Power storage cell
The power storage cell addresses uneven electrode reactions by structuring the electrode into regions with varying resistance and composition, improving performance stability and longevity.
Patent Information
- Application Number
- JP2023077739
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2043-05-10
AI Technical Summary
The power storage cell experiences uneven electrode reactions in the length and width directions of the strip electrode, leading to performance deterioration.
The electrode is designed with distinct regions: a first region where the current collector is exposed, a second region with higher reaction resistance and current density, and a third region with lower resistance, utilizing varying BET specific surface areas and binder mass fractions to adjust reaction resistance.
This design reduces reaction unevenness in the width direction, enhancing the electrode's performance stability and longevity.
Smart Images

Figure 2024162339000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an energy storage cell. [Background technology]
[0002] Japanese Patent Application Laid-Open No. 2018-018680 (Patent Document 1) discloses a strip-shaped electrode. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2018-018680 A Summary of the Invention [Problem to be solved by the invention]
[0004] The energy storage cell includes a power generating element. The power generating element includes, for example, a wound electrode body. The wound electrode body is formed by winding a strip electrode into a spiral shape. The strip electrode has a current collecting portion. The current collecting portion is electrically connected to an electrode terminal (external terminal). For example, the current collecting portion may be disposed at an end portion in the longitudinal direction of the strip electrode. When the current collecting portion is disposed at an end portion in the longitudinal direction, unevenness in the electrode reaction may occur in the longitudinal direction of the strip electrode. Hereinafter, the unevenness in the electrode reaction may also be referred to as "uneven reaction." The uneven reaction may promote performance degradation.
[0005] In order to reduce the uneven reaction in the longitudinal direction, it is conceivable to form a current collecting portion that extends continuously in the longitudinal direction at the end of the width direction of the strip-shaped electrode, but in this case, there is a possibility that uneven reaction in the width direction will occur.
[0006] An object of the present disclosure is to reduce reaction unevenness in the width direction of the strip-shaped electrode. [Means for solving the problem]
[0007] 1. The energy storage cell includes a wound electrode body and an electrode terminal. The wound electrode body includes a strip electrode. In a plan view, the strip electrode has a length direction and a width direction. The width direction is perpendicular to the length direction. The strip electrode is wound in the length direction to form a wound electrode body. The strip electrode includes a current collector and a composite layer. The composite layer includes active material particles. The composite layer is disposed on the surface of the current collector. In the width direction in a plan view, the strip electrode includes a first region, a second region, and a third region. The first region is disposed at an end in the width direction. In the first region, the current collector is exposed. In the first region, the current collector is electrically connected to the electrode terminal. The second region and the third region are covered by the composite layer. In the width direction, the second region is disposed between the first region and the third region. The second region has a reaction resistance per unit area larger than that of the third region.
[0008] The first region corresponds to the current collecting section. The second region is closer to the current collecting section (first region) than the third region. The second region tends to have a higher current density than the third region. It is believed that the electrode reaction is promoted in the second region more than in the third region, which causes the reaction to become uneven.
[0009] In the storage cell described in "1" above, the reaction resistance per unit area varies locally. Hereinafter, "reaction resistance per unit area" is also referred to simply as "reaction resistance." The second region has a larger reaction resistance than the third region. That is, the electrode reaction is less likely to proceed in the second region than in the third region. Therefore, it is expected that the reaction unevenness in the width direction of the strip electrode will be reduced.
[0010] 2. The storage cell according to "1" above may have, for example, the following configuration: In the second region, the mixture layer includes first active material particles. In the third region, the mixture layer includes second active material particles. The first active material particles have a smaller BET specific surface area than the second active material particles.
[0011] It is believed that the smaller the BET specific surface area of the active material particles, the smaller the reaction field (reaction area) between the active material particles and carrier ions (e.g., Li ions). It is believed that the smaller the reaction area, the higher the reaction resistance. In other words, the reaction resistance of each region can be adjusted by the BET specific surface area of the active material particles.
[0012] 3. The storage cell according to "1" or "2" above may include, for example, the following configuration. In the second region, the composite layer includes first composite particles. In the third region, the composite layer includes second composite particles. Each of the first composite particles and the second composite particles includes active material particles and a binder. The binder covers at least a portion of the surface of the active material particles. The first composite particles have a larger mass fraction of the binder than the second composite particles.
[0013] For example, the active material particles and the binder may form a composite particle. The binder may inhibit ion conduction. It is considered that the reaction resistance may increase in the portion of the surface of the active material particle to which the binder is attached. It is considered that the mass fraction of the binder in the composite particle corresponds to the amount of the binder attached and the coverage of the active material particle. It is considered that the reaction resistance may increase as the mass fraction of the binder in the composite particle increases. In other words, the reaction resistance of each region can be adjusted by the mass fraction of the binder in the composite particle.
[0014] 4. The energy storage cell according to any one of the above items "1" to "3" may include, for example, the following configuration. In the second region, the mixture layer includes a first layer and a second layer. In a cross-sectional view of the strip electrode, the first layer is disposed between the current collector and the second layer. The second layer has a smaller mass fraction of active material particles than the first layer.
[0015] In the surface layer (second layer) of the composite layer, the mass fraction of the active material particles is small, and thus an increase in reaction resistance is expected. The mass fraction of the active material particles in the second layer may be, for example, zero. For example, the second layer may be formed by applying a polymer solution to the surface of the first layer.
[0016] 5. The energy storage cell according to any one of "1" to "4" above may include, for example, the following configuration. The band-shaped electrode has an inner circumferential surface and an outer circumferential surface. In the wound electrode body, the inner circumferential surface is disposed on the inner circumferential side. The outer circumferential surface is the surface opposite to the inner circumferential surface. A first mixture layer is disposed on the inner circumferential surface. A second mixture layer is disposed on the outer circumferential surface. The first mixture layer has a reaction resistance per unit area larger than that of the second mixture layer.
[0017] In the wound electrode body, the inner peripheral surface tends to dissipate heat less easily than the outer peripheral surface. That is, the inner peripheral surface tends to become hotter than the outer peripheral surface. Due to the temperature difference between the inner peripheral surface and the outer peripheral surface, there is a possibility that uneven reaction occurs between the inner peripheral surface and the outer peripheral surface. Compared to the mixture layer (second mixture layer) on the outer peripheral surface, the mixture layer (first mixture layer) on the inner peripheral surface has a large reaction resistance, so that the temperature difference between the inner peripheral surface and the outer peripheral surface can be reduced. It is expected that the reduction in temperature difference will reduce uneven reaction between the inner peripheral surface and the outer peripheral surface.
[0018] Hereinafter, an embodiment of the present disclosure (hereinafter, may be abbreviated as "the present embodiment") will be described. However, the present embodiment does not limit the technical scope of the present disclosure. The present embodiment is illustrative in all respects. The present embodiment is non-restrictive. The technical scope of the present disclosure encompasses all modifications within the meaning and scope equivalent to the description of the claims. For example, it is also intended from the beginning that any configuration may be extracted from the present embodiment and arbitrarily combined. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1 is a schematic cross-sectional view showing an example of a power storage cell according to the present embodiment. [Diagram 2] FIG. 2 is a schematic plan view showing an example of a strip-shaped electrode in this embodiment. [Diagram 3] FIG. 3 is a conceptual diagram of a composite particle in this embodiment. [Figure 4] FIG. 4 is a first schematic cross-sectional view showing an example of a strip-shaped electrode in this embodiment. [Diagram 5]FIG. 5 is a second schematic cross-sectional view showing an example of a strip-shaped electrode in this embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] <Terminology explanation> The "reaction resistance per unit area" is measured by the following procedure. A fully discharged storage cell is disassembled to recover the strip-shaped electrodes, and samples of a predetermined area are cut out from each of the measurement targets (second region, third region). An evaluation cell (single cell or half cell) is prepared. The evaluation cell includes the sample as a working electrode. The counter electrode may be, for example, Li foil. AC impedance measurement is performed. A Cole-Cole plot is created based on the measurement results. In the Cole-Cole plot, two intersections between the arc and the real axis (horizontal axis) are identified. The difference (absolute value) between the two intersections is regarded as the reaction resistance. The reaction resistance is divided by the opposing area of the sample (working electrode) and the counter electrode to obtain a value per unit area.
[0021] "Specific surface area" refers to the surface area per unit mass. "BET specific surface area" refers to the specific surface area measured by gas adsorption method (BET single point method). The adsorbate in the gas adsorption measurement is nitrogen.
[0022] "Planar view" refers to viewing an object from a line of sight parallel to the thickness direction of the object (e.g., a strip electrode). Planar view corresponds to a plan view. "Cross-sectional view" refers to viewing an object from a line of sight perpendicular to the thickness direction of the object. Cross-sectional view corresponds to a cross-sectional view.
[0023] Geometric terms (e.g., "parallel," "orthogonal," etc.) should not be interpreted in a strict sense. For example, "parallel" may deviate slightly from the strict meaning of "parallel." Geometric terms may include, for example, tolerances, errors, etc. in design, work, manufacturing, etc. The dimensional relationships in each drawing may not match the actual dimensional relationships. To aid the reader's understanding, the dimensional relationships (length, width, thickness, etc.) in each drawing may be changed. Furthermore, some configurations may be omitted.
[0024] "Electrically connected" means that two objects are electrically connected to each other. The two objects may be directly connected to each other. An electrically conductive member may connect the two objects to each other.
[0025] Terms expressed in the singular also refer to the plural form unless otherwise specified. For example, the term "particle" refers not only to a single particle, but also to a plurality of particles (a particle group) and an aggregate of particles (powder).
[0026] For example, a numerical range such as "m to n%" includes the upper and lower limits unless otherwise specified. In other words, "m to n%" indicates a numerical range of "m% or more and n% or less." Also, "m% or more and n% or less" includes "more than m% but less than n%."
[0027] The term "storage cell" refers to a cell that can be charged. The storage cell is also referred to as, for example, a "secondary battery". The storage cell may be any battery system. The storage cell may be, for example, a lithium ion battery. The storage cell may be any liquid battery, polymer battery, or all-solid-state battery. The storage cell may have any external shape. The storage cell may be, for example, cylindrical, rectangular, or pouch-shaped. The pouch-shaped refers to a form in which the exterior body is a pouch made of a metal foil laminate film. In this embodiment, a cylindrical liquid battery is described as an example.
[0028] <Energy storage cell> FIG. 1 is a schematic cross-sectional view showing an example of a storage cell in this embodiment. The storage cell 100 is cylindrical. The storage cell 100 has a height direction (H direction) and a radial direction (R direction). The storage cell 100 includes a wound electrode body 50. The storage cell 100 may further include a case 30. The case 30 houses the wound electrode body 50. The case 30 may be made of metal, for example. The case 30 is cylindrical. The case 30 may include, for example, a cap 31 and a can 32. The storage cell 100 includes an electrode terminal. For example, the cap 31 and the can 32 may each function as an electrode terminal. That is, the cap 31 may have a polarity different from that of the can 32. When the cap 31 is positive, the can 32 is negative. When the cap 31 is negative, the can 32 is positive. For example, a gasket 33 may electrically isolate the cap 31 from the can 32 .
[0029] The wound electrode body 50 has a cylindrical or columnar outer shape. For example, when the energy storage cell 100 is rectangular or pouch-shaped, the wound electrode body 50 may be pressed in the R direction to form the wound electrode body 50 into a flat shape.
[0030] The wound electrode body 50 includes a positive electrode 51 and a negative electrode 52. Both the positive electrode 51 and the negative electrode 52 are strip-shaped electrodes. That is, the wound electrode body 50 includes strip-shaped electrodes. The wound electrode body 50 may further include a separator 53. The separator 53 is interposed between the positive electrode 51 and the negative electrode 52. The separator 53 electrically separates the positive electrode 51 from the negative electrode 52. For example, the positive electrode 51, the separator 53, and the negative electrode 52 may be stacked in this order to form a laminate. The laminate may be spirally wound to form the wound electrode body 50. For example, the wound electrode body 50 may be stored in the case 30 so that the winding axis of the wound electrode body 50 is parallel to the H direction.
[0031] Separator 53 may include, for example, a porous film made of resin. An electrolytic solution (not shown) can permeate separator 53. The electrolytic solution may include, for example, an organic solvent and a supporting electrolyte (for example, a Li salt).
[0032] The first current collecting tab 61 electrically connects the positive electrode 51 and the cap 31. The second current collecting tab 62 electrically connects the negative electrode 52 and the can 32. The energy storage cell 100 may have, for example, a "tabless structure". The tabless structure does not have a current collecting tab. In the tabless structure, a strip-shaped electrode (at least one of the positive electrode 51 and the negative electrode 52) can be directly connected to an electrode terminal.
[0033] <Strip electrode> FIG. 2 is a schematic plan view showing an example of a strip electrode in this embodiment. The strip electrode 10 in FIG. 2 may be either a positive electrode 51 or a negative electrode 52. The strip electrode 10 has a length direction (L direction) and a width direction (W direction). The W direction is perpendicular to the L direction. The strip electrode 10 is wound in the L direction to form a wound electrode body 50. The W direction of the strip electrode 10 corresponds to the H direction of the energy storage cell 100. In the strip electrode 10, the ratio of the L direction dimension to the W direction dimension may be, for example, any of 2 or more, 5 or more, 10 or more, or 100 or more.
[0034] The strip-shaped electrode 10 includes a current collector 11 and a composite layer 12. The current collector 11 has electrical conductivity. The current collector 11 can be a base material of the strip-shaped electrode 10. The current collector 11 may include, for example, a metal foil or the like. The current collector 11 may include, for example, at least one selected from the group consisting of Al, Cu, Ti, Ni, and Fe.
[0035] The composite material layer 12 is disposed on the surface of the current collector 11. The composite material layer 12 may be disposed, for example, on only one surface of the current collector 11. The composite material layer 12 may be disposed, for example, on both surfaces of the current collector 11. The composite material layer 12 can be formed by coating the surface of the current collector with a composite material.
[0036] The mixture layer 12 includes active material particles. The mixture layer 12 may further include a binder, a conductive material, and the like. The active material particles can cause an electrode reaction (positive electrode reaction or negative electrode reaction). The active material particles can include any component. The active material particles may include, for example, a positive electrode active material. The positive electrode active material may include, for example, at least one selected from the group consisting of LiCoO2, LiNiO2, LiMnO2, LiMn2O4, Li(NiCoMn)O2, Li(NiCoAl)O2, and LiFePO4. The active material particles may include, for example, a negative electrode active material. The negative electrode active material may include, for example, graphite, soft carbon, hard carbon, Si, SiO, Si-C, a Si-based alloy, Sn, SnO, a Sn-based alloy, and Li4Ti5O. 12 The material may contain at least one selected from the group consisting of: Here, "Si-C" refers to a composite material of Si and carbon.
[0037] The binder can bind the solid material. The binder can include any component. The binder may include at least one selected from the group consisting of polyvinylidene fluoride (PVdF), polytetrafluoroethylene (PTFE), vinylidene fluoride-hexafluoropropylene copolymer (PVdF-HFP), styrene butadiene rubber (SBR), carboxymethyl cellulose (CMC), polyimide (PI), polyamideimide (PAI) and polyacrylic acid (PAA). The amount of the binder may be, for example, 0.1 to 10 parts by mass with respect to 100 parts by mass of the active material particles.
[0038] The conductive material can form an electron conduction path. The conductive material can include any component. The conductive material may include at least one selected from the group consisting of carbon black, vapor-grown carbon fiber, carbon nanotubes, and graphene flakes. The amount of the conductive material may be, for example, 0.1 to 10 parts by mass with respect to 100 parts by mass of the active material particles.
[0039] <1st area, 2nd area, 3rd area> In the W direction in a plan view (FIG. 2), the strip electrode 10 includes a first region 101, a second region 102, and a third region 103. The first region 101 is disposed at an end in the W direction. The first region 101 may be disposed at only one end in the W direction. The first region 101 may be disposed at both ends in the W direction. In the first region 101, the current collector 11 is exposed. The first region 101 may be referred to as, for example, a "non-coated portion". The first region 101 may be formed continuously over the entire area in the L direction. The first region 101 may be formed in a part of the L direction.
[0040] The first region 101 is a current collecting section. That is, in the first region 101, the current collector 11 is electrically connected to the electrode terminal (the cap 31 or the can 32). The first current collecting tab 61 may electrically connect the current collector 11 and the cap 31 (see FIG. 1). The second current collecting tab 62 may electrically connect the current collector 11 and the can 32 (see FIG. 1). Each current collecting tab may be welded to the first region 101, for example. For example, in the case of a tabless structure, the first region 101 (current collector 11) may be bent toward the inner circumference in the wound electrode body 50 to form an end face (see FIG. 2). The end face may be perpendicular to the winding axis of the wound electrode body 50. The end face may be flat or curved. The end face may have projections and recesses. A current collecting plate may be welded to the end face. The end face may be in surface contact with the current collecting plate. A cap 31 or the like may be directly welded to the end face.
[0041] The second region 102 and the third region 103 are covered by the composite layer 12. The second region 102 and the third region 103 may be referred to as, for example, a "coated portion". In the W direction, the second region 102 is disposed between the first region 101 and the third region 103. The second region 102 may be adjacent to the first region 101. The second region 102 may be adjacent to the third region 103.
[0042] The second region 102 has a larger reaction resistance than the third region 103. Therefore, it is expected that the reaction unevenness in the W direction will be reduced. The ratio (r2 / r3) of the reaction resistance (r2) of the second region 102 to the reaction resistance (r3) of the third region 103 may be, for example, any of 1.1 or more, 1.5 or more, 2 or more, 5 or more, or 10 or more. The ratio (r2 / r3) may be, for example, any of 10 or less, 5 or less, 2 or less, or 1.5 or less.
[0043] The second region 102 and the third region 103 may be formed, for example, by applying two types of composite materials in a stripe pattern. The dimension (W2) of the second region 102 and the dimension (W3) of the third region 103 in the W direction may satisfy the relationship of, for example, "W2 / W3=5 / 5 to 1 / 9" or "W2 / W3=3 / 7 to 1 / 9". The dimension (W1) of the first region 101 in the W direction may be set arbitrarily in accordance with, for example, the current collecting structure.
[0044] <Specific surface area> The reaction resistance of each region may be adjusted, for example, by the BET specific surface area of the active material particles. For example, in the second region 102, the composite layer 12 may contain first active material particles. In the third region 103, the composite layer 12 may contain second active material particles. The first active material particles may have a smaller BET specific surface area than the second active material particles. Since the BET specific surface area (S1) of the first active material particles is smaller than the BET specific surface area (S2) of the second active material particles, the second region 102 may have a larger reaction resistance than the third region 103. The chemical composition of the first active material particles may be the same as or different from that of the second active material particles.
[0045] The ratio (S1 / S2) of the BET specific surface area (S1) of the first active material particles to the BET specific surface area (S2) of the second active material particles may be, for example, 0.9 or less, 0.8 or less, 0.7 or less, 0.6 or less, 0.5 or less, 0.4 or less, 0.3 or less, 0.2 or less, or 0.1 or less. The ratio (S1 / S2) may be, for example, 0.1 or more, 0.2 or more, 0.3 or more, 0.4 or more, 0.5 or more, 0.6 or more, 0.7 or more, or 0.8 or more. The BET specific surface area (S1) and the BET specific surface area (S2) are each independently, for example, 0.1 to 10 m 2 / g.
[0046] <Composite particles> FIG. 3 is a conceptual diagram of a composite particle in this embodiment. For example, the composite particle 5 includes an active material particle 1 and a binder 2. The binder 2 covers at least a part of the surface of the active material particle 1. The composite particle 5 may further include a conductive material (not shown). For example, the binder 2 may fix the conductive material to the active material particle 1. The composite particle 5 may be formed by any particle composite treatment. For example, the active material particle 1 and the binder 2 may be mixed under conditions in which a strong shear force is applied to form the composite particle 5. For example, the particle composite treatment may be performed using a product named "Mechano Hybrid" manufactured by Nippon Coke & Engineering Co., Ltd.
[0047] For example, the reaction resistance of each region may be adjusted by the mass fraction of the binder in the composite particle. For example, in the second region 102, the composite layer 12 may contain the first composite particle. In the third region 103, the composite layer 12 may contain the second composite particle. The first composite particle may have a mass fraction of the binder larger than that of the second composite particle. The mass fraction (B1) of the binder in the first composite particle is larger than the mass fraction (B2) of the binder in the second composite particle, so that the second region 102 may have a reaction resistance larger than that of the third region 103. The chemical composition of the active material particles and the binder in the first composite particle may be the same as or different from that of the second composite particle.
[0048] The ratio (B1 / B2) of the mass fraction (B1) of the binder in the first composite particle to the mass fraction (B2) of the binder in the second composite particle may be, for example, any one of 1.1 or more, 1.5 or more, 2 or more, 5 or more, or 10 or more. The ratio (B1 / B2) may be, for example, any one of 10 or less, 5 or less, 2 or less, or 1.5 or less. The mass fraction (B1) of the binder and the mass fraction (B2) of the binder may each independently be 0.1 to 10%.
[0049] <Multilayer structure> FIG. 4 is a first schematic cross-sectional view showing an example of a strip electrode in this embodiment. The thickness direction (T direction) of the strip electrode 10 corresponds to the R direction of the energy storage cell 100. For example, in the second region 102, the composite layer 12 may have a multi-layer structure, so that the reaction resistance of each region may be adjusted. For example, in the second region 102, the composite layer 12 may include a first layer 12L and a second layer 12U. The first layer 12L and the second layer 12U may be referred to as, for example, a lower layer and an upper layer. In a cross-sectional view (FIG. 4), the first layer 12L is disposed between the current collector 11 and the second layer 12U. The second layer 12U may have a mass fraction of active material particles smaller than that of the first layer 12L. The ratio (A2 / A1) of the mass fraction (A2) of the active material particles in the second layer 12U to the mass fraction (A1) of the active material particles in the first layer 12L may be, for example, 0.9 or less, 0.8 or less, 0.7 or less, 0.6 or less, 0.5 or less, 0.4 or less, 0.3 or less, 0.2 or less, or 0.1 or less. The ratio (A2 / A1) may be, for example, 0.1 or more, 0.2 or more, 0.3 or more, 0.4 or more, 0.5 or more, 0.6 or more, 0.7 or more, or 0.8 or more. The mass fraction (A2) of the active material particles in the second layer 12U may be, for example, zero.
[0050] The second layer 12U may contain, for example, an inorganic filler, a solid electrolyte, a gel electrolyte, a polymer, or the like. The second layer 12U may contain, for example, at least one selected from the group consisting of alumina, boehmite, titania, polyethylene (PE), PI, aramid, PVdF, PVdF-HFP, PAA, CMC, polyvinyl alcohol (PVA), and polyethylene oxide (PEO). When the second layer 12U does not contain active material particles, the second layer 12U may extend in the W direction so as to cover, for example, a part of the surface of the current collector 11. The first layer 12L may have, for example, the same composition as the composite layer 12 in the third region 103. For example, the second layer 12U may be formed by applying a polymer solution (for example, a PVdF-HFP solution, etc.) to the surface of the second region 102 (composite layer 12).
[0051] <Gradation (composition gradient)> The composition of the composite layer 12 may change in the second region 102. For example, the composition of the composite layer 12 may change continuously or stepwise in the W direction. For example, the composition of the composite layer 12 may change so that the reaction resistance increases toward the first region 101 (current collecting portion). For example, the mass fraction of the active material particles may decrease toward the first region 101. For example, the mass fraction of the binder may increase toward the first region 101.
[0052] <Inner and outer surfaces> FIG. 5 is a second schematic cross-sectional view showing an example of the strip electrode in this embodiment. The strip electrode 10 has an inner circumferential surface P1 and an outer circumferential surface P2. In the wound electrode body 50, the inner circumferential surface P1 is disposed on the inner circumferential side. The outer circumferential surface P2 is the opposite surface to the inner circumferential surface P1. The first composite layer 12F is disposed on the inner circumferential surface P1. The second composite layer 12B is disposed on the outer circumferential surface P2. For example, the first composite layer 12F may have a larger reaction resistance than the second composite layer 12B. For example, the second region 102 in the first composite layer 12F may have a larger reaction resistance than the second region 102 in the second composite layer 12B. For example, the third region 103 in the first composite layer 12F may have a larger reaction resistance than the third region 103 in the second composite layer 12B.
[0053] The reaction resistance (r B ) The reaction resistance (r F ) ratio (r F / r B ) may be, for example, 1.1 or more, 1.5 or more, 2 or more, 5 or more, or 10 or more. F / r B ) may be, for example, 10 or less, 5 or less, 2 or less, or 1.5 or less. [Explanation of symbols]
[0054] 1 active material particle, 2 binder, 5 composite particle, 10 strip electrode, 11 current collector, 12 composite layer, 12F first composite layer, 12B second composite layer, 12L first layer, 12U second layer, 30 case, 31 cap, 32 can, 33 gasket, 50 wound electrode body, 51 positive electrode, 52 negative electrode, 53 separator, 61 first current collecting tab, 62 second current collecting tab, 100 storage cell, 101 first region, 102 second region, 103 third region, P1 inner surface, P2 outer surface.
Claims
1. A wound electrode body and an electrode terminal are included. The wound electrode body includes a strip-shaped electrode, In a plan view, the strip-shaped electrode has a length direction and a width direction, The width direction is perpendicular to the length direction, the strip-shaped electrode is wound in the length direction to form the wound electrode body, the strip-shaped electrode includes a current collector and a composite layer, The mixture layer contains active material particles, the mixture layer is disposed on a surface of the current collector, In the width direction in the plan view, the strip-shaped electrode includes a first region, a second region, and a third region, The first region is disposed at an end in the width direction, The current collector is exposed in the first region, In the first region, the current collector is electrically connected to the electrode terminal, the second region and the third region are covered with the composite layer, In the width direction, the second region is disposed between the first region and the third region, and The second region has a reaction resistance per unit area larger than that of the third region. Energy storage cell.
2. In the second region, the mixture layer includes first active material particles, In the third region, the mixture layer includes second active material particles, and The first active material particles have a smaller BET specific surface area than the second active material particles. The storage cell according to claim 1 .
3. In the second region, the composite layer includes first composite particles, In the third region, the composite layer includes second composite particles, each of the first composite particles and the second composite particles includes the active material particles and a binder; The binder covers at least a part of the surface of the active material particles, and the first composite particles have a greater mass fraction of the binder than the second composite particles; The storage cell according to claim 1 .
4. In the second region, the composite layer includes a first layer and a second layer, In a cross-sectional view of the strip electrode, the first layer is disposed between the current collector and the second layer, and the second layer has a smaller mass fraction of the active material particles than the first layer; The storage cell according to claim 1 .
5. the strip electrode has an inner circumferential surface and an outer circumferential surface; In the wound electrode body, the inner circumferential surface is disposed on the inner circumferential side, The outer circumferential surface is an opposite surface to the inner circumferential surface, A first composite layer is disposed on the inner circumferential surface, A second composite layer is disposed on the outer circumferential surface; and The first mixture layer has a reaction resistance per unit area that is larger than that of the second mixture layer. The storage cell according to any one of claims 1 to 4.
Citation Information
Patent Citations
Nonaqueous electrolyte secondary battery and manufacturing method of electrode for nonaqueous electrolyte secondary battery
JP2008311164A
Nonaqueous electrolyte secondary battery and battery pack
JP2016072110A
Nonaqueous electrolyte secondary battery
JP2016162618A
Negative electrode for lithium ion secondary battery
JP2020129479A
Power storage element
JP2021128851A