Method for producing retractable lining cloth
A production method and interlining technology, which are applied in the processing of textile materials, fabric rubbing/softening treatment, solvent treatment, etc., can solve the problems of lack of in-depth research on fabrics, only focusing on adhesion fastness, lack of interlining, etc., to achieve softness and smoothness. The effect of plump hand feeling, good wearing performance and high elasticity
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2015-03-25
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention relates to a production method of lining cloth. Background technique
[0002] With the improvement of people's living standards, on the one hand, people pay more and more attention to the comfort, durability, sportiness and personalization of clothing. The ever-changing fabrics come one after another, and people are increasingly favoring natural fiber fabrics, water-absorbent fabrics and elastic fabrics such as: Tencel, cotton, viscose, hemp, cupro, silk, nylon, modified polyester, spandex, cotton and Lycra Blending, etc., these fabrics are characterized by water absorption swelling, drying shrinkage, and large changes in size. Their relative positions will shift due to wetting-drying, which is the main reason for wrinkling and blistering at the bonding part of the interlining and the fabric. reason. Therefore, higher requirements are put forward for the shrinkage rate and followability of interlinings, and ordinary interlinings can no ...
Examples
Embodiment Construction
[0018] Base fabric made of PTT, PBT, PET fiber or core-spun yarn
[0019] (1) Desizing and relaxation
[0020] Add desizing aids into the high temperature and high pressure overflow dyeing machine, desizing aids include desizing agent TF-127, strong degreasing agent TF-129B, sodium hydroxide, refining agent TF-108, etc., among which desizing agent TF-127 -127 1.0-4.0 g / L, powerful degreasing agent TF-129B 0.5-3 g / L, sodium hydroxide 1-10 g / L, refining agent TF-108 0.5-6 g / L. Then raise the temperature to 70-130°C, keep it for 20-60 minutes, then cool down and wash with water, and then take out the cloth.
[0021] (2) Dyeing
[0022] Make the dye adhere or fix (enter) the inside of the fiber, so that the interlining can obtain uniform, firm and colorful colors, and ensure that it is the same as the sample. In order to maintain the good elasticity of the fiber, the dyeing continues in a relaxed state, using a high-temperature, high-pressure liquid jet dyeing machine or a high...