Measuring method and device for graphite-containing articles and ingot growth system

By designing a coil device for measuring the electromagnetic physical properties of the ingot growth container and the thermal insulation material, the problem of difficult measurement and selection in the existing technology is solved, and the reproducibility and efficiency of the ingot growth are improved.

CN112748155BActive Publication Date: 2024-10-25EIN CRYSTAL CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202011184512.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-08-31
Filing Date
2020-10-29
Publication Date
2024-10-25
Estimated Expiration
2040-10-29

AI Technical Summary

Technical Problem

During the ingot growth process, it is difficult to effectively measure and select ingot growth containers and thermal insulation materials with excellent electromagnetic physical properties using existing technology, resulting in low reproducibility and low efficiency of ingot growth.

Method used

By designing a measuring device including a coil part of a wound wire, the induction heating characteristics are used to measure the electromagnetic physical properties of the ingot growth container and the insulation material, including equivalent series resistance, equivalent series inductance and quality factor, providing a simplified measurement method To select containers and materials with excellent properties.

Benefits of technology

It achieves fast and reliable measurement of the electromagnetic physical properties of the ingot growth container and insulation material, ensures the reproducibility and efficiency of the ingot growth, and provides a basis for selecting containers and materials with more favorable characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112748155B_ABST
    Figure CN112748155B_ABST
Patent Text Reader

Abstract

The present invention relates to a measuring method, a measuring device, and an ingot growth system for measuring physical properties related to induction heating characteristics of a graphite-containing article. The measuring method includes: a configuration step of configuring a graphite-containing article in a coil portion including a wound wire; and a measuring step of applying a measuring power supply to the coil portion through a measuring member electrically connected to the coil portion to measure electromagnetic physical properties induced in the coil portion. The measuring method measures the electromagnetic physical properties of graphite-containing articles such as ingot growth containers and insulation materials and provides data required for selection, thereby ensuring further improvement in the reproducibility of ingot growth.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for measuring a graphite article, an apparatus for measuring a graphite ingot, and an ingot growing system, etc. The present invention relates to an apparatus for measuring an ingot growing container, a method for measuring an ingot growing container using the apparatus, etc. The present invention relates to an apparatus for measuring thermal insulation materials, a method for measuring thermal insulation materials using the apparatus, etc. Background Art

[0002] Induction heating is a method of supplying high-frequency alternating current to a coil to heat an object by utilizing Joule heat generated by eddy currents produced by electromagnetic induction.

[0003] When an ingot is grown by an apparatus having an induction heating member and an insulating material, the weight (density), thermal conductivity, resistance and other properties of the ingot growth container and the insulating material have a great influence on the ingot growth. Therefore, it is necessary to know in advance the electromagnetic properties of the ingot growth container and / or the insulating material heated by induction heating in order to ensure the reproducibility of ingot growth.

[0004] The above-mentioned background technology is technical information possessed by the inventor for the derivation of the contents disclosed in this specification or technical information acquired during the derivation process, and is not necessarily a known technology disclosed to the public before the contents disclosed in the application specification.

[0005] As a related prior art, there is “Evaluation method of quartz glass crucible, and method for producing single crystal silicon” disclosed in Korean Patent Publication No. 10-2014-0104500. Summary of the invention

[0006] Problem that the invention aims to solve

[0007] An object of the present invention is to provide a measurement method, a measurement device, an ingot growth system, etc. for measuring physical properties related to induction heating characteristics of a graphite-containing article.

[0008] Another object of the present invention is to provide an ingot growth container measuring device and an ingot growth container measuring method that can measure and select the electromagnetic properties of an ingot growth container in a simpler method. In addition, another object of the present invention is to ensure improved reproducibility when the electromagnetic properties of an ingot growth container are measured and selected and the selected ingot growth container is applied to ingot growth.

[0009] Another object of the present invention is to provide a thermal insulation material measuring device and a thermal insulation material measuring method that can measure the electromagnetic properties of a thermal insulation material in a simpler method. In addition, another object of the present invention is to measure the electromagnetic properties of a thermal insulation material and ensure improved reproducibility when the electromagnetic properties are applied to ingot growth.

[0010] Means used to solve problems

[0011] In order to achieve the above-mentioned purpose, a measurement method of one embodiment includes the following steps to measure the physical properties of a graphite-containing article related to induction heating characteristics: a configuration step of configuring the graphite-containing article in a coil portion including a wound conductive wire; and a measurement step of applying a measuring power supply to the coil portion through a measuring component electrically connected to the coil portion to measure the electromagnetic physical properties induced in the coil portion.

[0012] The electromagnetic property may include an element related to a change in an induced electromotive force generated in the coil portion based on the graphite-containing article or an element related to an electrical resistance of the graphite-containing article.

[0013] The electromagnetic property may be at least one selected from the group consisting of an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil unit.

[0014] The graphite-containing article may have a generally cylindrical outer shape.

[0015] The graphite-containing article may be an ingot growth container and / or an insulation material.

[0016] The cross section of the ingot growth container is substantially circular or elliptical, and the ingot growth container has an internal space. The cross section of the ingot growth container is substantially circular or elliptical, and the ingot growth container has an internal space, and may be a cylindrical shape with a closed lower end and an open upper end.

[0017] The cross section of the heat insulating material is substantially circular or elliptical, and the upper and lower ends of the heat insulating material may be open. In addition, the cross section of the heat insulating material is substantially circular or elliptical, and the upper and lower ends of the heat insulating material may be closed.

[0018] The coil part may have a receiving space located inside.

[0019] The ingot growth container may be disposed in the accommodation space.

[0020] The heat insulating material may be disposed outside the coil portion.

[0021] The length of the accommodating space may be greater than 100 mm.

[0022] The length of the storage space can be measured in different ways according to the measurement method, and is measured substantially parallel to the bottom surface, and is measured based on the inner diameter of the circular or cylindrical coil portion. In addition, when the length of the storage space varies according to the measured height, the longest length is used as the reference. When the cross-section of the coil portion is circular, the diameter of the storage space is regarded as the length of the storage space.

[0023] The circumference of the inner diameter of the coil part (unit: mm) and the cross-sectional area of ​​the wire of the coil part (unit: mm 2 ) can be in a ratio of 100:1.57 to 100:161.

[0024] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the graphite-containing article; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the graphite-containing article. The coil portion can be a ring-shaped coil type in which the x-direction thickness is greater than or equal to the z-direction thickness.

[0025] A ratio of a circumference (unit: mm) of an inner diameter of the coil portion of the toroidal coil type to a thickness (mm) of the conductive wire may be 100:0.194 to 100:1.09.

[0026] The graphite-containing article is an ingot growth container, and an equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A to the annular coil may be 2.35Ω to 4.56Ω.

[0027] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the graphite-containing article; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the graphite-containing article. The coil portion can be a hollow coil type in which the z-direction thickness is greater than the x-direction thickness.

[0028] A ratio of a circumference (unit: mm) of an inner diameter of the coil portion of the air-core coil type to a thickness (mm) of the conductive wire may be 100:0.194 to 100:1.09.

[0029] The graphite-containing article is an ingot growth container, and an equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A to the air-core coil type coil portion may be 3.50Ω to 7.24Ω.

[0030] The graphite-containing article is a thermal insulation material, and an equivalent series resistance value of the thermal insulation material measured by applying an AC power supply of 100 kHz and 0.1 A to the air-core coil type coil portion may be 10.57Ω to 14.16Ω.

[0031] A measuring device according to another embodiment includes: a coil portion including a wound conductive wire; and a measuring member electrically connected to the coil portion, wherein the measuring member applies a measuring power source to the coil portion to measure electromagnetic properties of a graphite-containing article, wherein the electromagnetic properties are properties related to induction heating characteristics.

[0032] The electromagnetic property may be one or more selected from the group consisting of an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil unit.

[0033] The coil part may have an accommodation space located inside.

[0034] The ingot growth container may be disposed in the accommodation space.

[0035] The heat insulating material may be disposed outside the coil portion.

[0036] The length of the accommodating space may be greater than 100 mm.

[0037] The length of the storage space can be measured in different ways according to the measurement method, and is measured substantially parallel to the bottom surface, and is measured based on the inner diameter of the circular or cylindrical coil portion. In addition, when the length of the storage space varies according to the measured height, the longest length is used as the reference. When the cross-section of the coil portion is circular, the diameter of the storage space is regarded as the length of the storage space.

[0038] The circumference of the inner diameter of the coil part (unit: mm) and the cross-sectional area of ​​the wire of the coil part (unit: mm 2 ) can be in a ratio of 100:1.57 to 100:161.

[0039] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the graphite-containing article; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the graphite-containing article. The coil portion can be a ring-shaped coil type in which the x-direction thickness is greater than or equal to the z-direction thickness.

[0040] A ratio of a circumference (unit: mm) of an inner diameter of the coil portion of the toroidal coil type to a thickness (mm) of the conductive wire may be 100:0.194 to 100:1.09.

[0041] The graphite-containing article is an ingot growth container, and an equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A to the annular coil may be 2.35Ω to 4.56Ω.

[0042] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the graphite-containing article; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the graphite-containing article. The coil portion can be a hollow coil type in which the z-direction thickness is greater than the x-direction thickness.

[0043] A ratio of a circumference (unit: mm) of an inner diameter of the coil portion of the air-core coil type to a thickness (mm) of the conductive wire may be 100:0.194 to 100:1.09.

[0044] The graphite-containing article is an ingot growth container, and an equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A to the air-core coil type coil portion may be 3.50Ω to 7.24Ω.

[0045] The graphite-containing article is a thermal insulation material, and an equivalent series resistance value of the thermal insulation material measured by applying an AC power supply of 100 kHz and 0.1 A to the air-core coil type coil portion may be 10.57Ω to 14.16Ω.

[0046] The ingot growth system of another embodiment is a system including a graphite-containing object and a heating component to grow a silicon carbide ingot, wherein the graphite-containing object is an ingot growth container or an insulating material, and the ingot growth container includes: a main body having an internal space for configuring a raw material; and a silicon carbide seed configured on the upper part of the main body or on the main body, the graphite-containing object has an equivalent series resistance value measured by a measuring device as an electromagnetic indirect characteristic value, the equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A is 3.50Ω to 7.24Ω, and the equivalent series resistance value of the insulating material measured by applying an AC power supply of 100 kHz and 0.1A can be 10.57Ω to 14.16Ω.

[0047] The silicon carbide ingot may be induced to grow at a speed of more than 100 mm / hr.

[0048] To achieve the above object, a crystal ingot growth container measuring device according to one embodiment includes: a coil portion including a wound conductive wire; and a measuring component electrically connected to the coil portion, wherein the measuring component applies a measuring power supply to the coil portion to measure the electromagnetic properties of the crystal ingot growth container.

[0049] The electromagnetic property may include a factor related to a change in an induced electromotive force generated in the coil portion by the ingot growth container or a factor related to a resistance of the ingot growth container.

[0050] The ingot growth container may be disposed within a range within which an induced electromotive force induced by power applied to the coil portion reaches.

[0051] The coil part has a receiving space located inside, and the ingot growth container may be located in the receiving space.

[0052] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the crystal ingot growth container; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the crystal ingot growth container. The coil portion can be a ring coil type whose x-direction thickness is greater than or equal to the z-direction thickness.

[0053] The cross-section of the coil portion has: an x-direction thickness measured in the direction parallel to the bottom surface or the upper surface of the ingot growth container, i.e., the x-direction; and a z-direction thickness measured in the side direction of the ingot growth container, i.e., the z-direction perpendicular to the x-direction. The coil portion may be a hollow coil type in which the z-direction thickness is greater than the x-direction thickness.

[0054] The length of the accommodating space may be greater than 100 mm.

[0055] The ingot growth container may be a graphite crucible for ingot growth.

[0056] The measuring component may be an LCR meter.

[0057] The electromagnetic property may be one or more selected from the group consisting of an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil unit.

[0058] The electromagnetic property and the direct current value flowing in the ingot growth container when the induction heating member heats the ingot growth container or a factor related thereto are determined by a coefficient R 2 It may be 0.9 or more.

[0059] The circumference (mm) of the side of the ingot growth container and the cross-sectional area (mm) of the wire of the coil part 2 ) can be in a ratio of 100:1.57 to 100:161.

[0060] A ratio of a circumference (mm) of a side of the ingot growth container to a thickness (mm) of the wire is 100:0.194 to 100:1.09.

[0061] In order to achieve the above purpose, a method for measuring a crystal ingot growth container in one embodiment may include: a configuration step of configuring a crystal ingot growth container in a coil portion including a wound conductive wire; and a measurement step of applying a measuring power supply to the coil portion via a measuring component electrically connected to the coil portion to measure electromagnetic properties induced in the coil portion.

[0062] To achieve the objective, the ingot growth container of an embodiment includes graphite, and an equivalent series resistance value measured by applying an AC power supply of 100 kHz and 0.1 A to the annular coil type ingot growth container measuring device may be 2.35Ω to 4.56Ω.

[0063] To achieve the objective, the ingot growth container of an embodiment includes graphite, and an equivalent series resistance value measured by applying an AC power supply of 100 kHz and 0.1 A to the hollow coil type ingot growth container measuring device may be 3.50Ω to 7.24Ω.

[0064] To achieve the above object, the thermal insulation material measuring device of the present invention may include: a coil portion including a wound conductive wire; and a measuring member electrically connected to the coil portion, wherein the measuring member applies a measuring power supply to the coil portion to measure the electromagnetic properties of the thermal insulation material.

[0065] The electromagnetic property may include a factor related to a change in an induced electromotive force generated in the coil portion by the thermal insulation material or a factor proportional to the resistance of the thermal insulation material.

[0066] The heat insulating material may be arranged within a range reached by an induced electromotive force induced by power applied to the coil portion.

[0067] The coil part has a receiving space located inside, and the heat insulating material may be formed to surround the outer side of the coil part.

[0068] The cross-section of the coil portion has: an x-direction thickness measured in the x-direction parallel to the bottom surface or the upper surface of the insulating material; and a z-direction thickness measured in the z-direction perpendicular to the x-direction in the side direction of the insulating material. The coil portion can be a hollow coil type in which the z-direction thickness is greater than the x-direction thickness.

[0069] The electromagnetic property may be one or more selected from an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil portion.

[0070] The insulation material measuring method of the present invention may include: a configuration step of configuring an insulation material adjacent to a coil portion including a wound conductive wire; and a measurement step of applying a measuring power supply to the coil portion via a measuring component electrically connected to the coil portion to measure electromagnetic properties induced in the coil portion.

[0071] The insulating material for ingot growth of the present invention comprises: an ingot growth container; and an insulating material surrounding the outer surface of the ingot growth container. The equivalent series resistance value measured by applying an AC power supply of 100kHz and 0.1A to the insulating material measuring device can be 10.57Ω to 14.16Ω.

[0072] Effects of the Invention

[0073] The graphite-containing article measurement method, measurement device, ingot growth system, etc. of the present invention can reliably measure the electromagnetic properties of the graphite-containing article in a short time and with a relatively simple method.

[0074] By applying a measurement method, the electromagnetic properties of an ingot growth container can be reliably measured in a short time with a relatively simple method. In addition, the following data can be provided: when an ingot is grown by induction heating of the ingot growth container, the electromagnetic properties such as resistance of the ingot growth container and the thermal properties based on the induction can be predicted, and an ingot growth container with more favorable properties can be selected. This can more reliably ensure the reproducibility of ingot growth. In addition, the electromagnetic properties of the ingot growth container can be quickly measured with a simplified method.

[0075] In addition, by applying the measurement method, the electromagnetic properties of the thermal insulation material can be reliably measured in a short time and in a relatively simple method. In addition, when the ingot is grown by induction heating of the ingot growth container, the resistance, electromagnetic properties and thermal characteristics of the ingot growth container and the thermal insulation material can be predicted, and data on the thermal insulation material with more favorable characteristics can be provided. In this way, the reproducibility of the ingot growth can be ensured, and the electromagnetic properties of the thermal insulation material can be quickly measured in a simplified method. BRIEF DESCRIPTION OF THE DRAWINGS

[0076] Figure 1 and Figure 2 This is a conceptual diagram showing an example of an ingot growth container measuring device according to an embodiment.

[0077] Figure 3A , Figure 3B , Figure 3C This is a graph showing the relationship between the DC current value of the ingot growth container and the electromagnetic property value induced in the toroidal coil when the ingot growth container is inductively heated in the test example.

[0078] Figure 4A , Figure 4B , Figure 4C This is a graph showing the relationship between the DC current value of the ingot growth container and the electromagnetic property value induced in the air-core coil when the ingot growth container is inductively heated in the test example.

[0079] Figure 5 and Figure 6 It is a schematic diagram showing an example of a coil portion of an ingot growth container measuring device according to an embodiment and a cross-section thereof.

[0080] Figure 7 It is a perspective view showing the arrangement of the coil portion, the heat insulating material, and the ingot growth container according to the present invention.

[0081] Figure 8 Is magnification Figure 7 A partially enlarged view of the cross section BB' of the coil portion.

[0082] Fig. 9 It is a perspective view showing the thermal insulation material measuring device of the present invention.

[0083] Fig.10 : is a graph showing the relationship between the equivalent series resistance value of the thermal insulation material measured in the examples and comparative examples and the weight of the thermal insulation material.

[0084] Fig.11 This is a graph showing average growth rates when silicon carbide ingots are grown through a heat insulating material in Examples and Comparative Examples.

[0085] Fig.12 This is a conceptual diagram illustrating the structure of an ingot growing apparatus (growing section) in cross section.

[0086] Fig.13 Block diagram showing the structure of the ingot growth system and the measurement of electromagnetic properties (thin solid lines), data flow (double solid lines) and movement of the physical ingot growth container (thick solid lines).

[0087] Description of Reference Numerals

[0088] 10: Coil parts 100a, 100b: Measuring device

[0089] 11: Initial winding wire 12, 12a, 12b: Lead wire

[0090] 13: Inner circumference of coil 200: Ingot growth container, insulated body

[0091] 210: Outer surface of the ingot growth container and the outer surface of the insulated body

[0092] 300: Measuring member 400: Insulating material DETAILED DESCRIPTION

[0093] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings so that a person skilled in the art can easily implement the present invention. However, the present invention can be implemented in a variety of different embodiments and is not limited to the embodiments described in this specification. Throughout the specification, similar parts are marked with the same reference numerals.

[0094] In the present specification, unless otherwise stated, when a certain structure “includes” another structure, it means that the other structures may also be included without excluding the other structures.

[0095] In this specification, when a certain structure is “connected” to another structure, this includes not only the case of “directly connected” but also the case of “connected by connecting other structure therebetween”.

[0096] In the present specification, B being located on A means that B is directly in contact with A or that B is located on A with another layer provided between B and A, and it should not be limitedly interpreted as B being in contact with the surface of A.

[0097] In the present specification, the term "combination thereof" included in the expression in Markush form means a mixture or combination of one or more selected from the group consisting of multiple structural elements described in the expression in Markush form, and means including one or more selected from the group consisting of the multiple structural elements.

[0098] In the present specification, the description "A and / or B" means "A or B or A and B".

[0099] In this specification, unless otherwise stated, the terms "first", "second" or "A", "B" and the like are used to distinguish the same terms.

[0100] In this specification, an expression in the singular includes an expression in the plural unless a different meaning is clearly indicated in a sentence.

[0101] Several graphite-containing objects are used in ingot growth, and their electromagnetic properties have a great influence on the grown ingot. However, in most cases, even objects with the same shape or weight have different electromagnetic properties, which hinders ensuring the reproducibility of ingot growth.

[0102] When an ingot is grown in an ingot growth container by induction heating, the weight, density, thermal conductivity, resistance and other properties of the ingot growth container and / or the insulating material surrounding the ingot growth container may have a significant impact on the ingot growth.

[0103] Among multiple ingot growth containers, each ingot growth container has different characteristics. In addition to the weight difference which is easier to measure, the thermal conductivity and resistance characteristics are also different. Such differences will affect the growth rate or quality of the ingot grown using the ingot growth container. The thermal conductivity, resistance and other characteristics of the ingot growth container itself can be confirmed by directly performing induction heating in the ingot growth container. However, induction heating takes a relatively long time and requires the entire ingot growth container to be heated and cooled, so the measurement efficiency is low.

[0104] In addition, the properties of each insulation material are different. In addition to the weight difference, which is easier to measure, the thermal conductivity and resistance characteristics are also different. This difference will affect the speed or quality when the ingot grows. The thermal conductivity and resistance of each insulation material can be confirmed by induction heating, but induction heating takes a relatively long time and requires the heating and cooling process of the insulation material and / or the ingot growth container, so the measurement efficiency is low, and the performance of the insulation material may also change during the induction heating process.

[0105] The inventor proposes a crystal ingot growth container measuring device and a crystal ingot growth container measuring method, which can pre-master the electromagnetic properties of the crystal ingot growth container in a relatively simple way, thereby ensuring sufficient reproducibility when the crystal ingot grows. In addition, the inventor proposes a thermal insulation material measuring device and a thermal insulation material measuring method, which can pre-master the electromagnetic properties of the thermal insulation material of the crystal ingot growth container in a relatively simple way, thereby ensuring sufficient reproducibility when the crystal ingot grows.

[0106] Measuring device

[0107] A measuring device according to an embodiment includes: a coil portion including a wound conductive wire; and a measuring member electrically connected to the coil portion, the measuring member applying a measuring power supply to the coil portion to measure an electromagnetic property of a graphite-containing article. The electromagnetic property is a property related to induction heating characteristics.

[0108] Figure 1 and Figure 2 is a conceptual diagram showing an example of a crystal ingot growth container measuring device according to an embodiment, Figure 3A , Figure 3B , Figure 3C This is a graph showing the relationship between the DC current value of the ingot growth container and the electromagnetic property value induced in the toroidal coil during induction heating of the ingot growth container in the test example. Figure 4A , Figure 4B , Figure 4C is a graph showing the relationship between the DC current value of the ingot growth container and the electromagnetic property value induced in the air-core coil during induction heating of the ingot growth container in the test example, Figure 5 and Figure 6 This is a conceptual diagram showing an example of a coil portion of an ingot growth container measuring device according to an embodiment and a cross section thereof.

[0109] Hereinafter, the present invention will be described in detail by taking an ingot growth container as an example of a graphite-containing article with reference to the drawings.

[0110] The ingot growth container measuring device 100a, 100b of one embodiment includes: a coil unit 10 including a wound conductive wire; and a measuring member 300 electrically connected to the coil unit, the measuring member applying a measuring power supply to the coil unit to measure the electromagnetic properties of the ingot growth container 200.

[0111] The electromagnetic property may be a factor related to the amount of change in the induced electromotive force generated in the coil part 10 by the ingot growth container 200. The induced electromotive force is an electromotive force generated by a change in magnetic flux, and when the power supply for measurement applied to the coil part is an AC power supply, an induced current is formed in the ingot growth container by the generated alternating magnetic field, thereby applying the induced electromotive force to the coil part.

[0112] The electromagnetic property may also be a factor related to the electrical resistance of the ingot growth container 200 .

[0113] The electromagnetic property may be an electromagnetic property induced when a measuring AC power source having a specific frequency and voltage is applied to the coil portion 10 containing the ingot growth container 200 through the measuring member 300. The frequency of the measuring AC power source may be 1 mHz to 200 kHz, or 10 Hz to 100 kHz. The voltage of the measuring AC power source may be 5 mV to 5 V, or 10 mV to 5 V. Within the frequency and voltage range, effective induction can be achieved so that the coil portion exhibits the target electromagnetic property.

[0114] The electromagnetic property and the DC current value of the ingot growth container or a factor related thereto when the ingot growth container is heated by an induction heating member that applies a power supply of a predetermined frequency and voltage. 2 It can be greater than 0.9, and the determination coefficient can also be greater than 0.95. The determination coefficient can be less than 0.9999, or less than 0.999. In addition, the electromagnetic property can be in a linear relationship with the DC current value. If the electromagnetic property has a linear relationship with the DC current value with a determination coefficient greater than 0.9, it is possible to select an ingot growth container having a similar value to the DC current value flowing in the ingot growth container during ingot growth. In addition, taking into account other physical properties of the ingot growth container (weight, etc.), the ingot growth container can predict the growth rate trend of the ingot during ingot growth, and the reproducibility of ingot growth can be ensured.

[0115] Specifically, the electromagnetic property may be one or more selected from the group consisting of equivalent serial resistance, equivalent serial inductance, and quality factor. Generally, the equivalent serial resistance or equivalent serial inductance is a factor used when measuring the characteristics of a circuit including a capacitor or an inductor. In the present invention, the factor is applied to measure the electromagnetic property of the coil portion containing the ingot growth container, thereby measuring the electromagnetic property of the ingot growth container.

[0116] The coil unit 10 may include lead wires 12a and 12b extending outward, and each lead wire may be electrically connected to the measuring member 300. The lead wires may correspond to both ends of a wire when the wire is wound.

[0117] The coil part 10 may include an accommodation space 13 located inside. The length (width) of the accommodation space may be greater than 100 mm and less than 300 mm, but there is no limitation as long as the ingot growth container is accommodated so that an induced electromotive force can be applied. When the wire of the coil part is wound in a circular shape, the accommodation space 13 may be in a shape corresponding to the bottom surface or the upper surface of the ingot growth container, and may be circular.

[0118] The coil part 10 may be configured such that the inside of the coil part faces the ingot growth container 200, and the distance at which the current can be induced to the ingot growth container when the measuring AC power is applied to the coil part. Specifically, the ingot growth container may be accommodated in the hollow accommodation space 13 inside the coil part, such as Figure 5 and Figure 6 As shown, the coil part and the ingot growth container may be in a state of being separated by a predetermined interval. That is, the ingot growth container may be arranged within a range reached by the induced electromotive force induced by the measuring AC power source applied to the coil part, and may be arranged so that when the ingot growth container is heated by the induction heating member, the DC current value flowing in the ingot growth container or a factor related thereto and the electromagnetic property satisfy a relationship of a determination coefficient of 0.9 or more.

[0119] like Figure 5 As shown, the cross section AA' of the coil portion 10 may have an x-direction thickness Tx measured in the x-direction parallel to the bottom surface or the upper surface of the ingot growth container 200, and a z-direction thickness Tz measured in the z-direction perpendicular to the x-direction in the lateral direction of the ingot growth container. In this case, the coil portion may be in the shape of a large annular coil whose maximum thickness in the x-direction is greater than or equal to the thickness in the z-direction.

[0120] The x-direction thickness Tx of the coil part 10 may be in a direction that spreads outward from the ingot growth container accommodated in the coil part and in parallel with a cross section of the ingot growth container.

[0121] When the coil portion 10 is in the shape of the annular coil, the thickness Tx in the x direction may be more than 8 times the thickness Tz in the z direction, or more than 10 times. The thickness in the x direction may be less than 45 times the thickness in the z direction, or less than 40 times. In addition, the number of windings of the coil portion conductor including the initial winding conductor 11 may be more than 5 turns and less than 45 turns. Within the range of the thickness in the x direction, the thickness in the z direction and the number of windings, waste of the conductor and reduction of the coefficient of determination can be prevented, and more reliable electromagnetic property measurement results can be obtained.

[0122] When the coil unit 10 is in the annular coil shape, the inner circumference of the coil unit may be in contact with the side surface 210 of the ingot growth container 200, or may be separated from the side surface by a predetermined interval. The shape of the wire wound around the coil unit may be substantially the same as the side surface shape of the ingot growth container.

[0123] When the coil portion 10 is in the shape of a toroidal coil, a layer of toroidal coils may be provided, and the height thereof may be the same as the thickness of the conductor. The toroidal coil of the layer may be provided along the outer circumference of the first winding conductor 11, and the subsequent winding conductors may be provided continuously, and the first winding conductor and the subsequent winding conductor may be located on the same plane. Even if the conductor is wound in one layer on the same plane to form a toroidal coil, height deviation may occur in some parts.

[0124] When the coil portion 10 is in the annular coil shape, an annular coil in which a conducting wire is continuously wound may be stacked on the annular coil of one layer, or an irregularly wound coil other than an annular coil shape may be stacked.

[0125] When the coil part 10 is in the annular coil shape, the cross section at the center thereof may be arranged to be parallel to the cross section of the ingot growth container 200. At this time, the center of the coil part may be arranged at the uppermost or lowermost part of the ingot growth container, but there is no limitation as long as it is at a position where the electromagnetic property of the coil part is induced.

[0126] In addition, if Figure 6 As shown, the cross section BB' of the coil portion may have an x-direction thickness Tx measured in the x-direction parallel to the bottom surface or the upper surface of the ingot growth container 200, and a z-direction thickness Tz measured in the z-direction perpendicular to the x-direction in the lateral direction of the ingot growth container. In this case, the coil may be in the shape of an air-core coil whose z-direction thickness is greater than that of the x-direction thickness.

[0127] When the coil part 10 is in the hollow coil shape, the inner peripheral surface of the coil part may be arranged to contact the side surface 210 of the ingot growth container 200, or the ingot growth container may be accommodated inside the coil part at a predetermined interval.

[0128] When the coil portion 10 is in the shape of the air-core coil, the shape of the inner circumference of the coil portion may correspond to the shape of the side surface 210 of the ingot growth container.

[0129] When the coil portion 10 is in the air-core coil shape, the x-direction thickness Tx may be in a direction extending toward the outside of the ingot growth container accommodated in the coil portion and in parallel with the cross section of the ingot growth container.

[0130] When the coil portion 10 is in the shape of the hollow coil, the z-direction thickness Tz may be more than 5 times the x-direction thickness Tx, or more than 10 times. The z-direction thickness may be less than 50 times the x-direction thickness, or less than 40 times. In addition, the number of windings of the coil portion conductor may be more than 10 turns, more than 12 turns, or more than 15 turns. The number of windings of the conductor may be less than 50 turns, less than 45 turns, or less than 40 turns. By having a coil portion having the thickness and winding number range, the measurement reliability of the electromagnetic properties is improved, and the waste of the conductor is minimized, so that the determination coefficient value can be made greater than 0.9.

[0131] The conductor of the coil portion 10 can be formed by coating a wire formed by twisting more than 50 and less than 2000 plain wires, and the plain wire can also be coated. Specifically, the conductor can be a litz wire. The diameter of the plain wire can be more than 0.05 mm, or more than 0.08 mm. The diameter of the plain wire can be less than 0.2 mm, or less than 0.125 mm. Within the above-mentioned number and diameter range, the processing process of the conductor can be simplified, and the energy loss caused by the skin effect can be minimized.

[0132] The diameter of the conductive wire may vary according to the circumference of the ingot growth container, the diameter of the element wire, and the number of the element wires.

[0133] The ingot growth container 200 may be in the shape of a cylinder with a predetermined cross section, and an outer diameter D O It can be a specified shape, or it can have an outer diameter D O and an inner diameter and including an inner space and an open upper portion.

[0134] The circumference (mm) of the side of the ingot growth container 200 and the cross-sectional area (mm) of the wire of the coil part 10 2) can be in the range of 100:1.57 to 100:161, or in the range of 100:2.35 to 100:121. Figure 5 and Figure 6 As shown, the cross-sectional area of ​​the conductor of the coil portion refers to the sum of the cross-sectional areas of the conductors constituting the coil portion minus the sum of the conductor portions of the sheathing portion, and may be the sum of the cross-sectional areas of the conductors in the region of any surface extending from the center of the coil portion toward the outside. In addition, the ratio of the side circumference (mm) of the ingot growth container to the thickness (mm) of the conductor may be 100:0.194 to 100:1.09, or 100:0.291 to 100:0.82. Within the range of the ratio, the electromagnetic properties of the target ingot growth container can be easily measured, and the measured electromagnetic properties and the DC current value can achieve a determination coefficient R 2 The linear relationship is above 0.9.

[0135] The ingot growth container 200 may be a graphite crucible for growing an ingot, or may be a graphite crucible for growing a silicon carbide ingot.

[0136] The measuring member 300 can apply an AC power supply of the aforementioned frequency and voltage to the coil portion containing the ingot growth container, and can measure the equivalent series resistance, equivalent series inductance, quality factor, etc. induced when the AC power supply is applied. Specifically, the measuring member can be an LCR meter.

[0137] Figure 7 is a perspective view showing the arrangement of the coil portion, the heat insulating material, and the ingot growth container of the present invention, Figure 8 Is magnification Figure 7 A partially enlarged view of the cross section BB' of the coil portion. Fig. 9 is a perspective view showing a thermal insulation material measuring device of the present invention, Fig.10 is a graph showing the relationship between the equivalent series resistance value of the thermal insulation material measured in the embodiment and the comparative example and the weight of the thermal insulation material, Fig.11 This is a graph showing the average growth rate when a silicon carbide ingot is grown through a heat insulating material in Examples and Comparative Examples.

[0138] Hereinafter, the present invention will be described in more detail by taking a heat insulating material as an example of a graphite-containing article with reference to the drawings.

[0139] The thermal insulation material measuring device according to one embodiment includes: a coil portion 10 including a wound conductive wire; and a measuring member 300 electrically connected to the coil portion for applying a measuring power source to the coil portion to measure the electromagnetic property of the thermal insulation material 400 .

[0140] The electromagnetic property may be a factor related to the amount of change in the induced electromotive force generated by the insulating material in the coil portion 10. The induced electromotive force is an electromotive force generated by a change in magnetic flux, and when the power supply for measurement applied to the coil portion is an AC power supply, an induced current is formed in the insulating material by the generated alternating magnetic field, thereby applying the induced electromotive force to the coil portion.

[0141] The electromagnetic property may be a factor proportional to the electrical resistance of the thermal insulation material 400 .

[0142] The electromagnetic property may be an electromagnetic property induced when a measuring AC power source having a specific frequency and voltage is applied to the coil unit 10 through the measuring member 300 .

[0143] At this time, the thermal insulation material 400 may be located outside the coil portion. The coil portion may be located on the outer surface of a support body, and as an example, the support body may be the insulated body 200. When a thermal insulation material measuring device using an insulated body as the support body is applied, it is easier to confirm the electromagnetic properties of the thermal insulation material when it is actually arranged together with the insulated body.

[0144] The frequency of the measuring AC power supply may be 1 mHz to 200 kHz, or 10 Hz to 100 kHz. The voltage of the measuring AC power supply may be 5 mV to 5 V, or 10 mV to 5 V. Within the frequency and voltage range, effective induction can be achieved so that the coil portion exhibits target electromagnetic properties.

[0145] Specifically, the electromagnetic property may be one or more selected from equivalent serial resistance, equivalent serial inductance, and quality factor. Generally, the equivalent serial resistance or equivalent serial inductance is a factor used when measuring the characteristics of a circuit including a capacitor or an inductor. In the present invention, the factor is applied to measure the electromagnetic property of the coil portion arranged adjacent to the insulating material 400, thereby measuring the electromagnetic property of the insulating material more quickly and meaningfully.

[0146] The coil unit 10 may include lead wires 12a and 12b extending outward, and each lead wire may be electrically connected to the measuring member 300. The lead wires may correspond to both ends of a wire when the wire is wound.

[0147] The coil portion 10 may include an accommodation space 13 located inside. The length (width) of the accommodation space may be greater than 100 mm and less than 300 mm, but there is no limitation as long as the insulated object 200 can correspond and induced electromotive force can be applied. The wire of the coil portion may be wound so that the cross section of the accommodation space becomes circular, and the accommodation space 13 may be cylindrical with a size capable of accommodating the insulated object.

[0148] The coil portion 10 may include a configuration space (not shown) located on the outside. The configuration space is a space for configuring the thermal insulation material. A thermal insulation material formed in a specified shape may be configured in the configuration space, and the size or shape is not limited as long as it is within the range reached by the induced electromotive force. In the case where the thermal insulation material is used for ingot growth, the thermal insulation material may have a shape that surrounds a main body of a crucible as an insulated body, and may have a cylindrical shape as an example. When the conductive wire of the coil portion is wound in a circular shape, the configuration space may be a shape corresponding to the outer side surface of the coil portion or the inner side surface of the thermal insulation material, and may be cylindrical as an example.

[0149] The coil part 10 may be arranged side by side with a surface of the insulating material 400. As an example, the coil part may be arranged side by side with a side of the insulating material, and the bottom or top surface of the insulating material may be arranged side by side with the coil part.

[0150] The distance at which the current can be induced to the thermal insulation material when the measuring AC power supply is applied to the coil portion can be configured. Specifically, the insulated body 200 can be located in the hollow accommodation space 13 inside the coil portion, and the thermal insulation material can be arranged at a predetermined interval outside the coil portion. That is, the thermal insulation material can be arranged within the range reached by the induced electromotive force induced by the measuring AC power supply applied to the coil portion.

[0151] like Figure 7 and Figure 8 As shown, the cross section BB' of the coil part 10 may have an x-direction thickness Tx measured in the x-direction parallel to the bottom surface or the upper surface of the heat insulating material 400, and a z-direction thickness Tz measured in the z-direction perpendicular to the x-direction in the lateral direction of the heat insulating material. In this case, the coil part 10 may have a large hollow coil shape in which the z-direction thickness is greater than the x-direction thickness.

[0152] The coil part 10 may be disposed such that the inner peripheral surface 13 contacts the side surface of the insulated object 200 , and may be disposed in a gap between the insulated object and the heat insulating material 400 .

[0153] The shape of the inner circumferential surface 13 of the coil portion 10 may be a shape corresponding to the side shape of the insulated body 200 .

[0154] The x-direction thickness Tx of the coil part 10 may be in a direction that spreads outward from the heat insulating material 400 in parallel with the cross section.

[0155] The z-direction thickness Tz of the coil portion 10 may be more than 5 times the x-direction thickness Tx, or more than 10 times. The z-direction thickness may be less than 50 times the x-direction thickness, or less than 40 times. In addition, the number of windings of the coil portion wire may be more than 10 turns, or more than 12 turns, or more than 15 turns. The number of windings of the wire may be less than 50 turns, or less than 45 turns, or less than 40 turns. By having a coil portion having the above-mentioned thickness and winding number range, the measurement reliability of the electromagnetic properties is improved, and the waste of wire is minimized.

[0156] The conductor of the coil portion 10 can be formed by coating a wire formed by twisting more than 50 and less than 2000 plain wires, and the plain wire can also be coated. Specifically, the conductor can be a litz wire. The diameter of the plain wire can be more than 0.05 mm, or more than 0.08 mm. The diameter of the plain wire can be less than 0.2 mm, or less than 0.125 mm. Within the above-mentioned number and diameter range, the processing process of the conductor can be simplified, and the energy loss caused by the skin effect can be minimized.

[0157] The diameter of the conductive wire may vary according to the circumference of the insulated object 200 and the insulating material 400 , the diameter of the element wire, and the number of the element wires.

[0158] The insulated body 200 may be in a cylindrical shape with a predetermined cross section, and the outer diameter D0 may be in a predetermined shape, or may be in a shape having an outer diameter and an inner diameter and including an inner space and being open at the top.

[0159] The insulating material 400 may be in the shape of a cylinder with a predetermined cross section, may be in the shape of a predetermined inner diameter D1, or may be in the shape of an outer diameter and an inner diameter and including an inner space with an upper and lower open portion. The insulated object 200 may be arranged in the inner space of the insulating material, and a predetermined interval may be provided between the insulating material and the insulated object.

[0160] As an example, the insulated body 200 may be a heated body that can be heated by an external heating member, or may be a crystal ingot growth container that can be heated by an induction heating member. The insulated body may be a graphite crucible for crystal ingot growth, or may be a graphite crucible for silicon carbide crystal ingot growth.

[0161] The thermal insulation material 400 may include a carbon-based felt, specifically, graphite felt, rayon-based graphite felt, or asphalt-based graphite felt.

[0162] The insulating material 400 can be applied to an ingot growth device for growing silicon carbide ingots. Specifically, the insulating material 400 can be applied to the following ingot growth device, which includes: an ingot growth container 200 having an internal space; an insulating material 400 disposed on the outer surface of the ingot growth container and surrounding the ingot growth container; a heating component for adjusting the temperature of the ingot growth container; a reaction chamber including the ingot growth container surrounded by the insulating material; a vacuum device connected to the interior of the reaction chamber for adjusting the vacuum degree of the reaction chamber; a pipeline connected to the interior of the reaction chamber for allowing gas to flow into the interior of the reaction chamber; and a mass flow controller for controlling the inflow of gas.

[0163] The measuring member 300 can apply an AC power supply of the aforementioned frequency and voltage to the coil portion having the insulated body 200 disposed inside and the insulating material 400 disposed outside, and can measure the equivalent series resistance, equivalent series inductance, quality factor, etc. induced when the AC power supply is applied. Specifically, the measuring member can be an LCR meter.

[0164] By using the electromagnetic property value of the insulating material measured by the measuring component 300, together with or separately from other measuring components such as weight, an insulating material with similar electromagnetic properties is selected and used as the insulating material of the ingot growth container, thereby ensuring reproducibility during ingot growth.

[0165] Measurement method

[0166] A measurement method according to one embodiment includes: a configuration step of configuring a graphite-containing article in a coil portion including a wound conductive wire; and a measurement step of applying a measuring power source to the coil portion via a measuring member electrically connected to the coil portion to measure electromagnetic properties induced in the coil portion, thereby measuring properties of the graphite-containing article related to induction heating characteristics.

[0167] As examples of the measurement method, an ingot growth container measurement method and an insulating material measurement method are described respectively.

[0168] A method for measuring a crystal ingot growth container according to one embodiment includes: a configuration step of configuring a crystal ingot growth container on a coil portion including a wound conductive wire; and a measurement step of applying a measuring power supply to the coil portion via a measuring component electrically connected to the coil portion to measure electromagnetic properties induced in the coil portion.

[0169] The arranging step is a step of arranging an ingot growth container as a measurement object on the coil portion.

[0170] In the configuration step, the coil portion may be configured to face the ingot growth container, and the distance at which the current can be induced to the ingot growth container when the measuring AC power supply is applied to the coil portion may be configured. Specifically, the ingot growth container may be configured to be accommodated in the hollow accommodation space inside the coil portion, such as Figure 5 and Figure 6 As shown, the coil part and the ingot growth container may be arranged to be separated by a predetermined interval. That is, the ingot growth container may be arranged within a range reached by the induced electromotive force induced by the measuring AC power source applied to the coil part, and may be arranged so that when the ingot growth container is heated by the induction heating member, the DC current value flowing in the ingot growth container or a factor related thereto and the electromagnetic property satisfy a linear relationship with a determination coefficient of 0.9 or more.

[0171] The coil portion may be the same as the coil portion described above.

[0172] When the coil portion is in the annular coil shape, the inner peripheral surface of the coil portion may be in contact with the side surface of the ingot growth container, or may have a predetermined gap therebetween.

[0173] When the coil part is in the shape of the hollow coil, the inner peripheral surface of the coil part may be in contact with the side surface of the ingot growth container and may be spaced apart from the side surface by a predetermined interval. The ingot growth container is arranged in the internal accommodation space of the coil part.

[0174] The ingot growth container and the relationship between the ingot growth container and the coil portion are the same as described above.

[0175] The measuring step is a step of applying a measuring AC power source having a specific frequency and voltage through a measuring member electrically connected to the coil portion, and measuring an electromagnetic property induced in the coil portion.

[0176] The electromagnetic property in the measuring step may include an element related to a change in an induced electromotive force generated in the coil portion by the ingot growth container or an element related to a resistance of the ingot growth container, which is the same as described above.

[0177] The electromagnetic property in the measuring step may have a determination coefficient R with respect to a DC current value flowing in the ingot growth container when the induction heating member applying a power supply of a predetermined frequency and voltage heats the ingot growth container or a factor related thereto. 2 The linear relationship is above 0.9, which is the same as described above.

[0178] The conditions of the AC power supply for measurement in the measurement step are the same as those described above.

[0179] A method for measuring an insulating material according to one embodiment includes: a configuration step of configuring an insulating material 400 adjacent to a coil portion 10 including a wound conductive wire; and a measurement step of applying a measuring power supply to the coil portion via a measuring member 300 electrically connected to the coil portion to measure electromagnetic properties induced in the coil portion.

[0180] The arrangement step is a step of arranging the heat insulating material 400 as the object to be measured on the coil part 10. In the arrangement step, the heat insulating material 400 may be arranged outside the coil part at a predetermined interval from the coil part. In the arrangement step, the insulated body 200 may be further arranged inside the coil part.

[0181] The coil part 10 of the configuration step can be configured at a distance where the current can be induced to the thermal insulation material 400 when the measuring AC power is applied. Specifically, the thermal insulation material 400 can be configured outside the coil part. At the same time, the insulated body 200 can be configured to be accommodated in the hollow accommodation space 13 inside the coil part or not configured as above.

[0182] The features of the coil portion 10 in the configuration step are as described above.

[0183] In the arrangement step, when the coil part 10 is in the shape of an air-core coil, the inner circumferential surface 13 of the coil part may contact the side surface of the insulated body 200, may be spaced apart from the side surface by a predetermined interval, and the insulated body may be arranged in the coil part internal accommodation space 13. Furthermore, the heat insulating material 400 may be spaced apart from the outer circumferential surface of the coil part by a predetermined interval and arranged outside the coil part.

[0184] The features of the insulated body 200 and the insulating material 400 of the configuration step are as described above.

[0185] The measuring step is a step of applying a measuring AC power supply of a specific frequency and voltage through a measuring member 300 electrically connected to the coil portion 10, and measuring the electromagnetic properties induced in the coil portion. Specifically, the frequency of the measuring AC power supply in the measuring step can be 1mHz to 200kHz, or 10Hz to 100kHz. The voltage of the measuring AC power supply can be 5mV to 5V, or 10mV to 5V. Within the frequency and voltage range, effective induction can be achieved so that the coil portion exhibits the target electromagnetic properties.

[0186] The electromagnetic property of the measuring step may include a factor related to a change in the induced electromotive force generated by the insulating material 400 or a factor proportional to the resistance of the insulating material, which is as described above.

[0187] The conditions of the AC power supply for measurement in the measurement step are as described above.

[0188] Ingot growth container

[0189] In one embodiment, the ingot growth container 200 includes graphite. When an AC power of 100 kHz and 0.1 A is applied to the ring-shaped coil type ingot growth container measuring device 100 a , the equivalent series resistance value measured may be 1.5 Ω to 7.3 Ω.

[0190] As described above, the annular coil type ingot growth container measuring device 100 a may be an ingot growth container measuring device including the coil portion 10 in the shape of an annular coil.

[0191] like Figure 5 As shown, the cross section AA' of the coil portion 10 in the shape of the annular coil may have an x-direction thickness Tx measured in the direction parallel to the bottom surface or the upper surface of the ingot growth container 200, i.e., the x-direction, and a z-direction thickness Tz measured in the side direction of the ingot growth container, i.e., the z-direction perpendicular to the x-direction. At this time, the maximum x-direction thickness of the coil portion may be greater than or equal to the z-direction thickness. Specifically, the ratio of the x-direction thickness to the z-direction thickness of the coil portion may be 14:1, and the number of windings may be 14 turns. The conductor constituting the coil portion may be a 3.5 mm diameter stranded wire formed by twisting and coating 750 0.1 mm diameter plain wires.

[0192] like Figure 1 and Figure 2 As shown, the ingot growth container 200 may be in the shape of a cylinder with a specified cross section, with an outer diameter D O It can be a specified shape, or it can have an outer diameter D O and an inner diameter and including an inner space and an open upper portion.

[0193] The outer diameter of the ingot growth container 200 is substantially the same as the circumference of the inner diameter of the coil portion. In this case, the measurement accuracy can be further improved.

[0194] The outer diameter D of the ingot growth container 200 is OWhen the diameter of the ingot growth container is 200mm to 220mm and the thickness from the outer diameter to the inner diameter is 10mm to 30mm, the equivalent series resistance Rs value measured by the annular coil type ingot growth container measuring device when the ingot growth container is in contact with and accommodated inside the coil portion 10 can be 2.25Ω to 4.56Ω, or 2.7Ω to 4.02Ω, or 2.99Ω to 3.65Ω. In addition, the equivalent series inductance Ls value measured by the annular coil type ingot growth container measuring device can be 27.44μH to 47.83μH, or 32.93μH to 42.09μH, or 36.59μH to 38.26μH. The measured equivalent series resistance value or equivalent series inductance value can have a determination coefficient R with the DC current value flowing in the ingot growth container when the induction heating member heats the ingot growth container or a factor related thereto. 2 The linear relationship is 0.9 or more. Thus, the ingot growth container to be measured can be selected based on the measurement result value so that it can present a similar DC current value during ingot growth.

[0195] In addition, the ingot growth container 200 of one embodiment includes graphite, and an equivalent series resistance value measured by applying an AC power of 100 kHz and 0.1 A to the air-core coil type ingot growth container measuring device 100 b may be 3.50 Ω to 7.24 Ω.

[0196] As described above, the air-coil type ingot growth container measuring device 100 b may be an ingot growth container measuring device including the coil portion 10 in the shape of an air-coil.

[0197] like Figure 6 As shown, the cross section BB' of the coil portion 10 in the hollow coil shape may have an x-direction thickness Tx measured in the direction parallel to the bottom surface or the upper surface of the ingot growth container 200, i.e., the x-direction, and a z-direction thickness Tz measured in the side direction of the ingot growth container, i.e., the z-direction perpendicular to the x-direction. At this time, the z-direction thickness may be greater than the x-direction thickness. Specifically, the ratio of the z-direction thickness to the x-direction thickness may be 27:1, and the number of windings may be 27 turns. The conductor constituting the coil portion may be a 3.5 mm diameter stranded wire formed by twisting and coating 750 0.1 mm diameter plain wires.

[0198] The specific method of the ingot growth container 200 is as described above.

[0199] The outer diameter of the ingot growth container 200 may be substantially the same as the circumference of the inner diameter of the coil portion, which can further improve the measurement accuracy.

[0200] The outer diameter D of the ingot growth container 200 isO When the diameter of the ingot growth container is 200mm to 220mm and the thickness from the outer diameter to the inner diameter is 10mm to 30mm, the equivalent series resistance Rs value measured by the annular coil type ingot growth container measuring device when the ingot growth container is in contact with and accommodated inside the coil portion 10 can be 3.50Ω to 7.24Ω, or 4.19Ω to 6.37Ω, or 4.65Ω to 5.79Ω. In addition, the equivalent series inductance Ls value measured by the annular coil type ingot growth container measuring device can be 74.42μH to 120.6μH, or 89.30μH to 111.67μH, or 99.22μH to 101.52μH. The equivalent series resistance value or the equivalent series inductance value can have a determination coefficient R with the DC current value flowing in the ingot growth container when the induction heating member heats the ingot growth container or a factor related thereto. 2 The linear relationship is 0.9 or more. Thus, the ingot growth container to be measured can be selected based on the measurement result value so that it can present a similar DC current value during ingot growth.

[0201] Insulation Materials

[0202] The thermal insulation material for ingot growth of one embodiment includes a cylindrical thermal insulation material 400, which surrounds the outer surface of the ingot growth container and corresponds to the outer surface shape of the ingot growth container. The equivalent series resistance value measured by applying an AC power supply of 100kHz and 0.1A to the above-mentioned thermal insulation material measuring device can be 10.57Ω to 14.16Ω.

[0203] As described above, the thermal insulation material measuring device may be a thermal insulation material measuring device including the coil portion 10 in an air-core coil shape.

[0204] like Figure 7 and Figure 8 As shown, the cross section BB' of the coil portion 10 in the hollow coil shape may have an x-direction thickness Tx measured in the direction parallel to the bottom surface or the upper surface of the insulating material 400, i.e., the x-direction, and a z-direction thickness Tz measured in the side direction of the insulating material, i.e., the z-direction perpendicular to the x-direction. At this time, the z-direction thickness may be greater than the x-direction thickness. Specifically, the ratio of the z-direction thickness to the x-direction thickness may be 27:1, and the number of windings may be 27 turns. The conductor constituting the coil portion may be a 3.5 mm diameter stranded wire formed by twisting and coating 750 0.1 mm diameter plain wires.

[0205] The specific methods of the ingot growth container 200 and the insulation material 400 are as described above.

[0206] When the outer diameter D0 of the ingot growth container 200 is 150 mm to 180 mm and the thickness from the inner diameter to the outer diameter is 10 mm to 30 mm, the equivalent series resistance Rs value measured by applying an AC power supply of 100 kHz and 0.1 A through the insulation material measuring device when the ingot growth container is in contact with and accommodated in the coil part 10 and the insulation material is located outside the coil part can be 10.57 Ω to 14.16 Ω or 11.95 Ω to 12.87 Ω.

[0207] Ingot Growth System

[0208] Fig.12 This is a conceptual diagram illustrating the structure of the ingot growing device (growing unit) in cross section. Fig.13 The block diagram shows the structure of the ingot growth system and the measurement of electromagnetic characteristics (thin solid line), data flow (double solid line) and movement of the physical ingot growth container (thick solid line). The ingot growth system will be described in more detail with reference to the accompanying drawings.

[0209] The ingot growth system of the present invention is a system that includes a graphite-containing object and a heating component to grow a silicon carbide ingot. The graphite-containing object is an ingot growth container or an insulating material. The ingot growth container includes: a main body having an internal space for configuring raw materials; and a silicon carbide seed configured on the upper part of the main body or on the main body. The graphite-containing object has an electromagnetic characteristic value measured by a measuring device, namely an equivalent series resistance value.

[0210] The equivalent series resistance value of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A may be 3.50 Ω to 7.24 Ω. ​​The value is based on a value measured by an air-core coil type measuring device.

[0211] The equivalent series resistance of the insulating material measured by applying an AC power supply of 100 kHz and 0.1 A may be 10.57Ω to 14.16Ω. The value is based on a value measured by using an air-core coil type measuring device with an ingot growth container disposed inside the coil part and the insulating material disposed outside the coil.

[0212] The silicon carbide ingot may be induced to grow at a speed of more than 100 mm / hr.

[0213] The ingot growth system 1000 of the present invention includes: a measuring unit 1, which measures indirect characteristics of an ingot growth container, etc.; a predicting unit 2, which calculates and displays information obtained by the measuring unit; and a growing unit 3, which uses an ingot growth container having a predicted result value to grow an ingot. The measuring unit can also measure the weight of the ingot growth container, etc.

[0214] The measuring unit 1 includes an ingot growth container 200 and ingot growth container measuring devices 100a and 100b, which can send and receive electromagnetic signals to each other.

[0215] The prediction unit 2 includes: a calculation unit 30, which is responsible for storing information and performing calculations in a predetermined manner; and an output unit 40, which is used to display the results of the calculations. There are no restrictions on the calculation unit as long as it can perform data storage and data calculations, and there are no restrictions on the output unit as long as it can display the output value. As an example, a computer and a display can be applied. The prediction unit can convert the electromagnetic characteristics measured in the measurement unit into values ​​such as the resistance of the ingot growth container or the insulating material as direct characteristics, and can predict the growth rate of the ingot, etc. The conversion refers to the calculation of the direct characteristics corresponding to the weight accumulated in the database and the electromagnetic characteristics measured by the measurement unit. The prediction refers to the calculation performed by the following formulas 1 and 2 when the direct characteristics corresponding to the weight accumulated in the database and the electromagnetic characteristics measured by the measurement unit are not set.

[0216] The growth part 3 includes an ingot growth container 200 and a heating member 600 to grow the ingot 100 .

[0217] The heating member induces the inner space to become a crystal growth atmosphere, the raw material P vapor is transferred to the seed crystal and deposited, a crystal growth atmosphere is created to form an ingot grown from the seed crystal, and growth of the ingot is induced.

[0218] The ingot growth container 200 includes: a body 210 having an internal space for disposing a raw material P; and a seed crystal disposed on the upper portion of or on the body.

[0219] The seed crystal may be supported by the cover 220 .

[0220] The ingot growth container or the body has an electromagnetic indirect characteristic value confirmed by applying an AC power source as a measurement power source, the indirect characteristic value being a value having a high correlation with a direct characteristic.

[0221] The electromagnetic indirect characteristic value includes an equivalent series resistance value, and the equivalent series resistance value has a correlation relationship with a direct current value flowing in the ingot growth container when the ingot growth container is heated by the heating member, with a determination coefficient of 0.9 or more.

[0222] The equivalent series resistance value is determined by an ingot growth container measuring device in which a coil portion including a wound conducting wire is arranged.

[0223] The growth rate and other characteristics can also be predicted based on the Pr value of the following formula 1 or the Pl value of the following formula 2 calculated based on the weight of the ingot growth container measured by the ring coil type ingot growth container measuring device and the indirect characteristics.

[0224] [Formula 1]

[0225]

[0226] [Formula 2]

[0227]

[0228] Specifically, when the Pr value based on Formula 1 is 6.05 or less, or the Pl value based on Formula 2 is 7.2 or less, an excellent ingot growth rate can be achieved. As an example, an ingot growth rate of approximately 100 mm / hr or more can be achieved.

[0229] The Pr value may be 6.0 or less. The Pr value may be 5.8 or less. The Pr value may be 5.7 or less. The Pr value may be 4.8 or more. The Pr value may be 5.1 or more.

[0230] The Pl value may be 7.0 or less. The Pl value may be 6.8 or less. The Pl value may be 6.0 or more. The Pl value may be 6.2 or more. The Pl value may be 6.5 or more. The Pl value may be 6.5 to 6.7.

[0231] In this case, a more excellent ingot growth rate can be achieved. As an example, the ingot growth rate can be 110 to 130 mm / hr or more.

[0232] Thus, for the measured ingot growth container, the ingot growth is induced by the ingot growth container having the characteristics favorable for the ingot growth according to the measurement result value, so that the ingot can be prepared more efficiently.

[0233] The growth rate and other characteristics can also be predicted based on the Pr value of the following formula 1 or the Pl value of the following formula 2 calculated by calculating the weight of the ingot growth container measured by the air-core coil type ingot growth container measuring device and indirect characteristics.

[0234] [Formula 1]

[0235]

[0236] [Formula 2]

[0237]

[0238] Specifically, when the Pr value based on Formula 1 is 9.46 or less or the Pl value based on Formula 2 is 18.5 or less, the ingot growth rate is better. As an example, the ingot growth rate can be 100 mm / hr or more.

[0239] The Pr value may be 8.91 or less. The Pr value may be 8.42 or less. The Pr value may be 8.30 or less. The Pr value may be 7.0 or more. The Pr value may be 8.0 or more.

[0240] The Pl value may be 18.1 or less. The Pl value may be 16.8 or more. The Pl value may be 17.1 or more. The Pl value may be 17.3 or more. The Pl value may be 17.4 to 18.1.

[0241] In this case, a more excellent ingot growth rate can be achieved. As an example, the ingot growth rate can be 110 to 130 mm / hr or more.

[0242] Thus, for the measured ingot growth container, the ingot growth is induced by the ingot growth container having the characteristics favorable for the ingot growth according to the measurement result value, so that the ingot can be prepared more efficiently.

[0243] Ingot preparation method

[0244] The ingot preparation method includes: a preparation step, in which a raw material material P and a seed crystal (seed crystal) are separated and arranged in an ingot growth container 200 having an internal space; a growth step, in which the temperature, pressure and atmosphere of the internal space are adjusted so that the raw material material sublimates and the ingot 100 grows on the seed crystal; and a cooling step, in which the ingot growth container is cooled to recover the ingot.

[0245] The ingot may be a silicon carbide ingot.

[0246] The raw material may include a carbon source and a silicon source, and may include silicon carbide particles as an example.

[0247] The seed crystal may be a silicon carbide seed crystal.

[0248] The seed crystal may be a 4H silicon carbide seed crystal.

[0249] The growing step may be performed in an inert gas atmosphere having a flow rate of 100 sccm to 300 sccm.

[0250] The cooling step may be performed in an inert gas atmosphere having a flow rate of 1 sccm to 250 sccm.

[0251] The thermal conductivity of the ingot growth container may be 120 W / mK or less.

[0252] The ingot recovered after the cooling step may be cut, polished, and surface ground to be arranged into wafers.

[0253] The raw material material P of the preparation step may be used in the form of powders having a carbon source and a silicon source, and a raw material obtained by necking the powders together or a silicon carbide powder obtained by carbonizing the surface thereof may be used.

[0254] The ingot growth container 200 of the preparation step may be a container suitable for the growth reaction of the ingot, and specifically, a graphite crucible may be used. For example, the ingot growth container may include: a body 210, including an internal space and an opening; and a cover 220, corresponding to the opening, to close the internal space. The cover may also include a seed crystal holder that is integral with or separate from the cover, and the seed crystal may be fixed by the seed crystal holder so that the seed crystal and the raw material can face each other.

[0255] The ingot growth container of the preparation step may have the features as described above.

[0256] Furthermore, the ingot growth container may have the thermal conductivity characteristics and the like described later.

[0257] The thermal conductivity of the ingot growth container 200 in the preparation step may be less than 120 W / mK and may be greater than 85 W / mK. When the thermal conductivity of the ingot growth container is less than 85 W / mK, the temperature gradient of the ingot growth container becomes too large during ingot growth, thereby increasing the possibility of cracks in the ingot and increasing the stress inside the ingot. When the thermal conductivity of the ingot growth container exceeds 120 W / mK, the current decreases during induction heating, the internal heating temperature also decreases, there is a risk of reduced ingot growth rate, and impurities are increased.

[0258] By using an ingot growth container having the thermal conductivity range, the temperature gradient of the ingot growth container can be stably achieved, and the ingot prepared in subsequent steps can achieve target mechanical characteristics.

[0259] The ingot growth container 200 of the preparation step may be surrounded and fixed by a heat insulating material 400, and the ingot growth container surrounded by the heat insulating material may be accommodated in a reaction chamber 500 such as a quartz tube. The temperature of the inner space of the ingot growth container can be controlled by the heat insulating material and a heating member 600 disposed outside the reaction chamber.

[0260] The heating member 600 may be a coil-shaped induction heating member. When a high-frequency alternating current is supplied to the induction heating member, an eddy current is generated in the ingot growth container 200, and the internal space of the ingot growth container may be heated by pyrolysis generated by the resistance of the ingot growth container.

[0261] The porosity of the thermal insulation material 400 in the preparation step may be 72% to 95%, 75% to 93%, or 80% to 91%. When a thermal insulation material having the above porosity is used, the generation of cracks in the grown ingot may be further reduced.

[0262] The compressive strength of the insulating material 400 in the preparation step may be greater than 0.2 MPa, greater than 0.48 MPa, or greater than 0.8 MPa. Furthermore, the compressive strength of the insulating material may be less than 3 MPa, or less than 2.5 MPa. When the insulating material has such a compressive strength, its thermal / mechanical stability is excellent, and the probability of ash generation is reduced, so that a silicon carbide ingot with better quality can be prepared.

[0263] The thermal conductivity of the thermal insulation material 400 at 2000°C may be 1.79 W / mK or less, or 1.24 W / mK or less. The thermal conductivity of the thermal insulation material at 2000°C may be 0.3 W / mK or more, or 0.48 W / mK or more. The thermal insulation material having the thermal conductivity range can block the heat release of the ingot growth container 200 during ingot growth and form a stable temperature gradient of the ingot growth container.

[0264] The density of the heat insulating material 400 in the preparation step may be greater than 0.13 g / cc, or greater than 0.17 g / cc. The density of the heat insulating material may be less than 0.28 g / cc, or less than 0.24 g / cc. The heat insulating material having the density range described above can suppress bending and twisting of the prepared ingot.

[0265] The reaction chamber 500 of the preparation step may include: a vacuum pump 700 connected to the inside of the reaction chamber for adjusting the vacuum degree inside the reaction chamber; a pipeline 810 connected to the inside of the reaction chamber for introducing gas into the reaction chamber; and a mass flow controller 800 for controlling. Through these, the flow rate of the inert gas can be adjusted in the subsequent growth step and cooling step.

[0266] The growing step is a step of sublimating the raw material substance P by adjusting the temperature, pressure, and atmosphere of the internal space, thereby growing the silicon carbide ingot 100 on the seed crystal.

[0267] The growing step may be performed by heating the ingot growth container 200 and the inner space of the ingot growth container using the heating unit 600, and the inner space may be depressurized to adjust the pressure while or in addition to the heating, and an inert gas may be injected to induce the growth of silicon carbide crystals.

[0268] The growing step may be performed at a temperature of 2000° C. to 2600° C. and a pressure of 1 to 200 torr. Silicon carbide ingots can be prepared more efficiently within the temperature and pressure ranges.

[0269] As an example, the growth step is performed under the condition that the temperature of the upper and lower parts of the ingot growth container 200 is 2100° C. to 2500° C. and the pressure of the inner space of the ingot growth container is 1 to 50 torr, or the temperature of the upper and lower parts is 2150° C. to 2350° C. and the pressure of the inner space of the ingot growth container is 1 to 30 torr. When the temperature and pressure conditions are applied to the growth step, a higher quality silicon carbide ingot can be prepared.

[0270] In the growth step, the temperature can be increased at a heating rate of 1°C / min to 10°C / min or a heating rate of 5°C / min to 10°C / min until the temperature reaches the temperature range, and may include a pre-growth process with a relatively low heating rate and a growth process with a high heating rate.

[0271] In the growth step, a predetermined flow rate of an inert gas may be added to the inside of the ingot growth container 200. As an example, the inert gas may flow from the raw material P to the seed crystal. At this time, the growth step may be performed under an inert gas atmosphere with a flow rate of 100 sccm to 300 sccm, or may be performed under an inert gas atmosphere with a flow rate of 150 sccm to 250 sccm. If the flow rate is less than 100 sccm, the impurity content may increase due to the reduction in the sublimation amount of the raw material. If the flow rate exceeds 300 sccm, the growth rate of the ingot is too fast, which may result in a decrease in the quality of the ingot. The growth step is performed within the flow rate range to form a stable temperature gradient in the ingot growth container and the internal space, which makes it easy to achieve the sublimation of the raw material, thereby helping the ingot to achieve the target mechanical properties.

[0272] For example, the inert gas in the growth step may be argon, helium, or a mixed gas thereof, and may also include a small amount of nitrogen.

[0273] The cooling step is a step of cooling the grown silicon carbide ingot under the conditions of a predetermined cooling rate and an inert gas flow rate.

[0274] In the cooling step, the cooling may be performed at a rate of 1°C / min to 10°C / min, or at a rate of 3°C / min to 9°C / min. In the cooling step, the cooling may be performed at a rate of 5°C / min to 8°C / min.

[0275] Similar to the growth step, in the cooling step, a predetermined flow rate of inert gas may be added to the inside of the ingot growth container 200. As an example, the inert gas may flow from the raw material P to the silicon carbide seed crystal. At this time, the cooling step may be performed under an inert gas atmosphere with a flow rate of 1 sccm to 300 sccm, or may be performed under an inert gas atmosphere with a flow rate of 10 sccm to 250 sccm. If the flow rate is less than 1 sccm, the cooling efficiency of the ingot decreases, and the temperature gradient of the ingot growth container is too large, which may lead to an increase in the crack generation rate of the ingot and the internal stress of the ingot. If the flow rate exceeds 300 sccm, the cooling rate increases excessively, which may lead to an increase in the crack generation rate of the ingot and the internal stress of the ingot. The cooling step is performed within the flow rate range to form a stable temperature gradient of the ingot growth container and the internal space, so that the cooling of the ingot can be easily achieved, thereby achieving the target mechanical properties.

[0276] The ratio Fg / Fc of the inert gas flow rate Fg in the growth step to the inert gas flow rate Fc in the cooling step may be 0.33 to 30, 0.6 to 25, or 0.6 to 6. With such a flow rate ratio, a gentle flow rate change is achieved during the growth and cooling steps, which helps the grown and cooled silicon carbide ingot to have better mechanical properties.

[0277] The cooling step may be performed simultaneously with the pressure adjustment of the inner space of the ingot growth container 200, or the pressure adjustment may be performed separately from the cooling step. The pressure adjustment may be performed in such a way that the pressure in the inner space is 800 Torr at maximum.

[0278] The recovery of the cooling step can be carried out by cutting the back of the ingot in contact with the seed crystal. The recovered ingot can be processed into a wafer form through subsequent processes.

[0279] The present invention is further described in detail below through specific examples. The following examples are merely illustrative to help understand the present invention, and the scope of the present invention is not limited thereto.

[0280] Example A

[0281] Example A-1: ​​Preparation of an ingot growth container measuring device 100a having a coil portion 10 in a toroidal coil shape

[0282] like Figure 1 As shown, as a crystal ingot growth container, prepare an outer diameter D O A graphite crucible with an inner diameter of 210 mm and an inner diameter of 190 mm is provided with a coil portion in the shape of a ring coil, the inner circumference of the ring coil is in contact with the outer circumference of the crucible, and has 14 turns of wire winding, and is located in the same plane. The wire uses a 3.5 mm diameter stranded wire made by twisting and covering 750 0.1 mm diameter plain wires. The inner diameter of the ring coil is 210 mm, and the outer diameter is 325 mm. The thickness of the ring coil in the direction parallel to the bottom surface of the crucible, that is, the x-direction thickness of the ring coil is 14 times the thickness in the z-direction thickness parallel to the height direction of the side of the ingot growth container. In addition, the ratio of the circumference of the crucible to the diameter of the stranded wire is 100:0.58.

[0283] The lead wires 12a and 12b at both ends of the twisted wire constituting the annular coil were connected to an LCR meter (HIOKI3522-50), and the zero point was adjusted so that when an AC power supply of 100kHz and 0.1A was applied, the value of the electromagnetic property (one of the equivalent series resistance, equivalent series inductance, and quality factor) of the coil portion became 0. Before the zero point adjustment, the equivalent series inductance value of the coil portion was 35.1uH, and the equivalent series resistance was 51.1mΩ.

[0284] Example A-2: Preparation of an ingot growth container measuring device 100b having a coil portion 10 in an air-core coil shape

[0285] As a crystal ingot growth container, prepare an outer diameter D O A graphite crucible with a diameter of 210 mm and an inner diameter of 190 mm is provided with a coil portion, the coil portion being in the shape of a hollow coil, the inner circumference of which is substantially in contact with and corresponds to the outer circumference of the crucible, and having 27 turns of wire winding. The wire uses a 3.5 mm diameter stranded wire formed by twisting and covering 750 0.1 mm diameter plain wires. The inner diameter of the hollow coil is 211 mm, the outer diameter is 224 mm, and the thickness of the hollow coil in the z direction parallel to the side height direction of the ingot growth container is 27 times the thickness in the x direction parallel to the bottom surface of the crucible. In addition, the ratio of the circumference of the crucible to the diameter of the stranded wire is 100:0.58.

[0286] The lead wires 12a and 12b at both ends of the stranded wire constituting the air-core coil were connected to an LCR meter (HIOKI3522-50), and the zero point was adjusted so that when an AC power supply of 100kHz and 0.1A was applied, the value of the electromagnetic property (one of the equivalent series resistance, equivalent series inductance, and quality factor) of the coil portion became 0. Before the zero point adjustment, the equivalent series inductance value of the coil portion was 131uH, and the equivalent series resistance was 1.03mΩ.

[0287] Example A-3: Electromagnetic Property Measurement of Ingot Growth Container 1

[0288] like Figure 1 As shown, in the case of an internal space with an outer diameter D O The outer circumference of the cylindrical graphite ingot growth container 200 with a diameter of 105 mm and a weight as shown in Tables 1 and 2 was contacted at the bottom of the prepared coil portion of the ring-shaped coil in the ingot growth container measuring device 100a. An AC power supply of 100 kHz and 0.1 A was applied to the coil portion by an LCR meter to measure the induced equivalent series resistance Rs, equivalent series inductance Ls and quality factor Q. The measurement took about 20 seconds.

[0289] Example A-4: Electromagnetic Property Measurement of Ingot Growth Container 2

[0290] The ingot growth container 200 of the measurement 1 is placed at a predetermined interval (52.5 mm) inside the hollow coil-shaped coil portion of the prepared ingot growth container measuring device 100b. An AC power supply of 100 kHz and 0.1 A is applied to the coil portion by an LCR meter to measure the induced equivalent series resistance Rs, equivalent series inductance Ls, and quality factor Q. The measurement takes about 20 seconds.

[0291] Example A-5: Silicon carbide ingot growth and growth rate measurement based on measured ingot growth container

[0292] The silicon carbide raw material is loaded into the lower part of the inner space of the ingot growth container of Table 1 and Table 2, and the silicon carbide seed crystal is arranged on the upper part. The ingot growth container is sealed and arranged in a reaction chamber with a heating coil outside.

[0293] The internal space of the ingot growth container is depressurized to adjust to a vacuum atmosphere, argon gas is injected to make the internal space become atmospheric pressure, and then the internal space is depressurized again. At the same time, power is applied to the heating coil to increase the temperature of the internal space to 2500°C at a heating rate of 5 to 10°C / min, and a silicon carbide ingot is grown for 100 hours on the silicon carbide seed crystal surface facing the silicon carbide raw material under a pressure of 5 Torr. At this time, the DC current value and the ingot growth rate of the ingot growth container are measured and confirmed by applying the same power supply as the ingot growth process within the lower temperature reference of 2200 to 2400°C of the ingot growth container when the growth process is performed using the growth equipment.

[0294] [Table 1]

[0295]

[0296] (Ls: equivalent series inductance, Rs: equivalent series resistance, Q: quality factor)

[0297] [Table 2]

[0298]

[0299] (Ls: equivalent series inductance, Rs: equivalent series resistance, Q: quality factor)

[0300] Refer to Table 1, 2, Figure 3A , Figure 3B , Figure 3C as well as Figure 4A , Figure 4B , Figure 4C , the Ls value induced by the toroidal coil and the DC current value present a linear relationship with a determination coefficient of 0.9834 ( Figure 3A The Rs value induced by the annular coil and the DC current value present a linear relationship with a determination coefficient of 0.9915 ( Figure 3B In addition, the Q value induced by the annular coil and the DC current value present a linear relationship with a determination coefficient of 0.9924 ( Figure 3C In addition, the Ls value induced by the hollow coil and the DC current value present a linear relationship with a determination coefficient of 0.9841 ( Figure 4A The Rs value induced by the hollow coil and the DC current value present a linear relationship with a determination coefficient of 0.9907 ( Figure 4B In addition, the Q value induced by the hollow coil and the DC current value show a linear relationship with a determination coefficient of 0.9922 ( Figure 4C ). This indicates that the prediction accuracy is high.

[0301] That is, it can be seen that the Ls, Rs and Q values ​​induced by the annular coil and the hollow coil show a linear relationship with the DC current value with a determination coefficient of more than 0.98, thereby confirming that when multiple crystal ingot growth containers are applied to crystal ingot growth based on induction heating, they can be selected in a manner that can present similar crystal ingot growth container DC current values.

[0302] Example B

[0303] Example B-1: Preparation of a hollow coil-shaped coil portion and an ingot growth device

[0304] A coil portion having a wire winding number of 25 turns and an air-core coil shape is provided. The wire is a 3.5 mm diameter stranded wire obtained by twisting and covering 750 0.1 mm diameter plain wires. The inner diameter of the coil portion is 172 mm, the outer diameter is 180 mm, and the thickness of the coil portion in the z direction parallel to the height direction of the side of the cylindrical thermal insulation material to be measured is 25 times the thickness in the x direction parallel to the bottom surface of the thermal insulation material.

[0305] The lead wires 12a and 12b at both ends of the twisted wire of the coil part were connected to an LCR meter (HIOKI 3522-50), and the zero point was adjusted so that when an AC power supply of 100kHz and 0.1A was applied, the value of the electromagnetic property (one of the equivalent series resistance, equivalent series inductance, and quality factor) of the coil part became 0. Before the zero point adjustment, the equivalent series inductance of the coil part was 131uH, and the equivalent series resistance was 4.01Ω.

[0306] Example B-2: Ingot growth based on thermal insulation materials selected by measuring electromagnetic properties

[0307] like Fig. 9 As shown in FIG. 3 , the coil portion of the thermal insulation material measuring device prepared is arranged between a cylindrical graphite ingot growth container having an inner space and an outer diameter D0 of 180 mm and an inner peripheral surface of a thermal insulation material surrounding the graphite ingot growth container and having a weight shown in Table 3. An AC power supply of 100 kHz and 0.1 A is applied to the coil portion by an LCR meter to measure the induced equivalent series resistance Rs, equivalent series inductance Ls, and quality factor Q. The measurement takes about 20 seconds.

[0308] Afterwards, a silicon carbide seed crystal is placed in the upper part of the ingot growth container surrounded by an insulating material having an equivalent series resistance measurement value of 11.88Ω to 12.87Ω, and a silicon carbide raw material powder is placed in the lower part. The ingot growth container is sealed and placed in a reaction chamber having a heating coil outside.

[0309] The inner space of the ingot growth container was depressurized to adjust to a vacuum atmosphere, argon gas was injected to make the inner space at atmospheric pressure, and then the inner space was depressurized again. At the same time, power was applied to the heating coil to increase the temperature of the inner space to 2500°C at a heating rate of 5 to 10°C / min, and the silicon carbide ingot was grown for 100 hours on the silicon carbide seed crystal surface facing the silicon carbide raw material under a pressure of 5 Torr. At this time, the average growth rate of the silicon carbide ingot is shown in Table 3.

[0310] Example B-3: Ingot growth based on arbitrary insulating materials without measured electromagnetic properties

[0311] Table 3 shows the average growth rate of the silicon carbide ingot grown in the same manner as in the above-described embodiment except that an ingot growth container surrounded by any insulating material whose electromagnetic properties were not measured was used.

[0312] [Table 3]

[0313]

[0314] Rs(Ω)*: Equivalent series resistance

[0315] From Table 3 and Fig.11 It can be confirmed that Examples 1 to 15, in which a silicon carbide ingot is grown through an ingot growth container surrounded by an insulating material having an equivalent series resistance measurement value of 11.88Ω to 12.87Ω, exhibited a growth rate of 0.12μm / hr to 0.14μm / hr. In contrast, Comparative Examples 1 to 3, in which a silicon carbide ingot is grown through an ingot growth container surrounded by an arbitrary insulating material whose electromagnetic properties are not measured, exhibited a growth rate of 0.04μm / hr.

[0316] Example B-4: Comparison of the correlation between the weight of the thermal insulation material and the measured value of the thermal insulation material measuring device

[0317] The correlation between the equivalent series resistance value of the thermal insulation material measured in the embodiment and the comparative example and the weight of the thermal insulation material is shown in FIG. Fig.10 Referring to this figure, it can be seen that the weight of the insulation material and the measured equivalent series resistance value have a determination coefficient R 2 It was confirmed that it was difficult to ensure the reproducibility of ingot growth when the thermal insulating material was selected only by weight and an ingot was grown using the thermal insulating material, as shown in the results of the comparative example.

[0318] By selecting a thermal insulation material having similar electromagnetic properties through the thermal insulation material measuring device and using the thermal insulation material as the thermal insulation material of the crystal ingot growth container, effective crystal ingot growth can be achieved.

[0319] Example C

[0320] (Silicon carbide ingot growth and growth rate measurement based on ingot growth container)

[0321] The results of Examples 1 to 30 that are the same as Example A are shown in the following Tables 4 and 5 together with the Pr and Pl values. Specifically, the silicon carbide raw material P is loaded into the lower part of the inner space of the ingot growth container, and the silicon carbide seed crystal is arranged at the upper part. The ingot growth container 200 is sealed and arranged in a reaction chamber 500 having a heating coil 600 outside.

[0322] The vacuum device 700 is used to reduce the pressure of the inner space of the ingot growth container to adjust it to a vacuum atmosphere, and argon gas is injected to make the inner space become atmospheric pressure, and then the inner space is reduced in pressure. At the same time, power is applied to the heating coil to increase the temperature of the inner space to 2500°C at a heating rate of 5 to 10°C / min, and the silicon carbide ingot is grown for 100 hours on the silicon carbide seed crystal surface facing the silicon carbide raw material under a pressure of 5 Torr. The internal pressure is adjusted by the flow controller 800 and the pipeline 810 connected thereto.

[0323] At this time, the DC current value and the ingot growth rate of the ingot growth container are measured and confirmed by applying the same power supply as in the ingot growth process at the lower temperature reference 2200 to 2400° C. of the ingot growth container during the growth process using the growth equipment. The Pr and Pl values ​​are evaluated by the above equations 1 and 2.

[0324] [Table 4]

[0325]

[0326] [Table 5]

[0327]

[0328] Referring to Tables 4 and 5, it is confirmed that when the data on electromagnetic indirect characteristics are not fully ensured, by calculating the Pr value or the Pl value, these values ​​can be used to predict the growth rate trend of the ingot to a certain extent. Although not shown in the figure, a linear result of more than 0.83 is shown, which allows prediction to a high degree and enables efficient processes.

[0329] The preferred embodiments of the present invention are described in detail above, but the scope of the present invention is not limited thereto. Various modifications and improvements implemented by ordinary technicians in the technical field to which the present invention belongs using the basic concepts of the present invention defined by the claims also fall within the scope of the present invention.

Claims

1. A method for measuring a graphite-containing article, wherein the physical properties of the graphite-containing article related to induction heating characteristics are measured, wherein: The graphite-containing article is an ingot growth container or an insulating material, The method for measuring the graphite-containing article comprises: a step of arranging a graphite-containing article on a coil portion including a wound conductive wire; and a measuring step of applying a measuring power supply to the coil portion by a measuring member electrically connected to the coil portion to measure an electromagnetic property induced in the coil portion; The electromagnetic property is at least one selected from the group consisting of an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil portion, The ratio of the circumference of the inner diameter of the coil part to the cross-sectional area of ​​the wire of the coil part is 100:1.57 to 100:161, wherein the unit of the circumference is mm and the unit of the cross-sectional area is mm. 2 , The equivalent series resistance of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A is 2.35Ω to 4.56Ω. The equivalent series resistance of the thermal insulation material measured by applying an AC power supply of 100 kHz and 0.1 A was 10.57Ω to 14.16Ω.

2. The method for measuring a graphite-containing article according to claim 1, wherein: The electromagnetic properties include factors related to changes in induced electromotive force generated in the coil portion based on the graphite-containing article or factors related to electrical resistance of the graphite-containing article.

3. The method for measuring a graphite-containing article according to claim 1, wherein: The coil portion has a receiving space located inside. The ingot growth container is arranged in the accommodation space, The heat insulating material is disposed outside the coil portion.

4. The method for measuring a graphite-containing article according to claim 3, wherein: The length of the accommodating space is greater than 100 mm.

5. A method for measuring a graphite-containing article, measuring a physical property of the graphite-containing article related to induction heating characteristics, comprising: a step of arranging a graphite-containing article on a coil portion including a wound conductive wire; as well as a measuring step of applying a measuring power supply to the coil portion by a measuring member electrically connected to the coil portion to measure an electromagnetic property induced in the coil portion; The graphite-containing article is an ingot growth container, The electromagnetic property is at least one selected from the group consisting of an equivalent series resistance, an equivalent series inductance, and a quality factor of the coil portion, The cross section of the coil portion has: an x-direction thickness measured in a direction parallel to the bottom or top surface of the graphite-containing article, i.e., the x-direction; and The thickness in the z direction is measured in the lateral direction of the graphite-containing article, i.e., in the z direction perpendicular to the x direction, The coil portion is a toroidal coil type whose thickness in the x direction is greater than or equal to its thickness in the z direction, The ratio of the circumference of the inner diameter of the coil portion of the annular coil type to the thickness of the conductive wire is 100:0.194 to 100:1.09, wherein the unit of the circumference is mm, and the unit of the thickness is mm, The equivalent series resistance of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A was 2.35Ω to 4.56Ω.

6. A method for measuring a graphite-containing article, measuring a physical property of the graphite-containing article related to induction heating characteristics, comprising: a step of arranging a graphite-containing article on a coil portion including a wound conductive wire; as well as The measuring step comprises applying a measuring power supply to the coil portion by a measuring member electrically connected to the coil portion to measure the electromagnetic property induced in the coil portion, wherein the cross section of the coil portion has: an x-direction thickness measured in a direction parallel to the bottom or top surface of the graphite-containing article, i.e., the x-direction; and The thickness in the z direction is measured in the lateral direction of the graphite-containing article, i.e., in the z direction perpendicular to the x direction, The coil portion is an air-core coil type whose thickness in the z direction is greater than its thickness in the x direction, The ratio of the circumference of the inner diameter of the coil part of the air-core coil type to the thickness of the conductor is 100:0.194 to 100:1.09, wherein the unit of the circumference is mm, and the unit of the thickness is mm, The graphite-containing article is an ingot growth container, The equivalent series resistance of the ingot growth container measured by applying an AC power supply of 100 kHz and 0.1 A was 3.50Ω to 7.24Ω.

7. A method for measuring a graphite-containing article, measuring a physical property of the graphite-containing article related to induction heating characteristics, comprising: a step of arranging a graphite-containing article on a coil portion including a wound conductive wire; as well as a measuring step of applying a measuring power supply to the coil portion by a measuring member electrically connected to the coil portion to measure an electromagnetic property induced in the coil portion; The cross section of the coil portion has: an x-direction thickness measured in a direction parallel to the bottom or top surface of the graphite-containing article, i.e., the x-direction; and The thickness in the z direction is measured in the lateral direction of the graphite-containing article, i.e., in the z direction perpendicular to the x direction, The coil portion is an air-core coil type whose thickness in the z direction is greater than its thickness in the x direction, The ratio of the circumference of the inner diameter of the coil part of the air-core coil type to the thickness of the conductor is 100:0.194 to 100:1.09, wherein the unit of the circumference is mm, and the unit of the thickness is mm, The graphite-containing article is a thermal insulating material, The equivalent series resistance of the thermal insulation material measured by applying an AC power supply of 100 kHz and 0.1 A was 10.57Ω to 14.16Ω.

Citation Information

Patent Citations

  • Method for evaluating silica glass crucible, method for producing silicon single crystals

    KR1020140104500A

  • Method for producing silicon carbide single crystal

    CN107208310A

  • Method for growing single crystal silicon carbide ingot having large diameter

    CN110168147A

  • Plasma generator

    EP1022933A2

  • Nitride single crystal and apparatus for producing the same

    JP2011026161A