Manufacturing process and infrared cut-off filter
By fabricating thin film materials with stepped power of an ion source and stacking them alternately, the problem of glass substrate warping and cracking caused by stress in the thin film system was solved, and a filter with low roughness and high processing reliability was achieved.
Patent Information
- Application Number
- CN202411050826.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-22
AI Technical Summary
Existing filter thin-film systems are prone to stress under high-power ion source bombardment, which can lead to glass substrate warping and breakage during subsequent processing.
The first and second thin film materials were fabricated using a stepped power ion source, and a low-reflection thin film system and a multilayer thin film system were formed by alternating superposition. The ion source power was gradually increased to reduce interface roughness and stress.
This reduces the roughness of the thin film interface, avoids fogging in the thin film system, and reduces the risk of glass substrate breakage in subsequent processing.
Smart Images

Figure CN118996345A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of optical filters, and in particular to a manufacturing process and an infrared cut-off filter. Background Art
[0002] One of the main problems that is prone to occur in the thin film system of the filter is the fogging of the thin film system. The main factors that cause the fogging of the thin film system include the surface roughness of the substrate and the roughness between different material layers in the thin film system. The roughness between different material layers in the thin film system is closely related to the process. In order to minimize the roughness between layers, the ion source is often used to assist, and the power of the ion source is relatively high, so that the high-energy atoms from the ion source can be used to bombard the interlayer surface to achieve the purpose of reducing the roughness between layers.
[0003] However, excessive ion source energy will also lead to increased film stress, especially for this ultra-multi-layer film system. Once the stress increases, and the glass is only 0.2mm thin, the glass warping will increase, and subsequent processing will become more difficult. The unevenness caused by warping will also increase the risk of glass breakage during subsequent processing (such as silk-screen printing, cutting and cleaning, etc.). Summary of the invention
[0004] The thin film system of the existing filter uses a high-power ion source to bombard the surface of the thin film material, which makes the glass substrate at risk of cracking in the subsequent processing technology.
[0005] In view of the above problems, a manufacturing process and an infrared cutoff filter are proposed. The first thin film material and the second thin film material are manufactured by adopting the stepped power of the ion source, and the first thin film material and the second thin film material are alternately superimposed to manufacture a low-reflection thin film system and a multi-layer thin film system. On the one hand, the density of the film layer is ensured, the roughness of the thin film interface is reduced, and the fogging of the thin film system is avoided. On the other hand, the stress of the thin film caused by excessive ion source power is avoided, and the risk of breakage of the glass substrate in subsequent processing technology is reduced.
[0006] In a first aspect, a manufacturing process for manufacturing an infrared cutoff filter comprises: Step 100, using ion source step power to produce a first thin film material; Step 200, using ion source step power to make a second thin film material; Step 300, alternately fabricating the first film material and the second film material on the first surface of the substrate glass to obtain a low-reflection film system; Step 400: alternately fabricate the first film material and the second film material on the second surface of the substrate glass to obtain a multilayer film system with high transmittance in the visible light range and cutoff in the infrared light range.
[0007] In combination with the manufacturing process described in the first aspect of the present invention, in a first possible implementation manner, step 100 includes: Step 110, dividing the first film material into a first thickness interval, a second thickness interval, ..., an nth thickness interval in sequence; Step 120, using a first ion source power, a second ion source power, ..., and an nth ion source power to respectively form a first thickness range, a second thickness range, ..., and an nth thickness range of the first thin film material by deposition; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the first thin film material.
[0008] In combination with the manufacturing process described in the first aspect of the present invention, in a second possible implementation manner, step 200 includes: Step 210, dividing the second film material into a first thickness interval, a second thickness interval, ..., an nth thickness interval in sequence; Step 220, using a first ion source power, a second ion source power, ..., and an nth ion source power to respectively form a first thickness range, a second thickness range, ..., and an nth thickness range of the second thin film material by deposition; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness range, the second thickness range, ..., and the nth thickness range of the second thin film material gradually approach the interface of the second thin film material.
[0009] In combination with the first possible implementation manner of the first aspect of the present invention, in a third possible implementation manner, the first film material is SiO2 low refractive index material, and the number of layers of the low reflection film system is 7-10 layers.
[0010] In combination with the second possible implementation manner of the first aspect of the present invention, in a fourth possible implementation manner, the second thin film material is a TiO2 high refractive index material, and the number of layers of the multilayer thin film system is 35-45 layers.
[0011] In a second aspect, an infrared cutoff filter is provided, using the manufacturing process described in the first aspect, comprising: Base material glass; Low reflection film system; Multilayer film systems; The low-reflection film system is made on the first surface of the substrate glass, and the multi-layer film system is made on the second surface of the substrate glass; The low-reflection film system and the multi-layer film system are respectively formed by alternately stacking a first film material and a second film material; The first thin film material is made by ion source step power coating; The second thin film material is made by ion source step power coating.
[0012] In combination with the manufacturing process described in the first aspect of the present invention, in a first possible implementation manner, the first thin film material includes a first thickness range, a second thickness range, ..., and an nth thickness range, and the first thickness range, the second thickness range, ..., and the nth thickness range of the first thin film material are respectively formed by coating with a first ion source power, a second ion source power, ..., and an nth ion source power; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the first thin film material.
[0013] In combination with the manufacturing process described in the first aspect of the present invention, in a second possible implementation manner, the second thin film material includes a first thickness range, a second thickness range, ..., and an nth thickness range, and the first thickness range, the second thickness range, ..., and the nth thickness range of the second thin film material are respectively formed by coating with a first ion source power, a second ion source power, ..., and an nth ion source power; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the second thin film material.
[0014] In combination with the first possible implementation manner of the second aspect of the present invention, in a third possible implementation manner, the first film material is SiO2 low refractive index material, and the number of layers of the low reflection film system is 7-10 layers.
[0015] In combination with the second possible implementation manner of the second aspect of the present invention, in a fourth possible implementation manner, the second thin film material is a TiO2 high refractive index material, and the number of layers of the multilayer thin film system is 35-45 layers.
[0016] The manufacturing process and infrared cutoff filter described in the present invention are implemented by adopting ion source step power to manufacture the first thin film material and the second thin film material, and using the first thin film material and the second thin film material to alternately stack to manufacture a low-reflection thin film system and a multi-layer thin film system. On the one hand, the density of the film layer is ensured, the roughness of the film interface is reduced, and the fogging of the thin film system is avoided. On the other hand, the stress of the film caused by excessive ion source power is avoided, and the risk of breakage of the glass substrate in subsequent processing technology is reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0018] Figure 1 This is a schematic diagram of the first process of the manufacturing process of the present invention; Figure 2 This is a schematic diagram of the second process of the manufacturing process of the present invention; Figure 3 This is a schematic diagram of the third process of the manufacturing process of the present invention; Figure 4 This is a schematic diagram of the structure of the infrared cutoff filter of the present invention; Figure 5 It is a first schematic diagram of the structure of the first thin film material in the infrared cut-off filter of the present invention; Figure 6 It is a second schematic diagram of the first thin film material structure in the infrared cut-off filter of the present invention; Figure 7 It is a first schematic diagram of the second thin film material structure in the infrared cut-off filter of the present invention; Figure 8 This is a second schematic diagram of the second thin film material structure in the infrared cutoff filter of the present invention. DETAILED DESCRIPTION
[0019] The following will be combined with the accompanying drawings in the invention to clearly and completely describe the technical solutions in the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments in the present invention, other embodiments obtained by ordinary technicians in this field without creative work are all within the scope of protection of the present invention.
[0020] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0021] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0022] It should be understood that the orientation or position relationship indicated by terms such as "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0023] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0024] The thin film system of the existing filter uses a high-power ion source to bombard the surface of the thin film material, which makes the glass substrate at risk of cracking in the subsequent processing technology.
[0025] In view of the above problems, a manufacturing process and an infrared cut-off filter are proposed.
[0026] First, as Figure 1 , Figure 1 The first process diagram of the manufacturing process of the present invention is as follows; a manufacturing process for manufacturing an infrared cutoff filter comprises: Step 100: using ion source step power to produce a first thin film material 11.
[0027] Preferably, if Figure 2 , Figure 2 Schematic diagram of the second process of the manufacturing process in the present invention; step 100 includes: step 110, dividing the first film material 11 into a first thickness interval, a second thickness interval, ..., and an nth thickness interval in sequence; step 120, using a first ion source power, a second ion source power, ..., and an nth ion source power to respectively coat the first film material 11 with a first thickness interval, a second thickness interval, ..., and an nth thickness interval; wherein the first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the first film material 11, such as Figure 5 , Figure 5 Schematic diagram of the structure of the first film material 11 in the mid-infrared cutoff filter of the present invention; preferably, the first film material 11 is SiO2 low refractive index material, and the number of layers of the low-reflection film system 10 is 7-10.
[0028] like Figure 6 , Figure 6 This is a second schematic diagram of the structure of the first film material 11 in the infrared cutoff filter of the present invention; the first film material 11 can be divided into two thickness ranges. If the thickness of the first film material 11 is 100nm, the thickness of the first thickness range is 90nm, and the thickness of the second thickness range is 10nm. In the first thickness range, the power can be set to 1000w-1200w, and in the second thickness range, the power can be set to 1200w-1400w, which can ensure that the roughness of the interface is at a relatively small level.
[0029] Step 200: using ion source step power to produce the second thin film material 31.
[0030] Preferably, if Figure 3 , Figure 3 Schematic diagram of the third process of the manufacturing process in the present invention; step 200 includes: step 210, dividing the second film material 31 into a first thickness interval, a second thickness interval, ..., and an nth thickness interval in sequence; step 220, using the first ion source power, the second ion source power, ..., and the nth ion source power to respectively coat the first thickness interval, the second thickness interval, ..., and the nth thickness interval of the second film material 31; wherein the first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval of the second film material 31 gradually approach the interface of the second film material 31, such as Figure 7 , Figure 7 FIG. 1 is a first schematic diagram of the structure of the second thin film material 31 in the infrared cutoff filter of the present invention.
[0031] Preferably, the second thin film material 31 is a TiO2 high refractive index material, and the number of layers of the multilayer thin film system 30 is 35-45 layers.
[0032] like Figure 8 , Figure 8 The second schematic diagram of the structure of the second film material 31 in the infrared cut-off filter of the present invention. The second film material 31 can be divided into two thickness ranges. If the thickness of the second film material 31 is 100nm, the thickness of the first thickness range is 90nm, and the thickness of the second thickness range is 10nm. In the first thickness range, the power can be set to 1000w-1200w, and in the second thickness range, the power can be set to 1200w-1400w, which can ensure that the roughness of the interface is at a relatively small level.
[0033] Step 300, alternately fabricate the first film material 11 and the second film material 31 on the first surface of the substrate glass 20 to obtain a low-reflection film system 10; Step 400, alternately fabricate the first film material 11 and the second film material 31 on the second surface of the substrate glass 20 to obtain a multilayer film system 30 with high transmittance in the visible light range and cutoff in the infrared light range.
[0034] like Figure 4 , Figure 4 The schematic diagram of the structure of the infrared cut-off filter of the present invention; the thickness of the substrate glass 20 of the infrared cut-off filter is 0.1mm-0.3mm, the reflective film system on the first side is usually 7-10 layers, the low refractive index material of the first film material 11 is SiO2, and the high refractive index material of the second film material 31 is TiO2. The multilayer film system 30 with high transmittance in the visible light range and cut-off in the infrared light range on the second side is usually 35-45 layers, the low refractive index material of the first film material 11 is SiO2, and the high refractive index material of the second film material 31 is TiO2.
[0035] Take the 40-layer infrared cut-off film system as an example: SiO2 is designed to have 20 layers, and the thickness of each layer is between 50-200nm; TiO2 is designed to have 20 layers, and the thickness of each layer is between 50-200nm.
[0036] SiO2 and TiO2 are stacked in an alternating manner to form a thin film system: SiO2 / TiO2 / SiO2 / TiO2 / SiO2.
[0037] By adopting the stepped power of the ion source to produce the first thin film material 11 and the second thin film material 31, and using the first thin film material 11 and the second thin film material 31 to alternately stack to produce the low-reflection thin film system 10 and the multi-layer thin film system 30, on the one hand, the density of the film layer is ensured, the roughness of the film interface is reduced, and the fogging of the thin film system is avoided. On the other hand, the stress of the film caused by excessive ion source power is avoided, and the risk of breakage of the glass substrate in subsequent processing technology is reduced.
[0038] Second, as Figure 4 , an infrared cutoff filter, adopts the manufacturing process of the first aspect, including a substrate glass 20, a low-reflection film system 10, and a multi-layer film system 30; the low-reflection film system 10 is manufactured on the first surface of the substrate glass 20, and the multi-layer film system 30 is manufactured on the second surface of the substrate glass 20; the low-reflection film system 10 and the multi-layer film system 30 are respectively formed by alternatingly stacking a first film material 11 and a second film material 31; the first film material 11 is manufactured by ion source step power coating; the second film material 31 is manufactured by ion source step power coating.
[0039] Preferably, the first thin film material 11 includes a first thickness interval, a second thickness interval,..., and an nth thickness interval, and the first thickness interval, the second thickness interval,..., and the nth thickness interval of the first thin film material 11 are respectively coated with a first ion source power, a second ion source power,..., and an nth ion source power; wherein, the first ion source power, the second ion source power,..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval,..., and the nth thickness interval gradually approach the interface of the first thin film material 11.
[0040] Preferably, the second thin film material 31 includes a first thickness range, a second thickness range, ..., and an nth thickness range, and the first thickness range, the second thickness range, ..., and the nth thickness range of the second thin film material 31 are respectively formed by coating with a first ion source power, a second ion source power, ..., and an nth ion source power; The first ion source power, the second ion source power, ... , and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ... , and the nth thickness interval gradually approach the interface of the second thin film material 31 .
[0041] Preferably, the first film material 11 is SiO2 low refractive index material, and the number of layers of the low reflection film system 10 is 7-10 layers.
[0042] Preferably, the second thin film material 31 is a TiO2 high refractive index material, and the number of layers of the multilayer thin film system 30 is 35-45 layers.
[0043] The manufacturing process and infrared cutoff filter of the present invention are implemented by adopting ion source step power to manufacture the first thin film material 11 and the second thin film material 31, and using the first thin film material 11 and the second thin film material 31 to alternately stack to manufacture the low-reflection thin film system 10 and the multilayer thin film system 30. On the one hand, the density of the film layer is ensured, the roughness of the film interface is reduced, and the fogging of the thin film system is avoided. On the other hand, the stress of the film caused by excessive ion source power is avoided, and the risk of breakage of the glass substrate in subsequent processing technology is reduced.
[0044] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A manufacturing process, characterized in that it is used to manufacture an infrared cut-off filter, comprising: Step 100, using ion source step power to produce a first thin film material; Step 200, using ion source step power to make a second thin film material; Step 300, alternately fabricating the first film material and the second film material on the first surface of the substrate glass to obtain a low-reflection film system; Step 400: alternately fabricate the first film material and the second film material on the second surface of the substrate glass to obtain a multilayer film system with high transmittance in the visible light range and cutoff in the infrared light range.
2. The manufacturing process according to claim 1, characterized in that: The step 100 comprises: Step 110, dividing the first film material into a first thickness interval, a second thickness interval, ..., an nth thickness interval in sequence; Step 120, using a first ion source power, a second ion source power, ..., and an nth ion source power to respectively form a first thickness range, a second thickness range, ..., and an nth thickness range of the first thin film material by deposition; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the first thin film material.
3. The manufacturing process according to claim 1, characterized in that: The step 200 comprises: Step 210, dividing the second film material into a first thickness interval, a second thickness interval, ..., an nth thickness interval in sequence; Step 220, using a first ion source power, a second ion source power, ..., and an nth ion source power to respectively form a first thickness range, a second thickness range, ..., and an nth thickness range of the second thin film material by deposition; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness range, the second thickness range, ..., and the nth thickness range of the second thin film material gradually approach the interface of the second thin film material.
4. The manufacturing process according to claim 2, characterized in that: The first film material is SiO2 low refractive index material, and the number of layers of the low reflection film system is 7-10 layers.
5. The manufacturing process according to claim 3, characterized in that: The second thin film material is TiO2 high refractive index material, and the number of layers of the multilayer thin film system is 35-45 layers.
6. An infrared cut-off filter, produced by the process according to any one of claims 1 to 5, characterized in that: include: Base material glass; Low reflection film system; Multilayer film systems; The low-reflection film system is made on the first surface of the substrate glass, and the multi-layer film system is made on the second surface of the substrate glass; The low-reflection film system and the multi-layer film system are respectively formed by alternately stacking a first film material and a second film material; The first thin film material is made by ion source step power coating; The second thin film material is made by ion source step power coating.
7. The infrared cutoff filter according to claim 6, characterized in that: The first thin film material includes a first thickness range, a second thickness range, ..., and an nth thickness range, and the first thickness range, the second thickness range, ..., and the nth thickness range of the first thin film material are respectively formed by coating with a first ion source power, a second ion source power, ..., and an nth ion source power; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the first thin film material.
8. The infrared cutoff filter according to claim 6, characterized in that: The second thin film material includes a first thickness range, a second thickness range, ..., and an nth thickness range, and the first thickness range, the second thickness range, ..., and the nth thickness range of the second thin film material are respectively formed by coating with a first ion source power, a second ion source power, ..., and an nth ion source power; The first ion source power, the second ion source power, ..., and the nth ion source power gradually increase, and the first thickness interval, the second thickness interval, ..., and the nth thickness interval gradually approach the interface of the second thin film material.
9. The infrared cutoff filter according to claim 7, characterized in that: The first film material is SiO2 low refractive index material, and the number of layers of the low reflection film system is 7-10 layers.
10. The infrared cutoff filter according to claim 8, characterized in that: The second thin film material is TiO2 high refractive index material, and the number of layers of the multilayer thin film system is 35-45 layers.