Semiconductor device and method for manufacturing the same

By forming a GaN field effect transistor on a SiC semiconductor substrate and using a low wettability metal layer and a polyimide wall structure, the short circuit problem caused by silver ion migration is solved and the reliability of the semiconductor device is improved.

CN110556301BActive Publication Date: 2024-10-29SUMITOMO ELECTRIC DEVICE INNOVATIONS
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201910455230.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-05-29
Publication Date
2024-10-29
Estimated Expiration
2039-05-29

AI Technical Summary

Technical Problem

Existing semiconductor devices are prone to silver ion migration problems under non-hermetic sealing packaging conditions, resulting in short circuits between the electrode pads and the backside metal film, affecting device reliability.

Method used

GaN field effect transistors are formed on a SiC semiconductor substrate and prevent silver ion migration by forming a metal layer with low wettability on the back surface, combined with a polyimide wall structure to prevent dendrite growth.

Benefits of technology

It effectively suppresses the migration of silver ions caused by the conductive adhesive, reduces the short circuit between the electrode pad and the backside metal film, and improves the reliability and stability of the semiconductor device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110556301B_ABST
    Figure CN110556301B_ABST
Patent Text Reader

Abstract

The present invention relates to a semiconductor device and a method for manufacturing the same. The semiconductor device includes a semiconductor chip in which a field effect transistor mainly containing GaN is formed on the surface of a SiC semiconductor substrate. The semiconductor device includes a metal substrate on which the back surface of the semiconductor chip is mounted through a conductive bonding material containing Ag and a resin mold configured to seal the semiconductor chip. A metal having a wettability lower than that of Au or Cu with respect to Ag is exposed in a region extending along the edge of the back surface.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority from Japanese Application No. JP2018-103823 filed on May 30, 2018, and JP2019-035716 filed on February 28, 2019, the entire contents of which are hereby incorporated by reference. Technical Field

[0003] The present disclosure relates to a semiconductor device and a method for manufacturing the same. Background Art

[0004] Japanese Unexamined Patent Publication No. 2013-093491 discloses a semiconductor device including a conductive substrate, a first adhesive disposed on the conductive substrate and containing a conductive metal component, and a semiconductor chip disposed on the first adhesive and bonded to the conductive substrate. In order to suppress migration due to the first adhesive, an example is disclosed in which a second adhesive not containing a conductive metal component is disposed on the conductive substrate, on the periphery of the bonding surface between the semiconductor chip and the conductive substrate. The second adhesive coats the first adhesive.

[0005] The source electrode disposed on the surface of the semiconductor chip in which the field effect transistor (FET) is formed is connected to the back electrode through a through hole formed in the substrate. The back electrode is disposed on the entire back surface of the semiconductor chip. The die mounting of the semiconductor chip on the package is performed by connecting the entire back electrode to the package via a soldering material (conductive resin such as silver paste, also referred to as a conductive adhesive material).

[0006] In the case of a non-hermetic sealed package, it is impossible to suppress the entry of moisture into the package. Therefore, by the presence of moisture in the side wall portion of the semiconductor chip, the ionization of silver (Ag) in the solder material is accelerated. In addition, the silver ions (Ag + ) is attracted to the electrode. That is, the so-called silver ion electromigration (climbing up the conductive adhesive, also called ion migration) is generated. Ion migration is a phenomenon in which ionized metal moves on the surface of a substance between electric fields. Metal ions are attracted to the electric field, reduced from an ionized state to a metal for some reason, and accumulate to form dendrites. When metal dendrites grow from the conductive adhesive material, the electrode pad and the back metal film are short-circuited, causing failure of the semiconductor device.

[0007] In the semiconductor device disclosed in Japanese Unexamined Patent Publication No. 2013-093491, migration is suppressed by curing the surface of the first adhesive containing the conductive metal component with the second adhesive not containing the conductive metal component. However, in order to cure the exposed surface of the first adhesive as the adhesive resin, another resin (i.e., the second adhesive) is required. Moreover, two heating processes are required for the coating process. In addition, it is not easy to apply an appropriate amount of the second adhesive only around the chip. Summary of the invention

[0008] A method for manufacturing a semiconductor device according to one aspect of the present invention includes: forming a field effect transistor mainly including GaN on a surface of a SiC semiconductor substrate, forming a formation region for a semiconductor chip in the field effect transistor, the formation region being divided by a scribe line having a first width; forming a first metal layer on the entire back surface of the SiC semiconductor substrate, wherein the first metal layer has a wettability with respect to Ag lower than that of Au or Cu; forming a second metal layer made of Au on a first region of the first metal layer, the first region not overlapping the scribe line; individualizing the semiconductor chips by dicing the SiC semiconductor substrate along the scribe line with a second width narrower than the first width; and mounting the semiconductor chips on a metal base by a conductive adhesive member containing Ag.

[0009] A semiconductor device according to one aspect of the present disclosure includes a semiconductor chip, in which a field effect transistor mainly containing GaN is formed on the surface of a SiC semiconductor substrate. The semiconductor device includes: a metal substrate on which the back surface of the semiconductor chip is mounted through a conductive adhesive material containing Ag; and a resin mold configured to seal the semiconductor chip, wherein a metal having a wettability lower than that of Au or Cu with respect to Ag is exposed in a region extending along an edge of the back surface.

[0010] A method for manufacturing a semiconductor device according to one aspect of the present disclosure includes: arranging electrode pads along a scribe area on a main surface of a substrate, the substrate having a plurality of device areas on the main surface surrounded by the scribe area; forming a back metal film on a back surface of the substrate, the back metal film being spaced apart from a first area in which the scribe area is projected onto the back surface; forming a polyimide wall extending along an edge of the back metal film on a second area between the first area and the back metal film; and cutting the substrate along the scribe area to produce semiconductor chips each including a device area.

[0011] A semiconductor device according to one aspect of the present disclosure includes: a substrate having a main surface and a back surface, the main surface including a device area; an electrode pad arranged on the main surface along the side of the substrate; a back metal film arranged on the back surface, the back metal film being spaced apart from the side of the substrate; and a polyimide wall, the polyimide wall being arranged on the back surface between the side of the substrate and the back metal film, the polyimide wall extending along the edge of the back metal film. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] The foregoing and other objects, aspects and advantages will be better understood from the following detailed description of preferred embodiments of the present invention with reference to the accompanying drawings, in which:

[0013] Figure 1A is an external view of the semiconductor device according to the first embodiment as viewed from the front side (upper side), and Figure 1B is an external view of the semiconductor device shown in FIG. 1 as viewed from the back side (lower side);

[0014] Figure 2 is a cross-sectional view of a semiconductor device of a first embodiment;

[0015] Figure 3 is a plan view showing an example of a semiconductor chip mounted on a semiconductor device according to the first embodiment;

[0016] Figure 4 is a cross-sectional view of a semiconductor chip mounting portion of a semiconductor device according to a first embodiment;

[0017] Figure 5 is a diagram showing a manufacturing flow of a semiconductor device according to a first embodiment;

[0018] Figures 6A to 6H are diagrams for explaining respective steps in a manufacturing flow of a semiconductor device according to a first embodiment;

[0019] Figures 7A to 7C are diagrams for explaining respective steps in a manufacturing flow of a semiconductor device according to a second embodiment;

[0020] Figure 8 is a plan view showing a configuration of a transistor 1A as an example of a semiconductor device according to the third embodiment;

[0021] Fig. 9 is a bottom view of transistor 1A;

[0022] Fig.10 It is along Figure 8 A cross-sectional view taken along line XX in FIG.

[0023] Fig.11 It is along Figure 8 A cross-sectional view taken along line XI-XI;

[0024] Fig.12 It is along Figure 8 A cross-sectional view taken along line XII-XII;

[0025] Fig.13A is a plan view showing the main surface 3a of the wafer-like substrate 3, and Fig. 13B is a bottom view showing the back surface 3b of the wafer-like substrate 3;

[0026] Figures 14A to 14C is a cross-sectional view showing the first half of the various steps included in the method of manufacturing the transistor 1A;

[0027] Figures 15A to 15C is a cross-sectional view showing the first half of the steps included in the method of manufacturing the transistor 1A;

[0028] Figures 16A to 16C is a cross-sectional view showing the first half of the steps included in the method of manufacturing the transistor 1A;

[0029] Figures 17A to 17C is a cross-sectional view showing the first half of the steps included in the method of manufacturing the transistor 1A;

[0030] Figures 18A to 18C is a cross-sectional view showing the first half of the steps included in the method of manufacturing the transistor 1A.

[0031] Figures 19A to 19C is a cross-sectional view showing the latter half of the steps included in the method of manufacturing the transistor 1A;

[0032] Figures 20A to 20C is a cross-sectional view showing the latter half of the steps included in the method of manufacturing the transistor 1A;

[0033] Figures 21A to 21C is a cross-sectional view showing the latter half of the steps included in the method of manufacturing the transistor 1A;

[0034] Figures 22A to 22C is a cross-sectional view showing the latter half of the steps included in the method of manufacturing the transistor 1A;

[0035] Fig.23A and 23B is a cross-sectional view showing the latter half of the steps included in the method of manufacturing the transistor 1A;

[0036] Fig.24A and 24B is a view showing a modification of a polyimide wall; and

[0037] Fig.25 is a plan view showing the configuration of a semiconductor device 500 according to the fourth embodiment. DETAILED DESCRIPTION

[0038] [Description of Embodiments of the Present Disclosure]

[0039] First, embodiments of the present disclosure will be listed and described.

[0040] A method for manufacturing a semiconductor device according to an embodiment of the present disclosure includes forming a field effect transistor mainly composed of GaN on a surface of a semiconductor substrate, wherein a formation area for a semiconductor chip is formed, the formation area is divided by a scribe line having a predetermined width, and the semiconductor substrate is made of SiC; a first metal layer is formed on the entire back surface of the semiconductor substrate, wherein the first metal layer has a wettability with respect to Ag lower than that of Au or Cu; a second metal layer made of Au is formed on an area of ​​the first metal layer, the area excluding an area inside a predetermined width of the scribe line; individualizing the semiconductor chips by dicing the semiconductor substrate along the scribe line with a width narrower than the predetermined width; and mounting the semiconductor chips on a metal base by a conductive adhesive member containing Ag.

[0041] According to this method of manufacturing a semiconductor device, it is possible to suppress ion migration caused by the conductive adhesive without hardening the surface of the conductive bonding member containing Ag, which corresponds to the conductive bonding material.

[0042] In an embodiment, the method may further include molding the semiconductor chip mounted on the metal substrate with a sealing resin. In this case, the semiconductor chip mounted on the semiconductor device can be protected from impact, light, heat, etc.

[0043] In an embodiment, the metal of the first metal layer may be NiCr, Ti or Ta. The above metals have a wettability with respect to Ag that is lower than that of Au or Cu. Therefore, even if the Ag contained in the conductive adhesive member disposed on the entire surface of the back electrode is ionized and the silver ions move toward the negative electrode, the silver ions cannot reach the negative electrode by traveling along the side wall of the semiconductor chip.

[0044] In an embodiment, forming the first metal layer may sequentially include continuously forming the first metal layer and the second metal layer by sputtering for the entire back surface of the semiconductor substrate; forming the second metal layer by performing selective plating on an area other than an area inside a predetermined width of the scribe line, wherein the first metal layer and the second metal layer formed by sputtering are considered to be seed metals; and removing the second metal layer formed by sputtering in an area inside the predetermined width of the scribe line. In this case, the second metal layer can be formed with good adhesion via the first metal layer on the back surface of the semiconductor substrate made of SiC. In addition, by removing the second metal layer in an area inside the predetermined width of the scribe line, the first metal layer can be exposed in an area around the back surface of the semiconductor chip.

[0045] In an embodiment, forming the first metal layer may include, in sequence, continuously forming the first metal layer and the second metal layer by sputtering for the entire back surface of the semiconductor substrate; forming the second metal layer by performing selective plating on an area other than an area inside the predetermined width of the scribe, wherein the first metal layer and the second metal layer formed by sputtering are considered to be seed metals, and further forming the first metal layer in an area inside the predetermined width of the scribe. In this case, it is possible to form the second metal layer with good adhesion via the first metal layer on the back surface of the semiconductor substrate made of SiC. In addition, by forming the first metal layer in the inner area of ​​the predetermined width of the scribe, the first metal layer can be exposed in the area around the back surface of the semiconductor chip.

[0046] A semiconductor device according to an embodiment of the present disclosure includes a semiconductor chip in which a field effect transistor mainly composed of GaN is formed on the surface of a semiconductor substrate made of SiC. The semiconductor device includes: a metal substrate on which the back surface of the semiconductor chip is mounted through a conductive adhesive member containing Ag; and a resin molding member configured to seal the semiconductor chip, wherein a metal having a wettability with respect to Ag lower than that of Au or Cu is exposed in an area around the back surface of the semiconductor chip.

[0047] According to this semiconductor device, it is possible to suppress ion migration caused by the conductive adhesive without hardening the surface of the conductive adhesive member containing Ag, which corresponds to the conductive adhesive material.

[0048] In an embodiment, the metal having a wettability lower than that of Au or Cu with respect to Ag may be NiCr, Ti or Ta. The above metals have a wettability lower than that of Au or Cu with respect to Ag. Therefore, even if Ag contained in the conductive adhesive member disposed on the entire surface of the back electrode is ionized and the silver ions move toward the negative electrode, the silver ions cannot reach the negative electrode by traveling along the side wall of the semiconductor chip.

[0049] In an embodiment, the metal with lower wettability may be exposed around the semiconductor chip with a width of 20 to 30 μm. By setting the width of the metal with lower wettability to at least 20 to 30 μm, migration of the conductive adhesive member containing Ag can be reliably suppressed.

[0050] A method for manufacturing a semiconductor device according to an embodiment of the present disclosure includes: arranging electrode pads along a scribe line area on a main surface of a substrate, the substrate having a plurality of device areas on the main surface surrounded by the scribe line area; forming a back metal film on the back surface of the substrate spaced apart from a first area in which the scribe line area is projected on the back surface; forming a polyimide wall extending along an edge of the back metal film on a second area between the first area and the back metal film; and cutting the substrate along the scribe line area to produce a plurality of semiconductor chips, each semiconductor chip including a device area.

[0051] In this manufacturing method, a back metal film is disposed on a back surface, spaced apart from a first region in which a scribed region is projected on the back surface. In addition, a polyimide wall extending along an edge of the back metal film is disposed on a second region between the first region and the back metal film. For example, when the back metal film of a semiconductor chip is bonded to another member via a conductive adhesive material, the growth of dendrites from the conductive adhesive material is suppressed by the polyimide wall. Therefore, it is possible to reduce a short circuit between the back metal film and the electrode pad caused by ion migration of a metal contained in the conductive adhesive material.

[0052] In an embodiment, forming the polyimide wall may include forming a polyimide wall spaced apart from the first region, wherein the back surface of the substrate may be exposed between the side of the substrate of each semiconductor chip and the polyimide wall of the semiconductor chip. In this case, the polyimide wall is reliably formed directly on the back surface of the substrate.

[0053] In an embodiment, the distance between the side of the substrate and the polyimide wall may be at least 100 μm. Therefore, even if a conductive bonding member such as a sintered metal type silver paste climbs up the polyimide wall, there is still a distance of at least 100 μm to the electrode pad. Therefore, the possibility of a short circuit between the back metal film and the electrode pad is reduced.

[0054] In an embodiment, the width in the direction orthogonal to the extending direction of the polyimide wall may be in the range of 50 to 100 μm. In this case, the growth of dendrites from the conductive adhesive material can be sufficiently suppressed.

[0055] In an embodiment, the semiconductor chip may be a field effect transistor, the planar shape of the semiconductor chip may be a rectangle, the gate pad as an electrode pad may be arranged along one side of a pair of sides facing each other of the rectangle and the drain pad may be arranged along the other side of the pair of sides, and wherein forming the polyimide wall may include forming the polyimide wall along at least one side. By forming the polyimide wall along one side where the gate pad is arranged, the short circuit between the gate pad and the back metal film can be effectively reduced.

[0056] In an embodiment, forming the polyimide wall may further include forming the polyimide wall along the other side. Although ion migration does not occur on the drain pad side, because the conductive bonding member does not protrude from the transistor, another circuit component can be arranged at a position closest to the transistor. In other words, the limitation of the mounting area based on the protrusion of the conductive bonding member can be reduced. In addition, by arranging other circuit components closest to the transistor, the degradation of high-frequency characteristics can be suppressed.

[0057] In an embodiment, forming the polyimide wall may further include forming the polyimide wall along the other pair of sides connected to the one pair of sides of the rectangle, thereby suppressing the growth of dendrites near the other pair of sides and more effectively reducing the short circuit between the gate pad and the backside metal film.

[0058] In an embodiment, the polyimide wall formed along the other pair of sides may have discontinuity. For example, when the polyimide wall is formed by screen printing, a mask located inside the polyimide wall can be supported.

[0059] In an embodiment, the method may further include mounting the semiconductor chip on the substrate having the metal surface using a conductive adhesive material including Ag.

[0060] The semiconductor device according to the embodiment of the present disclosure includes: a substrate having a main surface including a device region and a back surface; an electrode pad disposed on the main surface along the side of the substrate; a backside metal film disposed on the back surface spaced apart from the side of the substrate; and a polyimide wall disposed on the back surface between the side of the substrate and the backside metal film and extending along the edge of the backside metal film. Therefore, the semiconductor device may also include: a metal surface base having a substrate mounted thereon; and a conductive adhesive material containing Ag, the conductive adhesive material being inserted between the backside metal film and the surface of the substrate.

[0061] Details of the embodiments of the present disclosure

[0062] Specific examples of semiconductor devices and methods for manufacturing the same according to embodiments of the present disclosure will be described below with reference to the accompanying drawings. Note that the present disclosure is not limited to these illustrations, is shown by the claims, and is intended to include all modifications within the meaning and scope equivalent to the claims. In addition, the present disclosure includes any combination of embodiments as long as the combination is possible for multiple embodiments. Note that in the description of the drawings, the same elements are represented by the same reference numerals, and repeated explanations are omitted.

[0063] (Semiconductor Device According to First Embodiment)

[0064] Figure 1A is an external view of the semiconductor device according to the first embodiment as viewed from the front side (upper side), and Figure 1B As viewed from the back (lower side) Figure 1A External view of the semiconductor device shown in . Figure 2 1 is a cross-sectional view of a semiconductor device according to the first embodiment. The semiconductor device 100 according to the first embodiment is provided with a chip carrier type package having 6-pin electrodes 130, and is constituted by a resin package except for a metal base 110 on the bottom surface.

[0065] like Figure 2 As shown in , the semiconductor device 100 includes a metal substrate 110, a semiconductor chip 200, and an input / output matching circuit 400. The semiconductor chip 200 and the input / output matching circuit 400 are mounted on the metal substrate 110 made of copper (Cu). The semiconductor chip 200 and the input / output matching circuit 400 are connected by a bonding wire 140. The semiconductor chip 200 and the input / output matching circuit 400 are mounted on the metal substrate 110 via a conductive adhesive member 150 (hereinafter referred to as a "silver-containing adhesive member") containing silver (Ag) as a conductive resin. As the Ag-containing adhesive member 150, a material in which an Ag filler is mixed in a resin, a silver solder containing Ag, Cu, and zinc (Zn) as main components, or the like is used.

[0066] The semiconductor device 100 includes a sidewall member 120 and an electrode 130. The resin sidewall member 120 surrounding the metal substrate 110 is provided in the semiconductor device 100. The electrode 130 is formed on the outer surface of the sidewall member. The electrode 130 is electrically connected to the wiring formed on the bottom of the inner surface of the sidewall. More specifically, the electrode 130 on the outer surface is formed by plating the surface of the groove in the resin of the sidewall member 120. In addition, the wiring on the inner surface of the sidewall and the input / output matching circuit 400 are also connected by the bonding wire 140. The inside surrounded by the sidewall member 120 is filled with resin 160, whereby the semiconductor chip 200 and the input / output matching circuit 400 are sealed by the resin. Therefore, the semiconductor chip 200 is molded by the sealing resin.

[0067] Figure 3 2 is a plan view showing an example of a semiconductor chip mounted on a semiconductor device according to the first embodiment. The semiconductor chip 200 is an example of a field effect transistor (FET). For example, a GaN epitaxial layer 211 made of gallium nitride (GaN) is formed on the surface of a silicon carbide (SiC) substrate 201 described later, and the surface of the GaN epitaxial layer 211 is covered with an insulating layer 212. In addition, a drain electrode 240 and a source electrode 220 are arranged with a finger gate electrode 230 included in the semiconductor chip 200 inserted between the drain electrode 240 and the source electrode 220. The drain electrode 240 is gathered at Figure 3 The source electrode 220 is gathered on the source pad 221 in the lower part of the figure. In addition, the gate electrode 230 is gathered on the drain pad 241 in the upper part of the figure. Figure 3 The source pad 221 is in contact with the GaN epitaxial layer 211 through an opening formed in the insulating film 212. The gate pad 231 and the drain pad 241 may be formed on the insulating film 211, or may be formed to be in contact with the GaN epitaxial layer 211, like the source pad 221. In the GaN epitaxial layer 211, the peripheral area of ​​the semiconductor chip 200 that does not overlap with the electrode is deactivated.

[0068] In the first embodiment, Figure 3 In the lower part, two source pads 221 sandwich the gate pad 231. In this example, the source electrode 220 is coupled to the source pad 221 individually, but the present invention is not limited to this. For example, as a wire from the source electrode 220 to the source pad 221, a wire commonly connected between the source electrode 220 and the source pad 221 can be provided. In addition, although the source pad 221 and the gate pad 231 are set to the same size, the present invention is not limited to this. From the viewpoint of reducing the gate capacitance, the source pad 221 can be set wide and the gate pad 231 can be set narrow.

[0069] In a high frequency device, from the viewpoint of reducing the image capacitance between the gate and the drain and performing high-speed switching, the drain electrode 240 and the gate electrode 230 face each other across the device active region (the region where each electrode is located). In the planar arrangement of the semiconductor chip 200, the distance between the edge of the gate pad 231 and the edge of the semiconductor chip 200 is set to, for example, 50 to 70 μm.

[0070] Figure 4 is a cross-sectional view of a semiconductor chip mounting portion in the semiconductor device according to the first embodiment. Figure 4 Shown along Figure 32 is a cross section taken along line IV-IV of semiconductor chip 200 shown in FIG. In semiconductor chip 200 , as described above, GaN epitaxial layer 211 is formed on the surface of SiC substrate 201 , and source pad 221 and gate pad 231 are formed on the surface of GaN epitaxial layer 211 . Figure 4 The structure shown in FIG. 2 is an example in which the gate pad 231 is formed to be in contact with the GaN epitaxial layer 211. The source pad 221 is electrically connected to a back electrode 260 made of Au (gold) formed substantially on the entire back surface of the semiconductor chip 200 through a through hole 250 formed in the SiC substrate 201. In the semiconductor chip 200, the entire back electrode 260 is die-bonded on the metal base 110 through the bonding member 150 containing Ag.

[0071] Most conventional semiconductor chips, including those used for high frequency use, are devices mainly made of gallium arsenide (GaAs). In addition, laterally diffused metal oxide semiconductors (Si-LDMOS) are also partially used as high frequency devices. From the perspective of the withstand voltage of a semiconductor chip whether it is made of GaAs or silicon (Si), the maximum value of the bias voltage applied to the gate (the maximum value of the negative bias voltage relative to the source potential) is generally negative several volts. However, with the promotion of the application of wide-gap GaN-based materials as shown in the first embodiment as semiconductor materials, the negative maximum value of the gate bias can be set large.

[0072] Here, the resin package has almost no effect of suppressing the ingress of moisture into the package. Therefore, the presence of the resin package is hardly considered in terms of water blocking capability in the field of semiconductor devices. As a result, Ag contained in the adhesive resin as a filler tends to react with moisture to accelerate ionization (Ag + ). When a negative bias is applied to the gate, the ionized silver ions Ag in the binding resin + The ions may climb up the side of the semiconductor chip 200 toward the gate pad 231 and may reach the gate pad 231. That is, so-called ion migration occurs.

[0073] In order to solve this problem, in the first embodiment, a metal having a wettability lower than that of Au or Cu with respect to Ag is exposed in an area around the back surface of the semiconductor chip 200. Nickel chromium (NiCr), titanium (Ti), and tantalum (Ta) are considered as metals having a wettability lower than that of Au or Cu with respect to Ag. Figure 4 In the example shown in , a NiCr layer 251 is formed between the SiC substrate 201 and the back electrode 260. In addition, instead of Au forming the back electrode 260, the NiCr layer 251 is exposed in the area around the back surface of the semiconductor chip 200. The area around the back surface of the semiconductor chip 200 corresponds to an area located at and near the edge of the back surface.

[0074] As a result, the Ag-containing adhesive member 150 closely adheres to the Au forming the back electrode 260, but tends to be repelled by the NiCr layer 251. Therefore, the Ag-containing adhesive member 150 is less likely to exist in the area around the back surface of the semiconductor chip 200. The ionized silver ions Ag in the Ag-containing adhesive member 150 + It is unlikely to climb up the side of the semiconductor chip 200 toward the gate pad 231. This is because Ag + Due to Ag + The NiCr layer 251 is not easily moved on the surface of the NiCr layer 251 due to the low wettability between the NiCr layer 251 and the NiCr layer 251. Therefore, migration can be suppressed. From the viewpoint of reliably suppressing migration, the NiCr layer 251 formed on the area around the back surface of the semiconductor chip 200 may be exposed with a width of 20 to 30 μm.

[0075] (Method of Manufacturing Semiconductor Device According to First Embodiment)

[0076] Next, a method of manufacturing the semiconductor device according to the first embodiment will be described. Figure 5 is a diagram showing a manufacturing flow of a semiconductor device according to a first embodiment, and Figures 6A to 6H 1 and 2 are diagrams for explaining respective steps in a manufacturing flow of the semiconductor device according to the first embodiment. Fig. 6A The through hole forming process is shown. Figure 6B The metal layer formation process is shown. Figure 6C shows the photoresist formation process, Fig.6D The back electrode formation process is shown. Fig. 6E shows the photoresist removal process, Fig. 6F The etching process is shown. Figure 6G shows the dicing process, and Figure 6H Note that in these drawings, for simplicity, only the portion around the source pad 221 of the semiconductor chip 200 is schematically shown.

[0077] (Pretreatment process)

[0078] First, in the pre-treatment process of step S1, a GaN epitaxial layer 211 is formed on the surface of the SiC substrate 201. Subsequently, FETs that will become a plurality of semiconductor chips 200 are manufactured on the GaN epitaxial layer 211. Figure 3As shown in , a source region and a drain region are formed in a GaN epitaxial layer 211 by doping. Subsequently, an insulating layer 212, a source electrode 220, a drain electrode 240, and a gate electrode 230 are provided on the surface of the GaN epitaxial layer 211. These electrodes are connected to a source pad 221, a drain pad 241, and a gate pad 231, respectively, and as a result, a FET is manufactured. Each of the plurality of semiconductor chips is divided by a scribe line having a predetermined width.

[0079] (Through-hole formation process)

[0080] Next, in step S2, Fig. 6A As shown in , a wafer having a plurality of FETs formed thereon is provided on a glass support substrate 300. For example, the FET forming surface, that is, the GaN epitaxial layer 211 side, is attached to the glass support substrate 300 by an adhesive 310. Thereafter, the SiC substrate 201 is ground to thin the wafer thickness to about 100 μm. After grinding, a through hole 250 is formed from the back surface of the wafer toward the source pad 221. The respective electrodes or pads of the FET are formed on the GaN epitaxial layer 211 in the wafer. When the SiC substrate 201 and the GaN epitaxial layer 211 are etched to form the through hole 250, the metal of the source pad 221 is used as a stop layer.

[0081] (Metal layer formation process)

[0082] Next, in step S3, Figure 6B As shown in FIG. 2 , after forming a through hole 250 in a SiC substrate 201, a NiCr layer 251 and an Au layer 252 are formed on the entire back surface of the SiC substrate 201 by sputtering. The thickness of the NiCr layer 251 is, for example, about 100 nm, and the thickness of the Au layer 252 is also, for example, about 100 nm. The NiCr layer 251 corresponds to a first metal layer having a wettability lower than that of Au or Cu with respect to Ag in the present disclosure.

[0083] (Photoresist Formation Process)

[0084] Next, in step S4, Figure 6C As shown in FIG. 2 , a photoresist 270 having a pattern covering a scribe line is formed on the Au layer 252. The photoresist 270 is not provided in the through hole 250 formed in the previous step. The thickness of the photoresist 270 is set according to the thickness of Au by plating in the next step. Here, the scribe line is a line that divides the area of ​​the semiconductor chip formed on the wafer. By setting the scribe line, a predetermined width is set between adjacent semiconductor chips. In the present disclosure, this width is referred to as the scribe line width. In the first embodiment, the width of the scribe line is determined by Figure 6CThe width D1 in FIG. 2 indicates that the width of the photoresist 270 is equal to the width D1 of the scribe line. Therefore, the photoresist 270 is formed in a grid shape having a width D1 on the back surface of the wafer.

[0085] (Back electrode formation process)

[0086] Next, in step S5, Fig.6D As shown in FIG. 2 , the Au layer 261 is formed by selective electrolytic plating on the area not covered by the photoresist 270, wherein the NiCr layer 251 and the Au layer 252 formed by sputtering are regarded as seed metals. In this case, the Au layer 261 is also formed in the through hole 250 exposed to the photoresist 270. The Au layer 261 is used as the back electrode 260 to be described later. The Au layer 261 corresponds to the second metal layer in the present disclosure.

[0087] (Photoresist removal process)

[0088] Next, in step S6, Fig. 6E As shown in FIG. 6 , an Au layer 261 is formed on the back surface of the SiC substrate 201 by electrolytic selective plating, and then the photoresist 270 is removed. The photoresist 270 is provided with a width D1 of the scribe line of the semiconductor chip 200. Therefore, after step S6, a rectangular island of a thick Au layer 261 formed by plating and a lattice of a thin Au layer 252 formed by sputtering appear on the back surface of the SiC substrate 201 from which the photoresist 270 has been removed. The width of the grid is the width D1.

[0089] (Etching process)

[0090] Next, in step S7, Fig. 6F As shown in , the Au layer 252 and the Au layer 261 on the back surface of the SiC substrate 201 are removed by wet etching using a KI solution (potassium iodide solution) as an etchant. In this case, the Au layer 252 formed as a seed metal is completely removed because it is much thinner than the Au layer 261 formed by plating. Therefore, the NiCr layer 251 located below the Au layer 252 is exposed with a lattice of width D1. In addition, the Au layer 261 formed by plating is also etched to have a predetermined thickness.

[0091] (Dicing process)

[0092] Next, the glass support substrate 300 is removed from the Fig. 6FThe wafer of the process shown in FIG. 1 is formed by a wafer 200 of the process shown in FIG. 2 and the back surface of the SiC substrate 201 is cleaned. The extension tape 320 is attached to the back surface of the SiC substrate 201. Since the back electrode 260 made of the Au layer 261 is formed on substantially the entire back surface of the SiC substrate 201, the extension tape 320 is attached to the back electrode 260. Thereafter, in step S8, dicing is performed as shown in FIG. Figure 6G , to obtain individual semiconductor chips 200. Here, scribing is performed along the scribe line, for example, within the width D1 of the scribe line using a scribe blade having a width D2 narrower than the width D1 of the scribe line. Therefore, the back electrode 260 made of Au does not exist in the width D1 of the scribe line on the back surface of the SiC substrate 201, and the NiCr layer 251 is exposed. When scribing using a laser is performed, scribing is performed with a width D2 narrower than the width D1 of the scribe line. In the first embodiment, the width D1 of the scribe line and the width D2 of the scribe are determined so that the width of the remaining NiCr layer 251 is, for example, 20 to 30 μm. The width of the remaining NiCr layer 251 corresponds to (D1-D2) / 2.

[0093] (Die bonding process)

[0094] Next, in step S9, Figure 6H As shown in FIG. 1 , the semiconductor chip 200 is separated from the expansion tape 320, thereby individualizing the semiconductor chip 200. In addition, the individual semiconductor chips 200 are die-bonded to the metal substrate 110 using the Ag-containing adhesive member 150. The NiCr layer 251 is exposed in a region around the back surface of the semiconductor chip 200 with a width of 20 to 30 μm. Therefore, even if the semiconductor chip 200 is die-bonded with the Ag-containing adhesive member 150, the Ag-containing adhesive member 150 does not expand in the region where the NiCr layer 251 is exposed on the semiconductor chip 200, and the NiCr layer 251 may remain exposed. Therefore, Ag is suppressed. + Climb up the side surface of the semiconductor chip 200 .

[0095] (Packaging process)

[0096] After the above process, in step S10, Figure 2 As shown in FIG. 1 , the input / output matching circuit 400 is die-bonded on the metal substrate 110. The semiconductor chip 200 and the input / output matching circuit 400 are connected by bonding wires 140. Furthermore, resin sealing is performed using the resin sidewall member 120 and the resin 160. Thus, the packaged semiconductor device 100 is obtained.

[0097] (Semiconductor device and manufacturing method thereof in second embodiment)

[0098] Next, a semiconductor device and a method for manufacturing the same according to a second embodiment will be described. Figures 7A to 7C is a diagram for explaining each step in a manufacturing flow of a semiconductor device according to a second embodiment, and Fig. 7A The metal layer formation process is shown. Figure 7B shows the dicing process, and Figure 7C The bonding process is shown. Figure 5 The semiconductor manufacturing method according to the second embodiment is obtained by replacing the etching process of step S7 with the metal layer forming process of step S11 in the manufacturing process of the semiconductor device of the first embodiment shown in FIG. Therefore, the manufacturing method of the second embodiment includes the following steps: Figure 5 Steps S1 to S6, step S11 and steps S8 to S10 shown in .5.

[0099] (Metal layer formation process)

[0100] In the method for manufacturing a semiconductor device according to the second embodiment, after completing Figure 5 After the photoresist removal process shown in step S6, the Au layer 252 formed by sputtering will not be Fig. 6E 7 , a NiCr layer 253 is further formed on the Au layer 252 within the width D1 of the scribe line. As a result, the region within the width D1 of the scribe line has a three-layer metal configuration of the NiCr layer 251, the Au layer 252, and the NiCr layer 253 in this order from the SiC substrate 201 side.

[0101] (Dicing process)

[0102] The method of forming the NiCr layer 253 within the width D1 of the scribe line includes, for example, the following method. First, a NiCr layer having a thickness of about 100 nm is formed on the entire back surface of the SiC substrate 201 by sputtering. Next, a photoresist covering about 10 μm around the width D1 of the scribe line and its width direction is formed by patterning. The exposed NiCr layer is removed by reactive ion etching or trimming using a chlorine-based gas as a reactive gas. Therefore, the Au layer 261 in the area corresponding to the back electrode 260 can be exposed, and the NiCr layer 253 can be left within the width D1 of the scribe line. In the manufacturing method according to the second embodiment, the plated Au layer 261 is not etched. Therefore, the thickness of the Au layer 261 can be set to a predetermined thickness in advance in the back electrode formation process of step S5.

[0103] (Die bonding process)

[0104] Next, the glass support substrate 300 is removed from the Fig. 7AThe wafer of the process shown in FIG. 1 is prepared, and the back surface of the SiC substrate 201 is cleaned. Thereafter, the extension tape 320 is attached. The back electrode 260 made of the Au layer 261 is formed substantially on the entire back surface of the SiC substrate 201. Therefore, the extension tape 320 is attached to the back electrode 260. Thereafter, in step S8, dicing is performed, as shown in FIG. Figure 7B , to obtain individual semiconductor chips 200 . Here, dicing is performed along the scribe line using a dicing blade having a width D2 narrower than the width D1 of the scribe line. Therefore, the NiCr layer 253 is exposed in the width D1 of the scribe line on the back surface of the SiC substrate 201 .

[0105] Next, in step S9, Figure 7C As shown in FIG. 1 , the semiconductor chip 200 is separated from the expansion tape 320, thereby individualizing the semiconductor chip 200. In addition, the individual semiconductor chip 200 die is bonded to the metal substrate 110 using the Ag-containing bonding member 150. The NiCr layer 253 is exposed in a region around the back surface of the semiconductor chip with a width of 20 to 30 μm. Therefore, even if the semiconductor chip 200 is die-bonded with the Ag-containing bonding member 150, the Ag-containing bonding member 150 does not expand in the region where the NiCr layer 253 is exposed in the semiconductor chip 200, and the NiCr layer 253 may remain exposed. Therefore, Ag is suppressed. + Climb up the side of the semiconductor chip 200. The subsequent packaging process is the same as the method of manufacturing the semiconductor device according to the first embodiment.

[0106] (Third Embodiment)

[0107] Figure 8 1 is a plan view showing the configuration of a field effect transistor (hereinafter simply referred to as a transistor) 1A as an example of a semiconductor device according to the third embodiment. Fig. 9 is a bottom view of transistor 1A. Fig.10 It is along Fig.10 Cross-sectional view taken along line XX. Fig.11 It is along Figure 8 A cross-sectional view taken along line XI-XI. Fig.12 It is along Figure 8 As shown in these figures, the transistor 1A includes a substrate 3, insulating films 5 to 9, a gate electrode 21, a source electrode 22, a drain electrode 23, a gate pad 31, a source wiring 32, a drain wiring 33, a field plate 35 (see Fig.12 ), metal vias 44 (see Fig.10 ), back metal film 45 and polyimide wall 46A. Figure 8 In this figure, the insulating films 5 to 9 are not shown.

[0108] The substrate 3 is a plate-like member with a rectangular planar shape, and has a flat main surface 3a and a flat back surface 3b opposite to the main surface 3a. In addition, the substrate 3 has a pair of side faces 3d and 3e and a pair of side faces 3f and 3g. A pair of side faces 3d and 3e face each other in any direction X along the main surface 3a, and extend along the direction Y intersecting (e.g., orthogonal) the X direction. In addition, a pair of side faces 3f and 3g face each other in the Y direction, and connect a pair of side faces 3d and 3e extending along the X direction. When observed in the normal direction of the main surface 3a, a pair of side faces 3d and 3e form a pair of side faces of the rectangular substrate 3, and a pair of side faces 3f and 3g form another pair of side faces of the rectangular substrate 3 connecting a pair of side faces.

[0109] The substrate 3 includes a growth substrate 30 and a nitride semiconductor layer 4 formed on the growth substrate 30. The growth substrate 30 is, for example, a SiC substrate, and includes a back surface 3b. The growth substrate 30 is used for epitaxial growth of the nitride semiconductor layer 4.

[0110] The nitride semiconductor layer 4 is an epitaxial layer formed on the growth substrate 30. The nitride semiconductor layer 4 constitutes the main surface 3a of the substrate 3. When the transistor 1A is a high electron mobility transistor (HEMT), the nitride semiconductor layer 4 includes, for example, an AlN buffer layer in contact with the main surface 3a, a GaN channel layer disposed on the AlN buffer layer, an AlGaN (or InAlN) barrier layer disposed on the GaN channel layer, and a GaN capping layer disposed on the barrier layer. The AlN buffer layer is undoped, and its thickness is, for example, in the range of 10 to 20 nm. The GaN channel layer is undoped, and its thickness is, for example, in the range of 0.4 to 1.2 μm. The thickness of the barrier layer is, for example, in the range of 10 to 30 nm. However, in the case of the InAlN barrier layer, the thickness is set to be less than 20 nm. The GaN capping layer is n-type, and its thickness is, for example, 5 nm.

[0111] The insulating films 5 to 9 constitute an insulating laminated structure located on the nitride semiconductor layer 4. The insulating films 5 to 9 are arranged on substantially the entire surface of the main surface 3a. The insulating films 5 to 9 mainly contain silicon compounds such as SiN, SiO2 and SiON. In the third embodiment, the insulating films 5 to 9 are in contact with each other, but another layer may be arranged between at least one set of two layers.

[0112] A plurality of source electrodes 22 are provided on the nitride semiconductor layer 4 and are connected to the insulating film 5 through a source opening 51 (see Fig.12 ) makes ohmic contact with the nitride semiconductor layer 4. Figure 8As shown in , a plurality of source electrodes 22 are arranged along the Y direction, and the planar shape of each source electrode 22 has a rectangular shape in which the direction X is the longitudinal direction. The source electrode 22 is formed in which a stacked structure including, for example, a Ti layer, an Al layer, and a Ti layer (or a Ta layer, an Al layer, and a Ta layer) is alloyed and mainly includes Al.

[0113] A plurality of drain electrodes 23 are provided on the nitride semiconductor layer 4 and are connected to the insulating film 5 through a drain opening 52 (see Fig.12 ) is in ohmic contact with the nitride semiconductor layer 4. Figure 8 As shown in , a plurality of drain electrodes 23 are alternately arranged with the source electrodes 22 in the Y direction, and the planar shape of each drain electrode 23 has a rectangular shape in which the direction X is the longitudinal direction. The drain electrode 23 is also formed in which a stacked structure including, for example, a Ti layer, an Al layer, and a Ti layer (or a Ta layer, an Al layer, and a Ta layer) is alloyed and mainly includes Al.

[0114] The gate electrode 21 includes a plurality of portions (finger portions) disposed on the nitride semiconductor layer 4 and portions extending from the finger portions toward one side surface 3d of the substrate 3. The finger portions of each gate electrode 21 extend in the direction X and are located between the source electrode 22 and the drain electrode 23. The finger portions of the gate electrode 21 are formed in the insulating film 5 through the gate opening 53 (see FIG. Fig.12 ) is in Schottky contact with the nitride semiconductor layer 4. The contact width (gate length) between the gate electrode 21 and the nitride semiconductor layer 4 in the Y direction is, for example, 0.5 μm. The gate electrode 21 has a stacked structure including a Ni layer and an Au layer on the Ni layer. In one example, the Ni layer is in contact with the nitride semiconductor layer 4, and the Au layer is in contact with the Ni layer. Alternatively, a Pd layer may be inserted between the Ni layer and the Au layer.

[0115] The field plate 35 is a metal film disposed along the gate electrode 21. Fig.12 As shown in FIG. 1 , the insulating film 7 is interposed between the field plate 35 and the gate electrode 21. The field plate 35 has a stacked structure of, for example, a Ti layer (or a Ta layer) and an Au layer.

[0116] The gate pad 31 is an example of an electrode pad in the third embodiment. The gate pad 31 is a metal film provided on a portion of the gate electrode 21 close to the side surface 3d. The gate pad 31 is electrically connected to the gate electrode 21 with low resistance because the gate pad 31 is connected to the gate electrode 21 through the opening 56 (see FIG. Fig.11 ) is in contact with the gate electrode 21. In the third embodiment, a plurality of gate pads 31 are arranged in the Y direction along the side 3d of the substrate 3. Each gate pad 31 is electrically connected to an external wiring through a bonding wire. Fig.11As shown in FIG. 1 , the surface of each gate pad 31 is exposed from the opening of the insulating film 9. Each gate pad 31 has a stacked structure including, for example, a TiW layer and an Au layer on the TiW layer.

[0117] The source wiring 32 is a metal film provided on the nitride semiconductor layer 4. The source wiring 32 includes a plurality of portions (pad portions) 32a alternately provided side by side with the plurality of gate pads 31 along the side 3d and a portion (finger portion) 32b extending on the respective source electrodes 22 and covering the respective source electrodes 22. Since each source electrode 22 is in contact with the finger portion 32b, the source wiring 32 is electrically connected to each source electrode 22 with low resistance. Furthermore, as shown in FIG. Fig.10 As shown in , the pad portion 32a of the source wiring 32 arranged side by side with the gate pad 31 is exposed from the opening of the insulating film 9 and is electrically connected to the back metal film 45 through the metal through hole 44 penetrating the substrate 3. The pad portion 32a of the source wiring 32 of the third embodiment includes a lower layer 36 in contact with the nitride semiconductor layer 4. The lower layer 36 is used to stop etching when forming a through hole 3c for forming the metal through hole 44 in the substrate 3. The lower layer 36 has, for example, the same stacking structure as the gate electrode 21. The remaining portion of each source wiring 32 except the lower layer 36 has a stacking structure similar to the stacking structure of the gate pad 31, for example, a stacking structure including a TiW layer and an Au layer on the TiW layer. The stacking structure is in contact with the nitride semiconductor layer 4 around the lower layer 36.

[0118] The metal via 44 is a wiring provided in the through hole 3c, which penetrates the substrate 3 (the growth substrate 30 and the nitride semiconductor layer 4) from the back surface 3b to the main surface 3a. The metal via 44 extends from the back surface 3b of the substrate 3 to the lower layer 36 of the source wiring 32 and contacts the lower layer 36. The metal via 44 is provided to electrically connect the back metal film 45 provided on the back surface 3b and the source electrode 22 having a low resistance via the source wiring 32. When the transistor 1A is mounted on a base member defined as a ground potential (reference potential), the base member and the back metal film 45 are electrically connected via a conductive adhesive material such as sintered silver paste. Therefore, the ground potential is applied to the source electrode 22.

[0119] like Fig. 9 As shown in FIG. 1 , the planar shape of the back metal film 45 is similar to the back surface 3b, and has a rectangular shape in the third embodiment. The outer peripheral edge of the back metal film 45 is arranged along the side surfaces 3d to 3g of the substrate 3 and is spaced apart from the side surfaces 3d to 3g of the substrate 3. The distance L1 between the side surfaces 3d to 3g of the substrate 3 and the back metal film 45 is, for example, in the range of 250 to 300 μm. The thickness t1 of the back metal film 45 (see Fig.10) is, for example, in the range of 3 to 10 μm. The backside metal film 45 has a stacked structure including, for example, a TiW layer and an Au layer on the TiW layer.

[0120] The drain wiring 33 is a metal film disposed on the nitride semiconductor layer 4. The drain wiring 33 has a stacked structure similar to that of the gate pad 31 and the source wiring 32, for example, a stacked structure including a TiW layer and an Au layer on the TiW layer. The drain wiring 33 extends on the corresponding drain electrode 23, and has a portion (finger portion) 33b covering each drain electrode 23. The drain wiring 33 is electrically connected to the drain electrodes 23 having low resistance respectively by contacting the respective drain electrodes 23. In addition, the portion 33a (drain pad) of the drain wiring 33 located near the side 3e is another example of an electrode pad in the third embodiment, and is arranged along the side 3e and has a rectangular shape in which, for example, the Y direction is longitudinal. The portion 33a of the drain wiring 33 is electrically connected to the external wiring through a bonding wire. Therefore, the surface of the portion 33a of the drain wiring 33 is exposed from the opening of the insulating film 9.

[0121] The polyimide wall 46A is a bank-like structure made of polyimide, is provided on the back surface 3b between the side surfaces 3d to 3g of the substrate 3 and the back metal film 45, and extends along the edge of the back metal film 45. Figure 8 , the polyimide wall 46A is indicated by a hidden line (dashed line). The polyimide wall 46A of the third embodiment is in contact with the back surface 3b and is spaced apart from the side surfaces 3d to 3g of the substrate 3 and the back metal film 45. The distance L2 between the side surfaces 3d to 3g of the substrate 3 and the polyimide wall 46A is at least 100 μm. The distance L3 between the back metal film 45 and the polyimide wall 46A is, for example, in the range of 50 to 100 μm. Fig.10 As shown in , the thickness t2 of the polyimide wall 46A based on the back surface 3b is thicker than the thickness t1 of the back metal film 45. The thickness t1 is, for example, in the range of 3 to 10 μm. In the embodiment, the thickness t1 is 10 μm. The width W in the direction orthogonal to the extension direction of the polyimide wall 46A is, for example, in the range of 50 to 100 μm. The shape of the cross section perpendicular to the extension direction of the polyimide wall 46A can be, for example, various shapes such as square, rectangle, trapezoid and semicircle.

[0122] like Fig. 9As shown in, the polyimide wall 46A of the third embodiment extends along the four sides of the rectangular back surface 3b, and has a rectangular frame plane shape. Specifically, the polyimide wall 46A has a part 46a extending along one side (side 3d) and a part 46b extending along the other side (side 3e) of a pair of sides of the back surface 3b facing each other in direction X. In addition, the polyimide wall 46A of the third embodiment has a part 46c extending along one side (side 3f) and a part 46d extending along the other side (side 3g) of another pair of sides connecting the above-mentioned pair of sides. Parts 46a to 46d are connected to each other at their respective ends, and have a rectangular frame shape as a whole. However, parts 46c and 46d have discontinuous parts 46e and 46f, which are disconnected in the middle in the extension direction. Discontinuous parts 46e and 46f are, for example, formed at the center of parts 46c and 46d in direction X.

[0123] A method for manufacturing the transistor 1A of the third embodiment having the above configuration will be described. First, a nitride semiconductor layer 4 is formed on a wafer-like growth substrate 30, and a wafer-like substrate 3 is manufactured. Specifically, first, an AlN buffer layer is epitaxially grown on the wafer-like growth substrate 30, a GaN channel layer is epitaxially grown on the AlN buffer layer, an AlGaN (or InAlN) barrier layer is epitaxially grown on the GaN channel layer, and a GaN cap layer is epitaxially grown on the AlGaN (or InAlN) barrier layer. By placing Ar + Ions are implanted into portions other than the active region of the nitride semiconductor layer 4 to form an inactive region. Thus, a wafer-like substrate 3 is produced.

[0124] Fig.13A 1 is a plan view showing a portion of the main surface 3 a of the wafer-like substrate 3 in an enlarged manner. Fig. 13B 2 is a bottom view showing a portion of the back surface 3b of the wafer-shaped substrate 3 in an enlarged manner. Fig.13A As shown in FIG. 1 , the wafer-like substrate 3 has a scribe area 3h (indicated by hatching in the drawing) on ​​the main surface 3a. The scribe area 3h has a lattice-like plane shape extending in the X and Y directions. A plurality of regions 3i defined by the scribe area 3h are device regions forming the transistor 1A, and each is rectangular. Each region 3i includes at least one active region. In addition, as shown in FIG. Fig. 13B As shown in FIG. 1 , the back surface 3b of the wafer-like substrate 3 includes a region 3j (a hatched first region in the drawing) obtained by projecting the scribe region 3h onto the back surface 3b. The region 3j has a grid-like planar shape extending along directions X and Y, like the scribe region 3h.

[0125] Figures 14A to 18C is a cross-sectional view showing the first half of steps included in a method of manufacturing the transistor 1A. Fig.14A ,15A , 16A, 17A and 18A each show corresponding to Figure 8 The cross section of line XX in . Fig. 14B , 15B , 16B, 17B and 18B each show a corresponding Figure 8 A cross section along line XI-XI. Fig. 14C , 15C , 16C, 17C and 18C each show a corresponding Figure 8 Cross section of line XII-XII.

[0126] like Figures 14A-14C As shown in , the insulating film 5 is deposited on the main surface 3a of the substrate 3. For example, when the insulating film 5 is made of a silicon compound such as SiN, the insulating film 5 is deposited by a plasma CVD method or a low-pressure CVD (LPCVD) method. In the case of LPCVD, the film forming temperature is, for example, 850°C, and the film forming pressure is, for example, 10Pa or less. The film forming raw materials are, for example, NH3 and SiH2Cl2. When the plasma CVD method is used, a temperature of 300°C, SiH4 and NH3 as raw material gases, N2 as a dilution gas, an RF frequency of 13.56MHz, and a power of 50W for a plasma generating device are selected as film forming conditions. The thickness of the insulating film 5 is, for example, in the range of 60 to 100nm, and is 60nm in the embodiment.

[0127] Then, if Fig. 15C As shown in , a source opening 51 corresponding to the source electrode 22 and a drain opening 52 corresponding to the drain electrode 23 are formed in the insulating film 5. Specifically, a resist mask having an opening pattern corresponding to the source opening 51 and the drain opening 52 is formed on the insulating film 5, and the insulating film 5 is etched by the opening pattern. Thus, the source opening 51 and the drain opening 52 are formed. Thereafter, using a lift-off method, the source electrode 22 is formed in the source opening 51, and the drain electrode 23 is formed in the drain opening 52. That is, while retaining the resist mask, metal layers (for example, Ti / Al / Ti or Ta / Al / Ta) for the source electrode 22 and the drain electrode 23 are sequentially deposited using physical vapor deposition or the like. The thickness of each Ti layer (or Ta layer) is, for example, in the range of 10 to 30 nm (10 nm in the embodiment), and the thickness of the Al layer is, for example, in the range of 200 to 400 nm (300 nm in the embodiment). After the metal material deposited on the resist mask is removed together with the resist mask, heat treatment (annealing) is performed in a temperature range of 500 to 600° C. (550° C. in the embodiment). Thus, the source electrode 22 and the drain electrode 23 are alloyed. The time for maintaining the temperature in the range of 500 to 600° C. is, for example, one minute.

[0128] Then, if Figures 15A to 15C As shown in FIG. 5 , an insulating film 6 covering the insulating film 5, the source electrode 22, and the drain electrode 23 is deposited. For example, when the insulating film 6 is made of a silicon compound such as SiN, the insulating film 6 is deposited by a plasma CVD method. The film formation temperature is, for example, 300° C., and the film formation raw materials are, for example, NH 3 and SiH 4. The thickness of the insulating film 6 is, for example, 100 nm.

[0129] Subsequently, the gate electrode 21 and the lower layer 36 of the source wiring 32 are formed. First, a resist for electron beam (EB) is deposited on the insulating film 6, and an opening pattern for the gate electrode 21 and the lower layer 36 is formed in the EB resist by EB writing. Next, the insulating film 6 and the insulating film 5 are continuously etched through the opening pattern of the EB resist to form a gate opening 53 and an opening 54 penetrating the insulating films 5 and 6, as shown in FIG. Fig. 16B and 16C As shown in , the nitride semiconductor layer 4 is exposed. Thereafter, using a lift-off method, the gate electrode 21 is formed in the gate opening 53, and at the same time, the lower layer 36 of the source wiring 32 is formed in the opening 54. That is, while the EB resist remains, metal layers (for example, Ni / Au or Ni / Pd / Au) for the gate electrode 21 and the lower layer 36 are sequentially deposited using physical vapor deposition or the like. The thickness of the Ni layer is, for example, in the range of 70 to 150 nm (in the embodiment, 100 nm), the thickness of the Pd layer is, for example, in the range of 50 to 100 nm (in the embodiment, 50 nm), and the thickness of the Au layer is, for example, in the range of 300-700 nm (in the embodiment, 500 nm). Thereafter, the metal material deposited on the EB resist is removed together with the EB resist.

[0130] Then, if Figures 17A to 17C As shown in , the insulating film 7 is deposited. First, the insulating film 7 is formed on the entire surface of the main surface 3a to cover the insulating film 6, the gate electrode 21 and the lower layer 36. For example, when the insulating film 7 is made of a silicon compound such as SiN, the insulating film 7 is deposited by a plasma CVD method. The film formation temperature is, for example, 300°C, and the film formation raw materials are, for example, NH3 and SiH4. The thickness of the insulating film 7 is, for example, 100nm.

[0131] Then, if Fig. 17CAs shown in , the field plate 35 is formed on the insulating film 7 along the finger-shaped portion of the gate electrode 21. In this process, the field plate 35 is formed using, for example, a lift-off method. That is, a resist mask having an opening pattern corresponding to the planar shape of the field plate 35 is formed, and a metal layer (for example, Ti (or Ni) / Au) for the field plate 35 is sequentially deposited using physical vapor deposition or the like. In the embodiment, the thickness of the Ti layer (or Ni layer) is 10 nm, and the thickness of the Au layer is 200 nm. Thereafter, the metal material deposited on the resist mask is removed together with the resist mask.

[0132] Subsequently, an insulating film 8 covering the insulating film 7 and the field plate 35 is deposited. First, the insulating film 8 is formed on the entire surface of the main surface 3a. For example, when the insulating film 8 is made of a silicon compound such as SiN, the insulating film 8 is deposited by a plasma CVD method. The film formation temperature is, for example, 300°C, and the film formation raw material is, for example, NH3 and SiH4.

[0133] Then, if Fig.17A As shown in , the insulating films 7 and 8 on the lower layer 36 are removed by etching to form an opening 59 and expose the lower layer 36. Fig. 17C As shown in , the insulating films 5 to 8 in the regions corresponding to the source wiring 32 and the drain wiring 33 are removed by etching to form openings 57 and 58, and the source electrode 22 and the drain electrode 23 are exposed. Fig. 17B As shown in , the insulating films 7 and 8 in the region corresponding to the gate pad 31 are removed by etching to form an opening 55, and the gate electrode 21 is exposed. Specifically, a resist mask having an opening pattern corresponding to each of the openings 55, 57 to 59 is formed on the insulating film 8, and the insulating films 5 to 8 are etched through the opening pattern to form each of the above-mentioned openings.

[0134] In addition, in this process, along Fig.13A The scribe region 3h shown in FIG. 1 forms an opening 55 for the gate pad 31, an opening for the source pad 32a, and an opening for the portion 33a of the drain wiring 33. Specifically, the opening 55 for the gate pad 31 and the opening for the source pad 32a are alternately arranged along the portion of the scribe region 3h for forming the side 3d. In addition, an opening for the portion 33a of the drain wiring 33 is formed along the portion of the scribe region 3h for forming the side 3e.

[0135] After removing the resist mask, as Figures 18A to 18C As shown in FIG. 1 , the gate pad 31, the source wiring 32, and the drain wiring 33 are formed together. In this process, the gate pad 31, the source pad 32a, and the portion 33a of the drain wiring 33 are formed along Fig.13ASpecifically, gate pads 31 and source pads 32a are alternately arranged along a portion of scribe region 3h forming side 3d, and portion 33a of drain wiring 33 is arranged along a portion of scribe region 3h forming side 3e.

[0136] For this purpose, first, a seed metal layer (Ti / TiW / Ti / Au) is formed on the entire surface of the main surface 3a by sputtering. The thickness of each Ti layer is, for example, 10 nm, the thickness of the TiW layer is, for example, 100 nm, and the thickness of the Au layer is, for example, 100 nm. Next, a resist mask having an opening in each predetermined formation area of ​​the gate pad 31, the source wiring 32, and the drain wiring 33 is formed on the seed metal layer. Electrolytic plating is performed to form an Au layer in the opening of the resist mask. At this time, the thickness of the Au layer is, for example, 3 μm. After the plating process, the resist mask is removed and the exposed seed metal layer is removed. Thus, the above-mentioned gate pad 31, source wiring 32, and drain wiring 33 are formed together.

[0137] Subsequently, an insulating film (passivation film) 9 is deposited on the entire surface of the main surface 3a. For example, when the insulating film 9 is made of a silicon compound such as SiN, the insulating film 9 is deposited by a plasma CVD method. The film forming temperature is, for example, 300°C, and the film forming raw material is, for example, NH3 and SiH4. After that, an opening of the insulating film 9 is formed on the gate pad 31, the source pad 32a, and the portion 33a of the drain wiring 33 to expose these. Thus, the process on the main surface 3a side is completed.

[0138] Figures 19A to 22C 1A is a schematic diagram showing a cross section of the latter half of the steps included in the method of manufacturing the transistor 1A. Figures 19A-22C In the figure, the structure of the components other than the lower layer 36 on the other main surface 3a is omitted. Fig.19A As shown in , a protective resist 61 is formed on the main surface 3a by spin coating, and the resist 61 covers all components on the main surface 3a. Next, a support substrate 62 is attached to the resist 61. The support substrate 62 is made of, for example, SiO2. Subsequently, the back surface 3b of the substrate 3 is polished to thin the substrate 3. At this time, for example, the growth substrate 30 having a thickness of 500μm is thinned to 100μm.

[0139] Then, if Fig.19B As shown in FIG. 1 , a seed metal film 63 (eg, TiW / Au) is formed on the back surface 3 b and the side surface of the substrate 3 by, for example, a sputtering method. After a resist pattern 65 is formed at a position facing the lower layer 36, as shown in FIG. Fig.19C As shown in FIG. 1 , a Ni mask 64 is formed by plating Ni. Fig. 20AAs shown in , the resist pattern 65 is removed, and the exposed portion of the seed metal film 63 is etched away. Thus, the region of the back surface 3b facing the lower layer 36 is exposed through the opening of the Ni mask 64. When the seed metal film 63 is made of TiW / Au, the seed metal film 63 can be easily removed by reactive ion etching (RIE) using a fluorine-based gas.

[0140] Subsequently, the substrate 3 (growth substrate 30 and nitride semiconductor layer 4) is etched through the opening of the Ni mask 64 to form a hole 3c penetrating the substrate 3 (see Fig.10 In this process, the hole 3c is formed by reactive ion etching (RIE). Fig. 20B As shown in FIG. 1 , first, the growth substrate 30 is etched by RIE using a fluorine-based gas. When all the growth substrates 30 are etched, the Ni mask 64 ( Fig. 20C ). Next, the reaction gas is changed, and the nitride semiconductor layer 4 is etched by RIE using a chlorine-based gas ( Fig.21A ).

[0141] Lower layer 36 comprises Ni layer and Au layer on Ni layer, and as the etching of nitride semiconductor layer 4 proceeds, Ni layer is exposed first. At this time, Ni layer is slightly etched by chlorine-based gas, but the etching rate of Ni by chlorine-based gas is much less than the etching rate of nitride semiconductor by chlorine-based gas. Therefore, etching can be stopped in lower layer 36. Even if Ni layer is removed by sputtering effect, because Au layer much thicker than Ni layer is arranged on Ni layer, etching by chlorine-based gas is reliably stopped on Au layer. Therefore, through hole 3c from back surface 3b of substrate 3 to lower layer 36 is formed, and lower layer 36 is exposed to back surface 3b side by through hole 3c.

[0142] In the above-mentioned etching process, the Ni mask 64 is removed when all the growth substrates 30 are etched, and then the nitride semiconductor layer 4 is etched by the chlorine-based gas. It is necessary to remove the Ni mask 64 by the next process, but just after the through hole 3c is formed, the Ni layer of the lower layer 36 is exposed in the through hole 3c. If the removal process of the Ni mask 64 is performed in this state, the Ni layer of the lower layer 36 is also removed at the same time. Therefore, before the Ni layer of the lower layer 36 is exposed, that is, after the etching of the growth substrate 30 is completed, and before the etching of the nitride semiconductor layer 4 is started, the Ni mask 64 is removed.

[0143] When etching the nitride semiconductor layer 4 , etching can be performed using a fluorine-based gas continuously from the growth substrate 30 , and the nitride semiconductor layer 4 is etched by a sputtering effect.

[0144] Then, if Fig.21BAs shown in FIG. 1 , a seed metal film 66 (eg, TiW / Au) is formed on the back surface 3b of the substrate 3 and the inner surface of the through hole 3c (including the exposed lower layer 36) by, for example, sputtering. Fig.13A ) overlaps the area 3j (see Fig. 13B ) is formed on the resist pattern 67. At this time, the width in the direction orthogonal to the extending direction of the resist pattern 67 is made larger than the width of the region 3j (that is, the width of the scribed region 3h). In other words, when viewed from the normal direction of the back surface 3b, the region 3j is included in the resist pattern 67, and the edge of the region 3j is located within the resist pattern 67.

[0145] Afterwards, if Fig. 21C As shown in FIG. 1 , electrolytic plating is performed on the seed metal film 66 exposed from the resist pattern 67 to form a backside metal film 45 on the back surface 3b and to form a metal through hole 44 from the back surface 3b to the lower layer 36 in the through hole 3c. Since the width of the resist pattern 67 is greater than the width of the region 3j, the backside metal film 45 is formed apart from the region 3j. Thereafter, as shown in FIG. Fig.22A As shown in FIG. , the resist pattern 67 is removed, and the exposed seed metal film 66 ( Fig. 22B ).

[0146] Then, if Fig. 22C As shown in FIG. 3 , a polyimide wall 46A extending along the edge of the back metal film 45 is formed by coating the area (second area) between the coating area 3j and the back metal film 45. The coating method of the polyimide wall 46A is, for example, screen printing. In the third embodiment, the parts 46a and 46b of the polyimide wall 46A (see Fig. 9 ) are formed along corresponding portions of the region 3j corresponding to the side faces 3d and 3e of the substrate 3. The portions 46c and 46d of the polyimide wall 46A (refer to Fig. 9 ) are formed along corresponding portions of the region 3j corresponding to the side faces 3f and 3g of the substrate 3.

[0147] In this process, the polyimide wall 46A is formed to be spaced apart from the region 3j and the backside metal film 45. Fig. 9 As shown in FIG. 1 , the side surface 3b of the substrate 3 is exposed between the back surfaces 3b to 3g of the substrate 3 and the polyimide wall 46A and between the polyimide wall 46A and the back metal film 45 of the completed transistor 1A. Furthermore, in this process, discontinuous portions 46e and 46f are formed in portions 46c and 46d of the polyimide wall 46A formed along the corresponding portions of the region 3j corresponding to the side surfaces 3f and 3g of the substrate 3. By providing such discontinuous portions 46e and 46f, it is possible to support the mask located inside the polyimide wall 46A during screen printing.

[0148] Subsequently, the protective resist 61 is removed to separate the components on the main surface 3a side of the substrate 3 from the support substrate 62 ( Fig.23A ). Heat treatment is performed to solidify the polyimide wall 46A. The temperature of the heat treatment is, for example, 250° C., and the heat treatment time is, for example, 1 hour. Thereafter, the back surface 3b of the substrate 3 is attached to the expansion tape, and dicing (slicing) is performed along the scribe line region 3h to separate the plurality of regions 3i (device region, see Fig.13A ) are separated from each other. A plurality of semiconductor chips ( Fig. 23B ). Through the above-mentioned process, the transistor 1A of the third embodiment is completed.

[0149] The effect obtained by the transistor 1A of the third embodiment described above will be described together with a conventional example. Typically, the back metal film 45 is conductively bonded to the metal base member by a conductive adhesive material. In many cases, the base member is set to a reference potential (ground potential). In this case, when a negative voltage lower than the reference potential is applied to the gate electrode 21, an electric field that makes the gate pad 31 side negative is generated between the gate pad 31 and the base member. Under a humid environment, due to this electric field, ion migration of metals (e.g., Ag, Au, Cu, etc.) contained in the conductive adhesive material may occur. Ion migration is a phenomenon in which ionized metals move on the surface of a substance between electric fields. Metal ions are attracted to the electric field, reduced from an ionized state to a metal for some reason, and accumulate to form dendrites. When metal dendrites grow from the conductive adhesive material, the gate pad 31 and the back metal film 45 are short-circuited, causing the operation of the transistor to fail.

[0150] In recent years, the development of wide-gap semiconductors mainly made of GaN, SiC, Ga2O3, etc. has been promoted and is in practical use. Since wide-gap semiconductors have high withstand voltage, the performance of semiconductors is improved by increasing the power supply voltage to increase mobility or reduce parasitic capacitance between electrodes. Therefore, in the case of wide-gap semiconductors, the above-mentioned electric field is strong, and ion migration is likely to occur.

[0151] Therefore, in the transistor 1A of the third embodiment, the back metal film 45 is provided on the back surface 3b having a certain distance from the side surfaces 3d to 3g of the substrate 3, and the polyimide wall 46A extending along the edge of the back metal film 45 is provided on the back surface 3b between the side surfaces 3d to 3g and the back metal film 45. The growth of dendrites from the conductive adhesive material is suppressed by the polyimide wall 46A. Therefore, the short circuit between the back metal film 45 and the gate pad 31 due to the ion migration of the metal contained in the conductive adhesive material can be reduced.

[0152] In the third embodiment, the polyimide wall 46A can be formed spaced apart from the region 3j, and the back surface 3b of the substrate 3 can be exposed between the side 3d to 3g of the substrate 3 and the polyimide wall 46A. In this case, the polyimide wall 46A is reliably formed directly on the back surface 3b of the substrate 3. If there is no spacing, process variations may increase the possibility of forming the polyimide wall 46A on the back metal film 45. The adhesion of the back metal film 45 to the polyimide is low. In this case, the distance between the side 3d to 3g of the substrate 3 and the polyimide wall 46A can be at least 100μm. Thus, even if a conductive bonding member such as a sintered metal type silver paste crawls on the polyimide wall 46A, there is still a distance of 100μm to the gate pad 31 and the possibility of the gate pad 31 and the ground potential short circuit is reduced.

[0153] In the third embodiment, the polyimide wall 46A may be formed spaced apart from the back metal film 45, and the back surface 3b of the substrate 3 may be exposed between the back metal film 45 and the polyimide wall 46A. In this case, since the back metal film 45 mainly composed of Au having poor adhesion to polyimide and the polyimide wall 46A do not contact each other, peeling of the polyimide wall 46A can be reduced.

[0154] In the third embodiment, the width W in the direction orthogonal to the extending direction of the polyimide wall 46A may be in the range of 50 to 100 μm. In this case, the growth of dendrites from the conductive adhesive material can be sufficiently suppressed.

[0155] In the third embodiment, the planar shape of the transistor 1A may be a rectangle. The gate pad 31 may be arranged along one side (side 3d) of a pair of sides facing each other in the rectangle, and the drain wiring 33 may be arranged along the other side (side 3e) of the pair of sides, and the polyimide wall 46A may be formed at least along one side (side 3d). As described above, a negative bias may be applied to the gate pad 31. By forming the polyimide wall 46A along one side (side 3d) where the gate pad 31 is arranged, the short circuit between the gate pad 31 and the back metal film 45 can be effectively reduced.

[0156] In the third embodiment, the polyimide wall 46A can be further formed along the other side (side 3e). Although ion migration does not occur on the drain pad 33a side, because the conductive bonding member does not protrude from the transistor 1A, another circuit element can be arranged at a position closest to the transistor 1A. The limitation of the mounting area based on the protrusion of the conductive bonding member can be alleviated, and by arranging another circuit component at a position closest to the transistor 1A, the degradation of high-frequency characteristics can be suppressed.

[0157] In the third embodiment, the polyimide wall 46A can be further formed along the other pair of sides (sides 3f and 3g). Thus, the growth of dendrites on the sides 3f and 3g can be suppressed, and the short circuit between the gate pad 31 (and the drain wiring 33) and the back metal film 45 can be more effectively reduced.

[0158] (Revise)

[0159] Fig.24A and Fig. 24B is a view showing a modification of the polyimide wall of the third embodiment. Fig.24A The polyimide wall 46B shown in FIG. 4 includes the portion 46a of the polyimide wall 46A of the third embodiment and a portion of the portions 46c and 46d closer to the portion 46a than the discontinuous portions 46e and 46f, but does not include the portion 46b or a portion of the portions 46c and 46d closer to the portion 46b than the discontinuous portions 46e and 46f. Even in such a configuration, as in the third embodiment, it is possible to reduce the short circuit between the backside metal film 45 and the gate pad 31 due to the ion migration of the metal contained in the conductive adhesive material.

[0160] Fig. 24B The polyimide wall 46C shown in does not include the discontinuous parts 46e and 46f of the third embodiment, and forms parts 46c and 46d continuously. In other words, the polyimide wall 46C surrounds the back metal film 45 from all sides without a gap. Even in this mode, the same functions and effects as those of the third embodiment can be obtained. In this example, because the mask on the inner side of the polyimide wall 46C cannot be supported, screen printing cannot be applied. Therefore, it is preferable to use a method such as applying photosensitive polyimide and performing pattern exposure (photolithography).

[0161] (Fourth embodiment)

[0162] Fig.25 is a plan view showing the configuration of a semiconductor device 500 according to the fourth embodiment. Fig.25 5 shows a state where the cover of the semiconductor device 500 is removed. The semiconductor device 500 includes the transistor 1A of the third embodiment, a package 501, an input matching circuit 506, an output matching circuit 508, and an output capacitor 509. The transistor 1A, the input matching circuit 506, the output matching circuit 508, and the output capacitor 509 are accommodated in the package 501. The package 501 has a non-sealed structure in which airtight sealing is not performed.

[0163] Package 501 includes substrate 503, sidewall 504, two input leads 550 and two output leads 560. Substrate 503 is a plate-like member having a flat main surface 503a made of metal. Substrate 503 can be made of, for example, copper, an alloy of copper and molybdenum, an alloy of copper and tungsten. Substrate 503 can be a laminate including at least one of a copper plate, a molybdenum plate, a tungsten plate, an alloy plate of copper and molybdenum, and an alloy plate of copper and tungsten. The surface of substrate 503 is plated with nickel-chromium (nickel-chromium alloy)-gold, nickel-gold, nickel-palladium-gold, silver or nickel, nickel-palladium, etc. Gold, silver and palladium are plating materials, and NiCr and Ni, etc. are seed materials. When plating materials and seed materials are included, rather than when only plating materials are included, adhesion can be improved. The thickness of substrate 503 is, for example, 0.5 to 1.5 mm. The plane shape of substrate 503 is, for example, rectangular.

[0164] The side wall 504 is a substantially rectangular frame-shaped member made of ceramic as a dielectric. The side wall 504 has a pair of parts 541 and 542 facing each other in the X direction along the main surface 503a of the substrate 503, and a pair of parts 543 and 544 facing each other in the Y direction intersecting the X direction. The parts 541 and 542 extend parallel to each other along the Y direction, and the parts 543 and 544 extend parallel to each other along the Y direction. The cross section of each of the parts 541 to 544 perpendicular to the extension direction is rectangular or square. The height of the side wall 504 in the normal direction of the main surface 503a is, for example, 0.5 to 1.0 mm. The side wall 504 is bonded to the main surface 503a of the substrate 503 by an adhesive material such as silver solder.

[0165] The input lead 550 and the output lead 560 are plate-like members made of metal, for example, a thin metal plate of copper, copper alloy or iron alloy. One end of the input lead 550 in the X direction is attached to the upper surface of the portion 541 of the side wall 504. The input lead 550 is insulated from the main surface 503a of the substrate 503 by the portion 541 of the side wall 504. One end of the output lead 560 in the X direction is attached to the upper surface of the portion 542 of the side wall 504. The output lead 560 is insulated from the main surface 503a of the substrate 503 by the portion 542 of the side wall 504.

[0166] The transistor 1A, the input matching circuit 506, the output matching circuit 508, and the output capacitor 509 are mounted in a region surrounded by the side wall 504 on the main surface 503a of the substrate 503. The transistor 1A, the input matching circuit 506, the output matching circuit 508, and the output capacitor 509 are arranged in this order starting from the portion 541 of the side wall 504. The input matching circuit 506 and the output matching circuit 508 are, for example, parallel plate capacitors in which electrodes are arranged on the upper and lower surfaces of a ceramic substrate.

[0167] The input matching circuit 506, the transistor 1A and the output matching circuit 508 are fixed on the substrate 503 by a conductive adhesive material such as a sintered conductive paste. The conductive adhesive material contains at least one of Ag, Au and Cu. In an embodiment, the conductive adhesive material is a sintered silver paste. The conductive adhesive material for fixing the transistor 1A is inserted between the back metal film 45 of the transistor 1A and the main surface 503a of the substrate 503, electrically connecting them, and firmly bonding them. The input matching circuit 506 is installed on the input side of the transistor 1A, and the output matching circuit 508 is installed on the output side of the transistor 1A. The input matching circuit 506 is electrically connected to the transistor 1A through a plurality of bonding wires (not shown), the transistor 1A is electrically connected to the output matching circuit 508 through a plurality of bonding wires (not shown), the output matching circuit 508 is electrically connected to the output capacitor 509 through a plurality of bonding wires (not shown), and the output capacitor 509 is electrically connected to the output lead 560 through a plurality of bonding wires (not shown).

[0168] The input matching circuit 506 performs impedance matching between the input lead 550 and the transistor 1A. One end of the input matching circuit 506 is electrically connected to the input lead 550 through a bonding wire. The other end of the input matching circuit 506 is electrically connected to the gate pad 31 of the transistor 1A through a bonding wire (see FIG. Figure 8 ).

[0169] The output matching circuit 508 adjusts its impedance between the transistor 1A and the output lead 560 to provide the desired output of the high frequency signal appearing on the output lead 560 with maximum efficiency. One end of the output matching circuit 508 is electrically connected to the portion 33a of the drain wiring 33 of the transistor 1A through a bonding wire (see Figure 8 The other end of the output matching circuit 508 is electrically connected to the output lead 560 via a bonding wire and an output capacitor 509 .

[0170] In manufacturing the semiconductor device 500, the transistor 1A manufactured by the method according to the third embodiment is mounted on the substrate 503 using a conductive bonding material containing Ag (e.g., sintered silver paste). Specifically, the sintered silver paste is applied to a predetermined area of ​​the main surface 503a of the substrate 503, and the transistor 1A is arranged thereon. Next, heat treatment is performed (e.g., at 200°C for 1 hour under an N2 atmosphere). Thus, the solvent of the sintered silver paste is volatilized, and the metal containing Ag is sintered.

[0171] The semiconductor device 500 of the fourth embodiment includes the transistor 1A of the third embodiment. Therefore, the growth of dendrites caused by the ion migration of the conductive bonding material inserted between the transistor 1A and the main surface 503a of the substrate 503 is suppressed, and the short circuit between the main surface 503a of the substrate 503 and the gate pad 31 can be reduced. In addition, as in the fourth embodiment, when the package 501 for accommodating the transistor 1A has a non-sealed structure, the usefulness of the transistor 1A is more significant.

[0172] The semiconductor device and the manufacturing method thereof according to the present disclosure are not limited to the above-described embodiments, and various other modifications are possible. For example, although the contents of the present disclosure are applied to the field effect transistor in the third embodiment, the present invention is not limited thereto.

Claims

1. A method for manufacturing a semiconductor device, comprising: forming a field effect transistor mainly including GaN on a surface of a SiC semiconductor substrate in which a formation region for a semiconductor chip is formed, the formation region being divided by a scribe line having a first width; forming a first metal layer over the entire back surface of the SiC semiconductor substrate, wherein the first metal layer has a wettability with respect to Ag lower than a wettability of Au or Cu; forming a second metal layer made of Au on a first region of the first metal layer, the first region not overlapping the scribe line; individualizing the semiconductor chips by dicing the SiC semiconductor substrate along the scribe line with a second width narrower than the first width; as well as The semiconductor chip is mounted on a metal substrate via a conductive adhesive member containing Ag.

2. The method of manufacturing a semiconductor device according to claim 1, further comprising molding the semiconductor chip mounted on the metal substrate with a sealing resin. 3 . The method for manufacturing a semiconductor device according to claim 1 , wherein the first metal layer comprises at least one of NiCr, Ti, and Ta.

4. The method for manufacturing a semiconductor device according to claim 1, in, When forming the first metal layer and forming the second metal layer, the following steps are performed in sequence: On the entire back surface of the SiC semiconductor substrate, continuously forming the first metal layer and the second metal layer by sputtering; selectively plating the second metal layer on a second area excluding the first area, wherein the first metal layer and the second metal layer are considered as seed metals; and The second metal layer on the first region is removed.

5. The method for manufacturing a semiconductor device according to claim 1, in, When forming the first metal layer and forming the second metal layer, performing: On the entire back surface of the SiC semiconductor substrate, the first metal layer and the second metal layer are continuously formed by sputtering; and The second metal layer is selectively plated on a second region excluding the first region, wherein the first metal layer and the second metal layer are considered as seed metals, and the method further includes forming a third metal layer in the first region.

6. A method for manufacturing a semiconductor device, the method comprising: Arranging electrode pads along a scribe line region on a main surface of a substrate having a plurality of device regions surrounded by the scribe line region on the main surface; forming a backside metal film on a back surface of the substrate, the backside metal film being spaced apart from a first region in which the scribe line region is projected on the back surface; forming a polyimide wall extending along an edge of the backside metal film on a second area between the first area and the backside metal film; as well as The substrate is cut along the scribe line regions to produce semiconductor chips, each of which includes the device region.

7. The method for manufacturing a semiconductor device according to claim 6, wherein forming the polyimide wall comprises forming the polyimide wall spaced apart from the first region, and The back surface of the substrate is exposed between a side surface of the substrate of each semiconductor chip and the polyimide wall of the semiconductor chip. 8 . The method of manufacturing a semiconductor device according to claim 7 , wherein a distance between the side surface of the substrate and the polyimide wall is at least 100 μm.

9. The method of manufacturing a semiconductor device according to claim 6, wherein a width in a direction orthogonal to an extending direction of the polyimide wall is in a range of 50 to 100 μm.

10. The method for manufacturing a semiconductor device according to claim 6, The semiconductor chip is a field effect transistor, the planar shape of the semiconductor chip is a rectangle, the gate pad is arranged as the electrode pad along one side of a first pair of sides facing each other of the rectangle, and the drain pad is arranged along the other side of the first pair of sides, and The forming of the polyimide wall includes forming the polyimide wall along at least one side. 11 . The method for manufacturing a semiconductor device according to claim 10 , wherein said forming said polyimide wall comprises further forming said polyimide wall along said other side. 12 . The method for manufacturing a semiconductor device according to claim 10 , wherein forming the polyimide wall comprises further forming the polyimide wall along a second pair of sides connected to the first pair of sides of the rectangle.

13. The method for manufacturing a semiconductor device according to claim 12, wherein the polyimide wall formed along the second pair of sides has a discontinuous portion. 14 . The method of manufacturing a semiconductor device according to claim 6 , further comprising mounting the semiconductor chip on a substrate having a metal surface using a conductive bonding material containing Ag.

15. A semiconductor device comprising a semiconductor chip in which a field effect transistor mainly comprising GaN is formed on a surface of a SiC semiconductor substrate, the semiconductor device comprising: a metal substrate, on which the back surface of the semiconductor chip is mounted via a conductive adhesive material containing Ag, the back surface being opposite to a mounting surface of the metal substrate; and a resin mold configured to seal the semiconductor chip, wherein a metal having a wettability with respect to Ag lower than that of Au or Cu is exposed in a region extending along an edge of the back surface, wherein the backside metal film of the semiconductor chip is disposed on the back surface and is spaced apart from the side surface of the SiC semiconductor substrate, and wherein the metal is exposed from the backside metal film on the region.

Citation Information

Patent Citations

  • Information processing device, system, and control method therefor, and program thereof

    JP2018103823A

  • Nmr measuring apparatus

    JP2019035716A

  • Semiconductor device and manufacturing method of the same

    US20140264383A1

  • Power semiconductor device and method for manufacturing same

    US20190172812A1