A drying tool for nanoporous composite materials

CN112059949BActive Publication Date: 2024-11-26EAST CHINA UNIV OF SCI & TECH
View PDF 0 Cites -1 Cited by

Patent Information

Application Number
CN202010823337.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-17
Publication Date
2024-11-26
Estimated Expiration
2040-08-17

AI Technical Summary

Technical Problem

In the prior art, the thermal protection composite material is unpredictable deformation due to capillary tension and internal stress during drying, which affects the dimensional contour accuracy and yield of the product.

Method used

A drying tool for nanopore composite materials is designed, including inner face plate and outer face plate. Through structures such as locking and thickness limiting blocks, the drying process of the composite material is controlled to ensure that it does not deform during drying, and through Vacuum sealing and elastic pressure-applied devices achieve a tight fit, limiting micro shrinkage, and improving product dimensional contour accuracy.

Benefits of technology

It effectively overcomes the unpredictable deformation of the composite material during the drying process, improves the product dimensional contour accuracy and yield, and ensures the complete drying and deformation-free composite material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112059949B_ABST
    Figure CN112059949B_ABST
Patent Text Reader

Abstract

The invention relates to a drying tool for nanoporous composite materials, comprising an inner profile hole plate, an outer profile hole plate, a thickness limiting block, etc. The various parts of the drying device work together to achieve shape-preserving drying of the nanoporous composite materials. The tool has a simple structure, is easy to operate, can be reused, and has low cost. The tool maintains the shape, the limit block limits the thickness, the elastic pressure device provides uniform elastic constraints, and the heating and drying process is adjusted in stages and steps to achieve shape-preserving drying of the nanoporous composite materials, ensure complete drying of the composite materials, no deformation or micro-deformation, and improve the size profile accuracy and yield rate of the product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of drying tools, and in particular to a drying tool for nanoporous composite materials. Background Art

[0002] Thermal protection materials are one of the key technologies to ensure the safe service of hypersonic vehicles under extreme working conditions. When an aircraft is flying at hypersonic speed, its surface will produce intense friction with the atmosphere, and the severe aerodynamic heating will cause the surface temperature to rise sharply. The local temperature may even exceed 2000℃, which will cause the temperature inside the aircraft to rise. The temperature rise will lead to the degradation of internal materials and structural performance. Therefore, thermal protection materials are needed to protect the aircraft fuselage and internal equipment to keep the temperature within the allowable range to ensure the structural integrity and operational safety of the aircraft.

[0003] As an important part of thermal protection materials, composite materials have received increasing attention from technicians in the field of thermal protection in recent years. However, the preparation of thermal protection composite materials is a systematic project, including resin research and development, preform design and material selection, mold tooling design and processing, composite material molding and processing, and many other links. Patent CN201911266938.7 discloses a high-strength nanoporous ceramic ablative heat-resistant composite material and a preparation method thereof. Patent CN201911325924.8 discloses a preparation method for a low-density heat-resistant composite rotary component. The two patents introduce in detail a preparation method for a thermal protection material, but neither of the two patents elaborates on the drying tooling and drying method. However, the drying tooling and drying method are key factors affecting the final size profile of the composite component. Summary of the invention

[0004] The purpose of the present invention is to overcome the defects of the above-mentioned prior art and provide a drying tool for nanoporous composite materials that can achieve composite materials, shape retention, complete drying, no deformation, and improve product size contour accuracy and yield rate.

[0005] The drying tooling of the present invention effectively overcomes the unexpected deformation of the composite material caused by capillary tension and internal stress of the material during the drying process, ensures complete drying of the thermal protection composite material, achieves no deformation or slight deformation of the final product, and greatly improves the dimensional profile accuracy and yield rate of the product.

[0006] The purpose of the present invention can be achieved by the following technical solutions:

[0007] Thermal protection materials have many advantages such as low density, low cost, ablation resistance, erosion resistance, and thermal insulation. However, as an important part of thermal protection materials, thermal protection composite materials use fiber needle-punched structure preforms as reinforcement, phenolic resin as matrix, and alcohol as solvent.

[0008] After long-term observation and thinking, the designers learned that due to the uneven density of the needle-punched structure reinforcement, there is an uneven distribution of internal forces in the preparation process. During the drying process, there is surface tension at the contact surface between the solvent and the gas in the nanopores, and there is adhesion at the contact surface between the solvent and the solid. The combined effect of these two forces leads to capillary tension. The uneven internal stress and capillary tension of the composite material cause unexpected deformation and warping when the composite material is dried in an unconstrained state, affecting the product shape and contour of the composite material. The following specific solutions are then adopted to solve the above problems:

[0009] A drying tool for nanoporous composite materials, comprising an inner profile hole plate and at least one outer profile hole plate. During drying, the inner profile hole plate and the outer profile hole plate are connected and locked to form a cavity. The nanoporous composite material to be dried is located in the cavity, and two sides of the nanoporous composite material are simultaneously bonded to the inner profile hole plate and the outer profile hole plate.

[0010] Furthermore, the outer shapes of the inner profile hole plate and the outer profile hole plate match the shape of the nanoporous composite material, and the shape of the nanoporous composite material includes a flat plate, a curved plate and a rotating body.

[0011] Furthermore, a thickness limiting block is provided between the inner profile surface plate and the outer profile surface plate to prevent the nanoporous composite material from being over-compressed.

[0012] Furthermore, the profile surface plate is provided with a plurality of thickness limiting block grooves for positioning the thickness limiting blocks, and the depth of the grooves is 2-5 mm.

[0013] Furthermore, during drying, the thickness limiting block is arranged between the inner profile hole plate and the outer profile hole plate. This situation often occurs in the drying of flat plate composite materials and curved plate composite materials. The height of the thickness limiting block is slightly smaller than the distance between the inner profile hole plate and the outer profile hole plate, which can play a certain limiting role in the micro-shrinkage process of the composite material and prevent the composite material from being over-compressed.

[0014] Furthermore, during drying, the thickness limiting block is arranged between each profile surface plate. This situation is often found in the drying of composite materials of rotary parts, because there are generally at least two profile surface plates.

[0015] Furthermore, the inner profile hole plate and / or the outer profile hole plate are provided with holes with a diameter of 1-5 mm and a spacing of 1-10 mm at the joints with the nanoporous composite material. If the hole diameter is too large and the spacing is too small, the hole plate structure will be useless and the purpose of controlling the drying process cannot be achieved. If the hole diameter is too small and the spacing is too large, the solvent will evaporate too slowly and the drying cannot proceed smoothly. After repeated practice, it is considered that the diameter is 2 mm and the spacing is 3 mm as the better solution.

[0016] Furthermore, the edge of the inner profile surface plate is provided with a plurality of positioning grooves for positioning, and the edge of the outer profile surface plate is provided with positioning bosses matching the positioning grooves. This situation often exists in the drying of flat plate composite materials and curved plate composite materials. Sometimes pins can also be used for positioning.

[0017] Furthermore, the inner profile surface plate and the outer profile surface plate are connected and locked by a locking bolt and a locking nut matching the locking bolt. This situation often occurs in the drying of flat plate composite materials and curved plate composite materials. In this case, the locking is mechanical locking.

[0018] Furthermore, a pressure dividing plate and / or an elastic pressure device is provided between the locking bolt and the profile surface plate. The elastic pressure device can be an elastic pressure material or mechanism such as expansion rubber, high expansion metal or spring, such as expansion rubber, the thickness of which is determined by the thickness of the dried nanoporous composite material, the thickness of the composite material is not greater than 20 mm, the thickness of the elastic pressure device is preferably 3-5 mm, the thickness of the composite material is greater than 20 mm, and the thickness of the elastic pressure device is preferably 5-8 mm.

[0019] Furthermore, a pressure dividing plate and / or an elastic pressure applying device is provided between the locking nut and the inner profile hole plate.

[0020] Furthermore, an inner profile hole panel base is provided below the inner profile hole panel, and the inner profile hole panel and the outer profile hole panel are both located above the inner profile hole panel base.

[0021] Furthermore, the outer profile hole panel is paved with a breathable felt, and the breathable felt is provided with a vacuum sealing bag, which is connected to the exhaust pipe and the vacuum system, and a sealing strip is provided between the base of the inner profile hole panel and the vacuum sealing bag. The vacuum negative pressure value shall not be less than 950 mbar. At this time, the locking is pneumatic locking, which is mostly used for drying composite materials of rotary parts.

[0022] After the outer and inner surface plates of the present invention are closed, the drying rate of the composite material is limited, and the differential process of direct drying of the composite material is transformed into a differential process. Since the composite material is in close contact with the outer and inner surface plates, even if the product shrinks slightly during the drying process, the tooling will provide continuous follow-up pressure to ensure that the composite material and the tooling are closely attached during the drying process. The interfacial bonding tension generated by the attachment ensures that the composite material is almost not deformed during the drying process, thereby improving the dimensional contour accuracy and yield rate of the product. This effect can only be achieved in a very subtle differential process. However, in order to allow the drying process to proceed smoothly, the outer and inner surface plates are both provided with a large number of small holes, so that the solvent in the composite material can be fully volatilized when the composite material is dried in the drying tooling, but this volatilization is definitely much slower than the drying rate in an open system.

[0023] The method for drying using the above-mentioned tooling comprises the following steps:

[0024] (1) Assemble the drying tooling: Place the composite material on the inner profile hole plate, place the thickness limiting block into the groove of the outer profile hole plate, place the inner profile hole plate in place with the outer profile hole plate, place the elastic pressure device and the pressure dividing plate under the locking screw and / or above the locking nut, and lock the inner profile hole plate with the outer profile hole plate;

[0025] (2) Heating and drying: The drying tool is placed in the heating device, and the temperature is adjusted in stages. When the composite material is completely dry, the drying tool is cooled to room temperature at a rate of no more than 1°C / min, and the drying tool is taken out of the heating device. The temperature adjustment is divided into two stages. In the first stage, the temperature is raised to 40-60°C and dried for 12-24 h. In the second stage, the temperature is raised to 80-120°C and dried for 12-24 h.

[0026] (3) Disassemble the drying tool: remove the locking screws and locking nuts, remove the pressure divider, remove the elastic pressure device, and check whether it can be used again, remove the exterior surface panel, remove the composite material, and maintain the drying tool.

[0027] Compared with the prior art, the present invention has the following advantages:

[0028] (1) The outer and inner surface plates of the present invention can bring a certain pressure to the composite material when they are closed and positioned. At the same time, the existence of the thickness limiting block can ensure the theoretical thickness of the composite material. Even if the product shrinks slightly during the drying process, the tooling will provide continuous follow-up pressure to ensure that the composite material and the tooling are closely fitted during the drying process, ensuring that the composite material does not deform during the drying process. The outer and inner surface plates are both provided with a large number of small holes, so that the solvent in the composite material can be fully volatilized when the composite material is dried in the drying tooling, thereby ensuring the theoretical density of the product, thereby improving the dimensional profile accuracy and yield rate of the product;

[0029] (2) The outer surface plate and the inner surface plate of the present invention are positioned by a boss, so that the two are more matched and faster, thereby improving the efficiency and success rate of tooling drying;

[0030] (3) A pressure dividing plate and / or an elastic pressure applying device is provided outside the profile surface panel of the present invention. The elastic pressure applying device can continuously apply pressure according to the drying process to ensure that the composite material and the tooling are closely fitted during the drying process and that the composite material does not deform during the drying process;

[0031] (4) In view of the fact that it is difficult to apply pressure inside and outside the rotary parts, the present invention innovatively adopts a pneumatic locking measure to control the pressure of the outer and inner surface plates by controlling the vacuum degree, thereby ensuring that the composite material and the tooling are closely fitted during the drying process and that the composite material does not deform during the drying process;

[0032] (5) The drying tooling of the present invention mainly includes flat plate drying tooling, curved plate drying tooling and rotary body drying tooling, covering almost all nanoporous heat-resistant composite material structure forms. The tooling will provide continuous follow-up pressure to ensure that the composite material and the tooling fit tightly during the drying process, ensure that the composite material does not deform during the drying process, and improve the size contour accuracy and yield rate of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 This is a disassembly diagram of the drying tooling for the flat plate composite material in Example 1;

[0034] Figure 2 This is a diagram of the drying tooling assembly of the flat plate composite material in Example 1;

[0035] Figure 3 A bottom view of the drying tooling for the curved plate composite material in Example 2;

[0036] Figure 4 This is a diagram of the drying tooling assembly of the curved plate composite material in Example 2;

[0037] Figure 5 Schematic diagram of the drying tooling for the composite material of the rotary component in Example 3;

[0038] Figure 6 This is a front view of the drying tooling for the composite material of the rotary component in Example 3;

[0039] Figure 7 It is a front cross-sectional view of the drying tooling for the composite material of the rotary component in Example 3;

[0040] As shown in the figure: inner profile hole plate 1 of flat part, thickness limiting block 2 of flat part, composite material flat part 3, outer profile hole plate 4 of flat part, pressure dividing plate 5 of flat part, hard silicone rubber 6, locking bolts of flat part 7, outer profile hole plate 8 of curved plate part, locking bolts of curved plate part 9, pressure dividing plate 10 of curved plate part, spring 11, inner profile hole plate 12 of curved plate part, composite material curved plate part 13, thickness limiting block 14 of curved plate part, inner profile hole plate 15 of rotary part, composite material rotary part 16, outer profile hole plate 17 of rotary part, thickness limiting block 18 of rotary part, sealing strip 19, vacuum sealing bag 20, breathable felt 21, base 22 of inner profile hole plate of rotary part. DETAILED DESCRIPTION

[0041] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and do not limit the present invention.

[0042] A drying tool for nanoporous composite materials is mainly divided into a flat plate drying tool, including seven parts: a flat plate inner profile hole plate 1, a flat plate thickness limiting block 2, a composite material flat plate 3, a flat plate outer profile hole plate 4, a flat plate pressure dividing plate 5, a hard silicone rubber 6, and a flat plate locking bolt 7. A curved plate drying tool includes seven parts: a curved plate outer profile hole plate 8, a curved plate locking bolt 9, a curved plate pressure dividing plate 10, a spring 11, a curved plate inner profile hole plate 12, a composite material curved plate 13, and a curved plate thickness limiting block 14. A rotary component drying tool includes eight parts: a rotary component inner profile hole plate 15, a composite material rotary component 16, a rotary component outer profile hole plate 17, a rotary component thickness limiting block 18, a sealing strip 19, a vacuum sealing bag 20, a breathable felt 21, and a rotary component inner profile hole plate base 22.

[0043] The diameter of the holes of the inner and outer surface plates described above is 1-5 mm, preferably 2 mm, and the hole spacing is 1-10 mm, preferably 3 mm. The number of thickness limiting blocks of the three drying tools is 4, and the positioning method of the three tools is preferably boss positioning.

[0044] The drying tooling for rotary parts is slightly different from that for flat parts and curved parts. The thickness limit block of the drying tooling for rotary parts is placed between the outer surface plates to limit the outer thickness of the rotary parts. Since the locking of the rotary parts is a vacuum negative pressure environment, it can ensure that the outer surface plate continues to move and fit the rotary parts, without the need for elastic material expansion and pressure. Therefore, the rotary drying tooling removes the elastic force device and the pressure divider plate, and replaces them with air-conducting material breathable felt, which can make the vacuum negative pressure act continuously, evenly and stably on the outer surface plate. The inner surface plates of the three types of tooling mentioned above can all be replaced by composite material forming molds, but the matching relationship needs to be considered. At the same time, the drying temperature should be appropriately increased during the drying process to extend the drying time. This operation can greatly reduce the tooling cost.

[0045] The present invention also provides a drying tool and method for a low-density ablation-resistant nanoporous composite material, including but not limited to the following embodiments:

[0046] Example 1

[0047] A drying tool for a low-density, ablation-resistant nanoporous composite flat sheet, such as Figure 1-2The tooling includes a flat plate inner profile hole plate 1, a flat plate thickness limiting block 2, a composite flat plate 3, a flat plate outer profile hole plate 4, a flat plate pressure dividing plate 5, a hard silicone rubber 6 and a flat plate locking bolt 7; the flat plate outer profile hole plate 4 is provided with four thickness limiting block grooves for positioning the flat plate thickness limiting block 2, and the groove depth is 2-5 mm. The flat plate inner profile hole plate 1 and the flat plate outer profile hole plate 4 are provided with holes with a diameter of 2 mm and a spacing of 3 mm.

[0048] The edge of the inner profile hole plate 1 of the flat plate is provided with four positioning grooves for positioning, and the edge of the outer profile hole plate 4 of the flat plate is provided with a positioning boss matching the positioning grooves. The inner profile hole plate 1 of the flat plate is connected and locked with the outer profile hole plate 4 of the flat plate to form a cavity, and the composite material flat plate 3 to be dried is placed in the cavity and fits with the inner profile hole plate 1 of the flat plate and the outer profile hole plate 4 of the flat plate at the same time. The flat plate thickness limiting block 2 is arranged between the inner profile hole plate 1 of the flat plate and the outer profile hole plate 4 of the flat plate, and the inner profile hole plate 1 of the flat plate and the outer profile hole plate 4 of the flat plate are connected and locked by the flat plate locking bolt 7 and the locking nut matching the flat plate locking bolt 7. A flat plate pressure dividing plate 5 and hard silicone rubber 6 are arranged between the flat plate locking bolt 7 and the outer profile hole plate 4 of the flat plate, wherein the hard silicone rubber 6 is in close contact with the outer profile hole plate 4 of the flat plate.

[0049] A method for drying a low-density ablation-resistant nanoporous composite material flat plate, the drying step comprising:

[0050] Step 1: Combine Figure 1-2 , place the composite material flat plate 3 on the flat plate inner profile hole plate 1, place the flat plate thickness limiting block 2 into the thickness limiting block groove of the flat plate outer profile hole plate 4, use the positioning boss for positioning, assemble the flat plate outer profile hole plate 4 in place, insert the flat plate pressure dividing plate 5 and the hard silicone rubber 6 on the flat plate locking bolt 7 respectively, pass the flat plate locking bolt 7 through the locking hole of the drying tooling, and lock the flat plate locking bolt 7 with a wrench;

[0051] Step 2: Place the drying tool in the heating equipment, raise the temperature of the heating equipment to 30-50℃, keep it warm for 12-24 hours, then raise the temperature to 75-95℃, keep it warm for 12-24 hours, and when the heating is completed, cool the drying tool to room temperature at a rate of no more than 1℃ / min, and take out the drying tool.

[0052] Step 3: Remove the locking bolts 7 of the flat plate, remove the pressure dividing plate 5 and the hard silicone rubber 6 of the flat plate, and check whether they can be reused, then remove the flat plate profile hole plate 4, remove the composite material flat plate 3, and maintain the dry tooling.

[0053] Example 2

[0054] A drying tool for low-density, ablation-resistant nanoporous composite curved plate parts, such as Figure 3-4 The tooling includes a curved plate outer profile hole plate 8, a curved plate locking bolt 9, a curved plate pressure plate 10, a spring 11, a curved plate inner profile hole plate 12, a composite curved plate 13 and a curved plate thickness limiting block 14; the curved plate outer profile hole plate 8 is provided with four thickness limiting block grooves for positioning the curved plate thickness limiting block 14, and the groove depth is 2-5 mm. The curved plate inner profile hole plate 12 and the curved plate outer profile hole plate 8 are provided with holes with a diameter of 2 mm and a spacing of 3 mm.

[0055] The edge of the inner profile hole plate 12 of the curved plate is provided with four positioning grooves for positioning, and the edge of the outer profile hole plate 8 of the curved plate is provided with a positioning boss matching the positioning grooves. The inner profile hole plate 12 of the curved plate is connected and locked with the outer profile hole plate 8 of the curved plate to form a cavity, and the composite material curved plate 13 to be dried is placed in the cavity and fits with the inner profile hole plate 12 of the curved plate and the outer profile hole plate 8 of the curved plate at the same time. The curved plate thickness limiting block 14 is arranged between the inner profile hole plate 12 of the curved plate and the outer profile hole plate 8 of the curved plate, and the inner profile hole plate 12 of the curved plate and the outer profile hole plate 8 of the curved plate are connected and locked by the curved plate locking bolt 9 and the locking nut matching the curved plate locking bolt 9. A curved plate pressure dividing plate 10 and a spring 11 are arranged between the curved plate locking bolt 9 and the outer profile hole plate 8 of the curved plate, wherein the spring 11 is in close contact with the outer profile hole plate 8 of the curved plate.

[0056] A method for drying a low-density, ablation-resistant nanoporous composite material curved plate, the drying step comprising:

[0057] Step 1: Combine Figure 3-4 , place the composite material curved plate 13 on the curved plate inner profile hole plate 12, put the curved plate thickness limiting block 14 into the thickness limiting block groove, insert the curved plate pressure dividing plate 10 and the spring 11 into the curved plate locking bolt 9, and tighten the curved plate locking bolt 9 with a wrench;

[0058] Step 2: Place the drying tool in the heating device, raise the temperature of the heating device to 30-50°C, keep it warm for 12-24 hours, then raise the temperature to 75-95°C, keep it warm for 12-24 hours, and when the temperature rise is finished, cool the drying tool to room temperature at a rate of no more than 1°C / min, and take out the drying tool;

[0059] Step 3: Remove the locking bolts 9 of the curved plate, remove the spring 11 and the pressure plate 10 of the curved plate, remove the outer profile hole plate 8 of the outer curved plate, remove the composite material curved plate 13, and maintain the dry tooling.

[0060] Example 3

[0061] A drying tool for a low-density, ablation-resistant nanoporous composite rotary component, such as Figure 5-7The rotary component includes a rotary component inner profile hole plate 15, a composite rotary component 16, two rotary component outer profile hole plates 17, a rotary component thickness limiting block 18, a sealing strip 19, a vacuum sealing bag 20, a breathable felt 21 and a rotary component inner profile hole plate base 22. The rotary component outer profile hole plate 17 is provided with four thickness limiting block grooves for positioning the rotary component thickness limiting block 18, and the groove depth is 2-5 mm. The rotary component inner profile hole plate 15 and the rotary component outer profile hole plate 17 are provided with holes with a diameter of 2 mm and a spacing of 3 mm.

[0062] The inner profile hole plate 15 of the rotary component is connected and locked with the outer profile hole plate 17 of the rotary component to form a cavity. The composite material rotary component 16 to be dried is placed in the cavity and is simultaneously fitted with the inner profile hole plate 15 and the outer profile hole plate 17 of the rotary component. The rotary component thickness limiting block 18 is arranged between the two outer profile hole plates 17 of the rotary component to limit the outer thickness of the composite material rotary component 16. The inner profile hole plate 15 of the rotary component and the outer profile hole plate 17 of the rotary component are both arranged above the base 22 of the inner profile hole plate of the rotary component. Since the locking of the composite material rotary component 16 is a vacuum negative pressure environment, it can ensure that the outer profile hole plate 17 of the rotary component continues to fit the composite material rotary component 16. There is no need for elastic material to expand and apply pressure, so the elastic force applying device and the pressure dividing plate are removed, and they are replaced by an air-conducting material breathable felt 21. The breathable felt 21 can make the vacuum negative pressure act continuously, evenly and stably on the outer profile hole plate. A sealing strip 19 is provided on the base 22 of the inner profile hole plate of the rotary component, and a breathable felt 21 is arranged on the outer profile hole plate 17 of the rotary component, and an exhaust pipe and a vacuum system are set, and sealed with a vacuum sealing bag 20. That is, the drying tool jacket is provided with a vacuum sealing bag 20, and the vacuum sealing bag 20 is connected to the exhaust pipe and the vacuum system. The vacuum negative pressure value shall not be less than 950 mbar. The sealing strip 19 is a sealing strip formed by the vacuum sealing bag 20, which mainly plays a sealing role. The sealing strip 19 is circumferentially glued to the base 22 of the inner profile hole plate, and the entire outer profile hole plate 17 of the rotary component is wrapped therein. Under the vacuum negative pressure, the vacuum sealing bag 20 is tightened to hold the outer profile hole plate 17 of the rotary component tightly, which is equivalent to pneumatic locking.

[0063] A method for drying a low-density, ablation-resistant nanoporous composite material rotary machine component, the drying step comprising:

[0064] Step 1: Place the composite rotary component 16 on the rotary component inner profile hole plate 15, put the rotary component thickness limiting block 18 into the thickness limiting block groove of the rotary component outer profile hole plate 17, assemble the two rotary component outer profile hole plates 17, arrange the sealing strip 19 on the rotary component inner profile hole plate base 22, arrange the breathable felt 21 on the rotary component outer profile hole plate 17, set the exhaust pipe, and seal it with a vacuum sealing bag 20. Connect the exhaust pipe and the vacuum system, and the vacuum negative pressure resin shall not be less than 950 mbar.

[0065] Step 2: Place the drying tool in the heating equipment, raise the temperature of the heating equipment to 30-50℃, keep it warm for 12-24 hours, then raise the temperature to 75-95℃, keep it warm for 12-24 hours, and when the heating is completed, cool the drying tool to room temperature at a rate of no more than 1℃ / min, and take out the drying tool.

[0066] Step 3: Tear off the vacuum sealing bag 20, remove the breathable felt 21, disassemble the rotary component outer surface plate 17, remove the composite rotary component 16, and maintain the drying tooling.

[0067] In summary, the profile accuracy error of the composite material dried in the free state in the prior art is about δ±6%, and the profile size deformation of some thin plate parts and curved plate parts is even greater, and the thickness tolerance is about ±0.2mm, and the deviation will be greater for thick parts. In Examples 1-3, the profile size accuracy error of the composite material obtained by the tooling and drying method of the present invention is less than δ±2%, and the thickness tolerance is less than ±0.1mm.

[0068] The above is only a preferred embodiment of the present invention, and does not limit the present invention in other forms. Any technician familiar with the profession may use the above disclosed technical content to change or modify it into an equivalent embodiment with equivalent changes. However, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the technical solution of the present invention still belongs to the protection scope of the technical solution of the present invention.

Claims

1. A drying tool for nanoporous composite materials, characterized in that: The tooling comprises an inner profile surface plate and an outer profile surface plate. During drying, the inner profile surface plate and the outer profile surface plate are connected and locked to form a cavity. The nanoporous composite material to be dried is located in the cavity, and two sides of the nanoporous composite material are simultaneously bonded to the inner profile surface plate and the outer profile surface plate. The outer shapes of the inner profile hole plate and the outer profile hole plate match the shape of the nanoporous composite material, and the shape of the nanoporous composite material includes a flat plate, a curved plate and a rotary plate; An inner profile hole plate base is provided below the inner profile hole plate of the rotary component, and the inner profile hole plate and the outer profile hole plate of the rotary component are both located above the inner profile hole plate base; The outer surface of the outer surface plate of the rotary component is paved with air-permeable felt, and a vacuum sealing bag is arranged outside the air-permeable felt. The vacuum sealing bag is connected to the exhaust pipe and the vacuum system, and a sealing strip for sealing is arranged between the base of the inner surface plate and the vacuum sealing bag.

2. A drying tool for nanoporous composite materials according to claim 1, characterized in that: Holes with a diameter of 1-5 mm and a spacing of 1-10 mm are distributed at the locations where the inner profile surface plate and / or the outer profile surface plate are bonded to the nanoporous composite material.

3. A drying tool for nanoporous composite materials according to claim 1, characterized in that: The inner profile hole plate and the outer profile hole plate of the flat plate and the curved plate are connected and locked by using locking bolts and locking nuts matched with the locking bolts.

4. A drying tool for nanoporous composite materials according to claim 3, characterized in that: A pressure dividing plate and / or an elastic pressure applying device is arranged between the locking bolt and the profile surface plate.

5. A drying tool for nanoporous composite materials according to claim 1, characterized in that: A thickness limiting block is arranged between the inner profile surface plate and the outer profile surface plate to prevent the nanoporous composite material from being over-compressed.

6. A drying tool for nanoporous composite materials according to claim 5, characterized in that: The outer profile surface plate is provided with a plurality of thickness limiting block grooves for positioning the thickness limiting block. During drying, the thickness limiting block is arranged between the inner profile surface plate and the outer profile surface plate.

7. A drying tool for nanoporous composite materials according to claim 1, characterized in that: The edges of the inner profile holes of the flat plate and the curved plate are provided with a plurality of positioning grooves for positioning, and the edges of the outer profile holes of the flat plate and the curved plate are provided with positioning bosses matching the positioning grooves.