be subsequently transferred. Some triplet excitons may be transferred to a silicon semiconductor (e.g., silicon emitter layer) in the form of a charge (e.g., electron or hole), as explained in more detail later herein. The transfer of triplet excitons may have different effects, according to some aspects. For example, the silicon semiconductor may experience an increase in current, which may be a result of singlet fission-generated excitons that are transferred to the silicon semiconductor. In certain cases, a silicon photovoltaic material may experience in increase in photoconversion efficiency when configured to operate with a singlet fission material. The singlet fission layer can be made of a suitable material. According to some embodiments, the singlet fission layer comprises tetracene, pentacene, tetracene-derivatives, diphenyltetracene, 5,12-bis((triisopropylsilyl)ethynyl)tetracene, anthracene-derivatives, 9,10- dicyanoanthracene, perylene diimide, perylene diimide derivatives, indigo derivatives, and aza- cibalackrot. Other singlet fission material are possible. The singlet fission layer may be fabricated or deposited using any suitable fabrication technique such as thermal evaporation, spin coating, dip coating, drop coating, physical vapor deposition, organic vapor phase deposition, among other techniques. In many embodiments an organic semiconductor layer is utilized. According to certain embodiments, when the organic semiconductor layer is positioned adjacent to the singlet fission layer, transfer of photogenerated triplet excitons from the singlet fission layer to the organic semiconductor layer may occur. Thus, according to certain embodiments, the organic layer can harvest triplet excitons by facilitating the transfer of such excitons from the singlet fission layer. Without wishing to be bound by theory, it is believed that the position of the energy levels of the organic semiconductor layer relative to the singlet fission layer may contribute to a stabilization of triplet excitons in the organic semiconductor layer. For example, in one embodiment, the energy level of a triplet exciton in the singlet fission layer is 0.1 eV higher than the energy level of a triplet exciton in the organic semiconductor layer, thus it be energetically favorable for the exciton to reside in the organic semiconductor layer. In some cases, the stabilization of the excitons in the organic semiconductor layer may contribute to a subsequent transfer of singlet fission-based charges to an inorganic semiconductor, as further described later herein. According to some embodiments, it may be advantageous to consider the energy of triplet excitons for at least some reasons described herein. This triplet exciton energy may represent the energy of excitons in at least one layer (e.g., organic semiconductor layer). The triplet exciton energy may also represent, in certain embodiments, the lowest-lying triplet exciton energy. In some embodiments, the triplet exciton energy is greater than or equal to 0.9 eV, greater than or equal to 1 eV, greater than or equal to 1.1 eV, greater than or equal to 1.2 eV, greater than or equal to 1.3 eV, greater than or equal to 1.4 eV, greater than or equal to 1.5 eV, greater than or equal to 1.6 eV, greater than or equal to 1.7 eV, greater than or equal to 1.8 eV, greater than or equal to 1.9 eV, greater than or equal to 2.0 eV, greater than or equal to 2.1 eV, or greater than or equal to 2.2 eV. In some embodiments, the triplet exciton energy is less than or equal to 2.2 eV, less than or equal to 2.1 eV, less than or equal to 2.0 eV, less than or equal to 1.9 eV, less than or equal to 1.8 eV, less than or equal to 1.7 eV, less than or equal to 1.6 eV, less than or equal to 1.5 eV, less than or equal to 1.4 eV, less than or equal to 1.3 eV, less than or equal to 1.2 eV, less than or equal to 1.1 eV, less than or equal to 1.0 eV, or less than or equal to 0.9 eV. Combinations of the above-mentioned ranges are possible (e.g., greater than or equal to 0.9 eV and less than or equal to 2.2 eV). The organic semiconductor layer may comprise an electron donating layer or an electron accepting layer. It should be understood that the terms “accepting” and “donating” as used herein refer to majority carrier that can be transported through the layer, that is, either electrons or holes. However, in certain embodiments, it may be appropriate to have organic semiconductor layers that transport both carriers simultaneously without a preference in the identity of the majority carrier. In addition, whether a charge is a hole or electron may not be limiting in this disclosure. However, for sake of clarity, some embodiments generally describe the term “charge”, “carrier”, or “charge carrier” which can refer to a hole or an electron, and when a charge is referred as “other”, it generally refers to the countercharge of the aforementioned charge. Some examples of electron accepting layers include but are not limited to C60, fullerene derivatives,[6,6] phenyl-C61-butyric acid methyl ester (PCBM), and 2,2'-[[12,13-bis(2- ethylhexyl)-12,13-dihydro-3,9-diundecylbisthieno[2",3":4',5']thieno[2',3':4,5]pyrrolo[3,2-e:2',3'- g][2,1,3]benzothiadiazole-2,10-diyl]bis[methylidyne(5,6-difluoro-3-oxo-lH-indene-2,1(3H)- diylidene)]]bis[propanedinitrile] (BTP-4F) (Y6). Some examples of electron donating layer include but are not limited to zinc phthalocyanine, phthalocyanines, copper phthalocyanine, and regioregular poly(3-hexylthiophene-2,5-diyl) (P3HT). Some examples of methods that a person skilled in the art could use, in conjunction with the guidance from this disclosure, to form or deposit the organic semiconductor layer may include atomic layer deposition, chemical vapor deposition, physical vapor deposition, sputtering, spin coating, dip coating, among others. It has been appreciated that properties of the organic semiconductor layer (e.g., morphology) may impact the performance of the fabricated device. In addition, according to some embodiments, it may be beneficial to have an organic semiconductor layer that substantially cover the surface of the underlying layer (e.g., an n-type emitter layer). If desired, one skilled in the art could use known routine tests such as X-ray scattering and / or electron microscopy to inspect the organic semiconductor layer formed to achieve the desired results. Certain embodiments involve a passivation layer for a variety of purposes or reasons. For example, a passivation layer disposed on a silicon semiconductor may allow the passivation of defects, such as intrinsic defects and / or trap states present in the surface the silicon semiconductor. In addition, according to some embodiments where an organic semiconductor material and a passivation layer are included in a photovoltaic material, the passivation layer may impede at least some of the carriers in the organic semiconductor material from recombining at the silicon semiconductor. With respect to the passivation layer, it may be advantageous to have a layer of a suitable thickness. According to certain embodiments, the thickness of the passivation layer may impact the ability of transferring triplet excitons to the inorganic semiconductor. Some effects that have been appreciated that may depend on the thickness of the passivation layer include the recombination of the carriers at the silicon surface and the ability of carriers to undergo tunneling. In accordance with some embodiments, the thickness of the layer can have a thickness of greater than or equal to 0.01 nm, greater than or equal to 0.02 nm, greater than or equal to 0.04 nm, greater than or equal to 0.06 nm, greater than or equal to 0.08 nm, greater than or equal to 0.1 nm, greater than or equal to 0.12 nm, greater than or equal to 0.14 nm, greater than or equal to 0.16 nm, greater than or equal to 0.18 nm, greater than or equal to 0.2 nm, greater than or equal to 0.4 nm, greater than or equal to 0.6 nm, greater than or equal to 0.8 nm, greater than or equal to 1 nm, greater than or equal to 2 nm, greater than or equal to 4 nm, greater than or equal to 6 nm, greater than or equal to 8 nm, or greater than or equal to 10 nm. In accordance with some embodiments, the thickness of the layer can have a thickness of less than or equal to 10 nm, less than or equal to 8 nm, less than or equal to 6 nm, less than or equal to 4 nm, less than or equal to 2 nm, less than or equal to 1 nm, less than or equal to 0.8 nm, less than or equal to 0.6 nm, less than or equal to 0.4 nm, less than or equal to 0.2 nm, less than or equal to 0.18 nm, less than or equal to 0.16 nm, less than or equal to 0.14 nm, less than or equal to 0.12 nm, less than or equal to 0.1 nm, less than or equal to 0.08 nm, less than or equal to 0.06 nm, less than or equal to 0.04 nm, less than or equal to 0.02 nm, or less than or equal to 0.01 nm. According to some embodiments, the passivation layer can be of a suitable type. For example, the passivation layer can be an oxide (e.g., Al2O3, HfO2, SiO2) or a Silicon containing compound (e.g., SiO2, Si3N4, and amorphous Silicon / a-Si). In certain cases, the passivation layer can be a ferroelectric layer (e.g., bismuth layered oxides). Some known methods in the art that can be used to fabricate a passivation layer, including atomic layer deposition, chemical vapor deposition, wet oxidation, dry oxidation, among other techniques. The passivation layer may comprise a compound selected from ZrO^ or HfO^N^. In accordance with some embodiments where ZrO^ or HfO^N^ are included, x and / or y can be greater than or equal to 0, greater than or equal to 0.5, greater than or equal to 1, greater than or equal to 1.5, or greater than or equal to 2. In accordance with some embodiments where ZrO^ or HfO^N^ are included, x and / or y can be less than or equal to 2, less than or equal to 1.5, less than or equal to 1, less than or equal to 0.5, or less than or equal to 0. Combinations of the above- mentioned ranges are possible (e.g., x and / or y can be greater than or equal to 0 and less than or equal to 2). The devices and related methods described herein may comprise a silicon semiconductor. In certain embodiments, the silicon semiconductor is configured to produce photogenerated carriers in the presence of electromagnetic radiation. It should be understood that the silicon semiconductor may be configured to operate simultaneously with other components of the device. For example, for a device having a singlet fission layer and a silicon semiconductor, where both are being exposed to electromagnetic radiation, the singlet fission layer may produce triplet excitons while the silicon semiconductor may also produce excitons. One set of embodiments describes a silicon semiconductor that is configured to generate carriers in the silicon semiconductor via a photovoltaic effect (e.g., absorption. In another set of embodiments including a photovoltaic device, the silicon semiconductor may be configured to operate with a passivation layer, an organic semiconductor layer, and a singlet fission layer, such that the photovoltaic device can collect photogenerated carriers that are generated in the silicon semiconductor as well as those that are transferred from the singlet fission layer. In certain embodiments, the device can have a singlet fission layer capable of producing two excitons (e.g.. triplet excitons, two holes, two electrons) per photon and a silicon semiconductor capable of producing one exciton (e.g., one silicon-generated exciton, one hole, one electron) per photon in the presence of electromagnetic radiation. In certain embodiments, the silicon semiconductor comprises an n-doped emitter layer or a p-doped emitter layer. Such emitter layers may be considered to be operable in devices such as photovoltaics, photodetectors, or the like. In most of the disclosure, the n-doped emitter layer and the p-doped emitter layer are herein referred to as the emitter layer. As understood by a person of ordinary skilled in the art, n-doped emitter layers primarily transport electrons, whereas p-doped emitter layers primarily transport holes. In embodiments including an emitter layer, such layer is configured to interact with electromagnetic radiation. In another set of embodiments including an emitter layer, such layer is configured to facilitate the movement of photogenerated carriers to be collected in a device. The emitter layer may be doped. In embodiments in which the emitter layer comprises an inorganic semiconductor, doping may be introduced in the form of impurities or defects. In one set of embodiments, the p-type emitter layer comprises p-doped silicon, and in another set of embodiments, the n-type emitter layer comprises n-doped silicon. Some examples of compounds that can dope the silicon emitter include boron, arsenic, phosphorus and gallium. The emitter layer can have a doping concentration, which can allow tunable properties such as electrical conductivity, absorption of electromagnetic radiation, among others. In accordance with some embodiments, the doping concentration of the emitter layer may have a doping concentration gradient. In certain embodiments, the doping gradient of the emitter layer facilitates the formation of an electric field with such emitter layer. For example, the presence of a doping gradient may facilitate the formation of an electric field between the organic semiconductor layer and the emitter layer (e.g., n-doped silicon emitter layer). In some embodiments, the silicon semiconductor comprises a p-type base or an n-type base. The base may be of a suitable material type. For example, a p-type base can be p-doped silicon, whereas an n-type base comprises n-doped silicon. Some examples of compounds that can dope the silicon base include boron, arsenic, phosphorus and gallium. In another aspect of this disclosure, the junction in a silicon semiconductor has a diffusion length. It has been recognized that the diffusion length may impact the ability of some carriers to recombine in the bulk. Therefore, in certain circumstances, it may be favorable to have a shallow junction depth (i.e., small diffusion length). In some embodiments, the diffusion length is greater than or equal to 1 nm, greater than or equal to 10 nm, greater than or equal to 50 nm, greater than or equal to 100 nm, greater than or equal to 500 nm, greater than or equal to 1 μm, greater than or equal to 10 μm, or greater than or equal to 100 μm. In some embodiments, the diffusion length is less than or equal to 100 μm, less than or equal to 10 μm, less than or equal to 1 μm, less than or equal to 500 nm, less than or equal to 100 nm, less than or equal to 50 nm, less than or equal to 10 nm, or less than or equal to 1 nm. In some embodiments, the doping concentration and / or doping gradient of the silicon semiconductor may impact the diffusion length In one set of embodiments, a vertical junction with a particular diffusion length is tuned to reduce bulk recombination. Vertical junctions can be found in device geometries such as conventional solar panels, for example. In another set of embodiments, the geometry of the junction is used to tune the junction depth. As seen in Fig.2A, radial junction of device 250 can have singlet fission layer 252, organic semiconductor layer 254, passivation layer 256, emitter layer 258, and base layer 260. In the present disclosure, it has been recognized that using a radial junction may minimize bulk recombination losses based on a radial geometry. As illustrated in Fig.2B with a schematic diagram of radial junction 270, a carrier in emitter layer has a higher probability of being transferred to base layer 276 than traveling through emitter layer 274, which could lead to bulk recombination, or being transferred to passivation layer 272, which could lead to surface combination. Therefore, in some aspects, the geometry of radial junctions can minimize recombination processes, which may not only benefit carriers generated in a silicon photovoltaic, but may also benefit carriers being transferred from a singlet fission layer. In some embodiments, it is believed that the presence of a radial junction may facilitate the transfer of an electron or a hole from a singlet fission process. In view of the appreciated benefit of radial junctions, some device architecture can be tuned. Some device architectures that take advantage of radial junctions include microstructures and nanostructures that have a surface with one or more layers shaped into cylinders, needles, wires, or other shapes. For example, herein described are microwires, which can be fabricated into different shapes and / or sizes. For example, the microwires can have a length, where such length is greater than or equal to 5 µm, greater than or equal to 10 µm, greater than or equal to 25 µm, greater than or equal to 50 µm, greater than or equal to 75 µm, or greater than or equal to 100 µm. In some embodiments, the length of the microwires is less than or equal to 100 µm, less than or equal to 75 µm, less than or equal to 50 µm, less than or equal to 25 µm, less than or equal to 10 µm, less than or equal to 5 µm. According to some embodiments, the microwires can have a diameter at its base that is greater than or equal to 1 µm, greater than or equal to 2 µm, greater than or equal to 4 µm, greater than or equal to 6 µm, greater than or equal to 8 µm, or greater than or equal to 10 µm. In some embodiments, the diameter of the microwires is less than or equal to 10 µm, less than or equal to 8 µm, less than or equal to 6 µm, less than or equal to 4 µm, less than or equal to 2 µm, or less than or equal to 1 µm. According to certain embodiments, the microwires are spaced from its neighbor by a length of greater than or equal to 1 µm, greater than or equal to 2 µm, greater than or equal to 4 µm, greater than or equal to 6 µm, greater than or equal to 8 µm, or greater than or equal to 10 µm. In some embodiments, the microwires are spaced from its neighbor by a length of less than or equal to 10 µm, less than or equal to 8 µm, less than or equal to 6 µm, less than or equal to 4 µm, less than or equal to 2 µm, or less than or equal to 1 µm. The microwires can be vertically aligned to increase the light- trapping capability of the device, although other configurations are possible (e.g., diagonally aligned). The device comprising an array of microwires may be configured to enhance the absorption of light in a variety of ways. For example, the array of microwires may be tapped, such that the diameter of the microwire gradually increases from top to bottom. According to some embodiments, the refractive index may vary across the microwire depending on the region of the microwire. For instance, one or more layers of the microwire (e.g., a silicon base layer) may have a refractive index of 4, whereas the environment surrounding the microwire, which is generally air, can have a refractive index of 1. In such cases, the refractive index may vary across the microwire, which can depend on properties of the microwire, such as the diameter or shape, for example. According to some embodiments, the effective refractive index of the microwire is affected by configurations of layers and microwire architecture. In certain embodiments, a suitable effective refractive index that maximizes absorption of electromagnetic radiation in the microwire may benefit the efficiency and / or performance of microwire-based photovoltaic devices. In embodiments where an organic semiconductor layer is included, the organic semiconductor layer can be positioned between the singlet fission layer and the passivation layer. There may be several benefits from having the organic semiconductor layer adjacent to, deposited on, or position on the passivation layer. For example, the organic semiconductor layer may create a strong electric field through the passivation layer which may extend to the inorganic semiconductor. Without wishing to be bound by theory, it is believed that the presence of a strong electric field through the passivation layer may promote the transfer of charges to the inorganic semiconductor. As schematically illustrated in Fig.3 with device 300, first, a singlet exciton is split into two triplet excitons in singlet fission layer 302 in the presence of electromagnetic radiation, followed by transfer of the triplet excitons to organic semiconductor layer 304, where at least one charge of an exciton is transferred through passivation layer 306 to silicon semiconductor 308. The transferred charge can then generate electric field 320, where such electric field may facilitate the transfer of a charge of the opposite charge to the previously transferred charge. Although Fig.3 shows the transfer of an electron to form a charged state that is separated by the passivation layer followed by the transfer of a hole, in certain embodiments where suitable layers are provided (e.g., an electron accepting layer), a similar mechanism but with the opposite charge may occur, as shown in Fig.4. In some embodiments, the charged state that is separated by the passivation layer has an energy level between the triplet energy level of the singlet fission material and the bandgap of the silicon semiconductor. For example, in embodiments including an organic semiconductor layer, the organic semiconductor layer may favor the formation of a charged stated that is between the triplet energy of the singlet fission layered material (e.g., 1.25 eV for tetracene) and the bandgap of silicon (1.1 eV). Without wishing to be bound by theory, it is believed that the formation of an electron or hole in the interface between the organic semiconductor material and the passivation layer may favor the formation of a charged state with a suitable energy level or degree of stability. According to certain embodiments, this strong electric field may repel minority carriers from the silicon semiconductor. For illustrative purposes, photovoltaic device 600 in Fig 5 shows a schematic process of repelling minority carriers (in this case, electrons) in the presence of a strong electric field. In such figure, device 600 include singlet fission layer 602, organic semiconductor layer 604, passivation layer 606, emitter layer 608, and base layer 610. In the same figure, a carrier is produced in the emitter layer and base layer, where such carrier (e.g., an electron or a hole) is generated in the silicon semiconductor (i.e., not transfered from a singlet fission layer). The carrier may be repelled by the presence of an electric field formed between the organic semiconductor layer and the emitter layer. Thus, such carriers that are repelled can contribute to the carriers that are to be collected in a photovoltaic cell, for example. With regards to the configuration of the material and / or layers described, as shown in Fig.1B, passivation layer 206 can be between organic semiconductor layer 204 and emitter layer 208. In addition, according to certain embodiments and as shown in Fig.1B, organic semiconductor layer 204 is between singlet fission layer 202 and passivation layer 206. Also shown in Fig.1B, emitter layer 208 can be between passivation 206 and base layer 210. According to certain embodiments, the electromagnetic radiation may have a wavelength range where the device can absorb light and / or be operated at. It should be understood that an interaction with electromagnetic radiation can also include transmission, scattering, excitations, among others. In some cases, the wavelength of the electromagnetic radiation is greater than or equal to 300 nm, greater than or equal to 400 nm, greater than or equal to 500 nm, greater than or equal to 600 nm, greater than or equal to 700 nm, greater than or equal to 800 nm, greater than or equal to 900 nm, greater than or equal to 1,000 nm, or greater than or equal to 1,100 nm, according to some embodiments. The wavelength is less than or equal to 1,100 nm, less than or equal to 1,000 nm, less than or equal to 900 nm, less than or equal to 800 nm, less than or equal to 700 nm, less than or equal to 600 nm, less than or equal to 500 nm, less than or equal to 400 nm, or less than or equal to 300 nm,. EXAMPLE 1 We present c-Si solar cell device designs, including materials (e.g., doped c-Si, donor / acceptor interface layers), and architectures (e.g., microwire geometry, junction shape and depth), demonstrating photovoltaic performance enhancement using a singlet exciton fission material (e.g., tetracene). Device performance results suggest that the device design may need a donor / acceptor interface layer (e.g., zinc phthalocyanine) between the SF layer and the silicon that generates a strong electric field at the device surface, and could benefit from a junction architecture (e.g., radial junction shape, shallow junction depth) with reduced bulk recombination losses. The combination of these design aspects could enable effective carrier collection from the triplet excitons that are transferred near the device surface closest to the triplet exciton sensitization layers. We anticipate the doping variation across the device architecture to be important not just for the triplet exciton sensitization interlayer performance but also in successful charge carrier extraction. Additionally, enhanced device absorption due to the geometry of the solar cell will allow us to observe greater than one electron generated per incident photon in silicon photovoltaics from sensitization by a singlet fission material. For photocurrent generation, it is important to collect the photo-generated electrons and holes at the respective electrodes. To achieve this, electrons need to reach the n-type region, while the holes need to reach the p-type region. Therefore, reducing the carrier (electron or hole) travel distance to reach the n-type or p-type region, also known as the diffusion length, is important for effective charge collection. However, in the case of Interdigitated Back Contact (IBC) designs, the carrier travel distance to reach the n-type region or p-type region can be quite long . Consequently, during their journey to the n-type or p-type region, carriers may recombine due to bulk recombination. This means that even if carriers move from organic materials (e.g., singlet fission materials) to crystalline silicon (c-Si), they may not reach the electrode. As a result, when singlet fission materials are applied to IBC c-Si solar cells, the current density (Jsc) does not increase, as shown in Fig.6. Hence, minimizing the diffusion length is of paramount importance in order to efficiently collect carriers. Forming a radial junction with shallow junctions is one of the most effective ways to minimize the diffusion length. A radial junction involves creating a three-dimensional junction along the surface of c-Si wire structures, resulting in a radial p-n junction with a base in the core and an emitter in the shell. When forming the radial junction, various wire structures can be considered, such as nanowires and microwires. Among these shapes, microwire-based radial junction solar cells have garnered significant attention due to their structural advantages, including ease of forming a radial junction and lower surface recombination compared to nanowires. c-Si microwires effectively separate and collect carriers at the radial junction due to the short required diffusion length, which is smaller than the microwire radius, for the photo- induced minority carriers. The diffusion length of carriers in the radial junction is less than 1 µm, which is at least 100 times shorter than that of conventional planar junctions (>100 µm) and IBC solar cells (~200 µm). Furthermore, vertically aligned microwire arrays demonstrate superior light-trapping capability, enhancing the overall c-Si absorption of incident light over a broad wavelength range of 300–1100 nm. Additionally, in tapered microwires (Fig.7), where the diameter gradually increases from top to bottom, the effective refractive index (n) of the tapered microwire gradually transitions from the air's index (1) to that of the c-Si substrate (~4), thus minimizing the impedance mismatch between air and tapered microwires. In addition to device geometry, applying additional electron donating (e.g., zinc phthalocyanine) or electron accepting (e.g., C60) material layers in between the silicon device surface and the singlet exciton fission layer (e.g., tetracene) can help in enhancing the charge carrier collection of the transferred triplet excitons right at the silicon surface . The electron donating / electron accepting layers can generate an electric field at the silicon surface that helps to drive the surface minority carriers away from the interface and towards the p-n junction of the device; for example , , the electron donating layer can generate a field to promote hole transport in the n-type silicon emitter layer to the junction between the emitter and the base. Consequently, swapping the emitter and base layer doping will result in the field direction being unfavorable for the device performance. Likewise, the electron accepting layer can generate a field to promote electron transport in the p-type silicon emitter layer to the junction between the emitter and the base. Furthermore, a thin passivation layer in between the electron donating / accepting layer and the silicon device emitter layer is important for passivating surface defect and trap states from quenching the transferred triplet exciton layers. In terms of potential other materials than can be used as each layer: • Singlet fission layer: tetracene, pentacene, tetracene-derivatives such as diphenyltetracene (DPT), 5,12-Bis((triisopropylsilyl)ethynyl)tetracene (TIPS-Tc), anthracene-derivatives such as 9,10-dicyanoanthracene (DCA), etc. • Electron donating layer: zinc phthalocyanine, other phthalocyanines such as copper phthalocyanine, Regioregular poly(3-hexylthiophene-2,5-diyl) (P3HT), etc. • Alternatively, electron accepting layer: C60, other fullerene derivatives such as [6,6] phenyl-C61-butyric acid methyl ester (PCBM), 2,2'-[[12,13-Bis(2-ethylhexyl)-12,13- dihydro-3,9-diundecylbisthieno[2",3":4',5']thieno[2',3':4,5]pyrrolo[3,2-e:2',3'- g][2,1,3]benzothiadiazole-2,10-diyl]bis[methylidyne(5,6-difluoro-3-oxo-lH-indene- 2,1(3H)- diylidene)]]bis[propanedinitrile] (BTP-4F) (Y6), etc. • Passivation layer: Al2O3, HfO2, SiO2, Si3N4, a-Si, etc. • Emitter: n-doped silicon, p-doped silicon, etc. • Base: p-doped silicon, n-doped silicon, etc. To deposit the singlet fission materials on to the c-Si microwire solar cells, thermal evaporation can be used. However, there are no restrictions on the deposition methods, and it is anticipated that various deposition techniques can be employed in an oxygen-free environment. Examples of both types of device structures with the relevant geometry and composition of layers is presented in Fig.8A and 8B. The photovoltaic properties of the c-Si microwire solar cells with singlet fission sensitization layers are presented. To assess the photovoltaic characteristics of the devices, current density-voltage (J-V) measurements were performed under AM 1.5 G illumination .. Type 2 microwire solar cells exhibited an increase in power conversion efficiency (PCE), while Device 1 did not show any improvement in PCE. Type 2 microwire solar cells without the singlet fission layer and the electron donating layer displayed a PCE of 12.4%, Open-circuit voltage (Voc) of 0.5 V, Jscof 37.06 mA / cm2, and a fill factor (FF) of 66.4%. On the other hand, Type 2 microwire solar cells with the singlet fission layer and electron donating layer achieved a PCE of 12.7% (Voc of 0.51 V, Jsc of 37.69 mA / cm2, and FF of 66.4%), indicating an increase in Jscby 0.63 mA / cm2compared to the solar cells without both layers. Furthermore, the enhancement in Jscwas further supported by external quantum efficiency (EQE) measurements (Figs.9A and 9B). As seen in the EQE spectra, the increase in Jsc was observed in the tetracene absorption region. This confirms that carriers from the singlet fission materials contribute to improving the Jscvalue of the c-Si microwire solar cells. Based on these results, we believe that successful energy transfer from tetracene to silicon is achievable in microwire cells with the proposed material interlayers. Crucially, the EQE spectra in this region is at 97%, suggesting a good likelihood for achieving over 100%, that is, demonstrating generation of >1 electron per incident photon (not shown before in silicon photovoltaics). Our results suggest that factors such as the type and concentration of doping, in addition to the materials at the interface between singlet fission layer and c-Si play a crucial role in this phenomenon. EXAMPLE 2 Single junction crystalline silicon solar cells are rapidly approaching their theoretical efficiency limit of 29% . There are substantial opportunities to improve performance if thermalization losses can be reduced in the visible and UV spectrum. For example, using singlet exciton fission in tetracene (Tc) to double the available carriers obtained from blue and green sunlight could increase the power conversion efficiency of a single-junction crystalline silicon solar cell to 35% . Singlet exciton fission in Tc generates two spin-1 triplet excitons with energies of 1.25 eV from one spin-0 singlet exciton with an energy of 2.4 eV. Spin conservation opposes the thermalization of a singlet into one triplet exciton, protecting the process against losses and contributing to a near ideal yield in many fission materials, including Tc . The triplet energy of Tc is just above that of the 1.1 eV band gap of crystalline silicon (c-Si), which is ideal for coupling to c-Si. However, transferring the energy from the two excitons formed from one high energy photon absorbed in Tc to c-Si and observing device enhancements has proven challenging . Depositing Tc directly onto hydrogen-terminated c-Si surfaces decreases the external quantum efficiency (EQE) of both silicon-Tc heterojunction solar cells and interdigitated back-contacted (IBC) solar cells . Inserting LiF spacers and pyrene passivation layers between the Tc and silicon also does not yield efficient triplet energy transfer. Introducing a thin interlayer of HfOxNy between Tc and c-Si, however, shows sensitization of c-Si by triplet excitons, albeit without demonstrating an increase in thephotocurrent of an IBCcell . The HfOxNyinterlayer is hypothesized to play a bifunctionalrole, acting to passivatesome silicon surface defects whilst simultaneously enabling triplet exciton transfer . Here, a two-component interface is proposed for efficient triplet exciton sensitization of c-Si. This approach is guided by the apparent ineffectiveness of previous efforts to directly transfer triplets from Tc to c-Si via a Dexter mechanism. The cells are instead designed based on the observed coupling between Tc and c-Si across thin HfOxNy interfaces. Evidence of triplet transfer is correlated with the presence of midgap defect states in HfOxNy, suggesting the possibility of sequential charge transfer via an intermediate charge-separated state supported by HfOxNy . Consequently, it is proposed to mediate sensitization with an initial charge transfer to silicon , followed by a sequential transfer of the remaining charge carrier. The energy of the intermediate charge-separated state must lie between the triplet energy of Tc (1.25 eV) and the bandgap of silicon (1.1 eV). Tc itself is an electron donor , but at least in previously studied interfaces, its highest occupied molecular orbital (HOMO) is too deep to support a charge separated state within the necessary energy range. Therefore, it is proposed to insert an additional electron donor at the interface with silicon that supports a state D+-ASi–with the appropriate energy, where D+represents the charged electron donor and ASi–describes the electron accepting role of silicon. The second component of the interface disclosed herein is a thin passivation layer necessary to prevent the transferred charge carriers from immediately recombining at the siliconsurface, while stillenabling carrier tunneling. Aluminum oxide (AlOx) is commonly used to passivate silicon solar cells . As presented herein, approximately 1-nm-thick layers of AlOx are used to both passivate the silicon surface and maintain charge tunneling across the interface. Zinc phthalocyanine as a donor material Zinc phthalocyanine (ZnPc) was studied as a candidate donor material at the Tc-Si interface. ZnPc is a common donor with a reported HOMO above that of Tc. The time- dependent functional theory (TDDFT) calculations (see below) and literature show that the excited Tc triplet state is 0.1-0.2 eV higher in energy than the ZnPc triplet, potentially enabling triplet harvesting at the interface prior to the formation of a charge separated state. Further calculations show that the Tc HOMO is 0.2 eV deeper than the ZnPc HOMO. Ultraviolet photoelectron spectroscopy was performed to determine the energetic alignment of ZnPc at interfaces between Tc and c-Si. In Fig.10A, the alignments for a highly n- doped Si surface (n+-Si) is summarized. The difference between the c-Si conduction band minimum and the HOMO level of ZnPc is approximately 1.20 eV, within the allowed energeticrange for the D+-ASi–state. Binding energy was neglected in the determination of the energy of the charge-separated state DZnPc+-ASi–due to expected charge screening and delocalization in silicon . Furthermore, there is minimal barrier for subsequent hole transfer to the bulk valence band of silicon, within measurement error. A negligible difference was observed in the Tc- Si energy alignment with and without the ZnPc layer. This confirms that the presence of the ZnPc layer lowers the energy of a donor-acceptor state with silicon, thereby enabling sequential charge transfer to silicon following triplet exciton formation. In contrast, the energetic alignment with a highly p-doped silicon surface (p+-Si) shown in Fig.10B exhibits a significant electron transfer barrier, and the charge separated state is the lowest energy state in the system, hindering overall energy transfer from Tc to silicon. Thus, it is suspected that the energy levels of Tc / ZnPc enable sequential charge transfer to n+-doped c-Si. The energetic alignment, however, is unfavorable for p+-doped c-Si. Silicon solar cell design for singlet fission sensitization Charge injection at the surface of silicon demands a solar cell design with efficient surface carrier collection. Here, shallow p-n junctions are employed, both in conventional planar geometries and microwire (MW) solar cells that employ shallow radial junctions. Shallow junctions efficiently extract charge carriers transferred to the surface of c-Si by reducing the propagation distance of minority carriers . The microwire structure also exhibits enhanced light absorption , particularly in the short wavelength region, reducing reflection losses. Following a previously reported protocol, tapered c-Si microwire arrays were fabricated with a spacing of 2 μm and a length of 15 μm. A radial junction is formed on the p-type tapered c-Si microwire arrays with an n-type emitter junction depth of 300 nm (see FIGs.11A and 11B) through a spin-on-dopant-based thermal doping process. To minimize recombination on the rear side, a back surface field (BSF) layer with a junction depth of 1 µm and a localized back contact is added. Then, a 1-nm-thick AlOx layer is formed using Atomic Layer Deposition (ALD) on the front side of the solar cell. A microgrid electrode is applied as the front electrode to efficiently collect carriers . This microgrid electrode covers only 2% of the active area (1 cm²),thereby reducing shading losses from the topelectrodes, while also increasing the depositionarea of Tc / ZnPc on the AlOx / c-Si surface. Nominally 1.5 nm of ZnPc followed by 30 nm of Tc is then thermally evaporated onto the front surface of the microwire cells. For more details on the full device fabrication procedure, see the Materials and Methods section. To investigate the role of ZnPc, a control device was also prepared through an identical method on a p+-n device where only the doping of the base microwire device structure was swapped. In Tc / ZnPc / n+-p Si MW, island-type growth is observed on the sides of the MWs, with similar but denser growth on the bottom region of the microwire arrays. Since thermal evaporation is a directional deposition technique, increased deposition is expected to occur on the horizontal surface (bottom region) than on the sidewalls of the MWs perpendicular to the deposition sources. The EQE spectra of the n+-p MW device before and after Tc and ZnPc deposition were measured. After deposition of Tc / ZnPc, a positive contribution is seen corresponding to the absorption spectrum of Tc, with a maximum EQE increase from 81.6% to 87.9% at 520 nm. The measured J-V curves of the devices also show that depositing ZnPc and Tc on the n+-p MW devices results in an enhancement in the short-circuit current density, with negligible decrease in the open-circuit voltage and fill factors, resulting in an overall enhancement in power conversion efficiency, see Table 1. It is notable that the introduction of molecular materials does not degrade the electrical characteristics of the silicon solar cell. These results suggest that the role of the molecular materials in this cell architecture is primarily excitonic in nature, and other than increased charge injection, decoupled from the operation of the junction itself. Table 1. Photovoltaic properties of n+-p Si MW solar cells with and without Tc / ZnPc Table 2. Photovoltaic properties of pyramidal-textured planar n+-p Si device with and without Tc / ZnPc As expected from the interfacial measurements, p+-n MW devices exhibit dramatically different behavior when coupled to Tc. The EQE spectra before and after Tc and ZnPc deposition was measured. Unlike the case with the n+-p MW device, shadowing is instead observed in the EQE spectra from absorption of Tc, dropping from 75.6% to 63.5% at 520 nm. This also confirms that the device performance enhancements observed in the n+-p devices are not solely from enhanced antireflective effects of adding the additional organic layers. n+-p and p+-n type planar devices are also fabricated with random surface pyramidal texturing, which is extensively utilized in the c-Si solar cell industry for its antireflective properties. The effects on the EQE spectra are consistent with the observations in the MW solar cells presented above, although the magnitude of the enhancement is slightly decreased. The role of charge tunneling in the formation of the D+-ASi–state is verified by replacing the 1-nm-thick AlOx passivation layer on an n+-p MW solar cell with a 10 nm-thickAl2O3 passivation layer. On the thicker sample, Tc shadowing was observed in the EQE spectra, demonstrating that coupling to c-Si is disrupted. It was verified that ZnPc is essential by fabricating control devices without the ZnPc donor layer on both n+-p and p+-n MW devices, where Tc shadowing is again observed in the EQE spectra. It is noted that while both n+-p and p+-n solar cells fabricated without the ZnPc layer exhibit shadowing from Tc, the shadowing is less in the n+-p MW device. This suggests that there may be a small number of triplet states from Tc that are able to undergo Dexter transfer or sequential charge transfer to c- Si, potentially via charge-separated states incorporating the tail of the Tc density of states. Discussion The overall Tc sensitization efficiency, ηTc, encompasses singlet fission efficiency in Tc, transport of triplets to the interface with silicon, triplet transfer efficiency at the interface, and extraction efficiency of charge carriers transferred to silicon. It is emphasized that singlet exciton transfer alone from Tc to c-Si in the n+-p MW device yields a maximum sensitization efficiency ηTc = 100%. Indeed, it is not possible to observe Tc peaks in the EQE of the silicon solar cell unless there is efficient (ηTc > 100%) coupling to triplets generated by singlet exciton fission. To evaluate ηTca transfer matrix model of the layers in the solar cell was performed .Calculationdetails are presented below. EQEpercentage differential (∆EQE / EQE0) where∆EQE = EQETc – EQE0 and EQETc and EQE0 are the efficiencies of the Tc and control devices were fitted. The fit yields a sensitization efficiency of ηTc = (138 ± 6)%, where 200% is the maximum theoretical enhancement possible for a photocurrent doubling process. Based on these results, it is expected that it is possible to significantly improve the performance of singlet exciton fission enhanced solar cells and photodetectors toward a peak quantum yield of two electrons per photon and an overall power efficiency that exceeds the conventional single junction limit. First, technologies from advanced-node field-effect transistors can be adopted to improve the performance of the thin passivation layer. Second, conformal coating and optimized Tc growth could substantially improve the coverage of sensitizing materials on the silicon surface. Finally, although it has long been the archetype fission material for coupling to silicon, Tc has poor photostability and will need to be replaced with a photostable analog. In conclusion, presented herein is efficient coupling between a silicon solar cell and singlet exciton fission in Tc. Control over the crucial interface between Tc and silicon is established by assuming sequential charge transfer mediated by a thin layer of ZnPc. The resulting observation of more than one electron per photon in a silicon solar cell provides the foundation for a new solar photovoltaic technology capable of accelerating the global adoption of renewable energy. Materials and Methods Fabrication of tapered c-Si microwire arrays The photoresist dot arrays (2 μm diameter, 1 μm spacing) were periodically patterned onto the c-Si wafer using AZ-nLOF-2035 photoresist (AZ Electronic Materials) via a photolithography process. The patterned c-Si wafer was then etched by deep reactive ion etching (DRIE, Tegal 200) with 1500 W source power, 100 W stage power, and 45 mTorr gas pressure using SF6 (250 sccm) and C4F8 (150 sccm) as source gases. Following the DRIE process, cleaning was conducted using a piranha solution (3:1 mixture of sulfuric acid and hydrogen peroxide (30% w / w in H2O)). To fabricate tapered c-Si microwires, the c-Si microwires were immersed in an HF / HNO3 / CH3COOH solution (RSE-100, Transene) for ~10 seconds. Fabrication of tapered c-Si microwire solar cells To fabricate n+-p-type MWs, after the fabrication of the tapered p-type c-Si microwire array on the c-Si wafers, a back surface field (BSF) layer was formed in a tube furnace under amixedatmosphere of O2(250 sccm) and N2(1000 sccm) at 980 °C using a boron spin-on- dopant source (B155, Filmtronics). Following the BSF layer formation, a SiO2layer was thermally grown on the wafer in a furnace. This SiO2 layer was removed from the front of the substrate with a buffered oxide etchant (BOE) after the backside was protected with photoresist (AZ4330, AZ Electronic Materials). Subsequently, an additional 200-nm-thick SiO2 diffusionbarrier wasdeposited on the rear side of the wafer via plasma-enhanced chemical vapordeposition (PEH-600). Next, an emitter layer was formed in a tube furnace under a mixed atmosphere of O2 (125 sccm) and N2 (500 sccm) at 800 °C using a phosphorus spin-on-dopant source (P509, Filmtronics). Then, after removing the oxide layer using BOE, SC1 and SC2 cleaning processes were conducted. An AlOx passivation layer with a thickness of 1 nm was deposited on the front side of the wafer, while a 10-nm-thick Al2O3layer was deposited on the rear side of the wafer via ALD (Lucida D100, NCD) and annealed under 500 sccm of a mixed gas of Ar / H2 (v / v = 96:4) at 500 °C in a tube furnace. Patterns for the microgrid electrodes and localized back contact surface were formed on the front and rear sides of the wafer, respectively, via photolithography, using AZ4330 photoresist. For electrode fabrication, the wafer was immersed in a BOE solution, and 600 nm thick Al films were deposited on both sides of the wafer via thermal evaporation. To fabricate p+-n-type MW, after fabricating the tapered n-type c-Si microwire array on the c-Si wafers, the process was the same as for n+-p-type MW, except for the BSF and emitter formation conditions. A BSF was formed in a tube furnace under a mixed atmosphere of O2(125 sccm) and N2 (500 sccm) at 860 °C using a phosphorous spin-on-dopant source (P509, Filmtronics). Then, an emitter layer was formed on the front surface of the wafers under a mixed atmosphere of O2(250 sccm) and N2(1000 sccm) at 880 °C using a boron spin-on-dopant source (B155, Filmtronics). Singlet fission top-side fabrication Before deposition, the samples were dipped in acetone for 5 minutes, and then in IPA for5minutes at a low sonication power. Afterward, the samples were dried with N2gas. After cleaning, the samples were transferred into a nitrogen glovebox for deposition of the organic layers. ZnPc was purchased from Luminescence Technology Corp (sublimed grade, 99% purity) and used as received. Tc was purchased from Sigma Aldrich (sublimed grade, > 99.99% trace metal basis) and purified once through a sublimation and recondensation process in a three-zone tube furnace before deposition. The organic layers were deposited by thermal evaporation in a vacuum chamber at a pressure of < 1×10-6torr.1.5 nm of ZnPc was deposited at a 0.2 Å / s rate, followed by 30 nm of Tc deposited at a 1 Å / s rate. Thickness calibrations were obtained from ellipsometry measurements performed on planar substrates. The surface area of the microwire substrates is much larger. Thus, the true area density of ZnPc (1.5 nm nominal thickness) and Tc (30 nm nominal thickness) in the microwire devices is expected to be lower The samples were then encapsulated in a dry nitrogen atmosphere (<1 ppm O2) with a glass slide and ultraviolet curable epoxy. A small piece of foil was placed to protect the active area during the UV exposure for the curing step. Photoelectron spectroscopy Tc and ZnPc layers were deposited on AlOx-silicon surfaces by thermal evaporation inanultrahigh-vacuum chamber (10-9 Torr) connected to the analysis chamber.1.5 nm of ZnPc was deposited at a rate of about 0.1 Å / s, followed by 20 nm of Tc at a deposition rate of about 1 Å / s. Then, ultra-violet and X-ray photoemission spectroscopy (UPS, XPS) measurements were conducted under ultrahigh vacuum conditions (10-10Torr) at room temperature. UPS utilized He I photons (21.22 eV) emitted by a discharged lamp to determine the work function of the sample and the energy position of the ZnPc and Tc HOMO with respect to the Fermi level. The experimental energy resolution for UPS is typically 0.10 eV. The position of the Si valence band maximum (EV), hidden by the organic and AlOx overlayers in UPS, was determined from the position of the Si 2p core level following the Kraut method . XPS was performed using non- monochromatized Al Kα X-rays (1486.70 eV). The Fermi level reference for all measurements was determined on a clean Au surface. Device measurements The current density–voltage curve of the fabricated solar cells was measured using a Newport Orel class A solar simulator (Model 91159) under AM 1.5G illumination. The incident flux was calibrated using a calibrated reference Si solar cell certified by Newport (Model 91150- KG5). The solar cells were measured from −1.0 to 1.0 V at a temperature of 25 °C in air. External quantum efficiency measurements were performed using a 150 W xenon lamp coupled to a Newport monochromator. The light output from the monochromator was mechanically chopped at a frequency of 330 Hz and the photocurrent from the device was measured through a lock-in amplifier. The light input intensity was measured using a Newport photodetector, responsivity calibrated by Newport. The surface morphology of the solar cells was characterized by SEM (Zeiss Merlin High-resolution SEM). Modeling Full details on the modeling performed to fit the differential EQE are presented in the Supplementary Text. A transfer-matrix method was used to simulate the absorption of light through the device stack. The fits were performed using custom MATLAB code. Tetracene and zinc phthalocyanine calculations The triplet excited state energies and the highest occupied molecular orbital (HOMO) energies for tetracene (Tc) and zinc phthalocyanine (ZnPc) molecules are calculated using several methods with Q-Chem 5.4 . The structures of the molecules are optimized with the standard hybrid PBE0 functional and def2-TZVP basis set in gas phase . The PBE0 functional is used and compared to tuned range-separated functionals, LRC- ^PBE, to better evaluate the molecular orbital energies. These functionals are tuned uniquely for each molecule per Koopman’s theorem to ensure consistency between ionization and frontier orbital energies . This tuning matches the ionization energy for the ground and anionic states to each’s negative HOMO energy (Eq.1). ^(^+)− ^(^)= −^(^^^^^) (1)These functionals are tuned for gas phase molecules without solvent. Time-dependent density functional theory (TDDFT) with the Tann-Dancoff Approximation (TDA) is used to examine the excited triplets for the molecules. This method is shown, and in this case proven, to be less susceptible to triplet instability issues than TDDFT . ΔSCF energies are also calculated for the triplet excitations on both molecules for comparison. The calculations are performed with and without implicit polarizable continuum model solvent in the integral equation formalism (IEF-PCM) . The IEF-PCM solvent is given a weak dielectric of 3.0 to roughly simulate molecules in a thin, organic film, as in the experimental solar cell. To the best of Applicant’s knowledge, the dielectric constants for these films are not reported, so a conservative constant is used in the lower range for pentacene and other similar systems . Regardless, changing this constant has little influence on the results. The TDA triplet, ΔSCF triplet, ground state HOMO, and ionization energies for each functional for both molecules without IER-PCM solvent are given in eV in Table 3. The same data, with IEF-PCM solvent correction, is given in Table 4. Table 3. TDA triplet, ΔSCF triplet, ground state HOMO, and ionization energies for each functional for both molecules without IER-PCM solvent, given in eV Table 4. TDA triplet, ΔSCF triplet, ground state HOMO, and ionization energies for each functional for both molecules with IER-PCM solvent correction, given in eV. Here, the tuned functionals for each molecule show agreement between the ionization energy and HOMO energy levels, so these functionals are used to approximate the HOMO energy delta between Tc and ZnPc. LRC- ^PBE207 for Tc yielded an ionization energy of 6.7 eV, while LRC- ^PBE156gave an ionization energy of 6.3 eV for ZnPc. These are in good agreement with established experimental values for the gas phase molecules . In applying IEF-PCM corrections, the aim is to better simulate the molecules in a thin film rather than in the gas phase. The ionization energy is taken to be the ground state HOMO for each of the molecules, which is a better proxy for the frontier orbital energies and orderingwith solventcorrections. Using these ionization energies for tetracene with LRC- ^PBE207(5.7 eV) and ZnPc with LRC- ^PBE156 (5.5 eV), the difference in the HOMOenergies is estimated to beapproximately 0.2 eV. This deeper Tc HOMO level agrees with experimental XPS data and confirms the molecular difference and ordering, even when the compounds are not deposited on the silicon cell. It is also found that the triplet energies are affected little by the IEF-PCM corrections from the TDA and ΔSCF calculations. It is estimated that, through this survey of methods, thetetraceneT1energy is about 1.4 eV, while the ZnPc T1energy is about 1.2 eV. Again, thisaligns withexperimental values and relative ordering for the two molecules within errors of density functional theory. Ultraviolet and X-ray photoelectron spectroscopy (UPS & XPS) measurements UPS and XPS are used to determine the energy alignments of Tc / ZnPc / AlOx / Si. The energy difference between the Si2p core level (ESi2p3 / 2) and the valence band edge (Ev) is calibrated using an argon-ion sputtered H-passivated Si surface. UPS measures Ev(Si) located at 0.4 eV below the Fermi level (EF), and XPS measures ESi2p3 / 2(Si) at 99.35 eV below EF, which gives ESi2p3 / 2(Si) - Ev(Si) = 99.35 – 0.4 = 98.95 eV. This energy difference is comparable to values in literature (40). Therefore, for n+-doped c-Si, Ev is at 99.91 eV – 98.95 eV = 0.96 eV below EF, and for p+-doped c-Si, at 98.95 eV – 98.95 eV ~ 0 eV, withinexperimental resolution atthe Fermi level.Optical modeling and tetracene sensitization efficiency calculations The absorption of light by each of the layers in the complete device stack and the total reflection is simulated using the transfer matrix method^^. The optical absorption of each layer in theTc / ZnPc / n^ − p device is calculated for a stack with 30 nm of tetracene ^^^^^^,^^^^^^, 1.5 nmof zinc phthalocyanine ^^^^ / 0,^^^^^^. As the control, the optical absorption is also calculated in each layer of an unsensitized n^-p device comprising 1 nm of Al^O^^Abs'()*+,^^^^^, and 180. m of silicon To obtain the efficiency of tetracene sensitization, the percentage differential externalquantum efficiency ( EQE)5△ ^7^ / ^7^^) that results from coupling to tetracene is analyzed.89:9= 9:9=>?9:9; is defined, where ^7^^ is the silicon cell EQE before Tc and ZnPcdeposition and ^7^^^is the silicon cell EQE after Tc and ZnPc deposition. Table 5. Fitted tetracene sensitization efficiency values for each microwire device structure investigated herein. Microwire cells are especially effective at absorbing incident light^^. Consequently, it is assumed that total device reflection losses are negligible in the microwire cells such that device EQEs are approximately equivalent to the device internal quantum efficiencies (IQEs): 89:99:9;≈△D:9D:9;with the subscripts as defined previously. It is assumed E7^^can be described by: where G30,^^^^is the internal quantum efficiency of the silicon without the deposited organic layers and H / 0,^^^^is the simulated fractional absorption of the silicon layer relative tothe total device stack absorption without the deposited organic layers, H IJ3KL=>M; / 0,^^^^ = ∑IJ3O,=>M;. Alloptical absorption simulations are performed in a planar geometry using optical constants experimentally determined in the planar geometry. Next, it is assumed that E7^^^can be described by: where is the internal quantum efficiency of the silicon with the deposited organic layers, G^^is the tetracene sensitization efficiency (ranging from 0 to 200%, encompassing efficiency of singlet fission, triplet exciton transport, triplet exciton transfer, and extraction of transferred carriers to silicon), H / 0,^^^^^and H^^,^^^^^are the simulated fractional absorption of the silicon and tetracene layers, respectively. The tetracene contribution to the IQE is treated as a separate additional term, because the extraction of carriers absorbed by the silicon cell directly is expected to differ from the extraction of transferred carriers from tetracene. This gives the following expression: To evaluate the relative effect of adding the organic layers to the device stack, G / 0,^^^^=1. Then, to obtain a lower bound for G^^, it was also assumed G / 0,^^^^^ = 520 nm) = 1 (i.e.that the deposition of organic layers does not affect the passivation quality of the siliconsurface). Finally, G^^ is fit at F = 520 nm. The simulated △9:95W)9:9;5W) is presented for different G^^values above. An optimal fit for G^^ = 138% was obtained. As noted in the Materials andMethods section, the material optical constants and experimental thickness calibrations are obtained from ellipsometry measurements performed on planar substrates. Consequently, the true area density of ZnPc ( 1.5 nm nominal thickness) and Tc ( 30 nm nominal thickness) in the microwire devices is substantially lower, leading to an overestimate of H^^,^^^^^and an interpretation of fits for G^^as a lower bound. A similar analysis can be carried out for the other microwire device structures that are studied in this work. Table 5 summarizes the obtained fit parameters for G^^in different device structures. Uncertainty ranges are calculated from the maximum and minimum fit values for G^^across the tetracene absorption region ( F = 415 − 545 nm ).It is observed that the assumption of a wavelength-independent internal quantumefficiency for silicon only yields good fits for the n^ − pSiMW51 nmAlOb) devices. Allowing to vary results in the following values reduction in silicon quantum yield at shorter wavelengths is consistent with a deterioration in silicon passivation. This suggests that adding the organic layers may degrade the passivation quality for the devices that do not show transfer. EXAMPLE 3 The following example relates to interfacial engineering for triplet exciton sensitization of silicon photovoltaics. Thermalization is the main source of losses in silicon solar cells. Singlet fission can be used to reduce thermalization losses, but it is difficult to directly transfer triplet excitons to silicon. A passivation layer such as HfOxNy enables triplet exciton sensitization of silicon. There are various pathways through which triplets can be transferred from tetracene to silicon, for example, Dexter transfer and charge transfer. Samples with a HfOx interlayer show different characteristics from HfOxNy. To rationally design an interface that enables triplet transfer from Tc to Si, some components and characteristics of the CT-state- mediated transfer-based interface are: coupling layer (energetically favorable CT-state formation and passivation layer (thin, chemically passivate Si surface defects). Quantum efficiency spectra can reveal information about the triplet transfer efficiency (tetracene absorption region showing peaks). A demonstration of silicon photocurrent enhancement from singlet exciton fission is shown via photoluminescence studies (tetracene absorption peaks in silicon photoluminescence), photovoltaic device design (microwire solar cells are a great platform for probing singlet fission sensitization), and external quantum efficiency spectra. Triplet-charge annihilation could explain the magnetic field effect shape. Characteristic sharp rise at low magnetic fields, instead of inflection-type shape for SF. d^eImonotonically decreases with increased magnetic field. Number of intermediate TC state with spin character of charge (doublet) determines overall rate of TCA While several embodiments of the present invention have been described and illustrated herein, those of ordinary skill in the art will readily envision a variety of other means and / or structures for performing the functions and / or obtaining the results and / or one or more of the advantages described herein, and each of such variations and / or modifications is deemed to be within the scope of the present invention. More generally, those skilled in the art will readily appreciate that all parameters, dimensions, materials, and configurations described herein are meant to be exemplary and that the actual parameters, dimensions, materials, and / or configurations will depend upon the specific application or applications for which the teachings of the present invention is / are used. Those skilled in the art will recognize, or be able to ascertain using no more than routine experimentation, many equivalents to the specific embodiments of the invention described herein. It is, therefore, to be understood that the foregoing embodiments are presented by way of example only and that, within the scope of the appended claims and equivalents thereto, the invention may be practiced otherwise than as specifically described and claimed. The present invention is directed to each individual feature, system, article, material, and / or method described herein. In addition, any combination of two or more such features, systems, articles, materials, and / or methods, if such features, systems, articles, materials, and / or methods are not mutually inconsistent, is included within the scope of the present invention. The indefinite articles “a” and “an,” as used herein in the specification and in the claims, unless clearly indicated to the contrary, should be understood to mean “at least one.” The phrase “and / or,” as used herein in the specification and in the claims, should be understood to mean “either or both” of the elements so conjoined, i.e., elements that are conjunctively present in some cases and disjunctively present in other cases. Other elements may optionally be present other than the elements specifically identified by the “and / or” clause, whether related or unrelated to those elements specifically identified unless clearly indicated to the contrary. Thus, as a non-limiting example, a reference to “A and / or B,” when used in conjunction with open-ended language such as “comprising” can refer, in one embodiment, to A without B (optionally including elements other than B); in another embodiment, to B without A (optionally including elements other than A); in yet another embodiment, to both A and B (optionally including other elements); etc. As used herein in the specification and in the claims, “or” should be understood to have the same meaning as “and / or” as defined above. For example, when separating items in a list, “or” or “and / or” shall be interpreted as being inclusive, i.e., the inclusion of at least one, but also including more than one, of a number or list of elements, and, optionally, additional unlisted items. Only terms clearly indicated to the contrary, such as “only one of” or “exactly one of,” or, when used in the claims, “consisting of,” will refer to the inclusion of exactly one element of a number or list of elements. In general, the term “or” as used herein shall only be interpreted as indicating exclusive alternatives (i.e. “one or the other but not both”) when preceded by terms of exclusivity, such as “either,” “one of,” “only one of,” or “exactly one of.” “Consisting essentially of,” when used in the claims, shall have its ordinary meaning as used in the field of patent law. As used herein in the specification and in the claims, the phrase “at least one,” in reference to a list of one or more elements, should be understood to mean at least one element selected from any one or more of the elements in the list of elements, but not necessarily including at least one of each and every element specifically listed within the list of elements and not excluding any combinations of elements in the list of elements. This definition also allows that elements may optionally be present other than the elements specifically identified within the list of elements to which the phrase “at least one” refers, whether related or unrelated to those elements specifically identified. Thus, as a non-limiting example, “at least one of A and B” (or, equivalently, “at least one of A or B,” or, equivalently “at least one of A and / or B”) can refer, in one embodiment, to at least one, optionally including more than one, A, with no B present (and optionally including elements other than B); in another embodiment, to at least one, optionally including more than one, B, with no A present (and optionally including elements other than A); in yet another embodiment, to at least one, optionally including more than one, A, and at least one, optionally including more than one, B (and optionally including other elements); etc. As used herein, “wt%” is an abbreviation of weight percentage. As used herein, “at%” is an abbreviation of atomic percentage. Some embodiments may be embodied as a method, of which various examples have been described. The acts performed as part of the methods may be ordered in any suitable way. Accordingly, embodiments may be constructed in which acts are performed in an order different than illustrated, which may include different (e.g., more or less) acts than those that are described, and / or that may involve performing some acts simultaneously, even though the acts are shown as being performed sequentially in the embodiments specifically described above. Use of ordinal terms such as “first,” “second,” “third,” etc., in the claims to modify a claim element does not by itself connote any priority, precedence, or order of one claim element over another or the temporal order in which acts of a method are performed, but are used merely as labels to distinguish one claim element having a certain name from another element having a same name (but for use of the ordinal term) to distinguish the claim elements. In the claims, as well as in the specification above, all transitional phrases such as “comprising,” “including,” “carrying,” “having,” “containing,” “involving,” “holding,” and the like are to be understood to be open-ended, i.e., to mean including but not limited to. Only the transitional phrases “consisting of” and “consisting essentially of” shall be closed or semi- closed transitional phrases, respectively, as set forth in the United States Patent Office Manual of Patent Examining Procedures, Section 2111.03.
Claims
CLAIMS What is claimed is:
1. A device comprising: a singlet fission layer; an organic semiconductor layer; a passivation layer; and a base semiconductor; wherein the organic semiconductor layer is between the singlet fission layer and the passivation layer, and wherein the passivation layer is between the organic semiconductor layer and the base semiconductor.
2. A device comprising: a. a singlet fission layer; b. an electron donating layer or an electron accepting layer; c. a passivation layer; d. an n-type emitter layer or a p-type emitter layer; and e. a p-type base layer or an n-type base layer; wherein the electron donating layer or the electron accepting layer is between the outer singlet fission layer and the passivation layer, and wherein the passivation layer is between the electron donating layer or the electron accepting layer and the n-type emitter layer or the p-type emitter layer.
3. A method comprising: exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons; transferring, to a semiconductor, either an electron or a hole, without simultaneously transferring the other to the semiconductor thereby creating current in the semiconductor.
4. A method comprising: exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons; transferring, to a photovoltaic material, either an electron or a hole, without simultaneously transferring the other to the photovoltaic material thereby increasing the photoconversion efficiency of the photovoltaic material.
5. A method comprising: exposing a singlet fission material to electromagnetic radiation under conditions causing formation of triplet excitons; transferring at least some triplet excitons to a semiconductor; transferring electrons or holes to a base semiconductor thereby creating current in the base semiconductor from the formation of triplet excitons.
6. The method of any of the preceding claims, further comprising generating an electron or a hole in the photovoltaic material from the singlet fission material.
7. The device of any of the preceding claims, wherein the n-type emitter layer or the p- type emitter layer and / or the p-type base or the n-type base comprises an inorganic semiconductor.
8. The device of any of the preceding claims, wherein the device is configured to provide efficient charge carrier extraction from triplet excitons in the singlet fission layer to the inorganic semiconductor.
9. The device of any of the preceding claims, wherein the device comprises a diffusion length of less than or equal to 100 μm.
10. The device of any of the preceding claims, wherein the device comprises a vertical junction.
11. The device of any of the preceding claims, wherein the device comprises radial junctions.
12. The device of any of the preceding claims, wherein the device is configured to enhance absorption of light.
13. The device of any of the preceding claims, wherein the singlet fission layer is configured to enhance absorption of light.
14. The device of any of the preceding claims, wherein the electromagnetic radiation comprises a wavelength range from 300-1100 nm.
15. The device of any of the preceding claims, wherein the device comprises a multiplicity of microwires, wherein each microwire is 5-100 µm in length, 1-10 µm in diameter at its base, and spaced 1-10 µm from its neighbor.
16. The device of any of the preceding claims, wherein the singlet fission layer comprises a compound selected from tetracene, pentacene, tetracene-derivatives, diphenyltetracene, 5,12-bis((triisopropylsilyl)ethynyl)tetracene, anthracene-derivatives, 9,10-dicyanoanthracene, perylene diimide, perylene diimide derivatives, indigo derivatives, and aza-cibalackrot.
17. The device of any of the preceding claims, wherein the electron donating layer comprises a compound selected from zinc phthalocyanine, phthalocyanines, copper phthalocyanine, and regioregular poly(3-hexylthiophene-2,5-diyl) (P3HT).
18. The device of any of the preceding claims, wherein the electron accepting layer comprises a compound selected from C60, fullerene derivatives,[6,6] phenyl-C61- butyric acid methyl ester (PCBM), and 2,2'-[[12,13-bis(2-ethylhexyl)-12,13-dihydro- 3,9-diundecylbisthieno[2",3":4',5']thieno[2',3':4,5]pyrrolo[3,2-e:2',3'- g][2,1,3]benzothiadiazole-2,10-diyl]bis[methylidyne(5,6-difluoro-3-oxo-lH-indene- 2,1(3H)- diylidene)]]bis[propanedinitrile] (BTP-4F) (Y6).
19. The device of any of the preceding claims, wherein the thickness of the electron accepting layer and / or electron donating layer is greater than or equal to 0.1 nm and less than or equal to 100 nm.
20. The device of any of the preceding claims, wherein the passivation layer comprises a compound selected from Al2O3, HfO2, SiO2, Si3N4, and a-Si.
21. The device of any of the preceding claims, wherein the passivation layer comprises a compound selected from ZrO^ or HfO^N^, where x is greater than or equal to 0 and less than or equal to 2 and y is greater than or equal to 0 and less than or equal to 2 22. The device of any of the preceding claims, wherein the passivation layer comprises a ferroelectric layer.
23. The device of any of the preceding claims, where the thickness of the passivation later is greater than or equal to 0.01 nm and less than or equal to 10 nm.
24. The device of any of the preceding claims, wherein the emitter layer comprises n- doped silicon or p-doped silicon.
25. The device of any of the preceding claims, where the doping concentration of the silicon emitter layer varies from most concentrated at the surface of the layer, to least concentrated at the bottom of the layer.
26. The device of any of the preceding claims, wherein the base layer comprises a compound selected from p-doped silicon and n-doped silicon.
27. The device of any of the preceding claims, wherein the device generates at least one electron per incident photon.
28. The device of any of the preceding claims, wherein the microwires are tapered, wherein the diameter gradually increases from top to bottom.
29. The device of any of the preceding claims, wherein the effective refractive index (n) of the tapered microwire gradually transitions from the air's index (1) to that of the c- Si substrate (~4).
30. The device of any of the preceding claims, wherein the base semiconductor is a silicon semiconductor.
31. A photovoltaic device comprising the device of any one of the preceding claims.
32. A photodetector comprising the device of any one of the preceding claims.
Citation Information
Patent Citations
Excitonic energy transfer to increase inorganic solar cell efficiency
US20190259970A1
Interlayers for charge transfer-mediated triplet exciton transfer from a singlet exciton fission material to an inorganic semiconductor