An additive for effectively inhibiting Zhundong coal slagging and pollution and its application method
An application method and additive technology, applied in fuel additives, solid fuels, petroleum industry, etc., can solve the problems of cumbersome steps and small particle size, and achieve the effects of simple composition, inhibition of volatilization, and easy acquisition.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2019-11-22
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 1
Abstract
Description
Technical field:
[0001] The invention relates to an additive and an application method thereof, in particular to an additive capable of effectively inhibiting slagging pollution caused by Zhundong high-sodium coal combustion and an application method thereof. Background technique:
[0002] Coal plays a pivotal role in China's energy consumption, especially in power generation. At present, many coal bases in the central or eastern regions, after years of mining and utilization, have shown a trend of exhaustion of coal resources. Therefore, the discovery of the Zhundong coalfield in Xinjiang is very important to my country's energy security because of its very rich reserves (forecast: 390 billion tons). Although Zhundong coal is a good thermal coal with low ash and sulfur content and high volatile matter content, serious ash accumulation and pollution problems have occurred during the combustion and utilization of boilers, which affects the economical and safe operation of bo...
Examples
Embodiment 1
[0019] Composition and mass percent content of the Zhundong coal additive that this example implements: kaolin (50%), quartz sand (25%), magnesite (15%) and zeolite (10%);
Embodiment 2
[0021] Composition and mass percent content of the Zhundong coal additive that this example implements: kaolin (55%), quartz sand (20%), magnesite (15%) and zeolite (10%);
Embodiment 3
[0023] The composition and mass percentage content of the Zhundong coal additive that this example implements: kaolin (60%), quartz sand (20%), magnesite (10%) and zeolite (10%);