Method for detecting swelling capacity of inner hole of heated stainless steel sleeve with length-diameter ratio larger than 5
By using a ceramic cylindrical tube and a dial indicator system to accurately measure the expansion at the center of the inner hole of stainless steel sleeves, the problem of measuring the expansion at the center of the inner hole of stainless steel sleeves with a length-to-diameter ratio greater than 5 after heating is solved, ensuring the smooth installation process and avoiding jamming.
Patent Information
- Application Number
- CN202411490109.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-24
- Publication Date
- 2024-11-29
AI Technical Summary
In the existing technology, it is impossible to accurately measure the expansion of the inner hole center of stainless steel sleeves with an aspect ratio greater than 5 after heating, which may cause jamming during the sleeve insertion process.
A cylindrical tube made of ceramic material with an outer diameter smaller than the inner hole of the steel sleeve is equipped with pulleys and a dial indicator. By measuring the inner diameter of both ends of the stainless steel sleeve as a reference, and combining it with an adjustable connecting rod and a lifting device, the expansion of the center of the inner hole can be accurately measured.
It provides precise measurement data on the expansion of the inner hole center of the stainless steel sleeve, avoiding jamming during the sleeve insertion process and ensuring a stable connection between the stainless steel sleeve and the propeller shaft.
Smart Images

Figure CN119043138A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method capable of measuring the central expansion amount of the inner hole of a stainless steel sleeve with a length-to-diameter ratio greater than 5 on a propeller shaft in a marine propulsion system. Background Art
[0002] Stainless steel sleeves mainly refer to the stainless steel sleeves on the propeller shafts in the marine propulsion system. Figure 2 As shown in the figure, as the load of ship construction becomes larger and larger, the design length of the propeller shaft is also getting longer and longer. In order to ensure the stability of the propeller shaft, two stainless steel sleeves need to be added to the bearing gear position of the propeller shaft. On the one hand, the wear resistance of the bearing gear is increased, and on the other hand, the deformation of the propeller shaft due to its long length can be prevented. The stainless steel sleeve is embedded in the propeller shaft, mainly by heating the stainless steel sleeve to expand it and then insert it into the shaft, and shrink it after cooling, so that it is tightly combined with the shaft. However, due to the thin wall thickness of the stainless steel sleeve, generally about 20mm, the stainless steel sleeve with a length-to-diameter ratio greater than 5 is an extra-long steel sleeve. The overall heating temperature of the outer circle of the steel sleeve is 200-220℃, and the inner hole expansion is about 1.6mm. In practical operation, after the stainless steel sleeve is heated, it is more convenient to measure the inner hole expansion at the two end faces of the steel sleeve, but the inner hole expansion at the center of the steel sleeve cannot be measured. If the expansion of the center of the steel sleeve is too small, it will cause "stuck" phenomenon during the sleeve insertion process. Summary of the invention
[0003] Design purpose: In view of the problems existing in the background technology, a method for detecting the expansion of the inner hole of a stainless steel sleeve with a length-to-diameter ratio greater than 5 after heating is designed, which can accurately measure the expansion of the center of the inner hole of the stainless steel sleeve during the heating process to avoid the "stuck" phenomenon of the stainless steel sleeve during the insertion process due to the small expansion of the center of the inner hole of the stainless steel sleeve.
[0004] Design scheme: In order to achieve the above design objectives. The present invention has the following design scheme: Before heating the stainless steel sleeve, the inner hole size is measured at room temperature as the reference size, and the inner diameter at both end faces of the stainless steel sleeve is measured with an inner diameter micrometer. The measurement of the inner hole center of the stainless steel sleeve adopts the following method: Ceramic material is used to make a cylindrical tube (thickness 10mm) with an outer diameter smaller than the inner hole of the steel sleeve. The ceramic material has good high temperature resistance, small deformation under high temperature conditions, and high stability. The specific corresponding dimensions are as follows: Two sets of pulleys (two in each set) and a dial indicator (see Figure 3 ), the angle distribution is 120°, the 4 pulleys mainly support the ceramic cylinder and can slide freely in the sleeve, the dial indicator is installed on the top of the ceramic cylinder and connected to the sensor. The inner cavity of the ceramic cylinder is supported by a stainless steel plate with a thickness of 16mm, and the center of the stainless steel can be connected to the adjustable connecting rod.
[0005] The specific operations are: (1) The stainless steel sleeve is placed horizontally on the roller bracket, which is fixed on the horizontal ground rail. The roller bracket can be electrically adjusted. Use a horizontal measuring ruler to adjust the horizontal position of the stainless steel sleeve, and the horizontality is controlled within 0.1 mm; see Figure 1 ; (2) First use an inside micrometer to measure the inner diameter of the ports on both sides of the stainless steel sleeve, then place the ceramic cylinder in the inner hole of the stainless steel sleeve, with the dial indicator needle facing upward, and adjust the dial indicator to zero position at one side of the stainless steel sleeve as the measurement reference; (3) Use an adjustable connecting rod to connect the stainless steel support at the center of the ceramic cylinder. The other end of the adjustable connecting rod is connected to the vertical fixed rod. The level of the connecting rod is adjusted by the adjustable lifting device so that the connecting rod and the ceramic cylinder are in the same horizontal position, and the horizontality is controlled within 0.1 mm. (4) Start the motor-driven track flat car and push the ceramic cylinder into the sleeve at a uniform speed along the horizontal track of the ground rail. The pushing speed is controlled at 100 mm / min. (5) When the ceramic cylinder reaches 1 / 2 of the length of the stainless steel sleeve according to the penetration length of the adjustable connecting rod, record the dial indicator data and exit; (6) Turn on the electric roller frame, rotate the stainless steel sleeve 90°, repeat the above operation, and record the measurement data; (7) Keep the ceramic cylinder fixed and rotate the stainless steel sleeve 90°. Repeat the above operation and record the measurement data. After the above operations, the original size of the center of the inner hole of the stainless steel sleeve before heating can be determined.
[0006] (8) The outer circle is wrapped with electric heating rope and heated as a whole. The interval between each circle of electric heating rope is no more than 20mm to ensure the uniform heating of the stainless steel sleeve. After the heating temperature reaches 200-220℃ and the heat is kept, the diameter of the stainless steel sleeve is first measured with an internal micrometer and compared with the size before heating. When the inner hole expansion at the ports on both sides reaches 1.6mm or slightly greater than 1.6mm, the size of the inner hole center is measured. The port size is still used as the reference size. The inner hole expansion is measured according to the above operation method. The advancement speed of the ceramic cylinder is increased to 200mm / min to prevent the high temperature inside the stainless steel sleeve from causing damage to the dial indicator.
[0007] (9) By measuring the expansion at the center of the inner hole, it is determined that when the expansion reaches 1.6 mm or above, stainless steel can be inlaid.
[0008] Compared with the background technology, the present invention solves the bottleneck that the central expansion of the inner hole of the super-long stainless steel sleeve cannot be directly measured after heating, provides accurate measurement data, lays the foundation for the subsequent inlay of the stainless steel sleeve, and completely avoids the "stuck" phenomenon in the inlay process. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 This is an example of the implementation of the present invention. Figure 1 .
[0010] Figure 2 This is an example of the implementation of the present invention. Figure 2 .
[0011] Figure 3 This is an example of the implementation of the present invention. Figure 3 .
[0012] Figure 4 It is a schematic diagram of background technology. DETAILED DESCRIPTION
[0013] Refer to the attached Figure 1-3 A method for detecting the internal expansion of a stainless steel sleeve having an aspect ratio greater than 5 after heating. Before heating the stainless steel sleeve: 1) The stainless steel sleeve is placed horizontally on the roller bracket, which is fixed on the horizontal ground rail. The roller bracket can be electrically adjusted. A horizontal measuring ruler is used to adjust the horizontal position of the stainless steel sleeve, and the horizontality is controlled within 0.1mm; 2) First use an inside micrometer to measure the inner diameter of the ports on both sides of the stainless steel sleeve, then place the ceramic cylinder in the inner hole of the stainless steel sleeve, with the dial indicator needle facing upwards, and adjust the dial indicator to zero position at one side of the stainless steel sleeve as the measurement reference; 3) Use an adjustable connecting rod to connect the stainless steel support at the center of the ceramic cylinder. The other end of the adjustable connecting rod is connected to the vertical fixed rod. The level of the connecting rod is adjusted by the adjustable lifting device so that the connecting rod and the ceramic cylinder are in the same horizontal position, and the horizontality is controlled within 0.1mm; 4) Start the motor-driven track flat car, and push the ceramic cylinder into the sleeve at a uniform speed along the horizontal track of the ground track. The pushing speed is controlled at 100 mm / min; 5) When the ceramic cylinder reaches 1 / 2 of the length of the stainless steel sleeve according to the penetration length of the adjustable connecting rod, record the dial indicator data and exit; 6) Turn on the electric roller frame, rotate the stainless steel sleeve 90°, repeat the above operation, and record the measurement data; 7) Keep the ceramic cylinder fixed and rotate the stainless steel sleeve 90°, repeat the above operation and record the measurement data; After the above operations, the original size of the inner hole center of the stainless steel sleeve before reheating can be determined; After the stainless steel sleeve is heated: (8) The outer circle is wrapped with electric heating rope and heated as a whole. The interval between each circle of electric heating rope is no more than 20mm to ensure the uniform heating of the stainless steel sleeve. After the heating temperature reaches 200-220℃ and the heat is kept, the diameter of the stainless steel sleeve is first measured with an internal diameter micrometer and compared with the size before heating. When the inner hole expansion at the ports on both sides reaches 1.6mm or slightly greater than 1.6mm, the size of the inner hole center is measured. The port size is still used as the reference size. The inner hole expansion is measured according to the above operation method. The ceramic cylinder advancement speed is increased to 200mm / min. By measuring the expansion of the inner hole, it is determined that when the expansion reaches 1.6mm or more, the stainless steel can be inlaid.
[0014] It should be understood that although the above embodiments provide a relatively detailed textual description of the design ideas of the present invention, these textual descriptions are only simple textual descriptions of the design ideas of the present invention, rather than limitations on the design ideas of the present invention. Any combination, addition or modification that does not exceed the design ideas of the present invention shall fall within the protection scope of the present invention.
Claims
1. A method for detecting the expansion of the inner hole center of a stainless steel sleeve with an aspect ratio greater than 5 after heating, characterized in that: 1) The stainless steel sleeve is placed horizontally on the roller bracket, which is fixed on the horizontal ground rail. The roller bracket can be electrically adjusted. A horizontal measuring ruler is used to adjust the horizontal position of the stainless steel sleeve, and the horizontality is controlled within 0.1mm; 2) First use an internal micrometer to measure the inner diameter of the ports on both sides of the stainless steel sleeve, then push the ceramic cylinder horizontally into the center of the inner hole of the stainless steel sleeve, with the dial indicator needle facing upwards, and adjust the dial indicator to zero position at one side of the stainless steel sleeve as the measurement reference; 3) Use an adjustable connecting rod to connect the stainless steel support at the center of the ceramic cylinder. The other end of the adjustable connecting rod is connected to the vertical fixed rod. The level of the connecting rod is adjusted by the adjustable lifting device so that the connecting rod and the ceramic cylinder are in the same horizontal position, and the horizontality is controlled within 0.1mm; 4) Start the motor-driven track flat car, and push the ceramic cylinder into the sleeve at a uniform speed along the horizontal track of the ground track. The pushing speed is controlled at 100 mm / min; 5) When the ceramic cylinder reaches 1 / 2 of the length of the stainless steel sleeve according to the penetration length of the adjustable connecting rod, record the dial indicator data and exit; 6) Turn on the electric roller frame, rotate the stainless steel sleeve 90°, keep the ceramic cylinder from rotating, repeat the above operation, and record the measurement data; After the above operations, the original size of the inner hole center of the stainless steel sleeve before heating can be determined; 7) The outer circle of the stainless steel sleeve is wrapped with electric heating rope and heated as a whole. The interval between each circle of electric heating rope is no more than 20mm to ensure the uniform heating of the stainless steel sleeve. After the heating temperature reaches 200-220℃ and the heat is kept, the diameter of the stainless steel sleeve is first measured with an internal diameter micrometer and compared with the size before heating. When the expansion of the inner hole at the ports on both sides reaches 1.6mm or slightly greater than 1.6mm, the size of the center of the inner hole is measured, and the ceramic cylinder is pushed into the sleeve at a uniform speed along the horizontal track of the ground rail. The pushing speed is controlled at 200mm / min. According to the penetration length of the adjustable connecting rod, when it is judged that the ceramic cylinder has reached 1 / 2 of the length of the stainless steel sleeve, the dial indicator data is recorded and exited, the electric roller frame is turned on, and the stainless steel sleeve is rotated 90°. Keep the ceramic cylinder without rotating, repeat the above operation, measure the expansion of the center of the inner hole, and when the expansion of the center of the inner hole reaches 1.6mm or more, the stainless steel sleeve can be embedded on the shaft.