Method and apparatus for controlling warpage in wafer level packaging processes
By adopting multi-stage temperature treatment and polymer layer process for warpage correction in the semiconductor chip packaging process, the warpage problem is solved, the yield and chip flatness of the fine pitch RDL layer are improved, and efficient chip-level packaging is achieved.
Patent Information
- Application Number
- CN201911022264.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-26
- Filing Date
- 2019-10-25
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2039-10-25
AI Technical Summary
In semiconductor chip-level packaging processes, warping problems lead to a decrease in the formation capacity of the fine pitch RDL layer, thereby reducing the yield rate. The prior art solutions are expensive and time-consuming, and it is difficult to achieve high yield rate without carrier technology.
By fine pitch patterning on the substrate, multi-stage temperature treatment and through-hole formation and curing of the polymer layer, combined with chemical mechanical polishing and other processes, warpage correction is performed to control the warping of the substrate and form high fineness redistribution layer.
It is achieved to improve the yield rate of semiconductor chips without the need to add expensive carriers or complex tools, especially on fine pitch patterning at 5/5μm or 2/2μm levels, to achieve a yield rate of 90% or higher, and The warpage value of the substrate is reduced and the internal structural flatness of the chip is improved.
Smart Images

Figure CN111106019B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of U.S. Provisional Patent Application Serial No. 62 / 751,200, filed on October 26, 2018, which is incorporated herein by reference in its entirety. Technical Field
[0003] Embodiments of the present principles relate generally to semiconductor processes for packaging semiconductor devices. Background Art
[0004] Semiconductor wafers are processed to form structures on the surface of the wafer. Structures on specific areas of the wafer can be linked together to form microcircuits. The wafer can have many different microcircuits built on the surface of the wafer during processing. Once the wafer processing has been completed, the wafer is cut or diced to separate the microcircuits into semiconductor "chips". Chips typically contain complex circuits that need to interact with external components. The internal circuitry of the chip is too small to be directly connected to external components. In order to overcome the external connection problem, lead wires are formed that connect the internal circuitry of the chip to pads or solder balls, allowing external connections. During the subsequent packaging process of the semiconductor chip, the lead wires are formed in the so-called "redistribution layer".
[0005] Chips from different wafers can be combined together by placing the chips on a surface and pouring molding compound over the chips to form a new wafer or 'reconstructed wafer' again. The molding compound hardens so that the chips can be handled consistently for redistribution layer processing. A common technique is to bond the reconstructed wafer to a temporary carrier to provide rigidity during processing. However, temporary bonding and then peeling is expensive and time consuming, so carrier-free techniques can also be used. During the wafer-level packaging process, the wafer may become warped. Warping hinders the ability to form fine pitch RDL layers on the wafer, greatly reducing the yield.
[0006] Therefore, the inventors provide improved methods for controlling warpage during wafer level packaging processes. Summary of the invention
[0007] Methods are provided for controlling warpage in a wafer level packaging process to improve yield, especially for fine pitch RDL layers.
[0008] In some embodiments, a method for performing fine pitch patterning on a substrate in a wafer-level packaging process includes: performing a first warpage correction process on the substrate by ramping the substrate to a first temperature and maintaining the first temperature for a first duration and ramping the substrate to a second temperature and maintaining the second temperature for a second duration, wherein the first temperature is greater than the second temperature; forming a through hole in a polymer layer on the substrate; curing the polymer layer; performing a second warpage correction process on the substrate by ramping the substrate to a third temperature and maintaining the third temperature for a third duration and ramping the substrate to a fourth temperature and maintaining the fourth temperature for a fourth duration, wherein the third temperature is greater than the fourth temperature; and forming a redistribution layer on the substrate with fine pitch patterning having a line / space of 10 / 10 μm or less.
[0009] In some embodiments, the method may further include: wherein the fine pitch patterning has a line / space of 5 / 5 μm or less; wherein the fine pitch patterning has a line / space of 2 / 2 μm or less; wherein after the second warpage correction process, the substrate has a warpage of 500 μm or less; wherein after the second warpage correction process, the substrate has a warpage of 400 μm or less; wherein the first temperature of the first warpage correction process is greater than the third temperature of the second warpage correction process; wherein the first temperature of the first warpage correction process is approximately equal to the third temperature of the second warpage correction process; wherein a subsequent first temperature of a subsequent first warp correction process is based on the first temperature of the first warp correction process; wherein the first temperature is approximately the glass transition temperature of the polymer layer on the substrate; wherein the first temperature, the second temperature, the third temperature or the fourth temperature is obtained by linearly ramping up; wherein the first temperature is lower than the glass transition temperature of the polymer layer when a physical vapor deposition (PVD) process has been performed before the first warp correction process; wherein the substrate is a reconstructed wafer consisting of a plurality of dies; and / or a chemical mechanical polishing (CMP) process is performed to enhance the fine pitch patterning.
[0010] In some embodiments, a method for performing fine pitch patterning on a substrate in a wafer-level packaging process includes: determining a material composition, thickness, or previous processing of the substrate; heating the substrate to a first temperature within a first time period based on the material composition, thickness, or previous processing of the substrate; maintaining the substrate at the first temperature for a second time period; and cooling the substrate to a second temperature within a second time period based on the material composition, thickness, or previous processing of the substrate.
[0011] In some embodiments, the method may further include wherein the first temperature is approximately 150 degrees Celsius to 220 degrees Celsius, wherein the first temperature is reduced when previous processing of the substrate includes a physical vapor deposition (PVD) process, wherein the first temperature is greater than a glass transition temperature of a material of the substrate, and / or wherein the first temperature is approximately 175 degrees Celsius.
[0012] In some embodiments, a non-transitory computer-readable medium having instructions stored thereon, which when executed cause a method for performing fine pitch patterning on a substrate in a wafer-level packaging process to be performed, the method comprising: performing a first warpage correction process on the substrate by ramping the substrate to a first temperature and maintaining the first temperature for a first duration and ramping the substrate to a second temperature and maintaining the second temperature for a second duration, wherein the first temperature is greater than the second temperature; forming a through hole in a polymer layer on the substrate; curing the polymer layer; performing a second warpage correction process on the substrate by ramping the substrate to a third temperature and maintaining the third temperature for a third duration and ramping the substrate to a fourth temperature and maintaining the fourth temperature for a fourth duration, wherein the third temperature is greater than the fourth temperature; and forming a redistribution layer on the substrate with fine pitch patterning having a line / space of 10 / 10 μm or less.
[0013] In some embodiments, the method may further include wherein the first temperature of the first warp correction process is greater than the third temperature of the second warp correction process, wherein after the second warp correction process, the substrate has a warp of 400 μm or less, and wherein the fine pitch patterning has a line / space of 2 / 2 μm or less.
[0014] Other and further embodiments are disclosed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Embodiments of the present principles, briefly summarized above and discussed in more detail below, can be understood with reference to the exemplary embodiments of the present principles depicted in the accompanying drawings. However, the accompanying drawings illustrate only typical embodiments of the present principles and are therefore not to be considered limiting of scope, as the present principles may allow other equally effective embodiments.
[0016] Figure 1 A method of incorporating warpage control during a wafer level packaging process according to some embodiments of the present principles.
[0017] Figure 2 A method of adjusting warpage correction during a wafer level packaging process according to some embodiments of the present principles.
[0018] Figure 3 A method of performing warpage reduction according to some embodiments of the present principles.
[0019] Figure 4 is a cross-sectional view of a substrate processing system for controlling substrate warpage, according to some embodiments of the present principles.
[0020] For ease of understanding, the same reference numerals have been used as much as possible to designate the same elements common to the various figures. The drawings are not drawn to scale and may be simplified for clarity. The elements and / or features of one embodiment may be advantageously incorporated into other embodiments without further description. DETAILED DESCRIPTION
[0021] The disclosed method and apparatus allow warpage correction during fan-in and fan-out wafer-level packaging processes. Warpage correction can be performed before the first, second and / or nth redistribution layer (RDL) is formed. Warpage correction can also be inserted at any step during RDL manufacturing. The method can be completed in a carrier-free wafer-level packaging process or with a carrier-based wafer-level packaging process. Even though the carrier-based wafer-level packaging process provides a certain degree of rigidity, warpage may become a consideration as more and more layers are stacked. By controlling substrate warpage during the wafer-level packaging process, fine-pitch RDL patterning can be obtained at an intra-wafer yield to achieve high input / output (I / O) chip-to-chip interconnect wiring. The technology of the present principle neither introduces additional materials into the wafer-level packaging process nor introduces expensive carrier processes that require additional bonding / stripping, back grinding and copper pillar steps. The lack of complex process tools and added materials enables outsourced semiconductor assembly and test (OSAT) entities to perform these methods.
[0022] Warp correction can be advantageously done at any part of the fan-out flow or fan-in flow. The flexibility of inserting warp correction at any point in the process flow allows OSAT entities to take advantage of warp correction, whether the entity has a tool set to perform the full process or only a portion of the process. The technology of the present principle advantageously allows fine pitch patterning of less than 10 / 10μm l / s. In some embodiments, high yields can be obtained for RDL layers of 5 / 5μm l / s and even 2 / 2l / s. In some embodiments, for 5 / 5μm l / s, a yield of about 90% or more can be achieved. In some embodiments, for 2 / 2μm l / s, not only for patterning but also as an electrical function RDL, a yield of about 50% or more can be achieved. In some embodiments, warp correction provides a warp value of less than about 500μm. In some embodiments, warp correction provides a warp value of less than about 400μm. Most OSAT entities cannot achieve a cost-effective yield for 2 / 2μm l / s in a process flow without a carrier. Carrier-based processes require expensive tools that OSAT entities do not have. The technology of the present principles provides OSAT entities with the opportunity to create this cost effective method to produce 2 / 2 μm1 / s.
[0023] Figure 1100 is a method for incorporating warpage control during a wafer-level packaging process according to some embodiments. Warpage tends to occur whenever there is a sudden change in temperature during processing. The molding process and the polymer curing step are examples that may cause sudden changes in temperature and substrate warpage. In frame 102, a substrate is obtained for processing. In some embodiments, the substrate may include a reconstructed wafer consisting of multiple dies that have been overmolded into a single wafer. Curing during the overmolding process generates heat, which can cause warpage of the reconstructed wafer. Warpage makes it difficult to perform fine patterning on the wafer. In frame 104, a first warpage correction process as described below is performed on the substrate. In the case of a reconstructed wafer, the first warpage correction process produces a flatter surface that is better for fine pitch patterning. In frame 106, a through hole is constructed in a polymer layer on the substrate. In some embodiments, a through hole can be formed using a lithography process. The through hole is typically filled with copper material to allow connection between the layers of the substrate. In frame 108, the polymer layer with the through hole is cured. The polymer curing process can reach a temperature of 220 degrees Celsius, resulting in large warpage values after the via formation. In box 110, a second warpage correction process is performed on the substrate. The second warpage correction process smoothes the surface of the substrate so that subsequent processes can achieve fine pitch patterning. The second warpage correction process is particularly important after the high curing temperature of the polymer material used in the via formation process. In box 112, an RDL layer is built on the substrate. As described herein, in some embodiments, the warpage correction process can be repeated in a wafer-level packaging process so that a high-yield fine pitch RDL can be achieved.
[0024] In some embodiments, warp correction can be used in conjunction with a chemical mechanical polishing (CMP) process. The CMP process is used to reduce the step height after die overmolding. By performing a CMP process and warp correction, the yield of fine pitch patterning can be dramatically improved compared to either CMP processing or warp correction processing alone.
[0025] In some processes, a physical vapor deposition process (PVD) can be used. For example, after forming a through hole in the polymer layer, a metal layer can be deposited on the polymer layer using a PVD process to form an RDL layer. The inventors have found that special care should be taken when correcting the warpage after the PVD process. Heating during the warpage correction process may cause degassing of the polymer layer below the metal layer (PVD process). Degassing may cause blistering below the surface of the metal layer, which degrades the surface used for fine pitch patterning. In some embodiments, warpage correction may be performed until the PVD process, but it is no longer performed after the PVD process. In some embodiments, distributions for various processes and / or various materials used in the process can be formed to control the warpage correction temperature, ramp-up, and duration. These distributions allow optimization of the wafer-level packaging process to improve the fine pitch yield and produce repeatable results.
[0026] The inventors have discovered that even when warp correction is not the primary goal, the warp correction process has other benefits that can be exploited. In some embodiments, warp correction can be used even on low warp substrates to make the wafer softer and more relaxed.
[0027] Figure 2 The present invention is a method 200 for adjusting warpage correction during a wafer-level packaging process according to some embodiments. In block 202, a material composition of a substrate is determined or obtained from a previous process. In some embodiments, the glass transition temperature of each type of material can be used to adjust warpage correction parameters, such as temperature, duration, and temperature ramp time. In block 204, a thickness of a substrate is determined or obtained from a previous process. In some embodiments, the thickness of each type of material can be used to adjust warpage correction parameters, such as temperature, duration, and temperature ramp time. In block 206, a previous substrate process is determined or known from a current process. In some embodiments, a previous substrate process can be used to determine a thermal budget allocation or to determine whether a lower warpage correction temperature should be used (e.g., when the previous process includes a PVD process). In block 208, a warpage correction process is adjusted based on the material composition, thickness, and previous process of the substrate.
[0028] Figure 3The method 300 for performing warpage reduction according to some embodiments is provided. In block 302, a substrate is heated to a first temperature between about 150 degrees Celsius and about 220 degrees Celsius. In some embodiments, the first temperature may be based on the glass transition temperature of the substrate material. The glass transition temperature is the temperature at which a polymer changes from a glass-like material to a rubber-like material. The glass transition temperature of a material may be above about 160 degrees Celsius and about 170 degrees Celsius. For each substrate material, the glass transition temperature will vary. In some embodiments, the substrate is heated to a temperature close to or slightly above the glass transition temperature of the material. In some embodiments, the glass transition temperature is based on the material used as the substrate and the material used in the process. The first temperature value is adjusted accordingly. In some embodiments, the first temperature ramp may be linear, and the ramp-up time to obtain the first temperature may vary based on the material being heated and the material parameters (e.g., thickness, etc.). In block 304, the substrate is maintained at the first temperature for a first time period. The duration of the first temperature may be adjusted based on the type of material or substrate and other physical parameters (such as the thickness of the wafer). In block 306, the substrate is cooled to a second temperature less than the first temperature. The second temperature may be based on the type of material or substrate and other physical parameters (such as the thickness of the wafer). In some embodiments, the second temperature ramp may be linear, and the ramp time to obtain the second temperature may vary based on the material being heated and the material parameters (e.g., thickness, etc.). In some embodiments, the substrate may be cooled through a plurality of heat transfer channels in the substrate support to remove substrate warpage (see below). Figure 4 ).
[0029] In some embodiments, the first temperature for warp correction may be below the glass transition temperature to reduce potential outgassing of the polymer layer after the PVD process. In some embodiments, the first temperature of the first warp correction process may be higher than the first temperature of a subsequent warp correction process. In some embodiments, the first temperature of the warp correction process may be at least one first temperature based on a previous first temperature of the warp correction process. In some embodiments, the parameters of the first temperature ramp, the first temperature, the parameters of the second temperature ramp, and / or the second temperature may be adjusted based on the occurrence of a previous PVD process to reduce outgassing of the underlying polymer material. The inventors have discovered that a carefully controlled temperature transition at or near the glass transition temperature can reduce or eliminate outgassing of the underlying polymer layer while providing adequate warp correction, thereby improving yield after the PVD process.
[0030] Figure 4 A cross-sectional view of a substrate processing system 400 suitable for performing the method of the present principles according to some embodiments is depicted. Figure 4As shown, the substrate processing system 400 includes a chamber 402 enclosing a processing volume 403, a support 404 for supporting a substrate 406, a lift pin assembly 407, a vacuum source 410, a heat transfer supply 413, a radiant heat source (lamp array 412), a lamp driver 414, a controller 416, and a lamp driver AC power supply 418. A gas delivery system 430 for the chamber 402 may also be used in conjunction with or in place of the lamp array 412. The gas delivery system 430 may include a heating element 440, a heating element AC power supply 432, a gas temperature controller 434, and a gas flow control valve 438 for regulating the gas supply 436. One or more temperature sensors and associated hardware (not shown) may be provided and coupled to the controller to control the temperature within the processing volume 403. The substrate 406 is, for example, a semiconductor wafer. The substrate 406 may include an epoxy coating disposed on the substrate 406.
[0031] The lift bar assembly 407 includes a plurality of lift bars 409 extending through a corresponding plurality of lift bar channels 405 formed in the support 404. The lift bar assembly 407 can be raised and lowered by a drive mechanism 408, such as a motor or actuator, to raise or lower the substrate 406 off of a support surface 417 of the support 404. The chamber 402 can also include an opening 419 through which a robot (not shown) extends to insert / remove the substrate 406 onto / from the plurality of lift bars 409. The lift bar assembly 407 is movable between a first position, in which the substrate is proximate to the lamp array 412, and a second position, in which the substrate 406 rests on the support surface 417. In some embodiments, the substrate 406 is heated to a first predetermined temperature in the first position and cooled to a second predetermined temperature in the second position.
[0032] In some embodiments, the support 404 is a vacuum chuck to which a vacuum source 410 is coupled to chuck the substrate 406 to the support surface 417. In some embodiments, the support 404 may alternatively be an electrostatic chuck. The support 404 includes a plurality of heat transfer channels 411 fluidly coupled to a heat transfer supply 413. In some embodiments, for example, the heat transfer supply 413 may provide a coolant to the heat transfer channels 411 to cool the substrate 406 placed atop the support surface 417 of the support 404.
[0033] The lamp driver AC power supply 418 delivers AC power to the lamp driver 414, the operation of which is controlled by the controller 416. The lamp driver 414 distributes the power to the lamp array 412. In turn, the lamp array 412 generates heat to heat-treat the substrate 406 in the chamber 402. In some embodiments, the lamp array 412 includes one or more lamps, each of which can be individually controlled by the controller 416 through the lamp driver 414. Figure 4 As shown, three lamps (420, 422, 424) are shown, but a fewer or greater number of lamps may be used. Each lamp 420, 422, 424 may be individually controlled by the controller 416 to provide heat to the corresponding heating zone. Since the lamps may be individually controlled, the temperature in the heating zone may also be controlled.
[0034] In some embodiments, the gas delivery system 430 may provide an inert gas (such as, but not limited to, nitrogen or argon) from a gas supply 436 to reduce oxidation of the substrate 406, particularly to reduce oxidation of a metal wafer when heat is applied. A gas flow control valve 438 regulates the amount of gas supplied by the gas supply 436 to the processing volume 403. In some embodiments, the gas delivery system 430 may also include a heating element 440 to heat the gas as it enters the processing volume 403. The temperature of the heating element 440 is controlled by a gas temperature controller 434. The power for the heating element 440 is provided by a heating element AC power supply 432. During the warpage correction process, the gas provided by the gas delivery system 430 improves the temperature uniformity of the substrate 406.
[0035] Embodiments according to the present principles may be implemented in hardware, firmware, software, or any combination of the above. Embodiments may also be implemented as instructions stored using one or more computer-readable media, which may be read and executed by one or more processors. Computer-readable media may include any mechanism for storing or transmitting information in a form that can be read by a machine (e.g., a computing platform or a "virtual machine" running on one or more computing platforms). For example, a computer-readable medium may include any suitable form of volatile or non-volatile memory. In some embodiments, a computer-readable medium may include a non-temporary computer-readable medium.
[0036] The chamber 402 may also include a system controller 450. The system controller 450 includes a programmable central processing unit (CPU) 452 that can operate with a memory 454 and mass storage devices, input control units, and display units (not shown) coupled to various components of the processing system (such as power supplies, clocks, caches, input / output (I / O) circuits, and liners) to facilitate control of substrate processing. To facilitate control of the chamber 402 described above, the CPU 452 may be one of any form of general purpose computer processor that can be used in an industrial environment (such as a programmable logic controller (PLC)) for controlling various chambers and sub-processors. The memory 454 is coupled to the CPU 452, and the memory 454 is non-temporary and may be one or more of a random access memory (RAM), a read-only memory (ROM), a floppy disk drive, a hard disk, or any other form of digital storage device (whether local or remote). Support circuits 456 are coupled to the CPU 452 to support the processor. Application programs or programs for charged species generation, heating, and other processes are generally stored in the memory 454, typically as software routines. The software routines may also be stored and / or executed by a second CPU (not shown) located remotely from the processing chamber 402 controlled by the CPU 452 .
[0037] The memory 454 is in the form of a computer-readable storage medium containing instructions that facilitate the operation of the chamber 402 when executed by the CPU 452. The instructions in the memory 454 are in the form of a program product, such as a program that implements the method of the present disclosure. The program code can comply with any of a variety of different programming languages. In one example, the present disclosure can be implemented as a program product stored on a computer-readable storage medium for use with a computer system. One or more programs of the program product define the functions of various aspects (including the methods described herein). Exemplary computer-readable storage media include, but are not limited to: non-writable storage media (e.g., read-only memory devices within a computer, such as CD-ROM disks, flash memory, ROM chips, or any type of solid-state non-volatile semiconductor memory that can be read by a CD-ROM drive), on which information is persistently stored; and writable storage media (e.g., floppy disks or any type of solid-state random access semiconductor memory within a disk drive or hard drive), on which modifiable information is stored. When implementing computer-readable instructions indicating the functions of the methods described herein, such computer-readable storage media are aspects of the present disclosure.
[0038] While the foregoing is directed to embodiments of the present principles, other and further embodiments of the present principles may be devised without departing from the basic scope thereof.
Claims
1. A method for performing fine pitch patterning on a substrate in a wafer level packaging process, comprising: performing a first warpage correction process on the substrate by ramping the substrate to a first temperature and holding the first temperature for a first duration and ramping the substrate to a second temperature and holding the second temperature for a second duration, wherein the first temperature is greater than the second temperature; forming a through hole in a polymer layer on the substrate; curing the polymer layer; performing a second warpage correction process on the substrate by ramping the substrate to a third temperature and holding the third temperature for a third duration and ramping the substrate to a fourth temperature and holding the fourth temperature for a fourth duration, wherein the third temperature is greater than the fourth temperature; and A redistribution layer is formed on the substrate using fine pitch patterning with line / space of 10 / 10 μm or less. 2 . The method of claim 1 , wherein the fine pitch patterning has a line / space of 5 / 5 μm or less. 3 . The method of claim 1 , wherein the fine pitch patterning has a line / space of 2 / 2 μm or less. 4 . The method of claim 1 , wherein after the second warp correction process, the substrate has a warp of 500 μm or less. 5 . The method of claim 4 , wherein after the second warp correction process, the substrate has a warp of 400 μm or less. 6 . The method of claim 1 , wherein the first temperature of the first warpage correction process is greater than the third temperature of the second warpage correction process. 7 . The method of claim 1 , wherein the first temperature of the first warpage correction process is approximately equal to the third temperature of the second warpage correction process. 8 . The method of claim 1 , wherein a subsequent first temperature of a subsequent first warpage correction process is based on the first temperature of the first warpage correction process.
9. The method of claim 1, wherein the first temperature is approximately a glass transition temperature of the polymer layer on the substrate.
10. The method of claim 1, wherein the first temperature, the second temperature, the third temperature, or the fourth temperature is obtained by linearly ramping up. 11 . The method of claim 1 , wherein when a physical vapor deposition (PVD) process has been performed before the first warpage correction process, the first temperature is lower than a glass transition temperature of the polymer layer.
12. The method of claim 1, wherein the substrate is a reconstituted wafer comprised of a plurality of dies.
13. The method of claim 1, further comprising: A chemical mechanical polishing (CMP) process is performed to enhance the fine pitch patterning.
14. A non-transitory computer readable medium having instructions stored thereon, the instructions when executed causing a method of performing fine pitch patterning on a substrate in a wafer level packaging process, the method comprising: performing a first warpage correction process on the substrate by ramping the substrate to a first temperature and holding the first temperature for a first duration and ramping the substrate to a second temperature and holding the second temperature for a second duration, wherein the first temperature is greater than the second temperature; forming a through hole in a polymer layer on the substrate; curing the polymer layer; performing a second warpage correction process on the substrate by ramping the substrate to a third temperature and holding the third temperature for a third duration and ramping the substrate to a fourth temperature and holding the fourth temperature for a fourth duration, wherein the third temperature is greater than the fourth temperature; and A redistribution layer is formed on the substrate using fine pitch patterning with line / space of 10 / 10 μm or less.
15. The non-transitory computer-readable medium of claim 14, wherein the first temperature of the first warpage correction process is greater than the third temperature of the second warpage correction process, wherein after the second warpage correction process, the substrate has a warpage of 400 μm or less, and wherein the fine pitch patterning has a line / space of 2 / 2 μm or less.