Preparation method of reusable polyethylene glycol modified magnetic beads and application of reusable polyethylene glycol modified magnetic beads in exosome extraction

By preparing reusable polyethylene glycol-modified magnetic beads, the problems of strong equipment dependence and high cost in exosome separation methods were solved, efficient capture and separation of exosomes were achieved, costs were reduced, and the activity of exosomes and the structural stability of the magnetic beads were maintained.

CN120600502APending Publication Date: 2025-09-05SUZHOU NINGRAO BIOTECHNOLOGY CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202510770802.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-06-10
Publication Date
2025-09-05

AI Technical Summary

Technical Problem

Exosome isolation methods in existing technologies have problems such as strong equipment dependence, high cost, low purity, cumbersome operation, and poor reusability, which seriously restrict their industrial application prospects.

Method used

Reusable polyethylene glycol-modified magnetic beads are used to prepare carboxylated magnetic graphene oxide and couple it with amino-polyethylene glycol to form magnetic beads with superparamagnetism and hydrophobic environment for the capture and separation of exosomes.

Benefits of technology

The efficient capture and separation of exosomes is achieved, the cost is reduced, the activity of exosomes is maintained, and the magnetic beads are reusable and have a stable structure, making them suitable for the rapid separation of cell culture supernatants.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120600502A_ABST
    Figure CN120600502A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of reusable polyethylene glycol modified magnetic beads and application of the reusable polyethylene glycol modified magnetic beads in exosome extraction.The preparation method comprises the steps that EDC is added into carboxylated magnetic graphene oxide for a reaction, then NHS is added for a reaction, and a mixed solution is obtained; and adding an aqueous solution of aminated polyethylene glycol into the mixed solution, carrying out amidation reaction, carrying out magnetic suction washing with pure water, and drying. When the exosome is extracted by adopting the method disclosed by the invention, the exosome of 30-150nm can be obtained; the polyethylene glycol modified magnetic beads used in the invention have the advantages of low cost, fast preparation and strong magnetism, and can be completely separated from the solution within 30 s. The exosome is captured through a precipitation method, the activity of the exosome is not damaged after the exosome is released, the yield and the purity of the exosome are improved, the recovered magnetic beads can be repeatedly used, and the cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of nanobiomaterials and technologies, and specifically relates to a method for preparing reusable polyethylene glycol-modified magnetic beads and their application in exosome extraction. Background Art

[0002] Exosomes are nanoscale vesicles (30-150 nm in diameter) released by the fusion of intracellular multivesicular bodies (MVBs) with the cell membrane. They possess a typical phospholipid bilayer structure. Their surfaces are rich in markers such as tetraspanins (CD9 / CD63 / CD81), heat shock proteins (HSP70 / HSP90), and integrins, while their interiors carry functional proteins, mRNA, miRNA, and DNA fragments. According to the International Society for Extracellular Vesicles (ISEV) guidelines (MISEV2018), exosomes must be triple-validated by transmission electron microscopy (TEM) for morphological observation, nanoparticle tracking analysis (NTA) for particle size measurement, and Western blot for marker protein detection. As a key medium for intercellular communication, exosomes participate in the following physiological and pathological processes: (1) Disease diagnosis: Tumor-derived exosomes carry biomarkers such as PD-L1 and EGFRvIII, which are of great value in liquid biopsy; (2) Drug delivery: The natural targeting of exosomes makes them an ideal carrier for siRNA / mRNA delivery; (3) Tissue repair: Mesenchymal stem cell (MSC) exosomes promote angiogenesis by delivering miR-21, VEGF, etc. Therefore, the isolation and purification of cell exosomes is a difficult problem.

[0003] Exosome isolation methods in the prior art:

[0004] (1) Traditional ultracentrifugation: As the gold standard method for exosome isolation, differential centrifugation (300g→200g→10,000g→100,000g) is used to gradually remove cell debris and finally ultracentrifuge the exosomes. However, this method is highly equipment-dependent (requiring an ultracentrifuge, costing >$100,000 USD); the yield is low (30-50%), and high-speed centrifugation causes exosome aggregation; there are many co-precipitated pollutants (such as lipoproteins and protein aggregates); and the integrity of exosomes is easily destroyed.

[0005] (2) Commercial polymer precipitation reagents (such as PEG 8000): PEG dehydration is used to precipitate exosomes from the solution, but the purity is extremely poor (impurity protein accounts for >60%); subsequent purification steps (such as density gradient centrifugation) are required, and the operation is cumbersome; PEG residues interfere with downstream analysis (such as a decrease in the signal-to-noise ratio of mass spectrometry detection).

[0006] (3) Size exclusion chromatography (SEC): separation is achieved based on the particle size of exosomes through a porous gel column; however, the sample is severely diluted (the recovery volume is increased by 3-5 times); the column efficiency is easily clogged (viscous samples such as plasma require pre-filtration); and the equipment throughput is low (single processing volume <1 mL).

[0007] (4) Immunoaffinity capture method: by coupling antibodies to magnetic beads, exosomes are captured by antigen-antibody binding specificity; or by modifying the surface with aptamers, exosomes are captured by phosphatidylserine binding specificity. However, antibodies are expensive and require large amounts of antibody. After antibody coupling, activity is easily lost (activity retention is usually <60%); reusability is poor (efficiency drops by >50% after ≤3 times); and elution conditions are harsh (low pH or high salt can easily destroy the integrity of the exosome membrane).

[0008] (5) Microfluidics: Exosomes are separated on a chip through acoustic waves, electric fields, or nanostructures; however, the equipment is highly customized and difficult to scale up; the processing volume is limited (μL-level samples) and the reproducibility is poor (CV>15%).

[0009] (6) Patents CN 118258991 A and CN 117095895 A have problems in actual application, such as insufficient process reproducibility and low raw material utilization. These technical bottlenecks have caused the pilot-scale scale-up costs of the patented technology to exceed the expected value by 38%, seriously restricting its industrial application prospects. Summary of the Invention

[0010] To overcome the high cost problem caused by the inability to recycle exosomes during isolation in the prior art, the present invention aims to provide a method for preparing reusable polyethylene glycol-modified magnetic beads and their application in exosome extraction. The exosome capture magnetic beads prepared by this method can be reused, reducing costs.

[0011] To achieve the above-mentioned purpose, the technical solution provided by the present invention is:

[0012] A method for preparing reusable polyethylene glycol-modified magnetic beads comprises the following steps:

[0013] Adding EDC to the carboxylated magnetic graphene oxide, reacting the mixture, and then adding NHS to the mixture, reacting the mixture to obtain a mixed solution;

[0014] An aqueous solution of amino polyethylene glycol is added to the mixed solution to carry out an amidation reaction, and the mixed solution is magnetically washed with pure water and dried to obtain reusable polyethylene glycol-modified magnetic beads.

[0015] Furthermore, the molecular weight of the amino polyethylene glycol is 200-100000 Da.

[0016] Furthermore, the amino polyethylene glycol is linear amino polyethylene glycol, four-arm amino polyethylene glycol and eight-arm amino polyethylene glycol.

[0017] Furthermore, the molar ratio of carboxylated magnetic graphene oxide to EDC is 1:5-20; the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:5-20; and the molar ratio of amino polyethylene glycol to carboxylated magnetic graphene oxide is 20:1-10.

[0018] Furthermore, carboxylated magnetic graphene oxide is prepared by the following process:

[0019] The magnetic graphene oxide is ultrasonically dispersed in pure water, and then sodium hydroxide and chloroacetic acid are added to carry out a bath ultrasonic reaction to prepare the carboxylated magnetic graphene oxide.

[0020] Furthermore, the mass ratio of magnetic graphene oxide to sodium hydroxide is 1:20-50, the mass ratio of magnetic graphene oxide to chloroacetic acid is 1:20-30, and the bath ultrasonic reaction time is at least 2 hours.

[0021] A reusable polyethylene glycol-modified magnetic bead.

[0022] Application of reusable polyethylene glycol-modified magnetic beads in the extraction of exosomes.

[0023] An exosome extraction kit comprises reusable polyethylene glycol-modified magnetic beads and an elution solution.

[0024] A method for extracting exosomes, comprising the following steps:

[0025] Reusable polyethylene glycol-modified magnetic beads are added to the exosome sample, and the mixture is incubated in an ice bath to obtain a mixed solution; the exosomes in the mixed solution are eluted to obtain exosomes.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] The magnetic graphene oxide carrier in this invention combines the superparamagnetism of Fe₃O₄ with the π-π stacking of monolayer graphene oxide (GO) to enhance exosome adsorption capacity. The polyethylene glycol interface creates a hydrophobic environment for exosome precipitation, while the PEG-NH₂ spacer modification and hydrophobic environment create efficient exosome capture. Combined with the superparamagnetism of Fe₃O₄, the magnetic beads are reusable and maintain structural stability. After the polyethylene glycol capture and separation of exosomes, the recovered magnetic beads can be reused. This also eliminates the need for expensive equipment during the extraction process, demonstrating promising application prospects in the field of exosome extraction.

[0028] The method described in this invention can extract exosomes measuring 30-150 nm. Furthermore, the magnetic beads used in this invention are low-cost, quick to prepare, and possess strong magnetic properties, enabling complete separation from the solution within 30 seconds. The exosomes are then coupled with polyethylene glycol and captured by precipitation, with their activity preserved after release. Furthermore, the magnetic beads can be reused after exosome release, effectively reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is the SEM image of the MGO-linear PEG magnetic beads of Example 1;

[0030] Figure 2 This is the SEM image of the MGO-four-arm PEG magnetic beads of Example 2;

[0031] Figure 3 This is the SEM image of the MGO-eight-arm PEG magnetic beads of Example 3;

[0032] Figure 4 TEM images of exosomes obtained and separated from MGO-linear PEG magnetic beads in Example 4;

[0033] Figure 5 TEM images of exosomes obtained and separated from the MGO-four-arm PEG magnetic beads in Example 5;

[0034] Figure 6 TEM images of exosomes obtained and separated from the MGO-eight-arm PEG magnetic beads of Example 6;

[0035] Figure 7 Zeta potential diagram of the MGO-linear PEG magnetic beads used to obtain and separate exosomes in Example 4.

[0036] Figure 8 Zeta potential diagram of the MGO-four-arm PEG magnetic beads used to obtain and separate exosomes in Example 5.

[0037] Figure 9 Zeta potential diagram of the MGO-eight-arm PEG magnetic beads used to obtain and separate exosomes in Example 6. DETAILED DESCRIPTION

[0038] To facilitate understanding of the present invention, the present invention will be described more fully below with reference to the accompanying drawings. The accompanying drawings illustrate preferred embodiments of the present invention. However, the present invention may be implemented in a variety of different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided to provide a more thorough and comprehensive understanding of the disclosure of the present invention.

[0039] The experimental methods described in the following examples are conventional methods unless otherwise specified; the reagents and biological materials described are commercially available unless otherwise specified.

[0040] 1. Preparation method of polyethylene glycol modified magnetic beads

[0041] 1. Preparation of magnetic graphene oxide by hydrothermal method

[0042] Monolayer graphene oxide (MGO) is dispersed in ethylene glycol to obtain a graphene oxide solution, to which ferric chloride, sodium acetate, and polyethylene glycol are added. After mixing and stirring, a hydrothermal reaction (high-temperature and high-pressure reaction) is carried out. After the reaction is completed, the product is collected by centrifugation and magnetically washed with ethanol and pure water in sequence to obtain magnetic graphene oxide.

[0043] 2. Preparation of carboxylated magnetic graphene oxide

[0044] The magnetic graphene oxide obtained in step 1 is ultrasonically dispersed in pure water, and then sodium hydroxide and chloroacetic acid are added to perform ultrasonic reaction. After the reaction, ethanol and pure water are used for magnetic washing in sequence to obtain carboxylated magnetic graphene oxide, i.e., carboxylated magnetic beads.

[0045] 3. Aminated PEG (Mw 200-100000Da) coupling

[0046] EDC was added to the carboxylated magnetic graphene oxide obtained in step 2 and reacted for at least 30 minutes to activate the carboxyl group. NHS was then added and reacted in an ice bath for at least 30 minutes to obtain a mixed solution. Aminated polyethylene glycol PEG (Aminated PEG, Mw 200-100000Da) was dissolved in pure water and then added to the above mixed solution to carry out an amidation reaction. After the reaction, the mixture was magnetically washed with pure water and vacuum dried to obtain reusable polyethylene glycol-modified magnetic beads, namely exosome capture magnetic beads MGO-PEG (Mw 200-100000Da).

[0047] Aminated PEG can be linear (linear PEG-NH2), four-arm (four-arm PEG-NH2) and eight-arm (eight-arm PEG-NH2). The molecular weight of the amino PEG is 200-100,000 Da, corresponding to MGO-linear PEG magnetic beads, MGO-four-arm PEG magnetic beads and MGO-eight-arm PEG magnetic beads, respectively.

[0048] Furthermore, in step 1, the mass ratio of the monolayer graphene oxide to ferric chloride is 1:2-10; the mass ratio of the monolayer graphene oxide to sodium acetate is 1:20-80; the mass ratio of the monolayer graphene oxide to polyethylene glycol is 1:1-10; the mixture is mixed and stirred for at least 1 hour; after mixing and stirring, the reaction vessel (Teflon high-temperature and high-pressure reactor) is placed in a forced air drying oven for reaction at a reaction temperature of 180-200°C for at least 6 hours.

[0049] Furthermore, in step 2, the mass ratio of the magnetic graphene oxide to sodium hydroxide is 1:20-50, the mass ratio of the magnetic graphene oxide to chloroacetic acid is 1:20-30, and the bath ultrasonic reaction is carried out for at least 2 hours.

[0050] Furthermore, in step 3, the molar ratio of the carboxylated magnetic graphene oxide and EDC is 1:5-20; the molar ratio of the carboxylated magnetic graphene oxide and NHS is 1:5-20; and the molar ratio of the amino PEG (Mw 200-100000Da) and the carboxylated magnetic graphene oxide obtained in step 2 is 20:1-10.

[0051] 2. Exosome Extraction Method

[0052] 1. Initial isolation of exosomes

[0053] Collect cell culture supernatant, blood, urine, saliva, or other biological fluids and centrifuge at 3000g for 10-40 minutes. Discard the pellet (to remove nuclei, heavy mitochondria, and large cell debris) and collect the supernatant. Centrifuge the collected supernatant again at 10,000g for 10-40 minutes. Discard the pellet (to remove nuclei, heavy mitochondria, and large cell debris) and collect the supernatant. Aspirate the supernatant and filter it through a 0.22μm syringe filter to exclude molecules larger than 0.22μm. This will yield the primary exosome sample and store it at 4°C until exosome isolation.

[0054] 2. Magnetic adsorption of exosomes using MGO-PEG

[0055] Take 200-800 μL (1-4 mg) of one of the MGO-linear PEG magnetic beads, MGO-four-arm PEG magnetic beads, and MGO-eight-arm PEG magnetic beads and incubate with 1-5 mL of the initially isolated exosome sample in step 1 in an ice bath for 10-30 min.

[0056] 3. Exosome elution

[0057] After static incubation, the supernatant was removed by magnetic aspiration, and the magnetic beads in the tube were redispersed in 1-5 mL of pH 7.5 eluent. Exosomes were eluted by sonication for 10-30 minutes. The beads were removed using a magnet, and the exosomes were recovered from the supernatant. The recovered exosomes were filtered through a 0.22 μm filter, placed in cryovials, and stored at -80°C, achieving efficient isolation and recovery of exosomes.

[0058] This method achieves efficient separation and recovery of exosomes through specific capture by magnetic beads combined with gentle elution.

[0059] 4. Magnetic bead recycling

[0060] The magnetic beads were washed with ethanol and pure water in sequence, stored in pure water, and the efficiency remained >80% after 10 cycles.

[0061] 3. An exosome extraction kit

[0062] The kit comprises polyethylene glycol-modified magnetic beads and an eluent.

[0063] Principle of the present invention:

[0064] This invention prepares magnetic beads based on a graphene oxide substrate, resulting in a magnetic bead system with a high surface area and multiple binding sites. The superparamagnetic properties of Fe₃O₄ make the beads reusable and structurally stable. Polyethylene glycol (PEG) is introduced through a chemical reaction to construct a novel magnetic bead system that can quickly and effectively isolate exosomes from cell culture supernatant, reduce impurity adsorption, and release the exosomes in a manner that does not compromise their intrinsic activity, enabling their use in subsequent related applications. The resulting magnetic bead system is also stable and reproducible. The principle of polyethylene glycol (PEG) precipitation primarily involves the interaction between PEG and protein molecules, leading to the precipitation of exosomes. PEG possesses chain flexibility and high hydrophilicity. Long PEG chains provide significant steric hindrance, preventing nonspecific protein adsorption and thus separating exosomes. The molecular formula of linear PEG is H-(O-CH₂-CH₂)n-OH. Both the oxygen atoms and the terminal hydroxyl groups in the repeating unit can form hydrogen bonds with water, contributing to the chain flexibility and high hydrophilicity of PEG. PEG can surround and preferentially precipitate EVs through hydrophobic repulsion, and the PEG-coated EV pellet can then be separated from unbound PEG by shaking washing.

[0065] The polyethylene glycol-modified magnetic beads in this invention exhibit excellent colloidal stability (hydrated particle size dispersion index (PDI) <0.2) in aqueous systems (including but not limited to deionized water, phosphate buffer, and cell culture medium) through an optimized linear / branched PEG co-modification interface, while maintaining a high saturation magnetization (>60emu / g), enabling rapid separation within 5 seconds (recovery rate >95%) under conventional magnetic force. Their surface topology, constructed through controlled density grafting of PEG to form a three-dimensional hydrophilic network, precipitates exosomes through hydrophobic interactions. After elution and separation, they also possess excellent magnetic properties, ensuring effective recovery and separation under an external magnetic field.

[0066] The exosome-capturing function of polyethylene glycol-modified magnetic beads lies in the fact that the terminal amino groups of the PEG spacer arms are covalently coupled to the bead surface via EDC / NHS activation, forming a 15-20 nm thick hydration layer. The interaction between PEG and protein molecules surrounds and preferentially precipitates EVs through hydrophobic repulsion, enabling the beads to capture over 90% of exosomes within 10 minutes under physiological conditions (pH 7.0-7.4). PEG is then washed with shaking to separate the PEG-coated EVs (extracellular vesicles) from unbound PEG.

[0067] The exosome separation function of polyethylene glycol-modified magnetic beads lies in the fact that, under mild dissociation conditions, exosomes can be effectively dissociated using 0.5 mol / L NaCl solution or pH 7.5 buffer for 15 minutes, without affecting the biological activity of the exosomes. This avoids potential damage to the exosomes caused by harsh conditions, facilitating subsequent downstream analysis and applications. Furthermore, the material structure is minimally affected.

[0068] The reusability of polyethylene glycol-modified magnetic beads lies in their reusability and structural stability, combined with the superparamagnetic properties of Fe₃O₄. Separation of the beads by applying an external magnetic field allows for repeated capture, enrichment, and separation of exosomes. After ten cycles, the capture efficiency of the beads remained at a high level of 83±5%, demonstrating their excellent stability and durability. These results validate the feasibility and reliability of this material for practical applications.

[0069] In the present invention, magnetic graphene oxide carriers are synthesized by a hydrothermal method, modified with polyethylene glycol (PEG) space arms and constructed in a hydrophobic environment to obtain exosome capture magnetic beads, which achieve efficient capture and reversible release of exosomes. Exosomes can be harvested from cell culture supernatant at low cost without specialized equipment and reduce contamination by impurity proteins. The magnetic beads can be reused, effectively reducing costs.

[0070] Example 1: A method for preparing polyethylene glycol-modified magnetic beads, comprising the following steps:

[0071] (1) Preparation of magnetic graphene oxide: a single layer of graphene oxide was dissolved in ethylene glycol solvent, added to a Teflon high temperature and high pressure reactor, and ultrasonically dispersed for 8 minutes; then ferric chloride, sodium acetate and polyethylene glycol 8000 were added, mixed and stirred for 3 hours, and the reactor was transferred to a forced air drying oven and reacted at a high temperature of 200°C for 10 hours. After the reaction was completed, it was magnetically washed three times with ethanol and pure water respectively, and vacuum dried at 60°C to obtain magnetic graphene oxide.

[0072] The mass ratio of graphene oxide to ferric chloride is 1:5, the mass ratio of graphene oxide to sodium acetate is 1:25, and the mass ratio of graphene oxide to polyethylene glycol 8000 is 1:1.5.

[0073] (2) Preparation of carboxylated magnetic graphene oxide: The magnetic graphene oxide obtained in step 1 was ultrasonically dispersed in pure water for 8 minutes, sodium hydroxide and chloroacetic acid were added, and a bath ultrasonic reaction was carried out for 2 hours. The carboxylated magnetic graphene oxide was obtained after washing with ethanol and pure water.

[0074] The mass ratio of the magnetic graphene oxide to the sodium hydroxide is 1:35, and the mass ratio of the magnetic graphene oxide to the chloroacetic acid is 1:25.

[0075] (3) Coupling of amino-PEG (Mw 200-100000Da): Add EDC to the carboxylated magnetic graphene oxide obtained in step 2 and react for 30 minutes. Then add NHS and react in an ice bath for 2 hours to obtain a mixed solution. Dissolve linear PEG-NH2 in pure water and then add it to the mixed solution. Place it in a shaker and react for 24 hours. After the reaction, wash it with pure water magnetically and vacuum dry it to obtain polyethylene glycol-modified magnetic beads, namely MGO-linear PEG magnetic beads. SEM characterization see Figure 1 .

[0076] The molar ratio of carboxylated magnetic graphene oxide to EDC is 1:15, the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:10, and the mass ratio of amino PEG (Mw 200-100000Da) to carboxylated magnetic graphene oxide is 20:2.

[0077] Example 2

[0078] The difference from Example 1 is that the linear PEG-NH2 is replaced by four-arm PEG-NH2 to prepare reusable polyethylene glycol modified magnetic beads, namely MGO-four-arm PEG magnetic beads. The SEM characterization is shown in Figure 2 .

[0079] Example 3

[0080] The difference from Example 1 is that the linear PEG-NH2 is replaced by eight-arm PEG-NH2 to prepare reusable polyethylene glycol modified magnetic beads, namely MGO-eight-arm PEG magnetic beads. The SEM characterization is shown in Figure 3 .

[0081] from Figure 1-Figure 3 It can be seen that the graphene-grafted material amino-PEG is rich in amino groups. The EDS results show that there is a uniform N distribution on the surface of MGO-linear PEG magnetic beads, MGO-four-arm PEG magnetic beads, and MGO-eight-arm PEG magnetic beads. This proves that the amino-PEG is successfully bound to MGO-COOH through the amidation reaction, and the binding of the amino-PEG is relatively uniform.

[0082] Example 4: A method for extracting extracellular vesicles, comprising the following steps:

[0083] (1) Initial isolation of exosomes: The supernatant of breast cancer cell culture was collected and centrifuged at 3000g for 10 min. The pellet was discarded (nuclei, heavy mitochondria, and large cell debris were removed) and the supernatant was collected. The collected supernatant was centrifuged at 10000g for 30 min. The pellet was discarded (nuclei, heavy mitochondria, and large cell debris were removed) and the supernatant was collected. The supernatant was aspirated and filtered with a 0.22μm syringe filter to exclude molecules larger than 0.22μm and stored at 4°C before exosome isolation.

[0084] (2) Extracting exosomes using MGO-PEG: 500 μL (3 mg) of MGO-linear PEG prepared in Example 1 and 1 mL of the exosome sample initially isolated in step 1 were incubated in an ice bath for 20 min to obtain a magnetic bead-exosome complex.

[0085] (3) Exosome elution: After removing the supernatant by magnetic aspiration, the magnetic bead-exosome complex in the test tube was redispersed in 1 mL of pH 7.5 pure water and the exosomes were eluted by sonication for 20 min. The magnetic beads were removed using a magnet and the exosomes were recovered from the supernatant. The recovered exosomes were filtered through a 0.22 μm filter membrane and stored in cryovials at -80°C.

[0086] (4) Magnetic bead recycling: Use ethanol and pure water to magnetically wash the magnetic beads in turn, store them in pure water, and the efficiency remains >80% after recycling 10 times.

[0087] Example 5

[0088] The same as Example 4, except that the MGO-linear PEG magnetic beads in Example 4 were replaced with MGO-four-arm PEG magnetic beads.

[0089] Example 6

[0090] Same as Example 4, except that the MGO-linear PEG magnetic beads in Example 4 were replaced with MGO-eight-arm PEG magnetic beads.

[0091] Identification of exosomes:

[0092] (1) Exosomes obtained by electron microscopy:

[0093] 10 μL of the exosome extract obtained in Example 4, Example 5 and Example 6 was added dropwise to the copper mesh, adsorbed at room temperature for 10 minutes, and the excess liquid was removed with filter paper. Then 10 μL of 2% mass concentration of phosphotungstic acid solution was added dropwise to the copper mesh, stained at room temperature for 2 minutes, and the excess liquid was removed with filter paper. The copper mesh was dried at room temperature. The observation voltage was set to 120 kV, and transmission electron microscopy was used to observe that the obtained extracellular vesicles had a uniform particle size and a double membrane conformation, which was consistent with the morphology of exosomes. TEM characterization of the exosomes obtained and separated can be found in Figure 4-Figure 6 , Figure 4 This is a TEM image of exosomes after acquisition and separation of MGO-linear PEG (Mw 200-100000Da). It can be seen that the diameter of the separated exosomes is about 105nm, the biological morphology is complete, and the exosomes show a typical cup-shaped or biconcave disc-shaped structure with an intact membrane structure and clear boundaries. Figure 5 This is a TEM image of exosomes after acquisition and separation by MGO-four-arm PEG magnetic beads (Mw 200-100000Da). It can be seen that the diameter of the separated exosomes is about 110nm and the biological morphology is intact. Figure 6 This is a TEM image of exosomes after acquisition and separation of MGO-eight-arm PEG (Mw 200-100000Da). It can be seen that the diameter of the separated exosomes is about 90nm and the biological morphology is complete.

[0094] (2) Identification and extraction of exosomes using Zeta potential analyzer:

[0095] The extracted exosome proteins were identified. The exosomes extracted from Example 4, Example 5 and Example 6 were diluted to 10 8 -10 9 Particles / mL (protein concentration determined by BCA assay is approximately 0.1-1 μg / μL). Use a dedicated folded capillary electrophoresis cell (DTS1070) or a transparent disposable electrode cup to inject the sample until the electrode is submerged (approximately 1 mL). Avoid bubbles (eject by gently tapping the cuvette). Let the sample stand for 2 minutes to stabilize the temperature. Use a zeta potential meter to measure the zeta potential. For characterization of the zeta potential of the exosomes obtained and separated, see [1]. Figure 7-Figure 9 . Figure 7The zeta potential of exosomes obtained and separated from MGO-linear PEG (Mw 200-100,000 Da) is -22.2 mV. The zeta potential of exosomes in the literature (Théry et al., 2018, J Extracell Vesicles) ranges from -10 to -25 mV. Therefore, the zeta potential of the product is consistent with the results in the literature. Figure 8 The zeta potential of exosomes after acquisition and separation using MGO-four-arm PEG magnetic beads (Mw 200-100,000 Da) is -15.7 mV. The zeta potential of exosomes reported in the literature ranges from -10 to -25 mV, so the zeta potential of the product is consistent with the results in the literature. Figure 9 The Zeta potential of exosomes after MGO-octa-arm PEG (Mw 200-100000Da) acquisition and separation is shown. It can be seen that the Zeta potential of the exosomes after separation is -14.6mV. The Zeta potential of exosomes in the literature is distributed between -10 and -25mV, so the Zeta potential of the product is consistent with the results in the literature.

[0096] It can be seen that the exosome capture magnetic beads prepared by the present invention can effectively extract exosomes with high purity, and the extraction and separation methods adopted will not cause damage to the exosomes. The extracted exosomes are intact in morphology and can be used for downstream applications.

[0097] Example 7

[0098] (1) Preparation of magnetic graphene oxide: a single layer of graphene oxide was dissolved in ethylene glycol solvent, added to a Teflon high temperature and high pressure reactor, and ultrasonically dispersed for 8 minutes; then ferric chloride, sodium acetate and polyethylene glycol 8000 were added, mixed and stirred for 1 hour, and the reactor was transferred to a forced air drying oven and reacted at 180°C for 8 hours. After the reaction was completed, the product was magnetically washed three times with ethanol and pure water respectively, and vacuum dried at 60°C to obtain magnetic graphene oxide.

[0099] The mass ratio of graphene oxide to ferric chloride is 1:20, the mass ratio of graphene oxide to sodium acetate is 1:50, and the mass ratio of graphene oxide to polyethylene glycol 8000 is 1:1.

[0100] (2) Preparation of carboxylated magnetic graphene oxide: The magnetic graphene oxide obtained in step 1 was ultrasonically dispersed in pure water for 8 minutes, sodium hydroxide and chloroacetic acid were added, and a bath ultrasonic reaction was carried out for 3 hours. The carboxylated magnetic graphene oxide was obtained after washing with ethanol and pure water.

[0101] The mass ratio of the magnetic graphene oxide to the sodium hydroxide is 1:20, and the mass ratio of the magnetic graphene oxide to the chloroacetic acid is 1:30.

[0102] (3) Coupling of amino-PEG (Mw 200-100,000 Da): EDC was added to the carboxylated magnetic graphene oxide obtained in step 2 and reacted for 30 min. NHS was then added and reacted in an ice bath for 2 h to obtain a mixed solution. Linear PEG-NH2 was dissolved in pure water and then added to the mixed solution. The mixture was allowed to react on a shaker for 24 h. After the reaction, the beads were washed with pure water by magnetic suction and vacuum dried to obtain reusable polyethylene glycol-modified magnetic beads.

[0103] The molar ratio of carboxylated magnetic graphene oxide to EDC is 1:5, the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:20, and the mass ratio of amino PEG (Mw 200-100000Da) to carboxylated magnetic graphene oxide is 20:1.

[0104] Example 8

[0105] (1) Preparation of magnetic graphene oxide: a single layer of graphene oxide was dissolved in ethylene glycol solvent, added to a Teflon high temperature and high pressure reactor, and ultrasonically dispersed for 8 minutes; then ferric chloride, sodium acetate and polyethylene glycol 8000 were added, mixed and stirred for 2 hours, and the reactor was transferred to a forced air drying oven and reacted at 200°C for 6 hours. After the reaction was completed, it was magnetically washed three times with ethanol and pure water respectively, and vacuum dried at 60°C to obtain magnetic graphene oxide.

[0106] The mass ratio of graphene oxide to ferric chloride is 1:10, the mass ratio of graphene oxide to sodium acetate is 1:20, and the mass ratio of graphene oxide to polyethylene glycol 8000 is 1:6.

[0107] (2) Preparation of carboxylated magnetic graphene oxide: The magnetic graphene oxide obtained in step 1 was ultrasonically dispersed in pure water for 8 minutes, sodium hydroxide and chloroacetic acid were added, and a bath ultrasonic reaction was carried out for 4 hours. The carboxylated magnetic graphene oxide was obtained after washing with ethanol and pure water.

[0108] The mass ratio of the magnetic graphene oxide to the sodium hydroxide is 1:40, and the mass ratio of the magnetic graphene oxide to the chloroacetic acid is 1:20.

[0109] (3) Coupling of amino-PEG (Mw 200-100,000 Da): EDC was added to the carboxylated magnetic graphene oxide obtained in step 2 and reacted for 30 min. NHS was then added and reacted in an ice bath for 2 h to obtain a mixed solution. Linear PEG-NH2 was dissolved in pure water and then added to the mixed solution. The mixture was allowed to react on a shaker for 24 h. After the reaction, the beads were washed with pure water by magnetic suction and vacuum dried to obtain reusable polyethylene glycol-modified magnetic beads.

[0110] The molar ratio of carboxylated magnetic graphene oxide to EDC is 1:20, the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:15, and the mass ratio of amino PEG (Mw 200-100000 Da) to carboxylated magnetic graphene oxide is 20:10.

[0111] Example 9

[0112] (1) Preparation of magnetic graphene oxide: a single layer of graphene oxide was dissolved in ethylene glycol solvent, added to a Teflon high temperature and high pressure reactor, and ultrasonically dispersed for 8 minutes; then ferric chloride, sodium acetate and polyethylene glycol 8000 were added, mixed and stirred for 4 hours, and the reactor was transferred to a forced air drying oven and reacted at 190°C for 7 hours. After the reaction was completed, the product was magnetically washed three times with ethanol and pure water respectively, and vacuum dried at 60°C to obtain magnetic graphene oxide.

[0113] The mass ratio of graphene oxide to ferric chloride is 1:15, the mass ratio of graphene oxide to sodium acetate is 1:80, and the mass ratio of graphene oxide to polyethylene glycol 8000 is 1:10.

[0114] (2) Preparation of carboxylated magnetic graphene oxide: The magnetic graphene oxide obtained in step 1 was ultrasonically dispersed in pure water for 8 minutes, sodium hydroxide and chloroacetic acid were added, and a bath ultrasonic reaction was carried out for 5 hours. The carboxylated magnetic graphene oxide was obtained after washing with ethanol and pure water.

[0115] The mass ratio of the magnetic graphene oxide to the sodium hydroxide is 1:50, and the mass ratio of the magnetic graphene oxide to the chloroacetic acid is 1:23.

[0116] (3) Coupling of amino-PEG (Mw 200-100,000 Da): EDC was added to the carboxylated magnetic graphene oxide obtained in step 2 and reacted for 30 min. NHS was then added and reacted in an ice bath for 2 h to obtain a mixed solution. Linear PEG-NH2 was dissolved in pure water and then added to the mixed solution. The mixture was allowed to react on a shaker for 24 h. After the reaction, the beads were washed with pure water by magnetic suction and vacuum dried to obtain reusable polyethylene glycol-modified magnetic beads.

[0117] The molar ratio of carboxylated magnetic graphene oxide to EDC is 1:10, the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:5, and the mass ratio of amino PEG (Mw 200-100000 Da) to carboxylated magnetic graphene oxide is 20:5.

[0118] Example 10

[0119] 1. Initial isolation of exosomes

[0120] Saliva was collected and centrifuged at 3000 g for 10-30 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The collected supernatant was centrifuged again at 10,000 g for 10 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The supernatant was aspirated and filtered through a 0.22 μm syringe filter to exclude molecules larger than 0.22 μm. This yielded the primary exosome sample and stored at 4°C until exosome isolation.

[0121] 2. Magnetic adsorption of exosomes using MGO-PEG

[0122] Take 200 μL of MGO-eight-arm PEG magnetic beads and 1 mL of the exosome sample initially isolated in step 1 and incubate them in an ice bath for 10-30 minutes.

[0123] 3. Exosome elution

[0124] After static incubation, the supernatant was removed by magnetic aspiration, and the magnetic beads in the tube were redispersed in 1 mL of pH 7.5 eluent. Exosomes were eluted by sonication for 30 minutes. The beads were removed using a magnet, and the exosomes were recovered from the supernatant. The recovered exosomes were filtered through a 0.22 μm filter membrane, placed in cryovials, and stored at -80°C, achieving efficient isolation and recovery of exosomes.

[0125] Example 11

[0126] 1. Initial isolation of exosomes

[0127] Blood was collected and centrifuged at 3000 g for 10-30 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The collected supernatant was then centrifuged at 10,000 g for 20 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The supernatant was aspirated and filtered through a 0.22 μm syringe filter to exclude molecules larger than 0.22 μm. This yielded the primary exosome sample and stored at 4°C until exosome isolation.

[0128] 2. Magnetic adsorption of exosomes using MGO-PEG

[0129] Take 800 μL of MGO-linear PEG and 5 mL of the exosome sample initially isolated in step 1 and incubate them in an ice bath for 10-30 minutes.

[0130] 3. Exosome elution

[0131] After static incubation, the supernatant was removed by magnetic aspiration, and the magnetic beads in the tube were redispersed in 5 mL of pH 7.5 eluent. Exosomes were eluted by sonication for 20 minutes. The beads were removed using a magnet, and the exosomes were recovered from the supernatant. The recovered exosomes were filtered through a 0.22 μm filter, placed in cryovials, and stored at -80°C, achieving efficient isolation and recovery of exosomes.

[0132] Example 12

[0133] 1. Initial isolation of exosomes

[0134] Urine was collected and centrifuged at 3000 g for 10-30 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The collected supernatant was then centrifuged at 10,000 g for 40 minutes. The pellet (to remove nuclei, heavy mitochondria, and large cell debris) was discarded, and the supernatant was collected. The supernatant was aspirated and filtered through a 0.22 μm syringe filter to exclude molecules larger than 0.22 μm. This yielded the primary exosome sample and stored at 4°C until exosome isolation.

[0135] 2. Magnetic adsorption of exosomes using MGO-PEG

[0136] Take 500 μL of MGO-four-arm PEG magnetic beads and 3 mL of the exosome sample initially isolated in step 1 and incubate them in an ice bath for 10-30 minutes.

[0137] 3. Exosome elution

[0138] After static incubation, the supernatant was removed by magnetic aspiration, and the magnetic beads in the tube were redispersed in 3 mL of pH 7.5 eluent. Exosomes were eluted by sonication for 10 minutes. The beads were removed using a magnet, and the exosomes were recovered from the supernatant. The recovered exosomes were filtered through a 0.22 μm filter, placed in cryovials, and stored at -80°C, achieving efficient isolation and recovery of exosomes.

[0139] The above description is merely a description of the preferred embodiment of the present invention and is not to be construed as limiting the claims. The present invention is not limited to the above embodiment, and variations in the specific structure are permitted. Any variations made within the scope of the independent claims of the present invention are also within the scope of protection of the present invention.

[0140] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this invention pertains. The terms used herein in the specification of the present invention are for the purpose of describing specific embodiments only and are not intended to limit the present invention. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

Claims

1. A method for preparing reusable polyethylene glycol-modified magnetic beads, characterized in that: The following steps are involved: Adding EDC to the carboxylated magnetic graphene oxide, reacting the mixture, and then adding NHS to the mixture, reacting the mixture to obtain a mixed solution; An aqueous solution of amino polyethylene glycol is added to the mixed solution to carry out an amidation reaction, and the mixed solution is magnetically washed with pure water and dried to obtain reusable polyethylene glycol-modified magnetic beads.

2. The method for preparing reusable polyethylene glycol-modified magnetic beads according to claim 1, wherein: The molecular weight of amino polyethylene glycol is 200-100000 Da.

3. The method for preparing reusable polyethylene glycol-modified magnetic beads according to claim 1, characterized in that: The amino polyethylene glycol includes linear amino polyethylene glycol, four-arm amino polyethylene glycol and eight-arm amino polyethylene glycol.

4. The method for preparing reusable polyethylene glycol-modified magnetic beads according to claim 1, wherein: The molar ratio of carboxylated magnetic graphene oxide to EDC is 1:5-20; the molar ratio of carboxylated magnetic graphene oxide to NHS is 1:5-20; and the molar ratio of amino polyethylene glycol to carboxylated magnetic graphene oxide is 20:1-10.

5. The method for preparing reusable polyethylene glycol-modified magnetic beads according to claim 1, characterized in that: Carboxylated magnetic graphene oxide is prepared by the following process: The magnetic graphene oxide is ultrasonically dispersed in pure water, and then sodium hydroxide and chloroacetic acid are added to carry out a bath ultrasonic reaction to prepare the carboxylated magnetic graphene oxide.

6. The method for preparing reusable polyethylene glycol-modified magnetic beads according to claim 5, characterized in that: The mass ratio of magnetic graphene oxide to sodium hydroxide is 1:20-50, the mass ratio of magnetic graphene oxide to chloroacetic acid is 1:20-30, and the bath ultrasonic reaction time is at least 2 hours.

7. A reusable polyethylene glycol-modified magnetic bead prepared according to the method according to any one of claims 1 to 6.

8. Use of reusable polyethylene glycol-modified magnetic beads prepared according to the method according to any one of claims 1 to 6 in extracting exosomes.

9. An exosome extraction kit, characterized in that: The invention comprises reusable polyethylene glycol-modified magnetic beads prepared by the method according to any one of claims 1 to 6 and an eluent.

10. A method for extracting exosomes, characterized in that: The following steps are involved: The reusable polyethylene glycol-modified magnetic beads prepared by the method according to any one of claims 1 to 6 are added to the exosome sample, and the mixture is incubated in an ice bath to obtain a mixed solution; and the exosomes in the mixed solution are eluted to obtain exosomes.

Citation Information

Patent Citations

  • Magnetic bead, preparation method thereof and application of magnetic bead in extracellular vesicle extraction

    CN117095895A

  • Preparation method of Apt-S-S-rMGO exosome capture immunomagnetic bead and method for extracting exosome by using Apt-S-S-rMGO exosome capture immunomagnetic bead

    CN118258991A