Drilling process of aluminum-based PCB for electric drive of new energy automobile

Through the coating treatment of drilling knife and the clamping technology of phenolic resin pads, the problems of drilling knife softening and edge-covering are solved, which extends the life of drilling knife and improves the drilling pass rate of aluminum-based PCB boards.

CN118890788APending Publication Date: 2024-11-01CAMELOT HUBEI TECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411160963.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

When drilling aluminum-based PCB boards, traditional drilling knives are prone to heat and soften and wear severely, resulting in drilling insufficiency or breaking the knife, and the holes on the aluminum surface are prone to appear, reducing the drilling pass rate.

Method used

The drilling nozzle coating of the drilling knife is treated to increase the hard coating, clamp with phenolic resin pads with hardness higher than that of the aluminum-based PCB board, and precise drilling and retardation are performed through positioning fixtures and drilling machines to ensure The hole wall is smooth without any edge.

Benefits of technology

It extends the service life of the drilling tool, improves the drilling pass rate of aluminum-based PCB board, ensures that the orifices have no edges and smooth hole walls, and improves the yield rate of production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118890788A_ABST
    Figure CN118890788A_ABST
Patent Text Reader

Abstract

The invention provides a drilling technology of an aluminum-based PCB for an electric drive of a new energy automobile, and the technology comprises the following steps: carrying out the coating processing of a drill bit of a drilling cutter, so as to enable the surface of the drill bit of the drilling cutter to be coated with a hard coating. And sequentially laminating the first phenolic resin base plate, the aluminum-based PCB and the second phenolic resin base plate to obtain a combined plate layer. And carrying out limiting treatment on the combined plate layer through a positioning clamp. And the drilling cutter obtained after film coating treatment is installed on a drilling machine, and feeding drilling treatment is conducted on the combined plate layer located on the positioning clamp through the drilling machine. And the combined plate layer is subjected to tool retracting treatment through the drilling machine. And carrying out stripping treatment on the composition board layer subjected to the tool withdrawal treatment so as to obtain the drilled aluminum-based PCB. Wherein the hard coating is made of an amorphous diamond-like material, and the hardness of the first phenolic resin base plate and the hardness of the second phenolic resin base plate are both larger than the hardness of the aluminum-based PCB.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of circuit boards, and in particular to a drilling process for an aluminum-based PCB board used for electric drive of new energy vehicles. Background Art

[0002] With the continuous upgrading of electronic products, high-power electronic products are constantly emerging to meet people's higher performance requirements for electronic products. Today's high-power electronic products have higher and higher requirements for the heat dissipation of components. If the heat dissipation of the substrate is not good, it will cause the components to overheat, thereby reducing the reliability of the whole machine and shortening its service life. In this context, high-heat dissipation metal-based printed circuit boards came into being. Metal-based printed circuit boards are a special type of printed circuit boards, mainly copper substrates, aluminum substrates, stainless steel substrates and other different types. Aluminum substrates are favored in the field of new energy vehicles due to their excellent heat dissipation and high hardness.

[0003] However, aluminum-based PCBs are generally divided into aluminum substrates, PP resin layers, and copper foil layers that are laminated and stacked in sequence. Traditional drilling cutters are iron cutters. When drilling holes in aluminum-based PCBs, the friction between metals will generate a lot of heat. The drilling cutter is easily softened by heat, and is easily worn during drilling, which reduces the sharpness of the drilling cutter, resulting in the drilling cutter being unable to cut the aluminum-based PCBs, and even breaking the cutter. In addition, before drilling holes in aluminum-based PCBs, two drilling pads are required to clamp the aluminum-based PCBs up and down. Due to the high hardness of the aluminum substrate, the drilling cutter will squeeze the drilling pads downward with the aluminum substrate when drilling, resulting in the aluminum surface being flared, resulting in a decrease in the qualified rate of aluminum-based PCB drilling. Summary of the invention

[0004] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a drilling process for an aluminum-based PCB board for electric drive of new energy vehicles, which can prolong the service life of a drilling tool and avoid aluminum surface burring.

[0005] The purpose of this disclosure is achieved through the following technical solutions:

[0006] A drilling process for an aluminum-based PCB board for electric drive of a new energy vehicle comprises the following steps:

[0007] Performing coating treatment on the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating;

[0008] The first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate are stacked in sequence to obtain a composite board layer;

[0009] Performing position limiting processing on the combined board layer by using a positioning fixture;

[0010] The coated drilling tool is installed on a drilling machine, and the combined board layer located on the positioning fixture is drilled by the drilling machine;

[0011] Performing a back-cutting process on the combined board layer by using the drilling machine;

[0012] The combined board layer after the back-cutting process is subjected to a peeling process to obtain the aluminum-based PCB board after drilling;

[0013] Wherein, the hard coating is an amorphous diamond-like material, and the hardness of the first phenolic resin pad and the second phenolic resin pad are both greater than the hardness of the aluminum-based PCB board.

[0014] In one embodiment, the diameter of the drilling tool is 1.0 mm to 4.0 mm.

[0015] In one of the embodiments, the hole limit of the drilling tool is 300 or 500.

[0016] In one of the embodiments, the feed speed of the drilling machine is 0.2 m / min to 0.5 m / min.

[0017] In one embodiment, the rotation speed of the drilling machine is 25krpm to 35krpm.

[0018] In one embodiment, the calculation formula of the cutting amount of the drilling tool is as follows:

[0019]

[0020] In one of the embodiments, the cutting amount of the feed drilling process is 7 μm / r to 15 μm / r.

[0021] In one embodiment, the hard coating has a thickness of 1.5 μm to 2.5 μm.

[0022] In one of the embodiments, the retraction speed of the drilling machine is 8m / min.

[0023] In one of the embodiments, the aluminum substrate in the aluminum-based PCB board is a first-series aluminum plate or a fifth-series aluminum plate.

[0024] Compared with the prior art, the present invention has at least the following advantages:

[0025] 1. The drill tip of the drill cutter is coated with a hard coating on its surface. The hard coating is an amorphous diamond-like material, which can effectively improve the hardness, wear resistance and thermal stability of the drill tip, making it less likely for the drill tip to soften due to heat during drilling, and reducing the wear of the drill tip, thereby effectively extending the service life of the drill tip.

[0026] 2. The first phenolic resin pad, the aluminum-based PCB board and the second phenolic resin pad are stacked in sequence to obtain a composite board layer, that is, the two sides of the aluminum-based PCB are clamped by two phenolic resin pads, and the hardness of the first phenolic resin pad and the second phenolic resin pad is greater than that of the aluminum-based PCB board, that is, the phenolic resin board can provide more uniform pressure distribution and better support effect, so that the aluminum-based PCB board will not squeeze the phenolic resin pad when the drilling machine performs feed drilling on the composite board layer located on the positioning fixture, so that the hole opening of the aluminum-based PCB board has no burr and the hole wall is relatively smooth, and then the composite board layer after the feed drilling process is retracted by the drilling machine, which can take out the debris remaining in the hole, and finally the composite board layer after the retraction process is peeled off, and the aluminum-based PCB board with the best drilling effect is obtained after the phenolic resin pad is peeled off, so that the qualified rate of aluminum-based PCB board drilling can be effectively improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present disclosure and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0028] Figure 1 Flow chart of the drilling process for aluminum-based PCB boards used in new energy vehicle electric drives;

[0029] Figure 2 This is a physical picture of the aluminum-based PCB board after drilling in Example 2;

[0030] Figure 3 This is a physical picture of the aluminum-based PCB board after drilling in Comparative Example 1;

[0031] Figure 4 A physical picture of a drilling tool used in the drilling process disclosed in the present invention;

[0032] Figure 5 The figure is a picture of the finished product of an aluminum-based PCB board after being processed by the drilling process disclosed in the present invention. DETAILED DESCRIPTION

[0033] In order to facilitate the understanding of the present disclosure, the present disclosure will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present disclosure are given in the drawings. However, the present disclosure can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present disclosure more thoroughly and comprehensively understood.

[0034] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0035] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present disclosure. The terms used herein in the specification of the present disclosure are only for the purpose of describing specific embodiments and are not intended to limit the present disclosure. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0036] The present disclosure provides a drilling process for an aluminum-based PCB board for electric drive of new energy vehicles, comprising the following steps: coating the drill tip of a drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating. Stacking a first phenolic resin pad, an aluminum-based PCB board and a second phenolic resin pad in sequence to obtain a composite board layer. The composite board layer is limited by a positioning fixture. The coated drilling tool is mounted on a drilling machine, and the composite board layer located on the positioning fixture is subjected to a feed drilling process by the drilling machine. The composite board layer is subjected to a back-off process by the drilling machine. The composite board layer after the back-off process is subjected to a peeling process to obtain the aluminum-based PCB board after drilling. Wherein, the hard coating is an amorphous diamond-like material, and the hardness of the first phenolic resin pad and the second phenolic resin pad is greater than the hardness of the aluminum-based PCB board.

[0037] The above-mentioned drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles is to coat the drill bit of the drill cutter with a hard coating on the surface of the drill bit of the drill cutter. The hard coating is an amorphous diamond-like material, which can effectively improve the hardness, wear resistance and thermal stability of the drill bit, so that the drill cutter is not prone to heat softening during drilling, and reduce the wear of the drill cutter, thereby effectively extending the service life of the drill cutter.

[0038] Furthermore, the first phenolic resin pad, the aluminum-based PCB board and the second phenolic resin pad are stacked in sequence to obtain a composite board layer, that is, the two sides of the aluminum-based PCB are clamped by two phenolic resin pads, and the hardness of the first phenolic resin pad and the second phenolic resin pad is greater than that of the aluminum-based PCB board, that is, the phenolic resin board can provide more uniform pressure distribution and better support effect, so that when the drilling machine performs feed drilling processing on the composite board layer located on the positioning fixture, the aluminum-based PCB board will not squeeze the phenolic resin pad, so that the hole opening of the aluminum-based PCB board has no burr and the hole wall is relatively smooth, and then the composite board layer after the feed drilling processing is retracted by the drilling machine, which can take out the debris remaining in the hole, and finally the composite board layer after the retraction processing is peeled off, and the aluminum-based PCB board with the best drilling effect is obtained after the phenolic resin pad is peeled off, so that the qualified rate of the aluminum-based PCB board drilling can be effectively improved.

[0039] See also Figure 1 In order to better understand the drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles disclosed in the present invention, the drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles is further explained below:

[0040] A drilling process for an aluminum-based PCB board for electric drive of a new energy vehicle according to an embodiment of the present invention comprises the following steps:

[0041] S100, coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating.

[0042] In this embodiment, the surface of the drill bit of the drilling tool is plated by chemical vapor deposition, that is, an amorphous diamond-like material is plated on the drill bit of the drilling tool, so that the drill bit of the drilling tool is plated with a hard coating. The amorphous diamond-like material has high hardness and thermal stability, which can significantly improve the wear resistance of the drill bit of the drilling tool, and can still maintain good hardness when the drilling is heated, thereby avoiding softening and wear of the drilling tool, maintaining the sharpness of the drilling tool and extending the service life of the drilling tool, so that the aluminum-based PCB board has the best drilling effect, and further improves the qualified rate of aluminum-based PCB board drilling.

[0043] S200, stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer.

[0044] In this embodiment, since the conventional drilling pad is a melamine pad, its hardness is lower than that of the aluminum-based PCB board, when drilling, the aluminum-based PCB board is squeezed by the drilling cutter due to its own stress, which not only causes the hole opening to flash, but also the PP resin layer in the middle of the aluminum-based PCB board is pulled and squeezed, resulting in the thinning of the insulating layer, and finally causing the aluminum-based PCB board to fail the withstand voltage test, thereby reducing the production yield of the aluminum-based PCB board. Therefore, the present disclosure stacks the first phenolic resin pad, the aluminum-based PCB board and the second phenolic resin pad in sequence, and the hardness of the phenolic resin pad is higher than that of the aluminum-based PCB board, that is, the phenolic resin pad can provide a more uniform pressure distribution and a better supporting effect for the aluminum-based PCB board, so that the aluminum-based PCB board will not squeeze the phenolic pad when being drilled, and avoid the situation that the hole opening is flashed due to the stress problem of the aluminum-based PCB board itself, so that the aluminum-based PCB board obtains the best drilling effect, and further improves the qualified rate of the aluminum-based PCB board drilling.

[0045] S300, performing position limiting processing on the combined board layer by using a positioning fixture.

[0046] In this embodiment, in order to ensure the accuracy and stability of drilling, the combined board layer is limited and fixed by a positioning fixture, so that the combined board layer is limited and fixed in the positioning fixture, ensuring that the combined board layer will not be offset during drilling, thereby improving the accuracy of drilling, thereby effectively improving the qualified rate of drilling holes in aluminum-based PCB boards.

[0047] S400, installing the coated drilling tool on a drilling machine, and using the drilling machine to perform feed drilling on the combined board layer located on the positioning fixture.

[0048] In this embodiment, a drilling tool coated with a hard coating is installed on a drilling machine, and the drilling machine is used to perform feed drilling processing on the composite board layer fixed on the positioning fixture. The coating of the hard coating ensures the sharpness of the drilling tool, and the clamping of the phenolic resin pad ensures the clamping stability of the aluminum-based PCB board during drilling. The addition of both can improve the accuracy of the feed drilling processing and the drilling effect, so that the hole opening of the aluminum-based PCB board will not produce burrs and the hole wall is relatively smooth, ensuring the best drilling effect, thereby further improving the qualified rate of drilling holes in the aluminum-based PCB board.

[0049] Furthermore, in one embodiment, the specific operation steps of performing feed drilling processing on the combined board layer located on the positioning fixture by the drilling machine are:

[0050] Set the corresponding drilling parameters on the drilling machine according to the diameter of the drilling tool;

[0051] The drilling command of the drilling machine is received, and the drilling machine is controlled to drive the drilling tool to move toward the combined board layer according to the drilling parameters until the combined board layer is penetrated. In this embodiment, the drilling command of the drilling machine can be automatically generated after the drilling parameters are set through the human-machine interaction interface, thereby improving the intelligence and automation of the drilling operation of the drilling machine. For example, the drilling command of the drilling machine can be automatically generated after the drilling parameters are set through the human-machine interaction interface of the touch input screen of the drilling machine, thereby improving the intelligence and automation of the drilling operation of the drilling machine.

[0052] It should be noted that, since the thickness specifications of aluminum-based PCB boards are consistent, the corresponding drilling parameters are set for different tool diameters, which can ensure that the aluminum-based PCB boards obtain the best drilling effect, further improve the qualified rate of aluminum-based PCB board drilling, thereby effectively improving the production qualified rate of aluminum-based PCB boards.

[0053] S500, performing a back-cutting process on the combined board layer by using the drilling machine.

[0054] In this embodiment, a chip breaking groove is formed on the drill tip of the drilling tool, which can effectively discharge the residual chips when drilling. At the same time, when retracting the tool, the drill tip of the drilling tool can also perform a secondary cutting on the broken chips of the hole wall, so that the hole wall has a better smoothness, thereby achieving the best drilling effect for the aluminum-based PCB board.

[0055] Further, in one embodiment, the specific operation steps of using the drilling machine and performing a back-drilling process on the combined board layer after the feed drilling process are:

[0056] Set the retraction parameters on the drilling machine;

[0057] When the drilling machine completes the drilling command, the drilling machine automatically obtains and executes the tool retraction command, and drives the drilling tool away from the combined board layer according to the tool retraction parameters until the drilling tool is separated from the combined board layer.

[0058] S600, peeling off the combined board layer after the backing out process to obtain the aluminum-based PCB board after drilling.

[0059] In this embodiment, the combined board layer after the backing treatment is peeled off, that is, the first phenolic resin pad and the second phenolic resin pad clamped on both sides of the aluminum-based PCB board are peeled off to obtain an aluminum-based PCB board with the best drilling effect, so that the aluminum-based PCB board can meet the good product requirements in the subsequent voltage resistance test, thereby ensuring the good product rate of the aluminum-based PCB board.

[0060] In one embodiment, the diameter of the drilling tool is 1.0 mm to 4.0 mm, so that the diameter of the hole processed by the drilling tool is 1.0 mm to 4.0 mm, and the diameter of two adjacent specifications of the tool differs by 0.5 mm, which meets the setting of the standard hole.

[0061] In one embodiment, the hole limit of the drilling tool is 300 or 500. It is understandable that the hole limit refers to the maximum number of drilling times of the drilling tool, and the hole limits corresponding to different plates are also different. In this embodiment, the aluminum substrate of the aluminum-based PCB board adopts a first-series aluminum plate or a fifth-series aluminum plate, and the hole limit corresponding to the first-series aluminum plate is 500, and the hole limit corresponding to the fifth-series aluminum plate is 300. Further, after the drilling tool completes the maximum number of drilling times, the hard coating on the surface of the drill tip has been basically worn away, but the drill tip of the drilling tool is still intact, and the drill tip of the drilling tool can be subjected to a secondary coating treatment so that the surface of the drill tip of the drilling tool is re-coated with a hard coating, so as to realize the continuous use of the drilling tool and reduce the scrapping of the drilling tool, thereby effectively saving the drilling cost.

[0062] In one embodiment, the feed speed of the drilling machine is 0.2m / min to 0.5m / min. It is understandable that at this feed speed, the drill tip of the drilling tool can smoothly pass through the combined board layer to complete the hole opening process of the aluminum-based PCB board, and the feed speed of the drilling machine will affect the cutting amount.

[0063] In one embodiment, the rotation speed of the drilling machine is 25krpm to 35krpm. It is understandable that at this rotation speed, the drill tip of the drilling tool can cut holes in the aluminum-based PCB board, and the rotation speed of the drilling machine will also affect the cutting amount.

[0064] In one embodiment, the calculation formula of the cutting amount of the drilling tool is as follows:

[0065]

[0066] It can be understood that the optimal cutting amount corresponding to each specification can be obtained through the calculation formula of the cutting amount and multiple cutting experiments. In this way, the optimal drilling parameters corresponding to each specification can be obtained, further improving the qualified rate of aluminum-based PCB board drilling.

[0067] In one embodiment, the cutting amount of the feed drilling process is 7μm / r to 15μm / r. It can be understood that since the diameter of the drilling tool is 1.0mm to 4.0mm, the cutting amount of the feed drilling space process is 7μm / r to 15μm / r, where each specification has a corresponding optimal drilling parameter, which needs to be obtained after multiple cutting experiments.

[0068] It is understandable that each tool diameter has an optimal drilling parameter corresponding to it. In order to further improve the qualified rate of aluminum-based PCB board drilling, in one embodiment, the specific operation steps for obtaining the optimal drilling parameters are as follows:

[0069] First, select a drill of one specification;

[0070] Secondly, set multiple drilling parameter groups with different feed speeds and rotation speeds;

[0071] Then, according to the multiple drilling parameter groups, the drilling machine is driven to drill holes in different areas of the combined board layer in sequence, so that multiple through holes are obtained on the combined board layer;

[0072] Finally, multiple through holes of the combined board layer are scanned and measured, and the through hole with the best drilling effect is selected and its drilling parameter group is correspondingly recorded as the optimal drilling parameter.

[0073] It should be noted that the parameters of each drilling parameter group remain consistent during the tool retraction process, and the difference lies in the feed speed and rotation speed. The above operation steps can obtain the optimal drilling parameters for each specification of tool diameter, and can achieve the best drilling effect for aluminum-based PCB boards according to the processing requirements of different hole diameters. At the same time, the above operation steps can also obtain the optimal drilling parameters for aluminum-based PCB boards of different thicknesses corresponding to a single specification of tool diameter, thereby improving the adaptability of the drilling process.

[0074] Further, when the diameter of the drilling tool remains unchanged, the thickness of the aluminum-based PCB board has different specifications. In order to improve the adaptability of the drilling process, the optimal drilling parameters corresponding to different thicknesses are also different. The key to improving the drilling efficiency and the drilling pass rate lies in the thickness and drilling parameters of the aluminum-based PCB board. Since the thickness of the phenolic resin pad is fixed, the change in the thickness of the combined board layer is the change in the thickness of the aluminum-based PCB board. Therefore, in this embodiment, the thickness of the combined board layer is detected to simultaneously obtain the drilling parameters. The drilling parameters are the rotation speed and feed speed of the single-specification tool diameter. The combined board layer is fed and drilled according to the drilling parameters to obtain the best drilling effect, thereby further improving the pass rate of aluminum-based PCB board drilling. At the same time, this step is also adapted to the drilling requirements of drilling tools of different specifications, so that the drilling process of the present invention can adapt to the different drilling requirements of aluminum-based PCB boards of different thicknesses, improve the adaptability, and improve the pass rate of aluminum-based PCB board drilling, thereby effectively improving the production yield rate of aluminum-based PCB boards.

[0075] Furthermore, the thickness of the combined board layer is detected to simultaneously obtain drilling parameters, including: firstly, establishing a database of multiple combined board layer thicknesses and multiple drilling parameters in one-to-one correspondence; then, the thickness of the combined board layer to be detected is detected to obtain the actual thickness of the combined board layer; then, according to the actual thickness of the combined board layer, the drilling target parameter corresponding to the thickness of the combined board layer to be detected is retrieved, thereby improving the applicability and accuracy of the feed drilling process, thereby obtaining the best drilling effect. Furthermore, according to the drilling target parameters, the drilling machine is controlled to feed the combined board layer for feed drilling, so that no flash is generated in the hole wall of the combined board layer and the hole wall is relatively smooth, so that the aluminum-based PCB board obtains the best drilling effect, improves the qualified rate of aluminum-based PCB board drilling, and thus effectively improves the production yield rate of aluminum-based PCB boards.

[0076] Furthermore, the step of detecting the thickness of the composite board layer is specifically as follows: collecting data on the thickness of the composite board layer through a CCD microscope camera to obtain data on the composite board layer; denoising the data of the composite board layer; fitting the denoised data of the composite board layer to obtain a three-dimensional image of the data of the composite board layer; measuring the data of the composite board layer according to the three-dimensional image of the composite board layer to obtain corresponding drilling parameters, thereby improving the accuracy of the detection data of the drilling parameters and enabling automatic measurement. Furthermore, the step of collecting data on the thickness of the composite board layer through a CCD microscope camera is specifically as follows: scanning the surface of the composite board layer through a CCD microscope camera to obtain a three-dimensional image of the surface of the composite board layer. Furthermore, the step of measuring data on the aluminum plate according to the three-dimensional image of the composite board layer is specifically as follows: performing multiple measurements on multiple positions of the composite board layer according to the three-dimensional image of the composite board layer to obtain multiple actual thickness values ​​of the composite board layer; averaging the multiple actual thickness values ​​of the composite board layer to obtain the average actual thickness of the composite board layer. Furthermore, the step of calling the drilling target parameter corresponding to the thickness of the combined board layer to be tested according to the actual thickness of the combined board layer is specifically as follows: calling the drilling target parameter corresponding to the combined board layer to be tested according to the average value of the actual thickness of the combined board layer to match the actual drilling needs of the combined board layer. By averaging the actual thickness of the combined board layer, the data accuracy of the combined board layer is higher, and the combined board layer obtains the best drilling effect, so that the hole opening of the aluminum-based PCB board is free of burrs and the hole wall is smooth, so that the qualified rate of drilling of the aluminum-based PCB board is effectively improved, thereby effectively improving the production yield rate of the aluminum-based PCB board. At the same time, the above steps are also adapted to the processing requirements of different tool diameters, so that the best drilling effect can still be obtained on the different tool diameter processing requirements of aluminum-based PCB boards of different thicknesses, further improving the qualified rate of drilling of aluminum-based PCB boards, and greatly improving the adaptability of the drilling process.

[0077] In one embodiment, the thickness of the hard coating is 1.5 μm to 2.5 μm. It is understood that the amorphous diamond-like material is plated on the surface of the drill tip of the drilling tool by chemical vapor deposition, so that the drill tip is plated with a hard coating, and the thickness of the hard coating is between 1.5 μm and 2.5 μm, which is sufficient to significantly improve the wear resistance and thermal stability of the drill tip, thereby effectively extending the service life of the drilling tool.

[0078] In one embodiment, the drilling machine has a tool retracting speed of 8 m / min. It is understandable that the drilling cutter still keeps rotating during the tool retracting process, and the tool retracting speed of 8 m / min can cut off the debris in the hole wall for a second time, and can also make the drilling cutter quickly separate from the composite board layer to avoid excessive cutting of the hole wall, thereby effectively ensuring the smoothness of the hole wall, and further effectively improving the qualified rate of aluminum-based PCB board drilling.

[0079] In one embodiment, the aluminum substrate in the aluminum-based PCB board is a first-series aluminum plate or a fifth-series aluminum plate. It is understandable that the hardness of the fifth-series aluminum plate is higher than that of the first-series aluminum plate. The greater the hardness, the greater the wear of the hard coating. Therefore, the hole limits corresponding to aluminum plates of different hardness are also different.

[0080] Examples are listed below, but it should be noted that the following examples do not exhaust all possible situations, and the materials used in the following examples can be obtained from commercial channels unless otherwise specified.

[0081] In the following embodiments and comparative examples, the diameter of the drilling tool is 3.0 mm and the aluminum-based PCB board has the same thickness. The drilling effect of the aluminum-based PCB board is observed by changing different drilling parameters.

[0082] Example 1

[0083] Step 1: coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating, wherein the hard coating is an amorphous diamond-like material;

[0084] Step 2: stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer;

[0085] Step 3: Use a positioning fixture to limit the combined board layer;

[0086] Step 4: Install the coated drilling tool on the drilling machine, and use the drilling machine to perform feed drilling on the combined board layer on the positioning fixture, wherein the feed speed is 0.3m / min, the rotation speed is 25.0krpm, and the cutting amount is 12.0μm / r;

[0087] Step 5: Use a drilling machine to perform a back-drilling process on the combined plate layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0088] Step 6: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0089] Example 2

[0090] Step 1: coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating, wherein the hard coating is an amorphous diamond-like material;

[0091] Step 2: stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer;

[0092] Step 3: Use a positioning fixture to limit the combined board layer;

[0093] Step 4: Install the coated drilling tool on the drilling machine, and use the drilling machine to perform feed drilling on the combined board layer on the positioning fixture, wherein the feed speed is 0.3m / min, the rotation speed is 30.0krpm, and the cutting amount is 10.0μm / r;

[0094] Step 5: Use a drilling machine to perform a back-drilling process on the combined board layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0095] Step 6: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0096] Example 3

[0097] Step 1: coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating, wherein the hard coating is an amorphous diamond-like material;

[0098] Step 2: stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer;

[0099] Step 3: Use a positioning fixture to limit the combined board layer;

[0100] Step 4: Install the coated drilling tool on the drilling machine, and use the drilling machine to perform feed drilling on the combined board layer on the positioning fixture, wherein the feed speed is 0.3m / min, the rotation speed is 35.0krpm, and the cutting amount is 8.6μm / r;

[0101] Step 5: Use a drilling machine to perform a back-drilling process on the combined board layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0102] Step 6: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0103] Example 4

[0104] Step 1: coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating, wherein the hard coating is an amorphous diamond-like material;

[0105] Step 2: stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer;

[0106] Step 3: Use a positioning fixture to limit the combined board layer;

[0107] Step 4: Install the coated drilling tool on the drilling machine, and use the drilling machine to perform feed drilling on the combined board layer on the positioning fixture, wherein the feed speed is 0.4m / min, the rotation speed is 30krpm, and the cutting amount is 13.3μm / r;

[0108] Step 5: Use a drilling machine to perform a back-drilling process on the combined board layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0109] Step 6: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0110] Example 5

[0111] Step 1: coating the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating, wherein the hard coating is an amorphous diamond-like material;

[0112] Step 2: stacking the first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate in sequence to obtain a combined board layer;

[0113] Step 3: Use a positioning fixture to limit the combined board layer;

[0114] Step 4: Install the coated drilling tool on the drilling machine, and use the drilling machine to perform feed drilling on the combined board layer on the positioning fixture, wherein the feed speed is 0.5m / min, the rotation speed is 35.0krpm, and the cutting amount is 14.3μm / r;

[0115] Step 5: Use a drilling machine to perform a back-drilling process on the combined board layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0116] Step 6: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0117] Comparative Example 1

[0118] Step 1: stacking the first melamine backing plate, the aluminum-based PCB board and the second melamine backing plate in sequence to obtain a combined board layer;

[0119] Step 2: Use a positioning fixture to limit the combined board layer;

[0120] Step 3: Install the drilling tool on the drilling machine, and use the drilling machine to perform feed drilling processing on the combined board layer located on the positioning fixture, wherein the feed speed is 0.3m / min, the rotation speed is 30.0krpm, and the cutting amount is 10μm / r;

[0121] Step 4: Use a drilling machine to perform a back-drilling process on the combined plate layer after the feed drilling process, wherein the back-drilling speed is 8.0 m / min;

[0122] Step 5: Peel off the combined board layer after the back-cutting process to obtain the aluminum-based PCB board after drilling.

[0123] The drilling effects of the aluminum-based PCB boards of Examples 1-5 and Comparative Example 1 and the wear of the drill tips of the drilling cutters were observed. The results are shown in Table 1.

[0124] Table 1

[0125]

[0126] It can be seen from Table 1 that by comparing the data of Examples 1 to 5 and Comparative Example 1, Example 1 is the drilling process of the present invention, while Comparative Example 1 is the traditional drilling process. It can be seen that although the traditional drilling tool can drill holes, the drilling effect is poor, and the melamine pad cannot provide a good support effect for the aluminum-based PCB board, resulting in flashing at both the upper and lower hole openings, and the drill bit of the drilling tool is also worn. When the drilling process of the present invention is used to drill holes on the aluminum-based PCB board, the upper and lower hole openings do not flash, and the drill bit is not worn. This shows that the hard coating can significantly enhance the wear resistance of the drill bit, and the phenolic resin pad can provide better pressure distribution and better support effect, avoid flashing at the hole opening, and improve the qualified rate of aluminum-based PCB board drilling.

[0127] By comparing Examples 1 to 5, it can be seen that Example 2 is the best drilling parameter for a tool diameter of 3.0 mm, and Examples 4 and 5 show over-cutting, resulting in a rough hole wall. It can be seen that each tool diameter corresponds to an optimal drilling parameter, and the optimal drilling parameter can be obtained through multiple parameter adjustments, thereby improving the qualified rate of aluminum-based PCB board drilling, thereby effectively improving the production yield rate of aluminum-based PCB boards.

[0128] In summary, the drilling process disclosed in the present invention can extend the service life of the drilling tool, while improving the qualified rate of drilling holes in the aluminum-based PCB board, so that the hole opening of the aluminum-based PCB board is free of burrs and the hole wall is smooth, which greatly improves the production yield rate of the aluminum-based PCB board.

[0129] Compared with the prior art, the present invention has at least the following advantages:

[0130] 1. The drill tip of the drill cutter is coated with a hard coating on its surface. The hard coating is an amorphous diamond-like material, which can effectively improve the hardness, wear resistance and thermal stability of the drill tip, making it less likely for the drill tip to soften due to heat during drilling, and reducing the wear of the drill tip, thereby effectively extending the service life of the drill tip.

[0131] 2. The first phenolic resin pad, the aluminum-based PCB board and the second phenolic resin pad are stacked in sequence to obtain a composite board layer, that is, the two sides of the aluminum-based PCB are clamped by two phenolic resin pads, and the hardness of the first phenolic resin pad and the second phenolic resin pad is greater than that of the aluminum-based PCB board, that is, the phenolic resin board can provide more uniform pressure distribution and better support effect, so that the aluminum-based PCB board will not squeeze the phenolic resin pad when the drilling machine performs feed drilling on the composite board layer located on the positioning fixture, so that the hole opening of the aluminum-based PCB board has no burr and the hole wall is relatively smooth, and then the composite board layer after the feed drilling process is retracted by the drilling machine, which can take out the debris remaining in the hole, and finally the composite board layer after the retraction process is peeled off, and the aluminum-based PCB board with the best drilling effect is obtained after the phenolic resin pad is peeled off, so that the qualified rate of aluminum-based PCB board drilling can be effectively improved.

[0132] The above-mentioned embodiments only express several implementation methods of the present disclosure, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the disclosed patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present disclosure, and these all belong to the protection scope of the present disclosure. Therefore, the protection scope of the disclosed patent shall be subject to the attached claims.

Claims

1. A drilling process for an aluminum-based PCB board for electric drive of new energy vehicles, characterized in that: The steps include: Performing coating treatment on the drill tip of the drilling tool so that the surface of the drill tip of the drilling tool is coated with a hard coating; The first phenolic resin backing plate, the aluminum-based PCB board and the second phenolic resin backing plate are stacked in sequence to obtain a composite board layer; Performing position limiting processing on the combined board layer by using a positioning fixture; The coated drilling tool is installed on a drilling machine, and the combined board layer located on the positioning fixture is drilled by the drilling machine; Performing a back-cutting process on the combined board layer by using the drilling machine; The combined board layer after the back-cutting process is subjected to a peeling process to obtain the aluminum-based PCB board after drilling; Wherein, the hard coating is an amorphous diamond-like material, and the hardness of the first phenolic resin pad and the second phenolic resin pad are both greater than the hardness of the aluminum-based PCB board.

2. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 1 is characterized in that: The diameter of the drilling tool is 1.0 mm to 4.0 mm.

3. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 1 is characterized in that: The hole limit of the drilling tool is 300 or 500.

4. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 3 is characterized in that: The feed speed of the drilling machine is 0.2m / min to 0.5m / min.

5. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 4 is characterized in that: The rotation speed of the drilling machine is 25krpm to 35krpm.

6. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 5 is characterized in that: The calculation formula of the cutting amount of the drilling tool is as follows:

7. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 6 is characterized in that: The cutting amount of the feed drilling process is 7 μm / r to 15 μm / r.

8. The drilling process of the aluminum-based PCB board for the electric drive of new energy vehicles according to claim 1 is characterized in that: The hard coating has a thickness of 1.5 μm to 2.5 μm.

9. The drilling process of aluminum-based PCB board for new energy vehicle electric drive according to claim 1, characterized in that: The retraction speed of the drilling machine is 8m / min.

10. The drilling process of aluminum-based PCB board for new energy vehicle electric drive according to claim 3, characterized in that: The aluminum substrate in the aluminum-based PCB board is a first-series aluminum plate or a fifth-series aluminum plate.