Roll-to-roll injection molding inspection punching and welding production line and its process

By designing a roll-to-roll injection molding inspection, punching, and welding production line, defective injection molded parts can be detected and processed in real time. This solves the problem of unusable empty spaces on the material strip, improves the automation level and inspection efficiency of the production line, and ensures the efficient operation of downstream manufacturers' production lines.

CN110696279BActive Publication Date: 2024-11-01SUZHOU KEYTEC PRECISION COMPONENTS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911059007.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-11-01
Publication Date
2024-11-01
Estimated Expiration
2039-11-01

AI Technical Summary

Technical Problem

In existing injection molding production lines, the empty spaces on the material strip cannot be utilized, resulting in reduced production line efficiency for downstream manufacturers. Furthermore, existing testing methods are labor-intensive, inefficient, and unreliable, making it difficult to control the injection molding pass rate.

Method used

Design a roll-to-roll injection molding inspection, punching, and welding production line, including feeding, injection molding, inspection, welding, and receiving devices. The inspection system detects defective injection molded parts in real time, and the punching and welding device cuts and welds the defective strip to ensure the number of qualified injection molded parts per unit length of strip.

Benefits of technology

It enables automated detection and handling of defective injection molded parts, reduces empty spaces on the material strip, improves the production line efficiency of downstream manufacturers, reduces labor intensity, and improves the reliability and efficiency of detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110696279B_ABST
    Figure CN110696279B_ABST
Patent Text Reader

Abstract

The present invention discloses a roll-to-roll injection molding inspection, punching and welding production line, comprising: a discharge device, which unfolds the material strip and sends it to the injection molding machine; an injection molding machine and a mold, which perform injection molding on the material strip; a detection system, which detects the material strip and products before and after injection molding and before and after punching and welding, timely discovers or avoids defective products, and protects the mold; a welding system, which performs punching and welding on the material strip; a material collection device, which counts and reels the injection molded products on the finished material strip; and a material strip driving system, which drives the material strip to move between the discharge device and the material collection device. Among them, the punching and welding device of the welding system can not only punch out unqualified injection molded products on the material strip, but also cut off the material strip containing unqualified products, and then automatically weld the front and rear material strips, so as to ensure that each roll of the finished material strip produced has a specified number of qualified products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention particularly relates to an injection molding production line. Background Art

[0002] Injection molding of terminals is a common processing method. Generally, the terminals to be molded are first sent to the injection mold by a pulling machine, and then injection molding is performed. During this processing, both the terminals to be molded and the molded parts after injection molding need to be inspected. On the one hand, it is to prevent the deformed terminals to be molded from damaging the injection mold, and on the other hand, it is to prevent unqualified products after injection molding from flowing into the next process. However, most of the existing inspections are carried out through manual inspections, which have high labor intensity, low work efficiency and low reliability of inspection results. In addition, for unqualified injection molded parts, it is necessary to use a punching tool to punch the injection molded parts off the material strip to ensure that the injection molded parts on the material strip are all qualified products to meet the customer's usage needs.

[0003] The above parts can be automatically produced through automatic material pulling devices, automatic detection devices, and automatic punching devices. However, after punching, although the injection molded parts on the material strip are guaranteed to be qualified, a vacant space will be left after the injection molded parts on the material strip are punched. In this way, the punched material strip faces such a problem on the production line of the downstream manufacturer: the vacant space on the material strip cannot be used and can only be passed empty. If there are too many vacancies on a certain length of material strip, the production line efficiency of the downstream manufacturer will be reduced. In order to ensure the production line efficiency of downstream manufacturers, it is necessary to control the number of vacancies on the material strip within a certain range. Because there are too many factors affecting the qualified rate of terminal injection molding on the actual injection molding production line, it is difficult to control the qualified rate in the injection molding stage.

[0004] The existing practice is that the automatic detection device counts during detection, and the automatic material pulling device records the length of the material strip. When the number of unqualified injection molded parts on a certain length of the material strip exceeds a set value, the material strip is directly cut off and then welded. Because during the injection molding process, the injection molding machine generally injects multiple terminals at the same time. When one injection molded part is unqualified, it generally means that a batch of injection molded parts injected at the same time are all unqualified. Therefore, when punching, all the material strips where this batch of injection molded parts are located can be punched out, so that the number of vacancies on a section of the material strip can be reduced.

[0005] This method requires cutting the material strip and welding, which cannot be implemented on the existing automated production line. The existing production line needs to be improved to realize the functions of punching and welding the material strip. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide a roll-to-roll injection molding inspection, punching and welding production line, which automatically detects the terminals of the material strip after injection molding, punches out unqualified injection-molded parts from the material strip, and cuts and welds the material strip when there are too many unqualified injection-molded parts on the material strip, so as to ensure the number of qualified injection-molded parts per unit length of the material strip.

[0007] In order to solve the above technical problems, the present invention is implemented by the following technical solutions: a roll-to-roll injection molding detection punching and welding production line, comprising:

[0008] The unwinding device unwinds the rolled material strip and delivers it to the production line;

[0009] Injection molding machine, which performs injection molding on the material strip;

[0010] Injection molds;

[0011] Inspection system, inspecting the material strip before and after injection molding;

[0012] The welding system includes a punching and welding device and a simple welding device. The simple welding device is arranged after the unwinding device to weld different rolls of material strips into a continuous material strip. The punching and welding device and the simple welding device share a set of welding machine inverter power supply. The punching and welding device is arranged between the detection system and the receiving device to punch and weld the material strips that fail the detection.

[0013] The material receiving device rewinds the material strip that has passed through the injection molding machine, the detection system, and the welding system, and counts the injection molded parts on the material strip;

[0014] The material belt drive system drives the material belt to move between the unwinding device and the receiving device;

[0015] The punching and welding device comprises a movable slide, on which an injection molded part punching mechanism, a material strip punching mechanism and a welding electrode pressing adjustment mechanism are arranged, the movable slide can be moved so that one of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism is aligned with the material strip, the injection molded part punching mechanism can cut off the injection molded part on the material strip, and the material strip punching mechanism can cut off the material strip, the material strip driving system comprises a first material strip driving device arranged between the punching and welding device and the material receiving device, the first material strip driving device can act in both directions, driving the material strip to move from the punching and welding device to the material receiving device or move in the reverse direction, the first material strip driving device moves in the reverse direction so that the cut front section of the material strip is retreated and spliced ​​with the cut rear section of the material strip at the punching and welding device, and the welding electrode pressing adjustment mechanism presses and welds the spliced ​​material strips;

[0016] Among them, the detection system also detects the material strip after welding.

[0017] Furthermore, a movable slide is arranged below the material strip, and the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are fixed on the movable slide through a support frame, and the material strip passes through the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism. The fixed parts of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are all arranged on the slide and located below the material strip, and the movable parts are all arranged on the support frame and located above the material strip.

[0018] Furthermore, the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are arranged in a straight line in sequence on the movable slide, and the driving mechanism of the movable slide drives the movable slide to move linearly so that the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are aligned with the material strip respectively.

[0019] Furthermore, the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are arranged circumferentially on the movable slide, and the driving mechanism of the movable slide drives the movable slide to rotate so that the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are respectively aligned with the material strip.

[0020] Furthermore, the driving mechanism of the movable slide is a stroke-controllable driving mechanism or a two-stage fixed-stroke driving mechanism.

[0021] Furthermore, both the injection molded part punching mechanism and the material strip punching mechanism include a punching die, and the punching dies of the two mechanisms are arranged on the same punching machine or on different punching machines.

[0022] Further, the detection system includes a first detection device, which includes a front camera to photograph the front of the injection-molded material strip for detection;

[0023] The first detection device also includes an oblique camera, which is aimed at the material strip in the injection mold of the injection molding machine to photograph the material strip before and after the injection mold is molded;

[0024] The first detection device also includes a lighting lamp. The lighting lamp and the camera are both arranged in a box body. The box body is arranged on a fixed mold plate of the injection molding machine. A heat insulation board is arranged between the box body and the fixed mold. A fan and heat dissipation holes are arranged on one side of the box body. The heat insulation board is connected to a slide rail and a locking mechanism. The box body can move on the slide rail to approach or move away from the movable mold. The heat insulation board is provided with a cooling device. The cooling device can connect cooling water to the heat insulation board to cool the heat insulation board.

[0025] Furthermore, the detection system includes a second detection device, which includes a side camera to photograph the side of the material strip after injection molding for detection. The second detection device also includes a positioning mechanism, and the material strip passes through the middle of the positioning mechanism. The positioning mechanism includes a pressure head that can move up and down, and the pressure head can press the material strip to vertically position the material strip. The pressure head is provided with a contact sensor and / or an eccentric detection head to detect the size of the injection molded parts on the material strip when the material strip is vertically positioned. The second detection device also includes an adaptation detection tool, and the adaptation detection tool is provided with a tooling that cooperates with the injection molded parts on the material strip. The adaptation detection tool is actuated to perform adaptation testing on the tooling and the injection molded parts. The detection system also includes a welding and punching detection device. The incision detection device is arranged after the welding and punching device, and detects the incision of the injection molded parts on the material strip or the welding part of the material strip through a probe or a contact sensor.

[0026] Furthermore, the welding electrode pressing adjustment mechanism includes a base and a pressing head. The base is provided with a lifting block. The lifting block is arranged on the side of the material strip cut close to the front section of the material strip. The lifting block is lifted to make the front section of the material strip retreat to above the rear section of the material strip. An elastic pressing die is provided on the pressing head. The pressing head is pressed downward to make the elastic pressing die press the front section of the material strip and the rear section of the material strip together so that the welding electrode contacts the material strip.

[0027] A strip punching and welding process, characterized in that it comprises the following steps:

[0028] In the first step, a section of a strip is cut off and removed by using a strip punching mechanism, and the cut shapes of the front and rear sections of the strip after cutting are mutually engageable, and a plurality of overlapping points are distributed on the cuts;

[0029] In the second step, the front end of the cut material strip is returned to the top of the rear end of the material strip by using the material strip driving mechanism and the cuts are aligned, so that the front end of the material strip and the rear end of the material strip overlap at the overlap point;

[0030] In the third step, the welding mechanism presses the front section material strip and the rear section material strip together and spot welds them at the overlapping points to weld the front section material strip and the rear section material strip together.

[0031] The present invention is beneficial in that:

[0032] 1) After the terminal is injected in the injection molding machine, the detection system takes a photo of the material strip for detection. When unqualified injection molded parts are detected, the injection molded parts punching mechanism on the punching and welding device punches out the unqualified injection molded parts on the material strip, so that a vacancy is formed on the material strip. At the same time, the material strip drive system records the length of the material strip, and the detection system records the number of unqualified injection molded parts. When the number of unqualified injection molded parts recorded within a set material strip length exceeds the set value, the material strip punching mechanism on the punching and welding device cuts off and removes the material strip segment containing the unqualified injection molded parts, and the first material strip drive device moves in the opposite direction to make the cut front section of the material strip retreat and splice with the cut rear section of the material strip at the punching and welding device, and the welding electrode pressing adjustment mechanism presses and welds the spliced ​​material strips. In the above manner, the number of unqualified injection molded parts within the set material strip length can be controlled within the set value, and the number of qualified injection molded parts per unit length of the material strip can be guaranteed.

[0033] 2) The first detection device is installed on the injection molding machine, which can detect the injection molded parts immediately after injection molding. If the injection molded parts are detected to be unqualified, the injection molding machine can be immediately suspended through the control system, and maintenance personnel can perform inspections and maintenance to prevent the injection molding machine from producing unqualified injection molded parts in batches. The lighting lamp and camera are both installed in the box to protect their service life from being affected by the heat of the injection molding machine.

[0034] 3) In the second detection device, the side camera, the contact sensor and / or the eccentric detection head on the pressure head, and the matching detection tool cooperate with each other to perform detection, with high detection accuracy, and can detect multiple features of the injection molded parts.

[0035] 4) The mold can be replaced and debugged easily. The box with the camera can be moved easily when the mold is opened or closed. The conveyor wheels for the material belts above and below the mold can be moved easily, and it is also easy to return to the working position. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 It is an overall schematic diagram of the present invention;

[0037] Figure 2 This is a schematic diagram of the injection molding part of the present invention;

[0038] Figure 3 It is a partial schematic diagram of the punching and welding device of the present invention;

[0039] Figure 4 This is Embodiment 1 of the punching and welding device of the present invention;

[0040] Figure 5 This is the second embodiment of the punching and welding device of the present invention;

[0041] Figure 6 It is a schematic diagram of the welding electrode pressing adjustment mechanism of the present invention;

[0042] Figure 7This is a schematic diagram of the cutting and splicing of the material strip of the present invention;

[0043] Figure 8 for Figure 7 A partial schematic diagram of . DETAILED DESCRIPTION

[0044] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments:

[0045] like Figures 1 to 7 As shown, a roll-to-roll injection molding inspection punching and welding production line includes: a discharge device 1, which unwinds the rolled material strip 8 and sends it to the production line; an injection molding machine 2, which performs injection molding on the material strip; an injection mold 3; a detection system, which takes photos to detect the material strip 8 after injection molding; a welding system, which includes a punching and welding device 51 and a simple welding device 52, wherein the punching and welding device 51 is arranged between the detection system and the material receiving device 6, and punches and welds the material strip 8 that fails the inspection, and the simple welding device 52 is arranged after the discharge device 1, and welds the material strips 8 of different rolls into a continuous material strip 8, and the punching and welding device 51 and the simple welding device 52 share a set of welding machine inverter power supply; a material receiving device 6, which rewinds the material strip 8 and counts the injection molded parts on the material strip 8; a material strip driving system, which drives the material strip to move between the discharge device 1 and the material receiving device 6; wherein the punching and welding device 51 includes a movable slide 511, the movable slide 511 is provided with an injection molded part punching mechanism, a material strip punching mechanism and a welding electrode pressing adjustment mechanism. The movable slide 511 can be moved so that one of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 is aligned with the material strip 8. The injection molded part punching mechanism can cut off the injection molded parts on the material strip 8, and the material strip punching mechanism can cut the material strip 8. The material strip driving system includes a first material strip driving device 71 arranged between the punching and welding device 51 and the material receiving device 6. The first material strip driving device 71 can act in both directions to drive the material strip 8 to move from the punching and welding device 51 to the material receiving device 6 or move in the opposite direction. The first material strip driving device 71 moves in the opposite direction to make the cut front section material strip 81 retreat and be spliced ​​with the cut rear section material strip 82 at the punching and welding device 51, and the welding electrode pressing adjustment mechanism 515 presses and welds the spliced ​​material strip 8.

[0046] The unloading device 1 releases the rolled material strip 8, and pulls it to the injection molding machine 2 for injection molding through the material strip driving system. After the terminal is injected in the injection molding machine 2, the detection system takes a photo of the material strip 8 for detection. When unqualified injection molded parts are detected, the injection molded parts punching mechanism on the punching and welding device 51 punches out the unqualified injection molded parts on the material strip 8, so that a vacancy is formed on the material strip 8. At the same time, the material strip driving system records the length of the material strip 8, and the detection system records the number of unqualified injection molded parts. When the number of unqualified injection molded parts recorded within a set material strip length exceeds the set value, the material strip punching mechanism on the punching and welding device 51 cuts off and removes the material strip segment containing the unqualified injection molded parts, and the first material strip driving device 72 moves in the opposite direction to make the cut front section material strip 81 retreat and splice with the cut rear section material strip 82 at the punching and welding device 51, and the welding electrode pressing adjustment mechanism 515 presses and welds the spliced ​​material strip 8. By means of the above method, the number of unqualified injection molded parts within a set length of the material strip 8 can be controlled within a set value, thereby ensuring the number of qualified injection molded parts on a unit length of the material strip 8 .

[0047] In this embodiment, the movable slide 511 is arranged below the material strip 8, and the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are fixed on the movable slide 511 through the support frame 512, and the material strip 8 passes through the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515. The fixed parts of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are all arranged on the slide and located below the material strip, and the movable parts are all arranged on the support frame and located above the material strip. Specifically, the injection molding part punching mechanism includes an injection molding part punching movable die 5131 and an injection molding part punching fixed die 5132, the strip punching mechanism includes a strip punching movable die 5141 and a strip punching fixed die 5142, the welding electrode pressing adjustment mechanism 515 includes a base 5151 and a pressing head, and the injection molding part punching fixed die 5132, the strip punching fixed die 5142 and the base 5151 are arranged on the movable slide 511. Figure 4 and 5 shown.

[0048] In this embodiment, the injection molding part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are arranged in a straight line on the movable slide 511, and the driving mechanism of the movable slide 511 drives the movable slide to move linearly so that the injection molding part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are respectively aligned with the material strip 8. Figure 4 and 5 shown.

[0049] In another embodiment, the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are arranged in a circle on the movable slide 511, and the driving mechanism of the movable slide 511 drives the movable slide 511 to rotate so that the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 are respectively aligned with the material strip.

[0050] In this embodiment, the driving mechanism of the movable slide 511 is a stroke-controllable driving mechanism or a two-stage fixed stroke driving mechanism. The stroke-controllable driving mechanism, such as a servo motor or a stepping motor, can control the specific stroke of the movable slide 511; the two-stage fixed stroke driving mechanism, such as a two-stage air cylinder or oil cylinder, can also make the injection molding punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism 515 align with the material strip 8 respectively.

[0051] Preferably, on the movable slide 511, the injection molded part punching mechanism is aligned with the material strip 8 at the initial position. In the punching and welding device 51, punching of injection molded parts is the most commonly used function, so the injection molded part punching mechanism is set at the initial position. The next position is the material strip punching mechanism, and the next position is the welding electrode pressing and adjusting mechanism 515. Because when punching and welding the material strip, the material strip punching mechanism punches first, and then the welding electrode pressing and adjusting mechanism 515 welds the material strip 8. This type of arrangement structure can reduce the travel of the movable slide 511. The structure in which the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing and adjusting mechanism 515 are arranged in a straight line can be seen in Figure 4 and 5 , the circular arrangement structure can be simply adjusted.

[0052] In this embodiment, both the injection molding part punching mechanism and the strip punching mechanism include a punching die. The punching dies of the two mechanisms are arranged on the same punching machine or on different punching machines. The two situations are respectively as follows: Figure 4 and 5 As shown. Figure 4 In the embodiment, the injection molding die 5131 and the strip die 5141 are arranged on the same die cutting machine 516. Figure 5 The middle injection molded part punching movable die 5131 and the strip punching movable die 5141 are respectively arranged on different punching machines 516. When the punching dies of the two mechanisms are arranged on the same punching machine 516, the two punching dies will act at the same time, but since there is only one strip 8, there will be no influence.

[0053] In this embodiment, the detection system includes a first detection device 41, which includes a front camera 411 to photograph the front of the material strip 8 after injection molding for detection; the first detection device also includes an oblique camera 412, which is aimed at the material strip 8 in the injection mold 3 of the injection molding machine 2 to photograph the material strip 8 before and after the injection mold 3 is molded; the first detection device 41 also includes a lighting lamp, and the lighting lamp and the camera are both arranged in a box body 413, the box body 413 is arranged on the fixed mold plate 33 of the injection molding machine 2, and a heat insulation board 415 is arranged between the box body 413 and the fixed mold plate 33, a fan and a heat dissipation hole are arranged on one side of the box body 413, the heat insulation board 415 is connected to the slide rail 414 and the locking mechanism, the box body 413 can move on the slide rail 414 to approach or move away from the movable mold 32, and the heat insulation board 415 is provided with a cooling device, and the cooling device can connect cooling water to the heat insulation board 415 to cool the heat insulation board 415.

[0054] The heat shield 415 can isolate the heat around the injection nozzle and the heat emitted by the injection mold 3 from the camera, and the heat dissipation holes and the fan of the box body 413 can prevent the camera from working in a high temperature environment, thereby ensuring the service life of the camera. The box body 413 can move on the slide rail 414 to get close to or away from the movable mold 32, and the fixed mold 31 can be easily replaced. The horizontal injection molding machine generally adopts hoisting when replacing the fixed mold 31, and the fixed mold 31 is lifted up and down for replacement. The box body 413 can move on the slide rail 414, and the fixed mold 31 can be easily replaced by moving the box body 413 backward, and it can be pushed forward to get close to the movable mold 32 after replacement, which is more convenient for photographing and testing. When the injection mold is up and down, the camera box can be easily removed, and the camera box can be reset before injection molding. Behind the material belt to be photographed, a background with a large contrast between the color and the object to be photographed is set.

[0055] The tilted camera 412 shoots obliquely from the side, aiming at the material strip 8 that has just been moved into place on the injection mold 3. At the same time, the camera is also obliquely facing the movable mold 32, so it can shoot the relative position relationship between the material strip 8 and the movable mold 32, and the status before and after mold closing and demolding, which is convenient for monitoring the injection molding process.

[0056] A second material belt driving device 72 is provided on the movable mold 32 to provide sufficient driving force for the material belt 8 after injection molding to ensure that the material belt 8 can move normally. A damping wheel 731 is also provided on the movable mold 32, which is arranged below the movable mold 32. The second material belt driving device 72 is arranged above the movable mold 32, and the material belt 8 enters the injection mold 3 from the bottom of the movable mold 32. Due to the effect of the damping wheel 731, the material belt 8 will not relax. The damping wheel 731 can use a friction damper or a magnet damper. The damping force of the damper can be adjusted. The damper is connected to a gear or a ratchet. The teeth of the gear or the ratchet are in contact with the positioning holes on the edge of the material belt 8. When the material belt 8 moves forward, it drives the wheel to overcome the damping force and rotate. Under the premise of ensuring that the material belt 8 is tensioned, the damping force is adjusted to be as small as possible.

[0057] In this embodiment, the detection device includes a second detection device, which includes a side camera 421, which photographs the side of the material strip 8 after injection molding for detection. The second detection device also includes a positioning mechanism, and the material strip 8 passes through the middle of the positioning mechanism. The positioning mechanism includes a pressure head 422 that can move up and down. The pressure head 422 can press the material strip 8 to vertically position the material strip 8. The pressure head 422 is provided with a contact sensor and / or an eccentric detection head. When the material strip 8 is vertically positioned, the size of the injection molded parts on the material strip 8 is detected. The second detection device also includes an adaptation detection tool 423. The adaptation detection tool 423 is provided with a tooling that cooperates with the injection molded parts on the material strip 8. The adaptation detection tool 423 is actuated to perform adaptation testing on the tooling and the injection molded parts.

[0058] Since the side of the injection molded part is small in size and the material strip 8 is guided only by the driven wheel when moving, and there is no positioning device, it is impossible to ensure that the side of the material strip 8 is in a fixed horizontal position. Therefore, when the side camera 421 takes pictures for inspection, a pressure head 422 is required to press the material strip 8. At the same time, the action of the pressure head 422 pressing the material strip 8 can also play a role in fixing the rear section of the material strip 82 when the material strip 8 is cut. Contact sensors, eccentric detection heads and adapter detection tools 423 are conventional technologies for inspecting injection molded parts.

[0059] In this embodiment, the welding electrode pressing adjustment mechanism 515 includes a base 5151 and a pressing head. A lifting block 5152 is provided on the base 5151. The lifting block 5152 is provided on the side of the material strip cutout close to the front section material strip 81. The lifting block 5152 is lifted to make the front section material strip 81 retreat to the top of the rear section material strip 82. An elastic pressing die 5153 is provided on the pressing head. After the pressing head is pressed down, the elastic pressing die 5153 presses the front section material strip 81 and the rear section material strip 82 together, and then the welding electrode 5154 contacts the material strip 8. Figure 6 As shown in Figures ad, the lifting block 5152 falls back to a position flush with the base 5151 due to the downward pressure of the crimping head.

[0060] The reason for adopting this structure is that when the material strip punching mechanism punches the material strip, the cut is not a straight line, but a shape that is convenient for the front section material strip 81 and the rear section material strip 82 to be clamped together. Figure 7 2 shows two embodiments of the cutouts and their shapes after splicing. Therefore, the front strip 81 needs to be retracted above the rear strip 82, and the elastic pressing mold 5153 presses the front strip 81 and the rear strip 82 together to make the cutouts overlap. The front strip 81 and the rear strip 82 are clamped together to enhance the strength of the strips after welding.

[0061] The lifting block 5152 can be lifted by a driving device such as a cylinder and a transmission mechanism to achieve the action of falling back due to the downward pressure of the crimping head, or a passive driving mechanism such as Figure 4 and Figure 6As shown, one end of the lifting block 5152 close to the front section material strip 81 is hinged to the base 5151, and a swing rod 5155 is provided at the lower part of the other end. The middle part of the swing rod 5155 is hinged to the base 5151, one end is arranged below the lifting block 5152, and the other end is arranged at the material strip punching fixed die 5142. When the material strip punching movable die 5141 is pressed down, the swing rod 5155 is pressed down at this end, and the swing rod 5155 swings to lift the movable end of the lifting block 5152, so that the movable end of the lifting block 5152 swings upward with the hinged end as the rotation center, and the lifting action of the lifting block 5152 is realized. In addition, at this time, the hinged end of the lifting block 5152 is at a lower position, which is convenient for the front section material strip 81 to rise to a certain height when it retreats. The swing rod 5155 can be provided with a gear fixing mechanism, such as a spring ball mechanism, or the rotation damping of the swing rod 5155 can be adjusted, so that it maintains the current posture after swinging until the pressing head is pressed down, pressing the lifting block 5152 and the swing rod 5155 together.

[0062] The first material belt driving device 71 and the second material belt driving device 72 drive the material belt 8 to move by cooperating with the holes on the edge of the material belt 8. The specific driving mechanism can adopt a fixed-stroke driving mechanism such as a cylinder, or a controllable-stroke driving mechanism such as a servo motor, and the actuator can be a gear or a ratchet.

[0063] The detection system also includes a welding and punching detection device 43, which is arranged after the welding and punching detection device 51. The welding and punching detection device 43 detects the incision of the injection molded part or the welding point of the material strip 8 through a probe or a contact sensor. It can be used to detect the punching mold on the welding and punching device 51. When an abnormality is found in the incision or the welding point of the material strip, the punching mold can be replaced in time.

[0064] A strip punching and welding process comprises the following steps:

[0065] In the first step, a section of a strip 8 is cut off and removed by using a strip punching mechanism, and the cut shapes of the front strip 81 and the rear strip 82 after cutting are mutually engageable, and a plurality of overlapping points 83 are distributed on the cuts;

[0066] In the second step, the front end material strip 81 after cutting is returned to the top of the rear end material strip 82 by using the material strip driving mechanism and the cutouts are aligned, so that the front end material strip 81 and the rear end material strip 82 overlap at the overlap point 83;

[0067] In the third step, the welding mechanism presses the front section material strip 81 and the rear section material strip 82 together and spot welds them at the overlap point 83 to weld the front section material strip 81 and the rear section material strip 82 together.

[0068] Figure 7 Two examples of strip cutouts are shown. Figure 8A partial schematic diagram of the incision is shown, and the overlap points 83 scattered on the incision can be seen. The front section material strip 81 and the rear section material strip 82 are welded and connected at the scattered overlap points 83. The deformation of the material strip 8 during welding is small, which facilitates the control of the thickness of the material strip 8 at the welding point, so that the welded material strip 8 can be moved on the production line and rolled in the material receiving device, and can also be directly used on the production line of downstream manufacturers.

[0069] For the overlap point 83, when the material strip 8 is cut, the cross section of the overlap point 83 can be bent or flattened at the same time. A relatively simple implementation scheme is as follows: Figure 6 As shown in (b), the lower right corner of the overlap point 83 of the cut of the front strip 81 is flattened into a chamfered shape, for example: the chamfer height is 0.5 strip thickness, and the angle is about 45 degrees; and the upper left corner of the overlap point 83 of the cut of the rear strip 82 is also flattened into a chamfered shape, for example: the chamfer height is 0.5 strip thickness, and the angle is about 45 degrees. The overlap length of the overlap point 83 of the front strip 81 and the rear strip 82 is 0.5 strip thickness. Before welding, 0.5 strip thickness is used for pressing and overlapping positioning. When welding, only the remaining 0.5 strip thickness needs to be melted and welded. The height of the chamfer varies depending on the thickness of the strip 8, and is based on the strip 8 running without breaking after welding. Since the chamfering position is inside the die blade, the chamfer can be directly designed on the die blade, and the punching and chamfering can be completed in one step. The process of punching and chamfering the material strip can be found in the utility model patent with patent number 201620272363.5 and patent name "Electronic component assembly machine for lead frame".

[0070] like Figure 8 As shown, the overlap point 83 is arranged in a dot matrix, which is conducive to the deformation caused by the distributed heating during welding. The more uniform the dot matrix is ​​arranged, the more uniform the distributed heating is, and the smaller the welding deformation is; so that the hot processing process of welding can reach the accuracy of cold processing. In the welding process, the inverter is used to control its heating and cooling temperature curve to obtain the required metal crystal phase structure. For example, for the material strip of ferroalloy, the cooling curve is set with reference to its crystal phase structure state diagram, which can overcome the brittleness of its overlap point and make the material strip not easy to break. When the process parameters monitored by the inverter exceed the set tolerance range, the alarm can be stopped in time, and the automatic working state can be restored after the operator handles it. To ensure the welding quality.

[0071] It should be emphasized that the above are only preferred embodiments of the present invention and do not limit the present invention in any form. Any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A roll-to-roll injection molding inspection punching and welding production line, characterized in that: include: The unwinding device unwinds the rolled material strip and delivers it to the production line; Injection molding machine, which performs injection molding on the material strip; Injection molds; Inspection system, inspecting the material strip before and after injection molding; The welding system includes a punching and welding device and a simple welding device. The simple welding device is arranged after the material discharge device, and welds the material strips of different rolls into a continuous material strip. The punching and welding device and the simple welding device share a set of welding machine inverter power supply; the punching and welding device is arranged between the detection system and the material receiving device, and punches and welds the material strips that fail the detection; the material receiving device rewinds the material strips that pass through the injection molding machine, the detection system and the welding system and counts the injection molded parts on the material strip; the material strip driving system drives the material strip to move between the material discharge device and the material receiving device; wherein the punching and welding device includes a moving slide, and the moving slide is provided with an injection molded part punching mechanism, a material strip punching mechanism and a welding electrode pressing adjustment mechanism. The moving slide can move so that one of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism is aligned with the material strip, and the injection molded part punching mechanism can cut off the injection molded parts on the material strip. The material strip punching mechanism can cut the material strip, and the material strip driving system includes a first material strip driving device arranged between the punching and welding device and the material receiving device. The first material strip driving device can act in both directions to drive the material strip to move from the punching and welding device to the material receiving device or in the reverse direction. The first material strip driving device moves in the reverse direction to make the cut front section of the material strip retreat and splice with the cut rear section of the material strip at the punching and welding device, and the welding electrode pressing and adjusting mechanism presses and welds the spliced ​​material strips; wherein, the detection system also detects the material strip after welding; wherein, the welding electrode pressing and adjusting mechanism includes a base and a pressing joint, and the base is provided with a lifting block, and the lifting block is arranged on the side of the material strip cut close to the front section of the material strip, and the lifting block is lifted to make the front section of the material strip retreat to above the rear section of the material strip, and the pressing joint is provided with an elastic pressing die, and the pressing joint is pressed downward so that the elastic pressing die presses the front section of the material strip and the rear section of the material strip together, and then the welding electrode contacts the material strip.

2. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1 is characterized in that: The movable slide is arranged below the material strip, and the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are fixed on the movable slide through a support frame, and the material strip passes through the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism. The fixed parts of the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are all arranged on the slide and located below the material strip, and the movable parts are all arranged on the support frame and located above the material strip.

3. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1 is characterized in that: The injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are arranged in a straight line in sequence on the movable slide, and the driving mechanism of the movable slide drives the movable slide to move linearly so that the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are aligned with the material strip respectively.

4. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1 is characterized in that: The injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are arranged circumferentially on the movable slide, and the driving mechanism of the movable slide drives the movable slide to rotate so that the injection molded part punching mechanism, the material strip punching mechanism and the welding electrode pressing adjustment mechanism are aligned with the material strip respectively.

5. The roll-to-roll injection molding inspection, punching and welding production line according to claim 3 or 4, characterized in that: The driving mechanism of the movable slide is a stroke-controllable driving mechanism or a two-stage fixed stroke driving mechanism.

6. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1, characterized in that: The injection molded part punching mechanism and the material strip punching mechanism both include punching dies, and the punching dies of the two mechanisms are arranged on the same punching machine or respectively arranged on different punching machines.

7. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1 is characterized in that: The detection system includes a first detection device, which includes a front camera to photograph the front of the material strip after injection molding for detection; the first detection device also includes an oblique camera, which is aimed at the material strip in the injection mold of the injection molding machine to photograph the material strip before the injection mold is closed and after demolding; the first detection device also includes a lighting lamp, and the lighting lamp and the camera are both arranged in a box body, the box body is arranged on the fixed mold plate of the injection molding machine, a heat insulation board is arranged between the box body and the fixed mold, a fan and a heat dissipation hole are arranged on one side of the box body, the heat insulation board is connected to the slide rail and the locking mechanism, the box body can move on the slide rail to approach or move away from the movable mold, and the heat insulation board is provided with a cooling device, and the cooling device can connect cooling water to the heat insulation board to cool the heat insulation board.

8. The roll-to-roll injection molding inspection, punching and welding production line according to claim 1, characterized in that: The detection system includes a second detection device, which includes a side camera to photograph the side of the material strip after injection molding for detection. The second detection device also includes a positioning mechanism, and the material strip passes through the middle of the positioning mechanism. The positioning mechanism includes a pressure head that can move up and down, and the pressure head can press the material strip to vertically position the material strip. The pressure head is provided with a contact sensor and / or an eccentric detection head to detect the size of the injection molded parts on the material strip when the material strip is vertically positioned. The second detection device also includes an adaptation detection tool, and the adaptation detection tool is provided with a tooling that cooperates with the injection molded parts on the material strip. The adaptation detection tool is actuated to perform adaptation testing on the tooling and the injection molded parts. The detection system also includes a welding and punching detection device, which is arranged after the punching and welding device, and detects the incision of the injection molded parts on the material strip or the welding part of the material strip through a probe or a contact sensor.

9. A strip punching and welding process, applied to the roll-to-roll injection molding inspection punching and welding production line as claimed in any one of claims 1 to 8, characterized in that: The method comprises the following steps: first, using a strip punching mechanism to cut off and remove a section of a strip, wherein the cutout shapes of the front strip and the rear strip after cutting are mutually engageable, and a plurality of overlapping points are distributed on the cutouts; second, using a strip driving mechanism to return the cutout front strip to the top of the rear strip and align the cutouts, wherein the front strip and the rear strip overlap at the overlapping points; In the third step, the welding mechanism presses the front section material strip and the rear section material strip together and spot welds them at the overlapping points to weld the front section material strip and the rear section material strip together.