Method for hardening ink on a printing material
By adopting a three-step hardening process on the printing materials, pre-hardening, further hardening and supplementary hardening, the problems of insufficient ink hardening and low molecular components migration are solved, and high-quality printing results and healthy and safe packaging products are achieved.
Patent Information
- Application Number
- CN202010547669.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-17
- Filing Date
- 2020-06-16
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2040-06-16
AI Technical Summary
In the prior art, UV-hardenable ink hardening results are insufficient, resulting in the possibility of low molecular ink components migrating into packaging products, affecting health and printing quality.
Three-step hardening process is adopted: pre-hardening (nail-fixed), further hardening and supplementary hardening, where further hardening is carried out under an inert gas to improve the viscosity and peel resistance of the ink. Supplementary hardening ensures thorough hardening of the ink and reduces low molecular composition. Migration of ingredients.
The ink is fully hardened, the printing quality is improved, the migration of low-molecular components is reduced, and the ink components that are harmful to health are avoided into the packaging products, while saving inert gas use and equipment costs.
Smart Images

Figure CN112519408B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for curing ink on a printing material.
[0002] The technical field to which the invention belongs is the field of the graphics industry and in particular the field of curing, in particular by means of UV radiation, of liquid inks on sheet- or web-shaped printing materials, preferably made of paper, cardboard, kraft paper, plastic or composite materials. Background Art
[0003] The (preferably liquid or pasty) print medium / fluid (e.g. printing color, varnish or ink) on the print substrate is dried and / or hardened (or more generally treated), which can be done in different ways, also in combination: by acting with hot air, with electromagnetic radiation (e.g. UV or IR) or particle radiation (e.g. electrons), or by contacting the print substrate with a heated surface (e.g. a cylinder, roller or belt). In most cases, water-based print media are dried thermally (preferably with the aid of IR), while polymerizable print media are dried in most cases with the aid of UV. Mercury vapor lamps and increasingly LED emitters are used as UV radiation sources. It is also known that UV-curable inks can be hardened under inert gas.
[0004] The UV-curable ink is hardened, which can be carried out in multiple steps, for example: first a so-called pinning (pre-hardening) can be carried out and then a final hardening can be carried out: WO2019007979A1 discloses such UV hardening and subsequent UV hardening under inert gas. EP3045477A1 discloses similar content. EP2767407B1 also discloses similar content, wherein the initial hardening is the so-called pinning (Pinnen). The corresponding final hardening step is carried out under inert gas according to these documents. EP1473341B1 discloses two UV hardening steps; both steps are carried out under inert gas. EP2596874A1 discloses such drying (non-UV hardening) under inert gas and subsequent UV hardening.
[0005] In the prior art, the following problems may occur: the UV curing result of the ink is not sufficient (UV curable ink is not crosslinked / polymerized enough), and thus low molecular and potentially harmful ink components may migrate into the packaged product (such as food).
[0006] It is possible to (re)formulate the ink with high-molecular and therefore less migratory components, but this would result in a lower viscosity of the ink, which could lead to problems when printing with the ink.
[0007] The use of inert gas can avoid undesired migration, since in the oxygen-poor curing environment, less (potentially migrating) inhibitors can be used in the ink. However, curing under inert gas is very expensive, primarily because the corresponding components require a lot of construction space and require inert gas. Summary of the invention
[0008] The object of the present invention is therefore to provide an improvement over the prior art which, in particular, allows sufficient curing of UV-curable inks so that undesired migration of low-molecular ink components is reduced or avoided.
[0009] This object is achieved according to the invention by a method according to the invention.
[0010] Advantageous and therefore preferred developments of the invention are apparent from the description and the drawing.
[0011] According to the invention, a method for curing ink on a printing material is proposed, wherein at least one UV-curable ink is applied to the printing material in the form of droplets and is exposed to UV radiation by means of at least one first UV radiator and thus pre-cured, characterized in that the ink is exposed to UV radiation by means of at least one second UV radiator of a UV dryer under an inert gas, under an inert gas-enriched air, or under an oxygen-reduced air and thus further cured. ), and the ink is subsequently exposed to UV radiation by means of at least one third UV radiator of a further UV dryer and thereby re-hardened / supplemented hardened
[0012] The present invention advantageously enables UV-curable inks to be sufficiently cured, thereby reducing or avoiding undesired migration of low-molecular ink components.
[0013] According to the invention, this hardening is carried out in three successive steps: pre-hardening (or so-called nailing), further hardening, and supplementary hardening.
[0014] The purpose of the pre-hardening (pinning) is to increase the viscosity of the ink on the printing material and thereby prevent the ink from flowing too strongly on the printing material (in particular the printing point generated by the ink droplets on the printing material). The viscosity is only slightly increased in this case; the ink is not yet completely hardened. In this way, the printing quality can be improved, in particular by preventing different color inks from bleeding into each other (so-called "inter color bleeding").
[0015] The further hardening is used to further increase the viscosity of the ink (compared to the pre-hardening). Then, the ink adheres well to the printing material and has sufficient peeling resistance. The further curing is preferably carried out in such a way that more than 90% of the double bonds in the ink are converted.
[0016] Finally, the post-hardening serves to bind the monomers still present in the ink and thus reduce or avoid any migration.
[0017] 100% complete hardening cannot be achieved by means of three or more hardening steps. However, a sufficiently good hardening result can be achieved by the hardening method according to the invention.
[0018] Here, the second hardening step (also referred to as "further hardening" or alternatively as "intermediate hardening") - and preferably only this step - is carried out under inert gas, under air enriched with inert gas, or under oxygen-reduced air (i.e. not under ambient air as in the other two steps). The supplementary hardening (alternatively referred to as "final hardening") ensures that the ink leaving the printing press is largely and preferably substantially completely hardened.
[0019] That is, preferably only the second hardening step is carried out under an inert gas (alternatively referred to as protective gas), under an air enriched with an inert gas, or under an air reduced in oxygen, whereas all other hardening steps are preferably carried out under untreated air (e.g. ambient air). Here, "under an inert gas" means that preferably a substantially pure inert gas, such as nitrogen or helium, is used. Here, "under an air enriched with an inert gas" means that the proportion of inert gas (e.g. nitrogen or helium) in the air used or other gas mixture used is preferably significantly increased compared to ambient air. Here, "under an air reduced in oxygen" means that the proportion of oxygen in the air used or other gas mixture used is preferably significantly reduced compared to ambient air. In this case, this increase or decrease is "significant" if these measures preferably achieve: i) avoiding the suppression of free radicals (Radikales) generated by UV photons and photoinhibitors, which is problematic in terms of migration, and / or ii) avoiding insufficient and thus problematic crosslinking in terms of migration, or achieving sufficient crosslinking, and / or iii) being able to reduce the amount of photoinhibitors in the ink (which may migrate and thus be harmful to health) to a level that does not cause problems in terms of migration.
[0020] The device according to the invention for hardening under inert gas or the like (for example an inert gas housing with inert gas supply and conduction) can advantageously be limited to the second hardening step (or its location or workstation). In this way, construction space, components and the costs associated therewith can be saved. Furthermore, the amount of inert gas required can be reduced.
[0021] In this way, sufficient curing can advantageously be achieved (for industrially produced high-quality or even very high-quality printed products), in particular when the printed products are industrially post-processed (for example for the production of packaging).
[0022] In this way, it is also advantageously possible during the production of the packaging to substantially reduce or avoid the undesirable (because potentially harmful to health) migration of low-molecular components of the ink into the packaging and into the packaged product (for example food).
[0023] A preferred development of the invention can be characterized in that the ink is exposed to UV radiation by means of the first UV radiator under air. In this case, no inert gas system is required. Construction space and costs can be saved.
[0024] A preferred improvement of the invention can be characterized in that the ink is exposed to UV radiation under air by means of the third UV radiator. In this case, no inert gas equipment is required. Construction space and costs can be saved.
[0025] A preferred development of the invention can be characterized in that nitrogen (alternatively helium) is used as inert gas or protective gas.
[0026] A preferred development of the invention can be characterized in that the UV dryer comprises a plurality of (for example two, three or four) second UV radiators.
[0027] A preferred development of the invention can be characterized in that the second UV radiators are arranged in a common inert gas housing. The housing can be formed from sheet metal, wherein the shape is preferably adapted (eg curved) according to the transport path.
[0028] A preferred development of the invention can be characterized in that the further UV dryer comprises a plurality (for example two, three or four) of third UV radiators.
[0029] A preferred improvement of the present invention may be characterized in that the other UV dryer comprises at least two workstations spaced apart from each other, which have a plurality of third (or fourth) UV radiators. In the intermediate spaces along the intervals between the workstations, the printing material may be guided (e.g., in a serpentine manner) by means of a plurality of deflection rollers.
[0030] A preferred development of the invention can be characterized in that at least one second UV radiator and / or at least one third UV radiator and / or at least one fourth UV radiator hardens the ink through the printing material. This development is particularly advantageous in the case of (UV) permeable printing materials. In this case, the ink is preferably applied to the front side of the printing material, while the at least one radiator is arranged in the space on the back side of the printing material, or vice versa.
[0031] A preferred development of the invention can be characterized in that the printing material is moved along at least one second UV radiator by means of a (preferably heated) temperature control roller which assists in the curing.
[0032] Any combination of the features of the present invention, the improved solutions of the present invention and the embodiments of the present invention also constitutes an advantageous improved solution of the present invention. The improved solution of the present invention may also have a single feature or a combination of features disclosed in the above "technical field", "background technology" and "invention content" sections. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] The present invention and its preferred improvements are further described below based on preferred embodiments with reference to the accompanying drawings. In the accompanying drawings, corresponding features are indicated by the same reference numerals.
[0034] The accompanying drawings show:
[0035] Figure 1 : A schematic diagram of a printing press for carrying out the method; and
[0036] Figure 2 : Side view of ink printing press. DETAILED DESCRIPTION
[0037] Figure 1 A schematic view of an ink printing machine 1 (machine for short) is shown when carrying out a preferred embodiment of the method according to the invention. The machine processes a web-shaped printing material 2, preferably paper, cardboard or a plastic film. The printing material 2 is fed at A, for example, by a roller feeder and then printed with ink.
[0038] The printing takes place in the first station 3 of the machine, more precisely in the ink printing unit 3, which comprises a plurality of (preferably eight) print head arrangements 4, each of which has a plurality of ink printing heads for producing ink drops (preferably in accordance with the printed image to be printed). Preferably, a first UV radiator 5 is arranged directly behind each print head arrangement 4. These radiators 5 serve for pre-hardening of the ink, i.e. only partial polymerization (so-called fixing). This application by means of UV radiation preferably takes place in air (e.g. ambient air whose composition is unchanged) and not under an inert gas different from air. This fixing preferably takes place by means of UV radiation with a wavelength of 385 nm or (for white ink) 395 nm. The printing material 2 leaves the first station 3 at B and is further guided to C, where it is supplied to the second station 10.
[0039] The second station 10 is a UV dryer 10 having at least one (but preferably a plurality) second UV radiators 11 (for example two UV radiators 11a and 11b). These radiators are used for further curing of the ink, preferably for a large (but still not complete) curing (or polymerization) of the ink. In this case, this further curing of the ink is not carried out under (ambient) air, but under an inert gas, under an air enriched with an inert gas, under an oxygen-reduced air or under a functionally similar substance. Preferably, nitrogen is used as the inert gas; alternatively, helium or other noble gases can be used.
[0040] The UV radiators 11 can be designed, for example, as UV lamps (preferably mercury vapor lamps or alternatively UV LED radiators) and each have a power of between 200 W / cm and 300 W / cm (assuming a web transport speed of approximately 50 m / min).
[0041] For irradiation under inert gas, an inert gas housing 12 is provided, in which the second UV radiator 11 is preferably also located. The inert gas housing 12 can be formed from a (metal) sheet material. The inert gas housing 12 has an inert gas supply line 13 and an inert gas removal line 14.
[0042] It can be provided that the printing material 2 is guided along the second UV radiator 11 by means of a temperature-controlled roller 7 (or its temperature-controlled surface 8 or another temperature-controlled surface 8). Such temperature control (in particular heating) can assist the curing process. The temperature of the surface 8 can preferably be between 40° C. and 50° C. and can preferably be adjusted depending on the speed.
[0043] Next, the printing material web 2 can be guided through an optional flexographic printing unit 15, in which a UV-curable varnish can preferably be applied. At D, the web 2 leaves the second station 10 and is supplied to a third station 20 (i.e., another UV dryer 20) at E and optionally to a fourth station 30 (i.e., yet another UV dryer 30) at F'. The third station and the fourth station can be arranged spaced apart from each other, and the web 2 can have a meandering web course, in particular, between E' and F'.
[0044] The third station 20 comprises at least one (but preferably a plurality) third UV radiators 21 (for example two UV radiators 21a and 21b), which are used for the additional curing of the ink, preferably for the substantially complete curing (or polymerization) of the already pre-cured and further cured (and thus preferably largely cured) ink.
[0045] The optional fourth station 30 comprises at least one (but preferably a plurality) further third UV radiators 31 (for example two UV radiators 31a and 31b). These radiators are also used for supplementary hardening. The third radiator 21 and the further third radiator 31 can be collectively referred to as "third radiators".
[0046] The third UV radiator 21 and the optional further third UV radiator 31 can preferably be designed as mercury vapor lamps or alternatively as UV LED radiators and each have a power of 100 W / cm to 200 W / cm (assuming a web transport speed of approximately 50 m / min).
[0047] The post-hardening in the third station and the optional fourth station is preferably carried out under air (for example, ambient air whose composition is unchanged) and not under an inert gas different from air.
[0048] The additional curing of the ink in the third station and / or the fourth station (ie, irradiation with UV radiation) can be carried out from the printed side 40 of the printing material (see Figure 2 ) or can be carried out through the printing material 2 (starting from the unprinted back side of the printing material). Combinations (starting from the printed side and the unprinted side of the printing material) are also possible: for example, in the third station 20, the irradiation starts from the printed side, and in the fourth station 30, the irradiation starts from the unprinted side. Furthermore, in the second station 10, the irradiation can also be carried out starting from the unprinted side (through the printing material 2) and thus differ from what is shown in the figures.
[0049] Thus, the method according to the invention, which is carried out by way of example with the machine 1 shown, comprises: i) UV pre-hardening under air; subsequently ii) further UV hardening under inert gas, under air enriched with inert gas, under air reduced in oxygen or under functionally similar substances; and finally iii) UV post-hardening under air. Other preceding, intermediate or subsequent UV hardening steps or temperature control steps are also possible.
[0050] Figure 2 (also schematically) Figure 1 A side view of the machine 1 during the execution of a preferred embodiment of the method according to the invention.
[0051] contrast Figure 1 It can be seen that the web path 41 of the printing material 2 preferably runs in a meandering manner and can include a plurality of deflecting rollers 6 .
[0052] As shown, the inert gas housing 12 can be arranged in the region of the web guidance by means of the temperature control roller 7. The inert gas housing 12 can include (inlet and outlet) shields 9, which ensure that the inert gas supplied to the housing 12 in the inert gas supply line 13 is substantially discharged again in the inert gas discharge line 14 without leaking out uncontrolled at other locations.
[0053] from Figure 2 It can also be seen that the radiators 21a and 21b of the third station 20 apply UV radiation starting from the printed side of the printing material, and the radiators 31a and 31b of the fourth station 30 apply UV radiation starting from the unprinted side of the printing material 2 (that is, through the printing material 2). This is a preferred (but only exemplary) configuration.
[0054] The web running (or web transport) between these stations 3 , 10 and 20 , ie between B and C and between D and E, can be carried out by means of deflecting rollers 6 , and likewise between E′ and F′, ie between stations 20 and 30 .
[0055] Reference numerals list
[0056] 1 Ink printing machine
[0057] 2 Printing material / ribbon
[0058] 3 Ink printing agency / first stop
[0059] 4 Print head arrangement / ink printing head
[0060] 5. First UV radiator (for pre-curing)
[0061] 6 Deflection roller
[0062] 7 Temperature control roller
[0063] 8 Temperature-controlled surfaces
[0064] 9 Shielding
[0065] 10 UV dryer / second station
[0066] 11,11a,11b Second UV irradiator (for further hardening)
[0067] 12 Inert gas housing
[0068] 13 Inert gas supply line
[0069] 14 Inert gas guide pipe
[0070] 15 Flexographic printing press
[0071] 20 Another UV Dryer / Third Station
[0072] 21,21a,21b Third UV radiator (for additional hardening)
[0073] 30 Another UV Dryer / Station 4
[0074] 31,31a,31b Another third UV radiator (for additional hardening)
[0075] 40 Ink application / printed surface of substrate
[0076] 41 Path of the printing material
[0077] A to F The path along which the printing material travels through the machine
Claims
1. A method for hardening ink on a printing material, in, At least one UV-curable ink is applied in droplet form to a printing material (2) and exposed to UV radiation by means of at least one first UV radiator (5) and thereby pre-cured, It is characterized in that The ink is exposed to UV radiation by means of the first UV radiator (5) under ambient air, wherein the ink is exposed to UV radiation by means of at least one second UV radiator (11, 11a, 11b) of a UV dryer (10) not under ambient air but under an inert gas, under an inert gas-enriched air, or under an oxygen-reduced air and thereby further hardened, and The ink is subsequently exposed to UV radiation by means of at least one third UV radiator (21, 21a, 21b, 31, 31a, 31b) of a further UV dryer (20, 30) and thus post-cured, wherein the ink is exposed to UV radiation by means of the third UV radiator (21, 21a, 21b, 31, 31a, 31b) under ambient air.
2. The method according to claim 1, It is characterized in that Nitrogen gas was used as the inert gas.
3. The method according to claim 1, It is characterized in that The UV dryer (10) comprises a plurality of second UV radiators (11, 11a, 11b).
4. The method according to claim 3, It is characterized in that The second UV radiators (11, 11a, 11b) are arranged in a common inert gas housing (12).
5. The method according to any one of claims 1 to 4, It is characterized in that The further UV dryer (20, 30) comprises a plurality of third UV radiators (21, 21a, 21b, 31, 31a, 31b).
6. The method according to claim 5, It is characterized in that The further UV dryer (20, 30) comprises a third station (20) having a plurality of third UV radiators (21, 21a, 21b) and a fourth station (30) having a plurality of further third UV radiators (31, 31a, 31b).
7. The method according to any one of claims 1 to 4, It is characterized in that At least one second UV radiator (11, 11a, 11b) and / or at least one third UV radiator (21, 21a, 21b) and / or at least one further third UV radiator (31, 31a, 31b) hardens the ink through the printing material (2).
8. The method according to any one of claims 1 to 4, It is characterized in that The printing material (2) is moved along the at least one second UV radiator (11, 11a, 11b) by means of a temperature-controlled roller (7).