Experimental device and method for rock damage under dry-wet cycle coupled confining pressure
Through the test device and method under the coupled confining pressure of dry and wet cycles, the damage process of the slope rock mass is simulated, which solves the problem of difficulty in evaluating the damage performance of the slope rock mass in the existing technology and realizes the evaluation of the damage of the slope rock mass. Realistic quantification and prediction of geological hazard risks.
Patent Information
- Application Number
- CN202110274059.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-03-15
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-03-15
AI Technical Summary
Existing technology makes it difficult to accurately evaluate the damage performance of slope rock mass under dry-wet cycles and confining pressure, making it difficult to predict geological disaster risks.
A test device and method under dry-wet cycle coupled confining pressure are designed. By simulating the actual environment of the slope rock mass, using the test chamber and CT scanning technology, the damage process of the rock mass is quantified and the damage of the slope rock mass is reflected. Mechanisms and geological hazard risks.
It achieves real simulation and quantification of slope rock mass damage, simplifies the test process, reduces cost and time, reveals the relationship between the number of dry and wet cycles and the degree of damage, and provides an important basis for geological disaster research.
Smart Images

Figure CN112903467B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of rock damage and degradation detection, and in particular to a test device and method for rock damage under dry-wet cycle coupled confining pressure. Background Art
[0002] Under natural conditions, the rock mass near the groundwater level in the slope is often in a state of alternating dry and wet conditions; in particular, for the slope on the reservoir bank, the rock mass is often in a state of alternating dry and wet conditions due to rainfall and the rise and fall of the reservoir water level. This alternating dry and wet cycle is more serious than long-term immersion in the rock mass, and is considered "fatigue damage", which will develop cumulatively with the number of cycles.
[0003] When the rock mass is under dry-wet cycle conditions and subjected to confining pressure, the degradation will significantly reduce the overall strength and stability of the rock mass, and will aggravate the attenuation of stress waves in the rock mass. The reduction in rock mass strength and the large amount of wave energy dissipation will cause the rock mass to reach the critical state of collapse more quickly, thus causing geological disasters. Existing research only studies the macroscopic mechanical parameters of rocks under dry-wet cycle conditions or uses CT scanning technology to detect rock damage under conventional environmental conditions, and there is no program specifically for detailed research on slopes. Therefore, how to accurately evaluate the damage performance of slope rock mass or reservoir bank slope under fatigue damage and confining pressure is very important for the geological safety of these areas. Summary of the invention
[0004] In view of the problems existing in the prior art, the purpose of the present invention is to propose a test device and method for rock damage under the action of dry-wet cycle coupled confining pressure. The device can apply confining pressure to the rock mass while subjecting it to dry-wet cycle, simulating the environment and stress of the slope rock mass in actual conditions, thereby more realistically reflecting the damage of the slope rock mass over time; the method can quantify the actual damage process of the slope rock mass, providing an important basis for the study of the damage mechanism of the slope rock mass and the geological disasters therein.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions to achieve it.
[0006] (1) A test device for rock mass damage under dry-wet cycle coupled confining pressure, comprising a test box with an upper opening, the upper end of which is detachably provided with a box cover;
[0007] A rock sample to be tested is placed in the test box, and an isolation plate is horizontally arranged at the upper end of the rock sample to be tested, the isolation plate divides the test box into an upper pressurized area and a lower test area, and the isolation plate is connected to the inner side wall of the test box; a pressurized port and a water inlet are respectively opened on the side walls of the test box; and a vent hole is also opened at the bottom of the test box;
[0008] The pressurizing port is connected to a pressurizing component, and the water inlet is connected to a water supply component via a water pipe.
[0009] The characteristics and further improvements of the technical solution of the present invention are:
[0010] Furthermore, a support plate is sleeved on the middle part of the rock sample to be tested, the support plate is fixedly connected to the inner wall of the test box, and a water-permeable hole is opened on the support plate.
[0011] Furthermore, the support plate is a mesh support plate.
[0012] Furthermore, the isolation plate is a soft rubber plate or a silicone plate.
[0013] Furthermore, the thickness of the isolation plate is 5-10 mm.
[0014] Furthermore, the vent hole is connected to an air pump via a connecting pipe.
[0015] Furthermore, a drain outlet is provided on the connecting pipe.
[0016] Furthermore, a drain port is provided at the bottom of the test box, and the drain port is connected to a drain pipe.
[0017] Furthermore, the pressurizing component includes a boosting pump and an oil tank, the boosting pump is arranged between the pressurizing port and the oil tank, and the pressurizing port, the boosting pump and the oil tank are connected in sequence through an oil pipeline.
[0018] Furthermore, the water supply component includes a water tank and a water pump, the water pump is arranged between the water inlet and the water tank, and the water inlet, the water pump and the water tank are connected in sequence through a water pipe.
[0019] Furthermore, the water pipe, oil pipe, connecting pipe and drainage pipe are respectively provided with switch valves.
[0020] Furthermore, the water pipe and the oil pipe are respectively provided with pressure gauges.
[0021] (II) The test method for rock mass damage under dry-wet cycle coupled confining pressure is based on the above test device and includes the following steps:
[0022] Step 1, placing the rock sample to be tested in a sample box, and installing a box cover to seal the sample box;
[0023] Step 2, fill the test area of the test box with water and keep it for a period of time; then drain the water and continue to introduce air into the test area, during which time the air inside and outside the test box are kept circulating, completing a dry-wet cycle;
[0024] Step 3, according to the confining pressure test conditions required for the test, apply corresponding pressure to the pressurized area of the test box, and at the same time, inject water of corresponding pressure into the test area of the test box to perform confining pressure on the rock sample;
[0025] Step 4: Repeat steps 2 to 3 n times according to the number of dry-wet cycles n required for the test, and obtain the rock sample after n dry-wet cycles coupled with confining pressure;
[0026] Step 5, placing the test box after confining pressure in a CT machine for scanning to obtain a two-dimensional cross-sectional scanning image of the rock sample after confining pressure; based on the two-dimensional cross-sectional scanning image of the rock sample after confining pressure, calculating the damage degree of the rock sample after dry-wet cycle coupled confining pressure.
[0027] Furthermore, the specific formula for calculating the damage degree of the rock sample after the dry-wet cycle coupled confining pressure is:
[0028]
[0029] Among them, H0 is the average CT number of the initial rock sample to be tested, H n is the average CT number of the rock sample after n dry-wet cycles coupled with confining pressure.
[0030] Compared with the prior art, the present invention has the following beneficial effects:
[0031] (1) The present invention can more realistically simulate the dry-wet cycle and confining pressure environment of the slope rock, thereby more realistically reflecting the damage evolution process and damage mechanism of the slope rock;
[0032] (2) The test box of the present invention is light and hand-held. The entire test box can be placed in a CT scanner at any stage of the test to perform microscopic monitoring of rock damage. There is no need to take out the rock sample during the test. The test process is simple and fast with high authenticity, and can reveal the microscopic degradation mechanism of rock degradation under the action of dry-wet cycle coupled confining pressure.
[0033] (3) The present invention studies the degradation law of rock damage due to the number of dry-wet cycles coupled with confining pressure through CT scanning. The damage of rock samples is quantified by design, and a curve relationship between time, dry-wet cycles and damage degree can be produced, thereby revealing the damage law of slope rock samples. Compared with traditional tests, there is no need to prepare multiple groups of samples, and multiple groups of comparative tests can be carried out directly on the same sample, thereby greatly reducing the test cost and time. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0035] Figure 1 It is an overall structural diagram of a test device for rock mass damage under dry-wet cycle coupled confining pressure of the present invention;
[0036] Figure 2 It is a schematic diagram of the three-dimensional structure of the test box and its interior in the present invention;
[0037] Figure 3 A structural diagram of a support plate according to an embodiment of the present invention;
[0038] In the above figure, 1 is the test box; 101 is the box cover; 2 is the rock sample to be tested; 3 is the isolation plate; 4 is the pressurization port; 401 is the oil tank; 402 is the booster pump; 5 is the water inlet; 501 is the water tank; 502 is the water pump; 6 is the air vent; 601 is the air pump; 602 is the connecting pipe; 603 is the drain port; 7 is the support plate; 701 is the water permeable hole; 8 is the pressure gauge. DETAILED DESCRIPTION
[0039] The embodiments of the present invention will be described in detail below with reference to examples, but those skilled in the art will understand that the following examples are only used to illustrate the present invention and should not be construed as limiting the scope of the present invention.
[0040] Example 1
[0041] refer to Figure 1-3 The present invention provides a test device for rock damage under dry-wet cycle coupled confining pressure, comprising a test box 1 with an opening at the upper end, and a box cover 101 is detachably installed on the upper end of the test box 1; a rock sample 2 to be tested is placed in the test box 1, and an isolation plate 3 is horizontally arranged on the upper end of the rock sample 2 to be tested, and the isolation plate 3 divides the test box 1 into an upper pressurization area and a lower test area, and the isolation plate 3 is connected to the inner wall of the test box 1; a pressurization port 4 and a water inlet 5 are respectively opened on the side walls of the test box 1; a vent 6 is also opened at the bottom of the test box 1; the pressurization port 4 is connected to a pressurization component, and the water inlet 5 is connected to a water supply component through a water pipe.
[0042] In the above embodiment, the test box 1 is cylindrical, with an opening at the upper end for easy placement and sampling. The upper end of the test box 1 has an outer edge with screw holes, and the box cover 101 has corresponding screw holes, and the box cover 101 is fixedly connected to the box body of the test box 1 by bolts. In order to ensure the sealing inside the test box 1, a sealing ring is provided at the connection. The pressurizing component and the water supply component are respectively connected to the test box 1 through joints.
[0043] When conducting a dry-wet cycle test, the water provided by the water supply component enters the test area of the test box 1 from the water inlet 5 until the water submerges the rock sample 2 to be tested. After the rock sample 2 to be tested is submerged in water for a certain period of time (such as 24 hours), the water is drained from the vent 6, and then air is introduced from the vent 6 for a certain period of time (such as 24 hours) to air-dry the rock sample in the test box 1, thus completing a dry-wet cycle test; the above process is repeated multiple times to conduct multiple dry-wet cycle tests to simulate the long-term dry-wet alternating erosion process of slope rocks in the natural environment. Confining pressure test: water with a certain pressure is injected into the test box 1 from the water inlet 5 to place the rock sample 2 to be tested under a certain lateral pressure, and then a medium with a certain pressure is injected into the pressurized area of the test box 1 through the pressurization port 4 to place the rock sample 2 to be tested under a certain vertical pressure, thus forming a confining pressure effect to simulate the confining pressure environment of rocks in the natural environment. The pressure during the test is set according to the specific test requirements. The test box 1 of the device is light and hand-held. The entire test box 1 can be placed in a CT scanner at any stage of the test to perform microscopic monitoring of rock damage. There is no need to take out the rock sample during the test. The test process is simple, fast, and highly authentic, and can reveal the microscopic degradation mechanism of rock degradation under the action of dry-wet cycle coupled confining pressure.
[0044] refer to Figure 2 and Figure 3 According to one embodiment of the present invention, a support plate 7 is sleeved on the middle part of the rock sample 2 to be tested, the support plate 7 is fixedly connected to the inner wall of the test box 1, and a water permeable hole 701 is opened on the support plate 7.
[0045] refer to Figure 2 and Figure 3 According to one embodiment of the present invention, the support plate 7 is a mesh support plate 7.
[0046] In the above embodiments, the test area of the test box 1 has a support plate 7 with a central opening, and the test sample is placed on the bottom plate of the test box 1 through the central hole of the support plate 7. The support plate 7 provides lateral support for the test sample to maintain a vertical state during the confining pressure process. The support plate 7 is provided with water-permeable holes 701 or / and is designed to be mesh-shaped, so that it does not affect the immersion process of the test sample while having a supporting function.
[0047] refer to Figure 1 and Figure 2 According to one embodiment of the present invention, the isolation plate 3 is a soft rubber plate or a silicone plate.
[0048] refer to Figure 1 and Figure 2 According to one embodiment of the present invention, the thickness of the isolation plate 3 is 5-10 mm.
[0049] In the above embodiments, during the vertical pressurization process, the isolation plate 3 is a thin soft rubber or silicone plate, which can ensure that the vertical pressure applied by the pressurization area is transmitted to the sample to be tested, thereby ensuring the confining pressure effect on the sample to be tested.
[0050] refer to Figure 1 According to one embodiment of the present invention, the vent hole 6 is connected to an air pump 601 via a connecting pipe 602 .
[0051] refer to Figure 1 According to one embodiment of the present invention, a drain outlet 603 is provided on the connecting pipe 602 .
[0052] In the above embodiment, the vent hole 6 serves as a drain hole and an air inlet of the test box 1. In the drainage stage, the water in the test box 1 is discharged from the drain port 603 through the vent hole 6 via the connecting pipe 602. In the air-drying stage, the air pump 601 inputs air into the test box 1 through the vent hole 6 to simulate the air-drying process in nature.
[0053] refer to Figure 1 According to one embodiment of the present invention, a drain port 603 is further provided at the bottom of the test box 1 , and the drain port 603 is connected to a drain pipe.
[0054] In the above embodiment, the drain port 603 and the air inlet of the test box 1 are separated, and another drain port 603 is provided at the bottom of the test box 1, so that the drain port 603 can be used as an air outlet during the air-drying stage to accelerate the internal air circulation.
[0055] refer to Figure 1 According to one embodiment of the present invention, the pressurizing component includes a boosting pump 402 and an oil tank 401, and the boosting pump 402 is arranged between the pressurizing port 4 and the oil tank 401, and the pressurizing port 4, the boosting pump 402 and the oil tank 401 are connected in sequence through an oil pipeline.
[0056] refer to Figure 1 According to one embodiment of the present invention, the water supply component includes a water tank 501 and a water pump 502, the water pump 502 is arranged between the water inlet 5 and the water tank 501, and the water inlet 5, the water pump 502 and the water tank 501 are connected in sequence through a water pipe.
[0057] refer to Figure 1 According to one embodiment of the present invention, the water pipe, the oil pipe, the connecting pipe 602 and the drainage pipe are respectively provided with switch valves.
[0058] refer to Figure 1 According to one embodiment of the present invention, pressure gauges 8 are respectively provided on the water pipe and the oil pipe.
[0059] In the above embodiment, the pressurized medium is oil, and the booster pump 402 is used to pump the oil in the oil tank 401 to the pressurized area of the test box 1 at a certain pressure to apply vertical pressure to the sample to be tested. Similarly, the water pump 502 is used to apply lateral pressure; the pressure gauge 8 is used to monitor the pressure. The switch valve is used to control the inflow of various media.
[0060] Example 2
[0061] The test method for rock mass damage under dry-wet cycle coupled confining pressure is based on the above test device. This embodiment studies the damage law and degradation mechanism of sandstone under 1, 5, 10, and 15 dry-wet cycle coupled confining pressure. The rock material is selected from sandstone of the same origin and good quality, and is processed into a cylindrical specimen with a diameter of 50 mm and a height of 100 mm.
[0062] The test method includes the following steps:
[0063] Step 1, placing the rock sample to be tested in a sample box, and installing a box cover to seal the sample box;
[0064] Step 2: Fill the test area of the test box with water and keep it for 24 hours; then drain the water and continue to let air flow into the test area for 24 hours, during which time the air inside and outside the test box are kept circulating to complete a dry-wet cycle;
[0065] Step 3, according to the confining pressure test conditions required for the test, a pressure of 5 MPa is applied to the pressurized area of the test box, and at the same time, water of corresponding pressure (5 MPa) is injected into the test area of the test box to perform confining pressure on the rock sample;
[0066] Step 4: Repeat steps 2 to 3 n times according to the number of dry-wet cycles n required for the test, and obtain the rock sample after n dry-wet cycles coupled with confining pressure;
[0067] Step 5, placing the test box after confining pressure in a CT machine for scanning to obtain a two-dimensional cross-sectional scanning image of the rock sample after confining pressure; based on the two-dimensional cross-sectional scanning image of the rock sample after confining pressure, calculating the damage degree of the rock sample after dry-wet cycle coupled confining pressure.
[0068] The initial rock samples to be tested and the rock samples under 1, 5, 10, and 15 dry-wet cycle coupled confining pressure were placed in the Toshiba Aquilion16 spiral CT machine for scanning, and then three-dimensional reconstruction was performed using the image processing software MIMICS to intuitively display the development of pores in the rock and store the three-dimensional image of the sandstone sample. The average CT number automatically displayed by the Toshiba Aquilion16 spiral CT machine after each dry-wet cycle coupled confining pressure was recorded, and the corresponding damage degree was calculated according to the following formula:
[0069]
[0070] Among them, H0 is the average CT number of the initial rock sample to be tested, H n is the average CT number of the rock sample after n dry-wet cycles coupled with confining pressure.
[0071] The three-dimensional images of sandstone samples after 1, 5, 10, and 15 dry-wet cycle coupled confining pressures were compared to qualitatively analyze the degradation mechanism of rock pores under dry-wet cycle coupled confining pressure. The damage degree D of sandstone samples after 1, 5, 10, and 15 dry-wet cycle coupled confining pressures was obtained. n The relationship curve between the number of dry-wet cycle coupled confining pressure actions and the number of dry-wet cycle coupled confining pressure actions reveals the law of rock damage caused by repeated dry-wet cycle coupled confining pressure actions.
[0072] Example 3
[0073] The test method for rock damage under dry-wet cycle coupled confining pressure is based on the above test device. This embodiment studies the microscopic degradation mechanism of rock with filled joints under 1, 10, 20, and 30 dry-wet cycle coupled confining pressure. Artificially prepared rock with filled joints is used. The rock material is granite with good texture from the same origin. The filling material is lime mortar (ratio of water: lime: sand = 1:1:3), and the filling thickness is 5mm. Processed into a cylindrical specimen with a diameter of 50mm and a height of 100mm.
[0074] The test method includes the following steps:
[0075] Step 1, placing the rock sample to be tested in a sample box, and installing a box cover to seal the sample box;
[0076] Step 2: Fill the test area of the test box with water and keep it for 36 hours; then drain the water and continue to let air flow into the test area for 36 hours, during which time the air inside and outside the test box are kept circulating to complete a dry-wet cycle;
[0077] Step 3, according to the confining pressure test conditions required for the test, apply a pressure of 8 MPa to the pressurized area of the test box, and at the same time, inject water of corresponding pressure (5 MPa) into the test area of the test box to perform confining pressure on the rock sample;
[0078] Step 4: Repeat steps 2 to 3 n times according to the number of dry-wet cycles n required for the test, and obtain the rock sample after n dry-wet cycles coupled with confining pressure;
[0079] Step 5, placing the test box after confining pressure in a CT machine for scanning to obtain a two-dimensional cross-sectional scanning image of the rock sample after confining pressure; based on the two-dimensional cross-sectional scanning image of the rock sample after confining pressure, calculating the damage degree of the rock sample after dry-wet cycle coupled confining pressure.
[0080] The initial rock samples to be tested and the rock samples under 1, 10, 20, and 30 dry-wet cycle coupled confining pressure were placed in the Toshiba Aquilion16 spiral CT machine for scanning, and then three-dimensional reconstruction was performed using the image processing software MIMICS to intuitively display the development of pores in the rock and store the three-dimensional image of the sandstone sample. The average CT number automatically displayed by the Toshiba Aquilion16 spiral CT machine after each dry-wet cycle coupled confining pressure was recorded, and the corresponding damage degree was calculated according to the following formula:
[0081]
[0082] Among them, H0 is the average CT number of the initial rock sample to be tested, H n is the average CT number of the rock sample after n dry-wet cycles coupled with confining pressure.
[0083] The three-dimensional images of sandstone samples after 1, 10, 20, and 30 dry-wet cycle coupled confining pressures are compared to qualitatively analyze the degradation mechanism of rock pores under dry-wet cycle coupled confining pressure. The damage degree D of sandstone samples after 1, 10, 20, and 30 dry-wet cycle coupled confining pressures is obtained. n The relationship curve between the number of dry-wet cycle coupled confining pressure actions and the number of dry-wet cycle coupled confining pressure actions reveals the law of rock damage caused by repeated dry-wet cycle coupled confining pressure actions.
[0084] Although the present invention has been described in detail in general terms and in specific embodiments in this specification, it is obvious to those skilled in the art that some modifications or improvements may be made to the present invention. Therefore, these modifications or improvements made without departing from the spirit of the present invention all fall within the scope of protection claimed by the present invention.
Claims
1. The test device for rock damage under dry-wet cycle coupled confining pressure is characterized by: A test box with an open upper end is provided, wherein a box cover is detachably mounted on the upper end of the test box; A rock sample to be tested is placed in the test box, and an isolation plate is horizontally arranged at the upper end of the rock sample to be tested, the isolation plate divides the test box into an upper pressurized area and a lower test area, and the isolation plate is connected to the inner side wall of the test box; a pressurized port and a water inlet are respectively opened on the side walls of the test box; and a vent hole is also opened at the bottom of the test box; The pressurizing port is connected to a pressurizing component, and the water inlet is connected to a water supply component via a water pipe; The pressurizing component comprises a booster pump and an oil tank. The booster pump is arranged between the pressurizing port and the oil tank. The pressurizing port, the booster pump and the oil tank are connected in sequence through an oil delivery pipe.
2. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 1 is characterized in that: A support plate is sleeved on the middle part of the rock sample to be tested. The support plate is fixedly connected to the inner wall of the test box, and a water-permeable hole is opened on the support plate.
3. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 2 is characterized in that: The support plate is a mesh support plate.
4. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 3 is characterized in that: The isolation plate is a soft rubber plate or a silica gel plate.
5. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 4 is characterized in that: The thickness of the isolation plate is 5-10 mm.
6. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 1 is characterized in that: The vent hole is connected to an air pump via a connecting pipe, and a drain port is arranged on the connecting pipe.
7. The test device for rock damage under dry-wet cycle coupled confining pressure according to claim 1 is characterized in that: The water supply component comprises a water tank and a water pump. The water pump is arranged between the water inlet and the water tank. The water inlet, the water pump and the water tank are connected in sequence through a water pipe.
8. A test method for rock mass damage under dry-wet cycle coupled confining pressure, based on the test device according to any one of claims 1 to 7, characterized in that: The following steps are involved: Step 1, placing the rock sample to be tested in a sample box, and installing a box cover to seal the sample box; Step 2, fill the test area of the test box with water and keep it for a period of time; then drain the water and continue to introduce air into the test area, during which time the air inside and outside the test box are kept circulating, completing a dry-wet cycle; Step 3, according to the confining pressure test conditions required for the test, apply corresponding pressure to the pressurized area of the test box, and at the same time, inject water of corresponding pressure into the test area of the test box to perform confining pressure on the rock sample; Step 4: Repeat steps 2 to 3 n times according to the number of dry-wet cycles n required for the test, and obtain the rock sample after n dry-wet cycles coupled with confining pressure; Step 5, placing the test box after confining pressure in a CT machine for scanning to obtain a two-dimensional cross-sectional scanning image of the rock sample after confining pressure; based on the two-dimensional cross-sectional scanning image of the rock sample after confining pressure, calculating the damage degree of the rock sample after dry-wet cycle coupled confining pressure.
9. The test method for rock mass damage under dry-wet cycle coupled confining pressure according to claim 8 is characterized in that: The specific formula for calculating the damage degree of the rock sample after the dry-wet cycle coupled confining pressure is: Among them, H0 is the average CT number of the initial rock sample to be tested, H n is the average CT number of the rock sample after n dry-wet cycles coupled with confining pressure.
Citation Information
Patent Citations
Testing device for rock mass damage under dry-wet cycle coupling confining pressure effect
CN214503181U