Injection molding mold and method thereof, injection molded body and injection molded product

By designing multi-layer color cavity and specific structural areas in the injection mold, the problem of color transmission and color mixing at the color junction in the injection mold is solved, and the appearance effect and quality of the finished product are improved.

CN110576566BActive Publication Date: 2024-11-01LENS TECH CHANGSHA
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN201810622203.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-06-15
Publication Date
2024-11-01
Estimated Expiration
2038-06-15

AI Technical Summary

Technical Problem

When existing injection molds are in two- or multi-color injection molding, color transmission and color mixing are prone to occur at the color junction, which affects the appearance effect and quality of the finished product.

Method used

The injection molding mold design is adopted including the first mold, the second mold and the third mold, and the multi-layer color cavity is formed by closing the mold, and the structural design of the chamfered area, the straight line area and the chamfered area is used to avoid color junction. The appearance and quality of the finished product are improved by machining.

Benefits of technology

It effectively avoids color transmission and color mixing at the color junction, improves the compressive and impact strength of the injection molded embryo, reduces local cracking or poor cracking, and improves the appearance effect and quality of the finished product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110576566B_ABST
    Figure CN110576566B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of injection molding technology, and in particular to an injection molding mold and a method thereof, an injection molded body and an injection molded product. The injection molding mold comprises a first mold body, a second mold body and a third mold body; the first molding surface of the first mold body and the second molding surface of the second mold body can form a first color cavity; the first color cavity and the third molding surface of the third mold body can form a second color cavity; along the mold closing direction, the second molding surface comprises a first chamfered area, a straight area and a second chamfered area; the first chamfered area, the straight area and the second chamfered area form the side wall of the second color concave cavity portion of the second color cavity. The injection molding method uses an injection molding mold. The injection molded body is formed by injection molding using the injection molding mold. The injection molded product is formed by processing the injection molded body. The purpose of the present invention is to provide an injection molding mold and a method thereof, an injection molded body and an injection molded product to solve the technical problems of color transmission and color mixing at the color interface existing in the prior art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of injection molding technology, and in particular to an injection molding mold and a method thereof, an injection molding embryo and an injection molding product of materials such as ceramics, metals and high-hardness plastics. Background Art

[0002] Injection molding, also known as injection molding, is a molding method that combines injection and molding. The advantages of the injection molding method are fast production speed, high efficiency, automated operation, a wide variety of colors, shapes from simple to complex, sizes from large to small, and precise product size. The product is easy to update and can be made into complex-shaped parts. Injection molding is suitable for mass production and complex-shaped products and other molding and processing fields.

[0003] However, when the existing injection mold is used for two-color or multi-color injection molding, the color boundary will be transparent or mixed, and the affected area can reach 0.05mm-0.2mm, or even larger, which seriously affects the appearance of the finished product and reduces the quality of the finished product. For example, when two-color injection molding, due to the mold release angle, a thin-walled area is usually formed at the boundary of the two colors, and this area will produce color transparency or mixed color due to the thin wall.

[0004] Therefore, in order to solve the above problems, the present application provides a new injection molding mold and method thereof, an injection molded body and an injection molded product, so as to improve the appearance of the finished product and thus improve the quality of the finished product. Summary of the invention

[0005] The purpose of the present invention is to provide an injection molding mold to solve the technical problems of color penetration and color mixing at the color interface existing in the prior art.

[0006] The present invention also aims to provide an injection molding method to solve the technical problems of color penetration and color mixing at the color interface in the prior art.

[0007] The present invention also aims to provide an injection molded body and an injection molded product to solve the technical problems of color transmission and color mixing at the color boundaries existing in the prior art.

[0008] Based on the above first purpose, the injection molding mold provided by the present invention includes a first mold body, a second mold body and a third mold body; the first mold body is provided with a first molding surface, the second mold body is provided with a second molding surface; the third mold body is provided with a third molding surface;

[0009] When the first mold body and the second mold body are molded together, the first molding surface and the second molding surface form a first color cavity;

[0010] When the first mold body and the third mold body are molded together, the first color cavity and the third molding surface form a second color cavity; wherein part or all of the second molding surface is the interface between the first color cavity and the second color cavity;

[0011] The second color cavity comprises a second color concave cavity portion disposed within the first color cavity;

[0012] Along the mold closing direction, the second molding surface includes a first chamfered area, a straight area and a second chamfered area connected in sequence; the first chamfered area, the straight area and the second chamfered area form the side wall of the second color concave cavity portion.

[0013] An optional technical solution of the present invention is that the second color cavity includes a second color convex cavity portion connected to the second color concave cavity portion; the second color convex cavity portion protrudes from the first color cavity;

[0014] In a direction perpendicular to the mold closing direction, the area of ​​the second color convex cavity portion covers the area of ​​the second color concave cavity portion.

[0015] An optional technical solution of the present invention is that the injection molding mold includes a fourth mold body; the fourth mold body includes a fourth molding surface; and the fourth molding surface is the same as the first molding surface.

[0016] An optional technical solution of the present invention is that the chamfer radius of the first chamfered area is 0.2mm-1.0mm;

[0017] The length of the straight line area is 0.1mm-0.5mm;

[0018] The chamfer radius of the second chamfered area is 0.1 mm-1.0 mm.

[0019] Based on the above second purpose, the injection molding method provided by the present invention uses the injection molding mold, comprising the following steps:

[0020] The second mold body is molded together with the first mold body to form a first color cavity;

[0021] Injecting glue into the first color mold cavity to produce a first color body of the injection molded embryo body in the first color mold cavity;

[0022] The second mold body is separated from the first mold body, and the first color body of the injection molded embryo body is located on the first mold body;

[0023] The third mold body is molded together with the first mold body to form a second color cavity;

[0024] Injecting glue into the second color mold cavity so that the second color mold cavity produces a second color body of the injection molded embryo body on the first color body of the injection molded embryo body;

[0025] The third mold body is separated from the first mold body, and the injection molded embryo body is taken out.

[0026] An optional technical solution of the present invention is that the injection molding method includes a fourth mold body; the fourth mold body includes a fourth molding surface; the fourth molding surface is the same as the first molding surface;

[0027] While the third mold body is molded together with the first mold body, the fourth mold body is molded together with the second mold body to form a first color cavity;

[0028] While injecting glue into the second color cavity, inject glue into the first color cavity, so that the first color cavity produces a first color body of the injection molded embryo body A;

[0029] While the third mold body is separated from the first mold body, the fourth mold body is separated from the second mold body, and the first color body of the injection molded embryo body A is located on the fourth mold body;

[0030] The third mold body and the fourth mold body are molded together to form a second color cavity; at the same time, the second mold body and the first mold body are molded together to form a first color cavity;

[0031] Injecting glue into the second color mold cavity, so that the second color mold cavity produces the second color body of the injection molded body A on the first color body of the injection molded body A; at the same time, injecting glue into the first color mold cavity, so that the first color mold cavity produces the first color body of the injection molded body B;

[0032] The third mold body is separated from the fourth mold body, and the injection molded body A is taken out; at the same time, the second mold body is separated from the first mold body, and the first color body of the injection molded body B is located on the first mold body.

[0033] An optional technical solution of the present invention is that the injection molding method further comprises the following steps:

[0034] The surface covering layer of the second color body is removed from the injection molded body that has passed the inspection to form a first semi-finished product; wherein the surface covering layer of the second color body is a side of the second color body away from the first color body;

[0035] Loading the first semi-finished product into a degreasing kiln, performing thermal degreasing at 600°C-800°C for 40h-60h, and forming a second semi-finished product;

[0036] The qualified second semi-finished product is loaded into the main kiln and sintered at 1400℃-1500℃ for 25h-35h to form the third semi-finished product;

[0037] The third semi-finished product that has passed the inspection has its surface layer removed to form a finished product.

[0038] An optional technical solution of the present invention is that the third semi-finished product is formed into a finished product by removing the surface layer thereof, comprising:

[0039] According to the design requirements, the third semi-finished product is subjected to surface grinding to remove a fixed size to form a fourth semi-finished product;

[0040] The fourth semi-finished product is roughly ground, and rough polishing and fine polishing processes are used to obtain the finished product.

[0041] An optional technical solution of the present invention is that the second color cavity includes a second color convex cavity portion connected to the second color concave cavity portion; the second color convex cavity portion protrudes from the first color cavity; along a direction perpendicular to the mold closing direction, the area of ​​the second color convex cavity portion covers the area of ​​the second color concave cavity portion;

[0042] The surface covering layer of the second color body is removed, including the second color convex cavity portion, the second chamfered area of ​​the second color concave cavity portion, and part or all of the straight line area of ​​the second color concave cavity portion.

[0043] Based on the third object, the injection molded body provided by the present invention is formed by injection molding using the injection molding mold; the injection molded body includes a first color body and a second color body fixedly arranged on the first color body;

[0044] The first color cavity of the injection molding mold is used for injection molding to produce a first color body;

[0045] The second color cavity of the injection molding mold is used for injection molding to produce a second color body.

[0046] Based on the third object, the injection molded product provided by the present invention is processed by an injection molded embryo body, and the injection molded product includes a first color body,

[0047] It also includes a second color body corresponding portion formed by a second color concave cavity portion having a first chamfered area, or it also includes a second color body corresponding portion formed by a second color concave cavity portion having a first chamfered area and part or all of a straight line area.

[0048] Beneficial effects of the present invention:

[0049] The injection molding mold provided by the present invention comprises a first mold body, a second mold body and a third mold body; the first molding surface of the first mold body and the second molding surface of the second mold body can form a first color cavity, so as to produce a first color body of an injection molded body by injection molding of the first color cavity; the second color cavity can be formed by the first color cavity of the first mold body and the third molding surface of the third mold body, so as to produce a second color body of the injection molded body by injection molding of the second color cavity on the first color body of the injection molded body. The first chamfered area, the straight area and the second chamfered area are connected in sequence through the second molding surface. The second chamfered area and the first chamfered area make it easy to demold the second mold body from the first color body, and can also improve the compression and impact strength of the injection molded body, relieve the injection pressure of the second color body, reduce local cracking or dark cracks of the injection molded body, and improve the mechanical properties of the injection molded body; the straight area can basically avoid the phenomenon of color transmission and color mixing between the first color body and the second color body when injecting the second color body, so as to improve the quality of the injection molded body; the injection molded body is machined to remove the second chamfered area and all or part of the straight area to obtain a finished product with basically no color transmission and color mixing at the color junction, thereby improving the appearance effect and quality of the finished product.

[0050] The injection molding method provided by the present invention uses an injection molding mold, through a first chamfered area, a straight area and a second chamfered area, the second chamfered area and the first chamfered area make it easy for the second mold body to be demolded from the first color body, and can also improve the compression and impact strength of the injection molded body, relieve the injection pressure of the second color body, reduce local cracking or dark cracking of the injection molded body, and improve the mechanical properties of the injection molded body; the straight area can basically avoid the first color body and the second color body from having color transmission and color mixing when injecting the second color body, so as to improve the quality of the injection molded body; the injection molded body is machined to remove the second chamfered area and all or part of the straight area to obtain a finished product with basically no color transmission and color mixing at the color junction, thereby improving the appearance effect and quality of the finished product.

[0051] The injection molded embryo and injection molded product provided by the present invention are formed by injection molding using an injection molding mold. The second chamfered area and all or part of the straight line area can be removed by machining to obtain a finished product with basically no color transmission or color mixing at the color junction, thereby improving the appearance effect and quality of the finished product. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0053] Figure 1A cross-sectional view of an injection molding die provided in Embodiment 1 of the present invention;

[0054] Figure 2 for Figure 1 An enlarged view of area A of the injection molding mold shown;

[0055] Figure 3 for Figure 1 An enlarged view of area B of the injection molding mold shown;

[0056] Figure 4 for Figure 3 An enlarged view of area C of the injection molding mold shown;

[0057] Figure 5 for Figure 4 A schematic diagram of a C region of an injection molding mold with hidden cross-section lines shown;

[0058] Figure 6 A schematic diagram of a first mold body and a fourth mold body of an injection molding mold provided in Embodiment 1 of the present invention;

[0059] Figure 7 Schematic diagram of the second mold body and the third mold body of the injection molding mold provided in Example 1 of the present invention.

[0060] Icon: 100-injection molding mold; 110-first mold body; 111-first molding surface; 120-second mold body; 121-second molding surface; 1211-first chamfered area; 1212-straight area; 1213-second chamfered area; 130-third mold body; 131-third molding surface; 140-fourth mold body; 141-fourth molding surface; 150-first color cavity; 160-second color cavity; 161-second color concave cavity portion; 162-second color convex cavity portion; 200-injection molded body; 210-first color body; 220-second color body. DETAILED DESCRIPTION

[0061] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0062] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0063] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0064] Embodiment 1

[0065] See also Figure 1-Figure 7 As shown, this embodiment provides an injection molding mold; Figure 1 A cross-sectional view of the injection molding die provided in this embodiment, Figure 6 Schematic diagram of the first mold body and the fourth mold body of the injection molding mold, Figure 7 Schematic diagram of the second and third mold bodies of the injection molding mold; in order to show the structure more clearly, Figure 2 for Figure 1 An enlarged view of area A of the injection molding mold is shown. Figure 3 for Figure 1 An enlarged view of area B of the injection molding mold is shown. Figure 4 for Figure 3 An enlarged view of area C of the injection molding mold shown; Figure 5 for Figure 4 The schematic diagram of the C area hidden section line of the injection molding mold shown. Figure 1-Figure 4 Only the injection molded parts are displayed with cross-hatching, and the cross-hatching of other cross-sectional structures is hidden; Figure 4 and Figure 5 The second color cavity is separated by a dotted line into a second color concave cavity portion and a second color convex cavity portion, Figure 5 The first chamfered area, the straight area and the second chamfered area are separated by short dashed lines.

[0066] See also Figure 1-Figure 7As shown, the injection molding mold provided in this embodiment is suitable for injection molding of two-color or multi-color products; it can prevent two or more different colors of products from having color transmission after molding, sintering, and processing, and have no poor appearance, which can improve the overall appearance of the product and the quality of the product. The injection molding mold can be applied to injection molding products such as plastics and ceramics, and is particularly suitable for products made of ceramics, metals, and some high-hardness plastics.

[0067] The injection molding die 100 includes a first mold body 110 , a second mold body 120 and a third mold body 130 ; the first mold body 110 is provided with a first molding surface 111 , the second mold body 120 is provided with a second molding surface 121 ; the third mold body 130 is provided with a third molding surface 131 .

[0068] When the first mold body 110 and the second mold body 120 are molded together, the first molding surface 111 and the second molding surface 121 form a first color cavity 150; the first color cavity 150 is used to produce a first color body 210 of the injection molded body 200, such as Figure 2-Figure 5 shown.

[0069] When the first mold body 110 and the third mold body 130 are molded together, the first color cavity 150 and the third molding surface 131 form a second color cavity 160; that is, the first color body 210 and the third molding surface 131 form the second color cavity 160; the second color cavity 160 is used to produce the second color body 220 of the injection molded body 200; wherein, part or all of the second molding surface 121 is the interface between the first color cavity 150 and the second color cavity 160.

[0070] The second color cavity 160 includes a second color concave cavity portion 161 disposed in the first color cavity 150 ; that is, a portion of the second color body 220 formed by the second color concave cavity portion 161 is disposed in the first color body 210 .

[0071] Along the mold closing direction, the second molding surface 121 includes a first chamfered area 1211, a straight area 1212, and a second chamfered area 1213 connected in sequence; the first chamfered area 1211, the straight area 1212, and the second chamfered area 1213 form the side wall of the second color concave cavity 161. That is, the first chamfered area 1211, the straight area 1212, and the second chamfered area 1213 are the boundaries between the first color body 210 and the second color body 220. Among them, the first chamfered area 1211 is located at the bottom of the second color concave cavity 161, and the second chamfered area 1213 is located at the cavity opening of the second color concave cavity 161. Through the first chamfered area 1211, it is possible to prevent the second color body 220 from breaking the root of the first color body 210 during the injection molding process, and it is also possible to improve the overall strength of the injection molded embryo 200, thereby improving the overall strength of the finished product. The straight area 1212 provides a clear color overlap to basically avoid the color see-through and color mixing phenomenon at the color junction, and can also ensure that during the CNC processing of the surface excess of the injection molded body 200, the appearance cross-sectional area of ​​the first color body 210 and the second color body 220 of the finished product will not change due to the change of the demolding angle. The second chamfer area 1213 can relieve the injection pressure of the second color body 220 during the injection process, reduce the stress of the injection molded body 200, and improve the overall strength of the injection molded body 200.

[0072] The injection molding mold described in this embodiment includes a first mold body 110, a second mold body 120 and a third mold body 130; the first molding surface 111 of the first mold body 110 and the second molding surface 121 of the second mold body 120 can form a first color cavity 150, so as to produce a first color body 210 of the injection molded body 200 by injection molding through the first color cavity 150; the second color cavity 160 can be formed by the first color cavity 150 of the first mold body 110 and the third molding surface 131 of the third mold body 130, so as to produce a second color body 220 of the injection molded body 200 by injection molding through the second color cavity 160 on the first color body 210 of the injection molded body 200. The first chamfered area 1211, the straight area 1212 and the second chamfered area 1213 are connected in sequence through the second molding surface 121. The second chamfered area 1213 and the first chamfered area 1211 can facilitate the demolding of the second mold body 120 from the first color body 210, and can also improve the compression and impact resistance of the injection molded body 200, relieve the injection pressure of the second color body 220, reduce local cracking or dark cracking of the injection molded body 200, and improve the mechanical properties of the injection molded body 200; the straight area 1212 can basically avoid the first color body 210 and the second color body 220 from having color transmission or color mixing when injecting the second color body 220, so as to improve the quality of the injection molded body 200; the injection molded body 200 removes the second chamfered area 1213 and all or part of the straight area 1212 by machining to obtain a finished product with basically no color transmission or color mixing at the color junction, thereby improving the appearance effect and quality of the finished product.

[0073] Alternatively, see Figure 4 As shown, the injection molding mold in this embodiment produces an injection molded body 200 by injection molding; the injection molded body 200 includes a first color body 210 and a second color body 220 fixedly disposed on the first color body 210;

[0074] The first color cavity 150 of the injection molding mold is used for injection molding to produce a first color body 210, and the second color cavity 160 of the injection molding mold is used for injection molding to produce a second color body 220. The first color body 210 and the second color body 220 have different colors.

[0075] Optionally, the injection molded product in this embodiment is processed using the injection molded embryo 200 , and the injection molded product includes a first color body 210 .

[0076] The injection molded product also includes a corresponding portion of a second color body 220 formed by a second color concave cavity portion 161 having a first chamfered area 1211, that is, the injection molded body 200 is processed to remove the second chamfered area 1213 and all straight areas 1212 to obtain a finished product with basically no color transparency or color mixing at the color junction, thereby improving the appearance and quality of the injection molded product.

[0077] Alternatively, the injection molded product further includes a corresponding portion of the second color body 220 formed by the second color concave cavity portion 161 having the first chamfered area 1211 and part or all of the straight area 1212. That is, the injection molded body 200 is processed to remove the second chamfered area 1213 and part or all of the straight area 1212 to obtain a finished product with substantially no color transmission or color mixing at the color boundary, thereby improving the appearance and quality of the injection molded product.

[0078] See also Figure 2-Figure 5 As shown, in an optional scheme of this embodiment, the second color cavity 160 includes a second color convex cavity portion 162 connected to the second color concave cavity portion 161; the second color convex cavity portion 162 protrudes from the first color cavity 150; optionally, a second color body 220 is formed by injection molding in the second color concave cavity portion 161 and the second color convex cavity portion 162.

[0079] In the direction perpendicular to the mold closing direction, the area of ​​the second color convex cavity portion 162 covers the area of ​​the second color concave cavity portion 161. Through the second color convex cavity portion 162, the second color body 220 in the second color concave cavity portion 161 can be completely filled in the second color concave cavity portion 161, thereby improving the appearance and quality of the finished product.

[0080] Optionally, along the mold closing direction, the thickness of the second color protruding cavity portion 162 is 0.3 mm-0.8 mm; for example, the thickness of the second color protruding cavity portion 162 is 0.3 mm, 0.4 mm, 0.45 mm, 0.65 mm, 0.7 mm, etc.

[0081] Optionally, along the mold closing direction, the thickness of the second color protruding cavity portion 162 is 0.5 mm.

[0082] In an optional solution of this embodiment, the injection molding mold includes a fourth mold body 140; the fourth mold body 140 includes a fourth molding surface 141; the fourth molding surface 141 is the same as the first molding surface 111. Optionally, the fourth mold body 140 is the same as the first mold body 110. The fourth mold body 140 is used to improve the production efficiency of the injection molded embryo 200. For example, the first mold body 110 and the fourth mold body 140 are fixed molds, and the second mold body 120 and the third mold body 130 are movable molds. The second mold body 120 and the first mold body 110 are first molded together to form a first color cavity 150 and inject the first color body 210 of the first injection molded embryo; then, the second mold body 120 is separated from the first mold body 110 and the first color body 210 of the first injection molded embryo is located on the first mold body 110; then, the third mold body 130 and the first mold body 110 are molded together to form a second color cavity 160 and inject the second color body 220 of the first injection molded embryo, and the fourth mold body 140 and the second mold body 120 are molded together to form a first color cavity 150 and inject the first color body 210 of the second injection molded embryo; then, the third mold body 130 and the first mold body 110 are molded together to form a second color cavity 160 and inject the second color body 220 of the first injection molded embryo; The first mold body 110 is separated from the first mold body 110 and the first injection molded body is taken out, the fourth mold body 140 is separated from the second mold body 120 and the first color body 210 of the second injection molded body is located on the fourth mold body 140; then, the third mold body 130 and the fourth mold body 140 are molded together to form the second color cavity 160 and the second color body 220 of the second injection molded body is produced by injection molding, the second mold body 120 and the first mold body 110 are molded together to form the first color cavity 150 and the first color body 210 of the third injection molded body is produced by injection molding; then, the third mold body 130 and the fourth mold body 140 are separated and the second injection molded body is taken out, the second mold body 120 and the first mold body 110 are separated and the first color body 210 of the third injection molded body is located on the first mold body 110; this cycle is repeated. That is, through the first mold body 110, the second mold body 120, the third mold body 130 and the fourth mold body 140, the injection molding efficiency of the injection molding mold is improved.

[0083] Optionally, the first mold body 110 and the fourth mold body 140 can be two mold bodies of a set of molds or mold bodies of two separate molds; optionally, the second mold body 120 and the third mold body 130 can be two mold bodies of a set of molds or mold bodies of two separate molds.

[0084] Optionally, the first mold body 110, the second mold body 120, the third mold body 130 and the fourth mold body 140 belong to a set of molds. Figure 1 , Figure 6 and Figure 7 As shown, the injection molding mold includes a fixed mold and a movable mold; the fixed mold includes a first mold body 110 and a fourth mold body 140, and the movable mold includes a second mold body 120 and a third mold body 130; by designing the first mold body 110, the second mold body 120, the third mold body 130 and the fourth mold body 140 as a set of molds, so that one injection molded embryo 200 can be injected by opening and closing the mold once, so as to improve the injection efficiency. It can be understood by those skilled in the art that the concepts of the fixed mold and the movable mold are relative, and the second mold body 120 and the third mold body 130 can be swapped by rotating the movable mold, and the first mold body 110 and the fourth mold body 140 can also be swapped by rotating the fixed mold.

[0085] In an optional solution of this embodiment, along the mold closing direction, the thickness of the second color concave cavity 161 is 0.4 mm-2.5 mm. For example, the thickness of the second color concave cavity 161 is 0.4 mm, 0.85 mm, 1.25 mm, 1.5 mm, 1.8 mm, 2.5 mm, etc.

[0086] Optionally, along the mold closing direction, the thickness of the second color concave cavity portion 161 is 1.0 mm.

[0087] In an optional solution of this embodiment, the chamfer radius of the first chamfer area 1211 is 0.2 mm-1.0 mm; for example, the chamfer radius of the first chamfer area 1211 is 0.2 mm, 0.3 mm, 0.45 mm, 0.6 mm, 0.8 mm, 1.0 mm, etc.

[0088] Optionally, the chamfer radius of the first chamfered area 1211 is 0.4 mm.

[0089] Optionally, the length of the straight area 1212 is 0.1 mm-0.5 mm; for example, the length of the straight area 1212 is 0.1 mm, 0.2 mm, 0.25 mm, 0.35 mm, 0.5 mm, etc.

[0090] Optionally, the length of the straight area 1212 is 0.4 mm.

[0091] Optionally, the chamfer radius of the second chamfered area 1213 is 0.1 mm-1.0 mm. For example, the chamfer radius of the second chamfered area 1213 is 0.1 mm, 0.3 mm, 0.45 mm, 0.6 mm, 0.8 mm, 1.0 mm, etc.

[0092] Optionally, the chamfer radius of the second chamfered area 1213 is 0.2 mm.

[0093] Embodiment 2

[0094] Embodiment 2 provides an injection molding method, which uses the injection molding mold described in Embodiment 1. The technical features of the injection molding mold disclosed in Embodiment 1 are also applicable to this embodiment, and the technical features of the injection molding mold disclosed in Embodiment 1 will not be described repeatedly.

[0095] Combined with the first embodiment Figure 1-Figure 7 As shown, the injection molding method provided in this embodiment is suitable for injection molding of two-color or multi-color products; it can make two or more different colors of products have no color transmission phenomenon after molding, sintering, and processing, and have no poor appearance, which can improve the overall appearance effect and quality of the product. The injection molding method can be applied to injection molding products such as plastics and ceramics, and is particularly suitable for ceramic products with high injection molding temperatures.

[0096] The injection molding method, using the injection molding mold described in the first embodiment, comprises the following steps:

[0097] The second mold body 120 is molded together with the first mold body 110 to form a first color cavity 150;

[0098] Injecting glue into the first color cavity 150 to produce a first color body 210 of the injection molded body 200 in the first color cavity 150;

[0099] The second mold body 120 is separated from the first mold body 110, and the first color body 210 of the injection molded body 200 is located on the first mold body 110;

[0100] The third mold body 130 is molded together with the first mold body 110 to form a second color cavity 160; that is, the first color body 210 is molded together with the first mold body 110 to form a second color cavity 160;

[0101] Injecting glue into the second color cavity 160 so that the second color cavity 160 produces the second color body 220 of the injection molded body 200 on the first color body 210 of the injection molded body 200;

[0102] The third mold body 130 is separated from the first mold body 110, and the injection molded body 200 is taken out. The injection molding method can prevent the second color body 220 from breaking the root of the first color body 210 during the injection molding process through the first chamfered area 1211, and can also improve the overall strength of the injection molded body 200, thereby improving the overall strength of the finished product. Through the first chamfered area 1211, the straight area 1212 and the second chamfered area 1213, the second chamfered area 1213 and the first chamfered area 1211 can facilitate the demolding of the second mold body 120 from the first color body 210, and can also improve the compression and impact resistance of the injection molded body 200, relieve the injection pressure of the second color body 220, reduce local cracking or dark cracking of the injection molded body 200, and improve the mechanical properties of the injection molded body 200; the straight area 1212 can basically avoid the first color body 210 and the second color body 220 from having color transmission and color mixing when injecting the second color body 220, so as to improve the quality of the injection molded body 200; the injection molded body 200 removes the second chamfered area 1213 and all or part of the straight area 1212 by machining to obtain a finished product with basically no color transmission and color mixing at the color junction, thereby improving the appearance effect and quality of the finished product.

[0103] Optionally, injection molding is performed in the first color cavity 150 by point-in-point injection.

[0104] Optionally, injection molding is performed in the second color cavity 160 by point-in-point injection.

[0105] In an optional solution of this embodiment, the injection molding method includes a fourth mold body 140; the fourth mold body 140 includes a fourth molding surface 141; the fourth molding surface 141 is the same as the first molding surface 111;

[0106] While the third mold body 130 is molded with the first mold body 110, the fourth mold body 140 is molded with the second mold body 120 to form a first color cavity 150;

[0107] While injecting glue into the second color cavity 160 , inject glue into the first color cavity 150 , so that the first color cavity 150 produces the first color body 210 of the injection molded embryo body A;

[0108] While the third mold body 130 is separated from the first mold body 110 , the fourth mold body 140 is separated from the second mold body 120 , and the first color body 210 of the injection molded embryo body A is located on the fourth mold body 140 ;

[0109] The third mold body 130 and the fourth mold body 140 are molded together to form a second color cavity 160, that is, the first color body 210 of the injection molded embryo body A is molded together with the fourth mold body 140 to form the second color cavity 160; at the same time, the second mold body 120 and the first mold body 110 are molded together to form a first color cavity 150;

[0110] Inject glue into the second color cavity 160 so that the second color cavity 160 produces the second color body 220 of the injection molded body A on the first color body 210 of the injection molded body A; at the same time, inject glue into the first color cavity 150 so that the first color cavity 150 produces the first color body 210 of the injection molded body B;

[0111] The third mold body 130 is separated from the fourth mold body 140 , and the injection molded body A is taken out; at the same time, the second mold body 120 is separated from the first mold body 110 , and the first color body 210 of the injection molded body B is located on the first mold body 110 .

[0112] In this cycle, a plurality of injection molded bodies 200 are obtained.

[0113] In an optional solution of this embodiment, the injection molding mold includes a fixed mold and a movable mold; the fixed mold includes a first mold body 110 and a fourth mold body 140 , and the movable mold includes a second mold body 120 and a third mold body 130 .

[0114] The injection molding method comprises the following steps:

[0115] Mold closing: When the movable mold and the fixed mold are closed, the third mold body 130 and the first mold body 110 are closed to form the second color cavity 160, and the fourth mold body 140 and the second mold body 120 are closed to form the first color cavity 150;

[0116] Glue injection: Glue is injected into the second color cavity 160 to produce the second color body 220 of the injection molded body 200 on the first color body 210 of the injection molded body 200, and glue is injected into the first color cavity 150 to produce the first color body 210 of the injection molded body A in the first color cavity 150;

[0117] Mold opening: when the movable mold and the fixed mold are opened, the third mold body 130 is separated from the first mold body 110 and the injection molded body 200 is taken out, the fourth mold body 140 is separated from the second mold body 120 and the first color body 210 of the injection molded body A is placed on the fourth mold body 140;

[0118] Rotation mold: the movable mold rotates 180 degrees so that the third mold body 130 corresponds to the fourth mold body 140, and the second mold body 120 corresponds to the first mold body 110;

[0119] Mold closing: When the movable mold and the fixed mold are closed, the third mold body 130 and the fourth mold body 140 are closed to form a second color cavity 160, that is, the first color body 210 of the injection molded embryo A is closed to form a second color cavity 160; the second mold body 120 and the first mold body 110 are closed to form a first color cavity 150;

[0120] Glue injection: Glue is injected into the second color mold cavity 160 so that the second color mold cavity 160 produces the second color body 220 of the injection molded body A on the first color body 210 of the injection molded body A; glue is injected into the first color mold cavity 150 so that the first color mold cavity 150 produces the first color body 210 of the injection molded body B;

[0121] Mold opening: When the movable mold and the fixed mold are opened, the third mold body 130 and the fourth mold body 140 are separated and the injection molded body A is taken out, the second mold body 120 and the first mold body 110 are separated and the first color body 210 of the injection molded body B is located on the first mold body 110.

[0122] Rotation mold: The movable mold rotates 180 degrees so that the second mold body 120 corresponds to the fourth mold body 140, and the third mold body 130 corresponds to the first mold body 110;

[0123] Mold closing: When the movable mold and the fixed mold are closed, the third mold body 130 and the first mold body 110 are closed to form the second color cavity 160, and the fourth mold body 140 and the second mold body 120 are closed to form the first color cavity 150;

[0124] In this cycle, a plurality of injection molded bodies 200 are obtained.

[0125] In an optional solution of this embodiment, the injection molding method comprises the following steps:

[0126] The surface covering layer of the second color body 220 is removed from the injection molded body 200 that has passed the inspection to form a first semi-finished product; wherein the surface covering layer of the second color body 220 is a side of the second color body 220 that is away from the first color body 210;

[0127] Loading the first semi-finished product into a degreasing kiln, performing thermal degreasing at 600°C-800°C for 40h-60h, and forming a second semi-finished product;

[0128] The qualified second semi-finished product is loaded into the main kiln and sintered at 1400℃-1500℃ for 25h-35h to form the third semi-finished product;

[0129] The third semi-finished product that has passed the inspection has its surface layer removed to form a finished product.

[0130] Optionally, removing the surface layer of the third semi-finished product to form a finished product includes:

[0131] According to design requirements, a fixed size is removed from the surface of the third semi-finished product using a grinder to form a fourth semi-finished product; optionally, a double-sided grinder is used to process the third semi-finished product into the fourth semi-finished product.

[0132] The fourth semi-finished product is roughly ground, and rough polishing and fine polishing processes are used to obtain the finished product.

[0133] Optionally, the second color cavity 160 includes a second color convex cavity portion 162 connected to the second color concave cavity portion 161; the second color convex cavity portion 162 protrudes from the first color cavity 150; along the direction perpendicular to the mold closing direction, the area of ​​the second color convex cavity portion 162 covers the area of ​​the second color concave cavity portion 161;

[0134] The surface covering layer of the second color body 220 including the second color convex cavity portion 162 , the second chamfered area 1213 of the second color concave cavity portion 161 and part or all of the straight area 1212 of the second color concave cavity portion 161 is removed.

[0135] The optional sizes of the first chamfered area 1211, the straight area 1212 and the second chamfered area 1213 have been described in detail in the first embodiment and will not be repeated here. Other features disclosed in the first embodiment are also applicable to this embodiment.

[0136] The injection molding method and the injection molded body 200 described in this embodiment have the advantages of the injection molding mold described in the first embodiment. The advantages of the injection molding mold disclosed in the first embodiment will not be repeatedly described here.

[0137] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. An injection molding mold, characterized in that: It comprises a first mold body, a second mold body and a third mold body; the first mold body is provided with a first molding surface, the second mold body is provided with a second molding surface; the third mold body is provided with a third molding surface; When the first mold body and the second mold body are molded together, the first molding surface and the second molding surface form a first color cavity; When the first mold body and the third mold body are molded together, the first color cavity and the third molding surface form a second color cavity; wherein part or all of the second molding surface is the interface between the first color cavity and the second color cavity; The second color cavity comprises a second color concave cavity portion disposed within the first color cavity; Along the mold closing direction, the second molding surface includes a first chamfered area, a straight area, and a second chamfered area connected in sequence; the first chamfered area, the straight area, and the second chamfered area form the side wall of the second color concave cavity; The first color cavity is used to produce a first color body of the injection molded body, and the second color cavity is used to produce a second color body of the injection molded body; the first chamfered area, the straight area and the second chamfered area are the boundaries between the first color body and the second color body; The second color cavity comprises a second color convex cavity portion connected to the second color concave cavity portion; the second color convex cavity portion protrudes from the first color cavity; In a direction perpendicular to the mold closing direction, the area of ​​the second color convex cavity portion covers the area of ​​the second color concave cavity portion.

2. The injection molding die according to claim 1, characterized in that: It includes a fourth mold body; the fourth mold body includes a fourth molding surface; the fourth molding surface is the same as the first molding surface.

3. The injection molding die according to claim 1, characterized in that: The chamfer radius of the first chamfered area is 0.2mm-1.0mm; The length of the straight line area is 0.1mm-0.5mm; The chamfer radius of the second chamfered area is 0.1 mm-1.0 mm.

4. An injection molding method, characterized in that: Using the injection molding mold according to any one of claims 1 to 3 comprises the following steps: The second mold body is molded together with the first mold body to form a first color cavity; Injecting glue into the first color mold cavity to produce a first color body of the injection molded embryo body in the first color mold cavity; The second mold body is separated from the first mold body, and the first color body of the injection molded embryo body is located on the first mold body; The third mold body is molded together with the first mold body to form a second color cavity; Injecting glue into the second color mold cavity so that the second color mold cavity produces a second color body of the injection molded embryo body on the first color body of the injection molded embryo body; The third mold body is separated from the first mold body, and the injection molded embryo body is taken out.

5. The injection molding method according to claim 4, characterized in that: comprising a fourth mold body; the fourth mold body comprising a fourth molding surface; the fourth molding surface being the same as the first molding surface; While the third mold body is molded together with the first mold body, the fourth mold body is molded together with the second mold body to form a first color cavity; While injecting glue into the second color cavity, inject glue into the first color cavity, so that the first color cavity produces a first color body of the injection molded embryo body A; While the third mold body is separated from the first mold body, the fourth mold body is separated from the second mold body, and the first color body of the injection molded embryo body A is located on the fourth mold body; The third mold body and the fourth mold body are molded together to form a second color cavity; at the same time, the second mold body and the first mold body are molded together to form a first color cavity; Injecting glue into the second color mold cavity, so that the second color mold cavity produces the second color body of the injection molded body A on the first color body of the injection molded body A; at the same time, injecting glue into the first color mold cavity, so that the first color mold cavity produces the first color body of the injection molded body B; The third mold body is separated from the fourth mold body, and the injection molded body A is taken out; at the same time, the second mold body is separated from the first mold body, and the first color body of the injection molded body B is located on the first mold body.

6. The injection molding method according to claim 4 or 5, characterized in that: The following steps are also included: The surface covering layer of the second color body is removed from the injection molded body that has passed the inspection to form a first semi-finished product; wherein the surface covering layer of the second color body is a side of the second color body away from the first color body; Loading the first semi-finished product into a degreasing kiln, performing thermal degreasing at 600°C-800°C for 40h-60h, and forming a second semi-finished product; The qualified second semi-finished product is loaded into the main kiln and sintered at 1400℃-1500℃ for 25h-35h to form the third semi-finished product; The third semi-finished product that has passed the inspection has its surface layer removed to form a finished product.

7. The injection molding method according to claim 6, characterized in that: The third semi-finished product removes the surface layer to form a finished product including: According to the design requirements, the third semi-finished product is subjected to surface grinding to remove a fixed size to form a fourth semi-finished product; The fourth semi-finished product is roughly ground, and rough polishing and fine polishing processes are used to obtain the finished product.

8. The injection molding method according to claim 6, characterized in that: The surface covering layer of the second color body is removed, including the second color convex cavity portion, the second chamfered area of ​​the second color concave cavity portion, and part or all of the straight line area of ​​the second color concave cavity portion.

9. An injection molded product, characterized in that: The injection molded product is formed by injection molding a molded body produced by injection molding according to any one of claims 1 to 3; the injection molded body comprises a first color body and a second color body fixedly arranged on the first color body; the injection molded product comprises the first color body, It also includes a second color body corresponding portion formed by a second color concave cavity portion having a first chamfered area, or it also includes a second color body corresponding portion formed by a second color concave cavity portion having a first chamfered area and part or all of a straight line area.

Citation Information

Patent Citations

  • Three-colour injection mould

    CN104526980A

  • Injection mold

    CN107839165A

  • Bicolor mold

    CN201559292U

  • Mold for bi-color light-transmitting air conditioner panel

    CN203901648U

  • Injection moulding mould and idiosome and injection molding of moulding plastics

    CN208290375U