Solar cell panel
The solar panel design with distinct light-absorbing and non-absorbing regions in the inspection area addresses visibility issues, enhancing alignment and recognition, thus improving processing accuracy and speed.
Patent Information
- Application Number
- PCT/JP2026/017706
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-08
- Filing Date
- 2026-05-08
- Publication Date
- 2026-11-12
AI Technical Summary
The visibility of inspection areas in solar panel manufacturing processes is compromised due to uneven film formation, leading to false detections and reduced productivity and processing accuracy.
A solar panel design with an inspection area comprising a first region containing anions and cations from the semiconductor layer and a second region with a thinner layer of the same material, differentiated by light absorption characteristics, allowing clear visual distinction and improved recognition using selective laser processing.
Enhances processing accuracy and production speed by ensuring easy alignment and identification of inspection areas, thereby improving overall productivity.
Smart Images

Figure JP2026017706_12112026_PF_FP_ABST
Abstract
Description
Solar panels
[0001] This disclosure relates to solar panels.
[0002] As a form of solar cell panel, for example, a solar cell with alignment marks, as described in Patent Document 1, has been proposed.
[0003] Japanese Patent Publication No. 2018-56213
[0004] In the manufacturing process of solar panels, inspection areas such as alignment marks created on the substrate at the initial stage of the manufacturing process are used to guarantee the processing accuracy of each subsequent manufacturing process.
[0005] In particular, since the area occupied by the integrated structure in a solar panel does not contribute to power generation, it is necessary to improve the processing accuracy of the integrated structure and reduce its area. For this reason, the processing accuracy and recognition accuracy of the inspection area are important.
[0006] In the manufacturing process of solar panels, it is desirable to utilize the inspection area once it has been formed in subsequent processes. In Patent Document 1, errors such as tilt are corrected using the previously formed inspection area, and a new inspection area is formed again, which leads to a decrease in productivity and processing accuracy.
[0007] However, in subsequent processes after the formation of the inspection area, such as semiconductor deposition or coating processes, uneven film formation can occur. In such cases, the uneven film may overlap with the inspection area, making it difficult to verify the inspection area. This can lead to frequent false detections and retries when performing alignment image inspection on the inspection area, resulting in reduced production speed and decreased processing accuracy in subsequent processes.
[0008] Therefore, in the manufacturing process of solar panels, it is necessary to design inspection areas that can be clearly verified even in subsequent processes after the formation of the inspection area.
[0009] Therefore, this disclosure provides a solar panel that can be aligned using an easily identifiable inspection area, and further improves processing accuracy and production speed in the manufacturing of solar panels.
[0010] The solar cell panel of this disclosure comprises: a substrate; a solar cell disposed on a first surface of the substrate and comprising a first conductive film and a semiconductor layer including a colored layer; and an inspection area disposed on the first surface of the substrate, wherein in the solar cell, the first conductive film and the semiconductor layer are stacked in this order from the substrate side; the inspection area comprises: a first region comprising a first layer comprising at least one anion contained in the semiconductor layer and at least one cation contained in the semiconductor layer; and a second region disposed between the first layer and the solar cell in a plan view, wherein the second region comprises a second layer having a smaller thickness in the stacking direction than the first layer and containing the same material as the first layer, or does not comprise the second layer. Here, the stacking direction means the direction in which the first conductive film and the semiconductor layer are stacked, and the plan view means the view of the solar cell panel along the stacking direction.
[0011] According to this disclosure, it is possible to provide a solar panel that can be aligned using an easily identifiable inspection area, thereby improving processing accuracy and production speed in the manufacturing of solar panels.
[0012] Figure 1 is a plan view showing the schematic configuration of a solar cell panel in Embodiment 1. Figure 2 is a cross-sectional view of the solar cell in the solar cell panel of Figure 1 along line A-A. Figure 3 is an enlarged plan view showing an example of an inspection area in the solar cell panel of Figure 1. Figure 4A is an example of a cross-sectional view of the inspection area in Figure 3 along line B-B. Figure 4B is a modified example of the cross-sectional view of the inspection area in Figure 3 along line B-B. Figure 5 is an enlarged plan view showing a modified example of an inspection area in the solar cell panel of Figure 1. Figure 6A is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6B is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6C is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6D is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6E is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6F is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 6G is a schematic process cross-sectional view showing the manufacturing method of the solar cell panel in Embodiment 1. Figure 7 is a cross-sectional view showing the first region of a solar cell in a solar panel in Embodiment 2. Figure 8 is a plan view showing the schematic configuration of a solar panel in an additional embodiment, corresponding to the plan view of Figure 1. Figure 9A is a schematic process cross-sectional view showing a method for forming both the power generation region and the inspection region. Figure 9B is a schematic process cross-sectional view showing a method for forming both the power generation region and the inspection region. Figure 9C is a schematic process cross-sectional view showing a method for forming both the power generation region and the inspection region. Figure 9D is a schematic process cross-sectional view showing a method for forming the power generation region. Figure 9E is a schematic process cross-sectional view showing a method for forming the power generation region. Figure 9F is a schematic process cross-sectional view showing a method for forming the power generation region. Figure 9G is a schematic process cross-sectional view showing a method for forming the power generation region. Figure 10 is a plan view and cross-sectional view illustrating the mark formation process of the mark region. Figure 11 is a flowchart of the alignment method when using a laser processing device. Figure 12 is a diagram showing the correction of misalignment by alignment marks.Figures 13(a) to 13(d) are plan views showing the manufacturing process of the laminated structure in Embodiment 3, and cross-sectional views along the line D-D in the plan view, respectively. Figures 14(a) to 14(d) are plan views showing the manufacturing process of the alignment marks in Embodiment 4, and cross-sectional views along the line E-E in the plan view, respectively.
[0013] (Knowledge leading to one aspect of this disclosure) In studying the fabrication process of perovskite solar cells, the inventors found that the following problems arise.
[0014] In perovskite solar cells, an inspection area is formed by removing the transparent conductive film on the glass substrate. In subsequent fabrication processes, alignment can be performed using this inspection area—that is, the area where the glass substrate is exposed or where the transparent conductive film is thin—as a reference. Since such an inspection area can be identified by the difference in surface irregularities, refractive index differences, and light absorption differences between areas with and without the transparent conductive film, it is effective in the manufacturing of solar cell panels using glass substrates.
[0015] However, if a film deposition process, such as a semiconductor layer, occurs after the formation of the inspection area, the superimposed film on the inspection area reduces its visibility. This is thought to be due to the reduction in the optical difference between areas with and without the aforementioned transparent conductive film, as well as noise caused by localized mottling of the deposited film.
[0016] Therefore, the inventors focused on the differences in the light absorption characteristics of solar cell materials and devised the following novel inspection area formation process using selective laser processing technology.
[0017] First, an inspection area is formed by removing a transparent conductive film deposited on the substrate. Next, a semiconductor layer is deposited on the inspection area, superimposing the inspection area and the deposited film. Then, the inspection area and its surroundings are irradiated with a laser having a wavelength of light that has low absorption in the semiconductor layer and high absorption in the transparent conductive film. At this time, the transparent conductive film absorbs the laser light around the inspection area, so the transparent conductive film and the semiconductor layer on the transparent conductive film are removed simultaneously. On the other hand, the components of the inspection area are not processed because they have low laser light absorption and remain on the substrate. Here, in this specification, a high laser light absorption rate for a certain layer or film means that the laser light absorption rate is 10% or more, although this depends on the state of the layer or film and the output of the laser light. Also, in this specification, a low laser light absorption rate for a certain layer or film means that the laser light absorption rate is 1% or less, although this depends on the state of the layer or film and the output of the laser light, and the absorption rate may be almost 0%.
[0018] The inspection area formed by this method clearly distinguishes from the surrounding areas where the substrate is exposed and where the thickness of the transparent conductive film and semiconductor layer has been reduced by laser processing, making recognition accurate and easy. From this, we have come to the realization that the above-described novel inspection area formation process can improve the productivity of solar panel manufacturing.
[0019] This disclosure provides a solar cell panel having highly visible alignment marks formed on a substrate using semiconductors.
[0020] The following is an overview of one aspect of this disclosure.
[0021] A solar cell panel in one aspect of the present disclosure comprises a substrate, a solar cell disposed on a first surface of the substrate and including a first conductive film and a semiconductor layer including a colored layer, and an inspection area disposed on the first surface of the substrate. In the solar cell, the first conductive film and the semiconductor layer are stacked in this order from the substrate side. The inspection area includes a first region comprising a first layer containing at least one anion and at least one cation contained in the semiconductor layer, and a second region disposed between the first layer and the solar cell in a plan view. The second region comprises a second layer having a smaller thickness in the stacking direction than the first layer and containing the same material as the first layer, or it does not comprise such a second layer.
[0022] With the above configuration, a clear visual difference is created between the first and second inspection areas, improving the recognition of the inspection area by, for example, an image inspection machine. Therefore, a solar panel in one embodiment of the present disclosure can be aligned using such easily identifiable inspection areas. As a result, a solar panel in one embodiment of the present disclosure can improve processing accuracy and production speed in manufacturing, thereby improving productivity.
[0023] Embodiments of the present disclosure will be described below with reference to the drawings.
[0024] (Embodiment 1) Figure 1 is a plan view showing the schematic configuration of the solar cell panel 1000 in Embodiment 1. Figure 2 is a cross-sectional view of the solar cell in the solar cell panel of Figure 1 along line A-A.
[0025] As shown in Figure 1, the solar cell panel 1000 in Embodiment 1 comprises a substrate 100, and solar cells 110 and an inspection area 140 arranged on a first surface 100a of the substrate 100. A portion of the solar cells 110 is in contact with the substrate 100, for example, as shown in Figure 2.
[0026] As shown in Figure 2, the solar battery cell 110 includes a first conductive film 210 and a semiconductor layer 220. The first conductive film 210 and the semiconductor layer 220 are stacked in this order from the substrate 100 side. The semiconductor layer 220 includes a colored layer. The semiconductor layer 220 may include, for example, an electron transport layer, a photoelectric conversion layer, and a hole transport layer arranged in order from the first conductive film 210 side. In this case, for example, the photoelectric conversion layer corresponds to the aforementioned colored layer. When the solar battery cell 110 uses, for example, a perovskite compound as the photoelectric conversion material, the photoelectric conversion layer, that is, the colored layer, contains the perovskite compound. Note that the stacking order of each layer in the semiconductor layer 220 is not limited to the above example, and the hole transport layer, the photoelectric conversion layer, and the electron transport layer may be arranged in this order from the first conductive film 210 side. The solar battery cell 110 may further include a second conductive film 230 disposed on the semiconductor layer 220.
[0027] Note that in this specification, the direction in which the first conductive film 210 and the semiconductor layer 220 are stacked is referred to as the "stacking direction", and the state when the solar battery panel 1000 and each constituent element included in the solar battery panel 1000 are viewed along the stacking direction is referred to as "plan view".
[0028] Figure 3 is an enlarged plan view showing an example of the inspection region 140 in the solar battery panel 1000 of Figure 1. FIG. 4A is an example of a cross-sectional view taken along line B-B in the inspection region 140 of FIG. 3. FIG. 4B is a modified example of the cross-sectional view taken along line B-B in the inspection region 140 of FIG. 3. Although FIG. 3 is a plan view, hatching is applied to the first region 310 to make the drawing easier to read regarding the shapes and arrangements of the first region 310 and the second region 320. The inspection region 140 will be described with reference to FIGS. 1 and 2, and FIGS. 3, 4A, and 4B showing examples of the inspection region 140.
[0029] The inspection region 140 includes a first region 310 and a second region 320. A part of the inspection region 140 is in contact with the substrate 100, for example, as shown in FIGS. 4A and 4B.
[0030] The first region 310 comprises a first layer 410 containing at least one anion and at least one cation contained in the semiconductor layer 220 of the solar cell 110. For example, the first layer 410 may contain anions and cations that constitute the photoelectric conversion material contained in the semiconductor layer 220 of the solar cell 110. For example, if the semiconductor layer 220 of the solar cell 110 contains a perovskite compound as the photoelectric conversion material, the first layer 410 may contain anions and cations that constitute the perovskite compound. As described above, the semiconductor layer 220 includes a colored layer, and the first region 310 comprises a first layer 410 containing anions and cations contained in the semiconductor layer 220. Therefore, the first region 310, like the semiconductor layer 220, is colored (for example, appears black) because it easily absorbs light. The first layer 410 may be in contact with the first surface 100a of the substrate 100, as shown in Figure 4A.
[0031] As shown in FIG. 1, the second region 320 is disposed between the first layer 410 and the solar cell 110 in a plan view. As shown in FIG. 4A, an example of the second region 320 does not include the first layer 410, nor does it include the second layer 420 described later. Therefore, a clear visual difference in color is generated between the second region 320 and the first region 310. Note that, as in the modification example shown in FIG. 4B, the second region 320 may include the second layer 420 having a smaller thickness in the stacking direction than the first layer 410. The second layer 420 is a layer containing the same material as the first layer 410. Here, that the second layer 420 contains the same material as the first layer 410 means that when the first layer 410 contains a plurality of types of materials, the second layer 420 contains at least one of the plurality of types of materials, and when the first layer 410 is formed of one type of material, it means that the second layer 420 contains the same material as that material. Note that the same material refers to a material in which all contained elements match each other, and for example, may be a material having the same composition. The second layer 420 may be formed of a material having the same composition as the first layer 410. Hereinafter, the same applies when a certain film or layer is described as containing the same material as another film or layer. Since the second layer 420 in the second region 320 has a smaller thickness in the stacking direction than the first layer 410 in the first region 310, it hardly absorbs light and appears white. Therefore, even when the second layer 420 is provided, the second region 320 has a more whitish color than the first region 310, and a clear visual difference in color is generated from the first region 310.
[0032] The solar cell panel 1000 according to the first embodiment having the above configuration produces a clear visual difference between the first region 310 and the second region 320 of the inspection region 140, so that the recognizability of the inspection region 140 is improved. Therefore, the solar cell panel 1000 according to the first embodiment can be aligned using the inspection region 140 with higher accuracy and faster speed than in the conventional art. As a result, the solar cell panel 1000 according to the first embodiment can improve the processing accuracy and production speed in manufacturing, and thus can improve productivity.
[0033] As shown in Figure 4B, the first region 310 may further include a third layer 430 between the first layer 410 and the substrate 100, which contains the same material as the first conductive film 210 included in the solar cell 110. The third layer 430 has a thickness in the stacking direction that is smaller than, for example, the first conductive film 210 of the solar cell 110. With this configuration, the first region 310 can also be formed in the process of manufacturing the solar cell 110 using selective laser processing technology.
[0034] As shown in Figure 4B, the second region 320 may further include a fourth layer 440 between the second layer 420 and the substrate 100, which contains the same material as the first conductive film 210. The fourth layer 440 has a smaller thickness in the stacking direction than the first conductive film 210 of the solar cell 110. With this configuration, the second region 320 can also be formed in the process of manufacturing the solar cell 110 using selective laser processing technology.
[0035] As shown in Figure 1, the inspection area 140 may be located outside the area on the first conductive film 210 of the solar cell 110 where the semiconductor layer 220 is laminated, in a plan view. "Outside" refers to the outer edge of the solar panel 1000 in a plan view. The inspection area 140 may be located outside the area of the solar cell 110 and spaced apart from the area of the solar cell 110 in a plan view. By arranging the inspection area 140 in the above-described positional relationship with the solar cell 110, manufacturing defects such as changes in shape due to laser processing for the manufacture of the solar cell 110 become less likely, and a highly identifiable inspection area 140 can be obtained.
[0036] The inspection area 140 has a portion that protrudes in the stacking direction relative to the position of the first surface 100a of the substrate 100, as shown in Figures 4A and 4B. With this configuration, the solar cell panel 1000 in Embodiment 1 can further improve the visibility of the inspection area 140.
[0037] The solar cell panel 1000 in Embodiment 1 may further include a collector electrode 120, as shown in Figure 1.
[0038] The solar cell 110 is electrically connected to the collector electrode 120. As shown in Figure 1, a portion of the solar cell 110 may be in contact with the collector electrode 120. For example, the solar panel 1000 may further include a current collection region to which the collector electrode 120 is electrically connected to a first conductive film 210 that does not have a semiconductor layer 220 laminated on it. For example, the first conductive film 210 may have an exposed surface portion that is not laminated on the semiconductor layer 220, and the collector electrode 120 may be connected to this surface portion as the current collection region. In this case, the inspection region 140 is positioned outside the area in the current collection region where the collector electrode 120 is located. With this configuration, the inspection region 140 is processed by laser processing that exposes the first conductive film 210 connected to the collector electrode 120, making it less likely for manufacturing defects such as changes in shape to occur and a highly identifiable inspection region 140 can be obtained.
[0039] The solar cell 110 and the inspection area 140 are, for example, not electrically connected. To realize such a configuration, for example, the solar panel 1000 in Embodiment 1 may further include an insulating area 130, as shown in Figure 1. The insulating area 130 is provided, in a plan view, for example, between the solar cell 110 and the inspection area 140, as shown in Figure 1. The insulating area 130 includes, for example, a portion where the first conductive film 210 is not provided. This configuration makes it possible to reduce the area occupied by the insulating area 130 and the inspection area 140 on the solar panel 1000, and to efficiently improve the power generation area.
[0040] The shapes of the first region 310 and the second region 320 in the inspection region 140 are not limited to a shape in which two linear bodies have one intersection point in a plan view, such as the cross mark shown in Figure 3, but may have other shapes.
[0041] For example, the first layer 410 of the first region 310 in the inspection region 140 may have a shape that includes at least one intersection point of two or more linear bodies in a plan view.
[0042] The first layer 410 of the first region 310 in the inspection region 140 may have a grid-like shape and arrow shapes in a plan view.
[0043] Furthermore, the first layer 410 of the first region 310 in the inspection region 140 may have a closed linear shape in a plan view.
[0044] The inspection area 140 may further comprise a third area. For example, the third area may comprise a sixth layer located inside the closed linear shape described above, having a smaller thickness in the lamination direction than the first layer 410, and containing the same material as the first layer 410.
[0045] Figure 5 is an enlarged plan view showing a modified inspection area in the solar cell panel 1000 of Figure 1. The modified inspection area 500 shown in Figure 5 is an example in which the third area is provided inside the closed linear shape described above. The inspection area 500 includes a first area 510, a second area 520, and a third area 530. The first area 510 has a shape that includes at least one intersection point of two or more linear bodies and has a closed linear shape. The third area 530 is located inside the closed linear shape of the first area 510. The third area 530 may include a sixth layer (not shown) which has a smaller thickness in the stacking direction than the first layer 410 and contains the same material as the first layer 410, or it may not include a sixth layer.
[0046] With the above configuration, in addition to the visual difference between the first region 510 and the second region 520 in the inspection region 500, a visual difference also occurs between the first region 510 and the third region 530. This improves the recognition of the inspection region 500 by the image inspection machine and further improves the productivity of the solar cell panel 1000.
[0047] The following describes in detail each component of the solar cell panel 1000 of Embodiment 1.
[0048] (Substrate) The substrate 100 is, for example, a light-transmitting substrate. Examples of light-transmitting substrates include glass substrates and plastic substrates. The material of the glass substrate is not particularly limited, and various types of glass such as soda-lime silicate can be used. The substrate 100 may also be a film, particularly a plastic film. Examples of materials for the plastic substrate and plastic film include polyimide, polyethylene terephthalate, polyethylene naphthalate, and cycloolefin polymers. When the solar cell panel 1000 according to Embodiment 1 is integrated with building materials, the substrate 100 may be a glass plate for building materials such as window glass.
[0049] (First conductive film 210) The first conductive film 210 functions as an electrode for extracting current from the semiconductor layer 220. The first conductive film 210 is, for example, translucent. The first conductive film 210 contains a conductive material.
[0050] The translucent conductive material may be a metal oxide or metal nitride. Examples of such materials include: (i) titanium oxide doped with at least one selected from the group consisting of lithium, magnesium, niobium, and fluorine; (ii) gallium oxide doped with at least one selected from the group consisting of tin and silicon; (iii) gallium nitride doped with at least one selected from the group consisting of silicon and oxygen; (iv) tin oxide doped with at least one selected from the group consisting of antimony and fluorine; (v) zinc oxide doped with at least one selected from the group consisting of boron, aluminum, gallium, and indium; (vi) indium-tin composite oxide (i.e., indium tin oxide); or (vii) composites thereof.
[0051] The translucent conductive material may include at least one selected from the group consisting of indium tin oxide (ITO), fluorine-doped tin oxide (FTO), indium zinc oxide (IZO), and aluminum zinc oxide (AZO).
[0052] Furthermore, the first conductive film 210 can be formed using an opaque material with a light-transmitting pattern. Examples of light-transmitting patterns include linear, wavy, grid-like, and perforated metal-like patterns with a large number of fine through-holes arranged regularly or irregularly. When the first conductive film 210 has such patterns, light can be transmitted through areas where there is no electrode material. Examples of opaque electrode materials include platinum, gold, silver, copper, aluminum, rhodium, indium, titanium, iron, nickel, tin, zinc, or alloys containing any of these. Conductive carbon materials can also be used.
[0053] The light transmittance of the first conductive film 210 may be, for example, 50% or more, or 80% or more. The wavelength of light to be transmitted depends on the wavelength used for power generation in the semiconductor layer 220. The thickness of the first conductive film 210 is, for example, in the range of 1 nm to 2000 nm.
[0054] (Semiconductor layer 220) The semiconductor layer 220 includes a colored layer. The colored layer is, for example, a photoelectric conversion layer. The semiconductor layer 220 may further include at least one selected from the group consisting of an electron transport layer and a hole transport layer. In Embodiment 1, the semiconductor layer 220 includes, for example, an electron transport layer, a photoelectric conversion layer, and a hole transport layer.
[0055] (Electron transport layer) The electron transport layer contains an n-type semiconductor. Examples of n-type semiconductors include oxide semiconductors such as TiO2, Nb-doped TiO2, Mg-doped TiO2, SnO2, CeO2, ZnO, Zn2SnO4, Nb2O3, WO3, SrTiO3, CaTiO3, nitride semiconductors such as GaN, and phenyl C 61 Examples include fullerene derivatives such as methyl butyrate (PCBM).
[0056] Furthermore, the electron transport layer may be a semiconductor with a band gap of 3.0 eV or more and 3.8 eV or less. By forming the electron transport layer with a semiconductor with a band gap of 3.0 eV or more, visible light and infrared light can be transmitted to the photoelectric conversion layer. More specific examples can be selected from n-type semiconductors. For example, TiO2 (rutile type 3.0 eV, anatase type 3.2 eV), SnO2 (3.6 eV), Nb2O5 (3.4 eV), GaN (3.4 eV), SrTiO3 (3.2 eV), and CaTiO3 (3.4 eV) can be cited. Here, the numbers in parentheses indicate typical band gap values.
[0057] The electron transport layer may include multiple layers made of different materials and structures. For example, by making the electron transport layer a porous structure, or by placing a porous structure on the photoelectric conversion layer side of the electron transport layer, the photoelectric conversion layer can be easily formed. The material of the photoelectric conversion layer penetrates into the voids of the porous structure, and the porous structure acts as a scaffold for the photoelectric conversion layer. Therefore, the material of the photoelectric conversion layer is less likely to be repelled or aggregated on the surface of the electron transport layer having a porous structure. Thus, the photoelectric conversion layer can be easily formed as a uniform film. Examples of materials for forming the porous structure include porous bodies in which insulating or semiconductor particles are linked together. Examples of porous body particles with electron transport properties include titanium oxide, tin oxide, and niobium oxide particles. On the other hand, if porous body particles with poor electron transport properties, such as aluminum oxide or silicon oxide particles, are used, they will only function as a scaffold for forming the photoelectric conversion layer, and the effect of an electron transport layer cannot be obtained. The electron transport layer having a porous structure can be formed, for example, by coating a nanomolecular dispersion of the porous body.
[0058] The voids in the porous electron transport layer are connected from one main surface to the other. This allows the material of the photoelectric conversion layer to fill the voids in the electron transport layer.
[0059] When the electron transport layer has a porous structure, light scattering occurs, and the effect of increasing the optical path length of light passing through the photoelectric conversion layer is also expected. When the optical path length increases, the amount of electrons and holes generated in the photoelectric conversion layer is predicted to increase.
[0060] (Photoelectric Conversion Layer) The photoelectric conversion layer includes a semiconductor layer having a photoelectric conversion function. Examples of the semiconductor material contained in the photoelectric conversion layer include silicon, compound semiconductors, and perovskite compounds. Examples of silicon include single crystal silicon, polycrystalline silicon, microcrystalline silicon, and amorphous silicon. Examples of the compound semiconductor include CdTe, GaAs, and CuInGaSe.
[0061] The perovskite compound may have a composition represented by the formula ABX₃. A is a monovalent cation. Examples of monovalent cations are alkali metal cations and organic cations. Examples of alkali metal cations are Li + , Na + , K + , Cs + , and Rb + . Examples of organic cations include methylammonium cation (CH₃NH₃ + ), formamidinium cation (HC(NH₂)₂ + ), ethylammonium cation (CH₃CH₂NH₃ + ), ammonium cation (NH₄ + ), hydrazinium cation (NH₃NH₂ + ), azetidinium cation ((CH₂)₃NH₂ + ), hydroxylammonium cation (NH₃OH + ), imidazolium cation (C₃N₂H₅ + ), dimethylammonium cation ((CH₃)₂NH₂ + ), tetramethylammonium cation ((CH₃)₄N + ), thiazolium cation (C₃H₄NS + ), 3-pyrrolinium cation (NC₄H₈ + ), tropylium cation (C₇H₇ + ), and guanidinium cation (CH₆N₃+ ) etc. B is a divalent cation. An example of a divalent cation is Sn 2+ , Ge 2+ Mg 2+ Ca 2+ , Sr 2+ Ba 2+ ,Cd 2+ Fe 2+ , Pd 2+ , Eu 2+ and Pb 2+ And so on. X is a monovalent anion. Examples of monovalent anions are halogen anions. Each of the sites A, B, and X may be occupied by multiple types of ions.
[0062] The photoelectric conversion layer may contain a perovskite compound.
[0063] The thickness of the photoelectric conversion layer is, for example, between 50 nm and 10 μm. The photoelectric conversion layer can be formed using methods such as solution coating, printing, vapor deposition, and sputtering.
[0064] (Hole transport layer) The hole transport layer can efficiently move holes generated in the photoelectric conversion layer to, for example, the second conductive film 230. As a result, current can be extracted efficiently.
[0065] The hole transport layer contains a hole transport material. The hole transport material is a material that transports holes. The hole transport material may be an organic or inorganic semiconductor.
[0066] Examples of organic substances include triphenylamine, triallylamine, phenylbenzidine, phenylenevinylene, tetrathiafulvalene, vinylnaphthalene, vinylcarbazole, thiophene, aniline, pyrrole, carbazole, triptycene, fluorene, azulene, pyrene, pentacene, perylene, acridine, or phthalocyanine.
[0067] Typical examples of organic materials used as hole transport materials include 2,2',7,7'-tetrakis-(N,N-di-p-methoxyphenylamine)9,9'-spirobiflourene (hereinafter sometimes abbreviated as "spiro-OMeTAD"), poly[bis(4-phenyl)(2,4,6-trimethylphenyl)amine] (hereinafter, These are sometimes abbreviated as "PTAA"), poly(3-hexylthiophene-2,5-diyl) (hereinafter sometimes abbreviated as "P3HT"), poly(3,4-ethylenedioxythiophene) (hereinafter sometimes abbreviated as "PEDOT"), 2-(3,6-Dimethoxy-9H-carbazol-9-yl)ethyl]phosphonic Acid (hereinafter sometimes abbreviated as "MeO-2PACZ"), or copper phthalocyanine.
[0068] Inorganic semiconductors used as hole transport materials are p-type semiconductors. Examples of inorganic semiconductors include Cu₂O, CuGaO₂, CuSCN, CuI, and NiO. x MoO x These are carbon materials such as V2O5 or graphene oxide.
[0069] The hole transport layer may include multiple layers made of different materials.
[0070] The thickness of the hole transport layer may be 1 nm or more and 1000 nm or less, preferably 10 nm or more and 200 nm or less. Within this range, sufficient hole transport characteristics can be achieved and low resistance can be maintained, so that photovoltaic power generation can be performed with high efficiency.
[0071] (Second conductive film 230) The second conductive film 230 may or may not be transparent.
[0072] As the material for the second conductive film 230, the same material as the material for the first conductive film 210 may be used.
[0073] Next, the manufacturing method of the solar cell panel 1000 in Embodiment 1 will be described with reference to Figures 6A to 6G. Figures 6A to 6G are schematic cross-sectional views of the manufacturing process of the solar cell panel 1000 in Embodiment 1. These cross-sectional views show the cross-section at a position corresponding to the cross-section along line A-A in Figure 1.
[0074] The inspection area 140 can be formed simultaneously using the process for manufacturing the solar cell 110. In the following description, the P1 groove is a dividing groove formed to cut the first conductive film 210 provided on the substrate 100. The P2 groove is a dividing groove formed to cut the semiconductor layer 220 formed on the first conductive film 210 on which the P1 groove is formed. The P3 groove is a dividing groove formed to cut the second conductive film 230 and the semiconductor layer 220 formed on the semiconductor layer 220 on which the P2 groove is formed.
[0075] First, as shown in Figure 6A, a precursor layer 21p of the first conductive film 210 is formed on the substrate 100. In the illustrated example, the precursor layer 21p is, for example, an FTO film. The FTO film is formed by known film formation methods such as chemical vapor deposition or sputtering.
[0076] Next, as shown in Figure 6B, the precursor layer 21p is scribed and divided, forming an integration line and creating the first conductive film 210 (P1 groove processing). Although not shown in Figure 6B, at this time, the precursor layer 21p is removed from the region where the inspection region 140 is formed, specifically the region where the first region 310 of the inspection region 140 is formed. For removing the precursor layer 21p formed of the FTO film, for example, an IR laser or a UV laser is used.
[0077] The laser irradiation energy used to remove the precursor layer 21p in the region where the first region 310 is formed is not particularly limited. However, by using irradiation energy equivalent to or greater than that used when performing P1 groove processing, for example, the precursor layer 21p can be effectively removed, making it easier for the first layer 410 of the first region 310 to remain after the laser irradiation process to the inspection region 140 described later, thereby improving the visibility of the inspection region 140.
[0078] Furthermore, in the second region 320, the precursor layer 21p may be removed to the extent that it cannot be detected by general elemental analysis methods. That is, the second layer 420 of the second region 320 may be removed to the greatest extent possible. This increases the visual difference between the first region 310 and the second region 320, further improving the visibility of the inspection region 140.
[0079] Here, common elemental analysis techniques include, for example, energy-dispersive X-ray spectroscopy (EDX), electron microanalysis (EPMA), Auger electron spectroscopy (AES), time-of-flight secondary ion mass spectrometry (TOF-SIMS), electron energy loss spectroscopy (EELS), and X-ray photoelectron spectroscopy (XPS).
[0080] Next, as shown in Figure 6C, the precursor layer 25p of the electron transport layer, the precursor layer 26p of the photoelectric conversion layer, and the precursor layer 27p of the hole transport layer are stacked on the first conductive film 210 in this order. The precursor layers 25p, 26p, and 27p are precursor layers of the semiconductor layer 220. In the illustrated example, the precursor layer 25p of the electron transport layer is, for example, an SnO2 film, the precursor layer 26p of the photoelectric conversion layer is, for example, a perovskite film containing a perovskite compound, and the precursor layer 27p of the hole transport layer is, for example, PTAA. These layers are also formed by known film formation methods such as coating, printing, and vapor deposition.
[0081] Next, an IR laser is irradiated onto the region where the inspection region 140 is formed. This removes the precursor layer of the semiconductor layer 220 deposited on the first conductive film 210 in the region where the inspection region 140 is formed, and this region becomes the second region 320. At this time, in the second region 320, not all of the precursor layer of the semiconductor layer 220 deposited on the first conductive film 210 may be removed, but some may remain. This remaining portion of the precursor layer becomes the second layer 420 of the second region 320. The precursor layer of the semiconductor layer 220 that is deposited on top of the removed first conductive film 210 remains even when irradiated with an IR laser, and this precursor layer becomes the first layer 410 of the first region 310. In this way, an inspection region 140 is formed in which the first region 310 and the second region 320 are clearly separated.
[0082] Furthermore, in the second region 320, the precursor layer of the semiconductor layer 220 deposited on the first conductive film 210 may be removed to the extent that it cannot be detected by general elemental analysis methods. In other words, the second layer 420 of the second region 320 may be removed to the greatest extent possible. This increases the visual difference between the first region 310 and the second region 320, further improving the visibility of the inspection region 140.
[0083] While there are no particular restrictions on the irradiation energy of the IR laser irradiating the inspection area 140, it is desirable to have conditions that allow for an appropriate visual difference between the first layer 410 in the first area 310 and the second layer 420 in the second area 320. In other words, if the irradiation energy of the IR laser is increased, the damage to the first layer 410 by light and heat will increase, which may change the shape and light absorption properties of the first area 310 and reduce its visibility. On the other hand, if the irradiation energy of the IR laser is increased, most of the second layer 420 will be removed, so the visual difference between the first area 310 and the second area 320 tends to become larger. Therefore, the processing conditions with the IR laser are determined by considering the state of the first layer 410 that is to be retained and the state of the second layer 420 that is to be removed after IR irradiation.
[0084] Next, as shown in Figure 6D, the laminate of precursor layers 25p, 26p, and 27p is scribed and divided into a laminate of electron transport layer 25, photoelectric conversion layer 26, and hole transport layer 27, i.e., semiconductor layer 220 (P2 groove processing).
[0085] Next, as shown in Figure 6E, a precursor layer 23p of the second conductive film 230 is deposited on the semiconductor layer 220. In the illustrated example, the precursor layer 23p is, for example, an ITO film. The ITO film is also deposited by a known deposition method such as sputtering. The conductive material constituting the precursor layer 23p fills the P2 groove and forms an internal connection portion.
[0086] Next, as shown in Figure 6F, the precursor layer 23p is scribed and divided to form the second conductive film 230 (P3 groove processing). This P3 groove penetrates each layer 25, 26, and 27 constituting the semiconductor layer 220 in the stacking direction, forming an integration line. At this time, the collector electrode 120 is also formed. Specifically, as shown in Figure 6G, the semiconductor layer 220 on the first conductive film 210 is removed in the current collection region 120a to which the collector electrode 120 is connected, exposing the first conductive film 210, and a lead wire is attached to that portion, for example, with solder.
[0087] Subsequently, the first conductive film 210 in the edge region is removed by IR laser processing. As a result, the semiconductor layer 220 and the second conductive film 230 deposited on the first conductive film 210 in the region irradiated with the IR laser are removed, and the substrate edge and the electrode collector are insulated. At the same time, the inspection region 140 is also irradiated with the IR laser, so the second conductive film 230 (ITO film) formed on the inspection region 140 may also be removed.
[0088] Alternatively, the inspection area 140 may be formed simultaneously in the step of removing the first conductive film 210 in the edge region. For example, such a step can be used in the processing of P2 grooves or P3 grooves, when aligning with the substrate edge as a reference and forming an inspection area 140 to be used in subsequent processes after edge insulation processing. This allows both the formation of the inspection area 140 and edge insulation processing to be performed in a single step, improving productivity.
[0089] As a result, the solar cell panel 1000 according to Embodiment 1, which is equipped with an inspection area 140, can be manufactured.
[0090] The inspection area 140 may be marked with information that allows for individual identification of the substrate 100, such as the lot number, QR code (registered trademark), or barcode. This improves management efficiency and thus enhances the productivity of the solar panel 1000.
[0091] The inspection area 140 may be superimposed on the frame member of the solar cell panel 1000, so as to be hidden by the frame member when viewed from the front (i.e., perpendicular to the light-receiving surface). This can improve the aesthetic appearance.
[0092] The inspection area 140 may be surrounded by the edge region of the solar cell panel 1000. By placing the inspection area 140 within the edge region in this way, the area of the solar cell 110 can be increased, and the amount of power generated per unit area of the solar cell panel 1000 can be increased.
[0093] The thickness of the first conductive film 210 (e.g., FTO film) in the second region 320 may be thinner than that of the edge region of the solar cell panel 1000.
[0094] If the FTO film thickness of the second region 320 and the film thickness of the second layer 420 are the same as those of the edge region, the edge region is designated as the second region.
[0095] The inspection area 140 may contain two or more items of the same shape. Reducing the number of detection patterns can reduce the burden of setting the detection patterns.
[0096] The inspection area 140 may be located at two or more of the four corners of the solar panel 1000. This allows for accurate alignment.
[0097] (Embodiment 2) Figure 7 is a cross-sectional view of the first region 700 of a solar cell in a solar panel according to Embodiment 2. Descriptions that overlap with Embodiment 1 described above will be omitted as appropriate. The first region 700 comprises a substrate 100, a third layer 430, a first layer 410, and a fifth layer 710. The third layer 430 has a smaller thickness in the stacking direction than, for example, the first conductive film 210 of the solar cell 110. The first layer 410 has a larger thickness in the stacking direction than the second layer 420 of the second region 320. The fifth layer 710 contains, for example, the same material as the second conductive film 230.
[0098] With the above configuration, the reflectivity of the first region 700 of the inspection area increases, and the edge recognition between the first region 700 and the second region improves. This improves the recognition of the inspection area and increases the productivity of solar panels.
[0099] (Additional Embodiments) Additional embodiments of the present disclosure are described below. These embodiments provide a more detailed explanation of the contents of Embodiment 1, with the addition of plan views and cross-sectional views of the alignment marks (i.e., inspection areas). The alignment marks are marks formed by the first and second areas in the inspection area, and the shape of the marks corresponds to the shape of the first area. In these additional embodiments, the same reference numerals are used for the same components as in Embodiment 1, and redundant explanations are omitted.
[0100] In accordance with the process flow described in Embodiment 1 with reference to the cross-sectional process diagrams from Figures 6A to 6G, the process for forming alignment marks in the inspection area will be described with reference to the drawings.
[0101] Figure 8 is a plan view showing the schematic configuration of a solar panel in an additional embodiment, corresponding to the plan view in Figure 1. Here, the alignment marks in the inspection area are "cross-shaped". The marks do not have to be cross-shaped; other shapes, as described later, may also be used.
[0102] Referring to Figures 9A to 9G, the process for forming the inspection area (mark area) will be explained in correspondence with the process for forming the power generation area (corresponding to the solar cell in Embodiment 1). Figures 9A to 9C are schematic cross-sectional views showing the methods for forming both the power generation area and the inspection area. Figures 9D to 9G are schematic cross-sectional views showing the method for forming the power generation area. The cross-sectional views in Figures 9A to 9G show the cross-section at a position corresponding to the cross-section along line A-A in Figure 8. Note that Figures 9A to 9G correspond to the processes in Figures 6A to 6G of Embodiment 1, respectively.
[0103] As shown in Figure 9A, in the marked region, the same film as the precursor layer 21p (for example, an FTO film) is deposited simultaneously with the deposition of the precursor layer 21p of the first conductive film 210 in the power generation region. Note that the cross-sectional view of the marked region shown in Figure 9A is a cross-sectional view along the line C1-C1 in the plan view of the marked region. Below, an example in which the first conductive film 210 is formed by an FTO film will be described.
[0104] As shown in Figure 9B, when forming the "P1 groove" in the power generation region, a predetermined area of the FTO film 21p in the mark region is simultaneously removed by laser 1 (IR laser: 1064 nm), and the FTO film 210 with the opening 210a formed thereon forms a cross-shaped alignment mark (referred to as mark 1) as shown in the plan view. The predetermined area in the mark region from which the FTO film 21p is removed corresponds to the shape of the mark 1 to be formed. Note that the cross-sectional view of the mark region shown in Figure 9B is a cross-sectional view along the line C2-C2 in the plan view of the mark region. Here, the FTO film 210 in the predetermined area may not be completely removed but may remain partially. The opening 210a may be formed as a recess with a very thin bottom thickness (for example, a bottom thickness of 200 nm or less).
[0105] The mark area is, for example, a square with sides of about 10 mm. Mark 1, for example, has a long side of about 5 mm and a width of about 50 microns. The cross shape, depending on the presence or absence of the FTO film 210, functions as an alignment mark. The position information of the alignment marks is stored in the manufacturing equipment.
[0106] Next, as shown in Figure 9C, precursor layers 25p for the electron transport layer, 26p for the photoelectric conversion layer, and 27p for the hole transport layer are deposited in the power generation region. Simultaneously, precursor layers 25p, 26p, and 27p are deposited in the mark region in the same manner. As described in Embodiment 1, precursor layer 26p is a perovskite film containing, for example, a colored perovskite compound, and the deposition makes the cross-shaped alignment marks formed on the FTO film 210 difficult to see. In this state, the alignment marks are not very effective. Note that the cross-sectional view of the mark region shown in Figure 9C is a cross-sectional view along the line C3-C3 in the plan view of the mark region.
[0107] The power generation region remains in the state shown in Figure 9C, and the mark formation process for the marked region will be explained. Figure 10 is a plan view and a cross-sectional view illustrating the mark formation process for the marked region. As shown in Figure 10, the marked region is irradiated with laser 1 (IR laser). The width of the laser is approximately 0.4 mm, and the laser scanning is performed with overlap. Therefore, if the marked region is 10 mm wide, the laser is scanned approximately 30 to 40 times when forming the marked region. As a result, the film deposited on the FTO film 210 is removed, and only the film formed on the opening 210a of the FTO film 210 remains. As explained in Embodiment 1, the IR laser used as laser 1 is transparent to the perovskite film, so the perovskite film remains as is, while the FTO film 210 (tin oxide) absorbs the energy of the IR laser and is therefore removed. The laminated film on the FTO film 210 is also removed at the same time. As a result, a convex alignment mark (mark 2) can be formed that neatly reflects the cross shape formed as an opening 210a (recess) in the FTO film 210.
[0108] Here, we have described an example in which alignment marks (mark 2) are formed after the precursor layers 25p, 26p, and 27p have been deposited. However, alignment marks (mark 2) may also be formed without forming the precursor layer 27p. That is, alignment marks (mark 2) can also be formed by irradiating the laminated film of precursor layers 25p and 26p with an IR laser.
[0109] Laser 1 is irradiated from the material side of the substrate 100, rather than from the back side. This is because the laser can be directly irradiated onto the film. As a result, a colored alignment mark 2 containing a perovskite film can be formed, which protrudes in a convex shape from the substrate 100.
[0110] After aligning alignment mark 1 and alignment mark 2, that is, after aligning alignment mark 2 with the position information of mark 1 stored in the manufacturing equipment, the "P2 groove" is formed as shown in Figure 9D. Laser 2 (green laser (532 nm) or UV laser (355 nm)) is used for P2 groove processing. This is because laser 2 is the wavelength absorbed by the perovskite film. By aligning mark 1 / mark 2, the laser can be irradiated to the designed location, and the "P2 groove" can be formed to the designed location.
[0111] Next, as shown in Figure 9E, when the precursor layer 23p of the second conductive film 230 in the power generation region is formed, the same film as the precursor layer 23p (for example, an ITO film) is simultaneously deposited in the mark region. Specifically, ITO is deposited on the top and sides of the alignment mark 2, but the alignment function is not lost.
[0112] After aligning alignment mark 1 and alignment mark 2, the P3 groove is formed using laser 2 as shown in Figure 9F. This allows the laser beam to be scanned to form the P3 groove at the designed location. Although not shown, in this state (with alignment marks 1 and 2 aligned), the laser 2 can be irradiated to any desired location in the power generation area, similar to the P3 groove, to form a groove at the desired location. Because the alignment is correct, the groove can be formed at the designed location.
[0113] As shown in Figure 9G, with this alignment achieved, the same laser 2 is used to perform P4 groove machining (side removal).
[0114] (Process using processing equipment) Figure 11 is a flowchart of the alignment method when using a laser processing device. The alignment method when using a laser processing device will be explained using the flowchart in Figure 11.
[0115] As explained earlier, two types of lasers (laser 1 and laser 2) are used. Processing device A is a laser processing device with a wavelength of 1064 nm, and processing device B is a laser processing device with a wavelength of 532 nm or 355 nm. Laser 1 is used to remove the FTO film, and laser 2 is used to process films containing perovskite compounds. Laser 1 in processing device A has a wavelength that has a low absorption rate for films containing perovskite compounds and a high absorption rate for FTO films. For example, it has been reported that an infrared laser with a wavelength of 1064 nm is absorbed by FTO films with an absorption rate of about 30% to 50% (Hisashi Fujii, "Changes in transmittance due to heating of fluorine-doped tin oxide films," Kanagawa Prefectural Institute of Industrial Science and Technology Research Report (KISTEC Research Report), 2020, p.13, August 2020). On the other hand, an infrared laser with a wavelength of 1064 nm is hardly absorbed by the film containing the perovskite compound, with an absorption rate of almost 0%. Laser 2 of processing apparatus B has a wavelength at which the absorption rate of the FTO film is low and the absorption rate of the film containing the perovskite compound is high. As an example, it has been reported that a green laser with a wavelength of 532 nm or an ultraviolet laser with a wavelength of 355 nm is absorbed by the film containing the perovskite compound with an absorption rate of about 50% to 70% (Zhao, Y., et al. ACS Applied Energy Materials 2023, 6, 5217-5229). On the other hand, a green laser with a wavelength of 532 nm or an ultraviolet laser with a wavelength of 355 nm is hardly absorbed by the FTO film, with an absorption rate of almost 0%. The use of the fundamental wavelength and harmonics of the YAG laser corresponding to laser 1 is described in the literature (Japanese Patent Publication No. 2010-62373).
[0116] The substrate (module substrate) of the solar cell panel is set in processing device A (S1). Alignment marks 1 are also formed in the inspection area by processing device A in accordance with the patterning of the FTO film in the power generation area (S2). This setting is originally for setting the device for patterning the FTO film in the power generation area. Therefore, marks 1 may be formed before setting in processing device A.
[0117] The substrate is transported from processing apparatus A to the film deposition apparatus, where a multilayer film containing a perovskite film (precursor layers 25p, 26p, 27p) is formed.
[0118] After transporting the substrate back to processing device A, the inspection area (mark area) is irradiated with laser 1 and scanned. This forms mark 2 as described above (S3).
[0119] After that, the substrate is transported from processing device A to processing device B. As shown in Figure 12, alignment mark 1 and alignment mark 2 are aligned in processing device B (S4). Figure 12 is a diagram showing the correction of positional misalignment caused by the alignment marks. Once the alignment is complete, the laminated film including the perovskite film is processed in processing device B using a laser 2 with a wavelength of 532 nm or a laser 2 with a wavelength of 355 nm, which is different from that of processing device A, and the P2 groove can be formed in the designed location (S5).
[0120] Even when working across multiple devices, the highly visible alignment allows for machining in the exact location specified.
[0121] (Regarding alignment marks) Alignment mark 1 has a concave cross shape (the center is recessed), and alignment mark 2 has a convex cross shape (the center protrudes), and these marks are formed in the same location. The alignment marks in this disclosure do not form multiple alignment marks in different locations as in Patent Document 1, so the power generation area is not unnecessarily sacrificed.
[0122] When forming grooves in power generation areas such as P2 grooves, the alignment marks become convex, creating a large difference from areas without marks, resulting in extremely high visibility.
[0123] (Embodiment 3) Embodiment 3 is a method for manufacturing a laminated structure including a film containing a perovskite compound. The method for manufacturing the laminated structure in this embodiment is a method for forming a self-aligned structure by irradiating and scanning with a laser.
[0124] Figures 13(a) to 13(d) are a plan view showing the manufacturing process of the laminated structure in this embodiment, and a cross-sectional view along the line D-D in the plan view, respectively.
[0125] In this embodiment, the manufacturing method of the laminated structure is as shown in Figure 13(a), in which an FTO film 810 having an aperture 810a is deposited on a glass substrate 800 as a base film. Then, as shown in Figure 13(b), a film 820 containing a perovskite compound is formed so as to span both a first region where no base film is formed and a second region adjacent to the first region where a base film is present. The film 820 containing the perovskite compound is formed on both the FTO film 810 (second region) and the aperture 810a (first region). Next, as shown in Figure 13(c), an IR laser (wavelength 1064 nm) is irradiated onto the FTO film 810 and the film 820 containing the perovskite compound located on and around the aperture 810a. Because the IR laser has a low absorption rate for the film 820 containing the perovskite compound, while the FTO film 810 has a high absorption rate, simply irradiating it with the laser eliminates the perovskite compound film 820 in the areas where the FTO film 810 is present. As a result, as shown in Figure 13(d), a laminated structure can be formed on the glass substrate 800 in a "self-alignment" manner, in which the film 820 containing the perovskite compound is laminated in the area corresponding to the opening 810a of the FTO film 810. From the boundary between the underlying FTO film 810 and the opening 810a, a laminated structure made of film 820 can be formed in a convex shape upward from the opening 810a. This convex structure can be used as an alignment mark and can be aligned with the alignment mark made of the opening 810a of the underlying film.
[0126] (Embodiment 4) Embodiment 4 is an embodiment in which the alignment mark is circular (circle-shaped). Figures 14(a) to (d) are a plan view showing the manufacturing process of the alignment mark in this embodiment and a cross-sectional view along the line E-E in the plan view, respectively. The difference between the alignment mark in this embodiment and the alignment mark shown in Figures 9B, 9C, and 10 is whether the shape is a circle or a cross. The method for forming the alignment mark is as shown in Figures 14(a) to (d).
[0127] Thus, the shape formed on the FTO film can be freely set, thereby forming a laminated structure corresponding to the marks formed as recesses in the FTO film. Of course, the structure can be formed self-aligning simply by irradiating it with a laser. Therefore, it is also possible to make the shape of the laminated structure manufactured by the manufacturing method of Embodiment 3 the shape shown in Figure 14.
[0128] (Note) The above description of embodiments discloses the following technologies.
[0129] (Technical 1) A solar cell comprising: a substrate; a solar cell disposed on a first surface of the substrate and comprising a first conductive film and a semiconductor layer including a colored layer; and an inspection area disposed on the first surface of the substrate, wherein in the solar cell, the first conductive film and the semiconductor layer are stacked in this order from the substrate side; the inspection area comprises: a first region comprising a first layer comprising at least one anion contained in the semiconductor layer and at least one cation contained in the semiconductor layer; and a second region disposed between the first layer and the solar cell in a plan view, wherein the second region comprises a second layer having a smaller thickness in the stacking direction than the first layer and containing the same material as the first layer, or does not comprise the second layer. Here, the stacking direction means the direction in which the first conductive film and the semiconductor layer are stacked, and the plan view means the view of the solar cell along the stacking direction.
[0130] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0131] (Technology 2) The solar cell panel according to Technology 1, wherein the first region further comprises a third layer between the first layer and the substrate, the third layer having a thickness in the stacking direction smaller than that of the first conductive film of the solar cell.
[0132] This allows for the creation of inspection areas in the solar cell manufacturing process using selective laser processing technology.
[0133] (Technical 3) The solar cell panel according to Technical 2, wherein the second region further comprises a fourth layer between the second layer and the substrate, the fourth layer having a thickness in the stacking direction smaller than that of the first conductive film of the solar cell.
[0134] This allows for the creation of inspection areas in the solar cell manufacturing process using selective laser processing technology.
[0135] (Technical 4) A solar cell panel according to any one of Technical 1 to 3, wherein the inspection area is located outside, in a plan view, the area on which the semiconductor layer is laminated on the first conductive film in the solar cell. Here, "outside" means the outer edge side of the solar cell panel in a plan view.
[0136] This allows for obtaining highly identifiable inspection areas.
[0137] (Technical 5) The solar cell panel according to Technical 4, further comprising a current collection region to which a current collector is electrically connected in the first conductive film in which the semiconductor layer is not laminated, wherein the inspection region is located outside the region in the current collection region in which the current collector is present.
[0138] This configuration allows the inspection area to be processed by laser processing that exposes the first conductive film connected to the electrode collector, reducing the likelihood of manufacturing defects such as changes in shape, and resulting in a highly identifiable inspection area.
[0139] (Technical 6) The solar cell panel according to any one of Technical 1 to 5, wherein the inspection area has a portion that protrudes in the stacking direction with respect to the position of the first surface of the substrate.
[0140] This can further improve the visibility of the inspection area.
[0141] (Technical 7) The solar cell further comprises a second conductive film laminated on the semiconductor layer, and the first region further comprises a fifth layer laminated on the first layer, comprising the same material as the second conductive film, according to any one of Technical 1 to 6.
[0142] This can further improve the visibility of the inspection area.
[0143] (Technical 8) A solar panel according to any one of Technical 1 to 7, wherein the solar cell and the inspection area are not electrically connected.
[0144] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0145] (Technical 9) The solar cell panel according to Technical 8, further comprising an insulating region between the solar cell and the inspection area in the plan view, including a portion where the first conductive film is not provided.
[0146] This configuration makes it possible to reduce the area occupied by the insulation and inspection regions on the solar panel, thereby efficiently improving the power generation area.
[0147] (Technical 10) The solar cell panel according to any one of Technical 1 to 8, wherein the first layer of the first region has a shape that includes at least one intersection point of two or more linear bodies in the plan view.
[0148] This can further improve the visibility of the inspection area.
[0149] (Technical 11) The solar cell panel according to any one of Technical 1 to 10, wherein the first layer of the first region has a closed linear shape in the plan view.
[0150] This can further improve the visibility of the inspection area.
[0151] (Technical 12) The solar cell panel according to Technical 11, wherein the inspection area further comprises a third area, the third area comprising a sixth layer located inside the closed linear shape, having a smaller thickness in the stacking direction than the first layer, and containing the same material as the first layer.
[0152] This can further improve the visibility of the inspection area.
[0153] (Technical 13) A method for forming an alignment mark, comprising: (i) forming a first film having a mark-shaped opening on a substrate; (ii) forming a second film containing a perovskite compound on the first film including the opening; and (iii) irradiating the opening and the area surrounding the opening of the first and second films with a laser to form the mark-shaped second film in a self-aligned manner, wherein the laser has a wavelength such that the absorption rate of the second film is low and the absorption rate of the first film is high.
[0154] This allows for the formation of alignment marks in a simple manner, which can further improve the visibility of the inspection area of solar panels.
[0155] (Technical 14) The method for forming an alignment mark according to Technical 13, wherein the opening formed in the first film in (i) is a recessed mark, and the second film with the mark shape formed in (iii) is a convex mark formed on the recessed mark.
[0156] This allows for the formation of alignment marks in a simple manner, which can further improve the visibility of the inspection area of solar panels.
[0157] (Technical 15) A method for manufacturing a photoelectric converter including a power generation area and an inspection area, the manufacturing method comprising: (I) forming a first dividing groove in the power generation area and removing it in the shape of a mark 1 in the inspection area from a first film formed on a substrate; (II) depositing a second film containing a perovskite compound on the first film in the power generation area and the inspection area, depositing the second film as a photoelectric conversion layer in the power generation area and depositing the second film on the mark shape in the inspection area; (III) irradiating the inspection area with a first laser to form a mark 2 with the second film deposited on the mark 1; (IV) aligning the position information of the mark 1 with the mark 2 to form a second dividing groove in the power generation area.
[0158] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0159] (Technical 16) The manufacturing method according to Technical 15, wherein apparatus A and apparatus B are provided, in (III), apparatus A forms the mark 2, in (IV), the substrate is moved to apparatus B, and apparatus B aligns the position information of mark 1 with the mark 2 to form the second divided groove in the power generation region, the laser of apparatus A has a wavelength at which the absorption rate of the second film is low and the absorption rate of the first film is high, and the laser of apparatus B has a wavelength at which the absorption rate of the first film is low and the absorption rate of the second film is high.
[0160] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0161] (Technical 17) The manufacturing method according to Technical 16, wherein the alignment of the position information of the mark 1 and the mark 2 in (IV) above includes: image recognition of the mark 2 with the device B; checking for any misalignment by comparing the recognized image of the mark 2 with the position information of the mark 1; and correcting the positional misalignment of the mark 2 with respect to the position information of the mark 1 if there is a misalignment.
[0162] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0163] (Technical 18) The manufacturing method according to Technical 16 or 17, wherein apparatus A comprises an infrared laser, and apparatus B comprises at least one selected from the group consisting of a green laser and an ultraviolet laser.
[0164] This allows for alignment using easily identifiable inspection areas, further improving processing accuracy and production speed in the manufacturing of solar panels.
[0165] (Technical 19) Alignment mark comprising a substrate and a film containing a perovskite compound disposed on the substrate, wherein the film containing the perovskite compound is convex with respect to the surface of the substrate.
[0166] This makes it possible to provide alignment marks that can further improve the visibility of the inspection area of solar panels.
[0167] (Technical 20) The alignment mark according to Technical 19, wherein the shape of the alignment mark is a cross, a circle, a double circle, or a combination thereof.
[0168] This makes it possible to provide alignment marks that can further improve the visibility of the inspection area of solar panels.
[0169] (Technical 21) A method for forming a laminated structure, comprising: selectively forming a base film; forming a film containing a perovskite compound so as to span both a first region where the base film is not formed and a second region adjacent to the first region where the base film is present; and irradiating the films containing the perovskite compound in the first and second regions with a laser to self-align, thereby removing the films containing the perovskite compound in the second region while leaving the films containing the perovskite compound in the first region, thereby forming a laminated structure in which films containing the perovskite compound are laminated in the first region, wherein the laser has a wavelength such that the absorption rate of the films containing the perovskite compound is low and the absorption rate of the base film is high.
[0170] This makes it possible to easily manufacture laminated structures that can be used, for example, as alignment marks to further improve the visibility of inspection areas on solar panels.
[0171] (Technical 22) The forming method according to Technical 21, wherein the laser is an infrared laser.
[0172] This makes it possible to easily manufacture laminated structures that can be used, for example, as alignment marks to further improve the visibility of inspection areas on solar panels.
[0173] The photoelectric conversion device disclosed herein can be used, for example, in a glass building material-integrated perovskite solar cell.
Claims
1. A solar cell comprising: a substrate; a solar cell disposed on a first surface of the substrate and comprising a first conductive film and a semiconductor layer including a colored layer; and an inspection area disposed on the first surface of the substrate, wherein in the solar cell, the first conductive film and the semiconductor layer are stacked in this order from the substrate side; the inspection area comprises: a first region comprising a first layer comprising at least one anion contained in the semiconductor layer and at least one cation contained in the semiconductor layer; and a second region disposed between the first layer and the solar cell in a plan view, wherein the second region comprises a second layer having a smaller thickness in the stacking direction than the first layer and containing the same material as the first layer, or does not comprise the second layer. Here, the stacking direction means the direction in which the first conductive film and the semiconductor layer are stacked, and the plan view means the view of the solar cell along the stacking direction.
2. The solar cell panel according to claim 1, wherein the first region further comprises a third layer between the first layer and the substrate, the third layer having a thickness in the stacking direction less than that of the first conductive film of the solar cell.
3. The solar cell panel according to claim 2, wherein the second region further comprises a fourth layer between the second layer and the substrate, the fourth layer having a thickness in the stacking direction less than that of the first conductive film of the solar cell.
4. The solar cell panel according to claim 1, wherein the inspection area is located outside, in a plan view, the area on which the semiconductor layer is laminated on the first conductive film in the solar cell. Here, "outside" means the outer edge side of the solar cell panel in a plan view.
5. The solar cell panel according to claim 4, further comprising a current collection region to which a current collector is electrically connected to the first conductive film in which the semiconductor layer is not laminated, wherein the inspection region is located outside the region in the current collection region in which the current collector is present.
6. The solar cell panel according to claim 1, wherein the inspection area has a portion that protrudes in the stacking direction with respect to the position of the first surface of the substrate.
7. The solar cell further comprises a second conductive film laminated on the semiconductor layer, and the first region further comprises a fifth layer laminated on the first layer, comprising the same material as the second conductive film, according to claim 1.
8. The solar panel according to claim 1, wherein the solar cell and the inspection area are not electrically connected.
9. The solar panel according to claim 8, further comprising an insulating region between the solar cell and the inspection area in the plan view, including a portion where the first conductive film is not provided.
10. The solar cell panel according to claim 1, wherein the first layer of the first region has a shape in plan view that includes at least one intersection point of two or more linear bodies.
11. The solar cell panel according to claim 1, wherein the first layer of the first region has a closed linear shape in the plan view.
12. The solar cell panel according to claim 11, wherein the inspection area further comprises a third area, the third area comprising a sixth layer located inside the closed linear shape, having a smaller thickness in the stacking direction than the first layer, and containing the same material as the first layer.
13. A method for forming an alignment mark, comprising: (i) forming a first film having a mark-shaped opening on a substrate; (ii) forming a second film containing a perovskite compound on the first film including the opening; and (iii) irradiating the first film and the second film with a laser to the opening and the region surrounding the opening to form the mark-shaped second film in a self-aligned manner, wherein the laser has a wavelength such that the absorption rate of the second film is low and the absorption rate of the first film is high.
14. The method for forming an alignment mark according to claim 13, wherein the opening formed in the first film in (i) is a recessed mark, and the second film with the mark shape formed in (iii) is a convex mark formed on the recessed mark.
15. A method for manufacturing a photoelectric converter including a power generation area and an inspection area, the manufacturing method comprising: (I) forming a first dividing groove in the power generation area and removing it in the shape of a mark 1 in the inspection area from a first film formed on a substrate; (II) depositing a second film containing a perovskite compound on the first film in the power generation area and the inspection area, depositing the second film as a photoelectric conversion layer in the power generation area and depositing the second film on the mark shape in the inspection area; (III) irradiating the inspection area with a first laser to form a mark 2 with the second film deposited on the mark 1; and (IV) aligning the position information of the mark 1 with the mark 2 to form a second dividing groove in the power generation area.
16. The manufacturing method according to claim 15, wherein apparatus A and apparatus B are provided, in (III), apparatus A forms the mark 2, in (IV), the substrate is moved to apparatus B, and apparatus B aligns the position information of mark 1 with the mark 2 to form the second divided groove in the power generation region, the laser of apparatus A has a wavelength at which the absorption rate of the second film is low and the absorption rate of the first film is high, and the laser of apparatus B has a wavelength at which the absorption rate of the first film is low and the absorption rate of the second film is high.
17. The manufacturing method according to claim 16, wherein the alignment of the position information of the mark 1 and the mark 2 in (IV) above includes: image recognition of the mark 2 with the device B; checking for any misalignment by comparing the recognized image of the mark 2 with the position information of the mark 1; and correcting the positional misalignment of the mark 2 with respect to the position information of the mark 1 if there is a misalignment.
18. The manufacturing method according to claim 16, wherein apparatus A comprises an infrared laser, and apparatus B comprises at least one selected from the group consisting of a green laser and an ultraviolet laser.
19. Alignment marks comprising a substrate and a film containing a perovskite compound disposed on the substrate, wherein the film containing the perovskite compound is convex with respect to the surface of the substrate.
20. The alignment mark according to claim 19, wherein the shape of the alignment mark is a cross, a circle, a double circle, or a combination thereof.
21. A method for forming a laminated structure, comprising: selectively forming a base film; forming a film containing a perovskite compound so as to span both a first region where the base film is not formed and a second region adjacent to the first region where the base film is present; and irradiating the films containing the perovskite compound in the first and second regions with a laser to self-align, thereby removing the films containing the perovskite compound in the second region while leaving the films containing the perovskite compound in the first region, thereby forming a laminated structure in which films containing the perovskite compound are laminated in the first region, wherein the laser has a wavelength such that the absorption rate of the films containing the perovskite compound is low and the absorption rate of the base film is high.
22. The forming method according to claim 21, wherein the laser is an infrared laser.