Organic light emitting display device

By using an organic insulating structure to replace the bending protective layer and covering the touch screen electrode in a flexible OLED device, the problems of connecting electrode cutout and bond damage during bending are solved, reducing ineffective space and manufacturing costs, and improving the flexibility of the device.

CN110391276BActive Publication Date: 2024-11-01SAMSUNG DISPLAY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201910311809.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-04-18
Filing Date
2019-04-18
Publication Date
2024-11-01
Estimated Expiration
2039-04-18

AI Technical Summary

Technical Problem

The existing flexible OLED devices are prone to damage to bonding of the connecting electrode notches and covering windows when bending, and there is a large ineffective space, which increases manufacturing cost.

Method used

An organic insulating structure is used instead of the bending protective layer, positioned in the bending area to lift the neutral plane, and an organic insulating layer is provided on the display panel to cover the touch screen electrodes, reducing the thickness of the bending area and the length of the peripheral area.

Benefits of technology

The bonding breakage of the cutouts of the connecting electrodes and the covering window is avoided, and the ineffective space and manufacturing costs are reduced, while improving the flexibility of the OLED device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110391276B_ABST
    Figure CN110391276B_ABST
Patent Text Reader

Abstract

The present application relates to an organic light-emitting display device. The organic light-emitting display device includes a display panel and a touch screen. The display panel includes a display area, a pad area, and a bending area, wherein the display area includes a light-emitting area and a peripheral area surrounding the light-emitting area, the pad area is spaced apart from the display area, and the bending area is located between the display area and the pad area. The touch screen is positioned on the display panel and includes a plurality of touch screen electrodes and an organic insulating structure. The plurality of touch screen electrodes are located in the display area. The organic insulating structure is positioned to cover the plurality of touch screen electrodes in the display area and extends from the display area to the bending area and the pad area in a first direction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] One or more aspects of the disclosed embodiments relate to an organic light emitting display device. One or more embodiments of the inventive concept relate to a flexible organic light emitting display device. Background Art

[0002] Flat panel display ("FPD") devices are widely used as displays of electronic devices because they are lightweight and thin, for example, compared to cathode ray tube ("CRT") display devices. Examples of FPD devices include liquid crystal display ("LCD") devices and organic light emitting display ("OLED") devices.

[0003] Recently, a flexible OLED device including a lower substrate and an upper substrate having a flexible material and capable of bending and / or folding a portion of a display panel included in the OLED device has been developed. For example, the lower substrate included in the display panel may be formed of a flexible substrate, and the upper substrate included in the display panel may have a thin film encapsulation structure. In addition, the flexible OLED device may further include a bending protection layer, a polarizing layer, a touch screen electrode layer, and the like. Here, the bending protection layer may raise the neutral plane of the display panel in the portion where the display panel is bent, and the polarizing layer and the touch screen electrode layer may be provided on the display panel. The lower protective film may be provided (e.g., positioned) below the display panel. Summary of the invention

[0004] One or more aspects of the disclosed embodiments relate to an organic light emitting display ("OLED") device.

[0005] According to certain exemplary embodiments, an OLED device includes a display panel and a touch screen. The display panel includes a display area, a pad area, and a bending area, wherein the display area includes a light-emitting area and a peripheral area around the light-emitting area, the pad area is spaced apart from the display area, and the bending area is located between the display area and the pad area. The touch screen is positioned on the display panel and includes a plurality of touch screen electrodes and an organic insulating structure. The plurality of touch screen electrodes are located in the display area. The organic insulating structure covers the plurality of touch screen electrodes in the display area and extends from the display area to the bending area and the pad area in a first direction.

[0006] In an exemplary embodiment, the organic insulating structure may be continuous in a portion of the pad region, the display region, and the bending region on the display panel.

[0007] In an exemplary embodiment, the plurality of touch screen electrodes may include a plurality of first touch screen electrodes and a plurality of second touch screen electrodes. The plurality of first touch screen electrodes may extend in a first direction and a second direction opposite to the first direction, and may be spaced apart from each other in a third direction intersecting the first direction and the second direction. The plurality of second touch screen electrodes are on the plurality of first touch screen electrodes and may extend in the third direction. The plurality of second touch screen electrodes are spaced apart from each other in the second direction. The plurality of first touch screen electrodes may intersect the plurality of second touch screen electrodes, respectively.

[0008] In an exemplary embodiment, the organic insulating structure may include a first organic insulating layer and a second organic insulating layer. The first organic insulating layer may cover the plurality of first touch screen electrodes and may extend in the first direction. The second organic insulating layer may be located on the first organic insulating layer, may cover the plurality of second touch screen electrodes and may extend in the first direction.

[0009] In an exemplary embodiment, the organic insulating structure may further include a third organic insulating layer under the plurality of first touch screen electrodes and the first organic insulating layer.

[0010] In exemplary embodiments, the first organic insulating layer, the second organic insulating layer, and the third organic insulating layer may each independently be essentially composed of an organic material.

[0011] In example embodiments, the second organic insulating layer may have a first thickness in the light emitting region and may have a second thickness in the bending region, wherein the second thickness is greater than the first thickness.

[0012] In exemplary embodiments, the second thickness of the second organic insulating layer may allow a neutral plane of the display panel to be raised in the bending region.

[0013] In an exemplary embodiment, the plurality of touch screen electrodes may include a plurality of first touch screen electrodes, a plurality of second touch screen electrodes, and a plurality of connection patterns. The plurality of first touch screen electrodes may extend in a first direction and a second direction opposite to the first direction, and may be spaced apart from each other in a third direction intersecting the first direction and the second direction. The plurality of second touch screen electrodes may be located at the same level as the plurality of first touch screen electrodes, and may be spaced apart from each other in the first direction and the second direction, wherein each of the plurality of second touch screen electrodes is located between two adjacent first touch screen electrodes among the plurality of first touch screen electrodes. The plurality of connection patterns may be located at a different level from the first touch screen electrodes and the second touch screen electrodes, and may electrically connect two second touch screen electrodes adjacent in the third direction among the plurality of second touch screen electrodes.

[0014] In an exemplary embodiment, the organic insulating structure may include a first organic insulating layer and a second organic insulating layer. The first organic insulating layer may cover a plurality of first touch screen electrodes and a plurality of second touch screen electrodes and may extend in a first direction. The second organic insulating layer may be located on the first organic insulating layer, may cover a plurality of connection patterns and may extend in the first direction.

[0015] In an exemplary embodiment, the organic insulating structure may further include a third organic insulating layer under the plurality of first touch screen electrodes and the first organic insulating layer. The first organic insulating layer, the second organic insulating layer, and the third organic insulating layer may each be independently composed of an organic material in nature.

[0016] In an exemplary embodiment, the display panel may further include a substrate, a semiconductor element on the substrate, a light emitting structure in the light emitting region on the substrate, and a thin film encapsulation structure on the light emitting structure.

[0017] In an exemplary embodiment, the semiconductor element may include: an active layer located on a substrate; a gate insulating layer covering the active layer on the substrate and extending in a first direction; a gate electrode located on the active layer; an insulating intermediate layer covering the gate electrode on the gate insulating layer and extending in the first direction; and a source electrode and a drain electrode located on the gate electrode.

[0018] In example embodiments, the gate insulating layer may have a first opening exposing the upper surface of the substrate in the bent region, and the insulating interlayer may have a second opening exposing the upper surface of the substrate in the bent region.

[0019] In an exemplary embodiment, the light emitting structure may include a lower electrode, a light emitting layer located on the lower electrode, and an upper electrode located on the light emitting layer. The thin film encapsulation structure may include a first thin film encapsulation layer, a second thin film encapsulation layer, and a third thin film encapsulation layer. The first thin film encapsulation layer may include one or more inorganic materials having flexibility. The second thin film encapsulation layer may be located on the first thin film encapsulation layer and may include one or more organic materials having flexibility. The third thin film encapsulation layer may be located on the second thin film encapsulation layer and may include one or more inorganic materials having flexibility.

[0020] In an exemplary embodiment, the touch screen may be directly located on the thin film encapsulation structure.

[0021] In an exemplary embodiment, the OLED device may further include at least one connection electrode. The at least one connection electrode may be located between the organic insulating structure of the touch screen and the substrate, and may electrically connect the light emitting structure and an external device.

[0022] In an exemplary embodiment, the OLED device may further include a lower protective film on a lower surface of the display panel opposite to the touch screen, a polarizing layer on the touch screen, and a window substrate on the polarizing layer.

[0023] In an exemplary embodiment, the lower protective film may include a first lower protective film pattern in the display region and a second lower protective film pattern in the pad region, wherein the lower surface of the display panel in the bending region is exposed.

[0024] In an exemplary embodiment, when viewed in a fourth direction intersecting the first direction and the second direction and being orthogonal (e.g., vertical) to the upper surface of the substrate, the bending region may be bent around an axis extending along a third direction, wherein the third direction intersects the first direction, the second direction, and the fourth direction. When the bending region is bent, the second lower protective film pattern may be located on a lower surface of the first lower protective film pattern in the fourth direction.

[0025] Since the OLED device according to the exemplary embodiment includes an organic insulating structure included in the touch screen, the organic insulating structure can be positioned in the bending area and can be used instead of the bending protection layer of the comparative OLED device. That is, the organic insulating structure can be arranged (e.g., positioned) in the bending area so that the neutral plane in the bending area is positioned at the portion where the connecting electrode is provided. Therefore, even when the bending area is bent, the cutout of the connecting electrode may not appear in the bending area. In addition, since the bending protection layer is not provided, the adhesive breakage of the cover window may not occur. Since the length of the peripheral area is relatively reduced, the ineffective space (e.g., non-display area) of the OLED device can be relatively reduced. In addition, since there is no bending protection layer, the manufacturing cost of the OLED device can be relatively reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Further details of the exemplary embodiments can be understood from the following description taken in conjunction with the accompanying drawings, in which:

[0027] Figure 1 is a plan view showing an organic light emitting display ("OLED") device according to an exemplary embodiment;

[0028] Figure 2 is used to describe electrical connections to Figure 1 A block diagram of external devices of an OLED device;

[0029] Figure 3 It is along Figure 1 A cross-sectional view taken along line II';

[0030] Figure 4 is corresponding to Figure 3 an enlarged cross-sectional view of area "A";

[0031] Figure 5 It is used to describe the Figure 3 A plan view of a touch screen electrode in an OLED device;

[0032] Figure 6 It is shown that the Figure 3 A plan view of an example of a touch screen electrode in an OLED device;

[0033] Figure 7 Is used to describe Figure 1 A cross-sectional view of a curved shape of an OLED device;

[0034] Figures 8 to 12 is a cross-sectional view showing actions of a method of manufacturing an OLED device according to an exemplary embodiment;

[0035] Fig.13 is a cross-sectional view showing an OLED device according to an exemplary embodiment;

[0036] Fig.14 is a cross-sectional view showing an OLED device according to an exemplary embodiment;

[0037] Fig.15 is corresponding to Fig.14 an enlarged cross-sectional view of area "D" of FIG.

[0038] Fig.16 is a cross-sectional view showing an OLED device according to an exemplary embodiment. DETAILED DESCRIPTION

[0039] Hereinafter, embodiments of the present inventive concept will be described in more detail with reference to the accompanying drawings.

[0040] Figure 1 is a plan view showing an organic light emitting display ("OLED") device according to an exemplary embodiment, and Figure 2 is used to describe electrical connections to Figure 1 Block diagram of the external devices of an OLED device. Figure 3 It is along Figure 1 A cross-sectional view taken along line II'.

[0041] Reference Figure 1 , Figure 2 and Figure 3 , the OLED device 100 may include a display panel 200 having a plurality of light emitting structures 500, a touch screen 400, a polarizing layer 430, a lower protective film 300, a cover window 415, and a pad electrode 470, but is not limited thereto.

[0042] The display panel 200 may have a display region 10, a bending region 50, and a pad region 60. The pad region 60 may be spaced apart from the display region 10, and the bending region 50 may be located between the display region 10 and the pad region 60. The pad electrode 470 may be electrically connected (or electrically coupled) to the external device 101 and may be disposed in the pad region 60.

[0043] The display region 10 may include a light emitting region 30 that emits light and a peripheral region 40 that surrounds the light emitting region 30. In an exemplary embodiment, a light emitting structure 500 (eg, Figure 4 The light emitting structure 500 of the embodiment of the present invention may be disposed in the light emitting region 30, and a plurality of wirings may be disposed in the peripheral region 40. The wirings may electrically connect the pad electrode 470 and the light emitting structure 500. For example, the wirings may include data signal wirings, scan signal wirings, light emitting wirings, initialization signal wirings, power supply wirings, etc. In addition, a scan driver, a data driver, etc. may be disposed in the peripheral region 40. A portion of the peripheral region 40 (e.g., Figure 4 The peripheral area 40) may be inserted between the light emitting area 30 and the bending area 50.

[0044] In an exemplary embodiment, around Figure 1 The width of the peripheral region 40 of the light emitting region 30 may be the same along the entire peripheral region 40, but is not limited thereto. For example, the peripheral region 40 may include a first region extending in the third direction D3 (corresponding to the row direction in the plan view of the OLED device 100) and a second region extending in the first direction D1 or the second direction D2 (corresponding to the column direction in the plan view of the OLED device 100). In other words, the first region of the peripheral region 40 may be positioned adjacent to the bending region 50 and the top of the display panel 200 opposite to the bending region 50 (such as Figure 1 ), and the second area of ​​the peripheral area 40 may be positioned at both sides (sides) of the display panel 200 (eg, as shown in FIG. 2 ). Figure 1 ). In some embodiments, the width of the second region (in the row direction) may be smaller than the width of the first region (in the column direction). As the bending region 50 is bent, the pad region 60 may be positioned on the lower surface of the OLED device 100 (refer to Figure 7 ).

[0045] In some embodiments, the display area 10, the light emitting area 30, the bending area 50, and the pad area 60 may each be in a quadrangular planar shape, but are not limited thereto. For example, the display area 10, the light emitting area 30, the bending area 50, and the pad area 60 may each independently be in a triangular planar shape, a rhombus planar shape, a polygonal planar shape, a circular planar shape, a racetrack planar shape, and / or an elliptical planar shape.

[0046] In an exemplary embodiment, the OLED device 100 may further include a connection electrode (eg, Figure 4 The touch screen 400 may be disposed on the display panel 200 in a continuous manner in the light emitting region 30, the peripheral region 40 between the light emitting region 30 and the bending region 50, the bending region 50, and a portion of the pad region 60. In some embodiments, the touch screen 400 may be disposed directly on the display panel 200. The connecting electrode may be disposed between the touch screen 400 and the substrate ( Figure 4 The substrate 110 of the OLED device 100 is disposed between the substrate 110 of the OLED device 100, and the wiring and the pad electrode 470 may be electrically connected. The light emitting structure 500 disposed in the light emitting area 30 and the external device 101 electrically connected to the pad electrode 470 may be electrically connected through the connection electrode disposed in the bending area 50 and the wiring disposed in the peripheral area 40. The external device 101 may be electrically connected to the OLED device 100 through a flexible printed circuit board (FPCB). The external device 101 may provide a data signal, a scan signal, a light emitting signal, a power supply voltage, a touch sensing voltage, etc. to the OLED device 100. In some embodiments, the driver integrated circuit may be mounted in (e.g., loaded in) the FPCB. In some exemplary embodiments, the driver integrated circuit may be mounted in the pad area 60 of the display panel 200 and positioned adjacent to the pad electrode 470.

[0047] The polarizing layer 430 may be disposed on the touch screen 400 in the display region 10. The polarizing layer 430 may block or reduce external light incident from the outside on the display panel 200. In an exemplary embodiment, the polarizing layer 430 may have a relatively small thickness.

[0048] The cover window 415 may be disposed on the polarizing layer 430. The cover window 415 may protect the polarizing layer 430, the touch screen 400, and the display panel 200.

[0049] The lower protective film 300 may be disposed on a lower surface of the display panel 200 (opposite to a surface of the display panel 200 adjacent to the touch screen 400), and may protect the display panel 200. In an exemplary embodiment, the lower protective film 300 may include a first lower protective film pattern 351 and a second lower protective film pattern 352. The first lower protective film pattern 351 may be disposed in the display region 10. The second lower protective film pattern 352 may be disposed in the pad region 60, and may be spaced apart from the first lower protective film pattern 351. For example, the lower protective film 300 may expose a portion of the lower surface of the display panel 200 located in the bending region 50.

[0050] Figure 4 is corresponding to Figure 3 an enlarged cross-sectional view of area "A" of Figure 5 It is used to describe the Figure 3 A plan view of touch screen electrodes in an OLED device. Figure 6 It is shown that the Figure 3 A plan view of an example of a touch screen electrode in an OLED device.

[0051] Reference Figure 4 , the OLED device 100 may include a display panel 200 (refer to Figure 3 ), touch screen 400, polarizing layer 430, cover window 415 and lower protective film 300, but not limited thereto. Display panel 200 may include substrate 110, buffer layer 115, semiconductor element 250, light emitting structure 500, fan-out wiring 1300, conductive pattern 460, first planarization layer 270, second planarization layer 275, connection electrode 330, wiring pattern 215, connection pattern 235, pixel defining layer 310 and thin film encapsulation (TFE) structure 450, but not limited thereto. Semiconductor element 250 may include active layer 130, gate insulating layer 150, first gate electrode 170, first insulating interlayer 190, second gate electrode 175, second insulating interlayer 195, source electrode 210 and drain electrode 230. In some embodiments, conductive pattern 460 may include first conductive pattern 401 and second conductive pattern 402, and fan-out wiring 1300 may include first fan-out wiring 301 and second fan-out wiring 302. The light emitting structure 500 may include a lower electrode 290, a light emitting layer 335, and an upper electrode 340. The TFE structure 450 may include first, second, and third TFE layers 451, 452, and 453, and the lower protective film 300 may include first and second lower protective film patterns 351 and 352.

[0052] In an exemplary embodiment, the touch screen 400 may include a touch screen electrode 380 and an organic insulating structure 390. The touch screen electrode 380 may include a first touch screen electrode 382 and a second touch screen electrode 384, and the organic insulating structure 390 may include a first organic insulating layer 392 and a second organic insulating layer 394.

[0053] In the present embodiment, the OLED device 100 including the substrate 110 and the TFE structure 450 both having flexibility may be bent on an axis relative to the third direction D3, and the OLED device 100 may be used as a flexible OLED device having a shape in which the bending region 50 is bent.

[0054] The substrate 110 may include a transparent and / or opaque insulating material. For example, the substrate 110 may include a flexible transparent resin substrate. In an exemplary embodiment, the substrate 110 may have a configuration in which a first organic layer, a first barrier layer, a second organic layer, and a second barrier layer are sequentially stacked. The first barrier layer and the second barrier layer may each independently include an inorganic material such as silicon oxide, and may block or reduce moisture and / or water that may penetrate through the first organic layer and the second organic layer. In certain embodiments, each of the first organic layer and the second organic layer may include an organic material such as a polyimide-based resin.

[0055] Since the substrate 110 is relatively thin and flexible, the substrate 110 may be disposed on a rigid glass substrate to help support the formation of the semiconductor element 250 and the light emitting structure 500. In certain embodiments, during the manufacture of the OLED device 100, after the buffer layer 115 is disposed on the second barrier layer of the substrate 110, the semiconductor element 250 and the light emitting structure 500 may be disposed on the buffer layer 115. After the semiconductor element 250 and the light emitting structure 500 are formed on the buffer layer 115, the rigid glass substrate on which the substrate 110 is disposed may be removed. In other words, since it may be difficult to directly form the semiconductor element 250 and the light emitting structure 500 on the relatively thin and flexible substrate 110, the semiconductor element 250 and the light emitting structure 500 may be formed on the substrate 110 and the rigid glass substrate, and then the rigid glass substrate may be removed, thereby leaving the substrate 110 including the first organic layer, the first barrier layer, the second organic layer, and the second barrier layer to serve as the substrate 110 of the OLED device 100.

[0056] In which the display panel 200 includes a display area 10 having a light emitting area 30 and a peripheral area 40, a bending area 50 and a pad area 60 (eg, Figure 4 In the embodiment shown in FIG. 1 , the substrate 110 may be divided into a light emitting region 30, a peripheral region 40 (for example, the peripheral region 40 interposed between the light emitting region 30 and the bending region 50), a bending region 50, and a pad region 60 (refer to FIG. 1 ). Figure 1).

[0057] In certain embodiments, the substrate 110 may include a quartz substrate, a synthetic quartz substrate, a calcium fluoride substrate, a fluoride-doped quartz substrate, a soda-lime glass substrate, a non-alkaline glass substrate, or the like.

[0058] In an exemplary embodiment, the substrate 110 includes four layers, but is not limited thereto. For example, in some exemplary embodiments, the substrate 110 may include a single layer or a plurality of layers.

[0059] The buffer layer 115 may be disposed on the substrate 110. In an exemplary embodiment, the buffer layer 115 may be completely disposed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the substrate 110, and may have a first opening that exposes a portion of the upper surface of the substrate 110 located in the bending region 50. The buffer layer 115 may prevent or reduce the diffusion of metal atoms and / or impurities from the substrate 110 into the semiconductor element 250. In addition, the buffer layer 115 may control the thermal conductivity in the crystallization process for forming the active layer 130, thereby obtaining a substantially uniform active layer 130. In addition, when the surface of the substrate 110 is relatively irregular, the buffer layer 115 may improve the surface flatness of the substrate 110. Depending on the type (or kind) of the substrate 110, at least two buffer layers 115 may be disposed on the substrate 110, or no buffer layer may be disposed. The buffer layer 115 may include a silicon compound, a metal oxide, or the like. For example, the buffer layer 115 may include silicon oxide (SiO x ), silicon nitride (SiN x ), silicon oxynitride (SiO x N y ), silicon carbide oxide (SiO x C y ), Silicon Carbon Nitride (SiC x N y ), aluminum oxide (AlO x ), aluminum nitride (AlN x ), tantalum oxide (TaO x ), hafnium oxide (HfO x ), zirconium oxide (ZrO x ), titanium oxide (TiO x )wait.

[0060] The active layer 130 may be disposed in the light emitting region 30 on the buffer layer 115. The active layer 130 may include an oxide semiconductor, an inorganic semiconductor (eg, amorphous silicon, polycrystalline silicon, etc.), an organic semiconductor, or the like.

[0061] The gate insulating layer 150 may be disposed on the active layer 130. The gate insulating layer 150 may cover the active layer 130 in the light emitting region 30 on the buffer layer 115, and may extend from the light emitting region 30 to the pad region 60 in the first direction D1. For example, the gate insulating layer 150 may sufficiently (or appropriately) cover the active layer 130 on the buffer layer 115, and may have a substantially flat upper surface without generating a step portion around the active layer 130. In certain embodiments, the gate insulating layer 150 may cover the active layer 130 on the buffer layer 115, and may have a substantially uniform thickness along the contour of the active layer 130. In an exemplary embodiment, the gate insulating layer 150 may be disposed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the buffer layer 115, and may have a second opening exposing a portion of the upper surface of the substrate 110 located in the bending region 50. The gate insulating layer 150 may include a silicon compound, a metal oxide, or the like.

[0062] The first gate electrode 170 may be disposed in the light emitting region 30 on the gate insulating layer 150. The first gate electrode 170 may be disposed on a portion of the gate insulating layer 150 under which the active layer 130 is positioned. The first gate electrode 170 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. For example, the first gate electrode 170 may include gold (Au), silver (Ag), aluminum (Al), platinum (Pt), nickel (Ni), titanium (Ti), palladium (Pd), magnesium (Mg), calcium (Ca), lithium (Li), chromium (Cr), tantalum (Ta), tungsten (W), copper (Cu), molybdenum (Mo), scandium (Sc), neodymium (Nd), iridium (Ir), aluminum alloy, aluminum nitride (AlN x ), silver alloy, tungsten nitride (WN x ), copper alloy, molybdenum alloy, titanium nitride (TiN x ), chromium nitride (CrN x ), tantalum nitride (TaN x ), strontium ruthenium oxide (SRO), zinc oxide (ZnO x ), indium tin oxide (ITO), tin oxide (SnO x ), indium oxide (InO x ), gallium oxide (GaO x ), indium zinc oxide (IZO), etc. These materials may be used alone or in appropriate combination thereof. In certain exemplary embodiments, the first gate electrode 170 may have a multi-layer structure including a plurality of layers.

[0063] The fan-out wiring 1300 may be disposed on the gate insulating layer 150 in the peripheral region 40 and the pad region 60 located adjacent to the bending region 50 (and on both sides of the bending region 50). As described above, the fan-out wiring 1300 may include a first fan-out wiring 301 and a second fan-out wiring 302. The first fan-out wiring 301 may extend along the second direction D2 in the peripheral region 40 on the gate insulating layer 150, and may be electrically connected to the light emitting structure 500 disposed in the light emitting region 30. The second fan-out wiring 302 may extend along the first direction D1 in the pad region 60 on the gate insulating layer 150, and may be electrically connected to the external device 101 (e.g., refer to FIG. 1 ) through the pad electrode 470 disposed in the pad region 60. Figure 1 and Figure 2 ). The fan-out wiring 1300 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. In an exemplary embodiment, the fan-out wiring 1300 and the first gate electrode 170 may be located at the same layer (e.g., at the same level) and may be formed simultaneously (or at the same time) using the same material. In some embodiments, the fan-out wiring 1300 and the second gate electrode 175 may be located at the same layer (e.g., at the same level). These may be used alone or in appropriate combination thereof. In some exemplary embodiments, the fan-out wiring 1300 may have a multilayer structure including a plurality of layers.

[0064] The first insulating interlayer 190 may be disposed on the first gate electrode 170. The first insulating interlayer 190 may cover the first gate electrode 170 in the light emitting region 30 on the gate insulating layer 150, and may extend in the first direction D1. In addition, the first insulating interlayer 190 may cover the first fan-out wiring 301 in the peripheral region 40 on the gate insulating layer 150 and cover the second fan-out wiring 302 in the pad region 60. For example, the first insulating interlayer 190 may fully (or appropriately) cover the first gate electrode 170, the first fan-out wiring 301, and the second fan-out wiring 302 on the gate insulating layer 150, and may have a substantially flat upper surface without generating a step portion around the first gate electrode 170, the first fan-out wiring 301, and / or the second fan-out wiring 302. In some embodiments, the first insulating interlayer 190 may cover the first gate electrode 170, the first fan-out wiring 301 and the second fan-out wiring 302 on the gate insulating layer 150, and may be provided to have a substantially uniform thickness along the contours of the first gate electrode 170, the first fan-out wiring 301 and the second fan-out wiring 302. In an exemplary embodiment, the first insulating interlayer 190 may be provided in the light emitting region 30, the peripheral region 40 and the pad region 60 on the gate insulating layer 150, and may have a third opening exposing a portion of the upper surface of the substrate 110 located in the bending region 50. The first insulating interlayer 190 may include a silicon compound, a metal oxide, or the like.

[0065] The second gate electrode 175 may be disposed in the light emitting region 30 on the first insulating interlayer 190. The second gate electrode 175 may be disposed on a portion of the first insulating interlayer 190 under which the first gate electrode 170 is positioned. In some embodiments, the first gate electrode 170 and the second gate electrode 175 may act as a storage capacitor. The second gate electrode 175 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In some exemplary embodiments, the second gate electrode 175 may have a multilayer structure including a plurality of layers.

[0066] The second insulating interlayer 195 may be disposed on the second gate electrode 175. The second insulating interlayer 195 may cover the second gate electrode 175 in the light emitting region 30 on the first insulating interlayer 190, and may extend in the first direction D1. For example, the second insulating interlayer 195 may fully (or appropriately) cover the second gate electrode 175 on the first insulating interlayer 190, and may have a substantially flat upper surface without generating a step portion around the second gate electrode 175. In some embodiments, the second insulating interlayer 195 may cover the second gate electrode 175 on the first insulating interlayer 190, and may be disposed to have a substantially uniform thickness along the contour of the second gate electrode 175. In an exemplary embodiment, the second insulating interlayer 195 may be disposed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the first insulating interlayer 190, and may have a fourth opening that exposes a portion of the upper surface of the substrate 110 positioned in the bending region 50. Here, the first to fourth openings may overlap each other. The second insulating interlayer 195 may include a silicon compound, a metal oxide, and the like.

[0067] The source electrode 210 and the drain electrode 230 may be disposed in the light emitting region 30 on the second insulating interlayer 195. The source electrode 210 may be in direct contact with the source region of the active layer 130 via a contact hole formed by removing a portion of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195. The drain electrode 230 may be in direct contact with the drain region of the active layer 130 via a contact hole formed by removing another portion of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195. The source electrode 210 and the drain electrode 230 may each independently include a metal, an alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, and the like. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the source electrode 210 and the drain electrode 230 may each independently have a multilayer structure including a plurality of layers. Thus, a semiconductor element 250 including an active layer 130 , a gate insulating layer 150 , a first gate electrode 170 , a first insulating interlayer 190 , a second gate electrode 175 , a second insulating interlayer 195 , a source electrode 210 , and a drain electrode 230 may be constructed (eg, formed).

[0068] In an exemplary embodiment, the semiconductor element 250 has a top gate structure, but is not limited thereto. For example, in some exemplary embodiments, the semiconductor element 250 may have a bottom gate structure.

[0069] In an exemplary embodiment, the OLED device 100 includes one semiconductor element 250, but is not limited thereto. For example, in some exemplary embodiments, the OLED device 100 may include at least one semiconductor element 250 and at least one storage capacitor.

[0070] The conductive pattern 460 may be disposed in the peripheral region 40 and the pad region 60 located adjacent to the bending region 50 on the second insulating interlayer 195. As described above, the conductive pattern 460 may include a first conductive pattern 401 and a second conductive pattern 402. The first conductive pattern 401 may be in direct contact with the first fan-out wiring 301 via a first contact hole in the peripheral region 40, wherein the first contact hole is formed by removing a first portion of the first insulating interlayer 190 and the second insulating interlayer 195, and the second conductive pattern 402 may be in direct contact with the second fan-out wiring 302 via a second contact hole in the pad region 60, wherein the second contact hole is formed by removing a second portion of the first insulating interlayer 190 and the second insulating interlayer 195. In an exemplary embodiment, the conductive pattern 460, the source electrode 210, and the drain electrode 230 may be located at the same layer (e.g., at the same level), and may be formed simultaneously (or at the same time) using the same material. In some embodiments, the conductive pattern 460 and the second gate electrode 175 may be located at the same layer (e.g., at the same level). The conductive pattern 460 may include metal, metal alloy, metal nitride, conductive metal oxide, transparent conductive material, etc. These may be used alone or in appropriate combination thereof. In some exemplary embodiments, the conductive pattern 460 may have a multilayer structure including a plurality of layers.

[0071] The first planarization layer 270 may be disposed on the second insulating interlayer 195, the source electrode 210, the drain electrode 230, and the conductive pattern 460. The first planarization layer 270 may cover the source electrode 210 and the drain electrode 230 in the light emitting region 30 on the second insulating interlayer 195, and may cover the conductive pattern 460 in the peripheral region 40 and the pad region 60 on the second insulating interlayer 195. In an exemplary embodiment, the first planarization layer 270 may be in direct contact with the following portions: the lower surface of the connection electrode 330; the sidewalls (e.g., the sidewalls of the first to fourth openings) of each of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195 located adjacent to the bending region 50; and the portion of the upper surface of the substrate 110 located in the bending region 50. In some embodiments, the first planarization layer 270 may completely (e.g., entirely) cover the conductive pattern 460. In other words, the first planarization layer 270 may be disposed below the connection electrode 330 in a portion of the peripheral region 40, the bending region 50, and a portion of the pad region 60 on the substrate 110, or may be disposed between the connection electrode 330 and the substrate 110. In some embodiments, the first planarization layer 270 may be entirely disposed in the light emitting region 30, the peripheral region 40, the bending region 50, and the pad region 60 on the substrate 110.

[0072] For example, the first planarization layer 270 may be configured to have a relatively large thickness. In this case, the first planarization layer 270 may have a substantially flat upper surface, and a planarization process may be further performed on the first planarization layer 270 to achieve a flat upper surface of the first planarization layer 270. In some embodiments, the first planarization layer 270 may cover the source electrode 210 and the drain electrode 230, the second insulating interlayer 195, and the sidewalls of the first opening to the fourth opening, and may be configured to have a substantially uniform thickness along the profile of the source electrode 210 and the drain electrode 230, the second insulating interlayer 195, and the sidewalls of the first opening to the fourth opening. The first planarization layer 270 may include an organic material and / or an inorganic material. In an exemplary embodiment, the first planarization layer 270 may include an organic material.

[0073] The wiring pattern 215 and the connection pattern 235 may be disposed in the light emitting region 30 on the first planarization layer 270. Scan signals, data signals, light emitting signals, initialization signals, power supply voltages, etc. may be transmitted through the wiring pattern 215. The connection pattern 235 may be spaced apart from the wiring pattern 215 in the light emitting region 30 on the first planarization layer 270. The connection pattern 235 may contact the drain electrode 230 via a contact hole formed by removing a portion of the first planarization layer 270 positioned in the light emitting region 30, and the lower electrode 290 and the drain electrode 230 may be electrically connected. The wiring pattern 215 and the connection pattern 235 may each independently include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the wiring pattern 215 and the connection pattern 235 may each independently have a multilayer structure including a plurality of layers.

[0074] The connection electrode 330 may be disposed in a portion of the peripheral region 40, the bending region 50, and a portion of the pad region 60 on the first planarization layer 270. The connection electrode 330 may be in direct contact with the conductive pattern 460, and may be electrically connected to the fan-out wiring 1300. For example, the first planarization layer 270 may include a first contact hole in the peripheral region 40 and a second contact hole in the pad region 60. Here, the first contact hole of the first planarization layer 270 may expose a portion of the first conductive pattern 401, and the second contact hole of the first planarization layer 270 may expose a portion of the second conductive pattern 402. The connection electrode 330 may be in direct contact with the first conductive pattern 401 via the first contact hole in the peripheral region 40 of the first planarization layer 270, and may be in direct contact with the second conductive pattern 402 via the second contact hole in the pad region 60 of the first planarization layer 270. Since the connection electrode 330 electrically connects the first fan-out wiring 301 and the second fan-out wiring 302 through the conductive pattern 460, the scan signal, data signal, light-emitting signal, initialization signal, power supply voltage, etc. provided from the external device 101 can be applied to the light-emitting structure 500. In an exemplary embodiment, the connection electrode 330, the wiring pattern 215 and the connection pattern 235 may be located at the same layer (for example, at the same level), and may be formed at the same time (or at the same time) using the same material. The connection electrode 330 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the connection electrode 330 may have a multilayer structure including a plurality of layers.

[0075] The second planarization layer 275 may be disposed on the wiring pattern 215, the connection pattern 235, the connection electrode 330, and the first planarization layer 270. The second planarization layer 275 may cover the wiring pattern 215 and the connection pattern 235 in the light emitting region 30 on the first planarization layer 270 and extend in the first direction D1, and may cover the connection electrode 330 in the peripheral region 40, the bending region 50, and the pad region 60. In other words, the second planarization layer 275 may be disposed on (or above) the entire (or substantially the entire) substrate 110.

[0076] In some embodiments, the OLED device 100 may further include a blocking region extending along the third direction D3 in a portion of the peripheral region 40 positioned between the light emitting region 30 and the bending region 50 (see FIG. 1 ). Figure 1). The blocking region may be positioned parallel to the bending region 50, wherein the first planarization layer 270, the second planarization layer 275, and the pixel defining layer 310 may not be disposed in the blocking region. For example, the first planarization layer 270, the second planarization layer 275, and the pixel defining layer 310 may not be disposed in the blocking region, so that the blocking region can block (or reduce) water and / or moisture that may penetrate into the light emitting region 30 through the first planarization layer 270 and the second planarization layer 275 disposed in the pad region 60 and / or the bending region 50.

[0077] The second planarization layer 275 may be provided to have a large thickness to sufficiently (properly) cover the wiring pattern 215, the connection pattern 235, and the connection electrode 330. In this case, the second planarization layer 275 may have a substantially flat upper surface, and a planarization process may be further performed on the second planarization layer 275 to achieve a flat upper surface of the second planarization layer 275. In certain embodiments, the second planarization layer 275 may cover the wiring pattern 215, the connection pattern 235, and the connection electrode 330, and may be provided to have a substantially uniform thickness along the contours of the wiring pattern 215, the connection pattern 235, and the connection electrode 330. The second planarization layer 275 may include an organic material and / or an inorganic material. In an exemplary embodiment, the second planarization layer 275 may include an organic material.

[0078] The lower electrode 290 may be disposed in the light emitting region 30 on the second planarization layer 275. The lower electrode 290 may contact the connection pattern 235 via a contact hole formed by removing a portion of the second planarization layer 275. In some embodiments, the lower electrode 290 may be electrically connected to the semiconductor element 250. The lower electrode 290 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In some exemplary embodiments, the lower electrode 290 may have a multilayer structure including a plurality of layers.

[0079] The pixel defining layer 310 may be disposed in the light emitting region 30 on the second planarization layer 275, and may expose a portion of the lower electrode 290. For example, the pixel defining layer 310 may extend in the first direction D1, may cover both sides of the lower electrode 290, and may be disposed in the peripheral region 40, the bending region 50, and the pad region 60. In some embodiments, the pixel defining layer 310 may be disposed only in the light emitting region 30, and may not be disposed in the peripheral region 40, the bending region 50, or the pad region 60. The pixel defining layer 310 may include an organic material and / or an inorganic material. In an exemplary embodiment, the pixel defining layer 310 may include an organic material.

[0080] The light emitting layer 335 may be disposed on the portion of the lower electrode 290 exposed by the pixel defining layer 310. The light emitting layer 335 may be formed using at least one of the appropriate light emitting materials capable of generating light of different colors (e.g., red light, blue light, and / or green light, etc.) according to the sub-pixel. In some embodiments, the light emitting layer 335 may generate white light by stacking a plurality of light emitting materials capable of generating light of different colors (such as red light, green light, blue light, etc.). In this case, a color filter may be disposed on the light emitting layer 335. The color filter may include at least one selected from a red color filter, a green color filter, and a blue color filter. In some embodiments, the color filter may include a yellow color filter, a cyan color filter, and / or a magenta color filter. The color filter may include a photosensitive resin, a color photoresist, and the like.

[0081] The upper electrode 340 may be disposed in the light emitting region 30 on the pixel defining layer 310 and the light emitting layer 335. The upper electrode 340 may include a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the upper electrode 340 may have a multilayer structure including a plurality of layers. Thus, a light emitting structure 500 including a lower electrode 290, a light emitting layer 335, and an upper electrode 340 may be constructed (e.g., formed).

[0082] The first TFE layer 451 may be disposed in the light emitting region 30 on the upper electrode 340. The first TFE layer 451 may cover the upper electrode 340 and may be disposed to have a substantially uniform thickness along the contour of the upper electrode 340. The first TFE layer 451 may prevent or reduce degradation of the light emitting structure 500 due to penetration of moisture, water, oxygen, etc. In addition, the first TFE layer 451 may protect the light emitting structure 500 from external impact. The first TFE layer 451 may include an inorganic material having flexibility.

[0083] The second TFE layer 452 may be disposed on the first TFE layer 451. The second TFE layer 452 may improve the flatness of the OLED device 100 and may protect the light emitting structure 500. The second TFE layer 452 may include an organic material having flexibility.

[0084] The third TFE layer 453 may be disposed on the second TFE layer 452. The third TFE layer 453 may cover the second TFE layer 452 and may be disposed to have a substantially uniform thickness along the contour of the second TFE layer 452. The third TFE layer 453 may prevent or reduce the degradation of the light emitting structure 500 due to the penetration of moisture, water, oxygen, etc. together with the first TFE layer 451 and the second TFE layer 452. In addition, the third TFE layer 453 may protect the light emitting structure 500 from external impacts together with the first TFE layer 451 and the second TFE layer 452. The third TFE layer 453 may include an inorganic material having flexibility. Thus, a TFE structure 450 including the first TFE layer 451, the second TFE layer 452 and the third TFE layer 453 may be constituted (e.g., formed). In some embodiments, the display panel 200 may include a substrate 110, a buffer layer 115, a semiconductor element 250, a light emitting structure 500, a fan-out wiring 1300, a conductive pattern 460, a first planarization layer 270, a second planarization layer 275, a connecting electrode 330, a wiring pattern 215, a connecting pattern 235, a pixel defining layer 310 and a TFE structure 450, but is not limited thereto.

[0085] In certain embodiments, the TFE structure 450 may have five layers in which the first to fifth TFE layers are stacked, or may have seven layers in which the first to seventh TFE layers are stacked.

[0086] The first touch screen electrode 382 may be disposed on the third TFE layer 453. In an exemplary embodiment, the first touch screen electrode 382 may be directly disposed on the third TFE layer 453.

[0087] like Figure 5 As shown in FIG. 1 , the OLED device 100 may include a plurality of first touch screen electrodes 382 (eg, Figure 4 1 and 2. One of the first touch screen electrodes 382 is shown in FIG. 1 . The first touch screen electrodes 382 may extend in a second direction D2 (or a first direction D1) parallel to an upper surface of the OLED device 100, and may be spaced apart from each other in a third direction D3. A first touch sensing voltage may be applied to the first touch screen electrodes 382. For example, the first touch screen electrodes 382 may include carbon nanotubes (CNTs), transparent conductive oxides (TCOs), ITOs, indium gallium zinc oxides (IGZOs), ZnO x , graphene, silver nanowire (AgNW), Cu, Cr, etc.

[0088] Refer again Figure 4 and Figure 5, the first organic insulating layer 392 may be disposed on the first touch screen electrode 382. The first organic insulating layer 392 may cover the first touch screen electrode 382 in the light emitting region 30, and may extend in the first direction D1. In an exemplary embodiment, the first organic insulating layer 392 may be disposed in the bending region 50 on the display panel 200. In some embodiments, the first organic insulating layer 392 may be continuously disposed in the display region 10, the bending region 50, and a portion of the pad region 60 on the display panel 200. For example, the first organic insulating layer 392 may fully (or appropriately) cover the first touch screen electrode 382 in the light emitting region 30 on the third TFE layer 453, and may have a substantially flat upper surface without generating a step portion around the first touch screen electrode 382. In some embodiments, the first organic insulating layer 392 may extend in the first direction D1, and may be disposed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the pixel defining layer 310. The first organic insulating layer 392 may include photoresist, acrylic fiber-based resin, polyimide-based resin, polyamide-based resin, siloxane-based resin, acrylic-based resin and / or epoxy-based resin. In some embodiments, the first organic insulating layer 392 may include polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polypropylene (PP), polycarbonate (PC), polystyrene (PS), polysulfone (PSul), polyethylene (PE), polyphthalamide (PPA), polyethersulfone (PES), polyarylate (PAR), polycarbonate oxide (PCO), modified polyphenylene oxide (MPPO), etc. In an exemplary embodiment, the first organic insulating layer 392 may be essentially composed of an organic material.

[0089] The second touch screen electrode 384 may be disposed on the first organic insulating layer 392. Figure 5 As shown in FIG. 1 , the OLED device 100 may include a plurality of second touch screen electrodes 384 (eg, Figure 4 1 and 2. In the embodiment of the present invention, one of the plurality of second touch screen electrodes 384 is shown in FIG. 1 . The second touch screen electrodes 384 may extend in a third direction D3 that intersects (e.g., is perpendicular to) the second direction D2, and may be spaced apart from each other in the second direction D2 (or the first direction D1). Here, the first touch screen electrode 382 may intersect the second touch screen electrode 384, and each of the first touch screen electrode 382 and the second touch screen electrode 384 may have a planar shape of a strip. A second touch sensing voltage may be applied to the second touch screen electrode 384.

[0090] The OLED device 100 can connect the touch screen electrodes 380 and the external device 101 (see Figure 2), and the first touch sensing voltage and the second touch sensing voltage generated by the external device 101 may be provided to the first touch screen electrode 382 and the second touch screen electrode 384, respectively. The external device 101 may sense (or detect) the changed capacitance between the first touch screen electrode 382 and the second touch screen electrode 384. For example, the first touch sensing voltage as a sensing input signal generated by the external device 101 may be applied to the first touch screen electrode 382, ​​and the second touch sensing voltage as a sensing output signal may be output (or provided) to the external device 101 through the second touch screen electrode 384. In some embodiments, the first touch sensing voltage may have a periodically changing voltage level, and the second touch sensing voltage may have a DC voltage level.

[0091] For example, when the user of the OLED device 100 contacts the upper surface of the OLED device 100 (e.g., the upper surface of the cover window 415), the capacitance of the first touch screen electrode 382 and the second touch screen electrode 384 corresponding to the contact surface may change. A capacitance change may be generated between the portion of the body connected to the upper surface of the OLED device 100 and the first touch screen electrode 382 and the second touch screen electrode 384, and a sensing output signal changed by the changed capacitance may be output to the external device 101 through the touch sensor wiring. The external device 101 may detect the changed sensing output signal. In other words, the OLED device 100 may detect the contact position of the user by using the first touch sensing voltage and the second touch sensing voltage. After the user's contact with the OLED device 100 ends, the external device 101 may provide the first touch sensing voltage and the second touch sensing voltage to the first touch screen electrode 382 and the second touch screen electrode 384, respectively.

[0092] The second touch screen electrode 384 may include CNT, TCO, ITO, IGZO, ZnO x , graphene, AgNW, Cu, Cr, etc. In some embodiments, the first touch screen electrode 382 and the second touch screen electrode 384 can be formed using the same material. Thus, the touch screen electrode 380 including the first touch screen electrode 382 and the second touch screen electrode 384 can be constructed (e.g., formed).

[0093] The second organic insulating layer 394 may be disposed on the second touch screen electrode 384. The second organic insulating layer 394 may cover the second touch screen electrode 384 in the light emitting region 30 and may extend in the first direction D1. In an exemplary embodiment, the second organic insulating layer 394 may be disposed in the bending region 50 on the display panel 200. In some embodiments, the second organic insulating layer 394 may be continuously disposed in the display region 10, the bending region 50, and a portion of the pad region 60 on the display panel 200. For example, the second organic insulating layer 394 may fully (or appropriately) cover the second touch screen electrode 384 in the light emitting region 30 on the first organic insulating layer 392, and may have a substantially flat upper surface without generating a step portion around the second touch screen electrode 384. In some embodiments, the second organic insulating layer 394 may extend in the first direction D1 and may be disposed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the first organic insulating layer 392. The second organic insulating layer 394 may include photoresist, acrylic fiber-based resin, polyimide-based resin, polyamide-based resin, siloxane-based resin, acrylic-based resin and / or epoxy-based resin. In some embodiments, the second organic insulating layer 394 may include PET, PEN, PP, PC, PS, PSul, PE, PPA, PES, PAR, PCO, MPPO, etc. In an exemplary embodiment, the second organic insulating layer 394 may be essentially composed of an organic material. In some embodiments, the second organic insulating layer 394 and the first organic insulating layer 392 may be formed using the same material. Thus, an organic insulating structure 390 including the first organic insulating layer 392 and the second organic insulating layer 394 may be constructed (e.g., formed).

[0094] In certain exemplary embodiments, the OLED device 100 may include Figure 6 The touch screen electrodes are 1380 instead of Figure 5 The touch screen electrode 1380 may include a first touch screen electrode 1382, a second touch screen electrode 1384 and a connection pattern 1180. Figure 6 As shown in , the OLED device 100 may include a plurality of first touch screen electrodes 1382 disposed on the third TFE layer 453. The first touch screen electrodes 1382 may extend in a second direction D2 (or a first direction D1) parallel to the upper surface of the OLED device 100, and may be spaced apart from each other in a third direction D3. The first touch screen electrodes 1382 may have a planar shape of a bar. For example, the first touch screen electrodes 1382 may have a planar shape of a bar including a plurality of protrusions. A first touch sensing voltage may be applied to the first touch screen electrodes 1382.

[0095] The OLED device 100 may include a plurality of second touch screen electrodes 1384 disposed on the third TFE layer 453. The second touch screen electrodes 1384 may be spaced apart from each other in the second direction D2 (or the first direction D1) between adjacent two of the first touch screen electrodes 1382. The second touch screen electrodes 1384 may be island-shaped. For example, the second touch screen electrodes 1384 may have a square planar shape and may be disposed between protrusions of the first touch screen electrodes 1382. In an exemplary embodiment, the first touch screen electrodes 1382 and the second touch screen electrodes 1384 may be located at the same layer (e.g., the same level).

[0096] The first organic insulating layer 392 may be disposed on the first touch screen electrode 1382 and the second touch screen electrode 1384. The first organic insulating layer 392 may cover the first touch screen electrode 1382 and the second touch screen electrode 1384 in the light emitting region 30, and may extend in the first direction D1. In an exemplary embodiment, the first organic insulating layer 392 may be disposed in the bending region 50 on the display panel 200. In some embodiments, the first organic insulating layer 392 may be continuously disposed in a portion of the display region 10, the bending region 50, and the pad region 60 on the display panel 200. For example, the first organic insulating layer 392 may fully (or appropriately) cover the first touch screen electrode 1382 and the second touch screen electrode 1384 in the light emitting region 30 on the third TFE layer 453, and may have a substantially flat upper surface without generating a step portion around the first touch screen electrode 382 and the second touch screen electrode 1384. In certain embodiments, the first organic insulating layer 392 may extend in the first direction D1 and may be disposed in a portion of the peripheral region 40 , the bending region 50 , and the pad region 60 on the pixel defining layer 310 .

[0097] In addition, the OLED device 100 may include a plurality of connection patterns 1180 disposed on the first touch screen electrodes 1382 and the second touch screen electrodes 1384. In some embodiments, the connection patterns 1180 may be disposed below the first touch screen electrodes 1382 and the second touch screen electrodes 1384. The connection patterns 1180 may contact (e.g., be electrically connected to) two second touch screen electrodes 1384 that are adjacent to each other in the third direction D3 among the plurality of second touch screen electrodes 1384. In an exemplary embodiment, the connection patterns 1180 may be located in a layer different from that of the first touch screen electrodes 1382 and the second touch screen electrodes 1384 (e.g., a different level). For example, the connection patterns 1180 may be disposed on or below the first touch screen electrodes 1382 and the second touch screen electrodes 1384.

[0098] The OLED device 100 may electrically connect the touch screen electrode 1380 and the external device 101 through the touch sensor wiring, and the first touch sensing voltage and the second touch sensing voltage generated by the external device 101 may be provided to the first touch screen electrode 1382 and the second touch screen electrode 1384, respectively. The external device 101 may detect a change in capacitance between the first touch screen electrode 1382 and the second touch screen electrode 1384. For example, the first touch sensing voltage as a sensing input signal generated by the external device 101 may be applied to the first touch screen electrode 1382, and the second touch sensing voltage as a sensing output signal may be output to the external device 101 through the second touch screen electrode 1384. Here, the first touch sensing voltage may have a voltage level that changes periodically, and the second touch sensing voltage may have a DC voltage level.

[0099] For example, when the user of the OLED device 100 contacts the upper surface of the OLED device 100, the capacitance of the first touch screen electrode 1382 and the second touch screen electrode 1384 corresponding to the contact surface may change. A changed capacitance may be generated between the portion of the body connected to the upper surface of the OLED device 100 and the first touch screen electrode 1382 and the second touch screen electrode 1384, and a sensing output signal changed by the changed capacitance may be output to the external device 101 through the touch sensor wiring. The external device 101 may detect the changed sensing output signal. In other words, the OLED device 100 may detect the contact position of the user by using the first touch sensing voltage and the second touch sensing voltage. After the user's contact with the OLED device 100 ends, the external device 101 may provide the first touch sensing voltage and the second touch sensing voltage to the first touch screen electrode 1382 and the second touch screen electrode 1384, respectively. Thus, the touch screen electrode 1380 including the first touch screen electrode 1382 and the second touch screen electrode 1384 may be constituted (e.g., formed).

[0100] The second organic insulating layer 394 may be disposed on the connection pattern 1180. The second organic insulating layer 394 may cover the connection pattern 1180 in the light emitting region 30 and may extend in the first direction D1. In an exemplary embodiment, the second organic insulating layer 394 may be disposed in the bending region 50 on the display panel 200. In some embodiments, the second organic insulating layer 394 may be continuously disposed in the display region 10, the bending region 50, and a portion of the pad region 60 on the display panel 200. For example, the second organic insulating layer 394 may fully (or appropriately) cover the connection pattern 1180 in the light emitting region 30 on the first organic insulating layer 392, and may have a substantially flat upper surface without generating a step portion around the connection pattern 1180. In some embodiments, the second organic insulating layer 394 may extend in the first direction D1 and may be disposed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the first organic insulating layer 392. Thus, an organic insulating structure 390 including a first organic insulating layer 392 and a second organic insulating layer 394 may be constructed (eg, formed).

[0101] Refer again Figure 4 , the polarization layer 430 may be disposed on the touch screen 400. The polarization layer 430 may overlap a portion of the light emitting region 30 and the peripheral region 40 on the substrate 110. The polarization layer 430 may include a linear polarization film and a λ / 4 phase delay film. The λ / 4 phase delay film may be disposed on the touch screen 400. The λ / 4 phase delay film may convert the phase of light. For example, the λ / 4 phase delay film may convert light oscillating up and down or light oscillating left and right into right-handed circularly polarized light or left-handed circularly polarized light, respectively. In certain embodiments, the λ / 4 phase delay film may convert right-handed circularly polarized light or left-handed circularly polarized light into light oscillating up and down or light oscillating left and right, respectively. The λ / 4 phase delay film may include a birefringent film including a polymer, an oriented film of a liquid crystal polymer, an orientation layer of a liquid crystal polymer, and the like.

[0102] The linear polarizing film may be disposed on the λ / 4 phase delay film. The linear polarizing film may selectively transmit incident light. For example, the linear polarizing film may transmit light oscillating up and down or light oscillating left and right. In this case, the linear polarizing film may include a horizontal stripe pattern or a vertical stripe pattern. When the linear polarizing film includes a horizontal stripe pattern, the linear polarizing film may block light oscillating up and down, and may transmit light oscillating left and right. When the linear polarizing film includes a vertical stripe pattern, the linear polarizing film may block light oscillating left and right, and may transmit light oscillating up and down. The light transmitted by the linear polarizing film may then be transmitted by the λ / 4 phase delay film. As described above, the λ / 4 phase delay film may convert the phase of light. For example, when incident light oscillating up and down and left and right passes through the linear polarizing film, the linear polarizing film including the horizontal stripe pattern may transmit light oscillating left and right. When the transmitted incident light oscillating left and right subsequently passes through the λ / 4 phase delay film, the incident light oscillating left and right may be converted into left-handed circularly polarized light. The incident light including left-handed circularly polarized light may be reflected at the upper electrode 340, and then the incident light may be converted into right-handed circularly polarized light. When the incident light including right-handed circularly polarized light subsequently passes through the λ / 4 phase delay film, the incident light may be converted into light that oscillates up and down. Here, the light that oscillates up and down may be blocked by the linear polarizing film including the horizontal stripe pattern. Therefore, the incident light may be removed by the linear polarizing film and the λ / 4 phase delay film (i.e., the polarizing layer 430). For example, the linear polarizing film may include an iodine-based material, a dye-containing material, a polyene-based material, etc. In an exemplary embodiment, the thickness of the polarizing layer 430 may be about 31 microns. In some embodiments, the polarizing layer 430 may be a thin film polarizing layer.

[0103] The cover window 415 may be disposed on the polarizing layer 430. The cover window 415 may overlap a portion of the bending region 50 on the substrate 110 and the display region 10. The cover window 415 may protect the polarizing layer 430 and the display panel 200. The cover window 415 may include a material having heat resistance and / or transparency. For example, the cover window 415 may include transparent plastic and / or glass having a transparency of about 95% or more. In some embodiments, the cover window 415 may have a multilayer structure including a plurality of layers.

[0104] For example, the comparative OLED device may include a polarizing layer having a thickness of about 132 microns (e.g., a polarizing layer having a relatively large thickness) and a bending protection layer having a thickness of about 100 microns. The polarizing layer may be disposed in the display area on the display panel, and the bending protection layer may be disposed in a portion of the peripheral area, the bending area, and a portion of the pad area on the display panel. Here, the polarizing layer may be in direct contact with the bending protection layer in the peripheral area, and the bending protection layer may be in direct contact with the first direction D1, the second direction D2, and the third direction D3 at a contact portion where the polarizing layer is in direct contact with the bending protection layer, in a direction perpendicular to the first direction D1, the second direction D2, and the third direction D3 (e.g., in the current Figure 4The bending protection layer may have a relatively large thickness in a direction extending from the substrate 110 to the cover window 415. For example, the bending protection layer may have a protrusion in the peripheral area. The thickness of the bending protection layer may be determined (set) so that the neutral plane is positioned at (or above) the portion of the bending area where the connection electrode is provided. In this way, when the bending area is bent, the connection electrode may not be damaged because the neutral plane of the bending area is positioned at the portion of the bending area where the connection electrode is provided.

[0105] However, in order to make such a comparative OLED device relatively thin, the thickness of the polarizing layer may have to be made thin. For example, the comparative OLED device may include a polarizing layer having a thickness of about 31 microns (e.g., a polarizing layer having a relatively thin thickness) and a bending protective layer having a thickness of about 100 microns. However, in this case, adhesion breakage of the cover window disposed on the polarizing layer having a relatively thin thickness may occur due to the protrusion of the bending protective layer. In addition, in order to avoid the bending protective layer from being separated from the display panel, when the bending protective layer of the comparative OLED device is bent, the bending protective layer may be arranged to overlap with the peripheral area and the pad area. Therefore, the length of the peripheral area of ​​the comparative OLED device may be increased to ensure the processing margin of the bending protective layer, and thus the invalid space (e.g., non-display area) of the comparative OLED device may be relatively increased.

[0106] In an exemplary embodiment of the present disclosure, an organic insulating structure 390 may be used instead of the bending protection layer, and the organic insulating structure 390 may be disposed in the bending region 50. For example, the organic insulating structure 390 may be disposed in the bending region 50 so that the neutral plane in the bending region 50 is positioned at a portion where the connecting electrode 330 is disposed. Here, the thickness of the organic insulating structure 390 may be determined so that the neutral plane in the bending region 50 is positioned at a portion where the connecting electrode 330 is disposed. In this case, since the organic insulating structure 390 is essentially composed of an organic material, an inorganic insulating layer may not be disposed in the bending region 50. In addition, since the bending protection layer is not disposed in the OLED device 100 of the present embodiment, adhesion breakage of the cover window 415 may not occur. In addition, since the length of the peripheral region 40 of the OLED device 100 (e.g., Figure 4 ) is relatively reduced, so the ineffective space (eg, non-display area) of the OLED device 100 can be relatively reduced.

[0107] The first lower protective film pattern 351 and the second lower protective film pattern 352 may be disposed on the substrate 110 (e.g., disposed on the lower surface of the substrate 110 opposite to the surface where the buffer layer 115 may be located). The first lower protective film pattern 351 may be disposed in the entire display area 10, and the second lower protective film pattern 352 may be disposed in the pad area 60, and the lower surface of the display panel 200 located in the bending area 50 (e.g., the lower surface of the substrate 110 located in the bending area 50) may be exposed. In some embodiments, the lower protective film 300 may expose the lower surface of the display panel 200 located in the bending area 50, and the first lower protective film pattern 351 and the second lower protective film pattern 352 may be spaced apart from each other. The lower protective film 300 may protect the display panel 200 from external impact. The lower protective film 300 may include PET, PEN, PP, PC, PS, PSul, PE, PPA, PES, PAR, PCO, MPPO, etc. The thickness of the lower protective film 300 may be about 50 microns.

[0108] The OLED device 100 according to the exemplary embodiment includes an organic insulating structure 390 included in the touch screen 400, and the organic insulating structure 390 may be used instead of the bending protection layer of the comparative OLED device and may be disposed in the bending region 50. For example, the organic insulating structure 390 may be disposed in the bending region 50 so that the neutral plane in the bending region 50 is positioned at (or on) a portion where the connecting electrode 330 is disposed. Therefore, although the bending region 50 is bent, a cut (or breakage) of the connecting electrode 330 may not occur in the bending region 50. In addition, since the bending protection layer of the comparative OLED device is not disposed (formed), adhesion breakage of the cover window 415 may not occur. Since the peripheral region 40 (e.g., as Figure 4 The length of the OLED device 100 may be relatively reduced, so the ineffective space (eg, non-display area) of the OLED device 100 may be relatively reduced. In addition, since no bending protection layer is provided, the manufacturing cost of the OLED device 100 may be relatively reduced.

[0109] Figure 7 Is used to describe Figure 1 A cross-sectional view of a curved shape of an OLED device.

[0110] Reference Figure 7 , since the bending region 50 may be curved around an axis relative to the third direction D3 (eg, Figure 1The second lower protective film pattern 352 is bent in the main axis direction of the bending region 50, so that the second lower protective film pattern 352 can be positioned to face the lower surface of the first lower protective film pattern 351. In some embodiments, the OLED device 100 may further include an adhesive layer interposed between the first lower protective film pattern 351 and the second lower protective film pattern 352. In this case, the first lower protective film pattern 351 and the second lower protective film pattern 352 may be fixed by the adhesive layer.

[0111] Figures 8 to 12 is a cross-sectional view illustrating actions of a method of manufacturing an OLED device according to an exemplary embodiment. Fig. 9 is corresponding to Figure 8 an enlarged cross-sectional view of region "B" of Fig.11 is corresponding to Fig.10 An enlarged cross-sectional view of area "C" is shown in FIG.

[0112] Reference Figure 8 , a display panel 200 may be provided. For example, Fig. 9 As shown in FIG. 1 , the substrate 110 may be formed on a rigid glass substrate 105. The substrate 110 may be formed using a flexible transparent resin substrate.

[0113] The buffer layer 115 may be formed on the substrate 110. In an exemplary embodiment, the buffer layer 115 may be completely formed in (e.g., completely cover) the light emitting region 30, the peripheral region 40, and the pad region 60 on the substrate 110, and may have a first opening exposing a portion of the upper surface of the substrate 110 located in the bending region 50. The buffer layer 115 may be formed using a silicon compound, a metal oxide, or the like. For example, the buffer layer 115 may include SiO x 、SiN x 、SiO x N y 、SiO x C y 、SiC x N y 、AlO x 、AlN x 、TaO x , HfO x 、ZrO x 、TiO x wait.

[0114] The active layer 130 may be formed in the light emitting region 30 on the buffer layer 115. The active layer 130 may be formed using an oxide semiconductor, an inorganic semiconductor, an organic semiconductor, or the like.

[0115] The gate insulating layer 150 may be formed on the active layer 130. The gate insulating layer 150 may cover the active layer 130 in the light emitting region 30 on the buffer layer 115, and may extend from the light emitting region 30 to the pad region 60 in the first direction D1. In an exemplary embodiment, the gate insulating layer 150 may be formed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the buffer layer 115, and may have a second opening that exposes a portion of the upper surface of the substrate 110 positioned in the bending region 50. The gate insulating layer 150 may be formed using a silicon compound, a metal oxide, or the like.

[0116] The first gate electrode 170 may be formed in the light emitting region 30 on the gate insulating layer 150. The first gate electrode 170 may be formed on a portion of the gate insulating layer 150 under which the active layer 130 is positioned. The first gate electrode 170 may be formed using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, or the like. For example, the first gate electrode 170 may include Au, Ag, Al, Pt, Ni, Ti, Pd, Mg, Ca, Li, Cr, Ta, W, Cu, Mo, Sc, Nd, Ir, aluminum alloy, AlN x , Silver alloy, WN x , copper alloy, molybdenum alloy, TiN x CrN x 、TaN x 、SRO、ZnO x 、ITO、SnO x 、InO x 、GaO x , IZO, etc. These may be used alone or in appropriate combination thereof. In certain exemplary embodiments, the first gate electrode 170 may have a multi-layer structure including a plurality of layers.

[0117] The first fan-out wiring 301 may extend along the second direction D2 in the peripheral region 40 on the gate insulating layer 150, and may be electrically connected to the light emitting structure 500 formed in the light emitting region 30. In addition, the second fan-out wiring 302 may extend along the first direction D1 in the pad region 60 on the gate insulating layer 150, and may be electrically connected to the external device 101 (e.g., see FIG. 4 ) through the pad electrode 470 formed in the pad region 60. Figure 1 and Figure 2). The first fan-out wiring 301 and the second fan-out wiring 302 may each be formed separately using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. Thus, a fan-out wiring 1300 including the first fan-out wiring 301 and the second fan-out wiring 302 may be formed. In an exemplary embodiment, the fan-out wiring 1300 and the first gate electrode 170 may be located at the same layer (e.g., at the same level) and may be formed simultaneously (or at the same time) using the same material. In certain embodiments, the fan-out wiring 1300 and the second gate electrode 175 (to be described below) may be located at the same layer (e.g., at the same level). In certain exemplary embodiments, the fan-out wiring 1300 may have a multilayer structure including a plurality of layers.

[0118] A first insulating interlayer 190 may be formed on the first gate electrode 170. The first insulating interlayer 190 may cover the first gate electrode 170 in the light emitting region 30 on the gate insulating layer 150, and may extend in the first direction D1. In certain embodiments, the first insulating interlayer 190 may cover the first fan-out wiring 301 in the peripheral region 40 on the gate insulating layer 150 and the second fan-out wiring 302 in the pad region 60. In an exemplary embodiment, the first insulating interlayer 190 may be formed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the gate insulating layer 150, and may have a third opening that exposes a portion of the upper surface of the substrate 110 positioned in the bending region 50. The first insulating interlayer 190 may be formed using a silicon compound, a metal oxide, or the like.

[0119] The second gate electrode 175 may be formed in the light emitting region 30 on the first insulating interlayer 190. The second gate electrode 175 may be formed on a portion of the first insulating interlayer 190 under which the first gate electrode 170 is positioned. The second gate electrode 175 may be formed using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, or the like. These may be used alone or in appropriate combination thereof. In certain exemplary embodiments, the second gate electrode 175 may have a multilayer structure including a plurality of layers.

[0120] A second insulating interlayer 195 may be formed on the second gate electrode 175. The second insulating interlayer 195 may cover the second gate electrode 175 in the light emitting region 30 on the first insulating interlayer 190, and may extend in the first direction D1. In an exemplary embodiment, the second insulating interlayer 195 may be formed in the light emitting region 30, the peripheral region 40, and the pad region 60 on the first insulating interlayer 190, and may have a fourth opening that exposes a portion of the upper surface of the substrate 110 positioned in the bending region 50. Here, the first to fourth openings may overlap each other. The second insulating interlayer 195 may be formed using a silicon compound, a metal oxide, or the like.

[0121] The source electrode 210 and the drain electrode 230 may be formed in the light emitting region 30 on the second insulating interlayer 195. The source electrode 210 may be in direct contact with the source region of the active layer 130 via a contact hole formed by removing a portion of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195. The drain electrode 230 may be in direct contact with the drain region of the active layer 130 via a contact hole formed by removing another portion of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195. The source electrode 210 and the drain electrode 230 may each independently be formed using a metal, an alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the source electrode 210 and the drain electrode 230 may each independently have a multilayer structure including a plurality of layers. Thus, the semiconductor element 250 including the active layer 130 , the gate insulating layer 150 , the first gate electrode 170 , the first insulating interlayer 190 , the second gate electrode 175 , the second insulating interlayer 195 , the source electrode 210 , and the drain electrode 230 may be formed.

[0122] A first conductive pattern 401 may be formed on the second insulating interlayer 195, and the first conductive pattern 401 may be in direct contact with the first fan-out wiring 301 via a first contact hole, wherein the first contact hole is formed by removing a first portion of the first insulating interlayer 190 and the second insulating interlayer 195 located in the peripheral region 40, and a second conductive pattern 402 may be formed on the second insulating interlayer 195, and the second conductive pattern 402 may be in direct contact with the second fan-out wiring 302 via a second contact hole, wherein the second contact hole is formed by removing a second portion of the first insulating interlayer 190 and the second insulating interlayer 195 located in the pad region 60. Thus, a conductive pattern 460 including the first conductive pattern 401 and the second conductive pattern 402 may be formed. In an exemplary embodiment, the conductive pattern 460, the source electrode 210, and the drain electrode 230 may be located at the same layer (e.g., at the same level), and may be formed simultaneously (or at the same time) using the same material. In some embodiments, the conductive pattern 460 and the second gate electrode 175 may be located at the same level. The conductive pattern 460 may be formed using metal, metal alloy, metal nitride, conductive metal oxide, transparent conductive material, etc. These may be used alone or in appropriate combination thereof. In some exemplary embodiments, the conductive pattern 460 may have a multilayer structure including a plurality of layers.

[0123] The first planarization layer 270 may be formed on the second insulating interlayer 195, the source electrode 210, the drain electrode 230, and the conductive pattern 460. The first planarization layer 270 may cover the source electrode 210 and the drain electrode 230 in the light emitting region 30 on the second insulating interlayer 195, and may cover the conductive pattern 460 in the peripheral region 40 and the pad region 60 on the second insulating interlayer 195. In an exemplary embodiment, the first planarization layer 270 may be in direct contact with the following portions: a lower surface of the connection electrode 330 (to be described below); a sidewall (e.g., sidewalls of the first to fourth openings) of each of the gate insulating layer 150, the first insulating interlayer 190, and the second insulating interlayer 195 located adjacent to the bending region 50; and a portion of the upper surface of the substrate 110 located in the bending region 50. In some embodiments, the first planarization layer 270 may completely (e.g., fully) cover the conductive pattern 460. For example, the first planarization layer 270 may be formed to have a large thickness. In this case, the first planarization layer 270 may have a substantially flat upper surface, and a planarization process may be further performed on the first planarization layer 270 to achieve a flat upper surface of the first planarization layer 270. In an exemplary embodiment, the first planarization layer 270 may be formed using an organic material.

[0124] The wiring pattern 215 and the connection pattern 235 may be formed in the light emitting region 30 on the first planarization layer 270. The connection pattern 235 may be spaced apart from the wiring pattern 215 in the light emitting region 30 on the first planarization layer 270. The connection pattern 235 may contact the drain electrode 230 via a contact hole formed by removing a portion of the first planarization layer 270 positioned in the light emitting region 30.

[0125] The connection electrode 330 may be formed in a portion of the peripheral region 40, the bending region 50, and a portion of the pad region 60 on the first planarization layer 270. The connection electrode 330 may directly contact the conductive pattern 460 and may be electrically connected to the fan-out wiring 1300.

[0126] A pad electrode 470 may be formed in the pad region 60 on the substrate 110. The pad electrode 470 may be electrically connected to the connection electrode 330 through the second fan-out wiring 302 and the second conductive pattern 402. In an exemplary embodiment, the connection electrode 330, the pad electrode 470, the wiring pattern 215, and the connection pattern 235 may be located at the same level and may be formed simultaneously (or at the same time) using the same material. The connection electrode 330, the pad electrode 470, the wiring pattern 215, and the connection pattern 235 may each independently be formed using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the connection electrode 330, the pad electrode 470, the wiring pattern 215, and the connection pattern 235 may each independently have a multilayer structure including a plurality of layers.

[0127] The second planarization layer 275 may be formed on the wiring pattern 215, the connection pattern 235, the connection electrode 330, and the first planarization layer 270. The second planarization layer 275 may cover the wiring pattern 215 and the connection pattern 235 in the light emitting region 30 on the first planarization layer 270 and extend in the first direction D1, and may cover the connection electrode 330 in the peripheral region 40, the bending region 50, and the pad region 60. In an embodiment, the second planarization layer 275 may be formed on (or above) the entire substrate 110. The second planarization layer 275 may be formed to have a large thickness to sufficiently (or appropriately) cover the wiring pattern 215, the connection pattern 235, and the connection electrode 330. In certain embodiments, the second planarization layer 275 may have a substantially flat upper surface, and a planarization process may be further performed on the second planarization layer 275 to achieve a flat upper surface of the second planarization layer 275. In an exemplary embodiment, the second planarization layer 275 may be formed using an organic material.

[0128] A lower electrode 290 may be formed in the light emitting region 30 on the second planarization layer 275. The lower electrode 290 may contact the connection pattern 235 via a contact hole formed by removing a portion of the second planarization layer 275. In some embodiments, the lower electrode 290 may be electrically connected to the semiconductor element 250. The lower electrode 290 may be formed using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, or the like. These may be used alone or in appropriate combination thereof. In some exemplary embodiments, the lower electrode 290 may have a multilayer structure including a plurality of layers.

[0129] The pixel defining layer 310 may be formed in the light emitting region 30 on the second planarization layer 275, and the pixel defining layer 310 may expose a portion of the lower electrode 290. In some embodiments, the pixel defining layer 310 may extend in the first direction D1, may cover both sides of the lower electrode 290, and may be formed in the peripheral region 40, the bending region 50, and the pad region 60. In some embodiments, the pixel defining layer 310 may be formed only in the light emitting region 30, and may not be formed in the peripheral region 40, the bending region 50, or the pad region 60. In an exemplary embodiment, the pixel defining layer 310 may be formed using an organic material.

[0130] The light emitting layer 335 may be formed on a portion of the lower electrode 290 exposed by the pixel defining layer 310. The light emitting layer 335 may be formed using at least one of appropriate light emitting materials capable of generating light of different colors (e.g., red light, blue light, green light, etc.) according to sub-pixels. In some embodiments, the light emitting layer 335 may generate white light by stacking a plurality of light emitting materials capable of generating light of different colors (such as red light, green light, blue light, etc.).

[0131] The upper electrode 340 may be formed in the light emitting region 30 on the pixel defining layer 310 and the light emitting layer 335. The upper electrode 340 may be formed using a metal, a metal alloy, a metal nitride, a conductive metal oxide, a transparent conductive material, etc. These may be used alone or in appropriate combinations thereof. In certain exemplary embodiments, the upper electrode 340 may have a multilayer structure including a plurality of layers. Thus, a light emitting structure 500 including the lower electrode 290, the light emitting layer 335, and the upper electrode 340 may be formed.

[0132] The first TFE layer 451 may be formed in the light emitting region 30 on the upper electrode 340. The first TFE layer 451 may cover the upper electrode 340 and may be formed to have a substantially uniform thickness along the contour of the upper electrode 340. The first TFE layer 451 may prevent or reduce degradation of the light emitting structure 500 due to penetration of moisture, water, oxygen, etc. In addition, the first TFE layer 451 may protect the light emitting structure 500 from external impact. The first TFE layer 451 may be formed using an inorganic material having flexibility.

[0133] The second TFE layer 452 may be formed on the first TFE layer 451. The second TFE layer 452 may improve the flatness of the OLED device 100 and may protect the light emitting structure 500. The second TFE layer 452 may be formed using an organic material having flexibility.

[0134] A third TFE layer 453 may be formed on the second TFE layer 452. The third TFE layer 453 may cover the second TFE layer 452, and may be formed to have a substantially uniform thickness along the contour of the second TFE layer 452. The third TFE layer 453 may prevent or reduce degradation of the light emitting structure 500 due to penetration of moisture, water, oxygen, etc., together with the first TFE layer 451 and the second TFE layer 452. In addition, the third TFE layer 453 may protect the light emitting structure 500 from external impacts together with the first TFE layer 451 and the second TFE layer 452. The third TFE layer 453 may be formed using an inorganic material having flexibility. In some embodiments, the TFE structure 450 may include a first TFE layer 451, a second TFE layer 452 and a third TFE layer 453, and the display panel 200 may include a substrate 110, a buffer layer 115, a semiconductor element 250, a light emitting structure 500, a fan-out wiring 1300, a conductive pattern 460, a first planarization layer 270, a second planarization layer 275, a connecting electrode 330, a wiring pattern 215, a connecting pattern 235, a pixel defining layer 310 and a TFE structure 450, but is not limited thereto.

[0135] Reference Fig.10 , a touch screen 400 may be formed on the display panel 200. Fig.11 As shown in FIG. 4 , the first touch screen electrode 382 may be formed on the third TFE layer 453. In an exemplary embodiment, the first touch screen electrode 382 may be directly formed on the third TFE layer 453. The first touch screen electrode 382 may be made of CNT, TCO, ITO, IGZO, ZnO x , graphene, AgNW, Cu, Cr, etc.

[0136] A first organic insulating layer 392 may be formed on the first touch screen electrode 382. The first organic insulating layer 392 may cover the first touch screen electrode 382 in the light emitting region 30 and may extend in the first direction D1. In an exemplary embodiment, the first organic insulating layer 392 may be formed in the bending region 50 on the display panel 200. In some embodiments, the first organic insulating layer 392 may be continuously disposed in a portion of the display region 10, the bending region 50, and the pad region 60 on the display panel 200. For example, the first organic insulating layer 392 may fully cover the first touch screen electrode 382 in the light emitting region 30 on the third TFE layer 453 and may have a substantially flat upper surface without generating a step portion around the first touch screen electrode 382. In addition, the first organic insulating layer 392 may extend in the first direction D1 and may be formed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the pixel defining layer 310. The first organic insulating layer 392 may be formed using photoresist, acrylic fiber-based resin, polyimide-based resin, polyamide-based resin, siloxane-based resin, acrylic-based resin, and / or epoxy-based resin, but is not limited thereto. In some embodiments, the first organic insulating layer 392 may be formed using PET, PEN, PP, PC, PS, PSul, PE, PPA, PES, PAR, PCO, MPPO, etc.

[0137] The second touch screen electrode 384 may be formed on the first organic insulating layer 392. The second touch screen electrode 384 and the first touch screen electrode 382 may be formed using the same material. Thus, the touch screen electrode 380 including the first touch screen electrode 382 and the second touch screen electrode 384 may be formed.

[0138] The second organic insulating layer 394 may be formed on the second touch screen electrode 384. The second organic insulating layer 394 may cover the second touch screen electrode 384 in the light emitting region 30 and may extend in the first direction D1. In an exemplary embodiment, the second organic insulating layer 394 may be formed in the bending region 50 on the display panel 200. In some embodiments, the second organic insulating layer 394 may be continuously formed in the display region 10, the bending region 50, and a portion of the pad region 60 on the display panel 200. For example, the second organic insulating layer 394 may fully (or appropriately) cover the second touch screen electrode 384 in the light emitting region 30 on the first organic insulating layer 392 and may have a substantially flat upper surface without generating a step portion around the second touch screen electrode 384. In some embodiments, the second organic insulating layer 394 may extend in the first direction D1 and may be formed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the first organic insulating layer 392. The second organic insulating layer 394 and the first organic insulating layer 392 may be formed using the same material. In the current embodiment, the organic insulating structure 390 may include a first organic insulating layer 392 and a second organic insulating layer 394, and the touch screen 400 may include the touch screen electrode 380 and the organic insulating structure 390. After the touch screen 400 is formed, the rigid glass substrate 105 may be removed from the substrate 110.

[0139] Reference Fig.12 , a polarizing layer 430 may be formed on the touch screen 400. The polarizing layer 430 may overlap a portion of the light emitting region 30 and the peripheral region 40 on the substrate 110. The polarizing layer 430 may include a linear polarizing film and a λ / 4 phase retardation film. The λ / 4 phase retardation film may be formed on the touch screen 400. The λ / 4 phase retardation film may be formed using a birefringent film containing a polymer, an oriented film of a liquid crystal polymer, an orientation layer of a liquid crystal polymer, and the like. A linear polarizing film may be provided on the λ / 4 phase retardation film. The linear polarizing film may be formed using an iodine-based material, a dye-containing material, a polyene-based material, and the like. In an exemplary embodiment, the thickness of the polarizing layer 430 may be about 31 microns. In some embodiments, the polarizing layer 430 may be a thin film polarizing layer.

[0140] A first lower protective film pattern 351 and a second lower protective film pattern 352 may be formed on the substrate 110 (e.g., formed on the lower surface of the substrate 110). The first lower protective film pattern 351 may be formed in the entire display area 10, and the second lower protective film pattern 352 may be formed in the pad area 60, so that the lower surface of the display panel 200 positioned in the bending area 50 (e.g., the lower surface of the substrate 110 positioned in the bending area 50) may be exposed. Thus, a lower protective film 300 including the first lower protective film pattern 351 and the second lower protective film pattern 352 may be formed. The lower protective film 300 may protect the display panel 200 from external impact. The lower protective film 300 may be formed using PET, PEN, PP, PC, PS, PSul, PE, PPA, PES, PAR, PCO, MPPO, etc. The thickness of the lower protective film 300 may be about 50 microns.

[0141] A cover window 415 may be formed on the polarizing layer 430. The cover window 415 may overlap a portion of the display region 10 and the bending region 50 on the substrate 110. The cover window 415 may protect the polarizing layer 430 and the display panel 200. The cover window 415 may be formed using a material having heat resistance and / or transparency. For example, the cover window 415 may include a transparent plastic and / or glass having a transparency of about 95% or more. In some embodiments, the cover window 415 may have a multilayer structure including a plurality of layers. According to the methods described herein, an OLED device 100 (e.g., such as Figure 3 ), and the OLED device 100 may be used as a flexible OLED device capable of bending (or being bent) in the bending region 50 .

[0142] Fig.13 3 is a cross-sectional view showing an OLED device according to one or more exemplary embodiments. In addition to including a third organic insulating layer 396, Fig.13 The configuration of the OLED device 700 shown in FIG. 7 may have the same Figures 1 to 7 The configuration of the OLED device 100 described above is substantially the same or similar to the configuration. Fig.13 No reference will be provided Figures 1 to 7 The described elements are substantially the same or similar elements and the description is repeated.

[0143] Reference Fig.13, the OLED device 700 may include a display panel 200, a touch screen 400, a polarizing layer 430, a cover window 415, a lower protective film 300, and the like. Here, the display panel 200 may include a substrate 110, a buffer layer 115, a semiconductor element 250, a light emitting structure 500, a fan-out wiring 1300, a conductive pattern 460, a first planarization layer 270, a second planarization layer 275, a connection electrode 330, a wiring pattern 215, a connection pattern 235, a pixel defining layer 310, and a TFE structure 450, but is not limited thereto, and the TFE structure 450 may include a first TFE layer 451, a second TFE layer 452, and a third TFE layer 453. In an exemplary embodiment, the touch screen 400 may include a touch screen electrode 380 and an organic insulating structure 390. The touch screen electrode 380 may include a first touch screen electrode 382 and a second touch screen electrode 384, and the organic insulating structure 390 may include a first organic insulating layer 392, a second organic insulating layer 394, and a third organic insulating layer 396. For example, Fig.13 The touch screen electrodes 380 in may correspond to Figure 5 In some embodiments, the touch screen electrodes 380 (including the first touch screen electrodes 382 and the second touch screen electrodes 384) shown in FIG. Fig.13 The touch screen electrodes 380 in may correspond to Figure 6 The touch screen electrodes 1380 (including the first touch screen electrodes 1382, the second touch screen electrodes 1384 and the connection pattern 1180) shown in FIG.

[0144] The third organic insulating layer 396 may be disposed on the third TFE layer 453. In some embodiments, the third organic insulating layer 396 may be disposed below the first touch screen electrode 382 and the first organic insulating layer 392. The third organic insulating layer 396 may cover the third TFE layer 453 in the light emitting region 30 and may extend in the first direction D1. In an exemplary embodiment, the third organic insulating layer 396 may be disposed in the bending region 50 on the display panel 200. In some embodiments, the third organic insulating layer 396 may be continuously disposed in a portion of the display region 10, the bending region 50, and the pad region 60 on the display panel 200. For example, the third organic insulating layer 396 may fully (or appropriately) cover the third TFE layer 453 in the light emitting region 30 and may have a substantially flat upper surface without a step portion. The third organic insulating layer 396 may extend in the first direction D1 and may be disposed in a portion of the peripheral region 40, the bending region 50, and the pad region 60 on the pixel defining layer 310. When the surface of the third TFE layer 453 is relatively irregular, the third organic insulating layer 396 can improve the surface flatness of the third TFE layer 453. The third organic insulating layer 396 may include photoresist, acrylic fiber-based resin, polyimide-based resin, polyamide-based resin, siloxane-based resin, acrylic-based resin and / or epoxy-based resin, but is not limited thereto. In certain embodiments, the third organic insulating layer 396 may include PET, PEN, PP, PC, PS, PSul, PE, PPA, PES, PAR, PCO, MPPO, etc. In an exemplary embodiment, the third organic insulating layer 396 may be essentially composed of an organic material.

[0145] The OLED device 700 according to the exemplary embodiment includes an organic insulating structure 390 included in the touch screen 400, wherein the organic insulating structure 390 may be used instead of the bending protection layer of the comparative OLED device and may be disposed in the bending region 50. Since the organic insulating structure 390 includes a first organic insulating layer 392, a second organic insulating layer 394, and a third organic insulating layer 396, the neutral plane in the bending region 50 may be easily positioned at (or above) a portion where the connection electrode 330 is disposed due to a relatively increased thickness of the organic insulating structure 390.

[0146] Fig.14 is a cross-sectional view showing an OLED device according to an exemplary embodiment, and Fig.15 is corresponding to Fig.14 In addition to including touch screen 1400, Fig.14 and Fig.15 The OLED device 800 shown in FIG. 8 may have the same Fig.13 The configuration of the OLED device 700 described above is substantially the same or similar to the configuration. Fig.14 and Fig.15 No reference will be provided Fig.13 The described elements are substantially the same or similar elements and the description is repeated.

[0147] Reference Fig.14 and Fig.15 , the OLED device 800 may include a display panel 200, a touch screen 1400, a polarizing layer 430, a cover window 415, a lower protective film 300, etc. In an exemplary embodiment, the touch screen 1400 may include a touch screen electrode 380 and an organic insulating structure 390. Here, the touch screen electrode 380 may include a first touch screen electrode 382 and a second touch screen electrode 384, and the organic insulating structure 390 may include a first organic insulating layer 392, a second organic insulating layer 394, and a third organic insulating layer 396. For example, Fig.14 The touch screen electrodes 380 in may correspond to Figure 5 In some embodiments, the touch screen electrodes 380 (including the first touch screen electrodes 382 and the second touch screen electrodes 384) shown in FIG. Fig.14 The touch screen electrodes 380 in may correspond to Figure 6 The touch screen electrodes 1380 (including the first touch screen electrodes 1382, the second touch screen electrodes 1384 and the connection pattern 1180) shown in FIG.

[0148] The second organic insulating layer 394 may be disposed on the second touch screen electrode 384. The second organic insulating layer 394 may extend in the first direction D1, may cover the second touch screen electrode 384 in the light emitting region 30, and may have a first thickness T1 in the light emitting region 30. In an exemplary embodiment, the second organic insulating layer 394 may have a second thickness T2 in the bending region 50 on the display panel 200. In certain embodiments, the second organic insulating layer 394 may have a first thickness T1 in the light emitting region 30 on the display panel 200 and a second thickness T2 in the bending region 50, and may be continuously disposed in a portion of the display region 10, the bending region 50, and the pad region 60 on the display panel 200. For example, the thickness of the second organic insulating layer 394 may be determined so that a neutral plane of the display panel 200 positioned in the bending region 50 is raised.

[0149] The OLED device 800 according to the exemplary embodiment includes an organic insulating structure 390 having a first organic insulating layer 392, a second organic insulating layer 394, and a third organic insulating layer 396, and the organic insulating structure 390 may be disposed in the bending region 50 and may be used instead of the bending protection layer of the comparative OLED device. In an embodiment in which the second organic insulating layer 394 is formed to have a second thickness T2 (which is a relatively large thickness) in the bending region 50, since the thickness of the organic insulating structure 390 in the bending region 50 may be relatively increased, the neutral plane in the bending region 50 may be easily positioned at (or above) a portion where the connection electrode 330 is disposed.

[0150] Fig.16 24 is a cross-sectional view showing an OLED device according to an exemplary embodiment. In addition to including a touch screen 2400 and an FPCB 710, Fig.16 The OLED device 900 shown in FIG. 1 may have the same Fig.14 and Fig.15 The configuration of the OLED device 800 described above is substantially the same or similar to the configuration. Fig.16 No reference will be provided Fig.14 and Fig.15 The described elements are substantially the same or similar elements and the description is repeated.

[0151] Reference Fig.16 , the OLED device 900 may include a display panel 200, a touch screen 2400, a polarizing layer 430, a cover window 415, a lower protective film 300, an FPCB 710, and the like.

[0152] The FPCB 710 may be disposed on the pad electrode 470. The FPCB 710 may be electrically connected to the external device 101 (see Figure 2 ).

[0153] The touch screen 2400 may have a first thickness T1 in the light emitting region 30 on the display panel 200 and a second thickness T2 in the bending region 50, and may be continuously formed in the display region 10, the bending region 50, and the pad region 60 on the display panel 200. In some embodiments, the touch screen 2400 may overlap a portion of the pad electrode 470 and a portion of the FPCB 710 in the pad region 60. Since the touch screen 2400 covers a portion of the FPCB 710, the FPCB 710 may not be separated from the pad electrode 470.

[0154] The terms used herein are only used for the purpose of describing specific embodiments and are not intended to limit the inventive concept. Unless the context clearly indicates otherwise, as used herein, the singular forms "a", "an" and "the" are intended to also include the plural forms. It will be further understood that when used in this specification, the terms "comprises" and / or "comprising" specify the presence of the features, wholes, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components and / or groups thereof.

[0155] Although the terms "first", "second", etc. may be used to describe various elements in this article, these elements should not be limited to these terms. These terms can be used to distinguish one element from another element. Therefore, without departing from the teaching of one or more embodiments, the first element discussed below may be referred to as the second element. Describing an element as a "first" element may not require or imply the presence of a second element or other elements. The terms "first", "second", etc. may also be used to distinguish between different categories or groups of elements in this article. For simplicity, the terms "first", "second", etc. may represent "first category (or first group), "second category (second group), etc., respectively.

[0156] As used herein, expressions such as "at least one of," "one of," and "selected from," when following a list of elements, may modify the entire list of elements rather than modifying the individual elements in the list. In addition, "may," when used in describing embodiments of the present invention, means "one or more embodiments of the present invention."

[0157] Furthermore, the terms "use," "using," and "used" may be construed as synonymous with the terms "utilize," "utilizing," and "utilized," respectively.

[0158] The terms "substantially," "about," and similar terms are used as terms of approximation rather than terms of degree, and are intended to account for the inherent variations in measured or calculated values ​​that those skilled in the art would recognize.

[0159] Although exemplary embodiments of the present invention have been described herein, it should be understood that the present invention should not be limited to those exemplary embodiments, but various changes and modifications may be made by one of ordinary skill in the art within the spirit and scope of the present invention as defined by the appended claims and their equivalents.

[0160] It will be understood that when an element is referred to as being "on," "connected to," or "coupled to" another element, the element may be directly on, directly connected to, or directly coupled to the other element, or there may also be one or more intervening elements. When an element is referred to as being directly "on," "directly connected to," or "directly coupled to" another element, there are no intervening elements. For example, when a first element is described as being "coupled to" or "connected to" a second element, the first element may be directly coupled to or connected to the second element, or the first element may be indirectly coupled to or connected to the second element via one or more intermediate elements.

[0161] In this context, "consisting essentially of" means that any additional ingredients will not substantially affect the chemical, physical, optical, or electrical properties of the corresponding layer.

[0162] The present invention can be applied to various display devices including OLED devices, for example, vehicle display devices, ship display devices, aircraft display devices, various portable communication devices, display devices for display or information transmission, medical display devices, etc.

[0163] The above is a description of exemplary embodiments and should not be construed as limiting thereof. Although several exemplary embodiments are described, it will be readily appreciated by those skilled in the art that many modifications may be made to the exemplary embodiments without substantially departing from the novel teachings and advantages of the inventive concept. Therefore, all such modifications are intended to be included within the scope of the inventive concept as defined in the claims and their equivalents. Therefore, it should be understood that the above is a description of various exemplary embodiments and should not be construed as being limited to the specific exemplary embodiments disclosed, and modifications to the disclosed exemplary embodiments as well as other exemplary embodiments are intended to be included within the scope of the appended claims and their equivalents.

Claims

1. Organic light-emitting display device, include: A display panel, comprising a display area, a pad area and a bending area, wherein the display area comprises a light emitting area and a peripheral area located around the light emitting area, the pad area is spaced apart from the display area, and the bending area is located between the display area and the pad area; and A touch screen is located on the display panel, and the touch screen includes: A plurality of touch screen electrodes are located in the display area; and an organic insulating structure covering the plurality of touch screen electrodes in the display area and extending from the display area to the bending area and the pad area in a first direction; Wherein, the display panel further includes: A fan-out wiring is arranged in the peripheral area and the pad area; a connection electrode disposed in the bending region and on the fan-out wiring; a planarization layer, disposed on the connecting electrode; and A pixel defining layer, disposed on the planarization layer; Wherein, the planarization layer and the pixel defining layer are arranged between the organic insulating structure and the connecting electrode in the bending area.

2. The organic light emitting display device according to claim 1, in, The organic insulating structure is continuous in a portion of the pad region, the display region, and the bending region on the display panel.

3. The organic light emitting display device according to claim 1, in, The plurality of touch screen electrodes include: a plurality of first touch screen electrodes extending in the first direction and a second direction opposite to the first direction, the plurality of first touch screen electrodes being spaced apart from each other in a third direction crossing the first direction and the second direction; and a plurality of second touch screen electrodes, located on the plurality of first touch screen electrodes, the plurality of second touch screen electrodes extending in the third direction and spaced apart from each other in the first direction and the second direction, wherein the plurality of first touch screen electrodes intersect with the plurality of second touch screen electrodes, and Wherein, the organic insulating structure comprises: a first organic insulating layer covering the plurality of first touch screen electrodes and extending in the first direction; and A second organic insulating layer is located on the first organic insulating layer, and the second organic insulating layer covers the plurality of second touch screen electrodes and extends in the first direction.

4. The organic light emitting display device according to claim 3, in, The organic insulating structure further comprises: a third organic insulating layer, located below the plurality of first touch screen electrodes and the first organic insulating layer, The first organic insulating layer, the second organic insulating layer and the third organic insulating layer are essentially independently composed of organic materials.

5. The organic light emitting display device according to claim 3, in, The organic insulating structure further comprises: a third organic insulating layer, located below the plurality of first touch screen electrodes and the first organic insulating layer, The second organic insulating layer has a first thickness in the light emitting region and a second thickness in the bending region, and the second thickness is greater than the first thickness.

6. The organic light emitting display device according to claim 1, in, The plurality of touch screen electrodes include: a plurality of first touch screen electrodes extending in the first direction and a second direction opposite to the first direction, the plurality of first touch screen electrodes being spaced apart from each other in a third direction intersecting the first direction and the second direction; a plurality of second touch screen electrodes located at the same level as the plurality of first touch screen electrodes, the plurality of second touch screen electrodes being spaced apart from each other in the first direction and the second direction, each of the plurality of second touch screen electrodes being located between two adjacent first touch screen electrodes among the plurality of first touch screen electrodes; and a plurality of connection patterns located at a different level from the plurality of first touch screen electrodes and the plurality of second touch screen electrodes, the plurality of connection patterns electrically connecting two second touch screen electrodes adjacent to each other in the third direction among the plurality of second touch screen electrodes, respectively; Wherein, the organic insulating structure comprises: a first organic insulating layer covering the plurality of first touch screen electrodes and the plurality of second touch screen electrodes and extending in the first direction; and A second organic insulating layer is located on the first organic insulating layer, and the second organic insulating layer covers the plurality of connection patterns and extends in the first direction.

7. The organic light emitting display device according to claim 6, in, The organic insulating structure further comprises: a third organic insulating layer, located below the plurality of first touch screen electrodes and the first organic insulating layer, The first organic insulating layer, the second organic insulating layer and the third organic insulating layer are essentially independently composed of organic materials.

8. The organic light emitting display device according to claim 1, in, The display panel further includes: substrate; A semiconductor element is located on the substrate; a light emitting structure, located in the light emitting region on the substrate; and A thin film encapsulation structure is located on the light emitting structure. Wherein, the semiconductor element comprises: An active layer, located on the substrate; a gate insulating layer covering the active layer on the substrate and extending in the first direction; A gate electrode, located on the active layer; an insulating intermediate layer covering the gate electrode on the gate insulating layer and extending in the first direction; and a source electrode and a drain electrode, located on the gate electrode, and The gate insulating layer has a first opening exposing an upper surface of the substrate in the bending region, and the insulating intermediate layer has a second opening exposing the upper surface of the substrate in the bending region.

9. The organic light emitting display device according to claim 8, The connecting electrode is located between the organic insulating structure of the touch screen and the substrate, and the connecting electrode electrically connects the light emitting structure and an external device; The organic light emitting display device further comprises: a lower protective film, located on a lower surface of the display panel opposite to the touch screen; A polarizing layer, located on the touch screen; as well as a window substrate, located on the polarizing layer, Wherein, the lower protective film comprises: A first lower protective film pattern, located in the display area; and A second lower protective film pattern is located in the pad region, Wherein, the lower surface of the display panel is exposed in the bent area.

10. The organic light emitting display device according to claim 9, in, When viewed in a fourth direction intersecting the first direction and orthogonal to the upper surface of the substrate, the curved region is curved around an axis extending along a third direction, wherein the third direction intersects the first direction and the fourth direction, and Wherein, when the bending area is bent, the second lower protection film pattern is located on a lower surface of the first lower protection film pattern in the fourth direction.

Citation Information

Patent Citations

  • Touch panel and touch panel integrated organic light emitting display device

    KR1020160048534A

  • Display apparatus and method of manufacturing the same

    KR1020170106621A

  • Display device

    US20160239133A1

  • Display device

    US20170358642A1