Phosphate binding agent and preparation method thereof
By controlling the particle size distribution of sucrose hydroxy iron oxide and regulating the solid content of aqueous suspension, the problem of large tail material loss during spray drying of phosphate binding agents in the prior art is solved, high yield and stability are achieved, and the economic value of industrial production is improved.
Patent Information
- Application Number
- CN202510366831.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-26
- Publication Date
- 2025-06-20
AI Technical Summary
During the spray drying process, existing phosphate binding agents have large losses of tail materials, low yields, and high equipment and operation requirements, making it difficult to meet the cost control and quality requirements of industrial production.
By controlling the D50 particle size distribution of sucrose hydroxy iron oxide in the range of 30.5-39.5 μm or D90 is less than 200 μm, phosphate binding agent is prepared by spray drying technology.
The yield of phosphate binding agent is improved by about 90%, and the iron release and dry weight loss rate are optimized, which improves the stability of the product and the economic value of industrial production.
Smart Images

Figure BDA0005330235490000071 
Figure BDA0005330235490000081 
Figure BDA0005330235490000091
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of medicine, and particularly relates to a phosphate binder and a preparation method thereof. Background Art
[0002] Sucrose hydroxyiron oxide belongs to phosphate binders and is the main drug for the clinical treatment of hyperphosphatemia. These drugs bind to phosphate in the gastrointestinal tract, reduce the absorption of dietary phosphate, and thus lower the blood phosphate level.
[0003] CN105764492B discloses a pharmaceutical composition containing phosphate adsorbent particles. Although the raw material particle size range D50 of sucrose hydroxyiron oxide is mentioned as 40 - 100 μm in this patent, it mainly focuses on the influence of particle size on the quality attributes of the preparation (such as friability, hardness, fluidity, compressibility, etc.), and does not pay attention to the yield and quality requirements of the raw material drug for the particle size distribution.
[0004] CN11898824A discloses that the particle size D50 of the phosphate adsorbent is 10 - 30 μm, and it is proposed that when D50 is greater than 30 μm, the material will adhere to the wall more during the spraying process, reducing the yield. However, in actual production, due to the too small particle size, a large amount of fine particle tailings will be generated during the spray drying process. These large amounts of fine particles are carried away by the wind from the exhaust port of the spray drying equipment, and the loss amount generated is far greater than the material adhering to the wall, thereby greatly reducing the actual yield of the raw material drug.
[0005] The preparation processes of particles with different particle size ranges are affected by various preparation parameters. Both of the above two patents choose to adjust the equipment parameters to obtain the required particle size range, which has relatively high requirements for the equipment and operation.
[0006] As is well known, in the process of industrial drug production, both cost control and quality requirements are of crucial importance. Therefore, it is necessary to provide a phosphate binder with good quality, high yield, simple operation and suitable for industrial production. Summary of the Invention
[0007] The purpose of the present invention is to provide a phosphate binder and a preparation method thereof. By controlling the D50 particle size distribution of sucrose hydroxyiron oxide within the range of 30.5 - 39.5 μm or D90 less than 200 μm, the product not only has good quality, but also has high yield, which is beneficial to improving the economic value of industrial production of the product.
[0008] The present invention provides a phosphate binder comprising a mixture of iron(III) hydroxyoxide, sucrose and one or more starches. Among them, the phosphate binder is sucrose hydroxyiron oxide, and has a particle size distribution with a D50 range of 30.5 μm to 39.5 μm or D90 less than 200 μm.
[0009] In certain embodiments, at least 40% of the particles in the phosphate binder have a particle size not exceeding 30.5 μm, at least 60% have a particle size not exceeding 39.5 μm, at least 80% have a particle size not exceeding 50 μm, at least 90% have a particle size not exceeding 80 μm, or at least 90% are less than 200 μm.
[0010] In certain embodiments, by mass percentage, the phosphate binder contains 25%-40% iron(III) hydroxide, 15%-40% sucrose, and 20%-40% starch.
[0011] The present invention also provides a composition for preparing a phosphate binder, which includes, by weight components: 30-50 parts of ferric chloride hexahydrate, 25-45 parts of sodium carbonate, 7.5-20 parts of sucrose, 8-10 parts of potato starch, 4-6 parts of pregelatinized starch, and an appropriate amount of purified water. In certain embodiments, it includes, by weight components: 40-50 parts of ferric chloride hexahydrate, 25-35 parts of sodium carbonate, 7.5-20 parts of sucrose, 8-10 parts of potato starch, 4-6 parts of pregelatinized starch, and an appropriate amount of purified water.
[0012] The present invention also provides a method for preparing a phosphate binder, which includes the following steps:
[0013] Step 1: Weigh sodium carbonate and purified water, feed them in a weight ratio of 1:1 to 1:30, stir to dissolve and filter to obtain a sodium carbonate solution and put it into a reaction vessel; weigh ferric chloride hexahydrate and purified water, feed them in a weight ratio of 5:0.5 to 1:10, stir to dissolve and filter to obtain a ferric chloride solution, add it to the sodium carbonate solution, and stir and react at 10-50 °C, controlling the pH between 7.0 and 11.0 to obtain a M1 reaction solution;
[0014] Step 2: Add purified water (the weight ratio of purified water to M1 is greater than 3 times), and use membrane filtration for cyclic desalination and concentration to obtain a ferric hydroxide suspension, that is, a M1 suspension;
[0015] Step 3: Stir and mix evenly under a stirring state of 10-300 r / min, take a sample to measure the iron content, and calculate the amounts of sucrose, starch, and purified water to be added according to the iron content in the M1 suspension.
[0016] Step 4: Add the prescribed amount of sucrose to the M1 suspension in sequence under a stirring state of 10-300 r / min to dissolve, obtaining M2;
[0017] Step 5: Add potato starch and pregelatinized starch to M2 under a stirring state of 10-300 r / min and stir evenly to obtain M3;
[0018] Step 6: Add purified water to M3 under stirring at 10 - 300 r / min to adjust the solid content, obtaining an aqueous suspension of M3.
[0019] Step 7: Spray-dry the aqueous suspension of M3 by high-speed centrifugal spray drying under stirring at 10 - 300 r / min to obtain sucrose hydroxyl iron oxide particles.
[0020] Step 8: Mix the sucrose hydroxyl iron oxide particles obtained by spray drying at a rotation speed of 5 - 40 Hz for 2 - 20 min, then collect the material and seal it for packaging.
[0021] The present invention provides a method for preparing a phosphate binder, in which the weight ratio of sodium carbonate to ferric chloride is between 0.2:1 and 10:1; the starch can be selected from one of corn starch or potato starch or a mixture thereof with a ratio of 1:0.1 - 0.1:1, preferably one of corn starch or potato starch, and the addition sequence is not restricted; the pore size of the desalination equipment is between 5 - 1000 nm; the water evaporation rate of spray drying is 5 kg / hour - 500 kg / hour, and the drying temperature is 100 - 250 °C; the rotation speed of the high-speed centrifugal spray for spray drying is 8000 r / min - 21000 r / min, preferably 10000 r / min - 20000 r / min. The inlet temperature of the high-speed centrifugal spray for spray drying is 100 °C to 250 °C, and the outlet temperature is 45 °C to 150 °C. The material spray flow rate is 5 kg - 500 kg / hour, and the inlet air flow rate is 1.0 - 5.0×10 4 m 3 The moisture or drying loss of the spray-dried product (sucrose hydroxyl iron oxide finished product) is 3% - 10%.
[0022] The present invention provides a method for preparing a phosphate binder, in which during the desalination, concentration of M1, addition of sucrose, starch, and spray drying processes, mechanical stirring, magnetic stirring, gas power, circulating flow, etc. can be used to keep the material in a uniform state in the container.
[0023] The present invention provides a method for preparing a phosphate binder, in which the sucrose hydroxyl iron oxide particles obtained by spray drying are mixed at a rotation speed of 5 - 40 Hz for 2 - 20 min and an appropriate amount of desiccant is added and sealed.
[0024] The hydroxyl iron oxide content in the M1 suspension is greater than 3%, and the mass percentage of the solid content in the aqueous suspension of M3 is 10% - 40%, preferably 10% - 35%.
[0025] The present invention provides a method for preparing a phosphate binder, wherein the relationship among iron: sucrose: corn starch: pregelatinized starch is 0.8 - 1.2: 1.2 - 1.8: 0.8 - 1.2: 0.3 - 0.7 in terms of %(m / m / m / m).
[0026] The present invention provides a method for preparing a phosphate binder, wherein the relationship between ferric chloride hexahydrate and sodium carbonate is 0.2: 1 to 1: 0.2 in terms of %(m / m / m / m). The concentration of ferric chloride hexahydrate is prepared at 5% - 50%, and the concentration of sodium carbonate is prepared at 5% - 50%.
[0027] The present invention provides a method for preparing a phosphate binder, wherein the content of iron hydroxide in the M1 suspension is greater than 3%, and the mass percentage of the solid content in the M3 aqueous suspension is 10% - 40%, preferably 10% - 35%.
[0028] The present invention provides a method for preparing a phosphate binder, wherein the D50 range of sucrose iron hydroxide particles is 30.5 μm - 39.5 μm.
[0029] The present invention provides a method for preparing a phosphate binder, wherein the D90 range of sucrose iron hydroxide particles is less than 200 μm or D90 < 200 μm.
[0030] The present invention provides a method for preparing a phosphate binder composition. The phosphate binder (sucrose iron hydroxide particles) is sieved and mixed, pressed, and packaged with one or more of one or more lubricants, anti-adhesives, and edible flavors in equal increments to obtain tablets.
[0031] The present invention also provides a pharmaceutical composition, which is made into different dosage forms, including but not limited to suspensions, tablets, capsules, etc., by using any one of the phosphate binders in the embodiments of the present invention and at least one pharmaceutically acceptable excipient.
[0032] The term "D10" refers to the particle size corresponding to when the cumulative particle size distribution percentage of the sucrose iron hydroxide raw material reaches 10%; the term "D50" refers to the particle size corresponding to when the cumulative particle size distribution percentage of the sucrose iron hydroxide raw material reaches 50%; the term "D90" refers to the particle size corresponding to when the cumulative particle size distribution percentage of the sucrose iron hydroxide raw material reaches 90%.
[0033] The particle size or particle size distribution of this technology can be obtained by dry and wet measurements.
[0034] The technical effects of the present invention are as follows:
[0035] The inventor of the present invention has made long-term and various attempts and experiments, and finally found that controlling the particle size range D50 of sucrose hydroxy iron oxide within 30.5 μm to 39.5 μm or D90 less than 200 μm can reduce the loss of tailings and the sticking of materials to the wall during spray drying, obtain a high yield of about 90%, and the iron release amount and drying loss rate are better than those of the small particle size group (D50 < 30.5 μm) and the large particle size group (D50 > 39.5 μm) or D90 less than 200 μm, improving the stability of the pharmaceutical composition. In addition, the inventor also found that by regulating the solid content of the aqueous suspension of iron(III) hydroxide, sucrose and starch within the range of 10% to 35%, the particle size distribution of D50 and D90 can be regulated, and sucrose hydroxy iron oxide with D50 within the range of 30.5 μm to 39.5 μm or D90 less than 200 μm can be obtained, with lower requirements for equipment and operation. In short, by controlling the D50 particle size distribution of sucrose hydroxy iron oxide within the range of 30.5 - 39.5 μm or the D90 particle size distribution within the range of less than 200 μm, the product not only has a high yield, but also has good quality, greatly improving the economic value of industrial production of the product. Detailed implementation mode
[0036] The above-mentioned inventive content of the present invention will be further described in detail below in conjunction with the specific implementation mode. It should be understood that these embodiments are only disclosed by way of illustration of the present disclosure and should not limit the scope of the present disclosure in any way.
[0037] Example 1
[0038] The preparation of the phosphate binder of this patent, where the relationship between iron: sucrose: corn starch: pregelatinized starch in M3 is 1:1.5:1:0.5 in terms of %(m / m / m / m). It includes the following steps:
[0039] Step 1: Dissolve 50 kg of ferric chloride hexahydrate in 200 kg of purified water to form a ferric chloride solution, and dissolve 50 kg of anhydrous sodium carbonate in 120 kg of purified water to form a sodium carbonate solution. Under the condition of a stirring speed of 100 ± 30 r / min, add the ferric chloride solution to the sodium carbonate solution, control the reaction temperature at 10°C to 50°C, the addition time at 10 to 90 min, and continue stirring until there are no bubbles on the liquid surface in the reaction system, and control the pH = 7 to 10 as the reaction end point.
[0040] Step 2: Desalt the reaction solution with a membrane filtration system, control the temperature of the circulating liquid at 10 to 50°C, monitor that the conductivity of the discharged water and the circulating liquid ≤ 10.0 ms / cm, start concentration, detect that the iron content is greater than 3%, and the conductivity of the discharged water and the circulating liquid ≤ 5 ms / cm, and stop concentration to obtain M1.
[0041] Step 3: Stir and mix for more than 10 minutes under the stirring state of 100 ± 30 r / min, take a sample to measure the iron content, and calculate the amounts of sucrose, starch and purified water to be added according to the iron content in the M1 suspension.
[0042] Step 4: Under the stirring state of 100 ± 30 r / min, add sucrose, control the temperature at 10 - 50 °C, and stir and mix for not less than 30 minutes until it dissolves to obtain M2.
[0043] Step 5: Under the stirring state of 100 ± 30 r / min, add potato starch and pregelatinized starch to M2 in sequence, control the temperature at 10 - 50 °C, and stir and mix for not less than 20 minutes to obtain M3.
[0044] Step 6: Under the stirring state of 100 ± 30 r / min, add an appropriate amount of purified water to M3 to adjust the solid content to obtain an M3 aqueous suspension (with a solid content of 10% - 35%), and control the temperature at 10 - 50 °C.
[0045] Step 7: Stir the M3 aqueous suspension, pump the feed with a peristaltic pump, the inlet air temperature is 100 - 200 °C, the centrifugal disk speed is 16000 ± 2000 r / min, adjust the feed rate until the outlet air temperature is 90 ± 40 °C, and set the outlet temperature to 90 ± 40 °C. During the spray drying process, control the moisture content of the sucrose hydroxyl iron oxide particles at 4% - 10%, and dry and collect the spray-dried material to obtain sucrose hydroxyl iron oxide particles.
[0046] Step 8: Under the rotation speed condition of 5 - 40 Hz, mix the sucrose hydroxyl iron oxide particles obtained by spray drying for 5 ± 3 min, collect the material, and add a desiccant for sealed packaging.
[0047] Example 2
[0048] This example is basically the same as Example 1, except that: in Step 6, the M3 aqueous suspension (with a solid content of 20%); in Step 7, the centrifugal disk speed is 18000 r ± 1000 / min; in Steps 4 and 5, the relationship between iron, sucrose, corn starch and pregelatinized starch in M1, calculated by %(m / m / m / m), is 1:1.5:1.2:0.5.
[0049] Example 3
[0050] This example is basically the same as Example 1, except that: in Step 6, the M3 aqueous suspension (with a solid content of 25%); in Step 7, the centrifugal disk speed is 20000 ± 1000 r / min; in Steps 4 and 5, the relationship between iron, sucrose, corn starch and pregelatinized starch in M1, calculated by %(m / m / m / m), is 1:1.5:1:0.5.
[0051] Example 4
[0052] This example is basically the same as Example 1, except that: in step 6, the M3 aqueous suspension (solid content is 27%), in step 7, the centrifugal disk speed is 20000 ± 1000 r / min, and in steps 4 and 5, the relationship of iron:sucrose:potato starch:pre-gelatinized starch in M1 is 1:1.5:0.75:0.75 in terms of %(m / m / m / m).
[0053] Example 5
[0054] This example is basically the same as Example 1, except that: in step 6, the M3 aqueous suspension (solid content is 30%), in step 7, the centrifugal disk speed is 14000 ± 1000 r / min, and in steps 4 and 5, the relationship of iron:sucrose:potato starch:pre-gelatinized starch in M1 is 1:1.5:0.5:1 in terms of %(m / m / m / m).
[0055] Comparative Example 1
[0056] This comparative example is basically the same as Comparative Example 1, except that: in step 6, the M3 aqueous suspension (solid content is 10%), and in step 7, the centrifugal disk speed is 18000 r ± 1000 / min.
[0057] Comparative Example 2
[0058] This comparative example is basically the same as Comparative Example 1, except that: in step 6, the M3 aqueous suspension (solid content is 35%), and in step 7, the centrifugal disk speed is 20000 ± 1000 r / min.
[0059] Test Example 1: Yield calculation, particle size distribution, and quality detection
[0060] The yield of the iron sucrose hydroxide particles obtained in Examples 1-5 and Comparative Examples 1-2 was calculated respectively, and the particle size distribution and quality were detected. The results are shown in Table 1.
[0061] Method for measuring D50 and D90: Measured according to the method for determining particle size and particle size distribution (General Rule 0982, Method 3), using a laser scattering particle size distribution analyzer and measuring by the dry method;
[0062] Yield calculation method:
[0063] Among them, Y represents the total iron yield;
[0064] N represents the total weight of the iron sucrose hydroxide particles;
[0065] A represents the iron content of the iron sucrose hydroxide particles;
[0066] m represents the feeding amount of ferric chloride hexahydrate;
[0067] The molecular weight of ferric chloride hexahydrate is 270.3;
[0068] 56 represents the atomic weight of iron.
[0069] Method for determining iron content: Take 0.2 g of the test sample, accurately weigh it, add 4 ml of hydrochloric acid solution (measure 20 ml of hydrochloric acid, add 100 ml of water and mix evenly to obtain), shake and let stand for 1 minute, add 25 ml of water, heat to dissolve, quickly cool to room temperature, add 2 g of potassium iodide, tightly stopper, shake well, place in the dark for 5 minutes, add 75 ml of water, immediately titrate with sodium thiosulfate standard solution (0.05 mol / L). When approaching the end point, add 2 mL of starch indicator solution and continue titrating until the blue color disappears, which is the end point. Correct the titration result with a blank test. Each 1 ml of sodium thiosulfate titrant (0.05 mol / L) is equivalent to 2.7925 mg of Fe.
[0070] Method for determining iron release: Refer to the second method (paddle method) in the general chapter "0931 Dissolution and Release Determination Method" of the fourth part of the Chinese Pharmacopoeia (2020 edition). Using hydrochloric acid solution with pH 3.0 as the medium, the release amount of ferric iron is determined by the volumetric method.
[0071] Method for determining loss on drying: Take 2 g of the test sample, dry it to constant weight at 105 °C, and calculate the loss on drying of the test sample from the weight loss and the sampling amount.
[0072] Table 1 Calculation of the yield of different sucrose hydroxy iron oxides, and particle size distribution and quality inspection results
[0073]
[0074] It can be seen from the measurement results in Table 2 that under the condition of the atomizer speed of 13000 r / min - 21000 r / min, in Examples 1 - 5 of the present invention, by regulating the solid content of the M3 suspension within the range of 10% - 30%, the particle size range D50 of sucrose hydroxy iron oxide can be maintained within 30.5 μm - 39.5 μm or D90 is less than 200 μm.
[0075] (1) Yield: The yields of sucrose hydroxy iron oxide with D50 within the range of 30.5 μm - 39.5 μm or D90 less than 200 μm (Examples 1 - 5) are all higher than those with D50 of 21.13 μm (Comparative Example 1) and D50 of 47.62 μm (Comparative Example 2). This is because in the actual production process, if the particle size is too small, a large amount of tailings will be generated, thus reducing the yield, while if the particle size is too large, it is easy to agglomerate and adhere to the wall, resulting in a decrease in the yield.
[0076] (2) Iron content: The iron content of Examples 1-5 and Comparative Example 2 can all reach over 20%, indicating that the iron content of the prepared products is qualified. However, in Comparative Example 1, due to the smaller particle size, the iron content loss is large, resulting in a significant decrease in iron content.
[0077] (3) Iron release: The iron release rate of Examples 1-5 can be stabilized below 0.8%, which is less than that of Comparative Example 1 and Comparative Example 2, indicating that the sucrose hydroxy iron oxide prepared in Examples 1-4 of the present invention has higher stability.
[0078] (4) Loss on drying: The loss on drying rates of Examples 1-5 and Comparative Example 1 can all be controlled below 7%, while the loss on drying rate of Comparative Example 2 is higher than 10%, which is not conducive to the stability control of the product; although the loss on drying rate of Comparative Example 1 is lower, its iron release amount is high, which is still not conducive to the stability control of the product.
[0079] Examples 6-9: Phosphate binder composition preparation
[0080] The sucrose hydroxy iron oxide particles, magnesium stearate, silicon dioxide, and edible flavor were mixed, compressed, and packaged in equal increments according to the prescription composition in Table 2 to obtain tablets. The specific preparation method of the compositions in Examples 6-9 includes the following steps:
[0081] (1) The sweeteners neohesperidin dihydrochalcone or acesulfame potassium and sucrose hydroxy iron oxide were added in equal increments and mixed for 1-5 min for 3-4 times.
[0082] (2) About half of the flavoring agents raspberry flavor or sweet orange flavor and the mixture in step (1) were added to the mixer. The mixer was rotated at 5-30 rpm and mixed for 5-30 min. Then the remaining flavor was added and mixed for 5-30 min, and then sieved.
[0083] (3) The glidants silicon dioxide or talc powder, the mixture in step (2), and about an equal amount of sucrose hydroxy iron oxide were added to the mixer. The mixer was rotated at 5-30 rpm and mixed for 5-30 min, and then sieved.
[0084] (4) The mixture ③ and about 3 times the amount of mixture ③ of sucrose hydroxy iron oxide were added to the mixer. The mixer was rotated at 5-30 rpm and mixed for 5-30 min. Then about 2 times the amount of sucrose hydroxy iron oxide was added and mixed for 5-30 min. Then the remaining sucrose hydroxy iron oxide was continuously mixed for 5-30 min.
[0085] (5) About an equal amount of the mixture in step (4) and magnesium stearate were taken and added to the mixer. The mixer was rotated at 5-30 rpm and mixed for 5-20 min. Then the obtained mixture was added to the mixer in step (4). The mixer was rotated at 5-30 rpm and mixed for 5-30 min to obtain the final mixture.
[0086] (6) Press the mixture into tablets (chewable tablets) using a rotary tablet press according to the particle content. The tablet press rotation speed is 5 - 40 rpm, the tablet hardness is 80 - 350 N, and the tablet diameter is 1 - 3 cm.
[0087] (7) Detect relevant indicators of the final mixture and tablets, and the results are shown in Table 3.
[0088] Table 2 Prescription composition of Examples 6 - 9
[0089]
[0090] Table 3 Detection results of Examples 6 - 9
[0091]
[0092] It can be seen from Examples 6 - 9 that during the process of preparing chewable tablets with sucrose hydroxyiron oxide prepared according to Examples 2 - 5, the fluidity and compressibility of the mixed materials of the composition are good, and the phosphorus binding rate of the pressed chewable tablets is relatively high and the iron release is relatively low, indicating that all quality indicators meet the requirements.
[0093] The above specific embodiments are only used to illustrate the technical solutions of the present invention and not to limit them. Although the present invention has been described in detail with reference to the examples, those of ordinary skill in the art should understand that the technical solutions of the present invention can be modified or equivalently replaced without departing from the scope of the technical solutions of the present invention, and they should all be covered within the scope of the claims of the present invention.
Claims
1. A phosphate binder comprising a mixture of iron (III) oxyhydroxide, sucrose and one or more starches, characterized in that: The phosphate binder is sucrose ferric oxyhydroxide, comprising a particle size distribution with a D50 ranging from 30.5 μm to 39.5 μm or a D90 less than 200 μm.
2. The phosphate binder according to claim 1, characterized in that At least 40% of the particles of the phosphate binder have a particle size of no more than 30.5 μm, at least 60% of the particles have a particle size of no more than 39.5 μm, at least 80% of the particles have a particle size of no more than 50 μm, at least 90% of the particles have a particle size of no more than 80 μm, or at least 90% of the particles have a particle size of less than 200 μm.
3. The phosphate binder according to claim 1 or 2, characterized in that According to mass percentage, the phosphate binder contains 25%-40% iron (III) oxyhydroxide, 15%-40% sucrose, and 20%-40% starch.
4. A composition for preparing a phosphate binder as claimed in any one of claims 1 to 3, characterized in that: The components include, by weight: 30-50 parts of ferric chloride hexahydrate, 25-45 parts of sodium carbonate, 7.5-20 parts of sucrose, 8-10 parts of potato starch, 4-6 parts of pregelatinized starch, and an appropriate amount of purified water.
5. The method for preparing a phosphate binder according to claim 4, characterized in that: The following steps are involved: Step 1: according to the feed ratio, weigh sodium carbonate and an appropriate amount of purified water, stir to dissolve, filter to obtain a sodium carbonate solution and put it into a reaction container; then according to the feed ratio, take ferric chloride hexahydrate and an appropriate amount of purified water, stir to dissolve, filter to obtain a ferric chloride solution, add it to the sodium carbonate solution, stir and react at 10-50° C. to obtain an M1 reaction solution, add part of the purified water to desalt and concentrate to obtain an iron oxyhydroxide suspension, i.e., an M1 suspension; Step 2: adding purified water and using membrane filtration to circulate desalination and concentration to obtain an iron oxyhydroxide suspension, namely, M1 suspension; Step 3: Stir the mixture evenly while stirring, take samples to determine the iron content, and calculate the amount of sucrose, starch and purified water to be added based on the iron content in the M1 suspension. Step 4: Add the prescribed amount of sucrose to the M1 suspension in sequence while stirring to dissolve, to obtain M2; Step 5: Add potato starch and pregelatinized starch to M2 under stirring, and stir evenly to obtain M3; Step 6: Add purified water to M3 under stirring to adjust the solid content to obtain an M3 aqueous suspension; Step 7: The M3 aqueous suspension is spray-dried by high-speed centrifugation under stirring to obtain sucrose iron oxyhydroxide particles.
6. The preparation method according to claim 5, characterized in that: The mass percentage of solid content in the M3 aqueous suspension is 10%-40%.
7. The preparation method according to claim 5 or 6, characterized in that: The mass percentage of solid content in the M3 aqueous suspension is preferably 10%-35%.
8. The preparation method according to claim 5, characterized in that: The rotation speed of the high-speed centrifugal spray is 10000r / min-21000r / min.
9. The preparation method according to claim 5, characterized in that: The D50 of the sucrose iron oxyhydroxide particles is in the range of 30.5 μm to 39.5 μm or the D90 is less than 200 μm.
10. A pharmaceutical composition, characterized in that The pharmaceutical composition comprises the phosphate binder according to any one of claims 1 to 9 and at least one pharmaceutically acceptable excipient, and is prepared into tablets through screening, mixing, pressing, packaging and other processes.
Citation Information