Biosensor with bridge-shaped multi-grid tunneling field effect transistor and preparation method of biosensor

By setting up a biomolecular detection chamber around the bridge source area of ​​the H-shaped bridge double PIN structure, the problem of insufficient conduction current and low sensitivity of the tunneling field effect transistor at low voltage is solved, and fast conduction and high sensitivity are achieved biomolecular detection.

CN119029038APending Publication Date: 2024-11-26XIDIAN UNIV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411115908.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

There are problems such as insufficient conduction current at low voltage, large subthreshold swing and low sensitivity based on tunneling field effect transistors.

Method used

A bridge-shaped multi-gate tunneling field effect transistor is designed, and four biomolecular detection chambers are arranged around the bridge-shaped source region of the H-shaped bridge-shaped double PIN structure, thereby enlarging the cavity area that accommodates the biomolecules. Improved band bending degree of gate voltage to source/channel junction.

Benefits of technology

The device is quickly turned on at low voltage, reducing the sub-threshold swing and threshold voltage, improving the sensitivity and conduction current of biomolecular detection, and overcoming the defect of insufficient conduction current in traditional TFET devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119029038A_ABST
    Figure CN119029038A_ABST
Patent Text Reader

Abstract

The invention discloses a biosensor with a bridge-shaped multi-grid tunneling field effect transistor and a preparation method thereof, the biosensor comprises a source region, two T-shaped channels are symmetrically arranged on two horizontal sides of the source region, and the bottom of the vertical part of each T-shaped channel is sequentially covered with a drain region and a drain electrode; the source region, the T-shaped channels on the two sides of the source region and the drain region form an H-shaped bridge-shaped double-PIN structure; the two vertical sides of the source region are covered with source electrodes, the two horizontal sides of each source electrode are provided with L-shaped biomolecule detection cavities located on the T-shaped channel, the top of the vertical part of each biomolecule detection cavity is covered with a gate oxide layer, and the top of the horizontal part of each biomolecule detection cavity is covered with a gate electrode; the gate oxide layer and the gate are horizontally aligned with the edge of the vertical part of the channel; according to the invention, the technical problems of insufficient device conduction current, large sub-threshold swing and low sensitivity when a field effect transistor detects biomolecules under low voltage are solved, and the sensitivity is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor devices, and in particular relates to a biosensor with a bridge-shaped multi-gate tunneling field effect transistor and a preparation method thereof. Background Art

[0002] A biosensor is a device that can detect specific molecules or biological events in an organism, converting biological signals into measurable electrical signals. With the continuous development of the biomedical field, biosensors play an increasingly important role in medical diagnosis, environmental monitoring, and food safety. The design and development of biosensors allow people to understand the situation in the body more quickly and accurately, promote the development of medical diagnosis and treatment, and also provide more effective means for environmental protection and food safety. Field effect transistor (FET)-based biosensors convert biological signals into electrical signals through biorecognition. They have a fast response speed, high detection accuracy, and low cost, so they have a very broad research prospect.

[0003] The first field effect transistor (FET) based biosensor was discovered by Bergveld in 1970, where a MOS transistor and glass electrode were used to detect ion activity. Since then, FET based sensing research has continued with increasing demand for various environmental, chemical, physical, and biological targets due to its attractive sensitivity, low cost, lightweight, and large-scale production advantages. These FET based biosensors have modern research prospects in the fields of energy production, parametric simulation and modeling, medical diagnostics, and analyzing biomolecular properties. However, these FET based biosensors face several complex issues and need to deal with the trade-offs of the semiconductor industry in terms of multiple short channel effects (SCE), high subthreshold swing (SS), and response time.

[0004] Recently, biosensors based on tunneling field effect transistors (TFETs) have attracted attention due to their design compatibility, small size, compatibility with CMOS manufacturing processes, mass production potential, label-free electrical detection, etc. They can be used to detect neutral or charged biomolecules using dielectric modulation (DM) technology, and also show excellent performance in terms of response speed because their subthreshold swing is not limited to 60 mV / dec at room temperature.

[0005] Cherik et al. proposed a new biosensor based on the concept of a covering layer (Cherik IC, Mohammadi S. Dielectric Modulated Doping-Less Tunnel Field-Effect Transistor, a Novel Biosensor Based on Cladding Layer Concept[J]. IEEE sensors journal, 2022, 22(11): 10308-10314.), which used the concept of a covering layer to introduce holes in the Ge source region. Two nanocavities for filling biological molecules were carved out in the cladding layer; however, the source region used germanium and the channel used silicon, which resulted in certain lattice defects in the source region and the channel, causing the performance of the device to deteriorate, but the sensitivity was not high.

[0006] Mukhopadhyay et al. proposed a diagonal tunneling dielectric modulated tunnel field effect transistor architecture (Mukhopadhyay SJ, Majumdar B, Chappanda K, et al. Performance Analysis of the Diagonal Tunneling-Based Dielectrically Modulated Tunnel FET for Bio-Sensing Applications[J]. IEEE sensors journal, 2021. DOI: 10.1109 / JSEN.2021.3103998.) for label-free biosensing applications; however, the electrical properties of diagonal tunneling before and after coupling with biomolecules do not change much, and its subthreshold swing and operating voltage are large, which is not suitable for application in the low-power field. Summary of the invention

[0007] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a biosensor with a bridge-shaped multi-gate tunneling field effect transistor and a preparation method thereof. By arranging four biomolecule detection cavities around the bridge-shaped source region of the H-type bridge-shaped double PIN structure, the cavity area for accommodating biomolecules can be increased, and the degree of band bending at the source region / channel junction due to the gate voltage can be effectively improved, thereby solving the technical problems of insufficient device on-current under low voltage, large subthreshold swing and low sensitivity of field effect transistors when detecting biomolecules.

[0008] In order to achieve the above object, the technical solution adopted by the present invention is as follows:

[0009] A biosensor with a bridge-shaped multi-gate tunneling field effect transistor comprises a source region 1, two T-shaped channels 4 are axially symmetrically arranged on the horizontal sides of the source region 1, and the bottom of the vertical part of the T-shaped channel 4 is sequentially covered with a drain region 5 and a drain electrode 8; the source region 1, the T-shaped channels 4 on both sides of the source region 1, and the drain region 5 form an H-shaped bridge-shaped double PIN structure; the vertical sides of the source region 1 are covered with source electrodes 6, and the horizontal sides of each source electrode 6 are provided with L-shaped biomolecule detection cavities 2 located on the T-shaped channels 4, the top of the vertical part of each biomolecule detection cavity 2 is covered with a gate oxide layer 3, and the top of the horizontal part of each biomolecule detection cavity 2 is covered with a gate 7, and the gate oxide layer 3 and the gate 7 are horizontally aligned with the edge of the vertical part of the channel 4.

[0010] The T-shaped channel 4 is an N-type lightly doped region with a doping concentration of 1×10 15 ~1×10 17 cm -3 , source region 1 is a P-type heavily doped region with a doping concentration of 5×10 18 ~1×10 20 cm -3 , the drain region 5 is an N-type heavily doped region with a doping concentration of 1×10 18 ~1×10 19 cm -3 .

[0011] The length of the vertical part of the T-shaped channel 4 is 10-20nm, and the length of the horizontal part is 8-12nm; the length of the source region 1 is 20-30nm; the thickness of the vertical part of the T-shaped channel 4 is 40-50nm, and the thickness of the horizontal part is 10-15nm; the thickness of the source region 1 is the same as the horizontal part of the T-shaped channel 4; the thickness of the biomolecule detection cavity 2 is 5-8nm, the thickness of the gate oxide layer 3 is 3-5nm; the thickness of the drain region 5 is 10-15nm.

[0012] The gate oxide layer 3 is made of HfO2, Al2O3 or SiO2, the source 6 and the drain 8 are made of polysilicon, and the gate 7 is made of metal hafnium, metal chromium or metal aluminum.

[0013] A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor as described above comprises the following steps:

[0014] Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor using an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer;

[0015] Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region 5; continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region;

[0016] Step 3: using an atomic layer deposition process to deposit HfO2, Al2O3 or SiO2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region;

[0017] Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P + Ion implantation is performed to form a source region 1 and T-shaped channels 4 located on both sides of the source region 1; thermal annealing is then performed;

[0018] Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer 3 and an L-shaped biomolecule detection cavity 2 located at the bottom of the gate oxide layer 3;

[0019] Step 6: depositing metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity 2 by a reactive sputtering process to form a gate 7;

[0020] Step 7: Using chemical vapor deposition process, polysilicon is deposited on both vertical sides of the source region 1 formed in step 4 to form a source electrode 6; polysilicon is deposited at the bottom of the drain region 5 formed in step 2 to form a drain electrode 8, and finally a biosensor with a bridge-shaped multi-gate tunneling field effect transistor is formed.

[0021] In step 1, the N-type semiconductor is a single crystal silicon wafer.

[0022] The doping concentration of the N-type heavily doped semiconductor in step 1 is 1×10 18 ~1×10 19 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 15 ~1×10 17 cm -3 .

[0023] In step 2, the etching regions of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer have the same length.

[0024] In step 4, thermal annealing is performed at 800-1000°C for 50-80 minutes; the doping concentration of the source region 1 is 5×10 18 ~1×10 20 cm -3 .

[0025] The parameters of the epitaxial growth process in step 1 are: growth temperature is 800-1200° C., growth gases are hydrogen and silane, the flow rate of silicon source gas is 50-100 sccm, the flow rate of hydrogen as carrier gas is 200-240 sccm, and the chamber pressure is 90-100 Pa; the dopant gas is phosphine (PH3);

[0026] The parameters of the dry etching process in step 2 are: the etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 50-60 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 30-50 sccm; the etching temperature is controlled at 25-30° C., the etching pressure is 80-85 mTorr, and the etching time is 30-50 min;

[0027] The parameters of the atomic layer deposition process in step 3 are: the precursor for depositing HfO2 is trimethoxy hafnium, the precursor for depositing SiO2 is dimethyl silicon oxide, and the precursor for depositing Al3O2 is trimethoxy aluminum; the purge gas is oxygen or nitrogen, the oxidant is water vapor, the temperature is controlled at 200-400° C., and the ambient pressure is maintained at 2-10 Torr; the thickness increased by 5-20 angstroms per cycle;

[0028] The parameters of the dry etching process in step 4 are: etching gas is hydrogen fluoride (HF), gas flow rate is 20-80 sccm, etching pressure is 10-50 mTorr, temperature is 20-25° C., and etching time is 20-30 min;

[0029] The parameters of the mask lithography technology are as follows: positive photoresist is used for photolithography, the photoresist coating speed is 3000-5000rpm, the pre-baking temperature is 90-100℃, and the time is 1-2min; ultraviolet light (UV) or deep ultraviolet light (DUV) is used for exposure, the exposure time is 30-90s, and then NaOH or KOH solution is used as a developer, and the development time is 60-90s; the mask is aligned, boron or indium is used as a dopant, and the energy of the injected ions is 30-60keV; Acetone (acetone) or NMP is used to remove the photoresist, and the removal time is 5-10min;

[0030] The parameters of the dry etching process in step 5 are: using an inductively coupled plasma (ICP) etcher to dry etch the reserved oxide layer formed in step 5, the etching gas is hydrogen fluoride (HF), the gas flow rate is 50-65 sccm, the reaction chamber pressure is 50-70 mTorr, the radio frequency power is 300-400 W, and the etching frequency is 13.56 MHz;

[0031] The parameters of the reactive sputtering process in step 6 are: target material temperature is 300-600°C, substrate temperature is 100-300°C, and the pressure of the sputtering chamber is 10 -8 ~10 -6 Torr, the sputtering power of the target material of the gate 7 is 40 to 180 W;

[0032] The parameters of the chemical vapor deposition process in step 7 are: the preheating temperature of the reaction chamber is 500-700°C, the pressure in the chamber is 10 2 ~10 3 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2), the gas flow rate is 5 to 10 sccm, and the diluent gas is hydrogen, the gas flow rate is 50 to 80 sccm.

[0033] Compared with the prior art, the present invention has the following beneficial effects:

[0034] (1) The present invention significantly increases the coupling modulation of the effective gate voltage on the source / channel junction energy band by arranging vertically placed biomolecule detection cavities around the bridge of the H-type bridge-shaped double PIN structure, so that the biosensor has a faster switching characteristic; compared with the traditional horizontally placed biomolecule detection cavity, the coupling degree between the gate and the channel is higher, so when the power supply voltage is not high, the energy band bending on the side of the biomolecule detection cavity close to the T-shaped channel can make the carrier enter the on state faster, with a smaller subthreshold swing and threshold voltage; when biomolecules with different dielectric constants or different charge densities enter the cavity, the difference in the change of electrical characteristics is also greater, so it has a high sensitivity.

[0035] (2) The present invention has a larger tunneling junction area than the traditional TFET structure by axially symmetrically arranging two T-channels with lower doping concentrations on both sides of the source region. In addition, the four sides of the source region can be controlled by the gate voltage. As the voltage increases, the probability of carrier tunneling around the source region increases sharply, thus overcoming the defect of insufficient on-current in traditional TFET devices.

[0036] (3) The biosensor of the present invention is prepared based on a vertical tunneling field effect transistor, and has a simple preparation process, low manufacturing cost and high production efficiency.

[0037] In summary, compared with the prior art, the present invention can increase the cavity area for accommodating biological molecules by arranging four biological molecule detection cavities around the bridge-shaped source region of the H-type bridge-shaped double PIN structure, effectively improves the degree of band bending at the source region / channel junction caused by the gate voltage, and solves the technical problems of insufficient device on-current at low voltage, large subthreshold swing and low sensitivity of field effect transistors when detecting biological molecules. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 This is a schematic diagram of the structure of the biosensor provided by the present invention.

[0039] Figure 2 This is a process flow chart for preparing the biosensor provided by the present invention.

[0040] Figure 3 This is a transfer characteristic curve diagram of computer-aided design software simulation of Example 1 provided by the present invention.

[0041] Figure 4 This is a sensitivity comparison diagram of Example 1 provided by the present invention when detecting biomolecules with different dielectric constants.

[0042] Figure 5 This is a transfer characteristic curve diagram of computer-aided design software simulation of Example 2 provided by the present invention.

[0043] Figure 6 This is a sensitivity comparison diagram of Example 2 provided by the present invention when detecting biomolecules with different dielectric constants.

[0044] Figure 7 This is a transfer characteristic curve diagram of computer-aided design software simulation of Example 3 provided by the present invention.

[0045] Figure 8 This is a sensitivity comparison diagram of Example 3 provided by the present invention when detecting biomolecules with different dielectric constants.

[0046] In the figure: 1 is the source region, 2 is the biomolecule detection cavity, 3 is the gate oxide layer, 4 is the channel, 5 is the drain region, 6 is the source, 7 is the gate, and 8 is the drain. DETAILED DESCRIPTION

[0047] The technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0048] like Figure 1 As shown, a biosensor with a bridge-shaped multi-gate tunneling field effect transistor includes a source region 1, two T-shaped channels 4 are axially symmetrically arranged on the horizontal sides of the source region 1, and the bottom of the vertical part of the T-shaped channel 4 is covered with a drain region 5 and a drain electrode 8 in sequence; the source region 1, the T-shaped channels 4 on both sides of the source region 1, and the drain region 5 form an H-shaped bridge-shaped double PIN structure; the vertical sides of the source region 1 are covered with source electrodes 6, and the horizontal sides of each source electrode 6 are provided with L-shaped biomolecule detection cavities 2 located on the T-shaped channels 4, the top of the vertical part of each biomolecule detection cavity 2 is covered with a gate oxide layer 3, and the top of the horizontal part of each biomolecule detection cavity 2 is covered with a gate 7, and the gate oxide layer 3 and the gate 7 are horizontally aligned with the edge of the vertical part of the channel 4.

[0049] The T-shaped channel 4 is an N-type lightly doped region with a doping concentration of 1×10 15 ~1×10 17 cm -3 , source region 1 is a P-type heavily doped region with a doping concentration of 5×10 18 ~1×10 20 cm -3, the drain region 5 is an N-type heavily doped region with a doping concentration of 1×10 18 ~1×10 19 cm -3 ;

[0050] The gate oxide layer 3 is made of HfO2, Al2O3 or SiO2, the source 6 and the drain 8 are made of polysilicon, and the gate 7 is made of metal hafnium, metal chromium or metal aluminum;

[0051] The length of the vertical part of the T-shaped channel 4 is 10-20nm, and the length of the horizontal part is 8-12nm; the length of the source region 1 is 20-30nm; the thickness of the vertical part of the T-shaped channel 4 is 40-50nm, and the thickness of the horizontal part is 10-15nm; the thickness of the source region 1 is the same as the horizontal part of the T-shaped channel 4; the thickness of the biomolecule detection cavity 2 is 5-8nm, the thickness of the gate oxide layer 3 is 3-5nm; the thickness of the drain region 5 is 10-15nm.

[0052] A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor comprises the following steps:

[0053] Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor by an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer; the N-type semiconductor is a single crystal silicon wafer; the doping concentration of the N-type heavily doped semiconductor is 1×10 18 ~1×10 19 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 15 ~1×10 17 cm -3 ;

[0054] The growth temperature is 800-1200° C., the growth gases are hydrogen and silane, the flow rate of the silicon source gas is 50-100 sccm, and the flow rate of the hydrogen as a carrier gas is 200-240 sccm, and the chamber pressure is 90-100 Pa; during the growth process, an appropriate amount of dopant gas is introduced, and the dopant gas is phosphine (PH3) to dope phosphorus atoms into the N-type silicon crystal, thereby achieving N-type doping;

[0055] Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region 5; continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region; the etching region lengths of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer are the same;

[0056] The etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 50-60 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 30-50 sccm; the etching temperature is controlled at 25-30° C., the etching pressure is 80-85 mTorr, and the etching time is 30-50 min;

[0057] Step 3: using an atomic layer deposition process to deposit HfO2, Al2O3 or SiO2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region;

[0058] The precursor for depositing HfO2 is trimethoxy hafnium, the precursor for depositing SiO2 is dimethyl silicon oxide, and the precursor for depositing Al3O2 is trimethoxy aluminum;

[0059] Before performing atomic layer deposition (ALD), ensure that the surface of the silicon substrate is clean, and chemical cleaning or hydrogen treatment may be required to remove oxides and organic residues to ensure optimal surface receptivity; introduce the precursor into the reaction chamber to adsorb it on the silicon surface, introduce a purge gas, which is oxygen or nitrogen, to remove unreacted precursors and by-products, introduce water vapor as an oxidant to react with the adsorbed precursor to form an etched area film; repeat the purge step to remove by-products and unreacted gases generated during the reaction; control the temperature at 200-400°C and maintain the ambient pressure at 2-10 Torr; increase the thickness of the etched area film by repeating the ALD cycle, with the thickness increasing by 5-20 angstroms per cycle;

[0060] Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P + Ion implantation is performed to form a source region 1 and a T-shaped channel 4 located on both sides of the source region 1; then thermal annealing is performed at 800-1000°C for 50-80 minutes to complete the activation of the impurity ions; the doping concentration of the source region 1 is 5×10 18 ~1×10 20 cm -3 ;

[0061] The etching gas is hydrogen fluoride (HF), the gas flow rate is 20-80 sccm, the etching pressure is 10-50 mTorr, the temperature is 20-25° C., and the etching time is 20-30 min;

[0062] The parameters of mask lithography technology are as follows: positive photoresist is used for photolithography, the photoresist coating speed is 3000-5000rpm, the pre-baking temperature is 90-100℃, and the time is 1-2min; ultraviolet light (UV) or deep ultraviolet light (DUV) is used for exposure, the exposure time is 30-90s, and then NaOH or KOH solution is used as the developer, and the development time is 60-90s; the mask is aligned, and boron or indium is used as the dopant, and the doping concentration is 5×10 18 ~1×10 20 cm -3 The energy of the implanted ions is 30-60 keV; Acetone or NMP is used to remove the photoresist, and the removal time is 5-10 minutes;

[0063] Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer 3 and an L-shaped biomolecule detection cavity 2 located at the bottom of the gate oxide layer 3;

[0064] The reserved oxide layer formed in step 5 is dry-etched by using an inductively coupled plasma (ICP) etcher, wherein the etching gas is hydrogen fluoride (HF), the gas flow rate is 50-65 sccm, the reaction chamber pressure is 50-70 mTorr, the radio frequency power is 300-400 W, and the etching frequency is 13.56 MHz;

[0065] Step 6: depositing metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity 2 by a reactive sputtering process to form a gate 7;

[0066] The target material temperature is 300-600°C, the substrate temperature is 100-300°C, and the pressure in the sputtering chamber is 10 -8 ~10 - 6 Torr, the sputtering power of the target material of the gate 7 is 40 to 180 W;

[0067] Step 7: using a chemical vapor deposition process to deposit polysilicon on both sides of the source region 1 formed in step 4 to form a source electrode 6; depositing polysilicon at the bottom of the drain region 5 formed in step 2 to form a drain electrode 8, and finally forming a biosensor having a bridge-shaped multi-gate tunneling field effect transistor;

[0068] The preheating temperature of the chemical vapor deposition (CVD) reaction chamber is 500-700°C and the pressure in the chamber is 10 2 ~10 3 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2), the gas flow rate is 5 to 10 sccm, and the diluent gas is hydrogen, the gas flow rate is 50 to 80 sccm.

[0069] Example 1

[0070] A biosensor with a bridge-shaped multi-gate tunneling field effect transistor, wherein the length of the vertical portion of the T-shaped channel 4 is 10nm, and the length of the horizontal portion is 8nm; the length of the source region 1 is 20nm; the thickness of the vertical portion of the T-shaped channel 4 is 40nm, and the thickness of the horizontal portion is 10nm; the thickness of the source region 1 is the same as that of the horizontal portion of the T-shaped channel 4; the thickness of the biomolecule detection cavity 2 is 5nm, the thickness of the gate oxide layer 3 is 3nm; and the thickness of the drain region 5 is 10nm.

[0071] A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor comprises the following steps:

[0072] Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor by an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer; the N-type semiconductor is a single crystal silicon wafer; the doping concentration of the N-type heavily doped semiconductor is 1×10 18 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 15 cm -3 ;

[0073] The growth temperature is 800° C., the growth gases are hydrogen and silane, the flow rate of the silicon source gas is 50 sccm, the flow rate of the hydrogen as a carrier gas is 200 sccm, and the chamber pressure is 90 Pa; during the growth process, an appropriate amount of dopant gas is introduced, and the dopant gas is phosphine (PH3) to dope phosphorus atoms into the N-type silicon crystal, thereby achieving N-type doping;

[0074] Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region 5; continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region; the etching region lengths of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer are the same;

[0075] The etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 50 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 30 sccm; the etching temperature is controlled at 25° C., the etching pressure is 80 mTorr, and the etching time is 30 min;

[0076] Step 3: using an atomic layer deposition process to deposit SiO2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region;

[0077] The precursor for depositing SiO2 is dimethyl silicon oxide;

[0078] Before performing atomic layer deposition (ALD), ensure that the surface of the silicon substrate is clean, and chemical cleaning or hydrogen treatment may be required to remove oxides and organic residues to ensure optimal surface receptivity; introduce the precursor into the reaction chamber to adsorb it on the silicon surface, introduce a purge gas, which is oxygen, to remove unreacted precursors and by-products, introduce water vapor as an oxidant to react with the adsorbed precursor to form an etched area film; repeat the purge step to remove by-products and unreacted gases generated during the reaction; control the temperature at 200°C and maintain the ambient pressure at 2Torr; increase the thickness of the etched area film by repeating the ALD cycle, with each cycle increasing the thickness by 5 angstroms;

[0079] Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P + Ion implantation is performed to form a source region 1 and a T-shaped channel 4 located on both sides of the source region 1; then thermal annealing is performed at 800°C for 50 minutes; the doping concentration of the source region 1 is 5×10 18 cm -3 ;

[0080] The etching gas is hydrogen fluoride (HF), the gas flow rate is 20sccm, the etching pressure is 10mTorr, the temperature is 20°C, and the etching time is 20min; positive photoresist is selected for photolithography, the photoresist coating speed is 3000rpm, the pre-baking temperature is 90°C, and the time is 1min; ultraviolet light (UV) is selected for exposure, the exposure time is 30s, and then NaOH solution is used as a developer, and the development time is 60s; the mask is aligned, boron is used as a dopant, and the energy of the injected ions is 30keV; Acetone is used to remove the photoresist, the removal time is 5min, and finally thermal annealing is performed to complete the activation of the impurity ions;

[0081] Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer 3 and an L-shaped biomolecule detection cavity 2 located at the bottom of the gate oxide layer 3;

[0082] The reserved oxide layer formed in step 5 is dry-etched by using an inductively coupled plasma (ICP) etcher, wherein the etching gas is hydrogen fluoride (HF), the gas flow rate is 50 sccm, the reaction chamber pressure is 50 mTorr, the radio frequency power is 300 W, and the etching frequency is 13.56 MHz;

[0083] Step 6: depositing metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity 2 by a reactive sputtering process to form a gate 7;

[0084] The target material temperature is 300°C, the substrate temperature is 100°C, and the pressure in the sputtering chamber is 10 -6 Torr, the sputtering power of the target material of the gate 7 is 40W;

[0085] Step 7: using a chemical vapor deposition process to deposit polysilicon on both sides of the source region 1 formed in step 4 to form a source electrode 6; depositing polysilicon at the bottom of the drain region 5 formed in step 2 to form a drain electrode 8, and finally forming a biosensor having a bridge-shaped multi-gate tunneling field effect transistor;

[0086] The preheat temperature of the chemical vapor deposition (CVD) reaction chamber is 500°C and the pressure in the chamber is 10 2 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2) with a gas flow rate of 5sccm, and the diluent gas is hydrogen with a gas flow rate of 50sccm.

[0087] Reference Figure 3 , the transfer characteristic curve obtained by using the biosensor of Example 1 to detect biomolecules with different dielectric constants, wherein K=2, 7, 12 represent biomolecules with different dielectric constants, and K=1 represents the dielectric constant of air, i.e., the situation when no biomolecules enter, V DS represents the drain-source voltage; since there are biomolecule detection cavities 2 around the bridge-shaped source region 1 of the H-type bridge-shaped double PIN structure, the coupling modulation of the effective gate voltage on the energy band at the source region / channel junction can be increased, so that the biosensor has a faster switching characteristic, and the source region 1 adopts a bridge-shaped structure, which also makes the biosensor have a higher on-current. Figure 3 It can be seen that when detecting biological molecules with K = 12, the value reached about 3.74×10 -5 A / μm, reaching about 5.49×10 -6 A / μm, reaching about 7.82×10 -10 A / μm, and the leakage current of the biosensor (I OFF ) is also relatively low, about 9.54×10 -17 A / μm, indicating that the biosensor has low power consumption.

[0088] Reference Figure 4 , Figure 4 : is a sensitivity comparison diagram of the biosensor of Example 1 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. The sensitivity is obtained by calculating the ratio of the saturated conduction current when biomolecules with different dielectric constants enter the cavity to the saturated conduction current when air enters the cavity, where V GS Represents the drain-source voltage, V DS Represents the drain-source voltage. Figure 4It can be seen that the sensitivity is about 8.47 when detecting biomolecules with K = 2, and the sensitivity is about 6.0×10 6 , when detecting biological molecules with K=12, it is about 4.1×10 7 , indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with larger dielectric constants. Compared with the traditional TFET biosensor, the sensitivity of the biomolecules with K=2 is improved by about 18.6 times, and the sensitivity of the biomolecules with K=7 is improved by about 1.7×10 4 times, and the detection of K = 12 biomolecules has been improved by about 1.9 × 10 4 times, indicating that the biosensor prepared by the present invention has higher sensitivity.

[0089] Example 2

[0090] A biosensor with a bridge-shaped multi-gate tunneling field effect transistor, wherein the length of the vertical portion of the T-shaped channel 4 is 20nm, and the length of the horizontal portion is 12nm; the length of the source region 1 is 30nm; the thickness of the vertical portion of the T-shaped channel 4 is 50nm, and the thickness of the horizontal portion is 15nm; the thickness of the source region 1 is the same as that of the horizontal portion of the T-shaped channel 4; the thickness of the biomolecule detection cavity 2 is 8nm, the thickness of the gate oxide layer 3 is 5nm; and the thickness of the drain region 5 is 15nm.

[0091] A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor comprises the following steps:

[0092] Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor by an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer; the N-type semiconductor is a single crystal silicon wafer; the doping concentration of the N-type heavily doped semiconductor is 1×10 19 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 17 cm -3 ;

[0093] The growth temperature is 1200° C., the growth gases are hydrogen and silane, the flow rate of the silicon source gas is 100 sccm, the flow rate of the hydrogen as a carrier gas is 240 sccm, and the chamber pressure is 100 Pa; during the growth process, an appropriate amount of dopant gas is introduced, and the dopant gas is phosphine (PH3) to dope phosphorus atoms into the N-type silicon crystal, thereby achieving N-type doping;

[0094] Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region 5; continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region; the etching region lengths of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer are the same;

[0095] The etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 60 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 50 sccm; the etching temperature is controlled at 30° C., the etching pressure is 85 mTorr, and the etching time is 50 min;

[0096] Step 3: using an atomic layer deposition process to deposit Al3O2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region;

[0097] The precursor for depositing Al3O2 is trimethoxyaluminum;

[0098] Before performing atomic layer deposition (ALD), ensure that the surface of the silicon substrate is clean, and chemical cleaning or hydrogen treatment may be required to remove oxides and organic residues to ensure optimal surface receptivity; introduce the precursor into the reaction chamber to adsorb it on the silicon surface, introduce a purge gas, which is nitrogen, to remove unreacted precursors and by-products, introduce water vapor as an oxidant to react with the adsorbed precursor to form an etched area film; repeat the purge step to remove by-products and unreacted gases generated during the reaction; control the temperature at 400°C and maintain the ambient pressure at 10 Torr; increase the thickness of the etched area film by repeating the ALD cycle, with each cycle increasing the thickness by 20 angstroms;

[0099] Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P + Ion implantation is performed to form a source region 1 and a T-shaped channel 4 located on both sides of the source region 1; then thermal annealing is performed at 1000°C for 80 minutes; the doping concentration of the source region 1 is 1×10 20 cm -3 ;

[0100] The etching gas is hydrogen fluoride (HF), the gas flow rate is 80sccm, the etching pressure is 50mTorr, the temperature is 25°C, and the etching time is 30min; positive photoresist is selected for photolithography, the photoresist coating speed is 5000rpm, the pre-baking temperature is 100°C, and the time is 2min; deep ultraviolet light (DUV) is selected for exposure, the exposure time is 90s, and then KOH solution is used as a developer, and the development time is 90s; the mask is aligned, indium is used as a dopant, and the energy of the injected ions is 60keV; NMP is used to remove the photoresist, the removal time is 10min, and finally thermal annealing is performed to complete the activation of the impurity ions;

[0101] Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer 3 and an L-shaped biomolecule detection cavity 2 located at the bottom of the gate oxide layer 3;

[0102] The reserved oxide layer formed in step 5 is dry-etched by using an inductively coupled plasma (ICP) etcher, wherein the etching gas is hydrogen fluoride (HF), the gas flow rate is 65 sccm, the reaction chamber pressure is 70 mTorr, the radio frequency power is 400 W, and the etching frequency is 13.56 MHz;

[0103] Step 6: depositing metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity 2 by a reactive sputtering process to form a gate 7;

[0104] The target material temperature is 600°C, the substrate temperature is 300°C, and the pressure in the sputtering chamber is 10 -8 Torr, the sputtering power of the target material of the gate 7 is 180W;

[0105] Step 7: using a chemical vapor deposition process to deposit polysilicon on both sides of the source region 1 formed in step 4 to form a source electrode 6; depositing polysilicon at the bottom of the drain region 5 formed in step 2 to form a drain electrode 8, and finally forming a biosensor having a bridge-shaped multi-gate tunneling field effect transistor;

[0106] The preheat temperature of the chemical vapor deposition (CVD) reaction chamber is 700°C and the pressure in the chamber is 10 3 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2) with a gas flow rate of 10sccm, and the diluent gas is hydrogen with a gas flow rate of 80sccm.

[0107] Reference Figure 5 The transfer characteristic curve obtained by using the biosensor of Example 2 to detect biomolecules with different dielectric constants is as follows: Figure 5 It can be seen that when detecting biological molecules with K = 12, the value reached about 2.07×10 -5A / μm, reaching about 2.51×10 -6 A / μm, reaching about 1.85×10 -10 A / μm, with a higher on-state current; at the same time, the leakage current (I OFF ) is also relatively low, about 1.26×10 -16 A / μm, indicating that the biosensor has low power consumption.

[0108] Reference Figure 6 , Figure 6 The figure is a comparison of the sensitivity of the biosensor of Example 2 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. Figure 6 It can be seen that the sensitivity is about 1.0×10 4 , the sensitivity is about 1.4×10 8 , when detecting biological molecules with K=12, it is about 1.2×10 9 , indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with larger dielectric constants. Compared with the traditional TFET biosensor, the sensitivity of the biomolecules with K=2 is increased by about 229.3 times, and the sensitivity of the biomolecules with K=7 is increased by about 3.9×10 5 times, and improved by about 5.5×10 when detecting biological molecules with K=12 compared to traditional TFET biosensors. 5 times, indicating that the biosensor prepared by the present invention has higher sensitivity.

[0109] Example 3

[0110] A biosensor with a bridge-shaped multi-gate tunneling field effect transistor, wherein the length of the vertical portion of the T-shaped channel 4 is 15nm, and the length of the horizontal portion is 10nm; the length of the source region 1 is 25nm; the thickness of the vertical portion of the T-shaped channel 4 is 45nm, and the thickness of the horizontal portion is 12nm; the thickness of the source region 1 is the same as that of the horizontal portion of the T-shaped channel 4; the thickness of the biomolecule detection cavity 2 is 6nm, the thickness of the gate oxide layer 3 is 4nm; and the thickness of the drain region 5 is 12nm.

[0111] A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor comprises the following steps:

[0112] Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor by an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer; the N-type semiconductor is a single crystal silicon wafer; the doping concentration of the N-type heavily doped semiconductor is 5×1018 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 16 cm -3 ;

[0113] The growth temperature is 1000° C., the growth gases are hydrogen and silane, the flow rate of the silicon source gas is 70 sccm, the flow rate of the hydrogen as a carrier gas is 220 sccm, and the chamber pressure is 90 Pa; during the growth process, an appropriate amount of dopant gas is introduced, and the dopant gas is phosphine (PH3) to dope phosphorus atoms into the N-type silicon crystal, thereby achieving N-type doping;

[0114] Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region 5; continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region; the etching region lengths of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer are the same;

[0115] The etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 55 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 40 sccm; the etching temperature is controlled at 25° C., the etching pressure is 80 mTorr, and the etching time is 40 min;

[0116] Step 3: using an atomic layer deposition process to deposit HfO2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region;

[0117] The precursor for depositing HfO2 is hafnium trimethoxide;

[0118] Before performing atomic layer deposition (ALD), ensure that the surface of the silicon substrate is clean, and chemical cleaning or hydrogen treatment may be required to remove oxides and organic residues to ensure optimal surface acceptance; introduce the precursor into the reaction chamber to make it adsorb on the silicon surface, introduce a purge gas, the purge gas is oxygen, remove unreacted precursors and by-products, introduce water vapor as an oxidant, and react with the adsorbed precursor to form an etched area film; repeat the purge step to remove by-products and unreacted gases generated during the reaction; the temperature is controlled at 300°C and the ambient pressure is maintained at 5Torr; the thickness of the etched area film is increased by repeating the ALD cycle, and the thickness is increased by 10 angstroms per cycle;

[0119] Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P +Ion implantation is performed to form a source region 1 and a T-shaped channel 4 located on both sides of the source region 1; then thermal annealing is performed at 900°C for 60 minutes; the doping concentration of the source region 1 is 1×10 19 cm -3 ;

[0120] The etching gas is hydrogen fluoride (HF), the gas flow rate is 50sccm, the etching pressure is 30mTorr, the temperature is 20°C, and the etching time is 25min; positive photoresist is selected for photolithography, the photoresist coating speed is 4000rpm, the pre-baking temperature is 90°C, and the time is 2min; ultraviolet light (UV) is selected for exposure, the exposure time is 50s, and then NaOH solution is used as a developer, and the development time is 80s; the mask is aligned, boron is used as a dopant, and the energy of the injected ions is 50keV; Acetone is used to remove the photoresist, and the removal time is 8min, and finally thermal annealing is performed to complete the activation of the impurity ions;

[0121] Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer 3 and an L-shaped biomolecule detection cavity 2 located at the bottom of the gate oxide layer 3;

[0122] The reserved oxide layer formed in step 5 is dry-etched by using an inductively coupled plasma (ICP) etcher, wherein the etching gas is hydrogen fluoride (HF), the gas flow rate is 60 sccm, the reaction chamber pressure is 60 mTorr, the RF power is 350 W, and the etching frequency is 13.56 MHz;

[0123] Step 6: depositing metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity 2 by a reactive sputtering process to form a gate 7;

[0124] The target material temperature is 500°C, the substrate temperature is 200°C, and the pressure in the sputtering chamber is 10 -7 Torr, the sputtering power of the target material of the gate 7 is 120W;

[0125] Step 7: using a chemical vapor deposition process to deposit polysilicon on both sides of the source region 1 formed in step 4 to form a source electrode 6; depositing polysilicon at the bottom of the drain region 5 formed in step 2 to form a drain electrode 8, and finally forming a biosensor having a bridge-shaped multi-gate tunneling field effect transistor;

[0126] The preheat temperature of the chemical vapor deposition (CVD) reaction chamber is 600°C and the pressure in the chamber is 10 3 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2), the gas flow rate is 8sccm, and the diluent gas is hydrogen, the gas flow rate is 60sccm.

[0127] Reference Figure 7 The transfer characteristic curve obtained by using the biosensor of Example 3 to detect biomolecules with different dielectric constants is as follows: Figure 7 It can be seen that when detecting biological molecules with K = 12, the value reached about 3.89×10 -7 A / μm, reaching about 1.01×10 -7 A / μm, reaching about 1.02×10 -10 A / μm, with a higher on-state current; at the same time, the leakage current (I OFF ) is also relatively low, about 1.20×10 -19 A / μm, indicating that the biosensor has low power consumption.

[0128] Reference Figure 8 , Figure 8 The figure is a comparison of the sensitivity of the biosensor of Example 3 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. Figure 8 It can be seen that the sensitivity is about 4.8×10 3 , the sensitivity is about 4.7×10 6 , when detecting biological molecules with K=12, it is about 1.82×10 7 , indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with larger dielectric constants. Compared with the traditional TFET biosensor, the sensitivity of the biomolecules with K=2 is improved by about 105.9 times, and the sensitivity of the biomolecules with K=7 is improved by about 1.3×10 4 times, and improved by about 8.5×10 when detecting biological molecules with K=12 compared to traditional TFET biosensors. 3 times, indicating that the biosensor prepared by the present invention has higher sensitivity.

Claims

1. A biosensor having a bridge-shaped multi-gate tunneling field effect transistor, characterized in that: The invention comprises a source region (1), two T-shaped channels (4) are axially symmetrically arranged on the horizontal sides of the source region (1), and the bottom of the vertical part of the T-shaped channel (4) is sequentially covered with a drain region (5) and a drain electrode (8); the source region (1), the T-shaped channels (4) on both sides of the source region (1), and the drain region (5) form an H-shaped bridge-shaped double PIN structure; the vertical sides of the source region (1) are covered with source electrodes (6), and the horizontal sides of each source electrode (6) are provided with an L-shaped biomolecule detection cavity (2) located on the T-shaped channel (4), the top of the vertical part of each biomolecule detection cavity (2) is covered with a gate oxide layer (3), and the top of the horizontal part of each biomolecule detection cavity (2) is covered with a gate electrode (7), and the gate oxide layer (3) and the gate electrode (7) are horizontally aligned with the edge of the vertical part of the channel (4).

2. A biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 1, characterized in that: The T-shaped channel (4) is an N-type lightly doped region with a doping concentration of 1×10 15 ~1×10 17 cm -3 The source region (1) is a heavily doped P-type region with a doping concentration of 5×10 18 ~1×10 20 cm -3 The drain region (5) is an N-type heavily doped region with a doping concentration of 1×10 18 ~1×10 19 cm -3 .

3. The biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 1, characterized in that: The length of the vertical portion of the T-shaped channel (4) is 10-20 nm, and the length of the horizontal portion is 8-12 nm; the length of the source region (1) is 20-30 nm; the thickness of the vertical portion of the T-shaped channel (4) is 40-50 nm, and the thickness of the horizontal portion is 10-15 nm; the thickness of the source region (1) is the same as that of the horizontal portion of the T-shaped channel (4); the thickness of the biomolecule detection cavity (2) is 5-8 nm, the thickness of the gate oxide layer (3) is 3-5 nm; and the thickness of the drain region (5) is 10-15 nm.

4. The biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 1, characterized in that: The material of the gate oxide layer (3) is HfO2, Al2O3 or SiO2, the material of the source (6) and the drain (8) are both polysilicon, and the material of the gate (7) is metal hafnium, metal chromium or metal aluminum.

5. A method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to any one of claims 1 to 4, characterized in that: The steps include: Step 1: epitaxially grow an N-type silicon layer on an N-type heavily doped semiconductor using an epitaxial growth process to form an N-type lightly doped silicon epitaxial layer; Step 2: using a dry etching process to first etch away the middle region of the N-type heavily doped semiconductor to form a drain region (5); continuing to etch the vertical sides of the N-type lightly doped silicon epitaxial layer until the N-type lightly doped silicon epitaxial layer is etched into an H-type bridge-shaped channel region; Step 3: using an atomic layer deposition process to deposit HfO2, Al2O3 or SiO2 on both sides of the middle bridge body of the H-type bridge channel region to form an oxide layer pre-etching region; Step 4: Use dry etching process to etch the central area of ​​the oxide layer pre-etching area to obtain four reserved oxide layers; at the same time, use mask lithography technology to perform P + Ion implantation is performed to form a source region (1) and T-shaped channels (4) located on both sides of the source region (1); and thermal annealing is then performed; Step 5: dry-etching the four reserved oxide layers using a dry etching process to form a gate oxide layer (3) and an L-shaped biomolecule detection cavity (2) located at the bottom of the gate oxide layer (3); Step 6: using a reactive sputtering process to deposit metal hafnium, metal chromium or metal aluminum on the L-shaped biomolecule detection cavity (2) to form a gate (7); Step 7: Using a chemical vapor deposition process, polysilicon is deposited on both vertical sides of the source region (1) formed in step 4 to form a source electrode (6); polysilicon is deposited at the bottom of the drain region (5) formed in step 2 to form a drain electrode (8), and finally a biosensor having a bridge-shaped multi-gate tunneling field effect transistor is formed.

6. The method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 5, characterized in that: In step 1, the N-type semiconductor is a single crystal silicon wafer.

7. The method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 5, characterized in that: The doping concentration of the N-type heavily doped semiconductor in step 1 is 1×10 18 ~1×10 19 cm -3 The doping concentration of the N-type lightly doped silicon epitaxial layer is 1×10 15 ~1×10 17 cm -3 .

8. The method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 5, characterized in that: In step 2, the etching regions of the N-type heavily doped semiconductor and the N-type lightly doped silicon epitaxial layer have the same length.

9. The method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 5, characterized in that: In step 4, thermal annealing is performed at 800-1000°C for 50-80 minutes; the doping concentration of the source region (1) is 5×10 18 ~1×10 20 cm -3 .

10. The method for preparing a biosensor having a bridge-shaped multi-gate tunneling field effect transistor according to claim 5, characterized in that: The parameters of the epitaxial growth process in step 1 are: growth temperature is 800-1200° C., growth gases are hydrogen and silane, the flow rate of silicon source gas is 50-100 sccm, the flow rate of hydrogen as carrier gas is 200-240 sccm, and the chamber pressure is 90-100 Pa; the dopant gas is phosphine (PH3); The parameters of the dry etching process in step 2 are: the etching gas is hydrogen fluoride (HF), and the etching gas flow rate is 50-60 sccm; the dilution gas is argon fluoride (ArF), and the dilution gas flow rate is 30-50 sccm; the etching temperature is controlled at 25-30° C., the etching pressure is 80-85 mTorr, and the etching time is 30-50 min; The parameters of the atomic layer deposition process in step 3 are: the precursor for depositing HfO2 is trimethoxy hafnium, the precursor for depositing SiO2 is dimethyl silicon oxide, and the precursor for depositing Al3O2 is trimethoxy aluminum; the purge gas is oxygen or nitrogen, the oxidant is water vapor, the temperature is controlled at 200-400° C., and the ambient pressure is maintained at 2-10 Torr; the thickness increased by 5-20 angstroms per cycle; The parameters of the dry etching process in step 4 are: etching gas is hydrogen fluoride (HF), gas flow rate is 20-80 sccm, etching pressure is 10-50 mTorr, temperature is 20-25° C., and etching time is 20-30 min; The parameters of the mask lithography technology are as follows: positive photoresist is used for photolithography, the photoresist coating speed is 3000-5000rpm, the pre-baking temperature is 90-100℃, and the time is 1-2min; ultraviolet light (UV) or deep ultraviolet light (DUV) is used for exposure, the exposure time is 30-90s, and then NaOH or KOH solution is used as a developer, and the development time is 60-90s; the mask is aligned, boron or indium is used as a dopant, and the energy of the injected ions is 30-60keV; Acetone (acetone) or NMP is used to remove the photoresist, and the removal time is 5-10min; The parameters of the dry etching process in step 5 are: using an inductively coupled plasma (ICP) etcher to dry etch the reserved oxide layer formed in step 5, the etching gas is hydrogen fluoride (HF), the gas flow rate is 50-65 sccm, the reaction chamber pressure is 50-70 mTorr, the radio frequency power is 300-400 W, and the etching frequency is 13.56 MHz; The parameters of the reactive sputtering process in step 6 are: target material temperature is 300-600°C, substrate temperature is 100-300°C, and the pressure of the sputtering chamber is 10 -8 ~10 -6 Torr, the sputtering power of the target material of the gate (7) is 40 to 180 W; The parameters of the chemical vapor deposition process in step 7 are: the preheating temperature of the reaction chamber is 500-700°C, the pressure in the chamber is 10 2 ~10 3 Torr; the silicon source gas is dimethylsilane (SiH2(CH3)2), the gas flow rate is 5 to 10 sccm, and the diluent gas is hydrogen, the gas flow rate is 50 to 80 sccm.