Semiconductor element and method for manufacturing the same
By performing multi-layer etching in the magnetic tunneling junction element, an asymmetric upper electrode surface and metal inner wire structure is formed, which solves the large area and electricity consumption of existing magnetoresistive random access memory and magnetic field sensing elements. The problem of insufficient sensitivity improves the stability and electrical performance of the component.
Patent Information
- Application Number
- CN201910609150.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-07-08
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-05-19
AI Technical Summary
The existing magnetoresistive random access memory and magnetic field sensing elements have problems such as large chip area, expensive manufacturing process, high power consumption, insufficient sensitivity and susceptibility to temperature changes.
A method of making semiconductor components is adopted to form a magnetic tunneling junction, an intermetal dielectric layer and an upper electrode, and perform multi-layer etching process processing to form an asymmetric upper electrode surface and an inner metal wire structure to reduce the electrode The difference in height with the dielectric layer reduces the occurrence of holes or gaps.
The sensitivity and stability of the component are improved, the height difference between the electrode and the dielectric layer is reduced, the material loss during the etching process is reduced, and the electrical performance of the component is improved.
Smart Images

Figure CN112201746B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor element and a manufacturing method thereof, and in particular to a magnetoresistive random access memory (MRAM) and a manufacturing method thereof. Background Art
[0002] It is known that the magnetoresistance (MR) effect is the effect that the resistance of a material changes with the change of an external magnetic field. The definition of its physical quantity is the resistance difference in the presence and absence of a magnetic field divided by the original resistance, which is used to represent the resistance change rate. At present, the magnetoresistance effect has been successfully used in hard disk production and has important commercial application value. In addition, by utilizing the characteristics of giant magnetoresistance materials having different resistance values under different magnetization states, magnetic random access memory (MRAM) can also be made. Its advantage is that the stored data can continue to be retained when no power is supplied.
[0003] The magnetoresistance effect is also used in the field of magnetic field sensors. For example, the electronic compass components of the global positioning system (GPS) in mobile phones are used to provide users with information such as their moving position. Currently, there are various magnetic field sensing technologies on the market, such as anisotropic magnetoresistance (AMR) sensing elements, giant magnetoresistance (GMR) sensing elements, magnetic tunneling junction (MTJ) sensing elements, etc. However, the disadvantages of the above-mentioned prior art usually include: more chip area, more expensive manufacturing process, more power consumption, insufficient sensitivity, and susceptibility to temperature changes, etc., and further improvement is necessary. Summary of the invention
[0004] An embodiment of the present invention discloses a method for manufacturing a semiconductor device. First, a magnetic tunneling junction (MTJ) is formed on a substrate and a top electrode is formed on the MTJ, then a first intermetallic dielectric layer is formed to surround the MTJ and the top electrode, a stop layer is formed on the first intermetallic dielectric layer, a second intermetallic dielectric layer is formed on the stop layer, a first etching process is performed to remove the second intermetallic dielectric layer and the stop layer, a second etching process is performed to remove a portion of the top electrode, and then a metal interconnect is formed to connect the top electrode.
[0005] Another embodiment of the present invention discloses a semiconductor element, which mainly includes a magnetic tunneling junction (MTJ) disposed on a substrate, an upper electrode disposed on the MTJ and an upper surface of the upper electrode next to a first side wall is different from an upper surface next to a second side wall of the upper electrode, and a first intermetallic dielectric layer surrounding the MTJ and the upper electrode. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figures 1 to 4 It is a schematic diagram of a method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0007] Main component symbols
[0008] 12 substrate 14 MTJ region
[0009] 16 Interlayer dielectric layer 20 Metal interconnect structure
[0010] 22 Metal interconnect structure 24 Intermetallic dielectric layer
[0011] 26 Metal interconnect 28 Stop layer
[0012] 30 Intermetallic dielectric layer 32 Metal interconnect
[0013] 34 Barrier layer 36 Metal layer
[0014] 40 first electrode layer 42 fixed layer
[0015] 44 barrier layer 46 free layer
[0016] 48 second electrode layer 50 MTJ
[0017] 52 lower electrode 54 upper electrode
[0018] 56 Spacer 58 Spacer
[0019] 60 Intermetallic dielectric layer 62 Stop layer
[0020] 64 Intermetallic dielectric layer 66 Patterned mask
[0021] 68 mask layer 70 mask layer
[0022] 72 mask layer 74 first etching process
[0023] 76 contact hole 78 second etching process
[0024] 80 Flat surface 82 Inclined surface
[0025] 84 Metal interconnects DETAILED DESCRIPTION
[0026] Please refer to Figures 1 to 4 , Figures 1 to 4 A schematic diagram of a method for manufacturing a semiconductor device, or more specifically, an MRAM cell, according to an embodiment of the present invention. Figures 1 to 4 As shown, a substrate 12 is first provided, for example, a substrate 12 made of a semiconductor material, wherein the semiconductor material can be selected from a group consisting of silicon, germanium, silicon-germanium composite, silicon carbide, gallium arsenide, etc., and a magnetic tunneling junction (MTJ) region 14 and a logic region (not shown) are preferably defined on the substrate 12.
[0027] The substrate 12 may include active (active) elements such as metal-oxide semiconductor (MOS) transistors, passive (passive) elements, conductive layers, and dielectric layers such as interlayer dielectric (ILD) 16 covering the substrate 12. More specifically, the substrate 12 may include planar or non-planar (such as fin-structured transistors) MOS transistor elements, wherein the MOS transistor may include a gate structure (such as a metal gate) and source / drain regions, spacers, epitaxial layers, contact hole etch stop layers and other transistor elements, and the interlayer dielectric layer 16 may be disposed on the substrate 12 and cover the MOS transistor, and the interlayer dielectric layer 16 may have a plurality of contact plugs electrically connected to the gate and / or source / drain regions of the MOS transistor. Since the related manufacturing processes of planar or non-planar transistors and interlayer dielectric layers are well known in the art, they are not further described here.
[0028] Then, metal interconnect structures 20 and 22 are sequentially formed on the interlayer dielectric layer 16 to electrically connect the aforementioned contact plugs, wherein the metal interconnect structure 20 includes an intermetallic dielectric layer 24 and a metal interconnect 26 embedded in the intermetallic dielectric layer 24, and the metal interconnect structure 22 includes a stop layer 28, an intermetallic dielectric layer 30 and a plurality of metal interconnects 32 embedded in the stop layer 28 and the intermetallic dielectric layer 30.
[0029] In the present embodiment, each metal interconnect 26 in the metal interconnect structure 20 preferably comprises a trench conductor, and the metal interconnect 32 in the metal interconnect structure 22 disposed in the MTJ region 14 comprises a via conductor. In addition, each metal interconnect 26, 32 in each metal interconnect structure 20, 22 may be embedded in the intermetallic dielectric layer 24, 30 and / or the stop layer 28 according to a single damascene process or a dual damascene process and electrically connected to each other. For example, each metal interconnect 26, 32 may further comprise a barrier layer 34 and a metal layer 36, wherein the barrier layer 34 may be selected from the group consisting of titanium (Ti), titanium nitride (TiN), tantalum (Ta) and tantalum nitride (TaN), and the metal layer 36 may be selected from the group consisting of tungsten (W), copper (Cu), aluminum (Al), titanium aluminum alloy (TiAl), cobalt tungsten phosphide (CoWP), etc., but is not limited thereto. Since the single damascene or dual damascene manufacturing process is well known in the art, it is not further described here. In addition, in this embodiment, the metal interconnect 26 preferably includes copper, the metal layer 36 preferably includes tungsten, the intermetallic dielectric layers 24 and 30 preferably include silicon oxide, and the stop layer 28 includes nitrogen doped carbide (NDC), silicon nitride, or silicon carbon nitride (SiCN), but is not limited thereto.
[0030] Then, an MTJ stack structure (not shown) is formed on the metal interconnect structure 22. In the present embodiment, the MTJ stack structure may be formed by first sequentially forming a first electrode layer 40, a fixed layer 42, a barrier layer 44, a free layer 46, and a second electrode layer 48. In the present embodiment, the first electrode layer 40 and the second electrode layer 48 preferably include conductive materials, such as but not limited to tantalum (Ta), platinum (Pt), copper (Cu), gold (Au), and aluminum (Al). The fixed layer 42 may be composed of an antiferromagnetic (AFM) material, such as iron manganese (FeMn), platinum manganese (PtMn), iridium manganese (IrMn), nickel oxide (NiO), etc., to fix or limit the magnetic moment direction of the adjacent layer. The barrier layer 44 may be composed of an insulating material including an oxide, such as aluminum oxide (AlOx) or magnesium oxide (MgO), but is not limited thereto. The free layer 46 may be made of a ferromagnetic material, such as iron, cobalt, nickel or alloys thereof such as cobalt-iron-boron (CoFeB), but is not limited thereto. The magnetization direction of the free layer 46 is "freely" changed by an external magnetic field.
[0031] Then, a patterned mask (not shown) is used as a mask to perform one or more etching processes to remove part of the MTJ stack structure to form upper and lower electrodes and MTJ 50 on the metal interconnect 32, wherein the first electrode layer 40 preferably becomes the lower electrode 52 of the MTJ 50 at this stage and the second electrode layer 48 becomes the upper electrode 54 of the MTJ 50. Then, a liner layer (not shown) is formed on the MTJ 50 to cover the surface of the intermetallic dielectric layer 30, and an etching process is performed to remove part of the liner layer to form a spacer surrounding the MTJ 50, for example, the spacer 56 is arranged on the left side of the MTJ 50 and the spacer 58 is arranged on the right side of the MTJ 50. In the present embodiment, the spacers 56 and 58 preferably include silicon oxide, but other dielectric materials can be selected according to the manufacturing process requirements, for example, silicon oxide, silicon oxynitride or silicon nitride carbide.
[0032] Next, another IMD layer 60 is formed to cover the MTJ 50, and then a planarization process is performed, such as using a chemical mechanical polishing (CMP) process to remove a portion of the IMD layer 60 and make the upper surface of the remaining IMD layer 60 roughly aligned with the upper surface of the spacers 56, 58 and the upper electrode 54. Then, a stop layer 62 is formed on the surface of the IMD layer 60, an IMD layer 64 is formed on the stop layer 62, and a patterned mask 66 is formed on the IMD layer 64. In the present embodiment, the stop layer 62 preferably comprises a nitrogen-doped carbide layer (nitrogendoped carbide, NDC), the intermetallic dielectric layer 64 preferably comprises an ultra-low dielectric constant dielectric layer, for example, it may comprise a porous dielectric material such as but not limited to silicon oxycarbide (SiOC), and the patterned mask 66 may include a mask layer 68, a mask layer 70 and a mask layer 72 in detail, wherein the mask layer 68 preferably comprises silicon oxynitride, the mask layer 70 comprises titanium nitride and the mask layer 72 comprises silicon oxide.
[0033] like Figure 2As shown, a first etching process 74 is then performed to remove a portion of the mask layer 72, a portion of the mask layer 70, a portion of the mask layer 68, a portion of the intermetallic dielectric layer 64, a portion of the stop layer 62, a portion of the spacer 58 and a portion of the intermetallic dielectric layer 60 to form a contact hole 76, wherein the mask layer 72 can be consumed in the etching process. In the present embodiment, the first etching process 74 preferably includes a dry etching process, which preferably uses octafluorocyclobutane (C4F8) and / or carbon tetrafluoride (CF4) as the main etching gas component to remove the above material layers without removing any upper electrode 54 to form the contact hole 76. It is worth noting that the first etching process 74 performed in this stage not only removes a portion of the mask layer above the upper electrode 54, but also removes a portion of the spacer 58 and a portion of the intermetallic dielectric layer 60 on one side of the upper electrode 54, thereby forming asymmetric spacers 56, 58 and allowing the contact hole 76 to penetrate into a portion of the intermetallic dielectric layer 60. Since the upper electrode 54 is not removed by the etching gas at this stage, the angle between the top of the upper electrode 54 and the right side wall or the angle between the top of the upper electrode 54 and the left side wall each includes a right angle.
[0034] Then as Figure 3 As shown, a second etching process 78 is performed to remove a portion of the upper electrode 54 and make the upper surface of the upper electrode 54 next to the first side wall different from the upper surface of the upper electrode next to the second side wall, wherein the second etching process 78 preferably includes a wet etching process, which mainly uses hydrogen peroxide (H2O2) and a fluorine-containing etchant such as but not limited to ammonium fluoride (NH4F) as the main etching components to remove a portion of the upper electrode 54. More specifically, the second etching process 78 performed in this stage preferably uses hydrogen peroxide to oxidize a portion of the upper electrode 54 composed of titanium nitride to form titanium oxynitride (TiON), and then uses a fluorine-containing etchant such as ammonium fluoride (NH4F) to remove the titanium oxynitride, so that the upper surface of the upper electrode 54 near the left side wall of the upper electrode 54 is different from the upper surface of the upper electrode 54 near the right side wall of the upper electrode 54. From a detailed perspective, the upper surface of the upper electrode 54 near the left side wall of the upper electrode 54 includes a flat surface 80 parallel to the surface of the substrate 12 because it is not removed by the second etching process 78, and the upper surface of the upper electrode 54 near the right side wall of the upper electrode 54 includes an inclined surface 82 or a curved surface that is not parallel to the surface of the substrate 12 because it is removed by the second etching process 78. From another perspective, the angle between the top of the upper electrode 54 and the left side wall is still a right angle of 90 degrees, but the angle between the top of the upper electrode 54 and the right side wall is preferably greater than 90 degrees.
[0035] like Figure 4As shown, the contact hole 76 is then filled with the required metal material, such as a barrier layer including titanium (Ti), titanium nitride (TiN), tantalum (Ta), tantalum nitride (TaN), etc., and a low-resistance metal layer selected from low-resistance materials such as tungsten (W), copper (Cu), aluminum (Al), titanium aluminum alloy (TiAl), cobalt tungsten phosphide (CoWP), etc., or a combination thereof. A planarization process is then performed, such as a chemical mechanical polishing process to remove part of the metal material to form a contact plug or metal interconnect 84 in the contact hole 76 to electrically connect the upper electrode 54 below.
[0036] Please refer to Figure 4 , Figure 4 A schematic diagram of the structure of a semiconductor device according to an embodiment of the present invention is also disclosed. Figure 4 As shown, the semiconductor element mainly includes an MTJ 50 disposed on a substrate 12, a lower electrode 52 disposed below the MTJ 50, an upper electrode 54 disposed above the MTJ 50, a spacer 56 disposed on the lower electrode 52, the MTJ 50 and the left side wall of the upper electrode 54, a spacer 58 disposed on the right side wall of the lower electrode 52, the MTJ 50 and the upper electrode 54, an intermetallic dielectric layer 60 surrounding the spacer 56 and the spacer 58, a stop layer 62 disposed on the intermetallic dielectric layer 60, an intermetallic dielectric layer 64 disposed on the stop layer 62, and a metal interconnect 84 disposed in the stop layer 62 and the intermetallic dielectric layer 64 and directly contacting the upper electrode 54.
[0037] In general, the upper surface of the upper electrode 54 near the left side wall of the upper electrode 54 is preferably different from the upper surface of the upper electrode 54 near the right side wall of the upper electrode 54. For example, the upper surface near the left side wall of the upper electrode 54 preferably includes a flat surface 80 parallel to the surface of the substrate 12, while the upper surface near the right side wall of the upper electrode 54 includes an inclined surface 82 or a curved surface that is not parallel to the surface of the substrate 12. In addition, the spacer 56 disposed on the left side of the upper electrode 54 and the spacer 58 disposed on the right side of the upper electrode 54 preferably have different heights, wherein the height of the spacer 58 is preferably lower than the height of the spacer 56, or the upper surface of the spacer 58 is preferably lower than the upper surface of the spacer 56 but the bottoms of the two are preferably cut flush. From the perspective of connecting the metal interconnect 84 above the upper electrode 54, the lower surface of the metal interconnect 84 disposed on the left side wall of the upper electrode 54 is preferably different from the lower surface of the metal interconnect 84 disposed on the right side wall of the upper electrode 54, wherein the lower surface of the metal interconnect 84 disposed on the left side wall of the upper electrode 54 preferably includes a flat surface 80 parallel to the surface of the substrate 12, while the lower surface of the metal interconnect 84 disposed on the right side wall of the upper electrode 54 includes an inclined surface 82 or a curved surface that is not parallel to the surface of the substrate 12. From another perspective, the angle between the top of the upper electrode 54 and the left side wall is still a right angle of 90 degrees, but the angle between the top of the upper electrode 54 and the right side wall is preferably greater than 90 degrees.
[0038] In summary, the present invention mainly forms an intermetallic dielectric layer to cover the MTJ first, then performs a first etching process to remove part of the intermetallic dielectric layer and expose the upper electrode above the MTJ, and then performs a second etching process to remove part of the upper electrode to trim the single upper electrode corner that originally presented a right angle into a roughly arc-shaped corner. Since one of the corners of the top of the upper electrode is formed by the arc-shaped corner formed by the above-mentioned two-stage etching process, the height difference between the upper electrode and the adjacent intermetallic dielectric layer can be reduced. In this way, after the conductive material is subsequently filled to form a metal interconnect, no holes or gaps will be generated between the metal interconnect and the upper electrode to affect the electrical performance of the device.
[0039] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.
Claims
1. A method for manufacturing a semiconductor element, It is characterized in that Include: forming a magnetic tunnel junction on a substrate and a top electrode on the magnetic tunnel junction; forming a first spacer on a first side wall of the upper electrode and a second spacer on a second side wall of the upper electrode, Forming a first intermetallic dielectric layer surrounding the magnetic tunnel junction, the first spacer, the second spacer and the top electrode; forming a stop layer on the first intermetallic dielectric layer; forming a second intermetallic dielectric layer on the stop layer; Performing a first etching process to remove a portion of the second intermetallic dielectric layer, a portion of the stop layer, and a portion of the second spacer to form a contact hole, wherein the contact hole exposes a portion of the second sidewall of the upper electrode, and the lowermost end of the third sidewall of the contact hole contacts the second sidewall of the upper electrode at a predetermined position; Performing a second etching process to remove a portion of the upper electrode so that the upper electrode has an etched upper surface formed by the second etching process, the etched upper surface contacts the third sidewall of the contact hole at the predetermined position, the upper surface of the upper electrode next to the second sidewall is the etched upper surface, and the etched upper surface of the upper electrode includes a curved surface; and A metal interconnect is formed to connect the upper electrode.
2. The method of claim 1, wherein the first etching process comprises a dry etching process.
3. The method of claim 1, wherein the second etching process comprises a wet etching process.
4. The method of claim 3, wherein the second etching process comprises hydrogen peroxide and fluorine. 5 . The method according to claim 1 , further comprising performing the second etching process to remove a portion of the upper electrode and make an upper surface of the upper electrode near the first sidewall different from an upper surface of the upper electrode near the second sidewall. The method of claim 5 , wherein an upper surface of the upper electrode adjacent to the first sidewall comprises a flat surface. 7 . The method according to claim 1 , wherein a corner of the upper electrode at the second sidewall is formed into a rounded corner by the first etching process and the second etching process.
8. The method according to claim 1, wherein an upper surface of the second spacer is lower than an upper surface of the first spacer.
9. A semiconductor device manufactured by the method of claim 1, It is characterized in that Include: A magnetic tunnel junction is disposed on the substrate; An upper electrode is disposed on the magnetic tunnel junction, wherein an upper surface of the upper electrode next to a first side wall is different from an upper surface of the upper electrode next to a second side wall; A first spacer disposed on the first side wall of the upper electrode; A second spacer is disposed on the second sidewall of the upper electrode, wherein an upper surface of the second spacer is lower than an upper surface of the first spacer; A first intermetallic dielectric layer surrounding the magnetic tunnel junction and the upper electrode; A stop layer is disposed on the first intermetallic dielectric layer; A second intermetal dielectric layer is disposed on the stop layer; as well as The metal inner connection line is arranged in the stop layer and the second intermetallic dielectric layer and connected to the upper electrode. 10 . The semiconductor device as claimed in claim 9 , wherein an upper surface of the upper electrode adjacent to the first sidewall comprises a flat surface. 11 . The semiconductor device as claimed in claim 9 , wherein a lower surface of the metal interconnection adjacent to the first sidewall of the upper electrode is different from a lower surface of the metal interconnection adjacent to the second sidewall of the upper electrode. 12 . The semiconductor device as claimed in claim 11 , wherein a lower surface of the metal interconnection adjacent to the first sidewall of the upper electrode comprises a flat surface.