System and method for suppressing defects, metal particle contamination and film growth on wafers
By using self-assembled monolayer (SAM) and actinic radiation technology on semiconductor wafers, the problem of metal contamination and defects in semiconductor manufacturing of metal-containing materials is solved, more efficient edge and backside protection is achieved, and manufacturing quality is improved.
Patent Information
- Application Number
- CN201980074237.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-11-13
- Filing Date
- 2019-11-12
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-11-12
AI Technical Summary
In the manufacturing process of semiconductor wafers, when using metal-containing materials, there are problems of metal contamination and defects. The existing technology is difficult to effectively prevent the adhesion of metal particles and optical materials, resulting in high edge and back defect rates, and conventional technology is difficult to prevent the material Not very effective cumulatively.
Using a self-assembled monolayer (SAM) as a barrier layer, the area of interest is exposed to actinic radiation, allowing the SAM to be removed in the target area, leaving a hydrophobic layer on the remaining surface of the substrate to prevent the adhesion of metals and other contaminants , and selectively remove the SAM layer during downstream processing.
It effectively prevents metal contamination and unnecessary film growth, improves the defect rate on the edge and back of the wafer, provides a cleaner edge process, and improves the quality of semiconductor manufacturing.
Smart Images

Figure CN112997292B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of priority to U.S. Provisional Application No. 62 / 760,589, filed on November 13, 2018, the entire contents of which are incorporated herein by reference. Background Art
[0003] This disclosure relates to microfabrication of semiconductor wafers. Silicon wafers are processed to make integrated circuits and other semiconductor devices. Semiconductor manufacturing involves many different steps of deposition, growth, patterning, removal, and cleaning of wafers. Various different materials are added and removed or partially removed while other materials remain. Various process controls attempt to prevent defects and contamination. Summary of the invention
[0004] In one aspect, the present disclosure relates to a method of processing a substrate. The method includes: receiving a substrate having a front side surface, a back side surface, and a side edge surface; coating the front side surface, the back side surface, and the side edge surface with a self-assembled monolayer; exposing a region of interest by actinic radiation, the actinic radiation causing a deprotection reaction within the self-assembled monolayer in the central region; and removing the self-assembled monolayer from the region of interest while retaining the self-assembled monolayer on the remaining surface of the substrate.
[0005] In one aspect, the method for processing a substrate includes: receiving a substrate having a front surface, a back surface, and a side edge surface; coating a target area of the front surface with a sacrificial film, the sacrificial film having a surface that prevents a specific material from adhering to the target area; coating the front surface, the back surface, and the side edge surface with a self-assembled monolayer, the self-assembled monolayer cannot adhere to the sacrificial film, and the self-assembled monolayer is hydrophobic; and removing the sacrificial film from the target area of the front surface.
[0006] In one aspect, the method for processing a substrate includes: receiving a substrate having a front surface, a back surface, and a side edge surface; coating a target area of the front surface with a sacrificial film; coating the front surface, the back surface, and the side edge surface with a self-assembled monolayer, the self-assembled monolayer being hydrophobic; and removing the sacrificial film from the target area of the front surface, wherein removing the sacrificial film also removes the self-assembled monolayer attached to the sacrificial film, thereby leaving the target area free of the self-assembled monolayer.
[0007] It should be noted that the Summary of the Invention section does not specify all embodiments and / or incremental novel implementation aspects of the disclosure or claimed invention. Instead, the Summary of the Invention only provides a preliminary discussion of different embodiments and corresponding points of novelty compared to conventional techniques. For additional details and / or possible viewpoints of the present invention and embodiments, the reader should consult the Detailed Description section of the disclosure and corresponding drawings as further discussed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1A is a schematic diagram showing a side view of a substrate according to one example.
[0009] Figure 1B is a schematic diagram showing a top view of a substrate according to an example.
[0010] Figure 2 is a schematic diagram showing a process flow according to one example.
[0011] Figure 3 is a schematic diagram showing the process flow of a self-assembled monolayer (SAM) inhibition according to one example.
[0012] Figure 4 is a flow chart of a method for suppressing defects, metal particle contamination, and film growth on a substrate according to one example.
[0013] Figure 5 is a schematic diagram illustrating an exemplary method for SAM removal according to one example.
[0014] Figure 6 is a schematic diagram illustrating another exemplary method for SAM removal according to an example.
[0015] Figure 7 is a schematic diagram illustrating another exemplary method for SAM removal according to an example.
[0016] Figure 8 is a schematic diagram showing an exemplary structure of a SAM material according to one example.
[0017] Fig. 9 is a schematic diagram showing a hydrocarbon chain SAM layer according to one example.
[0018] Fig.10 is a schematic diagram showing a fluorinated chain SAM layer according to one example. DETAILED DESCRIPTION
[0019] Referring now to the accompanying drawings, in which the same reference numerals represent the same or corresponding parts throughout the several views, the following description relates to a system and associated methods for preventing contamination by using a self-assembled monolayer coating. However, the technology described herein provides a coating process that can use metal-containing materials while preventing contamination, defects, and unnecessary film growth from these materials. The technology includes selectively applying and removing a self-assembled monolayer (SAM) as a barrier layer. The technology may include controlling the amount of SAM deposition and the amount of SAM removal.
[0020] Metal contamination on semiconductor wafers is a particular challenge when applying advanced photo-patternable materials and etch stop layers containing metals. These metal-containing materials can be used to produce high-resolution patterns on wafers and enable 3D logic, extreme ultraviolet lithography (EUV) and other advanced patterning schemes within optical lithography. However, using metal-containing materials is challenging due to the possibility of contamination.
[0021] Single and multi-module approaches exist to limit metal contamination by selectively blocking the adhesion of metal particles and metal-containing photomaterials (e.g., photoresists, bottom anti-reflective coatings (BARCs), metal-containing hard masks (MHMs)) through both additive and subtractive approaches. An additional impact of this process is an attempt to provide a cleaner edge process to improve defectivity at the wafer edge and backside using conventional materials currently available for production.
[0022] Conventional techniques for controlling edge and backside defectivity are less effective in preventing material accumulation. For example, edge coatings that create sacrificial layers can retain defects on the wafer. In addition, less effective spin-on material coatings can result in edge coating barriers, which can degrade coating performance.
[0023] Figure 1A is a schematic diagram showing a side view of a substrate 100 according to an example. The substrate 100 may include a front side surface 102 (ie, a working surface), a back side surface 104, and a side edge surface 106. In an example, the substrate 100 is disc-shaped and relatively thin. Figure 1B 1 shows a top view of the substrate 100. The edge region 108 of the front side surface 102 is an annular region extending a predetermined distance from the periphery of the front side surface toward the center point of the front side surface. The predetermined distance can be in the range of 1 mm to 5 mm. The annular region or the first annular region can be adjacent to the periphery of the substrate. The first annular region has a first outer periphery close to the periphery of the substrate and a first inner periphery away from the periphery of the substrate. In an example, the edge region 108 corresponds to a region in which no active devices are built.
[0024] Therefore, the technology herein includes a method for forming a protective film on a selected portion of a semiconductor substrate (wafer). In one embodiment, a specific SAM is coated on a substrate. As previously described herein, the substrate may include a front side surface (working surface) and a back side surface, as well as a side edge surface. Typically, such a substrate is disc-shaped and relatively thin. An initial SAM coating is formed on the substrate. The initial SAM coating may cover all surfaces, i.e., the front side surface, the back side surface, and the side surface. Such a monomer coating may be applied, for example, using vapor deposition or other deposition techniques. By way of non-limiting example, the deposition conditions may be a vacuum or atmospheric chamber from ambient temperature to 300 degrees Celsius. Depending on the type of coating applied and the intended application, the deposition conditions may be adjusted outside this range. The reaction with halogens may form HCl (hydrochloric acid), while the reaction with OH (hydroxyl) may form water. When silicon terminates with SiO, the attached moisture may stabilize the surface of SiOH. After the initial deposition of the SAM, the substrate may be rinsed to remove any unbound polymer or monomer material.
[0025] In the case where the substrate is fully coated, light is projected onto a specific target area. For example, a common substrate can have a circular and flat working surface (front side surface). The projection target area can be a circle with a diameter less than the outer diameter of the working surface, thereby leaving an outer ring that is not exposed to actinic radiation on the working surface. Exposure can be performed via a mask-based projection system or a maskless projection system. The SAM film can then be developed with a solvent or alkali according to the composition of the selected SAM, or light can be used to fractionate a portion of the molecule and leave it as a small molecule at atmospheric pressure or low pressure. Therefore, actinic exposure can cause partial photooxidation of the SAM molecules, which can then be washed out in a polar solvent.
[0026] Areas not exposed to actinic radiation can keep the complete SAM intact and adhere to the substrate. These areas can include the back surface, the side surface, and the peripheral edge of the front surface. Therefore, these areas remain hydrophobic. Depending on the physical properties of the specific substrate surface, the portion of the substrate not covered by the SAM can be hydrophilic. The result is that the substrate is protected except for the active area of interest on the working surface. The remaining surface of the substrate can be protected from atomic layer deposition (ALD) and chemical vapor deposition (CVD), solvent wetting, deionized water (DIW) wetting, and polymer adhesion. For this inhibition process, the initial ALD growth can be optimized, such as by not using ozone or oxygen plasma.
[0027] The superhydrophobic surface remains on the extreme edge of the front side surface of the substrate, but the remaining layer can be removed for downstream processing after processing materials with the risk of generating defects (materials containing metals or other contaminants). The surface where the chemical decomposition area exists can be modified to be hydrophobic or hydrophilic to adapt to direct coating to improve adhesion, thereby replacing the existing vapor phase priming process or surface passivation layer. The surface chemical reaction can be generated by utilizing a "click chemistry" reaction.
[0028] Figure 2 2 is a schematic diagram showing a process flow according to an example. At step 200, a monomer coating can be applied using vapor deposition at a temperature from room temperature to 300°C in a vacuum or atmospheric pressure. The substrate 100 has an initial self-assembled monolayer (SAM) coated on the front side surface 102 of the substrate 100, on the back side surface 104 of the substrate 100, and on the side edge surface 106 of the substrate 100. After the gas phase SAM is attached, the substrate 100 can be rinsed to remove any unbound polymer. Step 202 shows the substrate 100 after being exposed to light in a specific target area. Then, as will be understood by a person of ordinary skill in the art, the film can be developed in a solvent or alkali. This causes partial photooxidation of the SAM molecules. Step 204 shows the substrate after rinsing the substrate 100 to wash away any polar solvents. At step 206, the substrate 100 has two zones: a first zone 208 and a second zone 210. The first zone 208 has a modified coating. In the first area 208 (or exposed area), most of the polymer chains are removed and the remaining components are hydrophilic. Due to the type of barrier material, no coating or deposition occurs in the second area 210. SAM attachment causes the area where the SAM is not in contact with the alkane chain to extend outward in the second area 210. The second area 210 is hydrophobic. On the second area 210 (or non-exposed area), ALD / CVD deposition, solvent wetting, DIW wetting, and polymer adhesion are inhibited.
[0029] Figure 3 is a schematic diagram showing a SAM suppression process flow according to an example. Exposure can be controlled using a control knob or the like. Controlling exposure can adjust SAM loss, which in turn is related to a foothold for controllable nucleation suppression or improvement. As shown in steps 302 to 310, as the dose increases, more SAM is suppressed and more atomic layer deposition (ALD) molecules are formed on the surface of substrate 100.
[0030] The quantum efficiency may be lower, but this provides a linear process window to achieve controlled removal of the SAM. High dose / flux can be matched to the deposition tool. Any of a variety of wavelengths can be selected depending on the monomer composition. In one example, the wavelength can be in the range of 170nm to 400nm.
[0031] Figure 4 4 is a flow chart of a method 400 for inhibiting defects, metal particle contamination, and film growth on a substrate according to an example. At step 402, photosensitive molecules are attached to the entire surface of substrate 100 by vapor deposition to produce a super hydrophobic surface. For example, certain SAMs can be formed to have a non-wetting surface to prevent liquid adhesion. Such surfaces can be described as hydrophobic. Specifically, such surfaces can have a surface contact angle in a range that repels water or otherwise prevents water and certain other liquids (including some solvents) from adhering.
[0032] At step 404, light of a specific energy is applied to the region of interest or target area to release molecules from the surface of the region of interest or target area. The corresponding molecules decompose when interacting with the projected light.
[0033] At step 406, the region of interest is further processed, as further described below. For example, a photochemical or film (e.g., photoresist, BARC, organic planarization layer (OPL), metal-containing film, oxide, nitride) can be applied to the surface where the molecules were removed or broken. Where the molecules were not removed, the film and coating will be repelled and will not adhere.
[0034] Figure 5 The front side surface and back side surface of substrate 100 at different steps of the process are shown. 502 shows the front side surface of silicon substrate, and 504 shows the back side surface of silicon substrate. In one embodiment, a vapor deposition process that allows attachment to the entire surface of the substrate or wafer is used to apply a polytetrafluoroethylene SAM (self-assembled monolayer) containing chromophores at high density. 506 and 508 respectively show the front side surface and back side surface of substrate 100 after SAM deposition. Except for the peripheral edge that needs to be protected from metal and defect effects, the front side surface of the wafer can be exposed to actinic radiation, as described later in this article. 510 and 512 show the front side surface and back side surface of the substrate after exposure. The SAM layer is exposed to radiation to release a portion of the molecules attached to the chromophore and avoid adhesion to the surface, and can be removed or volatilized and removed in a vacuum. The coating of the subsequent metal-containing material will not adhere to the wafer edge. In the case of spin-cast metal-containing materials, the residual droplets can be removed with high efficiency without damaging the wafer surface using conventional semiconductor solvents or strong acids and bases. In the case of metal films, nitrides, oxides, etc. deposited by atomic layer deposition (ALD), the surface is passivated and the surface chemistry required for ALD-type reactions does not occur at this location. Schematic diagrams 514 and 516 show the front side surface and the back side surface of the substrate 100 after downstream processing.
[0035] In another embodiment, light projection hardware is used to deliver a light dose to an area of interest (e.g., a central region of a substrate) on a substrate (or wafer) to photodissociate the self-assembled monolayer. An example material that can be selected is a 365nm chromophore nitrobenzyl group. In another example, the selected 266nm chromophore has a Si-O-Si bond on the wafer surface. A barrier (hydrophobic) SAM is vapor-coated onto the entire substrate, and then the center portion is removed from the front side of the wafer, leaving a ring around the edge portion of the wafer. Subsequently, downstream processes can be performed with the top edge and bottom portions of the wafer protected.
[0036] Subsequent coatings of metal-containing materials will not adhere to the wafer edge because the material is still being modified at unexposed locations (e.g., the edge of the substrate). In the case of spin-cast metal-containing materials, residual droplets will be easily rinsed off with conventional semiconductor solvents. In the case of metal-containing films, the surface is passivated and the surface chemistry required for ALD-type reactions will not occur in the unexposed areas.
[0037] In another embodiment, the techniques described herein use light projection hardware to deliver a light dose to a region of interest in order to desorb entire molecules in the region of interest (eg, a central region of a substrate). Figure 6 602 and 604 show the front and back surfaces of a silicon substrate. 606 and 608 show the front and back surfaces with a vapor-coated barrier SAM layer. 610 shows an area of interest or target area exposed to 266 nm light. 612 shows the back surface of the substrate that was not exposed to 266 nm light. Subsequent coatings of metal-containing materials will not adhere to the wafer edge because the material has not yet desorbed from the unexposed areas as shown by 614 and 616. In the case of a spin-cast metal-containing material, residual droplets will be easily rinsed off with conventional semiconductor solvents, while in the case of a metal-containing film, the surface is passivated and the surface chemistry required for ALD-type reactions will not occur in the unexposed areas.
[0038] In another embodiment, the technology described herein uses a sacrificial layer of material such as a non-crosslinked photoresist, BARC, or thin film polymer to block the center portion of the wafer to the edge area. The method includes first selectively depositing or forming a sacrificial polymer layer before coating the wafer with a blocking SAM. Figure 3 , a sacrificial polymer layer is formed in the device area of the substrate. The device area may be the working surface of the wafer when the semiconductor device is formed. Basically, the circular area is slightly smaller than the diameter of the front side surface of the substrate. The diameter of the sacrificial polymer layer may be a few millimeters to a few centimeters smaller than the diameter of the front side surface of the substrate. The sacrificial polymer layer basically serves to prevent the hydrophobic SAM from being coated in this area.
[0039] When performing vapor coating deposition of a barrier SAM, a monomer coating is applied to all surfaces of the substrate (except for the area containing the sacrificial polymer). The SAM is essentially coated on the backside surface, on the side edge surface, and on the outer ring of the front side surface. The sacrificial polymer layer can then be removed, leaving the SAM protection area of the substrate (except for the active device formation area).
[0040] Figure 7 702 and 704 respectively show the front side surface and the back side surface of the silicon substrate. 706 and 708 show the front side surface and the back side surface of the substrate after a sacrificial polymer layer is deposited or formed on the substrate. Figure 7 As shown in (706), only the target area is covered by the sacrificial polymer layer. The remaining unblocked edge surface (greater than 145nm, depending on the chip manufacturer) is treated with a photoresponsive SAM such as polytetrafluoroethylene to prevent coating adhesion and / or film formation. 710 and 712 show the front and back surfaces of the substrate after treatment with the SAM. The sacrificial polymer in the center portion of the wafer is then removed using solvent wet stripping, leaving a resistive coating. 714 shows the front surface of the substrate after the sacrificial polymer layer is removed. The SAM surface is at the extreme edge portion of the working surface. Subsequent coatings of metal-containing materials will not adhere to the edge of the wafer, as shown in 718. In addition, subsequent coatings will not adhere to the back surface of the substrate, as shown by 716 and 720. In the case of spin-cast metal-containing materials, residual droplets can be easily rinsed off with conventional semiconductor solvents. In the case of metal-containing films, the surface is passivated and the surface chemistry required for ALD-type reactions does not occur at this location.
[0041] After optional chromophore removal or modification, several options are available for subsequent processing. One embodiment includes removing the non-stick portion of the molecule (SAM) and then using the remaining material in place of the hexamethyldisilazane (HMDS) chemistry as a tackifier. A given non-stick click molecule can be replaced with a different end to modify the surface contact angle, thereby improving bottom release of the developer. The entire molecule at the silicon surface in the exposed area can be removed. Highly selective chemistries (Si-containing chemistries, metal oxides, TEOS (tetraethyl orthosilicate)-like) can be altered to behave as an etch hard mask. Also, after removing the coating barrier portion, the wafer adsorbing portion of the molecule can be cross-linked at 365nm for high temperature applications.
[0042] Note that a variety of materials may be used to perform the techniques herein. Figure 8An example material that can be used herein is shown. SAM 800 is an organized assembly of molecules arranged at the interface between two phases of a substance. An example SAM 800 (or molecule) design can have a head 802 (or head group), a cleavable group 804, and a tail 806 (or tail group or inhibitor). The head 802 is positioned toward the interface, while the tail 806 is positioned away from the interface.
[0043] Head 802 can be any suitable chemical, including trichloro-mono-hydroxy-dithiolane. Cleavable group 804 can be nitrobenzyl-based, carbonyl-based or benzyl-based. Cleavable group 804 can be selected based on wavelength.
[0044] Tail 806 can be a relatively long inert straight chain hydrocarbon portion. Tail 806 includes a fully or partially fluorinated hydrocarbon chain oriented away from the interface. Tail 806 can include alkanes with a length of 2-30 carbons. Tail 806 can include additional branches and have different shapes.
[0045] The length of the deposited SAM precursor molecules can vary depending on the application and can determine or control the thickness (height) of the network solid on the substrate. For some applications, a thickness of 0.5 nm to 1.5 nm is preferred.
[0046] Fig. 9 Further illustrated are exemplary molecules that can be used herein. Molecules 902 and 904 are hydrocarbon chains. Molecule 902 shows the structure of 2-nitrobenzyl, 3-(11-mercaptoundecanoate), 5-undecane. Molecule 904 is 2-nitrobenzyl-(11-trichlorosilyl)-undecanoate.
[0047] Fig.10 Further exemplary molecules that can be used herein are shown. Molecules 1002 and 1004 show examples of fluorinated chains. Specifically, molecule 1002 is 2-nitrobenzyl, 3-(11-fluoromercaptoundecanoate), 5-undecane. Molecule 1004 is 2-nitrobenzyl-(11-trichlorosilyl)-fluoroundecanoate.
[0048] In one example, 2-nitrobenzyl 11-(trichlorosilyl) undecanoate can be synthesized as follows. The reaction is preferably performed under dark conditions. For example, aluminum foil can be used to exclude light from the reaction.
[0049] In the first step, 2.0 g (9.9 mmol) of undecyl-10-enoyl chloride was added to a solution of 1.68 g (10.9 mmol) (2-nitrophenyl) methanol. A solution of (2-nitrophenyl) methanol was obtained by dissolving methanol in a mixture of 0.88 ml (10.9 mmol) pyridine and 40 ml of dichloromethane. The reaction was stirred at ambient temperature for 48 hours until complete conversion was observed. The organic layer was extracted with 3 × 20 mL of 5% hydrochloric acid solution to remove excess pyridine and 20 mL of saturated sodium bicarbonate solution, then dried over sodium sulfate. The solvent was removed in vacuo, and then separated using a cyclohexane / ethyl acetate (8: 1) column to purify the product. 2.63 g of a white substrate was obtained with 83% of theoretical yield.
[0050] In the second step, 1.0 g (7.4 mmol) of trichlorosilane was added to a solution of 1.0 g (3.1 mmol) of (2-nitrobenzyl undec-10-enoate) dissolved in 5 ml of dichloromethane. As a catalyst, hexachloroplatinic acid was used. The reaction was stirred at ambient temperature for 24 hours until complete conversion was observed.
[0051] Exemplary yield: 1.38 g of white pale yellow liquid (97.3% of theory).
[0052] In other embodiments, hyperbranched carbon materials may be used as both the hydrophobic material and the fluorinated material.
[0053] In other embodiments, bifunctional photoreactive chromophores may be used. Two-photon deprotection can be achieved with a 780 nm laser, providing access to near-field sensing patterning.
[0054] One embodiment includes a method of processing a substrate. A substrate (such as a silicon wafer) can be received or transferred into a processing chamber. The substrate has a front side surface, a back side surface, and a side edge surface. The substrate can include bevels, notches, etc. The front side surface, the back side surface, and the side edge surface are coated with a self-assembled monolayer. The self-assembled monolayer is hydrophobic (or at least has an initial state of being hydrophobic). Note that subsequent processing of the substrate and exposure to other chemicals and species can degrade, change, or modify the initial surface energy to a second surface energy that can be more or less hydrophobic. The self-assembled monolayer can be a fluorinated material, a hyperbranched carbonaceous material, or other hydrophobic material.
[0055] A central region of the front surface is exposed by actinic radiation. The surface area of the central region is smaller than the surface area of the front surface. The actinic radiation causes a deprotection reaction with the self-assembled monolayer in the central region. For example, the self-assembled monolayer may include a chromophore or other additive that is reactive to a predetermined wavelength of light. The self-assembled monolayer is then removed from the central region of the front surface, while the self-assembled monolayer is retained on the remaining surface of the substrate. In other words, the entire wafer is coated with a hydrophobic film, and then the film is selectively removed from a portion of the working surface, leaving a circle of hydrophobic material on the edge of the working surface.
[0056] In the case where the central region of the substrate is not covered with the hydrophobic coating, and the remainder of the substrate is covered with the hydrophobic coating, further processing can continue. For example, a metal-containing film can be deposited on the substrate by spin coating deposition. This allows the metal-containing film to adhere to the uncovered central region, but not adhere (or adhere at all) to the surface coated with the self-assembled monolayer.
[0057] In other embodiments, the substrate can first make a sacrificial film formed on the inner area of the substrate, for example, so that the periphery of the working surface will not be covered by the sacrificial film. The sacrificial film can be selected to optionally prevent the adhesion of the self-assembled monolayer or accept the adhesion of the self-assembled monolayer. If the given sacrificial film used prevents the adhesion of the self-assembled monolayer, then the entire substrate can be coated with a SAM that coats other surfaces but cannot adhere to the sacrificial film. The sacrificial film can then be removed to expose the inner area of the working surface. Alternatively, if the given sacrificial film used accepts the adhesion of the SAM, the hydrophobic self-assembled monolayer is coated on all surfaces of the substrate (including the sacrificial film). Subsequently, the sacrificial film is removed or peeled off from the substrate, which removes the self-assembled monolayer material that adheres to the sacrificial film in the process. This makes the inner area no longer covered by the sacrificial film or the self-assembled monolayer, and the remaining surface of the substrate is still covered by the hydrophobic material.
[0058] Of course, for the sake of clarity, the order of discussion of the different steps described herein has been proposed. Generally, these steps can be performed in any suitable order. In addition, although each different feature, technology, configuration, etc. in this article may be discussed in different places of the present disclosure, it is intended that each concept can be performed independently of each other or in combination with each other. Therefore, the present invention can be implemented and viewed in many different ways.
[0059] In the foregoing description, specific details have been set forth, such as the specific geometry of the processing system and the description of the various components and processes used therein. However, it should be understood that the technology herein can be practiced in other embodiments that are separated from these specific details, and these details are for the purpose of explanation rather than limitation. The embodiments disclosed herein have been described with reference to the accompanying drawings. Similarly, for the purpose of explanation, specific numbers, materials, and configurations have been proposed in order to provide a thorough understanding. However, embodiments may be practiced without these specific details. Components having substantially the same functional structure are represented by similar reference numerals, and therefore any redundant description may be omitted.
[0060] Various techniques have been described as multiple independent operations to help understand various embodiments. The order of description should not be interpreted as meaning that these operations must be dependent on the order. In fact, these operations do not need to be performed in the order presented. The described operations can be performed in an order different from the described embodiments. In additional embodiments, various additional operations can be performed and / or the described operations can be omitted.
[0061] As used herein, "substrate" or "target substrate" generally refers to an object to be processed according to the present invention. A substrate may include any material portion or structure of a device (particularly a semiconductor or other electronic device), and may be, for example, a base substrate structure (such as a semiconductor wafer, a mask), or a layer (such as a thin film) on or overlying a base substrate structure. Thus, a substrate is not limited to any particular base structure, underlying layer, or overlying layer, patterned or unpatterned, but is contemplated to include any such layer or base structure, and any combination of layers and / or base structures. The description may refer to a specific type of substrate, but this is for illustrative purposes only.
[0062] Those skilled in the art will also appreciate that many changes may be made to the operation of the above-mentioned techniques while still achieving the same purpose of the present invention. The scope of this disclosure is intended to include these changes. Therefore, the foregoing description of the embodiments of the present invention is not intended to be restrictive. On the contrary, any limitation to the embodiments of the present invention is presented in the appended claims.
Claims
1. A method for processing a substrate, the method comprising: a receiving substrate having a front side surface, a back side surface, and side edge surfaces; coating the front side surface, the back side surface and the side edge surface with a self-assembled monolayer (SAM); exposing the region of interest to actinic radiation, the actinic radiation causing a deprotection reaction within the self-assembled monolayer within the region of interest; as well as The self-assembled monolayer is removed from the region of interest while retaining the self-assembled monolayer on the remaining surface of the substrate.
2. The method of claim 1, wherein: The self-assembled monolayer is a fluorinated material.
3. The method of claim 1, wherein: The self-assembled monolayer is a hyperbranched carbonaceous material.
4. The method of claim 1, wherein: The self-assembled monolayer is applied by vapor deposition.
5. The method of claim 1, further comprising: A metal-containing film is deposited on the substrate by spin-coating deposition and does not fully adhere to the surface coated with the self-assembled monolayer.
6. The method of claim 1, wherein: The self-assembled monolayer includes a chromophore that is reactive to a predetermined wavelength of light.
7. The method of claim 1, wherein: The substrate may further include a beveled edge surface.
8. The method of claim 1, wherein: The region of interest is an inner area of the front surface, which extends from the center point of the front surface to the edge area of the front surface, and the edge area of the front surface is an annular area extending a predetermined distance from the periphery of the front surface toward the center point of the front surface.
9. The method of claim 1, wherein: The region of interest is a central region of the front surface, and a surface area of the central region is smaller than a surface area of the front surface.
10. The method of claim 1, wherein: The self-assembled monolayer has an initial hydrophobic state.
11. The method of claim 1, wherein: Exposing the region of interest with actinic radiation includes delivering a dose of light to the region of interest.
12. The method of claim 11, wherein: The wavelength of the actinic radiation is 266 nm or 365 nm.
13. The method of claim 11, wherein: The light dose desorbs the SAM in the region of interest.
14. The method of claim 1, further comprising: removing the non-sticky portion of the SAM; as well as The remainder of the SAM is used as a tackifier.
15. A method for processing a substrate, the method comprising: a receiving substrate having a front side surface, a back side surface, and side edge surfaces; coating the target area of the front surface with a sacrificial film, the sacrificial film having a surface that prevents a particular material from adhering to the target area; coating the front surface, the back surface, and the side edge surface with a self-assembled monolayer, the self-assembled monolayer being unable to adhere to the sacrificial film, the self-assembled monolayer being hydrophobic; as well as The sacrificial film is removed from a target area of the front side surface.
16. The method of claim 15, wherein: The target area is a central area having a surface area that is smaller than the surface area of the front surface.
17. A method for processing a substrate, the method comprising: a receiving substrate having a front side surface, a back side surface, and side edge surfaces; coating a target area of the front surface with a sacrificial film; Coating the front surface, the back surface and the side edge surface with a self-assembled monolayer, the self-assembled monolayer being hydrophobic; as well as The sacrificial film is removed from the target area of the front surface, wherein removing the sacrificial film also removes the self-assembled monolayer attached to the sacrificial film, thereby leaving the target area free of the self-assembled monolayer.
18. The method of claim 17, wherein: The target area is a central area of the front surface, and the surface area of the central area is smaller than the surface area of the front surface.
19. The method of claim 17, wherein: The self-assembled monolayer is applied by vapor deposition.
20. The method of claim 17, wherein: The self-assembled monolayer is a fluorinated material.