Non-woven insulating fire- resistant material for clothing

LAE71UUndetermined Publication Date: 2022-06-24OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOSTYU FABRIKA NETKANYH MATERIALOV WES MIR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
LAE71
Authority / Receiving Office
LA · LA
Patent Type
Utility models
Current Assignee / Owner
Priority Date
2018-01-26
Filing Date
2018-12-26
Publication Date
2022-06-24
Estimated Expiration
2028-12-26

AI Technical Summary

Technical Problem

Existing non-woven insulating fire-resistant materials for clothing have insufficient fire resistance and thermal resistance due to a low content of non-flammable fibers, leading to weak bonding, fiber migration, and low integrity, which worsens with increased fire-resistant fiber content.

Method used

A non-woven insulating material composed of 20-30% bicomponent core-shell fibers and 70-80% oxidized polyacrylonitrile fibers, with a specific ratio and thermal bonding structure, forming a three-layer fabric with additional calendering for enhanced strength and thermal resistance.

Benefits of technology

The material achieves high fire resistance, total thermal resistance, and maintains integrity with a limited flame propagation index of 3, ensuring effective thermal protection and strength while preventing fiber migration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The utility model relates to a non-woven fibrous insulating material having fire-resistant properties, and is used for forming a lining layer in garments. The technical result of the proposed utility model lies in improving the fire-resistance and overall thermal resistance of an insulating material while preserving the integrity of said material. A non-woven insulating fire-resistant material for forming a lining layer in garments includes a blend of polymer fibres joined into a web by thermal bonding, and contains polymer fibres and bicomponent fibres of the concentric core-sheath variety. The bicomponent fibres have a linear density of 0.22 tex, and the polymer fibres include oxidized polyacrylonitrile fibres having a linear density of 0.17 tex, wherein the aforesaid blend contains (in mass%): 20-30% bicomponent fibres, and 70-80% oxidized polyacrylonitrile fibres. In such a blend, the ratio by mass of bicomponent fibres to oxidized polyacrylonitrile fibres is from 1:4 to 3:7. In terms of structure, the material is comprised of three layers: an upper layer, a lower layer, and an inner layer. The upper and lower layers are stronger than the inner layer and are formed by additional thermal bonding of the outer regions of the material using hot calender rolls.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Non-woven fire-resistant insulation material for clothing

[0002] This utility model relates to a non-woven fibrous insulating material with fire-resistant properties and is used to form the lining layer of garments. The proposed insulating material can be used as a lining for all types of clothing, special-purpose products, and accessories, primarily in the production of high-tech outerwear for protection against thermal hazards.

[0003] A non-woven fire-resistant insulating material is known from the prior art for forming a lining layer of a garment, comprising a mixture of polymer fibers combined into a fabric by thermal bonding, containing polymer fibers and a bicomponent fiber of the core-shell type with a concentric arrangement, wherein the polymer fibers include non-combustible fire-resistant viscose fibers (see RU 34549 U1, 10.12.2003 - selected as a prototype), wherein the total mass content of non-combustible fire-resistant viscose fibers and bicomponent fibers in the material is no more than 50%.

[0004] The disadvantages of the material used in the prototype include insufficient fire resistance, as the content of non-flammable, flame-retardant fibers is too low. When exposed to a gas burner, holes and edge burning occur in this material. Since the mass content of bicomponent fibers in the material is not specified, such a material may have insufficient fiber bonding, which will lead to a decrease in the strength of the insulating material, loss of its integrity, and high fiber migration due to insufficient bonding. Since the total mass content of non-flammable, flame-retardant viscose fibers and bicomponent fibers in the material is no more than 50%, increasing the content of non-flammable fibers (and improving fire resistance) in the prototype material will reduce the bicomponent fiber content, thereby reducing strength. The overall thermal resistance of the material is also very low.

[0005] The objective of this utility model is to eliminate the above mentioned disadvantages.

[0006] The technical result of the proposed utility model consists of simultaneously increasing the fire resistance and overall thermal resistance of the insulating material while maintaining its integrity (high strength). The claimed nonwoven, fire-resistant insulating material for forming the lining layer of a garment comprises a blend of polymer fibers thermally bonded into a fabric, and contains polymer fibers and bicomponent core-shell fibers in a concentric arrangement.

[0007] According to the utility model, the bicomponent fibers have a linear density of 0.22 tex, the polymer fibers include oxidized polyacrylonitrile fibers with a linear density of 0.17 tex, wherein said mixture contains, by weight %: bicomponent fibers - 20-30%, oxidized polyacrylonitrile fibers - 70-80%, and in such a mixture the ratio of the contents of the components of the bicomponent fibers to the oxidized polyacrylonitrile fibers by weight is from 1 / 4 to 3 / 7, and the material is structurally made in the form of three layers - upper, lower and inner, wherein the upper and lower layers have higher strength than the inner layer, and are formed by additional thermal bonding of the outer sections of the material with hot calender rollers.

[0008] Additionally, the unevenness of the web mass should not exceed 7%.

[0009] The utility model is illustrated by figures. Fig. 1 shows a graph of the dependence of the limited flame spread index according to GOST ISO 141 16 on the mass content of bicomponent fibers of a given density in the material (in %) and on the mass content of oxidized polyacrylonitrile fibers of a given density in the material (in %); a graph of the dependence of the total thermal resistance (in m 2 °C / W) on the mass content of bicomponent fibers of a given density in the material (in %) and on the mass content of oxidized polyacrylonitrile fibers of a given density in the material (in %); as well as a graph of the dependence of strength (breaking load along the length in N) on the mass content of bicomponent fibers of a given density in the material (in %) and on the mass content of oxidized polyacrylonitrile fibers of a given density in the material (in %). Fig. 2 shows the resulting structure of the claimed material.

[0010] A nonwoven, fire-resistant insulating material for forming the lining of a garment comprises a blend of polymer fibers thermally bonded into a web. As a non-limiting example, the fibers in the claimed insulating material are staple fibers 51 mm long. Another non-limiting example could be fibers 5-70 mm long. The fibers are bonded into the web (fabric) by thermal bonding, which is achieved by adding a binder in the form of a bicomponent fiber to the blend. The claimed material contains polymer fibers and a bicomponent fiber with a linear density of 0.22 tex, a core-shell type, and a concentric arrangement.As a non-limiting example, the shell polymer is selected from lower polyolefins (e.g., high-density polyethylene, polypropylene) or lower olefin copolymers (e.g., polyethylene copolymer or copolyethylene terephthalate) with a melting point of 110-180°C, while the core polymer is polyethylene terephthalate with a melting point of 230-270°C. Because the shell polymer has a melting point lower than that of the polyester fibers and the core polymer, the shell polymer, upon melting, bonds the fiber mixture and transforms it into a single web (mesh). The bicomponent fiber acts as a binder during thermal bonding. In the production of nonwoven materials, the binder is used both to form bonds between fibers and to redistribute loads between fibers, i.e., to ensure the coordinated operation of the fibrous elements under loads that cause deformation of the nonwoven material.As a non-limiting example, the core occupies an area of ​​50 to 95% of the total cross-sectional area of ​​the bicomponent fiber, and the cladding occupies an area of ​​5 to 50% of the total cross-sectional area of ​​the bicomponent fiber.

[0011] The polymer fibers consist of oxidized polyacrylonitrile fibers with a linear density of 0.17 tex. The polymer fiber blend, which constitutes the claimed material, contains 20 to 30% bicomponent fibers by weight (including the limiting values) and 70 to 80% oxidized polyacrylonitrile fibers (including the limiting values). In such a blend, the ratio of bicomponent fiber components to oxidized polyacrylonitrile fibers by weight ranges from 1 / 4 to 3 / 7, including the limiting values.

[0012] It was experimentally revealed and established that it is precisely with a mass content of 70-80% oxidized polyacrylonitrile fibers and 20-30% bicomponent fiber from the total mass of the material (i.e.when the ratio of the mass contents of the components of the bicomponent fibers to the oxidized polyacrylonitrile fibers by mass is from 1 / 4 to 3 / 7) in this specific mixture (with the specified mass content, with a specific linear density of 0.17 tex of polyacrylonitrile fibers, with a specific linear density of 0.22 tex of bicomponent fibers, with the specified thermal bonding into a web with additional thermal bonding of the outer sections of the material by hot calender rollers, with the specified design of the bicomponent fiber) the index of limited flame spread according to GOST ISO 14116 will be achieved while maintaining high strength of the insulating material (which is characterized by good integrity of the material, the absence of significant migration of insulation fibers and high tensile properties).

[0013] It has also been experimentally established and determined that it is precisely with a mass content of 70-80% oxidized polyacrylonitrile fibers and 20-30% bicomponent fiber from the total mass of the material in this particular mixture (with the specified mass content, with a specific linear density of 0.17 tex of polyacrylonitrile fibers, with a specific linear density of 0.22 tex of bicomponent fibers, with the specified thermal bonding into a web with additional thermal bonding of the outer sections of the material by hot calender rollers, with the specified design of the bicomponent fiber) that the highest total thermal resistance will be achieved (microscopic cells with air are formed) while maintaining high strength of the insulating material (which is characterized by good integrity of the material, the absence of significant migration of insulation fibers and high tensile properties).

[0014] Thus, it has been experimentally established that the stated specific described insulating material has both high fire resistance and total thermal resistance while maintaining its integrity (high strength).

[0015] Additionally, it was experimentally revealed that high fire resistance, total thermal resistance and strength are maintained while maintaining a mass unevenness of no more than 7%.

[0016] Experiments also revealed that the inclusion of low-density fibers (both bicomponent and oxidized polyacrylonitrile) in the blend creates small air-filled cells in the material's structure. This creates numerous small pores that are evenly distributed throughout the material and have the largest maximum filling volume (with fibers with a higher linear density, there would be fewer larger pores and a smaller total volume), which contributes to a significant increase in the material's overall thermal resistance. Experiments also revealed that oxidized polyacrylonitrile fibers with a linear density of 0.17 tex exhibit high fire resistance.

[0017] With a decrease in the content of oxidized polyacrylonitrile fibers in a specific fiber blend to less than 70% by weight (and a corresponding increase in the weight of bicomponent fibers to more than 30%), the 3rd index of limited flame spread according to GOST ISO 14116 will not be achieved, and a high total thermal resistance will not be achieved, although the material will be sufficiently strong (see Fig. 1). With an increase in the content of fire-resistant non-combustible fibers in the form of oxidized polyacrylonitrile fibers in a specific fiber blend to more than 80% by weight (and a corresponding decrease in the weight of bicomponent fibers to less than 20%), the strength and bondability of the material decrease sharply, the insulation fibers migrate in large quantities due to an insufficient number of bonds, the tensile properties decrease sharply and the material loses its integrity. The specified specific material with a higher content of oxidized polyacrylonitrile fibers (more

[0018] 80%) will not bond at all; it will be a combed fiber, not an insulator. With such a breach in the material's integrity, it is impossible to measure the flame spread index, thermal properties, and strength characteristics (see Fig. 1, to the left of 20% bicomponent fibers).

[0019] Therefore, it is the declared ratio of this specific fiber mixture and its structure in the declared material that will allow achieving both the 3rd index of limited flame spread (increased fire resistance of the insulating material), and the maximum total thermal resistance, while maintaining the integrity and absence of significant migration of the insulating fibers (maintaining the high strength of the insulating material).

[0020] It should be noted that selecting other linear densities of polyacrylonitrile and bicomponent fibers will result in a deterioration in the material's performance due to changes in the thermal bonding mechanism and fire-retardant properties. Therefore, the specified technical result is only achieved in a specific blend with a specific component density and mass content, with the specified thermal bonding into a web with additional thermal bonding of the outer sections of the material using hot calender rollers, and with the specified bicomponent fiber design.

[0021] GOST ISO 14116-2016, "Occupational safety standards system. Protective clothing and materials against heat and flame. Limited flame spread. Flame resistance requirements," establishes requirements and methods for assessing the flame-spread properties of materials, material assemblies, and special protective clothing (workwear). Workwear manufactured in accordance with this standard is designed to protect workers from accidental, short-term contact with small flames in the absence of a significant risk from other types of heat. The classification system applies to materials, material assemblies, and workwear tested in accordance with ISO 15025, Method A. This standard establishes technical requirements for workwear and its materials during design, production, and conformity assessment.

[0022] In this standard, a hole is defined as a break of at least 5 x 5 mm in size caused by melting, heating, or combustion of the test specimen. In this standard, the flame-limiting index is a number indicating that the material has flame-limiting properties in accordance with the established level.

[0023] Requirements corresponding to Limited Flame Spread Index 1: When the flame spreads on any of the specimens, the flame boundary or openings shall not reach the top or any of the vertical edges; none of the specimens shall produce burning residues; the residual glow shall not exceed 2 s (<2 s); the glow shall not spread from the charred surface to the intact area after the flame has been applied to the surface of the specimen in accordance with ISO 15025.

[0024] Requirements corresponding to Limited Flame Spread Index 2: when the flame spreads on any of the specimens, the flame limit shall not reach the top or any of the vertical edges; none of the specimens shall produce burning residues; the residual glow shall not exceed 2 s (<2 s); the glow shall not spread from the charred surface to the intact area after the flame has been applied to the surface of the specimen in accordance with ISO 15025; none of the specimens shall have holes (through) greater than 5 mm in size in any direction of the material used for flame protection.

[0025] Requirements corresponding to Limited Flame Spread Index 3: when the flame spreads on any of the specimens, the flame limit shall not reach the top or any of the vertical edges; none of the specimens shall produce burning residues; the residual glow shall not exceed 2 s (<2 s); the glow shall not spread from the charred part to the intact area after the flame has been applied to the surface of the specimen in accordance with ISO 15025; none of the specimens shall have holes larger than 5 mm in any direction of the material used for flame protection; the residual burning time of each specimen shall not exceed 2 s (<2 s). That is, the requirements corresponding to Limited Flame Spread Index 3 are the most stringent. Oxidized / reduced polyacrylonitrile fibers are flame-retardant, self-combusting fibers.Their high thermal characteristics are achieved by selecting the optimal linear density of fibers depending on other components of the material, their mass content, location, and bonding method.

[0026] The oxidation process of polyacrylonitrile (PAN) fibers is well known and can be accomplished by any method known to those skilled in the art. As one example, patent RU 2258104 Cl, issued August 10, 2005, describes the production of flame-resistant PAN fibers for textile applications, demonstrating the oxidation of these fibers by continuous, stepwise thermal action with heat removal.

[0027] A nonwoven, fire-resistant insulating material for a garment's lining is constructed in three layers: an upper (1), a lower (3), and an inner (2) (see Fig. 2). Upper (1) and lower (3) layers are stronger than the inner (2). Upper (1) and lower (3) layers are formed by additional thermal bonding of the outer sections of the material using hot calender rollers. Calendered layers (1 and 3) are produced by additional thermal bonding using a calender (hot rollers). The calendered layers provide additional fire resistance by preventing fiber migration from the surface of the material and by imparting integrity and structural strength to the material. The microcell size in the surface layers (calendered layers (1 and 3)) is smaller than in the main layer (2), further enhancing the overall thermal resistance of the material.The fibers in the calendered layer are arranged horizontally, just like in the main layer, and the calendered layer can have a thickness of 0.20 to 0.25 µm.

[0028] Unevenness in the mass of the sheet across its area, length, and width is no more than 7%. If the unevenness in mass exceeds 7%, unevenness in the properties of the insulating material occurs, resulting in a significant reduction in fire resistance, strength, and overall thermal resistance in areas where the mass is reduced.

[0029] The insulating material is a high-tech synthetic thermal insulation material developed from fine fibers with a low linear density and special fire-resistant properties. It provides superior thermal protection while maintaining light weight, effective breathability, softness, and volume. It retains warmth in high humidity, is easy to wash, and dries quickly, all while maintaining protective fire-resistant properties. Additionally, the insulating material boasts relatively high strength and bondability (due to thermal bonding with bicomponent fibers).

[0030] The material is given elasticity and flexibility also by thermally bonding the fibers and calendering the outer layers of the insulating material.

[0031] When sewing a garment, quilting can be done on standard quilting equipment. The recommended stitch spacing for through-quilting is 10 to 15 cm.

[0032] The thermal insulation properties of the material were determined using an MT-380 device using the total thermal resistance determination method in accordance with GOST 20489-75, which involves measuring the cooling time of the device plate in a specified range of temperature differences between the plate surface, the insulated material or package of materials, and the ambient air. The established size for the test samples is 360 x 500 mm. Testing of one sample is carried out on two test pieces, which are maintained in atmospheric conditions at a temperature of 20 (±2) °C and a relative air humidity of 60 (±2)%. Testing begins with determining the thickness of the nonwoven material using a thickness gauge at a pressure of 0.2 kPa at 10 points, then calculating the arithmetic mean of the measurement results. The sample is tucked with the front side facing the air flow with a tension sufficient to fix the sample. The actual values ​​​​of the surface density and thickness of the test sample are entered.The device automatically displays the total thermal resistance value R. cyM measured in m 2 °C / W.

[0033] Example 1 (comparative). The material in Example 1 is not the claimed material and contains 65% oxidized polyacrylonitrile fibers and 35% bicomponent fibers by weight. The linear density of the bicomponent fibers is 0.22 tex, and that of the oxidized polyacrylonitrile fibers is 0.17 tex. Test result according to GOST ISO 14116: the material meets index 2, but index 3 is not achieved. The total thermal resistance of the material is 0.48 m 2 °C / W. Breaking load by length / width: 18.6 / 41.2 N (Fig. 1).

[0034] Example 2. The material in example 2 is the claimed material and contains 70% oxidized polyacrylonitrile fibers and 30% bicomponent fibers by weight. The linear density of the bicomponent fibers is 0.22 tex, and that of the oxidized polyacrylonitrile fibers is 0.17 tex. Test result according to GOST ISO 14116: the material meets index 3, the material has the required index of limited flame spread (i.e., high fire resistance is ensured), as well as high thermal characteristics (a high total thermal resistance of 0.54 m is ensured). 2 °C / W), good tensile strength (tensile strength by length / width: 17.2 / 37.2 H) and has a relatively high strength of the insulating material

[0035] (Fig. 1).

[0036] Example 3. The material in example 3 is the claimed material and contains 80% oxidized polyacrylonitrile fibers and 20% bicomponent fibers by weight. The linear density of the bicomponent fibers is 0.22 tex, and that of the oxidized polyacrylonitrile fibers is 0.17 tex. Test result according to GOST ISO 14116: the material meets index 3, the material has the required index of limited flame spread (i.e., high fire resistance is ensured), as well as high thermal characteristics (a high total thermal resistance of 0.52 m is ensured). 2 °C / W), has the integrity of the insulating material (breaking load along the length / width: 8.3 / 21.8 N), see Fig. 1.

[0037] The presented examples confirm the cause-and-effect relationship between the essential features of the claimed material and the stated technical result. All features expressed in the claims of this utility model are essential, and each of these features contributes to both an increase in fire resistance and an increase in the overall thermal resistance of the material, as well as to the preservation of its integrity. However, these features cannot be separated or excluded (since doing so would restructure the entire bonding mechanism of the material and alter its structure and properties). Thus, the proposed non-woven fibrous fire-resistant insulating material for forming the lining layer of a garment simultaneously increases the fire resistance and overall thermal resistance of the insulating material while maintaining its integrity.

Claims

Utility model formula 1. A non-woven fire-resistant insulating material for forming a lining layer of a garment, comprising a mixture of polymer fibers combined into a fabric by thermal bonding, containing polymer fibers and bicomponent fibers of the core-shell type with a concentric arrangement, characterized in that the bicomponent fibers have a linear density of 0.22 tex, the polymer fibers include oxidized polyacrylonitrile fibers with a linear density of 0.17 tex, wherein said mixture contains, by weight %: bicomponent fibers 20-30 oxidized polyacrylonitrile fibers 70-80, Moreover, in such a mixture, the ratio of the content of the components of the bicomponent fibers to the oxidized polyacrylonitrile fibers by weight is from 1 / 4 to 3 / 7, and the material is structured in the form of three layers - upper, lower and inner, and the upper and lower layers have higher strength than the inner layer.

2. The material according to paragraph 1, characterized in that the upper and lower layers are formed by additional thermal bonding of the outer sections of the material with hot calender rollers.

3. The material according to paragraph 1, characterized in that the unevenness of the web weight is no more than 7%.