Semiconductor structure and method for forming the same
By forming a protective layer on the cobalt layer in the semiconductor device, the problem of corrosion of the cobalt material during the deposition of the tungsten layer is solved, and the electrical performance and interconnect structure quality of the semiconductor device are improved.
Patent Information
- Application Number
- CN201910698154.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-07-31
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2039-07-31
AI Technical Summary
In semiconductor devices, although materials with lower resistance such as cobalt are used to reduce RC delay, the performance improvement is limited because the cobalt material is prone to corrosion when depositing the tungsten layer.
After the cobalt layer is filled in the contact hole, a protective layer is formed to cover the cobalt layer to prevent corrosion of the cobalt layer by WF4 gas and improve the interconnect structure quality and performance of the cobalt layer.
Through the use of the protective layer, corrosion of the cobalt layer is avoided, and the electrical performance of the semiconductor structure and the quality of the interconnection structure are improved.
Smart Images

Figure CN112309956B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a forming method thereof. Background Art
[0002] In semiconductor devices, reducing RC delay (Resistance Capacitance Delay) can improve the performance of semiconductor devices. With the advancement of semiconductor process technology nodes, the integration of devices is getting higher and higher, and the critical dimension (CD) of devices is getting smaller and smaller. Accordingly, further reducing RC delay has become one of the important measures to improve the performance of semiconductor devices.
[0003] As the size of semiconductor devices continues to decrease, the critical dimensions of metal contacts and interconnect structures in the devices are also getting smaller and smaller. At present, in order to reduce RC delay, the materials used for contact plugs are usually materials with lower resistance, such as cobalt or tungsten, so as to improve the performance of semiconductor devices.
[0004] However, even if the contact hole plug is made of a material with a smaller resistance, the performance of the semiconductor device still needs to be improved. Summary of the invention
[0005] The technical problem solved by the present invention is to provide a semiconductor structure and a method for forming the same, so as to optimize the electrical performance of the semiconductor device.
[0006] To solve the above technical problems, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, forming a gate structure on the substrate, the substrate having a source doping region and a drain doping region on both sides of the gate structure; forming a first interlayer dielectric layer on the substrate, the top of the first interlayer dielectric layer is flush with the top of the gate structure; forming a contact hole in the first interlayer dielectric layer, and the contact hole exposes the substrate of the source doping region and the drain doping region; filling the contact hole with a cobalt layer, the top of the cobalt layer is lower than the top of the first interlayer dielectric layer; forming a protective layer on the cobalt layer, the protective layer covers the cobalt layer, and the top of the protective layer is lower than the top of the first interlayer dielectric layer.
[0007] Optionally, the step of forming a protective layer on the cobalt layer includes: depositing a protective layer on the cobalt layer, wherein a top of the protective layer is flush with a top of the first interlayer dielectric layer; and etching back the protective layer so that a top of the protective layer is lower than a top of the first interlayer dielectric layer.
[0008] Optionally, the protective layer is deposited by chemical vapor deposition, physical vapor deposition or atomic layer deposition.
[0009] Optionally, the material of the protective layer is TiN or TaN or Ta or Ti.
[0010] Optionally, the formation method also includes: forming a second interlayer dielectric layer on the protective layer, the top of the second interlayer dielectric layer is flush with the top of the first interlayer dielectric layer; forming a third interlayer dielectric layer on the second interlayer dielectric layer; forming a through hole in the second interlayer dielectric layer and the third interlayer dielectric layer to expose the protective layer; and filling a tungsten layer in the through hole.
[0011] Optionally, the material of the second interlayer dielectric layer is one or more of Si3N4, SiON, SiOC or SiC.
[0012] Optionally, the third interlayer dielectric layer is an oxide layer.
[0013] Optionally, before the cobalt layer is filled in the contact hole, a barrier layer is formed on the sidewall of the contact hole, and the top of the barrier layer is flush with the top of the first interlayer dielectric layer.
[0014] Optionally, after forming the barrier layer, the barrier layer is etched back so that the top of the barrier layer is lower than the top of the first interlayer dielectric layer.
[0015] Optionally, the step of filling the contact hole with a cobalt layer further includes: depositing a cobalt layer in the contact hole, wherein the cobalt layer covers the top of the first interlayer dielectric layer; planarizing the cobalt layer so that the top of the cobalt layer is flush with the top of the first interlayer dielectric layer; and etching the cobalt layer so that the top of the cobalt layer is flush with the top of the barrier layer.
[0016] Optionally, the barrier layer material is TiN or TiC.
[0017] Optionally, the method for depositing the cobalt layer includes an electrochemical plating process, an atomic layer deposition process, a chemical vapor deposition method or a physical vapor deposition method.
[0018] Optionally, the cobalt layer is planarized by a chemical mechanical polishing process, and the parameters of the chemical mechanical polishing process include: a polishing pressure of 1psi to 5psi, a polishing head rotation speed of 20rpm to 100rpm, and a pH value of the polishing liquid of 6 to 9.
[0019] Optionally, the process of etching the cobalt layer is wet etching or dry etching.
[0020] Optionally, the wet etching solution is deionized water with a pH value of 6 to 9.
[0021] Optionally, the etching gas for the dry etching is a halide-containing gas.
[0022] A semiconductor structure formed by the above method includes: a substrate; a gate structure located on the substrate, the substrate having a source doping region and a drain doping region on both sides of the gate structure; a first interlayer dielectric layer located on the substrate, and the top of the first interlayer dielectric layer is flush with the top of the gate structure; a cobalt layer located in the first interlayer dielectric layer, and the top of the cobalt layer is lower than the top of the first interlayer dielectric layer, and the cobalt layer is connected to the substrate; a protective layer covering the cobalt layer, and the top of the protective layer is lower than the top of the first interlayer dielectric layer.
[0023] Compared with the prior art, the technical solution of the embodiment of the present invention has the following beneficial effects:
[0024] The present invention forms a protective layer on the cobalt layer, and the protective layer is used to protect the cobalt layer, so as to prevent the WF4 gas used when depositing a tungsten layer on the cobalt layer from corroding the cobalt layer, thereby improving the corrosion problem of the cobalt layer, improving the quality and performance of the interconnection structure formed by the cobalt layer, and thus improving the electrical performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figures 1 to 11 is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention;
[0026] Fig.12 It is a schematic structural diagram of an embodiment of a semiconductor structure of the present invention. DETAILED DESCRIPTION
[0027] As can be seen from the background technology, even if the contact hole plug is made of a material with a lower resistance, the performance of the semiconductor device still needs to be improved. The reasons why the performance still needs to be improved are:
[0028] Since cobalt material has a small resistance and good gap filling performance, cobalt is currently the commonly used material for contact hole plugs in the field of semiconductor manufacturing, which is beneficial for reducing RC delay.
[0029] However, when cobalt is used as an interconnect material, the problem of cobalt corrosion may occur. For example, when a layer of tungsten material is deposited on the cobalt material as a connection between metal layers, the WF4 gas used when depositing the tungsten layer can easily corrode the cobalt material.
[0030] In order to solve the above technical problems, the inventors have provided a method for forming a semiconductor structure after research. After the cobalt layer is filled in the contact hole, a protective layer is formed on the cobalt layer. The protective layer covers the cobalt layer, which can prevent the WF4 gas from corroding the cobalt layer when a tungsten layer is subsequently deposited on the cobalt layer.
[0031] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0032] Figures 1 to 11 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention.
[0033] refer to Figure 1 , providing a substrate (not shown), forming a gate structure 100 on the substrate, and having source doping regions and drain doping regions (not shown) in the substrate on both sides of the gate structure.
[0034] In this embodiment, the substrate is a silicon substrate; in other embodiments, the material of the substrate may also be germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium.
[0035] In this embodiment, the gate structure 100 is a metal gate. Specifically, the gate structure 100 includes a work function layer 110 and a metal layer 120 located on the work function layer 110 .
[0036] In this embodiment, a gate protection layer 130 is disposed on the top of the gate structure 100 .
[0037] It should be noted that the step of providing a substrate also includes: forming a sidewall 200 on the sidewall of the gate structure 100; after forming the sidewall 200, forming a source-drain doped region (not shown) in the substrate on both sides of the gate structure 100, and the source-drain doped region is used as a source region or a drain region of the semiconductor device.
[0038] It should also be noted that the substrate surface and the side walls of the sidewalls 200 also form an etch stop layer 210. In the subsequent etching process for forming contact holes, the top of the etch stop layer 210 is used to define the stop position of the etching process, thereby avoiding the problem of insufficient etching or over-etching.
[0039] Continue to refer Figure 1 , a first interlayer dielectric layer 300 is formed on the substrate, and the top of the first interlayer dielectric layer 300 is flush with the top of the gate structure 100 .
[0040] The material of the first interlayer dielectric layer 300 is an insulating dielectric material. In this embodiment, the material of the first interlayer dielectric layer 300 is fluorine-containing silicon oxide. In other embodiments, the material of the first interlayer dielectric layer 300 may also be silicide-containing silicon oxide or phosphorus-containing silicon oxide.
[0041] Continue to refer Figure 1 , a contact hole 310 is formed in the first interlayer dielectric layer 300, and the contact hole 310 exposes the substrate of the source doping region and the drain doping region.
[0042] In this embodiment, a dry etching process is adopted to etch the first interlayer dielectric layer 300 and the etching stop layer 210 to form the contact hole 310 .
[0043] refer to Figure 2 , a cobalt layer 400 is filled in the contact hole 310 , and the top of the cobalt layer 400 is lower than the top of the first interlayer dielectric layer 300 .
[0044] In this embodiment, the step of filling the cobalt layer 400 in the contact hole 310 includes: depositing a cobalt layer in the contact hole 310, wherein the cobalt layer 400 covers the top of the first interlayer dielectric layer 300 (not shown); performing a planarization process on the cobalt layer 400, removing the cobalt layer 400 above the top of the first interlayer dielectric layer 300, so that the top of the cobalt layer 400 is flush with the top of the first interlayer dielectric layer 300 (refer to Figure 3 ); etching the cobalt layer 400 so that the top of the cobalt layer 400 is lower than the top of the first interlayer dielectric layer 300.
[0045] In this embodiment, the method for depositing the cobalt layer 400 in the contact hole 310 is chemical vapor deposition; in other embodiments, the cobalt layer may also be deposited by electrochemical plating process, atomic layer deposition process or physical vapor deposition process.
[0046] In this embodiment, a chemical mechanical polishing process is used to planarize the cobalt layer 400. The parameters of the chemical mechanical polishing process include a polishing pressure of 1psi to 5psi, a polishing head speed of 20rpm to 100rpm, a polishing liquid pH value of 6 to 9, and the polishing liquid contains a cobalt corrosion inhibitor.
[0047] In this embodiment, a wet etching process is used to etch the top of the cobalt layer 400, and the wet etching uses deionized water with a pH value of 6 to 9 as an etching solution.
[0048] In other embodiments, a dry etching process may be used to etch the top of the cobalt layer 400 , and the etching gas of the dry etching is a halide-containing gas, including HCl gas or HBr gas.
[0049] In this embodiment, after etching the cobalt layer 400, an alkaline cleaning solution with a pH value of 8 to 11 is used instead of pure water to clean the cobalt layer 400, and the alkaline cleaning solution is NH4OH; in other embodiments, the alkaline cleaning solution can also be a quaternary ammonium base, an amide or other organic weak base. This is because pure water can corrode cobalt, and the use of an alkaline cleaning solution can improve the corrosion problem of the cobalt layer 400 and obtain a cobalt layer with a better morphology.
[0050] It should be noted that, before filling the cobalt layer 400 into the contact hole 310, the forming method further includes: referring to Figure 4 A barrier layer 320 is formed on the side wall of the contact hole 310, and the thickness of the barrier layer 320 on the side wall is to refer to Figure 5 After forming the barrier layer 320, the barrier layer 320 is back-etched to reduce the height of the barrier layer 320 to to The top of the barrier layer 320 is lower than the top of the first interlayer dielectric layer 300 .
[0051] In this embodiment, the barrier layer 320 is used to prevent cobalt from diffusing into the surrounding dielectric layer, thereby preventing the diffusion of cobalt from damaging the performance of the semiconductor device; the barrier layer 320 is made of TiN or TaN or Ta or Ti.
[0052] In this embodiment, the barrier layer 320 is formed by chemical vapor deposition; in other embodiments, the barrier layer 320 may be formed by physical vapor deposition or atomic layer deposition.
[0053] In this embodiment, the barrier layer 320 is etched by a wet etching process; in other embodiments, the barrier layer 320 may also be etched by a dry etching process.
[0054] The reason for etching the barrier layer before filling the cobalt layer 400 is that: on the one hand, etching reduces the height of the barrier layer 320, so that there is no barrier layer on the side wall of the contact hole 310 near the opening, which provides a larger space for the subsequent deposition of the cobalt layer 400, facilitates the formation of the cobalt layer 400, and is beneficial to reducing the process difficulty of depositing the cobalt layer 400, and can obtain a cobalt layer with better morphology; on the other hand, etching the barrier layer 320 in advance avoids damage to the cobalt layer caused by etching the barrier layer 320 after depositing the cobalt layer 400, thereby affecting the performance of the semiconductor.
[0055] It should be noted that, since the barrier layer 320 is used to prevent the diffusion of the cobalt layer 400 , when the cobalt layer 400 is wet-etched, the top of the cobalt layer 400 is made flush with the top of the barrier layer.
[0056] refer to Figure 6 , a protection layer 410 is formed on the cobalt layer 400 , wherein the protection layer 410 covers the cobalt layer 400 , and a top of the protection layer 410 is lower than a top of the first interlayer dielectric layer 300 .
[0057] The protective layer 410 is used to protect the cobalt layer 400. Because tungsten materials are often used as connections between metal layers in semiconductor interconnect structures, when a tungsten layer is deposited on a cobalt layer, the WF4 gas used to form tungsten will cause corrosion of the cobalt material. Therefore, the protective layer 400 is used to prevent the cobalt layer 400 from being damaged when tungsten is subsequently deposited.
[0058] In this embodiment, the material of the protective layer 410 is TiN; in other embodiments, the material of the protective layer 410 may also be TaN or Ta or Ti.
[0059] It should be noted that the steps of forming the protective layer 410 include: Figure 7 , depositing a protective layer 410 on the cobalt layer 400, wherein the top of the protective layer 410 is flush with the top of the first interlayer dielectric layer 300; Figure 6 , back-etch the protective layer 410, so that the thickness of the protective layer remains at to The top of the protection layer 410 is lower than the top of the first interlayer dielectric layer 300 .
[0060] The top of the protection layer 410 is lower than the top of the first interlayer dielectric layer 300 in order to subsequently deposit a dielectric layer in the contact hole 310 to prevent the cobalt layer 400 from short-circuiting in subsequent processes.
[0061] In this embodiment, the method for depositing the protective layer 410 is chemical vapor deposition; in other embodiments, the method for depositing the protective layer 410 may also be physical vapor deposition or atomic layer deposition.
[0062] In this embodiment, a wet etch-back process is used to etch back the protection layer 410 ; in other embodiments, a dry etch-back process may also be used to etch back the protection layer 410 .
[0063] refer to Figure 8 The forming method further includes: forming a second interlayer dielectric layer 500 on the protective layer 410 .
[0064] The material of the second interlayer dielectric layer 500 is one or more of Si3N4, SiON, SiOC or SiC. In this embodiment, the second interlayer dielectric layer 500 is SiON.
[0065] In this embodiment, the second interlayer dielectric layer 500 is formed by chemical vapor deposition. In other embodiments, the second interlayer dielectric layer 500 may be formed by atomic layer deposition.
[0066] Continue to refer Figure 8, the second interlayer dielectric layer 500 is planarized so that the top of the second interlayer dielectric layer 500 is flush with the top of the first interlayer dielectric layer 300 .
[0067] In this embodiment, chemical mechanical polishing is used to planarize the second interlayer dielectric layer 500. The process parameters of the chemical mechanical polishing include a polishing pressure of 1psi to 5psi, a polishing head speed of 20rpm to 100rpm, a polishing liquid polishing particle size of 20nm to 150nm, and the polishing particles are silicon dioxide or cerium dioxide.
[0068] refer to Fig. 9 , a third interlayer dielectric layer 600 is formed on the second interlayer dielectric layer 500 , and the third interlayer dielectric layer 600 covers the first interlayer dielectric layer 300 and the top of the gate structure 100 .
[0069] In this embodiment, the third interlayer dielectric layer 600 is an oxide layer.
[0070] In this embodiment, the third interlayer dielectric layer 600 is formed by chemical vapor deposition.
[0071] refer to Fig.10 , a through hole 510 exposing the protection layer 410 is formed in the second interlayer dielectric layer 500 and the third interlayer dielectric layer 600 .
[0072] In this embodiment, a dry etching process is adopted to etch the second interlayer dielectric layer 500 and the third interlayer dielectric layer 600 to form the through hole 510 .
[0073] The third interlayer dielectric layer 600 and the second interlayer dielectric layer 500 are made of different materials so that when etching to form the through hole 510, the third interlayer dielectric layer 600 can also serve as an etching stop layer, thereby avoiding the problem of insufficient etching or over-etching.
[0074] refer to Fig.11 A tungsten layer 700 is filled in the through hole 510. The tungsten layer 700 is connected to the cobalt layer 400, and then connected to the source doping region and the drain doping region in the substrate through the cobalt layer 400.
[0075] In this embodiment, the method for filling the tungsten layer 700 is chemical vapor deposition; in other embodiments, the method for filling the tungsten layer 700 may also be one or more of chemical vapor deposition, physical vapor deposition or atomic layer deposition.
[0076] In other embodiments, the tungsten layer 700 may be filled in a multi-layer step-by-step manner.
[0077] It should be noted that, in the semiconductor interconnect structure, the tungsten layer 700 needs to be connected to the gate structure 100 in addition to being connected to the source doped region and the drain doped region in the substrate. Therefore, a through hole (not shown) exposing the gate structure 100 may be formed in the third interlayer dielectric layer 600, and a cobalt layer may be filled into the through hole to form an interconnect structure.
[0078] refer to Fig.12 , shows a schematic diagram of the structure of an embodiment of a semiconductor structure of the present invention. Accordingly, the present invention also provides a semiconductor structure. The semiconductor structure includes:
[0079] A substrate (not shown); a gate structure 100, located on the substrate, and the substrate on both sides of the gate structure 100 has a source doping region and a drain doping region (not shown); a first interlayer dielectric layer 300, located on the substrate, and the top of the first interlayer dielectric layer 300 is flush with the top of the gate structure 100; a cobalt layer 400, located in the first interlayer dielectric layer 300, and the top of the cobalt layer is lower than the top of the first interlayer dielectric layer 300, and the cobalt layer 400 is connected to the substrate; a protective layer 410, covering the cobalt layer 400, and the top of the protective layer 410 is lower than the top of the first interlayer dielectric layer 300.
[0080] In this embodiment, the gate structure 100 is a metal gate. Specifically, the gate structure 100 includes a work function layer 110 and a metal layer 120 located on the work function layer 110 .
[0081] In this embodiment, a gate protection layer 130 is disposed on the top of the gate structure 100 .
[0082] In this embodiment, the material of the protective layer 410 is TiN; in other embodiments, the material of the protective layer 410 may also be TaN or Ta or Ti.
[0083] It should be noted that the semiconductor structure further includes: a sidewall spacer 200 located on the sidewall of the gate structure 100 ; and an etch stop layer 210 located on a portion of the substrate surface and the sidewall of the sidewall spacer 200 .
[0084] It should also be noted that the semiconductor structure also includes: a contact hole 310, located in the first interlayer dielectric layer 300, exposing the substrate of the source doping area and the drain doping area, and the contact hole 310 is filled with the cobalt layer 400; a blocking layer 320, located between the side wall of the contact hole 310 and the cobalt layer 400, preventing the cobalt layer 400 from diffusing into the dielectric layer.
[0085] In this embodiment, the material of the barrier layer 320 is TiN; in other embodiments, the material of the barrier layer 320 may also be TiC.
[0086] It should also be noted that the semiconductor structure further includes: a second interlayer dielectric layer 500 , which is located on the protection layer 410 , and the top of the second interlayer dielectric layer 500 is flush with the top of the first interlayer dielectric layer 300 .
[0087] The semiconductor structure of the present invention can prevent the WF4 gas used in the subsequent deposition of the tungsten layer from corroding the cobalt layer by covering the protective layer 410 on the cobalt layer 400, thereby obtaining the cobalt layer 400 with better morphology, thereby improving the performance of the semiconductor device.
[0088] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, forming a gate structure on the substrate, wherein the substrate on both sides of the gate structure has a source doping region and a drain doping region; forming a first interlayer dielectric layer on the substrate, wherein a top of the first interlayer dielectric layer is flush with a top of the gate structure; forming a contact hole in the first interlayer dielectric layer, wherein the contact hole exposes the substrate of the source doping region and the drain doping region; Filling a cobalt layer in the contact hole, wherein the top of the cobalt layer is lower than the top of the first interlayer dielectric layer; forming a protective layer on the cobalt layer, wherein the protective layer covers the cobalt layer, and the top of the protective layer is lower than the top of the first interlayer dielectric layer; forming a second interlayer dielectric layer on the protective layer, wherein the top of the second interlayer dielectric layer is flush with the top of the first interlayer dielectric layer; forming a third interlayer dielectric layer on the second interlayer dielectric layer; forming through holes in the second interlayer dielectric layer and the third interlayer dielectric layer to expose the protective layer; A tungsten layer is filled in the through hole.
2. The method for forming a semiconductor structure according to claim 1, wherein: The step of forming a protective layer on the cobalt layer comprises: Depositing a protective layer on the cobalt layer, wherein a top of the protective layer is flush with a top of the first interlayer dielectric layer; The protection layer is etched back to make the top of the protection layer lower than the top of the first interlayer dielectric layer.
3. The method for forming a semiconductor structure according to claim 2, wherein: The protective layer is deposited by chemical vapor deposition, physical vapor deposition or atomic layer deposition.
4. The method for forming a semiconductor structure according to claim 1 or 2, wherein: The material of the protection layer is TiN or TaN or Ta or Ti.
5. The method for forming a semiconductor structure according to claim 1, wherein: The material of the second interlayer dielectric layer is one or more of Si3N4, SiON, SiOC or SiC.
6. The method for forming a semiconductor structure according to claim 1, wherein: The third interlayer dielectric layer is an oxide layer.
7. The method for forming a semiconductor structure according to claim 1, wherein: Before the cobalt layer is filled in the contact hole, a barrier layer is formed on the sidewall of the contact hole, and the top of the barrier layer is flush with the top of the first interlayer dielectric layer.
8. The method for forming a semiconductor structure according to claim 7, wherein: After forming the barrier layer, the barrier layer is etched back to make the top of the barrier layer lower than the top of the first interlayer dielectric layer.
9. The method for forming a semiconductor structure according to claim 8, wherein: The step of filling the contact hole with a cobalt layer further includes: Depositing a cobalt layer in the contact hole, wherein the cobalt layer covers the top of the first interlayer dielectric layer; performing a planarization process on the cobalt layer so that the top of the cobalt layer is flush with the top of the first interlayer dielectric layer; The cobalt layer is etched to make the top of the cobalt layer flush with the top of the barrier layer.
10. The method for forming a semiconductor structure according to claim 7, wherein: The barrier layer material is TiN or TiC.
11. The method for forming a semiconductor structure according to claim 9, wherein: The method for depositing the cobalt layer includes an electrochemical plating process, an atomic layer deposition process, a chemical vapor deposition method or a physical vapor deposition method.
12. The method for forming a semiconductor structure according to claim 9, wherein: The cobalt layer is planarized by a chemical mechanical polishing process, wherein the parameters of the chemical mechanical polishing process include: a polishing pressure of 1 psi to 5 psi, a polishing head rotation speed of 20 rpm to 100 rpm, and a pH value of a polishing liquid of 6 to 9.
13. The method for forming a semiconductor structure according to claim 9, wherein: The process of etching the cobalt layer is wet etching or dry etching.
14. The method for forming a semiconductor structure according to claim 13, wherein: The wet etching solution is deionized water with a pH value of 6-9.
15. The method for forming a semiconductor structure according to claim 13, wherein: The etching gas for the dry etching is a halide-containing gas.
16. A semiconductor structure, characterized in that: include: substrate; A gate structure is located on the substrate, and the substrate on both sides of the gate structure has a source doping region and a drain doping region; A first interlayer dielectric layer is located on the substrate, and a top of the first interlayer dielectric layer is flush with a top of the gate structure; a cobalt layer, located in the first interlayer dielectric layer, with a top of the cobalt layer lower than a top of the first interlayer dielectric layer, and the cobalt layer connected to the substrate; A protective layer, covering the cobalt layer, wherein a top of the protective layer is lower than a top of the first interlayer dielectric layer; A second interlayer dielectric layer is located on the protective layer, and a top of the second interlayer dielectric layer is flush with a top of the first interlayer dielectric layer; A third interlayer dielectric layer, located on the second interlayer dielectric layer; a through hole, wherein the through hole is located in the second interlayer dielectric layer and the third interlayer dielectric layer, and the through hole exposes the protective layer; The tungsten layer is located in the through hole.