Inspecting the bonding quality of transparent materials using optical coherence tomography

Through optical coherence tomography technology, the joint points and air gaps between transparent material layers are detected in electronic displays, and the problem of difficult detection of invisible joint points in the prior art is solved, and the welding quality and equipment reliability are improved.

CN112262310BActive Publication Date: 2024-11-05CARL ZEISS MEDITEC INC +3
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980039220.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-06-13
Filing Date
2019-06-12
Publication Date
2024-11-05
Estimated Expiration
2039-06-12

AI Technical Summary

Technical Problem

The prior art is difficult to effectively check the invisible bonding points between transparent material layers, especially in the production process of electronic displays, which leads to difficult detection of welding defects, affecting image quality and equipment reliability.

Method used

Optical coherence tomography (OCT) system uses a system to generate scan data to identify binding points and air gaps by focusing the beam below the bonding points between transparent material layers, and determine the width of the bonding points by combining visual inspection and other methods to define the physical parameters of the material. and quality.

Benefits of technology

It realizes efficient detection of invisible bonding points between transparent material layers, can identify welding defects and air gaps, ensure the quality of bonding points, and improves the image quality and equipment reliability of electronic displays.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112262310B_ABST
    Figure CN112262310B_ABST
Patent Text Reader

Abstract

An optical coherence tomography (OCT) system (63) is used to inspect a bond (66A, 66B, 66C) sandwiched between two materials (e.g., layers 62, 64 of a display). OCT distinguishes between a bond (e.g., a weld) and an air gap between the two materials. A bond is identified as a discontinuity of the air gap between the materials. By extracting various physical features of the bond and the gap between the two materials, the system determines whether the bond is defective.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates generally to the field of inspecting bonds of materials that are transparent relative to an inspection light source. More particularly, the present invention relates to inspecting invisible bonds between two layers of transparent material sandwiched between electronic image displays. Background Art

[0002] Image displays are an integral part of many different types of electronic devices. For example, televisions, desktop computers, laptop computers, tablet computers, handheld computers (e.g., personal digital assistants (PDAs), mobile phones, wearable electronic devices (e.g., smart watches), and other specialized electronic devices / tools may include displays for conveying visual information to a user. Such displays may include multiple layers (e.g., a lower substrate layer, multiple intermediate layers, and a top layer), all or some of which are transparent to the human eye, e.g., a glass layer, for conveying visual information from one layer to another.

[0003] Ensuring the bonding of these multiple layers can be challenging. Strong bonding is required because separation between the layers can result in display failure or image quality degradation. However, ensuring a strong bond may require visible bond marks, which are often unattractive or detract from the viewing experience. Therefore, the bonding areas of these layers are often covered by a dark border or frame. In addition, some common types of bonding (e.g., bonding layers or adhesives) may deteriorate over time, which may require an enclosure around the display to provide additional protection for the display.

[0004] It would be desirable to have a strong bonding method that would reduce the need for protective housings and be invisible to the user so as to eliminate the need to cover the bonding area. One promising technology is laser welding of glass, but these welds are often not visible or distinguishable from the surrounding area, which complicates inspection for weld defects.

[0005] It is an object of the present invention to provide a method of inspecting bonding areas within a layer of bonding material.

[0006] Another object of the present invention is to provide a method for inspecting invisible welds within a layer of transparent material.

[0007] Another object of the present invention is to provide a bonding inspection system suitable for a production line. Summary of the invention

[0008] The system and method for checking the bonding between two materials achieve the above-mentioned purpose. The two materials can be different materials or similar materials, and at least one material can be transparent. The two materials can be combined by using laser welding, hot melting, gluing, bonding film, etc. At least some of these bonding methods can produce invisible or transparent bonding (e.g., bonding area). For example, the two materials can be transparent glass layers used to construct electronic displays, and the bonding area can be invisible and sandwiched between the transparent glass layers. In the case of laser glass welding, the laser can be focused below the joint between the two glass layers, and the welding can grow from the lower glass layer into the upper glass layer, thereby forming a bonding area extending into the two glass layers, wherein the bonding point is at the joint of the two layers. Laser welding of glass is desirable because it produces a strong, invisible bond, which helps to construct an electronic display without a frame. However, since the bonding area is glass, like two bonding layers, the bonding area is basically invisible in the two bonding layers, so it is difficult to check for defects.

[0009] A physical layer (e.g., a layer of air or other material) may be located between the two bonding materials, and different layers may produce a dielectric surface. For example, it has been found that due to defects in the surfaces of the two material layers, even after bonding, a gap (e.g., an air gap) may exist between the two layers. The present invention may use an optical coherence tomography (OCT) system (e.g., a spectral domain point scanning system, a scanning source point scanning system, or a spectral domain line scanning system) to apply a sample beam through the first of the two materials (e.g., the top layer) to reach and acquire scanning data of the bonding point sandwiched between the two materials. That is, the OCT may scan an area including the bonding area so that the scan includes the bonding point area and the non-bonding area. Because the bonding area (and the bonding point) may be transparent (e.g., made of the same material as the two bonding layers), if the bonding area is completely uniform after welding, the OCT may not "see" the bonding point (or bonding area) between the two layers, but will "see" (e.g., image) the air gap (e.g., the physical layer between the two bonding materials) surrounding the bonding point at the junction between the two layers. It should be noted that the OCT system can be optimized for specular reflection of any dielectric surface. Thus, OCT can define physical parameters of the bond of two materials based on scan data alone, or in combination with other inspection methods (e.g., visual inspection, reflectometer, ellipsometer, or spectroscopic ellipsometer). The physical parameter can be any metrological property (e.g., measurable property), including at least one of the thickness, refractive index, and birefringence of at least one selected one of the two materials and any other physical layer therebetween. It should be noted that birefringence is generally not an intrinsic material property of glass, but is induced in the glass by stress. Therefore, stress-induced birefringence in glass may be a marker of high stress areas in the glass. It should also be noted that the OCT system can be a polarization-sensitive OCT (PS-OCT) (or can include functionality thereof), which can measure the birefringence properties of the bonded material and / or weld (e.g., two glass layers). For example, OCT can define the width span of the bond point. A lateral scan can produce bright intensity lines corresponding to air gaps between the layers, and dark areas corresponding to invisible bond points that are not detected. Therefore, the bond point produces a break on the bright intensity line, and the length of the break will correspond to the width span of the bond point along the scan direction. The defined physical parameter can then be used to selectively designate the bond of the two materials as defective or non-defective. For example, a good weld can be defined as having a span width no less than a predetermined threshold or within a predetermined width range. Alternatively, if the defined physical parameter is the axial position of the bond region, a good weld can be defined as being within a predetermined region of the junction of the two layers. Further alternatively, a good bond can be defined as having an air gap no greater than a predetermined maximum size air gap. In this case, a smaller air gap may appear as a narrower line in the OCT scan image compared to a larger air gap.Since laser glass welding tends to draw the two glass layers closer together in their vicinity, the width of the larger air gap (in the axial direction) can be compared to the width of the air gap (in the axial direction) adjacent to the bond point. A difference greater than a predetermined percentage (e.g., greater than 25%) may indicate a defective bond. By defining the full width half maximum (FWHM) width of the detected air gap width, the width can be correlated to the brightness measurement.

[0010] It should be noted that the OCT system can be a self-referencing system, thus lacking (or not requiring) a reference arm. For example, the OCT light source can be split into two beams, and a known relative delay can be introduced between the two beams. The two beams can then be combined to form an OCT beam for scanning the sample. The OCT is then self-referencing because a strong reflection from the sample (e.g., a reflection from the front surface of the glass (e.g., the top surface of the top glass layer)) acts as a reference beam, self-interfering through reflections from deeper within the structure (e.g., the binding area). The relative delay between the two beams remains constant regardless of movement in the axial direction, so that such movement of the sample does not adversely affect the OCT system. Similarly, the light collected from the sample can be split into two beams, and a known relative delay can be introduced between the two beams. The two beams can then be combined before the detector. The return light incident on the detector then forms self-interference based on the known delay introduced into the two beams. In such a design, one would typically choose the relative delay between the two beams to be similar to the distance between the reference surface and the region of interest to be imaged.

[0011] It should be noted that the scanning depth of OCT can be extended by using its complex conjugate component. However, this may produce mirror images. In the current case, the upper and lower boundaries of the two layers form bright lines in the OCT image, and the complex conjugate produces a dotted line in the OCT image. In order to determine which image line corresponds to the bond between the two bonding materials, the thickness of one of the two material layers can be used as a reference. For example, the top surface of the top layer is easily identified in the OCT image, and by knowing the thickness of the top layer, the target offset below the top surface of the top layer can be identified (for example, identifying the inspection area within the B scan). The line closest to the offset in the OCT image (or within the defined inspection area) can be identified as corresponding to the bond between the two material layers. Alternatively, since the real and virtual (e.g., complex conjugate) image signals move in phase and out of phase with the delay line, the delay line can be moved to distinguish between the real image signal and the virtual image signal.

[0012] The present system can be implemented in a production line to allow inspection before welding (e.g., to determine whether the gap is suitable for welding), inspection after welding, and / or in-process inspection during welding. For example, the OCT system can scan the bonded glass layers as the glass layers are bonded and advance along the production line. That is, when the OCT system applies its sample beam, the OCT system and the two bonded materials can be continuously displaced relative to each other along a first lateral dimension. For example, the bonded material can be stationary, and the OCT system can move (or scan) over the bonded material. Alternatively, the OCT system can be stationary, and the bonded material can be conveyed through the OCT system on a moving stage (e.g., a conveyor belt) while the OCT system scans through the moving bonded material in a direction perpendicular to the direction of movement of the bonded material (e.g., the first lateral dimension). In this case, the OCT system can also scan in a second direction opposite to the movement of the two bonded materials to offset (eliminate) the displacement of the bonded materials so that the scanning beam defines a scan line perpendicular to one side of the moving bonded material. Different scanning directions can be achieved by using one or more scanners in the OCT. The scanner can be one or more of a galvanometer scanner, a MEMS scanner, an electro-optical deflector, and / or a rotating polygon scanner. Alternatively, the OCT system may implement speckle-reduced wobbling scanning as described in US Publication No. 20070291277, which is assigned to the same assignee as the present invention and is incorporated herein by reference in its entirety.

[0013] Optionally, the OCT can generate multiple images (e.g., multiple B-scans of the same area) and provide an image for examination by averaging the multiple images. In addition, the image for examination can include a frontal image. In addition, the OCT system can be configured to avoid (e.g., lack) any scanning components. This can be achieved by implementing the OCT system as a full-field spectral domain OCT system or a full-field scanning source OCT system.

[0014] Other objects and attainments as well as a more complete understanding of the present invention will become apparent and readily appreciated by referring to the following description and appended claims taken in conjunction with the accompanying drawings.

[0015] The embodiments disclosed herein are merely examples, and the scope of the present disclosure is not limited to these embodiments. Embodiments according to the present invention are disclosed in the attached claims for methods, storage media, systems, devices and / or computer program products, wherein any features mentioned in one claim category (e.g., method) may be claimed in another claim category (e.g., system). Dependent claims or references in the attached claims are selected only for formal reasons. However, any subject matter resulting from an intentional reference to any previous claim may also be claimed, so that any combination of claims and their features may be disclosed and claimed, regardless of the dependencies selected in the attached claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In the drawings, like reference symbols / characters refer to like parts:

[0017] Figure 1 A mobile phone with a bezel-less display (flat screen) is shown;

[0018] Figure 2 Sample layers of an electronic display and sample locations of bonding points are shown;

[0019] Figure 3 Laser glass welding is shown bridging the gap between two glass layers;

[0020] Figure 4A An example of an optical coherence tomography (OCT) system is shown;

[0021] Figure 4B Shows the addition to Figure 4A An example configuration of components of an OCT system to include polarization sensitive OCT (PS-OCT) functionality;

[0022] Figure 4C Shows the application Figure 6 An alternative OCT system for examining material bonding with a simple setup that eliminates the need for a reference arm;

[0023] Figure 5 illustrates the operation of an OCT system and sample images produced by the OCT system;

[0024] Figure 6 shows a setup for examining the bonding of two materials using an OCT system;

[0025] Fig. 7A Two glass layers to be laser glass welded are shown;

[0026] Figure 7B Shows Fig. 7A Laser glass welding of two glass layers;

[0027] Figure 7C shows the bonding by laser welding Fig. 7A The glass layer;

[0028] Fig.7D yes Figure 7C Ideal close-up view of laser welding;

[0029] Figure 8 Two OCT A-scans of two bonded glass layers are shown, one A-scan at the laser weld and the other at the air gap location;

[0030] Fig. 9 An inverse view of an exemplary OCT B-scan of two bonded glass layers with three laser welds is shown;

[0031] Fig.10 A process for extracting OCT scan data related to laser glass welding is shown;

[0032] Fig.11 An OCT B-scan of laser glass welding is shown;

[0033] Fig.12 shows the inspection of laser welds using a combination of OCT B-scans and corresponding frontal images to identify various conditions of laser glass welding;

[0034] Fig.13 An example method for examining the bonding of two materials is shown;

[0035] Fig.14 An example computer device (or computer system) is shown. DETAILED DESCRIPTION

[0036] Commercial and consumer displays (e.g., flat-panel televisions, laptops, tablets, or mobile phones) may present a glass surface to the user. The manufacture of these products requires layering and joining of flat or curved glass or other visually transparent materials. These joins are achieved by gluing or mechanically joining the edges. Mechanical joints may be hidden behind bezels. Modern designs for computers, tablets, mobile phones, and televisions are often "bezel-less," or finished with exposed glass edges.

[0037] Current processes may use glue to bond the glass to the device. The gluing process is often difficult to control, and the gluing may be visible. Therefore, even all-glass front panels often have a black painted border that hides the glue.

[0038] Industry is investigating alternatives to gluing. One alternative is laser welding. Under well-controlled process conditions, welding is virtually invisible to the naked eye, making it a very attractive design for consumer electronics.

[0039] The dimensions of a laser weld cross section can be of the order of 20 to 50 micrometers. The problem with "invisible" laser welds is that they are difficult to inspect. Surface inspection techniques (e.g., ZEISS SurfMax deflectometry) can visualize the presence of a laser weld, but cannot determine whether the weld is at the correct depth.

[0040] The present invention solves the problem of how to inspect a bond point located between (e.g., sandwiched between) two or more layers of material. For illustrative purposes, the present invention is presented as applied to a specific example where one or more bond points are located between transparent layers and the bond points themselves may not be visible to an observer. As mentioned above, one area where this situation exists is the construction of electronic displays (e.g., flat panel electronic displays).

[0041] Electronic displays are usually composed of multiple layers or substrates stacked together, each of which has a different purpose. For example, the bottom layer can provide structural support, the upper layer can be a polarizing layer, the middle layer can provide / support a liquid crystal array or an organic light emitting diode (OLED) array, one or more other layers can provide a color filter, and other layers can provide a touch sensor circuit, etc. Since it is expected that the user will view images on the display, multiple layers need to be transparent. This makes the structure of the display complicated because the circuits and other components need to be hidden from the user. This usually requires a frame, such as a dark frame and / or a structural housing around the viewing area. Even if people try to hide the surrounding circuits, it is still difficult to ensure that the multiple layers of the display remain bonded to each other because the separation of the layers may cause the display to fail. Due to the need for transparency, glass is usually the material choice for some layers of the display. Although various transparent glass bonding technologies (e.g., transparent glue, bonding film and hot melt) have been tried to bond the layers of the display together, these technologies have limitations. For example, these technologies may not provide sufficient transparency, or may not provide sufficient structural bonding strength, or their bonding strength may decrease over time.

[0042] A promising glass bonding technology is laser glass welding, but this technology requires high-quality control because the resulting bond is invisible and a defective weld may not be easily discovered. Laser glass welding typically focuses the laser beam slightly below the boundary between the two glass layers. This creates a bonding area in the lower glass layer that grows upward toward the upper glass layer. Due to defects in the glass surface, a small air gap separates the two glass layers, but if the laser is focused at the right depth with the right energy, the bonding area will be pushed upward to pass through the gap and grow into the upper glass layer. This creates a bonding point that bridges the gap between the two glass layers and a bonding area that penetrates the two glass layers at the junction of the two glass layers. Laser glass welding does not require any additional bonding layer (e.g., a bonding agent), and the final bonding point is made of the same material as the two bonding layers, e.g., clear glass. Therefore, inspection of the final laser weld is not simple.

[0043] To inspect laser glass welds (or other joints / areas sandwiched between two layers of material), an optical coherence tomography (OCT) system is used to scan the joint between the two glass layers, including the joint. The OCT system can identify changes in refractive index encountered during the scanning operation. This enables OCT to identify air gaps between the glass layers, including gaps around laser glass welds. In this way, the present invention can identify various physical properties of laser welds, such as determining the cross-sectional dimensions of the laser weld at the joint, fractures in the weld, gap dimensions and non-uniformities in the area surrounding the laser weld; any of which can be used (alone or in combination) to identify defective laser glass welds.

[0044] In summary, the OCT system is used to inspect a bond between two materials. OCT distinguishes between a bond (e.g., a location of laser welding or glue, tape, heat fusion) and an air gap between the two materials. A bond is identified as a break in the air gap between the materials. In addition, if the welding process changes the refractive index of the material and is away from the expected position, the air gap will have a step change in the axial direction. If the bond itself is not complete, a break in the air gap will show a false signal, for example, the signal intensity at the break will be lower than the signal intensity obtained at the air gap. By extracting various physical features of the bond and the air gap between the two materials, the system determines whether the bond between the two materials is defective.

[0045] As an example of an electronic device, Figure 1A mobile phone 11 is shown having a display (flat screen) 13 with a bezel. The bezel may consist of a dark area 15 and / or a housing 17 that partially covers the display 13 and surrounds the viewing area of ​​the display 13. Other examples of electronic devices that may use an electronic display (e.g., display / screen 13) include televisions, desktop computers, notebook computers, tablet computers, handheld computers (e.g., personal digital assistants PDAs), wearable electronic devices (e.g., smart watches), dedicated electronic tools, and the like. It should be understood that although the display 13 is shown as having a rectangular shape, the display may be configured to have any shape, e.g., circular, triangular, hexagonal, and the like. As shown, the bezel limits the available viewable area of ​​the display 13, but the bezel is traditionally necessary to provide structural support and protection, and to hide the circuitry and bonding areas of the display 13 from the user. Similar to the display 13, the flat panel display is composed of multiple layers of material that need to be bonded together and secured.

[0046] Figure 2 Sample layers of electronic displays that can avoid the use of borders and sample example locations B1, B2, and B3 for bonding points are shown. The electronic display can be composed of multiple material layers 23, and in this example, the display has a curved edge that can extend the viewing area beyond the area traditionally covered by the border. Examples of such displays are provided in U.S. Publication 20160299527 of Kwok et al., the entire contents of which are incorporated herein by reference. Bonding locations B1, B2, and B3 can bond any or all of the bonding points between different layers 23. Bonding locations B1, B2, and B3 can be located anywhere on the display, including planar areas and curved areas. Depending on the arrangement of the glass layers to be bonded, the bonding locations can be located on any one side, all sides, or a combination thereof of the device. Peripheral circuits can be hidden at the ends of the display (e.g., beyond the curved area) to avoid the need for borders on these sides. Each layer can provide different display functions. For example, layer 23A can be an upper polarizing layer, and layer 23E can be a lower polarizing layer. In the case of a liquid crystal display, inner layer 23C constitutes the liquid crystal layer, and layers 23B and 23D can be substrate layers that support thin film transistors, conductive traces, color filter elements, etc. Optionally, touch sensor electronics can be constructed on other layers. For ease of viewing, some layers can be transparent substrates and made of different materials, such as transparent glass layers, plastic sapphire or other crystalline materials, transparent ceramic materials, etc. The different layers need to be firmly bonded together. Some typical bonding types include laser welding, heat fusion, gluing, adhesive films, etc. In particular, laser welding (e.g., laser glass welding) can provide a strong, invisible bond without the need for any bonding agent.

[0047] Figure 3A photograph and schematic diagram of a laser glass weld 31 bridging a gap 33 between an upper glass layer 35 and a lower glass layer 37 are shown. The laser glass weld can be constructed by applying a laser beam at a focal point 39 at the lower portion of the two glass layers to be welded (e.g., the lower glass layer 37). Preferably, the focal point 39 is close to the gap 33 between the upper glass layer 35 and the lower glass layer 37 and below the gap 33 (e.g., a boundary or air gap). This can produce a plasma region 40 (e.g., or a molten region or a bonding region) that grows upward toward the upper glass layer 35. The area surrounding the plasma region 32 can be referred to as a heat affected zone 32, in which the glass is heated. Under normal conditions, this region will have optical properties that can be a combination of the optical properties of the glass layer 35 and the glass layer 37. If the optical properties of the two glass layers 35 and 37 are sufficiently different or if any anomalies occur in the welding process, such as reaching a breakdown threshold of the material, it may cause the refractive index or optical path length of the detection beam to change. With the appropriate laser intensity and the appropriate focus position, the plasma region 40 and the heat-affected zone 32 can push the upper surface of the lower glass layer 37 upward to contact and grow into the upper glass layer 35. This produces a successful weld of the upper glass layer 35 and the lower glass layer 37. The extent and growth of the plasma region 40 and the heat-affected zone 32 depend on the intensity of the laser. If the focus 39 is too far below the gap 33, the plasma region may not bridge the gap 33, and the two glass layers 35 / 37 may not be successfully welded. If the focus is too close to the joint, the welded joint may be too thin to provide a determined bonding strength. In addition, if the laser power is insufficient, the plasma region may not bridge the gap 33 and the two glass layers 35 / 37. It should be noted that when the two glass layers 35 / 37 are welded together, they are pulled closer so that the gap 33 is reduced, at least in the peripheral area of ​​the laser weld (e.g., the joint). As shown, the laser weld can generally have an inverted teardrop shape, so that for a given laser power (the diameter of the plasma zone and the heat-affected zone can be determined), a relationship (or correlation) can be established between the diameter of the laser weld and the position of the focus. Therefore, the offset of the laser weld (or focus) in the axial direction (z direction) relative to the gap between the glass layers 35 / 37 can be determined. However, since current laser welds are generally invisible and are made of the same material as the two layers being bonded together (e.g., glass), it has been difficult to inspect such welds for defects to date, making it impossible to rely solely on laser glass welding to bond multiple glass layers to construct a borderless display. For example, Gupta's U.S. Publication 20170199405 applies laser glass welding to the side profile of a display, but relies on a bonding agent to bond the upper layer of the display to the lower layer, and therefore a borderless display cannot be achieved.

[0048] To ensure reliable laser glass welds, a method of checking such welds in production is needed. In some embodiments, the present invention indirectly monitors the quality of laser glass welds by observing the air gap around the laser glass weld between the upper glass layer and the lower glass weld.

[0049] Figure 4A An example of an optical coherence tomography (OCT) system is shown that can be used to provide OCTA images. For ease of illustration, the present OCT system is illustrated as imaging an eye, but it should be understood that the present OCT system (or variations of the present OCT system) can be used to image other samples, such as layers of bonding materials used in the construction of flat panel displays. Light from a light source J1 is typically routed along a sample arm through an optical fiber J3 to illuminate a sample J5, such as tissue in a human eye or other test sample. The light source J1 can be a broadband light source with a short temporal coherence length in the case of spectral domain OCT (SD-OCT), or a wavelength-tunable laser source in the case of swept source OCT (SS-OCT). The light is typically scanned with a scanner J7 between the output end of the optical fiber J3 and the sample J5, so that the light beam (dashed line J7) is scanned laterally (e.g., in the x-direction and / or y-direction) over the area or volume to be imaged. Light scattered from the sample J5 is collected, typically entering the same optical fiber J3 used to route the light for sample illumination. Reference light derived from the same light source J1 travels along a separate path (e.g., a reference arm), in this case, including an optical fiber J11 and a reflector J13 with an adjustable optical delay. Those skilled in the art will recognize that a transmission reference path may also be used, and that the adjustable delay may be placed in the sample or reference arm of the interferometer. The collected sample light is typically combined with the reference light in a fiber coupler J15 to form optical interference in a detector J17. Although a single fiber port J19 is shown leading to the detector J17, those skilled in the art will recognize that various designs of interferometers may be used for balanced or unbalanced detection of interference signals. The output from the detector J17 is provided to a processor (e.g., a computing device / system) J21. The results may be stored in the processor J21 and / or displayed on a display J23. The processing and storage functions may be located within the OCT system or instrument, or the functions may be performed on an external processing unit to which the collected data may be transmitted. The external processing unit may be dedicated to data processing or to performing other very general tasks that are not dedicated to the OCT device. The processor J21 may include, for example, a field programmable gate array (FPGA), a digital signal processor (DSP), an application specific integrated circuit (ASIC), one or more general purpose graphics processing units (GPGPU), a system on a chip (SoC), or a combination thereof.

[0050] The sample arm and reference arm in the interferometer can be composed of bulk optics, fiber optics or hybrid bulk optics systems and can have different structures, for example, Michelson, Mach-Zehnder or common path based designs known to those skilled in the art. The light beam used in this article can be any carefully guided light path. In time domain systems, the reference arm can have an adjustable optical delay to produce interference. Balanced detection systems are commonly used in time domain OCT (TD-OCT) and SS-OCT systems, while spectrometers are used in the detection ports of SD-OCT systems. The invention described herein can be applied to other types of OCT systems, for example, point scanning, multi-point scanning, partial field and full field imaging systems or speckle reduction swing scanning (for example, as described in U.S. Publication 20070291277, the entire contents of which are incorporated herein by reference).

[0051] In Fourier domain optical coherence tomography (FD-OCT), each measurement is a real-valued spectral interferogram (Sj(k)). The real-valued spectral data usually undergoes multiple post-processing steps, including background subtraction, dispersion correction, etc. The Fourier transform of the processed interferogram produces a complex-valued OCT signal output The absolute value of this complex OCT signal |Aj| reveals the distribution of scattering amplitudes (or intensities) at different path lengths, and therefore scattering as a function of depth (z-direction) in the sample. Similarly, the phase φj can also be extracted from the complex-valued OCT signal. The distribution of scattering as a function of depth is called an axial scan (A-scan) and can refer to a pixel on an image. A set of A-scans measured at adjacent locations in a sample produces a cross-sectional image (a tomogram or B-scan) of the sample and can be referred to as a fast scan (e.g., a lateral or transverse scan). A collection of B-scans collected at different transverse locations on the sample constitutes a data volume or cube (e.g., sometimes referred to as a slow scan). For a particular amount of data, the term "fast optical axis" can refer to the scanning direction along a single B-scan, while the "slow optical axis" can refer to the axis along which multiple B-scans are collected. A frontal image viewed along the axial direction (Z-direction) can be referred to as a frontal image and can be constructed by averaging the volume data along the axial direction. In addition, multiple scans of the same area of ​​a sample can be averaged together to provide a clearer structural image. There are many ways of generating B-scans known in the art, including but not limited to, in the horizontal or x-direction, in the vertical or y-direction, in the x and y diagonal, or in a circular or spiral pattern. The B-scan can be xz dimensional, but can be any cross-sectional image that includes a z dimension.

[0052] Figure 5The operation of an OCT system is shown, and sample images that can be produced by the OCT system are provided. The OCT beam is applied axially in the z direction to define a single A scan. This can be referred to as a one-dimensional (1D) scan or A scan. As described above, the returned backscatter is combined with a reference signal from a reference arm to extract axial position information. Multiple A scans can be performed adjacent to each other in a lateral scan (e.g., scanning the OCT beam in the X direction) to define a two-dimensional (2D) scan or B scan. This produces a 2D slice image of the test object. An example of a B scan of a laser glass weld 51 is shown. Multiple B scans can be performed adjacent to each other to produce a three-dimensional (3D or volume) scan, which can be referred to as a volume or cube. This can be achieved by scanning in the X-axis and Y-axis directions. By projecting the volume onto the XY plane, a front view or front view of the test object can be defined. A front image of a laser glass weld 53 is shown.

[0053] In some embodiments, a customized OCT system can be used to image a transparent layer sample after it has been laser welded at an inner surface interface. The present invention can assess the presence of a weld and the lateral dimensions of the weld within the material (e.g., between two layers). This method enables visual and automated inspection of laser welds or thermal fusion within a transparent medium.

[0054] Figure 6 A combined setup of using an OCT system 63 to examine a multi-layer sample 60 (e.g., a layer of air (or other physical layer) between two material layers) according to the present invention is shown. The OCT engine 61 provides data acquisition and scanning control. For example, the OCT engine 61 may include Figure 4AThe OCT system includes a light source J1, a light detector J17, a processor J21, a fiber coupler J15, and a reference arm. The OCT engine 61 applies a sample beam (e.g., an OCT beam) to a scanner 65 via an optical fiber and a collimating lens. In this example, the scanner 65 scans the OCT beam along the X-axis through a scanning lens 69 to create a B-scan 67 along the XZ plane. The OCT system 63 can be optimized for specular reflections of any dielectric interface between layers. The OCT beam scans a multilayer sample 60 (e.g., more than two layers), but in this example, the multilayer sample 60 is shown as including two bonded material layers (upper layer 62 and lower layer 64) with an air gap (e.g., an additional physical layer) therebetween, and three rows of bonding points (e.g., laser welds) 66A, 66B, and 66C sandwiched between the upper layer 62 and the lower layer 64. Laser welds 66A, 66B, and 66C may be formed in dotted and / or dashed patterns, and although they are schematically shown as being arranged linearly, they may be arranged in a single location or multiple locations in any free-form pattern. OCT engine 61 scans multiple layers of sample 60 as sample 60 moves continuously along the Y-axis direction. For example, a motion platform (e.g., a conveyor belt) may provide such motion. Alternatively, multiple layers of sample 60 may be stationary while the OCT system moves relative to sample 60. Alternatively, the OCT system may provide a second scanner to scan along the Y-axis (e.g., see Figure 4A The OCT system's scanner 67 is coupled to the X-scanner 67 to counteract the Y-axis motion of the multi-layer sample 60. In this manner, the X-scanner 67 can capture B-scans that are truly perpendicular to the sidewalls of the multi-layer sample 60, as if the sample 60 were stationary relative to the OCT system. The OCT engine 61 can process the scan data to provide an OCT image 68 and provide a combined examination, as explained more fully below.

[0055] The OCT system 63 can define / determine one or more physical parameters of the two bonded materials and any other physical layers therebetween, as explained more fully below. The physical parameters can be determined based on the scan data alone, or in combination with other inspection methods, such as visual inspection, a reflectometer, a deflectometer, an ellipsometer, or a spectroscopic ellipsometer. Visual inspection can be used to determine any obvious damage to the glass, such as the formation of air gaps or contamination or Newton's rings. A reflectometer can be used to determine a refractive index and / or thickness map of a sample based on complex reflections of the sample. An ellipsometer can be used to determine a polarization property map including a refractive index and thickness map of a sample. A spectroscopic ellipsometer can be used to determine a polarization property map including a refractive index and thickness map of a sample as a function of wavelength, and can determine these parameters more accurately than other methods.

[0056] Alternatively, the functionality of the OCT system 63 can be expanded. For example, the OCT system 63 can include material specific contrast, which can be used to directly distinguish different materials (e.g., tissues). That is, in addition to intensity, the present OCT can also take advantage of additional properties of light. For example, the present OCT can include the functionality of polarization-sensitive OCT (PS-OCT) and take advantage of the fact that some materials and tissues can change the polarization state of light, thereby adding additional contrast channels and providing quantitative information. The OCT system 63 can include the functionality of PS-OCT by including some additional components, which can be included in the OCT engine 61 where appropriate.

[0057] Figure 4B Shows the addition to Figure 4A An example configuration of components of an OCT system to incorporate polarization-sensitive OCT (PS-OCT) functionality. Figure 4AAll similar elements have similar reference symbols and are described above. It should be understood that any and all of these added components can be selectively and functionally removed (or circumvented or deactivated) as needed to achieve specific OCT functions, as understood by those skilled in the art. A polarization controller (not shown) can be added to the light source J1, and a polarizer J33 can also be added to the light source J1. A first quarter wave plate (QWP) J39 can be added to the reference arm, and a second QWP J37 can be added to the signal arm. A polarization beam splitter J31 can be placed after the light interferes and before any detectors to split the light beam into two orthogonal polarization states. Duplicate detectors J17 and J37 can then detect the two orthogonal polarization states. The processor J21 can then process the information to extract the Jones matrix elements. For a more comprehensive description of PS-OCT, see De Boer, Hitzenberger, and Yasuno, “Polarization sensitive optical coherence tomography—a review [Invited],” Biomedical Optics Express 1838, Vol. 8, No. 3, March 1, 2017, the entire contents of which are incorporated herein by reference. PS-OCT uses the information carried by polarized light to extract additional information about the material, which may help to better distinguish different materials. An example of using PS-OCT to examine material coherence is to determine the birefringence of a sample. This information may not be available using only a simple OCT system. This information can further be used to determine the stresses induced before and after the welding process. This can further be used to examine the degradation of the weld as it ages. Birefringence is a material property of crystals, but not of glass. However, birefringence can be induced in glass by stress, forming so-called “stress-induced birefringence.” This stress-induced birefringence of glass can be used as a marker for high stress areas of the glass. For example, if cracks are forming in glass (e.g., glass welding), it can be expected that these cracks will form in high stress areas, which can be identified by birefringence. In this way, the examination of birefringence in glass provides an immediate advantage by indicating locations that may be more susceptible to cracks or other damage.

[0058] Figure 4C Shows the application Figure 6 An alternative OCT system for examining material bonding. Figure 4A , Figure 4B and Figure 6 All elements of the elements have like reference numerals and are as described above. Figure 4C The OCT configuration eliminates the need for a reference arm, e.g. Figure 4A and Figure 4BFiber J11 and reflector J13. In this configuration, light from the light source J1 is routed through an optical coupler J41 along at least two delay paths J43A and J43B to corresponding reflectors (e.g., mirrors) J45A and J45B, each of which provides a different delay to achieve a self-referencing configuration. The distance offset (spacing) J47 between the reflectors J45A and J45B is known and is preferably similar to the region of interest to be imaged, for example, similar to the distance between the front surface of the sample 60 and the bonding area between the two glass layers. Therefore, the delay introduced by each reflector relative to the other is also known. The two differently delayed return signals from paths J43A and J45B are combined at the fiber coupler J41 and routed through the scanner J7 to the sample 60 to be imaged via a second fiber coupler J42. In the present case, the sample to be imaged is shown as Figure 6 The multi-layer sample 60, and the scanner is shown as Figure 4A and Figure 4B XY scanner J7. The scattered signals returning from the multi-layer sample 60 arrive at the photodetector J17 through the fiber coupler J42, where they form an interference pattern due to self-interference based on the different delays introduced by the paths J43A and J43B. In this way, the captured light is self-referenced and no separate reference arm is required. In addition, since the relative delay between the two signals from the paths J43A and J45B remains constant regardless of the axial motion, the performance of the OCT system is not adversely affected by the axial motion of the sample 60. As described above, the processor J21 can then convert the interference pattern into a spectrum for further analysis.

[0059] Thus, the OCT system 63 determines metrological characteristics (eg, measurable properties) including at least one of thickness, refractive index, and birefringence of at least one of the two materials and any other physical layers therebetween.

[0060] FIG. 7A to FIG. 7D The laser welding process is shown in Fig. 7A In laser welding, two glass samples are placed together with a small air gap between them. Optionally, a vacuum or clamping can be used to reduce the size of the gap before laser welding. Figure 7B Shows Fig. 7A Laser glass welding of two glass layers. The laser focuses and melts the surfaces of the two glasses (e.g., top and bottom glass). The weld is made inside the sample (e.g., bridging the gap between the upper and lower glass). Once the laser is turned off, the glass cools, hardens, and joins, creating a laser weld, such as Figure 7C shown. Fig.7D yes Figure 7CIdealized close-up view of a laser weld. The weld is made with the two pieces of glass being the same material and therefore completely transparent. If the two pieces of glass were different, the resulting weld would likely contain slightly different refractive index properties.

[0061] Figure 8 Two OCT A scans of two bonded glass layers 82 / 84 are shown, one A scan 81 is located at the laser weld 85 and the other A scan 83 is located at the air gap position 87. OCT is sensitive to scattering and specular reflection. The glass sheets (or layers) 82 / 84 and the laser weld 85 have high optical quality and uniformity and are free of scattering. Therefore, OCT signals are obtained from the specular reflection of the air / glass interface. Therefore, a single A scan 81 applied perpendicular to the surface of the top glass 82 and propagated through the weld 85 will detect two signals 71 / 72, one signal 71 at the top surface of the top glass 82, and one signal 72 at the bottom surface of the bottom glass 84. As shown, a single A scan 83 through the unwelded area will in turn detect four signals 73, 74, 75 and 76 at the top and bottom air-glass boundaries of each glass layer 82 / 84. Scanning the A scan in the x direction (e.g., transverse) results in a B scan, which represents a cross-section of the weld area.

[0062] Fig. 9 An inverse view of an exemplary OCT B-scan 94 of two bonded glass layers with three laser welds is shown. Typically in black and white images, Fig. 9 The areas shown as dark would be light representing strong scattered signals, but for ease of viewing, an inverse view of a typical black and white image is provided. Using the above method, the OCT system can detect the presence and width of a laser weld, as shown in B-scan 94. Line 93 represents the interface (e.g., a gap) between two bonded glass layers. As shown, line 93 is interrupted by three blank areas (low signal areas or no signal areas). These blank areas correspond to the locations where three welds are placed in parallel to bond two glass layers (e.g., two microscope slides or other structures with glass-glass bonding). The signal at the air gap 93 is significantly lower than the signal 95 at the top surface and the signal 97 at the bottom surface because the air gap is limited by the surface roughness of the two internal glass surfaces. Occasional contact between the two slides reduces the overall signal intensity. Through changes in signal intensity, the OCT system can infer the uniformity of the mechanical contact between the two slides. Interruptions in uniformity (e.g., an increase in signal intensity of more than 25%) may indicate a welding defect.

[0063] Various image enhancement, image processing and automatic detection of weld width techniques can be incorporated into this process. Fig.10An enhancement process for extracting OCT scan data associated with laser glass welding is shown. B-scan 101 shows multiple lines (real lines and dotted lines due to reflection images, e.g., caused by the application of complex conjugates in the operation of the OCT system, resulting from the application of Fourier transforms). Optionally, B-scan 101 can be binarized to produce B-scan 102. In order to identify the real line corresponding to the boundary between the two layers, an inspection region 103 where the target real line is expected to reside can be identified. As described above, the strongest signal line may correspond to the upper surface of the upper layer and the lower surface of the lower layer. Therefore, the inspection region 103 can be determined from the known depth (thickness) of the upper and / or lower layers. The inspection region 103 can then be extracted, as shown, for a closer inspection. The inspection region can also be mapped to the original B-scan 101. In this example, the X coordinate can correspond to the A-scan position and be associated with a unit of length. In this way, the width span of the weld along the B-scan can be detected. The lateral (lateral) resolution is preferably less than the expected width detection. In this example, the lateral coordinates of the three detected welds (corresponding to the detected gaps) are (165-188), (240-265), and (312-340). A good weld can be determined from a known good reference weld (e.g., a so-called "golden weld"). Various physical features can be extracted from the golden weld, and parameters for detecting defective welds can be constructed therefrom. Parameters that are considered more important for good welds may be weighted more heavily when distinguishing between good welds and defective welds.

[0064] Fig.11 Another OCT B scan of a laser glass weld is shown. The observed width of the detection gap can be used to determine if the weld is off target (e.g., if the laser focus is not at the expected depth). Figure 3 ), which can be determined by establishing a correlation between the weld width at the junction of the two layers and the focal point of the laser glass weld. This can be done by checking a gold weld as a reference. The present setup can be incorporated into existing production lines to provide automatic inspection and checking of welds (e.g., determining the correct position and size of the weld), for example, to ensure their alignment.

[0065] The above examples use transparent glass samples, but the present method can also be applied to other transparent materials (e.g. transparent to the OCT beam), where the transparency is defined relative to the OCT wavelength range, i.e., with this approach, the OCT system can detect bonds or welds inside materials that transmit the OCT wavelength. For example, the present system can inspect welds of opaque plastics at an appropriate wavelength to allow the OCT beam to pass through the plastic.

[0066] If the dispersion properties of the weld are determined, an OCT system with an appropriate wavelength can be selected in which the weld can also be directly observed. For example, the scattering properties of a material can be changed by melting and cooling. By understanding the scattering properties of a laser glass weld and assuming that they are different from its surrounding medium (e.g., non-welded glass), the frequency of the OCT beam can be selected that responds to the laser weld rather than the glass layer. This will produce a 3D image of the laser glass weld within the bonded material.

[0067] Furthermore, since the Z direction in OCT depends on the optical path length, i.e., the product of distance times the material refractive index, any anomaly in the material refractive index will show up as a discontinuity at the next air-sample interface. This is especially true if the two materials being welded together have different optical properties, such that the resulting weld area has different optical properties than the surrounding area, thereby enabling direct visualization of the weld area by the OCT system.

[0068] The method can also be used to measure the thickness of the sample before and after welding. This can detect any bulges or depressions in the welded sample caused by defects in the welding process. This method can further detect defects in the sample, such as bad boundaries, contamination, incomplete welds and damaged spots. In addition, the contrast, signal-to-noise ratio (SNR) and image quality of the B-scan can be improved by: a) averaging; b) using "wobble scanning" to reduce speckle (according to US 20070291277A1); c) avoiding the etalon effect by tilting the sample; and d) avoiding the etalon effect by tilting the incident beam using a y-scanner.

[0069] Frontal images generated by the OCT system can also be used to obtain additional information on weld anomalies in combination with or independently of visual inspection or B-scan data. Generating a frontal image over a given 2-D area helps detect any contaminants on the glass. The frontal image can be generated as a continuous image by applying relative motion between the sensor and the sample. As described above, the sample can be moved with the movement of the Y motion stage, or the OCT sensor can be moved relative to the sample. The frontal image can also be generated by scanning in the X and Y directions using a scanner in the scan head of the OCT system. The use of frontal analysis enhances the determination and quantification of the weld area. The frontal image can also be used to ensure that the OCT beam is perpendicular to the direction of motion of the glass material, thereby helping to determine perfect alignment of the OCT beam.

[0070] Fig.12The laser welds are inspected using a combination of OCT B-scans (upper row) and corresponding frontal images (lower row) to identify various cases of laser glass welding. Sample 1 shows a good laser weld. Sample 2 shows a defect due to a bad boundary. This is shown in the light spot of the boundary line (e.g., a break in its uniformity) in the B-scan and as an interruption of the laser weld in the weld pattern in the corresponding frontal image. Sample 3 is an example of contamination between two glass layers. In its B-scan, this is shown as a long bright line, indicating a relatively large separation between layers. As mentioned above, a good weld will generally reduce the separation between the layers. The contaminants are also visible in the corresponding frontal image. Sample 4 shows an incomplete weld. This particular defect is more obvious in the frontal image, where a break in the weld can be seen. However, the B-scan can also identify a break in the uniformity of the boundary line, which is an indication of a defective weld. Sample 5 shows an example of a damaged point in the weld. The B-scan shows the damaged point as multiple cracks smaller than the required width and intermittent bright spots. The damage is also obvious in the corresponding frontal image. This is also a case where the weld significantly changes the optical properties of the material, making the boundary discontinuous.

[0071] Fig.13 An example method for inspecting the bonding of two materials is shown. The method may start at step S1, where two (or more) bonding materials are provided (e.g., obtained) for inspection. The two materials may be bonded by at least one bonding point sandwiched therebetween. The two materials may be, for example, transparent glass layers, and the bonding point may be defined by laser glass welding. At step S3, an optical coherence tomography (OCT) system is used to apply a sample beam through the first of the two materials (e.g., through the top glass layer) to reach and acquire scan data of the bonding point sandwiched between the two materials. As described above, the sample beam may penetrate the two material layers so as to observe the air gap therebetween. At step S5, at least one physical parameter of the bonding of the two materials is defined based on the scan data. For example, the scan data may be used to determine the width span of the laser weld at the junction of the two material layers, or to identify a break in the laser weld, or an air gap greater than a maximum distance, or an inhomogeneity (e.g., a sudden change) in the size of the air gap, especially near the laser glass weld. At step S7, based on the defined physical parameters, the bonding of the two materials is selectively designated as defective. For example, if the width of a scanned laser weld is not within a predetermined range, the laser weld may be designated as defective. Similarly, if the air gap near a glass weld is greater than a predetermined maximum value, the weld may be designated as defective. Otherwise, the laser weld may be designated as non-defective.

[0072] Although this disclosure describes and illustrates the sequence of events occurring in a particular order Fig.13 However, the present disclosure contemplates the steps occurring in any suitable order. Fig.13 any suitable step of the method.

[0073] Fig.14 An example computer device (or computer system) is shown, for example, Figure 4A , Figure 4B and Figure 4C In some embodiments, one or more computer systems may execute Fig.13 The computer system may take any suitable physical form. For example, the computer system may be an embedded computer system, a system on a chip (SOC), a single board computer system (SBC) (e.g., a computer on a module (COM) or a system on a module (SOM)), a desktop computer system, a laptop or notebook computer system, a computer system grid, a mobile phone, a personal digital assistant (PDA), a server, a tablet computer system, or a combination of two or more of these systems. Where appropriate, the computer system may reside in a cloud, which may include one or more cloud components in one or more networks.

[0074] In some embodiments, the computer system includes a processor 202, a memory 204, a storage 206, an input / output (I / O) interface 208, a communication interface 210, and a bus 212. The computer system may also optionally include a display 214, such as a computer monitor or screen. The processor 202 includes hardware for executing instructions, such as instructions that constitute a computer program. For example, the processor 202 may be a general-purpose computing (GPGPU) on a central processing unit (CPU) or a graphics processing unit. The memory 204 may include a main memory for storing instructions that the processor 202 executes or saves temporary data during processing. For example, the memory 204 may include a random access memory (RAM), such as a dynamic RAM (DRAM) or a static RAM (SRAM). In some embodiments, the memory 206 may include a long-term or large-capacity storage for data or instructions. For example, the memory 206 may include a disk drive (HDD or SSD), flash memory, ROM, EPROM, or other types of non-volatile memory. The I / O interface 208 may include one or more interfaces for communicating with an I / O device, which is capable of communicating with a person (e.g., a user). The communication interface 210 may provide a network interface for communicating with other systems or networks. For example, the communication interface 210 may include a network interface controller (NIC) and / or a wireless NIC for communicating with another computer system on a network. The communication interface 210 may also include a Bluetooth interface or other types of packet-based communications. The bus 212 may provide a communication link between the above components of the computing system.

[0075] Although the present invention has been described in conjunction with a number of specific embodiments, it will be apparent to those skilled in the art that many further substitutions, modifications and variations will be apparent from the foregoing description. Therefore, the invention described herein is intended to include all such substitutions, modifications, applications and variations that may fall within the spirit and scope of the appended claims.

Claims

1. A method for examining a bond between two materials, the method using an optical coherence tomography (OCT) system to generate a sample beam of radiation, the two materials being glass and being laser bonded together at a bond point sandwiched between the two materials, wherein: The laser bonding is transparent to the sample beam, wherein an air gap exists between the two materials around or adjacent to the bonding point, the method comprising: applying the sample beam through a first material of the two materials and into a second material of the two materials to reach the junction and surrounding or adjacent air gap sandwiched between the two materials and acquiring scan data of the junction and surrounding or adjacent air gap sandwiched between the two materials; Based on the scan data, a combination of the two materials is selectively designated as defective.

2. The method according to claim 1, further comprising: defining metrological properties of the combination of the two materials based on the scan data, the metrological properties comprising at least one of a thickness, a refractive index, and a birefringence of at least one of the two materials and any other physical layer between the two materials; Therein, the combination of the two materials is designated as defective also based on the defined metrological property.

3. The method according to claim 1 or 2, further comprising: defining a measurement of a width span of the bond point at a joint between the two materials based on the scan data; Wherein, the combination of the two materials is designated as defective based at least in part on the measurement of the width span.

4. The method according to claim 1, wherein: The bonding point is a portion of a bonding area extending into the two materials, the method further comprising: Based on the scan data, an axial offset of the bond region relative to the joint between the two materials is defined, and the bond of the two materials is designated as defective based at least in part on the defined axial offset.

5. The method according to claim 4, wherein: The axial offset is determined based on a predetermined correlation between the axial offset and a width span of the joining point of the joint between the two materials.

6. The method according to claim 1, further comprising: determining a gap measurement of a gap at a joint between the two materials; Wherein, the combination of the two materials is designated as defective based at least in part on the gap measurement.

7. The method according to claim 6, wherein: Acquiring the scan data of the bond point as part of scanning the sample beam across a junction region between the two materials including the bond point, the method further comprising: defining an image of the bond between the two materials based on scanning of the sample beam across the bond region, a relative gap size of the bond between the two materials corresponding to a relative intensity in the defined image; comparing the relative strengths of a first region of the bond proximate the bond point to a second region of the bond distal from the bond point; and The combination of the two materials is designated as defective in response to the intensity of the second region being greater than the intensity of the first region by a predetermined percentage.

8. The method according to claim 1, wherein: The sample beam is also applied through the two materials, and the sample beam is laterally scanned across the two materials, the method further comprising: defining a two-dimensional cross-sectional image of the two materials based on a lateral scan through the two materials, the cross-sectional image providing a plurality of imaging lines including a real boundary line of the two materials and a virtual boundary line of the two materials, the virtual boundary line being generated by a complex conjugate image component and offset from the real boundary line; The imaging line closest to an axial position having a predetermined offset from an outer boundary of the selected one of the two materials, the predetermined offset being the thickness of the selected one of the two materials, is identified as a junction between the two materials.

9. The method according to claim 1, wherein: The junction is a portion of a junction region extending into the two materials, the junction region having light dispersion properties different from either of the two materials; selecting a wavelength of the sample light beam based on light dispersion characteristics of the boundary region to distinguish the boundary region from the two materials; and The sample beam penetrates the binding region and provides axial information of the binding region; The method also includes defining a three-dimensional image of the bonded area within the two materials.

10. The method according to claim 1, wherein: The two materials are bonded by one of laser welding, heat fusion, gluing and adhesive film.

11. The method according to claim 1, wherein: The OCT system is one of a spectral domain point scanning system, a scanning source point scanning system, a spectral domain line scanning system, a scanning source line scanning system, a full-field spectral domain and a full-field scanning source system.

12. The method according to claim 1, wherein: When the OCT system applies the sample beam, the OCT system and the two bonded materials are continuously displaced relative to each other along a first lateral dimension.

13. The method according to claim 12, wherein: The OCT system scans the sample beam in a first direction across the first lateral dimension and in a second direction opposite to a relative continuous displacement between the OCT system and the two bonded materials so as to counteract the relative continuous displacement.

14. The method according to claim 1, wherein: The OCT system includes at least one of a galvanometer scanner, a MEMS scanner, an electro-optical deflector, and a rotating polygon scanner.

15. The method according to claim 1, wherein: The scan data is obtained by using speckle reduction wobble scanning.

16. The method of claim 1, wherein: The scan data includes repeated scans of the binding point; and The method also includes generating a plurality of images from repeated scans of the binding site and averaging the plurality of images.

17. The method of claim 1, further comprising defining a front face image, designating the combination of the two materials as defective based at least in part on the front face image.

18. The method according to claim 12, wherein: The two joining materials are transparent glasses and the joining point is defined by transparent laser glass welding.

19. The method according to claim 12, wherein: The two combined materials are part of an electronic image display.

20. The method according to claim 1, wherein: The OCT system lacks any scanning components and is one of a full-field spectral domain OCT system and a full-field swept source OCT system.

21. The method according to claim 1, wherein: The OCT system is optimized for specular reflection at any dielectric interface.

22. The method of claim 1, wherein: The two materials are joined together by a welding process; The OCT system is a PS-OCT system; The PS-OCT system measures the birefringence properties of the two materials and the joint before, during and after the welding process; and The combination of the two materials is further designated as defective based on the measured birefringence characteristics.

23. The method according to claim 1, wherein: The OCT system has a light source, and a known delay is introduced into at least two light beams from the light source of the OCT system, the at least two light beams combining to form an OCT light beam.

24. The method of claim 1, further comprising: defining metrological properties of the combination of the two materials using the OCT system and at least one other inspection method, the other inspection method including visual inspection, reflectometry, deflectometry, ellipsometer, and spectroscopic ellipsometer, the metrological properties including at least one of thickness, refractive index, and birefringence of a selected at least one of the two materials and any other physical layer between the two materials; wherein the combination of the two materials is designated as defective based at least in part on the defined metrological characteristic.

25. The method of claim 1, wherein: The OCT system is self-referencing and lacks a separate reference arm.

26. A method for inspecting the bonding of two materials, the two materials being bonded together at a bonding point sandwiched between the two materials, the method comprising: Using an optical coherence tomography (OCT) system, applying a sample beam through a first material of the two materials to reach the junction sandwiched between the two materials, and acquiring scanning data of the junction sandwiched between the two materials; selectively designating a combination of the two materials as defective based on the scan data; Wherein, the bonding point is a portion of a bonding area extending into the two materials, and the method further comprises: based on the scanning data, defining an axial offset of the bonding area relative to the joint between the two materials, and designating the bonding of the two materials as defective at least in part based on the defined axial offset.

27. A method for inspecting the bonding of two materials, the two materials being bonded together at a bonding point sandwiched between the two materials, the method comprising: Using an optical coherence tomography (OCT) system, applying a sample beam through a first material of the two materials to reach the junction sandwiched between the two materials, and acquiring scanning data of the junction sandwiched between the two materials; selectively designating a combination of the two materials as defective based on the scan data; Wherein, the sample beam is also applied to pass through the two materials, and the sample beam is laterally scanned through the two materials, and the method further comprises: defining a two-dimensional cross-sectional image of the two materials based on a lateral scan through the two materials, the cross-sectional image providing a plurality of imaging lines including a real boundary line of the two materials and a virtual boundary line of the two materials, the virtual boundary line being generated by a complex conjugate image component and offset from the real boundary line; An imaging line closest to an axial location having a predetermined offset from an outer boundary of the selected one of the two materials, the predetermined offset being a thickness of the selected one of the two materials, is identified as a junction between the two materials.