Raw material formula of nano ivory jade
The technology of ivory and jade is applied in the field of raw material formulation of nano ivory and jade to achieve the effect of high compressive strength, high hardness and high flexural strength
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2020-06-26
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 1 
Figure 2
Abstract
Description
technical field
[0001] The invention relates to the field of nano ivory jade, in particular to a raw material formula of nano ivory jade. Background technique
[0002] Glass-ceramics is a new type of material developed in recent years. It has the characteristics of glass and ceramics. Glass-ceramics prepared with different formulas and processes can be used in electronic and electrical engineering, biomedicine, and chemical anticorrosion according to their characteristics. , mines, architectural decoration and other fields, but currently the nano-microcrystalline plates used in the architectural decoration industry generally have one or more aspects such as weather resistance, wear resistance, toughness, water absorption, corrosion resistance, compressive strength and hardness. Therefore, we propose a raw material formula of nano ivory jade. Contents of the invention
[0003] Based on the technical problems existing in the background technology, the present invention prop...
Examples
Embodiment 1
[0010] A kind of raw material formula of nano ivory jade is proposed in this embodiment, including the following mass percentages: Al2O3 is 3.7%, SiO2 is 63.85%, CaO is 8.83%, BaO is 3.6%, Na2O is 8.94%, K2O is 0.9% , CaF2 is 7.87%, Li2O is 0.22%, Sb2O3 is 0.4%, P2O5 is 1.34%, and MgO is 0.28%.
Embodiment 2
[0012] A raw material formula of nano-ivory jade is proposed in this embodiment, including the following mass percentages: 4.13% for Al2O3, 63.43% for SiO2, 8.85% for CaO, 3.61% for BaO, 8.83% for Na2O, and 1% for K2O , CaF2 is 7.9%, Li2O is 0.23%, Sb2O3 is 0.4%, P2O5 is 1.34%, and MgO is 0.28%.
[0013] The nano ivory jade that embodiment one to two makes, compares conventional nano ivory jade, and experimental data is as shown in the table below:
[0014]
[0015]
[0016] As can be seen from the above table, the raw material formula of the nano ivory jade proposed by the present invention has been significantly improved.