High-strength wear-resistant multilayer ceramic substrate and preparation method thereof

By modifying alumina powder and adding dispersants and other additives, a high-strength wear-resistant multi-layer ceramic substrate is prepared, which solves the insufficient strength and wear-resistant performance caused by agglomeration of alumina powder, and achieves the improvement of the high strength and wear-resistant performance of the substrate.

CN120554098AActive Publication Date: 2025-08-29HEBEI DINGCI ELECTRONIC TECH CO LTD
7 Cites 0 Cited by

Patent Information

Application Number
CN202511079568.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-08-04
Publication Date
2025-08-29
Estimated Expiration
2045-08-04

AI Technical Summary

Technical Problem

The strength and wear resistance of multi-layer ceramic substrates caused by agglomeration of alumina powders affect their high-end applications.

Method used

Modified alumina powder is used to improve the dispersion of alumina powder by diphenyl silicone glycol and biphenyl compound modifier, and a high-strength wear-resistant multi-layer ceramic substrate is prepared by combining dispersant, plasticizer, binder and sintering aid.

Benefits of technology

The strength and wear resistance of the multi-layer ceramic substrate are improved, and the performance problem of insufficient alumina powder agglomeration is solved.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of ceramic substrates, and provides a high-strength wear-resistant multilayer ceramic substrate and a preparation method thereof. The high-strength wear-resistant multilayer ceramic substrate comprises the following raw materials in parts by weight: 70-80 parts of aluminum oxide, 2-3 parts of a dispersant, 3-5 parts of a plasticizer, 8-12 parts of a binder, 8-10 parts of a sintering aid and 80-90 parts of water, the aluminum oxide is modified aluminum oxide, the modified aluminum oxide is obtained by modifying aluminum oxide with a modifier, and the modifier comprises diphenyl silanediol and a biphenyl compound. According to the technical scheme, the problems of insufficient strength and wear resistance of the multilayer ceramic substrate in the prior art are solved.