Microneedle array loaded with metal polyphenol, preparation method and application

Through the microneedle array loaded with metal polyphenols, the problems of endosomal escape and drug waste in intracellular delivery of biological macromolecules are solved, and the efficient delivery of ultra-large-sized plasmids is achieved, and gene editing is achieved in different cells, with extensive biomedical science Application prospects.

CN119157817APending Publication Date: 2024-12-20SUZHOU BANGJIA MEDICAL CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410091053.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-01-23
Publication Date
2024-12-20

AI Technical Summary

Technical Problem

During the delivery process, existing biological macromolecule intracellular delivery vectors have problems such as weak endosomal escape ability, waste of drugs and reduced activity of biological macromolecule, and it is difficult to efficiently deliver super-large-sized plasmids.

Method used

Using a microneedle array loaded with metal polyphenols, a nanocoated layer is formed by dropleting the mixed solution of polyphenols and metal salts to the microneedle array list, using the structure of the microneedle to penetrate the cell membrane, and through the adhesion of the metal polyphenols The combination of biological macromolecules is achieved by using sexual and chemical bonds.

Benefits of technology

Efficient intracellular delivery of biomacromolecules, especially the delivery of ultra-large-sized plasmids, and the vector can be recycled, which improves the drug presentation speed and the activity of biomacromolecules, and significantly improves the transfection efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119157817A_ABST
    Figure CN119157817A_ABST
Patent Text Reader

Abstract

The invention discloses a metal polyphenol loaded microneedle array, a preparation method and application, and the preparation method comprises the following steps: step 1, mixing a polyphenol solution and a metal salt solution to obtain a mixed solution; the molar ratio of polyphenol to metal salt is 4: 1; 2, dropwise adding the mixed solution obtained in the step 1 to the surface of the microneedle array, and cleaning after the mixed solution is deposited; the microneedle array loaded with the metal polyphenol can be obtained; the metal polyphenol loaded microneedle array obtained by the invention provides a biomacromolecule intracellular delivery system which is high in efficiency, high in biocompatibility, easy to operate, low in toxic and side effects and universal; according to the CRISPR / Cas9 vector, the problem of small nucleic acid load (not more than 5000bp) of various virus vectors is solved, the delivery of oversized (15,000-20,000 bp) CRISPR / Cas9 plasmids can be efficiently realized, effective gene editing of multiple gene loci in different cells can be realized, and the CRISPR / Cas9 vector has a wide application prospect in the field of biomedicine.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of biomaterials, and in particular to a metal polyphenol-loaded microneedle array, a preparation method and an application thereof. Background Art

[0002] Intracellular delivery of biomacromolecules refers to the delivery of biomacromolecules into target cells through specific methods, so that they can play relevant biological functions in cells. However, biomacromolecules have high molecular weight, large size, and mostly negative surface charge or a small amount of positive charge (some proteins and peptides), which makes it difficult for them to cross the cell membrane of the target cell and enter the cell. Currently reported macromolecular intracellular delivery carriers mainly include cationic liposomes, inorganic nanomaterials, polymer carriers, viral infection, cell-derived vesicles, etc. However, on the one hand, the biomacromolecules delivered by these methods have weak endosomal escape ability and are easily rapidly degraded by proteases; on the other hand, the method of releasing biomacromolecules from carriers through stimulus response in the intracellular environment often requires chemical or biological modification of biomacromolecules, which will reduce the biological activity of macromolecules.

[0003] Microneedle array is a new and efficient drug delivery technology. Its structure is similar to the needle of a traditional syringe, and the needle tip is symmetrically conical or asymmetrically beveled. The microneedle array has multiple micro needle structures, and the length of the needle is generally several hundred nanometers to several millimeters. Because the microneedles have sufficient length and mechanical strength, they can pierce the cell membrane and reduce the blocking effect of the phospholipid bilayer on the drug. However, when using microneedles alone for drug delivery, it is difficult for the drug to be enriched on the surface of the microneedle, and an excess of the drug needs to be added to dissolve in the solution. On the one hand, there are requirements for the solubility of the drug, and on the other hand, it will also cause a waste of the drug. Summary of the invention

[0004] In view of the problems existing in the prior art, the present invention provides a metal polyphenol-loaded microneedle array, a preparation method and an application thereof.

[0005] The technical solution adopted by the present invention is:

[0006] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0007] Step 1: Mixing a polyphenol solution and a metal salt solution to obtain a mixed solution; the molar ratio of the polyphenol to the metal salt is 4:1;

[0008] Step 2: Add the mixed solution obtained in step 1 dropwise onto the surface of the microneedle array, and wash after the mixed solution is deposited; thus, a microneedle array loaded with metal polyphenols can be obtained.

[0009] Furthermore, the polyphenols in step 1 are one or two or more of anthocyanins, catechins, gallic acid, and tannic acid.

[0010] Furthermore, the metal ion in the metal salt is Fe 3+ , Mn 2+ , Fe 2+ One or two or more of the following.

[0011] Furthermore, the mixed solution in step 1 is vortexed for 10 to 20 seconds, and the sedimentation time in step 2 is 10 to 20 minutes.

[0012] A metal polyphenol-loaded microneedle array has a microneedle height of 1 μm, a microneedle bottom diameter of 0.8 μm, and a center distance between adjacent microneedles of 1.2 μm.

[0013] An application of a microneedle array loaded with metal polyphenols, wherein the microneedle array loaded with metal polyphenols is used as a delivery carrier.

[0014] Furthermore, the metal polyphenol-loaded microneedle array is used as a macromolecular intracellular delivery carrier.

[0015] Furthermore, the metal polyphenol-loaded microneedle array is used to deliver chicken ovalbumin, nucleic acid aptamers, small interfering RNA, polypeptides, and plasmids.

[0016] Furthermore, the metal polyphenol-loaded microneedle array is used in the preparation of drugs.

[0017] A recycling method for a microneedle array loaded with metal polyphenols, wherein the microneedle array loaded with metal polyphenols is placed in a solution with a pH value of 3 to 5 and soaked for 5 to 10 minutes; the microneedle array can be recycled

[0018] The beneficial effects of the present invention are:

[0019] (1) The present invention performs functional modification on the surface of the microneedle array, and forms a nanocoating based on plant polyphenols on the modified microneedles. The nanocoating can effectively load different types of biomacromolecules and achieve cell penetration and delivery of biomacromolecules through the special structure of the microneedles;

[0020] (2) In the present invention, on the one hand, the microneedles can pierce the cell membrane and reduce the blocking effect of the phospholipid bilayer on the drug; on the other hand, the metal polyphenols have adhesion and can carry various biomacromolecules;

[0021] (3) The metal polyphenol coating of the present invention has strong adsorption properties and can also bind to biological macromolecules such as proteins and nucleic acids through hydrogen bonding, π-π stacking, hydrophobic interactions, etc.;

[0022] (4) The phenolic hydroxyl groups in the metal polyphenol coating of the present invention are protonated, forming competitive chelation between proton hydrogen and metal ions, resulting in the disintegration of the coating; therefore, the carrier of the present invention can be recycled and reused. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a morphology of the metal polyphenol loaded microneedle array obtained in Example 1 of the present invention, a is a scanning electron microscope image, the upper part is the unloaded coating, the lower part is the loaded coating, and b is an energy dispersive X-ray spectrum.

[0024] Figure 2 This is an X-ray photoelectron spectrum of the metal polyphenol-loaded microneedle array obtained in Example 1 of the present invention.

[0025] Figure 3 This is a schematic diagram of the cell puncture efficiency of the metal polyphenol-loaded microneedle array obtained in Example 1 of the present invention, a is the fluorescence staining result, and b is the statistical result.

[0026] Figure 4 This is a schematic diagram of the intracellular delivery efficiency of biomacromolecules by the metal polyphenol-loaded microneedle array obtained in Example 1 of the present invention.

[0027] Figure 5 Schematic diagram of the intracellular delivery efficiency of the biomacromolecule OVA of the microneedle array loaded with metal polyphenols and the microneedle array and metal polyphenols alone obtained in Example 1 of the present invention.

[0028] Figure 6 This is a schematic diagram of the intranuclear presentation efficiency of the metal polyphenol-loaded microneedle array obtained in Example 1 of the present invention for super-large-sized plasmids.

[0029] Figure 7 The delivery efficiency of the metal polyphenol-loaded microneedle arrays described in Examples 2 to 5 of the present invention for various biomacromolecules.

[0030] Figure 8 This is the nuclear delivery efficiency of the microneedle array loaded with metal polyphenols for plasmids described in Example 6 of the present invention, a is the result of GFP plasmid, and b is the result of RFP plasmid. DETAILED DESCRIPTION

[0031] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.

[0032] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0033] Step 1: Mix the polyphenol solution and the metal salt solution to obtain a mixed solution; the molar ratio of polyphenol to metal salt is 4:1; the polyphenol is one or two or more of anthocyanin, catechin, gallic acid, and tannic acid. The metal ion in the metal salt is Fe 3+ , Mn 2+ , Fe 2+ One or two or more of the following.

[0034] Step 2: Add the mixed solution obtained in step 1 dropwise onto the surface of the microneedle array, and wash after the mixed solution is deposited; the microneedle array loaded with metal polyphenols can be obtained. The mixed solution is vortexed for 10 to 20 seconds, and the deposition time in step 2 is 10 to 20 minutes.

[0035] A metal polyphenol-loaded microneedle array, wherein the microneedle height is 1 μm, the diameter of the microneedle bottom is 0.8 μm, and the center distance between adjacent microneedles is 1.2 μm (the microneedle array used in the present invention is prepared by existing technology, such as physical vapor deposition, and the improvement of the present invention does not lie in the preparation of the microneedles).

[0036] Example 1

[0037] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0038] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0039] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0040] Figure 1 Figure 1 is a morphology of the metal polyphenol loaded microneedle array obtained in Example 1. a is a scanning electron microscope image, the top is the unloaded coating, the bottom is the loaded coating, and b is an energy dispersive X-ray spectrum. Figure 1 As can be seen in the figure above, the shape and size of the microneedles are highly consistent and evenly arranged, with a height of about 887nm. The microneedle array after loading with metal polyphenols has no obvious changes in size and shape, and the surface functional modification will not have a significant effect on the puncture performance of the microneedles. Figure 1 As can be seen in middle b, the Fe element is evenly distributed on the microneedle.

[0041] Figure 2 The X-ray photoelectron spectrum of the metal polyphenol-loaded microneedle array obtained in Example 1. It can be seen from the figure that the CO single bond ratio on the functionalized microneedles has been significantly improved compared with that without metal polyphenol loading. This is due to the successful loading of tannic acid on its surface. The successful loading of metal polyphenols on the microneedle array enables the microneedles to bind and load biomacromolecules.

[0042] The functionalized modified microneedle array obtained in Example 1 was used to test the cell puncture efficiency, and the method was as follows:

[0043] Place the microneedle in a cell culture dish (needle facing up) and add 1x10 5 cells / mL of cell solution. Place the culture dish in a centrifuge, centrifuge at room temperature, 50g, for 60-100 seconds. Gently blow the cells off the microneedle with PBS (pH 7.4). Use Calcein AM / EthD-1 to stain the cells to test the puncture efficiency of the microneedle. Cells stained with Calcein AM (calcein) and EthD-1 are cells punctured by the microneedle. The results are shown in Figure 3 shown.

[0044] It can be seen from the figure that Calcein-AM can easily penetrate the membrane of living cells, be retained in the cell and emit strong green fluorescence. EthD-1 cannot penetrate the cell membrane of living cells, but can pass through the disordered area of ​​the dead cell membrane to reach the cell nucleus and embed into the cell's DNA double helix to produce red fluorescence. Living cells that have been successfully punctured by microneedles can be stained by Calcein AM and EthD-1 at the same time. Statistics show that the modified microneedle array SNNs have a puncture efficiency of about 98% for cells.

[0045] The functionalized modified microneedle array obtained in Example 1 was used to test the intracellular delivery of biomacromolecules, and the method was as follows:

[0046] When the cells grew to a density of about 80-90%, the culture medium was removed and 2 mL of 0.25% trypsin was added. After the cells shrank and became round under the microscope, 3 mL of complete culture medium was added to terminate the action of trypsin. The cells were dispersed and dropped by blowing. The cells were centrifuged at 200 g for 3 min, the supernatant was discarded, and the cell concentration was adjusted to 1×10 with culture medium containing 10% FBS. 5 cells / mL.

[0047] Place the functionalized microneedles prepared above in a cell culture dish, take 20 μL of biomacromolecules with a concentration of 1 μg / μL and drop them onto the surface of the microneedles, let stand on ice until the liquid is deposited, and then rinse the unbound biomacromolecules with phosphate buffered saline (PBS, pH 7.4). Add the cell suspension, place the cell culture dish in a centrifuge, and centrifuge at 50g for 60 to 100 seconds. Take out the microneedles and gently blow the cells off the microneedles with phosphate buffered saline (PBS, pH 7.4). Different biomacromolecules, including chicken ovalbumin (OVA), nucleic acid aptamers (AS1411), small interfering ribonucleic acid (siRNA), polypeptides (Polypeptide) and plasmids were prepared according to the above method, and the results are as follows. Figure 4As shown. 0.04% trypan blue was added to quench the fluorescence physically adsorbed on the cell membrane. The fluorescence in the cells was observed by laser confocal microscopy, and the biomacromolecule presentation efficiency of the cells was quantitatively analyzed by flow cytometry.

[0048] It can be seen from the figure that the modified microneedle SNNs have an intracellular presentation efficiency of about 90% for biological macromolecules in 293T, Hela and 4T1 cells.

[0049] The microneedle array obtained in Example 1 was used to load OVA (SNNs) according to the above method, and the intracellular delivery efficiency was tested respectively with the microneedle array (NNs) without metal polyphenol loading and metal polyphenol (MPN) according to the above method. The results are as follows: Figure 5 As shown in the figure, it can be seen that the modified microneedle SNNs can significantly improve the intracellular delivery efficiency of the biomacromolecule OVA. From the test results, it can be seen that the microneedle NNs and metal polyphenol MPN have a synergistic effect, which can greatly improve their intracellular delivery efficiency and make them have practical application value. It is not just a simple superposition of effects.

[0050] The same method as above was used to test the efficiency of the microneedle array modified in Example 1 for nuclear presentation of super-large plasmids. Figure 6 As shown in the figure, compared with the traditional carrier Lipofectamine (liposome), the transfection efficiency of Lipofectamine in 24 hours is ~75%, and the transfection efficiency of the functionalized microneedles in 6 hours is ~95%. The results show that the modified microneedle SNNs can significantly shorten the transfection time of biomacromolecules and improve the transfection efficiency.

[0051] Example 2

[0052] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0053] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0054] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0055] The microneedle array was placed in a cell culture dish, 10 μL (1.0 μg / μL) of nucleic acid aptamer (AS1411) was dripped onto the microneedle surface, and the liquid was allowed to settle on ice, and then the unbound biomacromolecules were washed with PBS (pH 7.4). The prepared microneedles were placed in a cell culture dish, cell suspension was added, and centrifuged at 50 g for 90 seconds to complete the intracellular delivery of macromolecules. The results are shown in Figure 2. Figure 7 As shown in the figure, it can be seen that the modified microneedle array SNNs have an intracellular presentation efficiency of about 90% for AS1411.

[0056] Example 3

[0057] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0058] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0059] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0060] The microneedle array was placed in a cell culture dish, 10 μL (1.0 μg / μL) of chicken ovalbumin (OVA) was added to the microneedle surface, and the liquid was allowed to settle on ice, and then the unbound biomacromolecules were washed with PBS (pH 7.4). The prepared microneedles were placed in a cell culture dish, the cell suspension was added, and the microneedles were centrifuged at 50 g for 90 seconds to complete the intracellular delivery of the macromolecules. The results are shown in Figure 2. Figure 7 As shown in the figure, it can be seen that the modified microneedle array SNNs have an intracellular presentation efficiency of about 90% for OVA.

[0061] Example 4

[0062] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0063] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0064] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0065] The microneedle array was placed in a cell culture dish, 10 μL (1.0 μg / μL) of small interfering RNA (siRNA) was dripped onto the microneedle surface, and the liquid was allowed to settle on ice, and then the unbound biomacromolecules were washed with PBS (pH 7.4). The prepared microneedles were placed in a cell culture dish, the cell suspension was added, and the microneedles were centrifuged at 50 g for 90 seconds to complete the intracellular delivery of the macromolecules. The results are shown in Figure 2. Figure 7 As shown in the figure, it can be seen that the modified microneedle array SNNs have an intracellular presentation efficiency of about 90% for siRNA.

[0066] Example 5

[0067] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0068] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0069] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0070] The microneedle array was placed in a cell culture dish, 10 μL (1.0 μg / μL) of peptide was added to the surface of the microneedles, and the liquid was allowed to settle on ice, and then the unbound biomacromolecules were washed with PBS (pH 7.4). The prepared microneedles were placed in a cell culture dish, the cell suspension was added, and centrifuged at 50 g for 90 seconds to complete the intracellular delivery of the macromolecules. The results are shown in Figure 2. Figure 7 As shown in the figure, it can be seen that the modified microneedle array SNNs have an intracellular presentation efficiency of about 90% for peptides.

[0071] Example 6

[0072] A method for preparing a microneedle array loaded with metal polyphenols comprises the following steps:

[0073] Step 1: Add 5 μL of 20 mg / mL tannic acid solution, 5 μL of 5 mg / mL Fe-containing 3+ The metal salt solution was vortexed for 20 seconds.

[0074] Step 2: Take 20 μL of the mixed solution and drop it onto the surface of the microneedle array, and let it stand for 20 minutes to allow the liquid to settle. Then, use phosphate buffered saline (PBS, pH 7.4) to rinse the excess unbound tannic acid and metal salt solution.

[0075] The microneedle array was placed in a cell culture dish, 10 μL (0.2 μg / μL) of plasmid was added to the microneedle surface, and the solution was placed on ice to allow the liquid to settle. Unbound biomacromolecules were then rinsed with PBS (pH 7.4). The prepared microneedles were placed in a cell culture dish, cell suspension was added, and centrifuged at 50 g for 90 seconds to complete the intracellular delivery of macromolecules. Figure 7 As shown in the figure, it can be seen that the modified microneedle array SNNs have an intracellular presentation efficiency of about 90% for plasmids.

[0076] Select GFP plasmid and RFP plasmid according to the above method, and the results are as follows. Figure 8 As shown in the figure, it can be seen that the modified microneedle SNNs have an intracellular presentation efficiency of about 95% for plasmids.

[0077] The present invention modifies metal polyphenols onto the surface of a microneedle array to obtain an efficient, safe, and platform-applicable intracellular delivery carrier for biomacromolecules. The application of microneedle carriers can effectively deliver a variety of biomacromolecules with different molecular weights and isoelectric points into cells, and does not require modification of the biomacromolecules, and can maintain the activity of the biomacromolecules. The microneedles have sufficient length and mechanical strength to pierce the cell membrane, destroy the blocking effect of the phospholipid bilayer on drugs, and can allow biomacromolecules to escape from lysosomes, greatly improving the presentation rate of drugs. The modified microneedles overcome the problem of small nucleic acid loading capacity (no more than 5,000 bp) existing in various viral vectors, and can efficiently achieve the delivery of ultra-large-sized (15,000-20,000 bp) CRISPR / Cas9 plasmids, and achieve effective gene editing of multiple gene sites in different cells, which has broad application prospects in the biomedical field.

[0078] The self-assembly of metals and polyphenols is affected by the pH of the solution, and the stability of the self-assembled coating is pH-dependent. Under low pH conditions, most of the phenolic hydroxyl groups on the polyphenol molecules are protonated, forming a competitive chelation between proton hydrogen and metal ions, resulting in the instability or even disintegration of MPN. Therefore, the microneedles can be washed with a solution of appropriate pH value to disintegrate the MPN covering the microneedles and make them recyclable.

[0079] It can be seen from the test results of the embodiment that when the microneedle carrier obtained by the present invention transfects super-large plasmids, compared with the traditional infectious agent Lipofectamine (liposome), the transfection efficiency of Lipofectamine in 24 hours is ~75%, and the transfection efficiency of the microneedles modified by MPN functionalization is ~95% in 6 hours. The microneedle SNNs modified by MPN significantly shortens the transfection time of super-large plasmids and improves the transfection efficiency. The microneedles modified by MPN functionalization can deliver 6 biomacromolecules: chicken egg white albumin (OVA), nucleic acid aptamer (AS1411), small interfering RNA (siRNA), polypeptide, GFP plasmid and RFP plasmid into a variety of cells, and the delivery efficiency is higher than 90%, realizing the high throughput, high efficiency and universality of the carrier. The microneedles modified by MPN functionalization can be washed with a suitable solution to disintegrate the MPN covering the microneedles so that they can be recycled and reused. After 2-3 rounds of recycling, the microneedle delivery efficiency of biomacromolecules can still be higher than 90%. 。

Claims

1. A method for preparing a microneedle array loaded with metal polyphenols, characterized in that: The following steps are involved: Step 1: mixing a polyphenol solution and a metal salt solution to obtain a mixed solution; the molar ratio of the polyphenol to the metal salt is 8:1 to 1:4; Step 2: Add the mixed solution obtained in step 1 dropwise onto the surface of the microneedle array, and wash after the mixed solution is deposited; thus, a microneedle array loaded with metal polyphenols can be obtained.

2. The method for preparing a microneedle array loaded with metal polyphenols according to claim 1, characterized in that: In step 1, the polyphenols are one or two or more of anthocyanidins, catechins, gallic acid and tannic acid.

3. The method for preparing a microneedle array loaded with metal polyphenols according to claim 1, characterized in that: The metal ion in the metal salt is Fe 3+ , Mn 2+ , Fe 2+ One or two or more of the following.

4. The method for preparing a microneedle array loaded with metal polyphenols according to claim 1, characterized in that: The mixed solution in step 1 is vortexed for 10 to 20 seconds, and the sedimentation time in step 2 is 10 to 20 minutes.

5. The microneedle array loaded with metal polyphenols obtained by the preparation method according to any one of claims 1 to 4, characterized in that: The height of the microneedle is 1 μm, the diameter of the bottom of the microneedle is 0.8 μm, and the center distance between adjacent microneedles is 1.2 μm.

6. The use of a microneedle array loaded with metal polyphenols as described in claim 5, characterized in that: The microneedle array loaded with metal polyphenols is used as a delivery carrier.

7. The use of a microneedle array loaded with metal polyphenols according to claim 6, characterized in that: The microneedle array loaded with metal polyphenols is used as a macromolecular intracellular delivery carrier.

8. The use of a metal polyphenol-loaded microneedle array according to claim 6, characterized in that: The metal polyphenol-loaded microneedle array is used for delivering chicken ovalbumin, nucleic acid aptamers, small interfering RNA, polypeptides, and plasmids.

9. The use of a metal polyphenol-loaded microneedle array according to claim 6, characterized in that: Application of the metal polyphenol-loaded microneedle array in the preparation of medicines.

10. The method for recycling a microneedle array loaded with metal polyphenols according to claim 5, characterized in that: The microneedle array loaded with metal polyphenols is placed in a solution with a pH value of 3 to 5 and soaked for 5 to 10 minutes; the microneedle array can be recovered.

Citation Information

Cited By

  • Metal polyphenol-loaded microneedle array, and preparation method therefor and use thereof